Production method of four-layer co-extrusion BOPP (biaxially-oriented polypropylene) pre-coating film

By introducing automatic thickness measurement equipment in the production process of BOPP pre-coated film, the problems of thickness detection in the existing technology are solved, and accurate measurement of film thickness and edge thickness are achieved, and production efficiency is improved. Product quality.

CN118927583APending Publication Date: 2024-11-12ZHEJIANG JINRUI THIN FILM MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310518912.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The lack of automated thickness detection in the production process of existing BOPP pre-coated films, resulting in insufficient automation of thickness measurement and easy to ignore the 'bending' phenomenon of film edge thickness, affecting product quality.

Method used

Using automatic thickness measurement equipment, the middle and edges of the film block are automatically measured through vacuum suction cups and measuring heads, including designing a rack, a loading rack, a thickness gauge platform and a loading rack, and using a linear module The skateboard realizes automatic pick-up and placement of film blocks, ensuring accurate detection of edge and middle thickness.

Benefits of technology

It realizes the automation of film thickness detection, reduces manual operation, improves detection efficiency, and accurately measure film edge thickness, reduces the probability of "bending" phenomenon, and improves product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118927583A_ABST
    Figure CN118927583A_ABST
Patent Text Reader

Abstract

The invention discloses a production method of a four-layer co-extrusion BOPP (biaxially-oriented polypropylene) precoating film, the BOPP precoating film comprises a base layer, a primer layer and a hot melt adhesive layer which are sequentially arranged from bottom to top, and the upper surface layer is composed of homo-polypropylene and anti-adhesion polypropylene master batch; the inner surface layer consists of homo-polypropylene and an antistatic agent; the core layer is homo-polypropylene; and the lower surface layer consists of homo-polypropylene and anti-adhesion polypropylene master batch. Raw materials of the upper surface layer, the inner surface layer, the core layer and the lower surface layer are fed into respective extruders to be mixed and plasticized, molten melts are fed into die heads respectively, the melts converge in the die heads and then pass through flat die head openings to form molten sheets, then the sheets are attached to chilling rollers through an air knife to be quenched to form unshaped sheets, and the unshaped sheets are subjected to extrusion molding to form the composite material. Then, after water bath cooling, the sheet is shaped to form a cast sheet, the cast sheet passes through a longitudinal drawing machine and a transverse drawing machine, the sheet is drawn into a thin film, and a base layer is prepared;
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of BOPP films, in particular to a production method of a four-layer co-extruded BOPP pre-coated film. Background Art

[0002] Pre-coated film is a flexible packaging material used for printed products. It is first coated with glue on the film by the pre-coated film processing factory according to the specifications and format, and then rewound for the user to choose, and then compounded with the printed product. The existing BOPP pre-coated film will undergo various tests, including testing the thickness of the film. During the test, the pre-cut film pieces are placed one by one on the film thickness gauge for thickness testing, which requires multiple manual placements and is not automated enough. In addition, after the BOPP pre-coated film is produced, there is a small probability of "warping". Warping is the phenomenon that the end diameter of the product is larger than the diameter due to the thickness of the film edge being greater than the average thickness. Because the probability of the "warping" phenomenon is small, it is easy to be ignored. The thickness of the film edge is usually not tested during the inspection, which needs further improvement. Summary of the invention

[0003] In view of the above-mentioned defects of the prior art, an object of the present invention is to provide a method for producing a four-layer co-extruded BOPP pre-coated film.

[0004] To solve the above problems, the technical solution of the present invention is: a method for producing a four-layer co-extruded BOPP pre-coated film, the BOPP pre-coated film comprising a base layer, a primer layer and a hot melt adhesive layer arranged in sequence from bottom to top, the base layer consisting of an upper surface layer, an inner surface layer, a core layer and a lower surface layer; The production method comprises the following steps: (1) The raw materials of the upper surface layer, the inner surface layer, the core layer and the lower surface layer are fed into respective extruders for mixing and plasticizing, and the molten melts are fed into the die heads respectively. After the melts are merged in the die heads, they pass through the flat die head opening to form molten sheets, and then the sheets are attached to the chilled rollers by air knives to be quenched to form unshaped sheets, and then the sheets are shaped to form cast sheets after being cooled in a water bath, and the cast sheets are then respectively passed through the longitudinal stretching machine and the transverse stretching machine to draw the sheets into thin films, thereby obtaining the base layer; (2) Corona treatment of the surface of the base layer; (3) Apply the primer layer on the surface of the base layer and dry it after application; (4) Compounding a layer of hot melt adhesive on the surface of the primer layer, and then cooling and shaping; (5) Testing the size and performance of the film, including measuring the thickness of the film, and measuring the thickness of the middle and edge of the film block by automatic thickness measuring equipment.

[0005] Furthermore, the upper surface layer is composed of homopolypropylene and anti-blocking polypropylene masterbatch; the inner surface layer is composed of homopolypropylene and antistatic agent; the core layer is homopolypropylene; and the lower surface layer is composed of homopolypropylene and anti-blocking polypropylene masterbatch.

[0006] Furthermore, in step (5), the automatic thickness measuring device includes a frame, a material unloading rack, a thickness gauge platform and a material receiving rack. A linear module extending left and right is installed on the upper end of the frame. A slide plate is slidably connected to the front end of the linear module. A vacuum suction cup and a measuring head that can move up and down are installed at the front end of the slide plate. The material unloading rack, the thickness gauge platform and the material receiving rack are located below the material receiving rack and the measuring head.

[0007] Furthermore, a first slide cylinder arranged in the up and down direction is installed on the left side of the front end of the skateboard, a first slide extending up and down is installed at the front end of the first slide cylinder, the lower end of the first slide is fixedly connected to the first lifting platform, and the vacuum suction cup is installed at the lower end of the first lifting platform.

[0008] Furthermore, a second slide cylinder arranged in the up and down direction is installed on the right side of the front end of the skateboard, a second slide extending up and down is installed at the front end of the second slide cylinder, a second lifting platform is fixedly connected to the lower end of the second slide, and a measuring head is installed at the lower end of the second lifting platform.

[0009] Furthermore, the material unwinding rack and the material receiving rack are located on the left and right sides of the thickness gauge platform.

[0010] Furthermore, three rows of measuring heads are installed at the bottom of the second lifting platform, one row of measuring heads is located at the front end edge of the second lifting platform, one row of measuring heads is located in the middle of the second lifting platform, and another row of measuring heads is located at the rear end edge of the second lifting platform.

[0011] Further, measuring the thickness of the film comprises the following steps: (1) Stack multiple cut film blocks up and down and place them on a material rack; (2) The linear module controls the slide to move to the left, moves the vacuum suction cup to the top of the unloading rack, and the first slide cylinder works to control the vacuum suction cup to move downward. The vacuum suction cup sucks a piece of film. The first slide cylinder controls the vacuum suction cup to move upward. Then the slide moves to the right, moves the vacuum suction cup to the top of the thickness gauge platform, and the first slide cylinder controls the vacuum suction cup to move downward. The vacuum suction cup puts down the film block and places the film block on the thickness gauge platform. (3) The slide moves to the left, so that the measuring head moves to the top of the thickness gauge platform. The second slide cylinder controls the measuring head to move downward. The measuring head contacts the film block to measure the thickness. After the measurement, the thickness gauge platform transmits the data to the background computer, and the second slide cylinder controls the measuring head to move upward. (4) The slide plate moves to the right, so that the vacuum suction cup is located directly above the thickness gauge platform. The vacuum suction cup moves downward to suck up the film block on the thickness gauge platform. The slide plate moves to the right, so that the vacuum suction cup moves to directly above the material receiving rack. The vacuum suction cup moves downward to place the measured film block on the material receiving rack.

[0012] Furthermore, the two rows of measuring heads located at the front and rear ends of the second lifting platform measure the edge thickness of the film block, and the row of measuring heads located in the middle of the second lifting platform measures the middle thickness of the film block.

[0013] The beneficial effect of the present invention is that the thickness of the middle position and the edge position of the film block is measured by the automatic thickness measuring device, and multiple manual taking and placing are not required, which is more automated. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a structural schematic diagram of the base layer of the present invention; Figure 2 It is a structural schematic diagram of the automatic thickness measuring device of the present invention; Figure 3 It is a schematic diagram of the distribution of the measuring heads of the present invention.

[0015] As shown in the figure: 1—upper surface layer, 2—inner surface layer, 3—core layer, 4—lower surface layer, 5—frame, 6—unloading rack, 7—thickness gauge platform, 8—collecting rack, 9—linear module, 10—slide plate, 11—vacuum suction cup, 12—measuring head, 13—first slide cylinder, 131—first slide, 14—first lifting platform, 15—second slide cylinder, 151—second slide, 16—second lifting platform. Implementation

[0016] In order to more intuitively and completely understand the technical solution of the present invention, a non-limiting feature description is now provided in conjunction with the accompanying drawings of the present invention as follows: like Figure 1 — Figure 3 As shown, a method for producing a four-layer co-extruded BOPP pre-coated film, the BOPP pre-coated film comprises a base layer, a primer layer and a hot melt adhesive layer arranged in sequence from bottom to top, the base layer consists of an upper surface layer 1, an inner surface layer 2, a core layer 3 and a lower surface layer 4; The production method comprises the following steps: (1) The raw materials of the upper surface layer 1, the inner surface layer 2, the core layer 3 and the lower surface layer 4 are fed into respective extruders for mixing and plasticizing, and the molten melts are respectively fed into the die heads, and the melts are merged in the die heads and then pass through the flat die head opening to form a molten sheet, and then the sheet is attached to a chilled roller by an air knife to be quenched to form an unshaped sheet, and then the sheet is shaped to form a cast sheet after being cooled in a water bath, and the cast sheet is then passed through a longitudinal stretching machine and a transverse stretching machine respectively to draw the sheet into a film, thereby obtaining a base layer; (2) Corona treatment of the surface of the base layer; (3) Apply the primer layer on the surface of the base layer and dry it after application; (4) Compounding a layer of hot melt adhesive on the surface of the primer layer, and then cooling and shaping; (5) Testing the size and performance of the film, including measuring the thickness of the film, and measuring the thickness of the middle and edge of the film block by automatic thickness measuring equipment.

[0017] The upper surface layer 1 is composed of homopolypropylene and anti-blocking polypropylene masterbatch; the inner surface layer 2 is composed of homopolypropylene and antistatic agent; the core layer 3 is homopolypropylene; the lower surface layer 4 is composed of homopolypropylene and anti-blocking polypropylene masterbatch. The components of the upper surface layer 1 are: 95% homopolypropylene, 5% anti-blocking polypropylene masterbatch; the components of the inner surface layer 2 are: 99% homopolypropylene, 1% antistatic agent; the components of the lower surface layer 4 are: 95% homopolypropylene, 5% anti-blocking polypropylene masterbatch.

[0018] In step (5), if Figure 2 As shown, the automatic thickness measuring equipment includes a frame 5, a material unloading frame 6, a thickness gauge platform 7 and a material receiving frame 8. A linear module 9 extending left and right is installed on the upper end of the frame 5. A slide plate 10 is slidably connected to the front end of the linear module 9. A vacuum suction cup 11 and a measuring head 12 that can move up and down are installed at the front end of the slide plate 10. The material unloading frame 6, the thickness gauge platform 7 and the material receiving frame 8 are located below the material receiving frame 8 and the measuring head 12. A first slide cylinder 13 arranged in the up and down direction is installed on the left side of the front end of the slide plate 10. A first slide 131 extending up and down is installed at the front end of the first slide cylinder 13. The lower end of the first slide 131 is fixedly connected to the first lifting platform 14. The vacuum suction cup 11 is installed at the lower end of the first lifting platform 14. A second slide cylinder 15 arranged in the up-down direction is installed on the right side of the front end of the slide 10, and a second slide 151 extending up and down is installed on the front end of the second slide cylinder 15. The lower end of the second slide 151 is fixedly connected to the second lifting platform 16, and the measuring head 12 is installed at the lower end of the second lifting platform 16. The unloading rack 6 and the receiving rack 8 are located on the left and right sides of the thickness gauge platform 7. The linear module 9 is used to drive the slide 10 to move left and right, the first slide cylinder 13 is used to drive the vacuum suction cup 11 to move up and down, and the second slide cylinder 15 is used to drive the measuring head 12 to move up and down.

[0019] Three rows of measuring heads 12 are installed at the bottom of the second lifting platform 16 , one row of measuring heads 12 is located at the front end edge of the second lifting platform 16 , one row of measuring heads 12 is located in the middle of the second lifting platform 16 , and another row of measuring heads 12 is located at the rear end edge of the second lifting platform 16 .

[0020] Measuring the thickness of a film includes the following steps: (1) Stacking a plurality of cut film blocks together and placing them on a material discharging rack 6; (2) The linear module 9 controls the slide plate 10 to move to the left, and moves the vacuum suction cup 11 to the top of the unloading rack 6. The first slide cylinder 13 works to control the vacuum suction cup 11 to move downward. The vacuum suction cup 11 sucks a piece of film. The first slide cylinder 13 controls the vacuum suction cup 11 to move upward. Then the slide plate 10 moves to the right, and the vacuum suction cup 11 moves to the top of the thickness gauge platform 7. The first slide cylinder 13 controls the vacuum suction cup 11 to move downward. The vacuum suction cup 11 puts down the film block, so that the film block is placed on the thickness gauge platform 7. (3) The slide plate 10 moves to the left, so that the measuring head 12 moves to the top of the thickness gauge platform 7. The second slide cylinder 15 controls the measuring head 12 to move downward. The measuring head 12 contacts the film block to measure the thickness. After the measurement, the thickness gauge platform 7 transmits the data to the background computer (not shown in the figure), and the second slide cylinder 15 controls the measuring head 12 to move upward. (4) The slide plate 10 moves to the right, so that the vacuum suction cup 11 is located directly above the thickness gauge platform 7. The vacuum suction cup 11 moves downward to suck up the film block on the thickness gauge platform 7. The slide plate 10 moves to the right, so that the vacuum suction cup 11 moves to directly above the material receiving rack 8. The vacuum suction cup 11 moves downward to place the measured film block on the material receiving rack 8.

[0021] like Figure 3 As shown, the two rows of measuring heads 12 located at the front and rear ends of the second lifting platform 16 measure the edge thickness of the film block, and the row of measuring heads 12 located in the middle of the second lifting platform 16 measures the middle thickness of the film block.

[0022] The present invention measures the thickness of the middle and edge positions of the film block by automatic thickness measuring equipment, and does not need to be manually taken in and out many times. When the film block on the unloading rack 6 is measured, a new film block is placed on it for measurement, and the film block on the receiving rack 8 is taken off together.

Claims

1. A method for producing a four-layer co-extruded BOPP pre-coating film, the BOPP pre-coating film comprising a base layer, a primer layer and a hot melt adhesive layer arranged in sequence from bottom to top, characterized in that: The base layer consists of an upper surface layer, an inner surface layer, a core layer and a lower surface layer; The production method comprises the following steps: (1) The raw materials of the upper surface layer, the inner surface layer, the core layer and the lower surface layer are fed into respective extruders for mixing and plasticizing, and the molten melts are fed into the die heads respectively. After the melts are merged in the die heads, they pass through the flat die head opening to form molten sheets, and then the sheets are attached to the chilled rollers by air knives to be quenched to form unshaped sheets, and then the sheets are shaped to form cast sheets after being cooled in a water bath, and the cast sheets are then respectively passed through the longitudinal stretching machine and the transverse stretching machine to draw the sheets into thin films, thereby obtaining the base layer; (2) Corona treatment of the surface of the base layer; (3) Apply the primer layer on the surface of the base layer and dry it after application; (4) Compounding a layer of hot melt adhesive on the surface of the primer layer, and then cooling and shaping; (5) Testing the size and performance of the film, including measuring the thickness of the film, and measuring the thickness of the middle and edge of the film block by automatic thickness measuring equipment.

2. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 1, characterized in that: The upper surface layer is composed of homopolypropylene and anti-blocking polypropylene masterbatch; the inner surface layer is composed of homopolypropylene and antistatic agent; the core layer is homopolypropylene; and the lower surface layer is composed of homopolypropylene and anti-blocking polypropylene masterbatch.

3. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 1, characterized in that: In step (5), the automatic thickness measuring equipment includes a frame, a material unloading rack, a thickness gauge platform and a material receiving rack. A linear module extending left and right is installed on the upper end of the frame. A slide plate is slidably connected to the front end of the linear module. A vacuum suction cup and a measuring head that can move up and down are installed at the front end of the slide plate. The material unloading rack, the thickness gauge platform and the material receiving rack are located below the material receiving rack and the measuring head.

4. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 3, characterized in that: A first slide cylinder arranged in the up and down direction is installed on the left side of the front end of the skateboard, a first slide extending up and down is installed at the front end of the first slide cylinder, a first lifting platform is fixedly connected to the lower end of the first slide, and a vacuum suction cup is installed at the lower end of the first lifting platform.

5. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 4, characterized in that: A second slide cylinder arranged in the up and down direction is installed on the right side of the front end of the slide plate, a second slide extending up and down is installed at the front end of the second slide cylinder, a second lifting platform is fixedly connected to the lower end of the second slide, and a measuring head is installed at the lower end of the second lifting platform.

6. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 5, characterized in that: The material unwinding rack and material collecting rack are located on the left and right sides of the thickness gauge platform.

7. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 6, characterized in that: Three rows of measuring heads are installed at the bottom of the second lifting platform, one row of measuring heads is located at the front end edge of the second lifting platform, one row of measuring heads is located in the middle of the second lifting platform, and another row of measuring heads is located at the rear end edge of the second lifting platform.

8. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 7, characterized in that: Measuring the thickness of a film includes the following steps: (1) Stack multiple cut film blocks up and down and place them on a material rack; (2) The linear module controls the slide to move to the left, moves the vacuum suction cup to the top of the unloading rack, and the first slide cylinder works to control the vacuum suction cup to move downward. The vacuum suction cup sucks a piece of film. The first slide cylinder controls the vacuum suction cup to move upward. Then the slide moves to the right, moves the vacuum suction cup to the top of the thickness gauge platform, and the first slide cylinder controls the vacuum suction cup to move downward. The vacuum suction cup puts down the film block and places the film block on the thickness gauge platform. (3) The slide moves to the left, so that the measuring head moves to the top of the thickness gauge platform. The second slide cylinder controls the measuring head to move downward. The measuring head contacts the film block to measure the thickness. After the measurement, the thickness gauge platform transmits the data to the background computer, and the second slide cylinder controls the measuring head to move upward. (4) The slide plate moves to the right, so that the vacuum suction cup is located directly above the thickness gauge platform. The vacuum suction cup moves downward to suck up the film block on the thickness gauge platform. The slide plate moves to the right, so that the vacuum suction cup moves to directly above the material receiving rack. The vacuum suction cup moves downward to place the measured film block on the material receiving rack.

9. The method for producing a four-layer co-extruded BOPP pre-coated film according to claim 8, characterized in that: The two rows of measuring heads located at the front and rear ends of the second lifting platform measure the edge thickness of the film block, and the row of measuring heads located in the middle of the second lifting platform measures the middle thickness of the film block.