Method for preparing cigarette carton based on dry-process reconstituted tobacco
The dry reconstructing tobacco leaves to prepare cigarette cartridges has been solved, and the environmental pollution and water resource consumption caused by wet papermaking has been improved, the physical strength and aroma of cigarettes have been improved, and the production effect of environmental protection and energy saving is achieved.
Patent Information
- Application Number
- CN202411299987.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-09-18
AI Technical Summary
The existing cigarette barrel production uses wet papermaking method to cause environmental pollution, and the water resources consumes huge amounts during the production process, and the physical strength and aroma of cigarettes are poor.
The cigarette cartridge was prepared by dry reconstructing tobacco leaves, and the cigarette cartridge with high physical strength and aroma was prepared by cutting, electrostatic powder spraying of cypressol glucoside and hot pressing.
It realizes environmentally friendly smoke barrel production, saves water resources and energy consumption, and improves the physical strength and aroma of cigarettes, and has antibacterial properties.
Smart Images

Figure BDA0005047343020000081 
Figure BDA0005047343020000082 
Figure BDA0005047343020000083
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of tobacco, and in particular relates to a method for preparing a cigarette carton based on dry-process reconstituted tobacco leaves. Background Art
[0002] Cigarette cartons are an important form of cigarette packaging. They use a special machine to arrange a certain number of small boxes of cigarettes neatly, and then use carton sheets to pack them into a carton. This form of packaging plays an important role in the transportation, storage and sales of cigarettes. It not only facilitates these processes, but also effectively protects cigarette products. In general, cigarette cartons have an indispensable position in the cigarette industry. It not only facilitates the transportation, storage and sales of cigarettes, but also provides strong support for the marketing promotion of cigarette brands and consumer experience through its unique design and practicality.
[0003] At present, the production of cigarette cartons usually adopts the wet papermaking method. The wet papermaking process will produce certain environmental pollution, with water pollution being the most serious. Every ton of pulp produced usually requires tens or even hundreds of tons of water, and the wastewater contains a large amount of organic matter, such as lignin, cellulose, etc., with high biochemical oxygen demand (BOD) and much suspended solids (SS). Summary of the invention
[0004] In view of this, the purpose of the present invention is to provide a method for preparing cigarette cartons based on dry-process reconstituted tobacco. The method expands the application field of dry-process reconstituted tobacco, is environmentally friendly, and the prepared cigarette cartons have good physical strength and are rich in tobacco aroma.
[0005] The present invention provides a method for preparing a cigarette carton based on dry reconstituted tobacco leaves, comprising the following steps:
[0006] a) cutting dry-process reconstituted tobacco leaves to obtain tobacco leaves;
[0007] b) spraying coniferyl glucoside on the surface of the tobacco leaf by an electrostatic powder spraying method to obtain a sprayed sheet;
[0008] c) placing one or more of the sprayed sheets in a press, hot pressing and forming them to obtain cigarette carton plates; cutting and assembling the cigarette carton plates to obtain cigarette carton boxes.
[0009] Preferably, in step b), the particle size of the coniferyl glucoside is 300-400 mesh.
[0010] Preferably, in step b), the spraying amount of the coniferyl glucoside is 0.1-0.3 wt % of the absolute dry mass of the tobacco leaf.
[0011] Preferably, in step b), the spraying voltage is 50-90 kV; the spraying current density is 0.5-2 mA / cm 2 .
[0012] Preferably, in step b), the spraying distance is 15 to 25 cm; the spraying speed is 10 to 20 m / min.
[0013] Preferably, in step c), the temperature of the hot pressing is 85-95° C.; the pressure of the hot pressing is 8-9 MPa.
[0014] Preferably, in step c), the hot pressing time is 2 to 3 minutes.
[0015] Preferably, the method further comprises: d) collecting the scraps cut in step a) and step c), crushing them, placing them in a mold and pressing them to obtain cigarette box plates; cutting and assembling the cigarette box plates to obtain cigarette boxes.
[0016] Preferably, in step d), the particle size of the crushed product is 30 to 50 meshes.
[0017] Preferably, in step d), the pressing pressure is 20-30 MPa.
[0018] Compared with the prior art, the present invention provides a method for preparing a cigarette box based on dry-process reconstituted tobacco, comprising the following steps: a) cutting the dry-process reconstituted tobacco to obtain tobacco leaves; b) spraying coniferyl glucoside on the surface of the tobacco leaves by electrostatic powder spraying to obtain a sprayed sheet; c) placing one or more of the sprayed sheets in a press, hot pressing and forming, to obtain a cigarette box board; cutting and assembling the cigarette box boards to obtain a cigarette box. The method provided by the present invention expands the application field of dry-process reconstituted tobacco, is environmentally friendly, and the obtained cigarette box has good physical strength and is rich in tobacco aroma. DETAILED DESCRIPTION
[0019] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0020] The present invention provides a method for preparing a cigarette carton based on dry reconstituted tobacco leaves, comprising the following steps:
[0021] a) cutting dry-process reconstituted tobacco leaves to obtain tobacco leaves;
[0022] b) spraying coniferyl glucoside on the surface of the tobacco leaf by an electrostatic powder spraying method to obtain a sprayed sheet;
[0023] c) placing one or more of the sprayed sheets in a press, hot pressing and forming them to obtain cigarette carton plates; cutting and assembling the cigarette carton plates to obtain cigarette carton boxes.
[0024] In the method provided by the present invention, in step a), the dry-process reconstituted tobacco contains an adhesive, and the adhesive includes but is not limited to carboxymethyl cellulose. More specifically, the dry-process reconstituted tobacco is a reconstituted tobacco product obtained by using a dry-process sheet base prepared by an air-laid process as a coating substrate, transferring a coating liquid containing tobacco particles, tobacco extracts, adhesives and other components to the surface of the substrate by multiple coatings, and drying in multiple stages.
[0025] In the method provided by the present invention, in step a), the cut shape is preferably a square, more preferably a rectangle.
[0026] In the method provided by the present invention, in step b), the particle size of the coniferyl glucoside is preferably 300-400 mesh, specifically 300 mesh, 310 mesh, 320 mesh, 330 mesh, 340 mesh, 350 mesh, 360 mesh, 370 mesh, 380 mesh, 390 mesh or 400 mesh.
[0027] In the method provided by the present invention, in step b), the spraying amount of the coniferyl glucoside is preferably 0.1-0.3wt% of the absolute dry mass of the tobacco leaf, specifically 0.1wt%, 0.11wt%, 0.12wt%, 0.13wt%, 0.14wt%, 0.15wt%, 0.16wt%, 0.17wt%, 0.18wt%, 0.19wt%, 0.2wt%, 0.21wt%, 0.22wt%, 0.23wt%, 0.24wt%, 0.25wt%, 0.26wt%, 0.27wt%, 0.28wt%, 0.29wt% or 0.3wt%.
[0028] In the method provided by the present invention, in step b), the spraying voltage is preferably 50 to 90 kV, specifically 50 kV, 55 kV, 60 kV, 65 kV, 70 kV, 75 kV, 80 kV, 85 kV or 90 kV; the spraying current density is preferably 0.5 to 2 mA / cm 2 , specifically 0.5mA / cm 2 , 0.6mA / cm 2 , 0.7mA / cm 2 , 0.8mA / cm 2 , 0.9mA / cm 2 , 1mA / cm2 , 1.1mA / cm 2 , 1.2mA / cm 2 , 1.25mA / cm 2 , 1.3mA / cm 2 , 1.4mA / cm 2 , 1.5mA / cm 2 , 1.6mA / cm 2 , 1.7mA / cm 2 , 1.8mA / cm 2 , 1.9mA / cm 2 or 2mA / cm 2 ; The spraying distance is preferably 15-25cm, specifically 15cm, 16cm, 17cm, 18cm, 19cm, 20cm, 21cm, 22cm, 23cm, 24cm or 25cm; the spraying speed is preferably 10-20m / min, specifically 10m / min, 11m / min, 12m / min, 13m / min, 14m / min, 15m / min, 16m / min, 17m / min, 18m / min, 19m / min or 20m / min.
[0029] In the method provided by the present invention, in step c), the temperature of the hot pressing is preferably 85-95°C, specifically 85°C, 86°C, 87°C, 88°C, 89°C, 90°C, 91°C, 92°C, 93°C, 94°C or 95°C; the pressure of the hot pressing is preferably 8-9MPa, specifically 8MPa, 8.1MPa, 8.2MPa, 8.3MPa, 8.4MPa, 8.5MPa, 8.6MPa, 8.7MPa, 8.8MPa, 8.9MPa or 9MPa; the time of the hot pressing is preferably 2-3min, specifically 2min, 2.1min, 2.2min, 2.3min, 2.4min, 2.5min, 2.6min, 2.7min, 2.8min, 2.9min or 3min.
[0030] In the method provided by the present invention, it is preferred to further include the following steps: d) collecting the scraps cut in step a) and step c), crushing them, placing them in a mold and pressing them to obtain cigarette box plates; cutting and assembling the cigarette box plates to obtain cigarette boxes.
[0031] In the method provided by the present invention, in step d), the mass ratio of the scraps from step a) to the scraps from step c) is preferably 1:(1-5), specifically 1:1, 1:2, 1:3, 1:4 or 1:5.
[0032] In the method provided by the present invention, in step d), the particle size of the crushed material is preferably 30-50 mesh, specifically 30 mesh, 35 mesh, 40 mesh, 45 mesh or 50 mesh.
[0033] In the method provided by the present invention, in step d), the pressing temperature is preferably 85-95°C, specifically 85°C, 86°C, 87°C, 88°C, 89°C, 90°C, 91°C, 92°C, 93°C, 94°C or 95°C; the pressing pressure is preferably 20-30MPa, specifically 20MPa, 21MPa, 22MPa, 23MPa, 24MPa, 25MPa, 26MPa, 27MPa, 28MPa, 29MPa or 30MPa; the pressing time is preferably 2-3min, specifically 2min, 2.1min, 2.2min, 2.3min, 2.4min, 2.5min, 2.6min, 2.7min, 2.8min, 2.9min or 3min.
[0034] The method provided by the present invention expands the application field of dry-process reconstituted tobacco leaves, is environmentally friendly, and the prepared cigarette carton has good physical strength and rich tobacco aroma. More specifically, the method of the present invention has the following advantages:
[0035] (1) At present, the production of cigarette cartons usually adopts the wet papermaking method. Compared with the traditional wet papermaking, dry papermaking has significant advantages: 1. Environmental protection. The biggest advantage of dry papermaking is that it does not use water as a production medium, thus avoiding the consumption of a large amount of water resources. 2. Energy saving. The production process of dry papermaking is relatively simple. It does not require high energy consumption steps such as cooking and bleaching like wet papermaking, so the energy consumption is lower. The dry-process reconstituted tobacco leaf is a dry-process sheet base made by the air-laid process as the coating substrate. The coating liquid containing tobacco particles, tobacco extracts and other components is transferred to the surface of the substrate by multiple coatings, and the reconstituted tobacco leaf product is obtained by multi-stage drying. Therefore, the process of preparing cigarette cartons based on dry-process reconstituted tobacco leaves is energy-saving and environmentally friendly, and the finished product is rich in tobacco aroma.
[0036] (2) In the production process of dry reconstituted tobacco, adhesives play a vital role. Adhesives can effectively bond tobacco fragments such as tobacco stems and tobacco dust together to form reconstituted tobacco with certain strength and flexibility. Therefore, under the action of high temperature and high pressure, the adhesive will reassemble, making the bonding between fibers tighter and giving the cigarette box better physical strength.
[0037] (3) Coniferyl alcohol glucoside is a lignin precursor with a variety of important biological and chemical properties. This compound can undergo polymerization with polysaccharides under the action of enzymes to produce dehydrogenated polymers (DHP) and a complex of the polymer and holocellulose. Coniferyl alcohol glucoside can inhibit fungal growth and melanization reactions. Therefore, the cigarette cartons prepared with coniferyl alcohol glucoside have antibacterial properties.
[0038] For the purpose of greater clarity, the invention is described in detail through the following examples.
[0039] In the following embodiments provided by the present invention, the dry-process reconstituted tobacco leaves used are prepared according to the following method:
[0040] (1) Hydrothermal treatment: 50-mesh tobacco straw powder and deionized water were mixed in a ratio of 1:8, and then heated to 160° C. in a hydrothermal reactor (with continuous stirring) and kept warm for 1.5 h. After cooling, the mixed solution was taken out and filtered to obtain a hydrothermal treatment raw material and a tobacco extract;
[0041] (2) Preparation of kraft softwood pulp: the ratio of spruce wood to cooking liquor was 1:5, the amount of alkali (the percentage of the amount of sodium hydroxide during cooking to the absolute dry raw material mass) was 18%, the degree of sulfidation was 25%, the amount of anthraquinone was 0.05%, the maximum cooking temperature was 165°C, the heating time was 2 hours, and the holding time was 2.5 hours;
[0042] (3) washing, screening and cleaning the slurry obtained in step (2);
[0043] (4) mixing the slurry obtained in step (3) with the tobacco extract prepared in step (1) in a volume ratio of 1:10, adding 1 g / L vanillin, and then immersing at 60° C. for 48 h;
[0044] (5) After the slurry in step (4) is dried, fluff pulp fibers are obtained, which are sent to the interior of a forming device by a feeding fan, and are broken up into dispersed fibers by a breaking roller rotating at high speed, and then filtered through a circular sieve. Under the adsorption effect of a negative pressure box, the wood pulp fibers are evenly dropped onto a forming mesh belt to obtain a substrate, and the thickness of the substrate is 0.6 mm;
[0045] (6) preparing a coating liquid (comprising 300 mesh burley tobacco powder particles, carboxymethyl cellulose adhesive, and glycerin atomizer), wherein the mass concentration of tobacco powder in the coating liquid is 30%, the mass concentration of adhesive is 1%, and the mass concentration of atomizer is 5%, and coating the coating liquid on the surface of the substrate in step (5) to a coating thickness of 1 mm;
[0046] (7) subjecting the substrate coated with the coating liquid obtained in step (6) to multi-stage drying to obtain dry-process reconstituted tobacco leaves; the multi-stage drying system has a total of 5 ovens, a hot air temperature of 100° C., and a vehicle speed of 100 m / min.
[0047] The basic performance parameters of the dry reconstituted tobacco leaves prepared by the above method are as follows: Basis weight: 218.1 g / m 2 , tensile index: 22.85N·m / g, elongation: 1.88%, tear index: 5.25mN·m 2 / g.
[0048] Example 1
[0049] (1) Cutting: Cut the dry-process reconstituted tobacco leaves into rectangles of 40 cm × 50 cm;
[0050] (2) Spraying coniferyl glucoside: Grind coniferyl glucoside into 300-mesh particles, and spray the coniferyl glucoside particles on the surface of dry-process reconstituted tobacco leaves by electrostatic powder spraying; wherein the amount of coniferyl glucoside is 0.1 wt % of the mass of the absolute dry-process reconstituted tobacco leaves, the spraying voltage is 50 kV, and the spraying current density is 0.5 mA / cm 2 , spraying distance is 15cm, spraying speed is 10m / min;
[0051] (3) Hot pressing and carton assembly: placing the dry-process reconstituted tobacco leaves sprayed with coniferyl glucoside in a press at a temperature of 85° C., a pressure of 8 MPa, and a time of 2 min to obtain a cigarette carton plate; cutting and assembling the cigarette carton plate to obtain a cigarette carton①;
[0052] (4) Collect the remaining scraps from (1) and (3), mix them evenly in a mass ratio of 1:2, and crush them into 30 meshes. Press them into shape in a mold with a length of 40 cm, a width of 50 cm, and a height of 1.5 mm at a pressing temperature of 85° C., a pressure of 20 MPa, and a pressing time of 2 min to obtain a cigarette box plate; cut and assemble the cigarette box plate to obtain cigarette box ②.
[0053] Example 2
[0054] (1) Cutting: Cut the dry-process reconstituted tobacco leaves into rectangles of 40 cm × 50 cm;
[0055] (2) Spraying coniferyl glucoside: grinding coniferyl glucoside into 350 mesh particles, and spraying the coniferyl glucoside particles on the surface of dry-process reconstituted tobacco leaves by electrostatic powder spraying; wherein the amount of coniferyl glucoside used is 0.2 wt % of the mass of the absolute dry-process reconstituted tobacco leaves, the spraying voltage is 70 kV, and the spraying current density is 1.25 mA / cm 2, spraying distance is 20cm, spraying speed is 15m / min;
[0056] (3) Hot pressing and carton assembly: placing the dry-process reconstituted tobacco leaves sprayed with coniferyl glucoside in a press at a temperature of 90° C., a pressure of 8.5 MPa, and a time of 2.5 min to obtain a cigarette carton plate; cutting and assembling the cigarette carton plate to obtain a cigarette carton①;
[0057] (4) Collect the remaining scraps from (1) and (3), mix them evenly in a mass ratio of 1:2, and then crush them into 40 meshes. Press them in a mold with a length of 40 cm, a width of 50 cm, and a height of 1.5 mm at a pressing temperature of 90° C., a pressure of 25 MPa, and a pressing time of 2.5 min to obtain a cigarette box plate; cut and assemble the cigarette box plate to obtain cigarette box ②.
[0058] Example 3
[0059] (1) Cutting: Cut the dry-process reconstituted tobacco leaves into rectangles of 40 cm × 50 cm;
[0060] (2) Spraying coniferyl glucoside: Grind coniferyl glucoside into 400 mesh particles, and spray the coniferyl glucoside particles on the surface of dry-process reconstituted tobacco leaves by electrostatic powder spraying; wherein the amount of coniferyl glucoside is 0.3 wt % of the mass of the absolute dry-process reconstituted tobacco leaves, the spraying voltage is 90 kV, and the spraying current density is 2 mA / cm 2 , spraying distance is 25cm, spraying speed is 20m / min;
[0061] (3) Hot pressing and carton assembly: placing the dry-process reconstituted tobacco leaves sprayed with coniferyl glucoside in a press at a temperature of 95° C., a pressure of 9 MPa, and a time of 3 min to obtain a cigarette carton plate; cutting and assembling the cigarette carton plate to obtain a cigarette carton①;
[0062] (4) Collect the remaining scraps from (1) and (3), mix them evenly in a mass ratio of 1:2, and then crush them into 50 mesh. Press them in a mold with a length of 40 cm, a width of 50 cm, and a height of 1.5 mm at a pressing temperature of 95° C., a pressure of 30 MPa, and a pressing time of 3 min to obtain a cigarette box plate; cut and assemble the cigarette box plate to obtain cigarette box ②.
[0063] Performance Evaluation
[0064] The performance tests were conducted on the cigarette box plates prepared in Examples 1 to 3 of the present invention. The specific test methods and test results are as follows:
[0065] (1) Static bending strength analysis (three-point bending)
[0066] The static bending strength of three-point bending is measured by applying a load to the middle of the specimen supported at two points. It is to determine the ratio of the bending moment and the bending section modulus of the specimen when the maximum load is applied. Cut a specimen of size 15mm×200mm and place the specimen in an environment with a temperature of (20±2)℃ and a relative humidity of (65±5)% until the mass is constant. The mass is considered constant if the difference between the two weighing results 24 hours apart does not exceed 0.1% of the mass of the specimen. Adjust the span of the two supports to at least 20 times the basic thickness of the specimen, and measure the center distance of the supports to an accuracy of 0.5mm. The specimen is placed flat on the support, with the long axis of the specimen perpendicular to the support roller and the center point of the specimen below the loading roller.
[0067] Load at a constant rate throughout the test. Adjust the loading speed so that the maximum load is reached within (60 ± 30) s. Record the maximum load to the nearest 1% of the measured value.
[0068] The static bending strength of the sample is calculated according to the following formula, accurate to 0.1MPa:
[0069]
[0070] Where:
[0071] ρ b ——static bending strength of the specimen, in megapascals (MPa);
[0072] F max ——The maximum load when the specimen fails, in Newton (N);
[0073] l 1 ——The distance between the two supports, in millimeters (mm);
[0074] b——specimen width, in millimeters (mm);
[0075] t——specimen thickness, in millimeters (mm).
[0076] (2) Internal bonding strength measurement
[0077] Internal bond strength is the measurement of the tensile strength of the sample surface when it is subjected to uniformly distributed tensile force until it is destroyed. Internal bond strength is the ratio of the maximum destructive tensile force perpendicular to the sample surface to the sample area.
[0078] Apply epoxy resin glue or melted hot melt glue or similar adhesive evenly on the surface of the chuck to bond the specimen to the chuck. Remove the glue squeezed out of the glue layer. Place the assembly in the clamping device and load until the specimen fails. The entire test should be loaded evenly, and the specimen should fail within (60±30)s from the start of loading. Record the maximum load value with an accuracy of 1%.
[0079] The internal bonding strength is calculated according to the following formula:
[0080]
[0081] Where:
[0082] σ ⊥ ——Internal bond strength of the specimen, in megapascals (MPa);
[0083] F max ——The maximum load when the specimen fails, in Newton (N);
[0084] l——specimen length, in millimeters (mm);
[0085] b——specimen width, in millimeters (mm).
[0086] (3) Test results:
[0087]
[0088] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for preparing cigarette cartons based on dry reconstituted tobacco leaves, It is characterized in that The following steps are involved: a) cutting dry-process reconstituted tobacco leaves to obtain tobacco leaves; b) spraying coniferyl glucoside on the surface of the tobacco leaf by an electrostatic powder spraying method to obtain a sprayed sheet; c) placing one or more of the sprayed sheets in a press, hot pressing and forming them to obtain cigarette carton plates; cutting and assembling the cigarette carton plates to obtain cigarette carton boxes.
2. The method according to claim 1, It is characterized in that In step b), the particle size of the coniferyl glucoside is 300-400 meshes.
3. The method according to claim 1, It is characterized in that In step b), the spraying amount of the coniferyl glucoside is 0.1-0.3 wt % of the absolute dry mass of the tobacco leaf.
4. The method according to claim 1, It is characterized in that In step b), the spraying voltage is 50-90 kV; the spraying current density is 0.5-2 mA / cm 2 .
5. The method according to claim 1, It is characterized in that In step b), the spraying distance is 15 to 25 cm; the spraying speed is 10 to 20 m / min.
6. The method according to claim 1, It is characterized in that In step c), the temperature of the hot pressing is 85-95° C.; the pressure of the hot pressing is 8-9 MPa.
7. The method according to claim 1, It is characterized in that In step c), the hot pressing time is 2 to 3 minutes.
8. The method according to claim 1, It is characterized in that Also includes: d) collecting the scraps cut from step a) and step c), crushing them, placing them in a mold and pressing them to obtain cigarette box plates; cutting and assembling the cigarette box plates to obtain cigarette boxes.
9. The method according to claim 8, It is characterized in that In step d), the particle size of the crushed product is 30 to 50 meshes.
10. The method according to claim 8, It is characterized in that In step d), the pressing pressure is 20-30 MPa.
Citation Information
Patent Citations
Flame-retarding waterproof antibacterial board paint
CN105086551A
Method of preparing cigarette packet or carton packaging paper with tobacco stalks
CN110055787A
Manufacturing process of tobacco bale carton capable of being mechanically baled
CN115742451A
Dry-process reconstituted tobacco with antibacterial property and preparation method of dry-process reconstituted tobacco
CN116250648A
Dry-process reconstituted tobacco and preparation method thereof
CN116268524A
Cited By
Preparation method of tobacco extract stabilizing module based on physicochemical separation technology, tobacco extract stabilizing module and application of tobacco extract stabilizing module
CN120549270A