3D core body of menstrual hygienic product and preparation method of 3D core body
By adopting the flow guide layer structure and folded edge sealing technology in the core of sanitary products during menstruation, the problems of slow absorption speed and surface residue are solved, and faster absorption and better user experience are achieved.
Patent Information
- Application Number
- CN202411088912.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
The core of existing menstrual sanitary products is slow to absorb, and the dust-free paper on the surface after absorption will retain darker menstrual blood color, affecting the user experience.
Adopt the flow-drain layer structure, including the second hot air cloth, the composite flow-drain and dust-free paper. The composite flow-drain contains three flow-drain layers to promote the lateral diffusion of liquid. The second hot air cloth allows liquid to penetrate quickly and cover the surface residue. The first hot air cloth forms a folded edge-enclosed polymer water-absorbing resin layer to improve structural stability.
It significantly improves absorption speed, reduces the residual liquid color on the core surface, improves the user experience, and improves the durability of the core.
Smart Images

Figure CN118986644A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of sanitary products, and in particular to a 3D core of a menstrual hygiene product and a preparation method thereof. Background Art
[0002] The core body is an indispensable component of menstrual hygiene products. It has the functions of absorbing and storing liquid. The core body generally comprises two layers of dust-free paper. A filling layer is arranged between the two layers of dust-free paper. The filling layer can be a highly absorbent resin or wood pulp fiber. The liquid enters the filling layer after passing through the dust-free paper on the surface, thereby achieving the effect of absorbing and storing liquid.
[0003] The problem with this type of core is that the absorption speed is slow, and for menstrual hygiene products, the dust-free paper on the surface after absorption will retain a darker color of menstrual blood, affecting the user experience. Summary of the invention
[0004] In order to improve the absorption speed of the core and improve the user experience, the present application provides a 3D core of a menstrual hygiene product and a preparation method thereof.
[0005] In the first aspect, the 3D core of a menstrual hygiene product provided in the present application adopts the following technical solution: A 3D core of a menstrual hygiene product, comprising a flow guide fabric layer, and: A polymer water-absorbing resin layer is disposed on one side of the guide fabric layer; A first hot air cloth is arranged on a side of the polymer water-absorbing resin layer away from the guide cloth layer; The guide cloth layer includes a second hot air cloth, a composite guide layer and dust-free paper which are arranged in sequence, the dust-free paper is arranged on a side of the polymer water-absorbent resin layer away from the first hot air cloth, both sides of the first hot air cloth are bent to form a folded edge, and the folded edge is arranged on a side of the second hot air cloth away from the composite guide layer; The composite guide layer includes a first guide layer, a second guide layer and a third guide layer. The third guide layer is arranged on a side of the dust-free paper away from the first hot air cloth.
[0006] By adopting the above technical solution, the first thing in the core that contacts the liquid is the guide cloth layer, which includes the second hot air cloth, the composite guide layer and the dust-free paper. Compared with the traditional core that only has dust-free paper, the composite guide layer contains three guide layers, which can promote the lateral diffusion of the liquid, that is, increase the absorption area, and clear the congestion during the liquid penetration process, thereby improving the absorption speed. The second hot air cloth can make the liquid quickly penetrate into the composite guide layer, and play a covering role after the liquid penetrates, reducing the residual liquid color on the surface of the core and improving the user experience.
[0007] The first hot air cloth forms a folded edge and seals the edges of the polymer water-absorbing resin layer and the guide cloth layer, which not only reduces the leakage of the polymer water-absorbing resin, but also improves the stability of the guide cloth layer with a multi-layer structure, forming a 3D core with high durability.
[0008] Optionally, the second hot air cloth is formed by thermal bonding of polyester fiber and ES coarse fiber at a weight ratio of 1:(0.5-0.7); the first guide layer is formed by thermal bonding of polyester fiber and first ES fine fiber at a weight ratio of 1:(1-1.2); The second guide layer is formed by thermal bonding of ES coarse fibers and wood pulp fibers in a weight ratio of 1:(0.2-0.4); The third guide layer is formed by thermal bonding of the first ES fine fibers, wood pulp fibers and bamboo fibers in a weight ratio of 1: (0.3-0.4): (0.2-0.3); The dust-free paper is formed by thermally bonding the second ES fine fibers and the wood pulp fibers in a weight ratio of 1:(0.1-0.2).
[0009] By adopting the above technical solution, the polyester fiber is hydrophobic and absorbs less liquid, so the second hot air cloth can make the liquid penetrate quickly and keep the surface of the 3D core dry. The ES fibers in the second hot air cloth and the first guide layer are different in thickness, and the ES fibers in the first guide layer account for a larger proportion, making the first guide layer denser than the second hot air cloth. When the liquid passes through the second hot air cloth, the denser first guide layer has a first slow infiltration effect on the liquid, so that the liquid has an initial tendency to diffuse laterally after reaching the guide cloth layer, and it helps to prevent the liquid from permeating back to the second hot air cloth, reducing the residual liquid color on the core surface.
[0010] The second guide layer uses ES coarse fiber and wood pulp fiber, and has a relatively loose structure. The wood pulp fiber has a certain water absorption, which makes the second guide layer have a certain water retention capacity, hindering the reverse osmosis of the liquid to reach the first guide layer. When the liquid reaches the second guide layer, the liquid has a preliminary lateral diffusion trend under the action of the first guide layer, so the lateral diffusion trend of the liquid in the second guide layer is amplified, and at the same time, it is ensured that the liquid can quickly pass through the second guide layer to ensure the absorption speed.
[0011] The third guide layer adopts ES fine fiber, wood pulp fiber and bamboo fiber. The relatively dense structure of the third guide layer plays a second slow seepage effect on the liquid. The bamboo fiber has a hollow structure and has good water conductivity. Combined with the lateral diffusion trend accumulated by the first and second guide layers, the liquid can quickly diffuse laterally in the third guide layer, increasing the absorption area, providing more space for the liquid to penetrate downward, and improving the absorption speed of the 3D core.
[0012] Optionally, the first ES fibers are pretreated ES fibers, and the pretreated ES fibers are formed by grafting hydroxy acrylate and N-hydroxymethyl acrylamide onto the surface of the first ES fibers.
[0013] When wearing menstrual hygiene products, they are often squeezed or even rubbed due to movements such as walking, standing up, and exercising. This can easily cause the structure of the guide fabric layer to become loose, which is not conducive to the lateral diffusion of the liquid and reduces the liquid absorption effect.
[0014] By adopting the above technical scheme, hydroxy acrylate and N-hydroxymethyl acrylamide are grafted and polymerized on the surface of the first ES fine fiber. On the one hand, hydrophilic groups are introduced to attract the liquid of the second hot air cloth into the first guide layer. On the other hand, the surface adhesion of the first ES fine fiber is improved. When the surface layer of the first ES fine fiber is partially melted, the degree of contact with the wood pulp fiber and bamboo fiber is increased, and hydrogen bonds are formed with the active groups of the wood pulp fiber and bamboo fiber. The bonding effect between the three guide layers is better, which improves the structural stability of the third guide layer and the ability to support liquid flow, further accelerates the absorption speed, and improves durability.
[0015] Optionally, the raw materials for preparing the pretreated ES fiber include first ES fine fibers, hydroxy acrylate, N-hydroxymethyl acrylamide, an initiator and a solvent, the molar concentration of the hydroxy acrylate in the solvent is 0.15 to 0.3 mol / L, the molar concentration of the N-hydroxymethyl acrylamide in the solvent is 0.25 to 0.35 mol / L, and the molar concentration of the initiator in the solvent is 0.005 to 0.01 mol / L.
[0016] By adopting the above technical solution and controlling the concentration of hydroxy acrylate and N-hydroxymethyl acrylamide, the grafting degree of the pretreated ES fiber can be effectively controlled, thereby controlling the bonding density of the third guide layer, ensuring that the liquid can penetrate smoothly while obtaining a fast lateral diffusion speed.
[0017] Optionally, the bamboo fiber is a pretreated bamboo fiber, and the pretreated bamboo fiber is formed by grafting an epoxy silane coupling agent onto the surface of the bamboo fiber.
[0018] By adopting the above technical solution, the hydrophilicity of bamboo fiber is strong, so that more liquid remains when the liquid passes through the third guide layer, which is not conducive to the rapid penetration of the liquid. Therefore, the epoxy silane coupling agent is grafted on the bamboo fiber to reduce the hydrophilicity of the bamboo fiber and give full play to the water-conducting ability of the bamboo fiber. In this way, the surface affinity of the bamboo fiber and the pre-treated ES fiber can be improved. The active epoxy group after grafting can also further react and bond with the wood pulp fiber and the pre-treated ES fiber under heating conditions, thereby improving the structural stability of the third guide layer and forming a good lateral guide channel.
[0019] Optionally, the raw materials for preparing the pretreated bamboo fiber include bamboo fiber and epoxy silane coupling agent, and the weight ratio of the bamboo fiber to the epoxy silane coupling agent is 1:(0.08-0.15).
[0020] Optionally, the fineness of the ES coarse fiber is 7 to 10D, and the fineness of the first ES fine fiber is 1 to 2D.
[0021] By adopting the above technical solution, the fineness of the ES fiber is controlled, thereby cooperating with polyester fiber, wood pulp fiber or bamboo fiber to control the penetration speed of each guide layer.
[0022] Optionally, the thickness ratio of the second hot air cloth, the composite guide layer and the dust-free paper is (0.16-0.2):1:(0.16-0.2), and the thickness ratio of the first guide layer, the second guide layer and the third guide layer is 1:(2.5-3):(1.5-2).
[0023] Optionally, the thickness ratio of the guide cloth layer, the polymer water-absorbing resin layer and the first hot air cloth is 1:(1.5-2):(0.125-0.142).
[0024] By adopting the above technical solution, the thickness of each layer structure is controlled to obtain a fast absorption speed.
[0025] In the second aspect, the present application provides a method for preparing a 3D core of a menstrual hygiene product using the following technical solution: A method for preparing a 3D core of a menstrual hygiene product comprises the following steps: The second hot air cloth, the composite guide layer and the dust-free paper are bonded by hot pressing to obtain a guide cloth layer; Spray glue on one side of the first hot air cloth, add and bond high molecular water-absorbent resin particles to form a high molecular water-absorbent resin layer; spray glue on one side of the dust-free paper to bond the guide cloth layer to the high molecular water-absorbent resin layer; The two sides of the first hot air cloth are bent to form folded edges, and the folded edges are pressed to make them adhere to the second hot air cloth to obtain a 3D core.
[0026] By adopting the above technical solution, the folded edge is used to enclose the guide fabric layer and the polymer water-absorbing resin layer, thereby improving the structural stability of the 3D core.
[0027] Optionally, the method for preparing the composite guide layer comprises the following steps: The polyester fiber and the first ES fine fiber are mixed, scattered, and air-combed to form a first fiber web, and the first fiber web is thermally bonded to form a first guide layer; The ES coarse fibers and wood pulp fibers are mixed, broken up, and air-combed to form a second fiber web, and the second fiber web is thermally bonded to form a second guide layer; The first ES fine fibers, wood pulp fibers and bamboo fibers are mixed, broken up, and air-combed to form a third fiber web, and the third fiber web is thermally bonded to form a third guide layer; The first guide layer, the second guide layer and the third guide layer are thermally bonded, compacted and cooled to obtain a composite guide layer.
[0028] By adopting the above technical solution, airflow carding can improve the uniformity of different fibers in each guide layer, thereby improving the yield rate.
[0029] In summary, this application has the following beneficial effects: 1. The 3D core of the present application is provided with a guide cloth layer, which includes a second hot air cloth, a composite guide layer and dust-free paper. Compared with the traditional core only provided with dust-free paper, the composite guide layer contains three guide layers, which can promote the lateral diffusion of liquid, that is, increase the absorption area, and clear the congestion during the liquid penetration process, thereby improving the absorption speed. The second hot air cloth can make the liquid quickly penetrate into the composite guide layer, and play a covering role after the liquid penetrates, reducing the residual liquid color on the surface of the core, and improving the use experience.
[0030] 2. The structure of the second guide layer of the present application is relatively loose, and the wood pulp fibers have a certain water absorption capacity, so that the second guide layer has a certain water retention capacity, which hinders the liquid from osmosis and reaching the first guide layer. When the liquid reaches the second guide layer, the liquid has a preliminary lateral diffusion trend under the action of the first guide layer, so the lateral diffusion trend of the liquid in the second guide layer is amplified, and at the same time, it is ensured that the liquid can quickly pass through the second guide layer to ensure the absorption speed. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 This is a planar structural diagram of the 3D core of Example 1 of the present application.
[0032] Figure 2 It is a planar structural diagram of the composite guide layer of the 3D core of Example 1 of the present application.
[0033] Description of reference numerals: 1. First hot air cloth; 11. Folded edge; 2. High polymer water-absorbing resin layer; 3. Guide cloth layer; 31. Second hot air cloth; 32. Composite guide layer; 321. First guide layer; 322. Second guide layer; 323. Third guide layer; 33. Dust-free paper. DETAILED DESCRIPTION
[0034] The following is combined with Figure 1-2 This application is described in further detail.
[0035] Example 1 like Figure 1 and Figure 2As shown, the 3D core of the menstrual hygiene product includes a guide fabric layer 3, a polymer water-absorbent resin layer 2 and a first hot air fabric 1. The polymer water-absorbent resin layer 2 is arranged on one side of the guide fabric layer 3, and the first hot air fabric 1 is arranged on the side of the polymer water-absorbent resin layer 2 away from the guide fabric layer 3.
[0036] The guide cloth layer 3 includes a second hot air cloth 31, a composite guide layer 32 and a dust-free paper 33 which are arranged in sequence. The second hot air cloth 31 is the skin-friendly side of the 3D core. The dust-free paper 33 is arranged on the side of the polymer water-absorbent resin layer 2 away from the first hot air cloth 1. The two sides of the first hot air cloth 1 are bent to form a folded edge 11, and the folded edge 11 is arranged on the side of the second hot air cloth 31 away from the composite guide layer 32.
[0037] The composite guide layer 32 includes a first guide layer 321 , a second guide layer 322 and a third guide layer 323 . The third guide layer 323 is disposed on a side of the dust-free paper 33 away from the first hot air cloth 1 .
[0038] The preparation method of the composite guide layer comprises the following steps: Polyester fiber and the first ES fine fiber are taken in a weight ratio of 1:1, the fineness of the polyester fiber is 1.5D, and the length is 30mm. The core layer of the first ES fine fiber is polypropylene, and the surface layer is polyethylene, the fineness is 1D, and the length is 8mm. The polyester fiber and the first ES fine fiber are mixed, broken up, and air combed to form a first fiber web. The first fiber web is penetrated by 125°C hot air to form a first guide layer.
[0039] ES crude fiber and wood pulp fiber are taken at a weight ratio of 1:0.2. The fineness of ES crude fiber is 7D, the core layer of ES crude fiber is polypropylene, the surface layer is polyethylene, the length is 8mm, and the fineness of wood pulp fiber is 3D, and the length is 4mm. The ES crude fiber and wood pulp fiber are mixed, broken up, and air combed to form a second fiber web. The second fiber web is penetrated by 125℃ hot air to make it bonded to form a second guide layer.
[0040] The first ES fine fiber, wood pulp fiber and bamboo fiber are taken in a weight ratio of 1:0.3:0.2. The core layer of the first ES fine fiber is polypropylene, the surface layer is polyethylene, the fineness is 1D, and the length is 8mm. The fineness of the wood pulp fiber is 3D, the length is 4mm, and the fineness of the bamboo fiber is 5D, and the length is 12mm. The first ES fine fiber, wood pulp fiber and bamboo fiber are mixed, broken up, and air combed to form a third fiber web. The third fiber web is penetrated by 125°C hot air to form a third guide layer.
[0041] The first guide layer, the second guide layer and the third guide layer are compacted and bonded by a 115° C. hot roller and cooled to obtain a composite guide layer, wherein the thicknesses of the first guide layer, the second guide layer and the third guide layer are 0.2 mm, 0.6 mm and 0.4 mm respectively.
[0042] The method for preparing the first hot air cloth and the second hot air cloth comprises the following steps: Polyester fiber and ES crude fiber are taken at a weight ratio of 1:0.5, the fineness of polyester fiber is 1.5D, the length is 30mm, the fineness of ES crude fiber is 7D, the core layer of ES crude fiber is polypropylene, the surface layer is polyethylene, and the length is 8mm; the polyester fiber and ES crude fiber are mixed, broken up, and air-combed to form a hot air cloth web, and the hot air cloth web is penetrated by 125℃ hot air to form a first hot air cloth and a second hot air cloth.
[0043] The method for preparing dust-free paper comprises the following steps: The second ES fine fiber and wood pulp fiber are taken at a weight ratio of 1:0.1. The core layer of the second ES fine fiber is polypropylene, the surface layer is polyethylene, the fineness is 1D, and the length is 8mm. The fineness of the wood pulp fiber is 3D, and the length is 4mm. The second ES fine fiber and the wood pulp fiber are broken up and combed by air flow to form a dust-free paper fiber web. The dust-free paper fiber web is penetrated by 125°C hot air to make it bonded to form dust-free paper.
[0044] A method for preparing a 3D core of a menstrual hygiene product comprises the following steps: The second hot air cloth, the composite guide layer and the dust-free paper are compacted and bonded by a 115°C hot roller and cooled to obtain a guide cloth layer. The thicknesses of the second hot air cloth, the composite guide layer and the dust-free paper in the guide cloth layer are 0.2 mm, 1.2 mm and 0.2 mm respectively.
[0045] EVA hot melt adhesive is sprayed on one side of the first hot air cloth, and polymer water-absorbing resin particles are added and bonded to form a polymer water-absorbing resin layer; EVA hot melt adhesive is sprayed on one side of the dust-free paper to bond the guide cloth layer to the polymer water-absorbing resin layer.
[0046] The two sides of the first hot air cloth are bent to form folded edges, and the folded edges are pressed to make them bonded to the second hot air cloth to obtain a 3D core. The thicknesses of the guide cloth layer, the polymer water-absorbing resin layer and the first hot air cloth are 1.6 mm, 2.4 mm and 0.2 mm, respectively.
[0047] Example 2 The difference between this embodiment and embodiment 1 is that the preparation methods of the 3D core and each fabric layer in the 3D core are different.
[0048] The preparation method of the composite guide layer comprises the following steps: Polyester fiber and the first ES fine fiber are taken in a weight ratio of 1:1.2, the fineness of the polyester fiber is 1.5D, and the length is 30mm. The core layer of the first ES fine fiber is polypropylene, and the surface layer is polyethylene, the fineness is 2D, and the length is 8mm. The polyester fiber and the first ES fine fiber are mixed, broken up, and air combed to form a first fiber web. The first fiber web is penetrated by 125°C hot air to form a first guide layer.
[0049] ES crude fiber and wood pulp fiber are taken at a weight ratio of 1:0.4. The fineness of ES crude fiber is 10D, the core layer of ES crude fiber is polypropylene, the surface layer is polyethylene, the length is 10mm, the fineness of wood pulp fiber is 3D, and the length is 4mm. The ES crude fiber and wood pulp fiber are mixed, broken up, and air combed to form a second fiber web. The second fiber web is penetrated by 125℃ hot air to make it bonded to form a second guide layer.
[0050] The first ES fine fiber, wood pulp fiber and bamboo fiber are taken in a weight ratio of 1:0.4:0.3. The core layer of the first ES fine fiber is polypropylene, the surface layer is polyethylene, the fineness is 2D, and the length is 8mm. The fineness of the wood pulp fiber is 3D, the length is 4mm, and the fineness of the bamboo fiber is 5D, and the length is 12mm. The first ES fine fiber, wood pulp fiber and bamboo fiber are mixed, broken up, and air combed to form a third fiber web. The third fiber web is penetrated by 125°C hot air to form a third guide layer.
[0051] The first guide layer, the second guide layer and the third guide layer are compacted and bonded by a 115° C. hot roller and cooled to obtain a guide fabric layer. The thicknesses of the first guide layer, the second guide layer and the third guide layer in the guide fabric layer are 0.2 mm, 0.5 mm and 0.3 mm respectively.
[0052] The method for preparing the first hot air cloth and the second hot air cloth comprises the following steps: Polyester fiber and ES crude fiber are taken at a weight ratio of 1:0.7, the fineness of polyester fiber is 1.5D, the length is 30mm, the fineness of ES crude fiber is 7D, the core layer of ES crude fiber is polypropylene, the surface layer is polyethylene, and the length is 8mm; the polyester fiber and ES crude fiber are mixed, broken up, and air-combed to form a hot air cloth web, and the hot air cloth web is penetrated by 125℃ hot air to form a first hot air cloth and a second hot air cloth.
[0053] The method for preparing dust-free paper comprises the following steps: The second ES fine fiber and wood pulp fiber are taken at a weight ratio of 1:0.2. The core layer of the second ES fine fiber is polypropylene, the surface layer is polyethylene, the fineness is 1D, and the length is 8mm. The fineness of the wood pulp fiber is 3D, and the length is 4mm. The second ES fine fiber and the wood pulp fiber are broken up and combed by air flow to form a dust-free paper fiber web. The dust-free paper fiber web is penetrated by 125°C hot air to make it bonded to form dust-free paper.
[0054] A method for preparing a 3D core of a menstrual hygiene product comprises the following steps: The second hot air cloth, the composite guide layer and the dust-free paper are compacted and bonded by a 115°C hot roller and cooled to obtain a guide cloth layer. The thicknesses of the second hot air cloth, the composite guide layer and the dust-free paper in the guide cloth layer are 0.2 mm, 1 mm and 0.2 mm respectively.
[0055] EVA hot melt adhesive is sprayed on one side of the first hot air cloth, and polymer water-absorbing resin particles are added and bonded to form a polymer water-absorbing resin layer; EVA hot melt adhesive is sprayed on one side of the third fiber layer to bond the guide cloth layer to the polymer water-absorbing resin layer.
[0056] The two sides of the first hot air cloth are bent to form folded edges, and the folded edges are pressed to make them bonded to the first fiber layer to obtain a 3D core. The thicknesses of the guide cloth layer, the polymer water-absorbing resin layer and the first hot air cloth are 1.4 mm, 2.8 mm and 0.2 mm, respectively.
[0057] Example 3 The difference between this embodiment and embodiment 1 is that the third guide layer is different. The preparation method of the third guide layer in this embodiment includes the following steps: The first ES fine fiber and wood pulp fiber are taken at a weight ratio of 1:0.3. The core layer of the first ES fine fiber is polypropylene, the surface layer is polyethylene, the fineness is 1D, and the length is 8mm. The fineness of the wood pulp fiber is 3D, and the length is 4mm. The first ES fine fiber and the wood pulp fiber are mixed, broken up, and air-combed to form a third fiber web. The third fiber web is penetrated by 125°C hot air to form a third guide layer.
[0058] Example 4 The difference between this embodiment and embodiment 1 is that the first ES fine fiber used in this embodiment is a pretreated ES fiber, and the preparation method of the pretreated ES fiber includes the following steps: Take potassium persulfate and water and mix them to obtain an initiator solution. Separately, evenly mix the first ES fine fiber, hydroxyethyl acrylate, N-hydroxymethyl acrylamide and water. The weight ratio of the first ES fine fiber to water is 1:50. Then, add the initiator solution dropwise while stirring. After the addition is completed, the molar concentration of hydroxyethyl acrylate in water is 0.15 mol / L, the molar concentration of N-hydroxymethyl acrylamide in water is 0.25 mol / L, and the molar concentration of the initiator in water is 0.005 mol / L. The reaction system is heated to 80°C and reacted for 2 hours. After the reaction is completed, filter and wash with water to obtain pretreated ES fibers.
[0059] Example 5 The difference between this embodiment and embodiment 1 is that the bamboo fiber used in this embodiment is pretreated bamboo fiber, and the preparation method of the pretreated bamboo fiber includes the following steps: The bamboo fiber was dispersed in a solvent with a mass ratio of ethanol to water of 1:9, and the mass ratio of bamboo fiber to solvent was 1:30. The fiber was heated to 70°C and KH560 silane coupling agent was added dropwise. The weight ratio of bamboo fiber to KH560 silane coupling agent was 1:0.08. After the addition was completed, the reaction was continued for 1 hour. After the reaction was completed, it was filtered and washed with ethanol and water to obtain pretreated bamboo fiber.
[0060] Example 6 The difference between this embodiment and embodiment 1 is that the first ES fine fiber used in this embodiment is a pretreated ES fiber, and the bamboo fine fiber used in this embodiment is a pretreated bamboo fiber.
[0061] The method for preparing the pretreated ES fiber comprises the following steps: Take potassium persulfate and water and mix them to obtain an initiator solution. Separately, evenly mix the first ES fine fiber, hydroxyethyl acrylate, N-hydroxymethyl acrylamide and water. The weight ratio of the first ES fine fiber to water is 1:50. Then, add the initiator solution dropwise while stirring. After the addition is completed, the molar concentration of hydroxyethyl acrylate in water is 0.15 mol / L, the molar concentration of N-hydroxymethyl acrylamide in water is 0.25 mol / L, and the molar concentration of the initiator in water is 0.005 mol / L. The reaction system is heated to 80°C and reacted for 2 hours. After the reaction is completed, filter and wash with water to obtain pretreated ES fibers.
[0062] The preparation method of pretreated bamboo fiber comprises the following steps: The bamboo fiber was dispersed in a solvent with a mass ratio of ethanol to water of 1:9, and the mass ratio of bamboo fiber to solvent was 1:30. The fiber was heated to 70°C and KH560 silane coupling agent was added dropwise. The weight ratio of bamboo fiber to KH560 silane coupling agent was 1:0.08. After the addition was completed, the reaction was continued for 1 hour. After the reaction was completed, it was filtered and washed with ethanol and water to obtain pretreated bamboo fiber.
[0063] Example 7 The difference between this embodiment and embodiment 1 is that the first ES fine fiber used in this embodiment is a pretreated ES fiber, and the bamboo fine fiber used in this embodiment is a pretreated bamboo fiber.
[0064] The method for preparing the pretreated ES fiber comprises the following steps: Take potassium persulfate and water and mix them to obtain an initiator solution. Separately, evenly mix the first ES fine fiber, hydroxyethyl acrylate, N-hydroxymethyl acrylamide and water. The weight ratio of the first ES fine fiber to water is 1:50. Then, add the initiator solution dropwise while stirring. After the addition is completed, the molar concentration of hydroxyethyl acrylate in water is 0.3 mol / L, the molar concentration of N-hydroxymethyl acrylamide in water is 0.35 mol / L, and the molar concentration of the initiator in water is 0.01 mol / L. The reaction system is heated to 80°C and reacted for 2 hours. After the reaction is completed, filter and wash with water to obtain pretreated ES fibers.
[0065] The preparation method of pretreated bamboo fiber comprises the following steps: The bamboo fiber was dispersed in a solvent with a mass ratio of ethanol to water of 1:9, and the mass ratio of bamboo fiber to solvent was 1:30. The fiber was heated to 70°C and KH560 silane coupling agent was added dropwise. The weight ratio of bamboo fiber to KH560 silane coupling agent was 1:0.15. After the addition was completed, the reaction was continued for 1 hour. After the reaction was completed, the fiber was filtered and washed with ethanol and water to obtain pretreated bamboo fiber.
[0066] Comparative Example 1 The difference between this comparative example and Example 1 is that the structure of the 3D core is different. In this comparative example, the composite guide layer is replaced with dust-free paper with a thickness of 1.6 mm.
[0067] Comparative Example 2 The difference between this comparative example and Example 1 is that the structure of the composite guide layer is different. In the composite guide layer in this comparative example, the first guide layer is replaced by a second hot air cloth with a thickness of 0.2 mm, that is, the composite guide layer includes a second hot air cloth, a second guide layer and a third guide layer.
[0068] Comparative Example 3 The difference between this comparative example and Example 1 is that the structure of the composite guide layer is different. In the composite guide layer in this comparative example, the second guide layer is replaced by a third guide layer with a thickness of 0.6 mm, that is, the composite guide layer includes a first guide layer with a thickness of 0.2 mm, a third guide layer with a thickness of 0.6 mm, and a third guide layer with a thickness of 0.4 mm.
[0069] Comparative Example 4 The difference between this comparative example and Example 1 is that the structure of the composite guide layer is different. In the composite guide layer in this comparative example, the third guide layer is replaced by a second guide layer with a thickness of 0.4 mm, that is, the composite guide layer includes a first guide layer with a thickness of 0.2 mm, a second guide layer with a thickness of 0.6 mm, and a second guide layer with a thickness of 0.4 mm.
[0070] Performance Testing Referring to QB / T 5650-2021 "Composite absorbent core for disposable paper sanitary products", the absorption rate and rewet amount of the 3D core were tested. Simulated menstrual blood was used as the test solution. The test results are recorded in Table 1.
[0071] In addition, in the above test, after the rewet test was completed, the depth of the color residue on the surface of the second hot air cloth was observed, and the depth levels were extremely dark, relatively dark, relatively light, and extremely light, and the observation results are shown in Table 1.
[0072] In addition, in the above test, after the back-infiltration test is completed, the guide fabric layer and the polymer water-absorbent resin layer are peeled off, and the polymer water-absorbent resin remaining on the guide fabric layer is removed. The absorption area of the simulated menstrual blood on the guide fabric layer is calculated by the hundred-grid method, and Comparative Example 1 is used as the reference group, and other embodiments and comparative examples are used as test groups, that is, the absorption area of Comparative Example 1 is used as a reference, and the absorption ratios of other embodiments and comparative examples relative to Comparative Example 1 are calculated according to the formula of test group / reference group. The larger the absorption ratio, the greater the degree of lateral diffusion. The calculation results are shown in Table 1.
[0073] In addition, the 3D core was taken and subjected to a wear simulation, and then the absorption speed was tested after the wear simulation. The wear simulation method is: the 3D core is impacted 200 times by a repeated impact tester, and then the 3D core is rubbed 20 times to complete the wear simulation. The test results are shown in Table 1.
[0074] Table 1 As shown in Table 1, Comparative Example 1 is an existing core with only dust-free paper on the surface. Compared with Comparative Example 1, the 3D core of Example 1 has a significant improvement in absorption speed, less re-seepage, lighter color residue, and a greater absorption ratio, that is, a greater degree of lateral diffusion, so the overall user experience of the 3D core is improved.
[0075] Comparing Example 1 with Comparative Example 2, it can be seen that the first guide layer adopts ES fiber with a different fineness from the second hot air cloth, thereby obtaining the effect of increasing the core absorption speed and reducing the rewet amount; comparing Example 1 with Comparative Example 3 and Comparative Example 4, it can be seen that the combination of the second guide layer and the third guide layer achieves a balance between longitudinal penetration and lateral diffusion of liquid when passing through the composite guide layer, thereby greatly improving the absorption speed.
[0076] Comparing Example 1 with Example 3, it can be seen that the bamboo fiber plays a role in absorbing and conducting water in the third guide layer, which greatly accelerates the absorption speed of the core.
[0077] Comparing Example 1 with Example 4, it can be seen that the pretreated first fine ES fiber not only effectively improves the absorption speed of the core body, but also the structure of the core body is still relatively stable after being used under the action of external force, maintaining a good absorption speed and good durability; comparing Example 1 with Example 5, it can be seen that the core body obtained by using the third guide layer of pretreated bamboo fiber has good durability; comparing Example 1 with Examples 6-7, it can be seen that by using the pretreated first fine ES fiber and bamboo fiber at the same time, the durability of the core body is further improved, and the degree of lateral diffusion is also further improved.
[0078] This specific implementation manner is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make non-creative modifications to the specific implementation manner as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.
Claims
1. A 3D core of a menstrual hygiene product, characterized in that: Includes a flow guide layer, and: A polymer water-absorbing resin layer is disposed on one side of the guide fabric layer; A first hot air cloth is arranged on a side of the polymer water-absorbing resin layer away from the guide cloth layer; The guide cloth layer includes a second hot air cloth, a composite guide layer and dust-free paper which are arranged in sequence, the dust-free paper is arranged on a side of the polymer water-absorbent resin layer away from the first hot air cloth, both sides of the first hot air cloth are bent to form a folded edge, and the folded edge is arranged on a side of the second hot air cloth away from the composite guide layer; The composite guide layer includes a first guide layer, a second guide layer and a third guide layer. The third guide layer is arranged on a side of the dust-free paper away from the first hot air cloth.
2. The 3D core of a menstrual hygiene product according to claim 1, characterized in that: The second hot air cloth is formed by thermal bonding of polyester fiber and ES crude fiber in a weight ratio of 1:(0.5-0.7); The first guide layer is formed by thermal bonding of polyester fiber and first ES fine fiber in a weight ratio of 1:(1-1.2); The second guide layer is formed by thermal bonding of ES coarse fibers and wood pulp fibers in a weight ratio of 1:(0.2-0.4); The third guide layer is formed by thermal bonding of the first ES fine fibers, wood pulp fibers and bamboo fibers in a weight ratio of 1: (0.3-0.4): (0.2-0.3); The dust-free paper is formed by thermally bonding the second ES fine fibers and the wood pulp fibers in a weight ratio of 1:(0.1-0.2).
3. The 3D core of a menstrual hygiene product according to claim 2, characterized in that: The first ES fine fibers are pretreated ES fibers, and the pretreated ES fibers are formed by grafting hydroxy acrylate and N-hydroxymethyl acrylamide onto the surface of the first ES fine fibers.
4. The 3D core of a menstrual hygiene product according to claim 3, characterized in that: The raw materials for preparing the pretreated ES fiber include first ES fine fibers, hydroxy acrylate, N-hydroxymethyl acrylamide, an initiator and a solvent, wherein the molar concentration of the hydroxy acrylate in the solvent is 0.15-0.3 mol / L, the molar concentration of the N-hydroxymethyl acrylamide in the solvent is 0.25-0.35 mol / L, and the molar concentration of the initiator in the solvent is 0.005-0.01 mol / L.
5. The 3D core of a menstrual hygiene product according to claim 2, characterized in that: The bamboo fiber is pretreated bamboo fiber, and the pretreated bamboo fiber is formed by grafting an epoxy silane coupling agent on the surface of the bamboo fiber.
6. The 3D core of a menstrual hygiene product according to claim 5, characterized in that: The raw materials for preparing the pretreated bamboo fiber include bamboo fiber and epoxy silane coupling agent, and the weight ratio of the bamboo fiber to the epoxy silane coupling agent is 1:(0.08-0.15).
7. The 3D core of a menstrual hygiene product according to claim 2, characterized in that: The fineness of the ES coarse fiber is 7-10D, and the fineness of the first ES fine fiber is 1-2D.
8. The 3D core of a menstrual hygiene product according to claim 1, characterized in that: The thickness ratio of the second hot air cloth, the composite guide layer and the dust-free paper is (0.16~0.2):1:(0.16~0.2), and the thickness ratio of the first guide layer, the second guide layer and the third guide layer is 1:(2.5~3):(1.5~2).
9. A method for preparing a 3D core of a menstrual hygiene product according to any one of claims 1 to 8, characterized in that: The following steps are involved: The second hot air cloth, the composite guide layer and the dust-free paper are bonded by hot pressing to obtain a guide cloth layer; Spray glue on one side of the first hot air cloth, add and bond high molecular water-absorbent resin particles to form a high molecular water-absorbent resin layer; spray glue on one side of the dust-free paper to bond the guide cloth layer to the high molecular water-absorbent resin layer; The two sides of the first hot air cloth are bent to form folded edges, and the folded edges are pressed to make them adhere to the second hot air cloth to obtain a 3D core.
10. The method for preparing a 3D core of a menstrual hygiene product according to claim 9, characterized in that: The preparation method of the composite guide layer comprises the following steps: The polyester fiber and the first ES fine fiber are mixed, scattered, and air-combed to form a first fiber web, and the first fiber web is thermally bonded to form a first guide layer; The ES coarse fibers and wood pulp fibers are mixed, broken up, and air-combed to form a second fiber web, and the second fiber web is thermally bonded to form a second guide layer; The first ES fine fibers, wood pulp fibers and bamboo fibers are mixed, broken up, and air-combed to form a third fiber web, and the third fiber web is thermally bonded to form a third guide layer; The first guide layer, the second guide layer and the third guide layer are thermally bonded, compacted and cooled to obtain a composite guide layer.
Citation Information
Cited By
3D (three-dimensional) sanitary towel based on viscose yarns and ES (ethylene-propylene side by side) fibers and preparation method thereof
CN120324192A
A 3D sanitary napkin based on viscose and ES fiber and its preparation method
CN120324192B