Light-emitting substrate, preparation method thereof and light-emitting device
Patent Information
- Application Number
- CN202380008296.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-15
- Publication Date
- 2024-11-15
AI Technical Summary
The traditional light-emitting substrate has a high welding void rate, resulting in high contact resistance between the light-emitting element and the driving substrate, and reduced photoelectric conversion efficiency.
A light-emitting substrate is designed, which includes a base substrate and a multi-layer metal pattern structure. By forming a mushroom-shaped top surface and a groove structure on the first metal pattern, combined with the coverage of the passivation layer and the second metal pattern, a full-scale structure is formed. All-round anti-oxidation protection and improved welding quality through fine seam structure.
It reduces the welding porosity, reduces the contact resistance, improves the photoelectric conversion rate and reliability, extends the repair times of the light-emitting components, and meets the needs of high partitions and high brightness.
Smart Images

Figure CN118974934A_ABST
Abstract
Description
Luminescent substrate and preparation method thereof, and luminescent device Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to a light-emitting substrate and a preparation method thereof, and a light-emitting device. Background Art
[0002] Compared to LCD and OLED displays, LED displays offer significant advantages in image quality, refresh rate, power consumption, and brightness. These advantages have led to a wide range of applications for LED displays, including traditional displays, near-eye displays, 3D displays, and transparent displays.
[0003] Overview
[0004] The present disclosure provides a light-emitting substrate, comprising:
[0005] a substrate; and
[0006] A first metal pattern is provided on one side of the base substrate, comprising: a first surface away from the base substrate, a second surface close to the base substrate, and a first side surface connecting the first surface and the second surface, wherein the first surface comprises a middle area and an edge area located outside the middle area;
[0007] The first surface is convex toward a side away from the base substrate, and the convex height of the middle area is greater than the convex height of the edge area.
[0008] In some embodiments, the first surface further comprises:
[0009] The secondary middle region is located between the middle region and the edge region, and the raised height of the secondary middle region is smaller than the raised height of the middle region and larger than the raised height of the edge region.
[0010] In some embodiments, the height of the protrusions of the first surface gradually decreases from the center of the first surface to the edge of the first surface; and
[0011] A ratio of a difference between the protrusion heights of the middle region and the edge region to the protrusion height of the edge region is greater than or equal to 0.1 and less than or equal to 0.4.
[0012] In some embodiments, the orthographic projection of the first surface on the base substrate covers the orthographic projection of the second surface on the base substrate, and the orthographic projection area of the first surface on the base substrate is larger than the orthographic projection area of the second surface on the base substrate.
[0013] In some embodiments, the angle between the first side surface and the second surface is greater than or equal to 80° and less than or equal to 120°.
[0014] In some embodiments, the first metal pattern further includes:
[0015] The first cross section is parallel to the base substrate and intersects with the edge of the first surface. The angle between the first cross section and the first side surface is an acute angle.
[0016] In some embodiments, the first side surface has a groove recessed toward the inside of the first metal pattern, and the groove is located on the first side surface close to the base substrate.
[0017] In some embodiments, the light-emitting substrate further comprises:
[0018] The second metal pattern is arranged on a side of the first metal pattern away from the base substrate, and the second metal pattern completely covers the first surface and the first side surface.
[0019] In some embodiments, the second metal pattern has a thin gap, and the thin gap is close to the intersection of the first side surface and the second surface.
[0020] In some embodiments, the light-emitting substrate further comprises:
[0021] a passivation layer, disposed on a side of the first metal pattern facing away from the base substrate, the passivation layer being provided with a first opening, the first opening being used to expose a middle area of the first surface, the passivation layer at least covering an edge area and the first side surface of the first surface; and
[0022] A second metal pattern is arranged on a side of the passivation layer facing away from the base substrate, the second metal pattern completely covers the middle area of the first surface, and the orthographic projection of the second metal pattern on the base substrate at least partially covers the orthographic projection of the passivation layer on the base substrate.
[0023] In some embodiments, an orthographic projection boundary of the second metal pattern on the base substrate is located between an orthographic projection boundary of the first opening on the base substrate and an orthographic projection boundary of the first metal pattern on the base substrate.
[0024] In some embodiments, an orthographic projection boundary of the second metal pattern on the base substrate is located on a side of an orthographic projection boundary of the first metal pattern on the base substrate away from an orthographic projection of the first opening on the base substrate.
[0025] In some embodiments, the light-emitting substrate further comprises:
[0026] A flat layer is located between the passivation layer and the second metal pattern, the orthographic projection of the flat layer on the base substrate completely overlaps with the orthographic projection of the passivation layer on the base substrate, and the surface of the flat layer facing away from the base substrate is parallel to the plane of the base substrate.
[0027] In some embodiments, the light-emitting substrate further comprises:
[0028] an isolation layer, arranged between the flat layer and the second metal pattern, a second opening being provided on the isolation layer, an orthographic projection of the second opening on the base substrate at least partially overlapping with an orthographic projection of the first opening on the base substrate, and the isolation layer covering a surface of the flat layer facing the second metal pattern and a side surface of the flat layer facing the first opening.
[0029] In some embodiments, the planar layer includes a first planar pattern, the first planar pattern overlaps with the first metal pattern in a normal direction of the base substrate, and a thickness of the first planar pattern is greater than 0 and less than or equal to 1 micron.
[0030] In some embodiments, a thickness of the second metal pattern located on a side of the first metal pattern facing away from the base substrate is greater than or equal to 2000 angstroms and less than or equal to 6000 angstroms.
[0031] In some embodiments, the thickness of the passivation layer located on a side of the first metal pattern facing away from the base substrate is greater than or equal to 2000 angstroms.
[0032] In some embodiments, the orthographic projection boundary of the first metal pattern on the base substrate is located within the orthographic projection boundary of the second metal pattern on the base substrate, and the distance between the orthographic projection boundary of the first metal pattern on the base substrate and the orthographic projection boundary of the second metal pattern on the base substrate is greater than or equal to 0.5 microns and less than or equal to 1.5 microns.
[0033] In some embodiments, the orthographic projection boundary of the first opening on the base substrate is located within the orthographic projection boundary of the second metal pattern on the base substrate, and the distance between the orthographic projection boundary of the first opening on the base substrate and the orthographic projection boundary of the second metal pattern on the base substrate is greater than or equal to 1 micron and less than or equal to 3 microns.
[0034] In some embodiments, a material of the second metal pattern includes at least one of the following: a nickel-vanadium alloy, a nickel-tungsten alloy, and a copper-nickel alloy.
[0035] In some embodiments, an angle formed by the intersection of the first surface and the first side surface is a rounded angle.
[0036] In some embodiments, the thickness of the first metal pattern is greater than or equal to 4 micrometers and less than or equal to 10 micrometers.
[0037] The present disclosure provides a light emitting device, comprising:
[0038] The light-emitting substrate according to any one of the embodiments; and
[0039] A light emitting diode is arranged on a side of the first metal pattern away from the base substrate and is connected to the first metal pattern. The first metal pattern is used to provide a driving signal to the light emitting diode to drive the light emitting diode to emit light.
[0040] The present disclosure provides a method for preparing a light-emitting substrate, comprising:
[0041] providing a substrate;
[0042] A first metal pattern is formed on one side of the base substrate, the first metal pattern including: a first surface away from the base substrate, a second surface close to the base substrate, and a first side surface connecting the first surface and the second surface, the first surface including a middle area and an edge area located outside the middle area; wherein the first surface bulges toward the side away from the base substrate, and the bulge height of the middle area is greater than the bulge height of the edge area.
[0043] In some embodiments, the step of forming a first metal pattern on one side of the base substrate includes:
[0044] forming a seed layer on one side of the substrate;
[0045] patterning a pattern defining layer on a side of the seed layer facing away from the base substrate, wherein the pattern defining layer is made of a removable insulating material and has a plurality of openings to expose the seed layer at corresponding positions;
[0046] forming a first metal material layer in the opening of the pattern defining layer;
[0047] removing the pattern defining layer;
[0048] An etching process is used to remove the portion of the seed layer not covered by the first metal material layer to form the first metal pattern. The first metal pattern includes the seed layer and the first metal material layer remaining after the etching process is completed.
[0049] In some embodiments, an angle between a side surface of the pattern defining layer facing the opening and a bottom surface of the pattern defining layer close to the base substrate is greater than or equal to 60° and less than or equal to 100°.
[0050] In some embodiments, the pattern defining layer includes at least one of the following:
[0051] A resin material having a relative molecular weight greater than or equal to 30,000 and less than or equal to 50,000; and
[0052] The photosensitizer has a mass fraction greater than or equal to 20%.
[0053] The above description is only an overview of the technical solution of the present disclosure. In order to more clearly understand the technical means of the present disclosure, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present disclosure more obvious and easy to understand, the specific implementation methods of the present disclosure are listed below.
[0054] BRIEF DESCRIPTION OF THE DRAWINGS
[0055] In order to more clearly illustrate the technical solutions in the embodiments of the present disclosure or related technologies, the following is a brief introduction to the drawings required for the description of the embodiments or related technologies. Obviously, the drawings described below are some embodiments of the present disclosure. For those skilled in the art, other drawings can be obtained based on these drawings without inventive efforts. It should be noted that the scales in the drawings are for illustration only and do not represent the actual scale.
[0056] FIG1 exemplarily shows a cross-sectional structural diagram of a light-emitting substrate provided by the present disclosure;
[0057] 2 to 8 exemplarily show schematic cross-sectional views of several light-emitting substrate embodiments;
[0058] FIG9 shows the optical reflectivity-wavelength curves of nickel-vanadium alloy under several annealing conditions;
[0059] Figure 10 shows the morphology of the solder paste after reflow;
[0060] FIG11 shows a cross-sectional view of a light-emitting substrate;
[0061] FIG12 shows a cross-sectional view of another light-emitting substrate;
[0062] FIG. 13 shows a cross-sectional structural diagram of a pattern defining layer.
[0063] Detailed description
[0064] To make the objectives, technical solutions, and advantages of the embodiments of the present disclosure more clear, the technical solutions in the embodiments of the present disclosure will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present disclosure, not all of the embodiments. All other embodiments obtained by ordinary technicians in this field based on the embodiments of the present disclosure without making any creative efforts shall fall within the scope of protection of the present disclosure.
[0065] In related technologies, a light-emitting substrate includes a driver substrate and a light-emitting element soldered to the driver substrate. The light-emitting element and the driver substrate are connected by solder. The inventors discovered that conventional light-emitting substrates suffer from a high solder void rate, resulting in high contact resistance between the light-emitting element and the driver substrate and reduced photoelectric conversion efficiency.
[0066] Referring to FIG1 , a schematic cross-sectional view of a light-emitting substrate provided by the present disclosure is shown. As shown in FIG1 , the light-emitting substrate includes: a base substrate 10; and a first metal pattern 11, which is disposed on one side of the base substrate 10. The first metal pattern 11 includes: a first surface S1 away from the base substrate 10, a second surface S2 close to the base substrate 10, and a first side surface S3 connecting the first surface S1 and the second surface S2. The first surface S1 includes a middle region and an edge region located outside the middle region. The first surface S1 is convex toward the side away from the base substrate 10, and the convex height of the middle region is greater than the convex height of the edge region.
[0067] As shown in FIG. 1 , the first metal pattern 11 further includes a first cross section P1 . The first cross section P1 is parallel to the base substrate 10 and intersects with an edge of the first surface S1 .
[0068] In the present disclosure, as shown in FIG1 , for any point A1 on the first surface S1 , the protrusion height H of point A1 is the distance between point A1 and the first cross-section P1 .
[0069] 1 , the middle region is a region of the first surface S1 close to the center of the first surface S1 , and the edge region is a region of the first surface S1 close to the edge of the first surface S1 .
[0070] When a light-emitting element (such as an LED) is soldered on the side of the first surface S1 facing away from the base substrate 10, since the protrusion height of the middle area of the first surface S1 is greater than the protrusion height of the edge area, during the soldering process, the light-emitting element first contacts the middle area of the first surface S1. In this way, bubbles in the solder can be discharged in time before the light-emitting element contacts the edge area, thereby reducing the soldering void rate, improving the soldering firmness, reducing the contact resistance, and thereby improving the photoelectric conversion rate and reliability.
[0071] In some embodiments, as shown in FIG1 , the first surface S1 further includes: a secondary middle region located between the middle region and the edge region, wherein a convex height of the secondary middle region is smaller than a convex height of the middle region and larger than a convex height of the edge region.
[0072] As shown in Figure 1, since the protrusion heights of the middle area, the sub-middle area and the edge area decrease in sequence, during the welding process, the light-emitting element first contacts the middle area of the first surface S1, and the bubbles in the solder in the middle area can be discharged in time before the light-emitting element contacts the sub-middle area, and then the light-emitting element contacts the sub-middle area, and the bubbles in the solder in the sub-middle area can be discharged in time before the light-emitting element contacts the edge area. This embodiment can further reduce the welding void rate, improve welding firmness, reduce contact resistance, and thus improve the photoelectric conversion rate and reliability.
[0073] In some embodiments, as shown in FIG1 , the height of the protrusion of the first surface S1 gradually decreases from the center of the first surface S1 to the edge of the first surface S1 , which can further reduce the welding void rate.
[0074] As shown in FIG1 , the top surface of the first metal pattern 11 forms a mushroom-shaped bulge, with the bulge being the highest at the center of the first surface S1 and gradually decreasing in height as it approaches the edge of the first surface S1. When the second surface S2 is a plane, as shown in FIG1 , the thickness of the first metal pattern 11 gradually decreases from the center of the first surface S1 to the edge of the first surface S1.
[0075] In some embodiments, the difference between the protrusion height of the middle region and the protrusion height of the edge region may be greater than or equal to 1 micrometer and less than or equal to 2 micrometers, such as 1.5 micrometers.
[0076] In some embodiments, the ratio of the difference between the protrusion heights of the middle region and the edge region to the protrusion height of the edge region is greater than or equal to 0.1 and less than or equal to 0.4, such as 0.2, 0.3, etc.
[0077] In some embodiments, the material of the first metal pattern 11 may include one or more metals such as copper, silver, and gold.
[0078] In some embodiments, the angle α formed by the intersection of the first surface S1 and the first side surface S3 is rounded. As shown in FIG1 , the rounded angle α, rather than the sharp angle, facilitates the subsequent film layer to completely cover the first metal pattern 11, especially the first side surface S3, thereby providing better protection for the first metal pattern 11.
[0079] In some embodiments, the angle σ between the first cross-section P1 and the first side surface S3 is an acute angle.
[0080] In order to allow subsequent film layers to completely cover the first side surface S3 of the first metal pattern 11 , in some embodiments, the angle σ between the first cross section P1 and the first side surface S3 may be an acute angle greater than or equal to 60°, such as 70°, 80°, etc.
[0081] In some embodiments, as shown in FIG. 1 , the orthographic projection of the first surface S1 on the base substrate 10 covers the orthographic projection of the second surface S2 on the base substrate 10 , and the orthographic projection area of the first surface S1 on the base substrate 10 is larger than the orthographic projection area of the second surface S2 on the base substrate 10 .
[0082] As shown in FIG1 , the longitudinal section (perpendicular to the base substrate 10 ) of the first metal pattern 11 is approximately an inverted trapezoid, with the short side of the inverted trapezoid close to the base substrate 10 and the long side being a convex arc.
[0083] The inventors have discovered that each time a light-emitting element is replaced or repaired, the thickness of the first metal pattern 11 decreases, which limits the number of repairs possible or increases the resistance of the first metal pattern 11. To address this issue, in some embodiments, the thickness of the first metal pattern 11 is greater than or equal to 4 microns and less than or equal to 10 microns, such as 5 microns, 6 microns, 8 microns, 9 microns, etc.
[0084] In this way, by setting the first metal pattern 11 with a larger thickness, the resistance of the first metal pattern 11 can be reduced, meeting the requirements of high partition and high brightness, and increasing the number of repairable times of the light-emitting element, thereby improving the performance and reliability of the light-emitting substrate.
[0085] In some embodiments, as shown in FIG1 , the angle β between the first side surface S3 and the second surface S2 is less than or equal to 120°. This facilitates subsequent film layers to completely cover the first metal pattern 11 , especially the first side surface S3 , thereby providing better anti-oxidation protection.
[0086] Furthermore, as shown in FIG1 , the angle β between the first side surface S3 and the second surface S2 may be greater than or equal to 80°. For example, the angle β between the first side surface S3 and the second surface S2 may be 90°, 100°, 110°, etc.
[0087] In some embodiments, as shown in FIG1 , the first side surface S3 has a groove 12 that is recessed toward the interior of the first metal pattern 11, and the groove 12 is located at a position on the first side surface S3 close to the base substrate 10. The groove 12 may be located at a position where the first side surface S3 intersects with the second surface S2, or may be located on the first side surface S3 at a position closer to the intersection of the first side surface S3 and the second surface S2.
[0088] It has been verified that when the angle β between the first side surface S3 and the second surface S2 is less than or equal to 120°, the groove 12 on the first side surface S3 can basically be wrapped by the subsequent film layer, and the first metal pattern 11 is not obviously oxidized, which will not affect product reliability.
[0089] In order to prevent the material of the first metal pattern 11 from being oxidized, in some embodiments, as shown in FIG2 , the light-emitting substrate further includes: a second metal pattern 21 , which is arranged on the side of the first metal pattern 11 away from the base substrate 10 , and the second metal pattern 21 completely covers the first surface S1 and the first side surface S3 .
[0090] As shown in FIG. 2 , the second metal pattern 21 completely wraps the exposed first surface S1 and first side surface S3 of the first metal pattern 11 , thereby fully protecting the first metal material and preventing oxidation.
[0091] To ensure that the second metal pattern 21 fully covers the first side surface S3, in some embodiments, as shown in FIG2 , the thickness H1 of the second metal pattern 21 on the first side surface S3 is greater than or equal to 500 angstroms, which can provide a good anti-oxidation effect on the first side surface S3.
[0092] In a specific implementation, due to factors such as the film formation process, the thickness of the first metal pattern 11, and the angle of the first side surface S3, the thickness H1 of the second metal pattern 21 on the first side surface S3 is less than the thickness H2 of the second metal pattern 21 on the first surface S1. For example, the thickness H1 of the second metal pattern 21 on the first side surface S3 is 1 / 4 of the thickness H2 of the second metal pattern 21 on the first surface S1. Therefore, to ensure that the thickness H1 of the second metal pattern 21 on the first side surface S3 is greater than or equal to 500 angstroms, the thickness H2 of the second metal pattern 21 on the first surface S1 can be greater than or equal to 2000 angstroms.
[0093] In some embodiments, the thickness H2 of the second metal pattern 21 located on the first surface S1 may be less than or equal to 6000 angstroms, which is not limited in the present disclosure.
[0094] For example, a magnetron sputtering process may be used to form a film, and then a photolithography process may be used to pattern the second metal pattern 21 .
[0095] As shown in Figure 2, the orthographic projection of the second metal pattern 21 on the base substrate 10 completely covers the orthographic projection of the first metal pattern 11 on the base substrate 10, and the orthographic projection area of the second metal pattern 21 on the base substrate 10 is larger than the orthographic projection area of the first metal pattern 11 on the base substrate 10.
[0096] In order to ensure that the second metal pattern 21 fully covers the first metal pattern 11, in some embodiments, as shown in Figure 2, the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 is located within the orthographic projection boundary of the second metal pattern 21 on the base substrate 10, and the distance between the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 (L1 as shown in Figure 2) is greater than or equal to 0.5 microns and less than or equal to 1.5 microns.
[0097] As shown in Figure 2, the distance between the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is defined as the first wrap length L1. The design value of the first wrap length L1 can be set to 1 micron. Due to the presence of alignment errors between different layers during the manufacturing process, the final first wrap length L1 is generally greater than or equal to 0.5 microns and less than or equal to 1.5 microns. This prevents the position of the second metal pattern 21 from being significantly shifted due to alignment errors, which could lead to the first metal pattern 11 being exposed. This embodiment ensures that the first metal pattern 11 is completely covered by the second metal pattern 21.
[0098] In a specific implementation, the second metal pattern 21 formed by the magnetron sputtering film forming process is prone to having a fine crack structure at the intersection of the first side surface S3 and the second surface S2 (as shown in the circle in Figure 11). Therefore, in some embodiments, the second metal pattern 21 can have a fine crack, and the fine crack is close to the intersection of the first side surface S3 and the second surface S2.
[0099] The inventors conducted a composition analysis on the first metal pattern 11 at the fine gap structure and found no obvious oxidation. The impact on product reliability can be ignored.
[0100] In order to prevent the material of the first metal pattern 11 from being oxidized, in some embodiments, as shown in any one of Figures 3 to 8, the light-emitting substrate further includes: a passivation layer 31, which is arranged on the side of the first metal pattern 11 away from the base substrate 10, and a first opening V1 is provided on the passivation layer 31, and the first opening V1 is used to expose the middle area of the first surface S1, and the passivation layer 31 at least covers the edge area and the first side surface S3 of the first surface S1; and a second metal pattern 21, which is arranged on the side of the passivation layer 31 away from the base substrate 10, and the second metal pattern 21 completely covers the middle area of the first surface S1, and the orthographic projection of the second metal pattern 21 on the base substrate 10 at least partially covers the orthographic projection of the passivation layer 31 on the base substrate 10.
[0101] As shown in any one of Figures 3 to 8, the first surface S1 can be divided into a middle area and an edge area located outside the middle area. The passivation layer 31 fully wraps the edge area of the first surface S1 and the first side surface S3. For example, a passivation material layer can first be formed on the entire surface of the side of the first metal pattern 11 facing away from the base substrate 10, that is, the orthographic projection of the passivation material layer on the base substrate 10 covers the entire base substrate 10; then, a hole is opened in the passivation material layer, that is, the passivation material layer covering the middle area of the first surface S1 is removed to form a first opening V1, thereby obtaining the passivation layer 31.
[0102] By forming the first opening V1 on the passivation layer 31 , it is convenient to solder the light emitting element on the first metal pattern 11 , or to connect the subsequent conductive layer to the first metal pattern 11 through vias.
[0103] In a specific implementation, the light-emitting substrate may include a plurality of first metal patterns 11 , wherein a portion of the first metal patterns 11 may be used for soldering light-emitting diodes, and a portion of the first metal patterns 11 may be connected to the conductive layer through vias.
[0104] To ensure that the passivation layer 31 fully covers the first side surface S3, in some embodiments, as shown in any one of Figures 3 to 8, the thickness H3 of the passivation layer 31 on the first side surface S3 is greater than or equal to 1000 angstroms. This can provide better anti-oxidation protection for the first side surface S3.
[0105] In a specific implementation, as shown in any one of Figures 3 to 8, due to factors such as the film formation process, the thickness of the first metal pattern 11, and the angle of the first side surface S3, the thickness H3 of the passivation layer 31 located on the first side surface S3 is less than the thickness H4 of the passivation layer 31 located on the first surface S1. For example, the thickness H3 of the passivation layer 31 located on the first side surface S3 is generally 1 / 2 of the thickness H4 of the passivation layer 31 located on the first surface S1. To ensure that the thickness H3 of the passivation layer 31 on the first side surface S3 is greater than or equal to 1000 angstroms, the thickness H4 of the passivation layer 31 located on the first surface S1 can be greater than or equal to 2000 angstroms.
[0106] For example, the passivation layer 31 may be formed by chemical vapor deposition and then patterned by photolithography.
[0107] In specific implementations, the second metal pattern 21 can have various embodiments. For example, in a first embodiment, as shown in FIG3 , FIG5 , or FIG7 , the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is located between the orthographic projection boundary of the first opening V1 on the base substrate 10 and the orthographic projection boundary of the first metal pattern 11 on the base substrate 10.
[0108] For example, as shown in FIG3, FIG5 or FIG7, the edge area of the first surface S1 covered by the passivation layer 31 can be further divided into a first edge area and a second edge area, where the first edge area is close to the middle area. The orthographic projection of the second metal pattern 21 on the base substrate 10 completely covers the middle area and the orthographic projection of the first edge area on the base substrate 10, and does not overlap with the orthographic projection of the second edge area on the base substrate 10.
[0109] As shown in Figure 3, Figure 5 or Figure 7, the orthographic projection of the second metal pattern 21 on the base substrate 10 completely covers the orthographic projection of the first opening V1 on the base substrate 10, and the orthographic projection area of the second metal pattern 21 on the base substrate 10 is larger than the orthographic projection area of the first opening V1 on the base substrate 10.
[0110] In order to ensure that the second metal pattern 21 fully covers the middle area, illustratively, as shown in Figure 3, Figure 5 or Figure 7, the orthographic projection boundary of the first opening V1 on the base substrate 10 is located within the orthographic projection boundary of the second metal pattern 21 on the base substrate 10, and the distance between the orthographic projection boundary of the first opening V1 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 (L2 as shown in the figure) is greater than or equal to 1 micron and less than or equal to 3 microns.
[0111] For ease of description, as shown in Figures 3, 5, or 7, the distance between the orthographic projection boundary of the first opening V1 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is defined as the second package length L2. The design value of the second package length can be set to 2 microns. Due to the presence of alignment errors between different layers during the manufacturing process, the final second package length L2 is generally greater than or equal to 1 micron and less than or equal to 3 microns.
[0112] In this way, the position of the second metal pattern 21 can be prevented from being shifted due to alignment deviation, thereby preventing the first metal pattern 11 from being exposed. This embodiment can ensure that the middle area not covered by the passivation layer 31 is completely covered by the second metal pattern 21.
[0113] By setting a passivation layer 31 between the first metal pattern 11 and the second metal pattern 21, the passivation layer 31 can fill and accumulate the inward-contracted depression of the first side surface S3 and the groove 12 on the first side surface S3, thereby facilitating the second metal pattern 21 to fully cover the first side surface S3, improving the fine crack problem at the intersection of the first side surface S3 and the second surface S2, and enhancing the anti-oxidation protection of the first metal pattern 11.
[0114] In a second embodiment, as shown in FIG. 4 , FIG. 6 or FIG. 8 , the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is located on a side of the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 away from the orthographic projection of the first opening V1 on the base substrate 10 .
[0115] As shown in Figure 4, Figure 6 or Figure 8, the orthographic projection of the second metal pattern 21 on the base substrate 10 completely covers the orthographic projection of the first metal pattern 11 on the base substrate 10, and the orthographic projection area of the second metal pattern 21 on the base substrate 10 is larger than the orthographic projection area of the first metal pattern 11 on the base substrate 10.
[0116] Exemplarily, as shown in Figure 4, Figure 6 or Figure 8, the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 is located within the orthographic projection boundary of the second metal pattern 21 on the base substrate 10, and the distance between the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 (L1 as shown in the figure) is greater than or equal to 0.5 microns and less than or equal to 1.5 microns.
[0117] As shown in Figures 4, 6, or 8, the distance between the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is defined as a first package length L1. The design value of the first package length L1 can be set to 1 micron. Due to the presence of alignment errors between different layers during the manufacturing process, the final first package length L1 is generally greater than or equal to 0.5 microns and less than or equal to 1.5 microns.
[0118] In the first embodiment, as shown in Figure 3, Figure 5 or Figure 7, since the orthographic projection of the second metal pattern 21 on the base substrate 10 does not completely cover the orthographic projection of the first surface S1 on the base substrate 10, the area of the second metal pattern 21 is relatively small, and therefore the stress of the light-emitting substrate is small, which can improve the warping problem of the light-emitting substrate that may be caused by excessive stress.
[0119] In the second embodiment, as shown in Figure 4, Figure 6 or Figure 8, since the orthographic projection of the second metal pattern 21 on the base substrate 10 completely covers the orthographic projection of the first surface S1 on the base substrate 10, double protection consisting of the passivation layer 31 and the second metal pattern 21 can be formed, thereby strengthening the anti-oxidation protection of the first metal pattern 11.
[0120] In some embodiments, as shown in any one of Figures 5 to 8, the light-emitting substrate further includes: a flat layer 51, located between the passivation layer 31 and the second metal pattern 21, the orthographic projection of the flat layer 51 on the base substrate 10 completely overlaps with the orthographic projection of the passivation layer 31 on the base substrate 10, and the surface of the flat layer 51 facing away from the base substrate 10 is parallel to the plane of the base substrate 10, thereby improving the flatness of the light-emitting substrate.
[0121] To improve the flatness of the surface of the flat layer 51 facing away from the base substrate 10 , the thickness of the flat layer 51 may be greater than or equal to 90% and less than or equal to 110% of the thickness of the first metal pattern 11 .
[0122] In some embodiments, as shown in any of Figures 5 to 8 , the planarization layer 51 includes a first planarization pattern 511. The first planarization pattern 511 overlaps with the first metal pattern 11 in the normal direction of the base substrate 10. The thickness of the first planarization pattern 511 is greater than 0 and less than or equal to 1 micron. This improves the surface planarity of the light-emitting substrate while preventing the formation of deep holes at the first opening V1.
[0123] For example, the planar layer 51 may include one or more resin materials such as acrylic resin and polyimide resin, which is not limited in the present disclosure.
[0124] In some embodiments, as shown in Figure 7 or Figure 8, the light-emitting substrate further includes: an isolation layer 71, which is arranged between the flat layer 51 and the second metal pattern 21, and a second opening V2 is provided on the isolation layer 71. The orthographic projection of the second opening V2 on the base substrate 10 at least partially overlaps with the orthographic projection of the first opening V1 on the base substrate 10, and the isolation layer 71 covers the surface of the flat layer 51 facing the second metal pattern 21 and the side of the flat layer 51 facing the first opening V1.
[0125] As shown in FIG. 7 or FIG. 8 , the orthographic projection of the first opening V1 on the base substrate 10 covers the orthographic projection of the second opening V2 on the base substrate 10 , and the orthographic projection area of the first opening V1 on the base substrate 10 is larger than the orthographic projection area of the second opening V2 on the base substrate 10 .
[0126] By providing an isolation layer 71 to cover the surface of the flat layer 51 , the adhesion of the second metal pattern 21 can be improved, and the flat layer 51 can be isolated from the outside world to prevent the intrusion of external water and oxygen, and to prevent the material of the flat layer 51 from absorbing water or oxidizing.
[0127] In some embodiments, the material of the second metal pattern 21 may include at least one of the following: a nickel alloy such as a nickel-vanadium alloy, a nickel-tungsten alloy, and a copper-nickel alloy.
[0128] For example, a magnetron sputtering process may be used to form a film, and then a photolithography process may be used to pattern the second metal pattern 21 .
[0129] In order to achieve a better anti-oxidation effect, the weight percentage of nickel in the material of the second metal pattern 21 is greater than or equal to 50%.
[0130] FIG9 shows optical reflectivity-wavelength curves of a nickel-vanadium alloy under various annealing conditions. The change in optical reflectivity before and after annealing can reflect the nickel-vanadium alloy's antioxidant properties. As shown in FIG9 , the reflectivity-wavelength curve after annealing at 150°C for 30 minutes is substantially identical to the unannealed reflectivity-wavelength curve. Furthermore, the reflectivity of the light-emitting substrate after annealing at 250°C for 30 minutes is not significantly different from that of the unannealed substrate. This demonstrates that the nickel-vanadium alloy exhibits excellent antioxidant properties and can provide antioxidant protection for the first metal pattern 11.
[0131] Verification has found that the oxidation resistance of nickel-tungsten alloy is similar to that of nickel-vanadium alloy, while copper-nickel alloy has slightly lower oxidation resistance. Therefore, the oxidation resistance of the second metal pattern 21 formed of nickel-vanadium alloy or nickel-tungsten alloy is better than that of the second metal pattern 21 formed of copper-nickel alloy.
[0132] In addition, nickel alloy has good solder paste wettability. Referring to Figure 10, it shows that under the condition that the steel mesh window size is 1000μm, the spreading diameter of the solder paste after reflow is greater than 1000μm. As shown in Figure a of Figure 10, the spreading size of the solder paste is 1156μm. It can be seen that nickel alloy has good solder paste wettability, which is beneficial to the welding of light-emitting components.
[0133] In some embodiments, the passivation layer 31 may include one or more materials selected from the group consisting of silicon nitride, silicon oxide, and silicon oxynitride.
[0134] In some embodiments, the isolation layer 71 may include one or more materials selected from the group consisting of silicon nitride, silicon oxide, and silicon oxynitride.
[0135] The present disclosure also provides a light-emitting device, comprising: a light-emitting substrate as provided in any embodiment; and a light-emitting diode, which is arranged on the side of the first metal pattern 11 away from the base substrate 10 and is connected to the first metal pattern 11, and the first metal pattern 11 is used to provide a driving signal to the light-emitting diode to drive the light-emitting diode to emit light.
[0136] Those skilled in the art will appreciate that the light-emitting device has the advantage of a front-light-emitting substrate.
[0137] The light-emitting diodes may be micro light-emitting diodes (Micro LEDs) and / or sub-millimeter light-emitting diodes (Mini LEDs), and the present disclosure does not limit this. Micro LEDs have a size of approximately 100 μm to 300 μm. Mini LEDs have a size of approximately 100 μm or less.
[0138] In some embodiments, the light emitting device is a lighting device that can be used as a light source to achieve lighting functions. For example, the light emitting device can be a backlight module in a liquid crystal light emitting device, a lamp for internal or external lighting, or various signal lights.
[0139] In other embodiments, the light-emitting device is a display device for realizing the function of displaying an image (i.e., a picture). The light-emitting device may include a display or a product including a display. Among them, the display may be a flat panel display (Flat Panel Display, FPD), a micro display, etc. If divided according to whether the user can see the back of the display, the display may be a transparent display or an opaque display. If divided according to whether the display can be bent or curled, the display may be a flexible display or an ordinary display (which may be called a rigid display). Exemplarily, products including displays may include: computer monitors, televisions, billboards, laser printers with display functions, telephones, mobile phones, electronic paper, personal digital assistants (Personal Digital Assistant, PDA), laptop computers, digital cameras, tablet computers, notebook computers, navigation systems, camcorders, viewfinders, vehicles, large-area walls, theater screens or stadium signs, etc.
[0140] The present disclosure also provides a method for preparing a light-emitting substrate, comprising:
[0141] Step S01: providing a base substrate 10 .
[0142] Step S02: Forming a first metal pattern 11 on one side of the base substrate 10. The first metal pattern 11 includes a first surface S1 away from the base substrate 10, a second surface S2 closer to the base substrate 10, and a first side surface S3 connecting the first surface S1 and the second surface S2. The first surface S1 includes a central region and an edge region located outside the central region. The first surface S1 is raised toward the side away from the base substrate 10, and the height of the raised central region is greater than that of the raised edge region.
[0143] The light-emitting substrate provided in any embodiment can be prepared by using the preparation method provided in the present disclosure.
[0144] In specific implementation, various implementations may be used to form the first metal pattern 11 on one side of the base substrate 10 , which are exemplarily described below.
[0145] In some embodiments, the first metal pattern 11 can be formed by a series of patterning processes including film formation, exposure, development, and etching. For example, a grayscale mask can be used in the exposure process, and finally the first metal pattern 11 with a mushroom-shaped top surface can be etched, as shown in FIG1 .
[0146] However, the thickness of the first metal pattern 11 formed by one patterning process in this embodiment is relatively small, generally less than or equal to 2 microns. Therefore, a first metal pattern 11 with a larger thickness requires multiple processes to complete, which is a more complicated process and has the risk of excessive stress.
[0147] In other embodiments, the first metal pattern 11 can also be formed using an additive electroplating process. Because the exchange rate of metal ions in the central region is faster, the growth rate in the central region is relatively fast, resulting in a naturally formed mushroom-shaped top surface. Furthermore, by controlling parameters such as the electroplating time, a thicker first metal pattern 11 can be formed, simplifying the process and reducing the risk of excessive stress.
[0148] The following describes step S02 by taking copper as the main material of the first metal pattern 11. In step S02, the step of forming the first metal pattern 11 on one side of the base substrate 10 may specifically include:
[0149] Step S11 : forming a seed layer on one side of the base substrate 10 .
[0150] For example, a magnetron sputtering process can be used to sequentially form a buffer layer and a seed metal layer on one side of the base substrate 10. The material of the buffer layer can include, for example, molybdenum, titanium, nickel alloy, molybdenum-neodymium alloy, or molybdenum, etc., which can improve the adhesion of the film layer. The thickness of the buffer layer can be, for example, greater than or equal to 300 angstroms and less than or equal to 500 angstroms. Since the main material of the first metal pattern 11 is copper, copper can be selected as the material of the seed metal layer, and the thickness of the seed metal layer can be, for example, greater than or equal to 3000 angstroms and less than or equal to 6000 angstroms.
[0151] Step S12: patterning a pattern defining layer 130 on the side of the seed layer facing away from the base substrate 10 , as shown in FIG13 . The pattern defining layer 130 is made of a removable insulating material and has a plurality of openings 131 to expose the seed layer at corresponding positions.
[0152] The material of the pattern defining layer 130 may be an organic insulating material, such as a photosensitive resin, a photoresist, etc.; or an inorganic material, such as silicon oxide, etc.
[0153] In a specific implementation, the thickness of the pattern defining layer 130 can be determined based on the thickness of the first metal pattern 11. To prevent the material of the first metal pattern 11 from growing beyond the opening of the pattern defining layer 130, the thickness of the pattern defining layer 130 can be controlled to be greater than the thickness of the first metal pattern 11. For example, the thickness of the pattern defining layer 130 can be greater than or equal to 120% of the thickness of the first metal pattern 11 and less than or equal to 130% of the thickness of the first metal pattern 11. This can improve the electroplating uniformity of the first metal pattern 11.
[0154] In some embodiments, the angle γ between the side surface of the pattern defining layer 130 facing the opening 131 and the bottom surface of the pattern defining layer 130 near the base substrate 10 is greater than or equal to 60° and less than or equal to 120°. The angle γ can be, for example, 70°, 80°, 90°, 100°, or 110°. In FIG13 , the angle γ is 80.45°.
[0155] By controlling the angle γ to be greater than or equal to 60°, the angle β between the first side surface S3 and the second surface S2 of the finally formed first metal pattern 11 can be less than or equal to 120°, which is beneficial to improving the coverage of subsequent film layers of the first metal pattern 11.
[0156] Exemplarily, the material of the pattern defining layer 130 includes a resin substrate, a photosensitive agent filled in the resin substrate, and a solvent. The pattern defining layer 130 can be formed using a series of patterning processes, including film formation, exposure, and development. To control the aforementioned angle γ to be greater than or equal to 60°, in some embodiments, the pattern defining layer 130 includes a resin material having a relative molecular weight greater than or equal to 30,000 and less than or equal to 50,000. This can improve the difference in developability between the exposed and unexposed areas during the exposure process for forming the pattern defining layer 130, thereby facilitating an increase in the angle γ.
[0157] To control the angle γ to be greater than or equal to 60°, in some other embodiments, the pattern defining layer 130 includes a photosensitive agent with a mass fraction of greater than or equal to 20%. This can improve the difference in developability between the exposed and unexposed areas during the exposure process of forming the pattern defining layer 130, thereby increasing the angle γ.
[0158] Step S13 : forming a first metal material layer in the opening 131 of the pattern defining layer 130 .
[0159] For example, the first metal material layer may be formed by electroplating, the electroplating current density may be 2ASD to 4ASD, and the thickness of the first metal material layer may be 5 micrometers to 10 micrometers, where ASD represents amperes per square foot.
[0160] Illustratively, the first metal material layer may be formed by chemical plating or electrochemical process, which is not limited in the present disclosure.
[0161] Step S14: Removing the pattern defining layer 130. In this step, the pattern defining layer 130 may be peeled off.
[0162] Step S15: Use an etching process to remove the portion of the seed layer not covered by the first metal material layer to form a first metal pattern 11. The first metal pattern 11 includes the seed layer 111 and the first metal material layer 112 remaining after the etching process is completed, as shown in any one of Figures 2 to 8.
[0163] In the etching process of step S15 , the first metal material layer does not need to be protected, so the surface of the first metal material layer is partially etched. The seed layer 111 and the first metal material layer 112 obtained after the etching are completed constitute the first metal pattern 11 .
[0164] In order to prevent the first metal pattern 11 from being oxidized, in the first embodiment, as shown in FIG. 2 , after step S02 , the above-mentioned preparation method may further include:
[0165] Step S21 : forming a second metal pattern 21 on a side of the first metal pattern 11 facing away from the base substrate 10 , wherein the second metal pattern 21 completely covers the first surface S1 and the first side surface S3 .
[0166] Figure 11 shows a cross-sectional view of the light-emitting substrate after completing step S21. Figures a and b shown in Figure 11 correspond to the actual images of the light-emitting substrate at the left and right positions shown in Figure 2, respectively. Figure c is an enlarged view of the dotted box in Figure a, and Figure d is an enlarged view of the dotted box in Figure b.
[0167] As shown in Figure 11, the top surface S1 of the first metal pattern 11 forms a mushroom-shaped bulge, and the first side surface S3 is formed with a groove 12 at the bottom corner position near the base substrate 10 (as shown in the dotted box position in Figure 11). This is because in the etching process of step S15, the bottom corner position will be etched inward, causing the bottom corner to shrink inward.
[0168] For example, the deposition thickness of the second metal pattern 21 on the first surface S1 may be greater than or equal to 2000 angstroms and less than or equal to 6000 angstroms.
[0169] For example, a magnetron sputtering process can be used to deposit a layer of nickel alloy on the surface of the first metal pattern 11 facing away from the base substrate 10, and then a series of composition processes such as exposure, development and etching processes can be used to form the second metal pattern 21. The second metal pattern 21 fully wraps the exposed first surface S1 and first side surface S3 of the first metal pattern 11, thereby fully protecting the material of the first metal material and preventing oxidation.
[0170] In this embodiment, as shown in FIG2 , the design value of the first package length L1 can be set to 1 micron. Due to the presence of alignment errors between different layers in the preparation process, the final first package length L1 is generally greater than or equal to 0.5 microns and less than or equal to 1.5 microns.
[0171] In a second embodiment, after step S02, as shown in any one of FIG. 3 to FIG. 8 , the preparation method may further include:
[0172] Step S31: A passivation layer 31 is formed on the side of the first metal pattern 11 facing away from the base substrate 10. A first opening V1 is provided on the passivation layer 31. The first opening V1 is used to expose the middle area of the first surface S1. The passivation layer 31 at least covers the edge area of the first surface S1 and the first side surface S3.
[0173] For example, a chemical vapor deposition process can be first used to form a passivation material layer on the entire surface of the side of the first metal pattern 11 facing away from the base substrate 10, that is, the orthographic projection of the passivation material layer on the base substrate 10 covers the entire base substrate 10; and then an exposure, development and etching process is used to open a hole in the passivation material layer, that is, the passivation material layer covering the middle area of the first surface S1 is removed to form a first opening V1, thereby obtaining a passivation layer 31.
[0174] Step S32: forming a second metal pattern 21 on the side of the passivation layer 31 facing away from the base substrate 10, wherein the second metal pattern 21 completely covers the middle area of the first surface S1, and the orthographic projection of the second metal pattern 21 on the base substrate 10 at least partially covers the orthographic projection of the passivation layer 31 on the base substrate 10.
[0175] For example, the deposition thickness of the second metal pattern 21 on the first surface S1 may be greater than or equal to 2000 angstroms and less than or equal to 6000 angstroms.
[0176] For example, a layer of nickel alloy may be deposited on the surface of the passivation layer 31 facing away from the base substrate 10 by magnetron sputtering, and then a series of patterning processes such as exposure, development, and etching may be used to form the second metal pattern 21 .
[0177] As shown in FIG. 3 , the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is located between the orthographic projection boundary of the first opening V1 on the base substrate 10 and the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 .
[0178] For ease of description, the distance between the orthographic projection boundary of the first opening V1 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is defined as the second wrap length. As shown in Figure 3, the design value of the second wrap length can be set to 2 microns. Due to the presence of alignment errors between different layers during the manufacturing process, the final first wrap length L1 is generally greater than or equal to 1 micron and less than or equal to 3 microns.
[0179] As shown in FIG. 4 , the orthographic projection boundary of the second metal pattern 21 on the base substrate 10 is located on a side of the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 away from the orthographic projection of the first opening V1 on the base substrate 10 .
[0180] As previously mentioned, first package length L1 is the distance between the orthographic projection boundary of the first metal pattern 11 on the base substrate 10 and the orthographic projection boundary of the second metal pattern 21 on the base substrate 10. As shown in FIG4 , the design value of first package length L1 can be set to 1 micron. Due to the presence of alignment errors between different layers during the fabrication process, the final first package length L1 is generally greater than or equal to 0.5 micron and less than or equal to 1.5 microns.
[0181] Figure 12 shows a cross-sectional view of the light-emitting substrate after completing step S32. Figures a and b shown in Figure 12 correspond to the actual images of the light-emitting substrate at the left and right positions shown in Figure 4, respectively. Figure c is an enlarged view of the dotted box in Figure a, and Figure d is an enlarged view of the dotted box in Figure b.
[0182] As shown in Figure 12, the top surface S1 of the first metal pattern 11 forms a mushroom-shaped bulge, and the first side surface S3 is formed with a groove 12 at the bottom corner position near the base substrate 10 (as shown in the dotted box position in Figure 12). This is because in the etching process of step S15, the bottom corner position will be etched inward, causing the bottom corner to shrink inward.
[0183] In some implementations, after step S31 and before step S32, the following steps may also be included:
[0184] Step S41: A flat layer 51 is formed on the side of the passivation layer 31 facing away from the base substrate 10, and the orthographic projection of the flat layer 51 on the base substrate 10 completely overlaps with the orthographic projection of the passivation layer 31 on the base substrate 10. The surface of the flat layer 51 facing away from the base substrate 10 is a plane parallel to the base substrate 10, thereby improving the flatness of the light-emitting substrate.
[0185] Accordingly, in step S32, the step of forming the second metal pattern 21 on the side of the passivation layer 31 facing away from the base substrate 10 includes:
[0186] Step S42 : forming a second metal pattern 21 on a side of the planar layer 51 facing away from the base substrate 10 .
[0187] For example, a passivation material layer and a flat material layer can be first formed on the entire surface of the side of the first metal pattern 11 facing away from the base substrate 10, that is, the orthographic projections of the passivation material layer and the flat material layer on the base substrate 10 cover the entire base substrate 10; and then the first opening V1 and the flat layer 51 on the passivation layer 31 are synchronously formed by exposure and development processes.
[0188] In some implementations, after step S41 and before step S42, the following steps may also be included:
[0189] Step S51: An isolation layer 71 is formed on the side of the flat layer 51 facing away from the base substrate 10, and a second opening V2 is provided on the isolation layer 71. The orthographic projection of the second opening V2 on the base substrate 10 at least partially overlaps with the orthographic projection of the first opening V1 on the base substrate 10. The isolation layer 71 covers the surface of the flat layer 51 facing the second metal pattern 21 and the side of the flat layer 51 facing the first opening V1.
[0190] As shown in FIG7 or FIG8, by providing an isolation layer 71 between the above-mentioned planar layer 51 and the second metal pattern 21, the adhesion of the second metal pattern 21 can be improved, and the intrusion of external water and oxygen can be prevented, and the material of the planar layer 51 can be prevented from absorbing water or oxidizing.
[0191] It should be noted that the flooding preparation method may also include more steps, which can be determined according to actual needs and is not limited by the present disclosure. The detailed description of the preparation method and the technical effects can be referred to the description of the light-emitting substrate above, which will not be repeated here.
[0192] In the present disclosure, “a plurality of” means two or more, and “at least one” means one or more, unless otherwise clearly defined.
[0193] In the present disclosure, the orientation or positional relationship indicated by the terms "upper" and "lower" is based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing the present disclosure and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation. Therefore, it should not be understood as a limitation on the present disclosure.
[0194] As used herein, the terms "comprises," "includes," or any other variations thereof are intended to encompass non-exclusive inclusion, such that a process, method, commodity, or apparatus that includes a list of elements includes not only those elements but also other elements not explicitly listed, or elements inherent to such process, method, product, or apparatus. In the absence of further limitations, an element defined by the phrase "comprising a ..." does not preclude the presence of additional identical elements in the process, method, commodity, or apparatus that includes the element.
[0195] References herein to "one embodiment," "some embodiments," "exemplary embodiments," "one or more embodiments," "an example," "an example," "some examples," and the like are intended to indicate that a particular feature, structure, material, or characteristic associated with that embodiment or example is included in at least one embodiment or example of the present disclosure. Schematic representations of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the particular features, structures, materials, or characteristics described may be included in any one or more embodiments or examples in any suitable manner.
[0196] In this document, relational terms such as first and second, etc. are used merely to distinguish one entity or operation from another entity or operation, but do not necessarily require or imply any actual relationship or order between these entities or operations.
[0197] When describing some embodiments, the expressions "coupled" and "connected" may be used. For example, when describing some embodiments, the term "connected" may be used to indicate that two or more components are in direct physical or electrical contact with each other. For another example, when describing some embodiments, the term "coupled" may be used to indicate that two or more components are in direct physical or electrical contact. However, the term "coupled" or "communicatively coupled" may also mean that two or more components are not in direct contact with each other, but still cooperate or interact with each other. The embodiments disclosed herein are not necessarily limited to the contents of this document.
[0198] “At least one of A, B and C” has the same meaning as “at least one of A, B or C” and both include the following combinations of A, B and C: A only, B only, C only, the combination of A and B, the combination of A and C, the combination of B and C, and the combination of A, B and C.
[0199] “A and / or B” includes the following three combinations: A only, B only, and a combination of A and B.
[0200] As used herein, the term "if" is optionally interpreted to mean "when" or "upon" or "in response to determining" or "in response to detecting," depending on the context. Similarly, the phrases "if it is determined that" or "if [stated condition or event] is detected" are optionally interpreted to mean "upon determining" or "in response to determining" or "upon detecting [stated condition or event]" or "in response to detecting [stated condition or event]," depending on the context.
[0201] The use of "for" or "configured to" herein is intended to be open and inclusive language that does not exclude devices adapted or configured to perform additional tasks or steps.
[0202] The use of "based on" or "according to" in this document is intended to be open and inclusive. A process, step, calculation, or other action based on one or more stated conditions or values may, in practice, be based on other conditions or values beyond the stated values. A process, step, calculation, or other action based on one or more stated conditions or values may, in practice, be based on other conditions or values beyond the stated values.
[0203] As used herein, "about," "substantially," or "approximately" includes the stated value and an average value that is within an acceptable range of deviation from the particular value as determined by one of ordinary skill in the art taking into account the measurements in question and the errors associated with the measurement of the particular quantity (i.e., the limitations of the measurement system).
[0204] As used herein, "parallel", "perpendicular", "equal", and "flush" include the situations described and situations similar to the situations described, the range of which is within an acceptable deviation range, wherein the acceptable deviation range is as determined by a person of ordinary skill in the art taking into account the measurement in question and the errors associated with the measurement of the specific quantity (i.e., the limitations of the measurement system). For example, "parallel" includes absolute parallelism and approximate parallelism, wherein the acceptable deviation range of approximate parallelism can be, for example, a deviation within 5°; "perpendicular" includes absolute perpendicularity and approximate perpendicularity, wherein the acceptable deviation range of approximate perpendicularity can also be, for example, a deviation within 5°. "Equal" includes absolute equality and approximate equality, wherein the acceptable deviation range of approximate equality can be, for example, the difference between the two being equal is less than or equal to 5% of either one. "Flush" includes absolute equality and approximate flushness, wherein the acceptable deviation range of approximate flushness can be, for example, the distance between the two being flush is less than or equal to 5% of either one's size.
[0205] It will be understood that when a layer or element is referred to as being on another layer or substrate, it can be directly on the other layer or substrate, or intervening layers may be present therebetween.
[0206] Exemplary embodiments are described herein with reference to cross-sectional and / or plan views that are idealized exemplary drawings. In the drawings, the thicknesses of layers and regions are exaggerated for clarity. Therefore, variations in shape relative to the drawings due to, for example, manufacturing techniques and / or tolerances are contemplated. Therefore, the exemplary embodiments should not be construed as limited to the shapes of the regions shown herein, but rather include deviations in shape due to, for example, manufacturing. For example, an etched region shown as a rectangle will typically have curved features. Therefore, the regions shown in the drawings are schematic in nature, and their shapes are not intended to illustrate the actual shape of regions of the device and are not intended to limit the scope of the exemplary embodiments.
[0207] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present disclosure, rather than to limit them. Although the present disclosure has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the present disclosure.
Claims
1. A light-emitting substrate, comprising: substrate substrate; as well as A first metal pattern is arranged on one side of the base substrate, comprising: a first surface away from the base substrate, a second surface close to the base substrate, and a first side surface connecting the first surface and the second surface, wherein the first surface comprises a middle area and an edge area located outside the middle area; The first surface is convex toward a side away from the substrate, and the convex height of the middle area is greater than the convex height of the edge area.
2. The light-emitting substrate according to claim 1, wherein: The first surface also includes: The sub-middle region is located between the middle region and the edge region, and the protrusion height of the sub-middle region is smaller than the protrusion height of the middle region and larger than the protrusion height of the edge region.
3. The light-emitting substrate according to claim 1 or 2, wherein: The protrusion height of the first surface gradually decreases from the center of the first surface to the edge of the first surface; and The ratio of the difference between the protrusion heights of the middle area and the edge area to the protrusion height of the edge area is greater than or equal to 0.1 and less than or equal to 0.
4.
4. The light-emitting substrate according to any one of claims 1 to 3, wherein: The orthographic projection of the first surface on the base substrate covers the orthographic projection of the second surface on the base substrate, and the orthographic projection area of the first surface on the base substrate is larger than the orthographic projection area of the second surface on the base substrate.
5. The light-emitting substrate according to any one of claims 1 to 4, wherein: An included angle between the first side surface and the second surface is greater than or equal to 80° and less than or equal to 120°.
6. The light-emitting substrate according to any one of claims 1 to 5, wherein: The first metal pattern further includes: The first cross section is parallel to the substrate and intersects with the edge of the first surface, and the angle between the first cross section and the first side surface is an acute angle.
7. The light-emitting substrate according to any one of claims 1 to 6, wherein: The first side surface has a groove recessed toward the inside of the first metal pattern, and the groove is located on the first side surface close to the base substrate.
8. The light-emitting substrate according to any one of claims 1 to 7, wherein: The light-emitting substrate further comprises: The second metal pattern is arranged on a side of the first metal pattern away from the base substrate, and the second metal pattern completely covers the first surface and the first side surface.
9. The light emitting substrate according to claim 8, wherein: The second metal pattern has a thin gap, and the thin gap is close to a position where the first side surface intersects with the second surface.
10. The light-emitting substrate according to any one of claims 1 to 7, wherein: The light-emitting substrate further comprises: a passivation layer, disposed on a side of the first metal pattern away from the base substrate, the passivation layer being provided with a first opening, the first opening being used to expose a middle area of the first surface, the passivation layer at least covering an edge area of the first surface and the first side surface; and A second metal pattern is arranged on a side of the passivation layer away from the base substrate, the second metal pattern completely covers the middle area of the first surface, and the orthographic projection of the second metal pattern on the base substrate at least partially covers the orthographic projection of the passivation layer on the base substrate.
11. The light emitting substrate according to claim 10, wherein: The orthographic projection boundary of the second metal pattern on the base substrate is located between the orthographic projection boundary of the first opening on the base substrate and the orthographic projection boundary of the first metal pattern on the base substrate.
12. The light emitting substrate according to claim 10, wherein: The orthographic projection boundary of the second metal pattern on the base substrate is located on a side of the orthographic projection boundary of the first metal pattern on the base substrate away from the orthographic projection of the first opening on the base substrate.
13. The light emitting substrate according to any one of claims 10 to 12, wherein: The light-emitting substrate further comprises: The flat layer is located between the passivation layer and the second metal pattern, the orthographic projection of the flat layer on the base substrate completely overlaps with the orthographic projection of the passivation layer on the base substrate, and the surface of the flat layer facing away from the base substrate is parallel to the plane of the base substrate.
14. The light emitting substrate according to claim 13, wherein: The light-emitting substrate further comprises: An isolation layer is arranged between the flat layer and the second metal pattern, and a second opening is arranged on the isolation layer. The orthographic projection of the second opening on the base substrate at least partially overlaps with the orthographic projection of the first opening on the base substrate, and the isolation layer covers the surface of the flat layer facing the second metal pattern and the side of the flat layer facing the first opening.
15. The light-emitting substrate according to claim 13 or 14, wherein: The planar layer includes a first planar pattern, the first planar pattern overlaps with the first metal pattern in a normal direction of the base substrate, and a thickness of the first planar pattern is greater than 0 and less than or equal to 1 micrometer.
16. The light-emitting substrate according to any one of claims 8 to 15, wherein: The thickness of the second metal pattern located on a side of the first metal pattern away from the base substrate is greater than or equal to 2000 angstroms and less than or equal to 6000 angstroms.
17. The light-emitting substrate according to any one of claims 10 to 15, wherein: The thickness of the passivation layer located on the side of the first metal pattern away from the substrate is greater than or equal to 2000 angstroms.
18. The light-emitting substrate according to claim 8 or 12, wherein: The orthographic projection boundary of the first metal pattern on the base substrate is located within the orthographic projection boundary of the second metal pattern on the base substrate, and the distance between the orthographic projection boundary of the first metal pattern on the base substrate and the orthographic projection boundary of the second metal pattern on the base substrate is greater than or equal to 0.5 microns and less than or equal to 1.5 microns.
19. The light-emitting substrate according to claim 11, wherein: The orthographic projection boundary of the first opening on the substrate is located within the orthographic projection boundary of the second metal pattern on the substrate, and the distance between the orthographic projection boundary of the first opening on the substrate and the orthographic projection boundary of the second metal pattern on the substrate is greater than or equal to 1 micron and less than or equal to 3 microns.
20. The light-emitting substrate according to any one of claims 8 to 19, wherein: The material of the second metal pattern includes at least one of the following: nickel-vanadium alloy, nickel-tungsten alloy and copper-nickel alloy.
21. The light-emitting substrate according to any one of claims 1 to 20, wherein: An angle formed by the intersection of the first surface and the first side surface is a rounded angle.
22. The light-emitting substrate according to any one of claims 1 to 21, wherein: The thickness of the first metal pattern is greater than or equal to 4 micrometers and less than or equal to 10 micrometers.
23. A light emitting device, comprising: The light-emitting substrate according to any one of claims 1 to 22; as well as A light emitting diode is arranged on a side of the first metal pattern away from the base substrate and connected to the first metal pattern. The first metal pattern is used to provide a driving signal to the light emitting diode to drive the light emitting diode to emit light.
24. A method for preparing a light-emitting substrate, comprising: providing a substrate base plate; A first metal pattern is formed on one side of the base substrate, the first metal pattern comprising: a first surface away from the base substrate, a second surface close to the base substrate, and a first side surface connecting the first surface and the second surface, the first surface comprising a middle area and an edge area located outside the middle area; wherein the first surface protrudes toward the side away from the base substrate, and the protrusion height of the middle area is greater than the protrusion height of the edge area.
25. The preparation method according to claim 24, wherein: The step of forming a first metal pattern on one side of the base substrate comprises: forming a seed layer on one side of the substrate; Patterning a pattern defining layer on a side of the seed layer away from the substrate, wherein the material of the pattern defining layer is a removable insulating material and the pattern defining layer has a plurality of openings to expose the seed layer at corresponding positions; forming a first metal material layer in the opening of the pattern defining layer; removing the pattern defining layer; An etching process is used to remove the portion of the seed layer not covered by the first metal material layer to form the first metal pattern, wherein the first metal pattern includes the seed layer and the first metal material layer remaining after the etching process is completed.
26. The preparation method according to claim 25, wherein: An angle between a side surface of the pattern defining layer facing the opening and a bottom surface of the pattern defining layer close to the base substrate is greater than or equal to 60° and less than or equal to 100°.
27. The preparation method according to claim 25 or 26, wherein: The pattern defining layer includes at least one of the following: A resin material, wherein the relative molecular weight of the resin material is greater than or equal to 30,000 and less than or equal to 50,000; and The photosensitizer has a mass fraction greater than or equal to 20%.