Optical functional layer, manufacturing method thereof and display device
By designing an optical functional layer consisting of a light-transmitting base layer and an anti-glare layer on the display device, the problem of easy cracking of anti-glare glass is solved, achieving good anti-glare effect and wear resistance, making it suitable for foldable display devices.
Patent Information
- Application Number
- CN202410999362.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-07-23
AI Technical Summary
The anti-glare glass in existing display devices is prone to cracking and has poor wear resistance during use, failing to meet higher usage requirements.
An optical functional layer was designed, including a light-transmitting base layer and an anti-glare layer. The anti-glare layer consists of multiple protrusions with a tangent slope of less than 0.1. The protrusions have a gentle slope and high uniformity. Combined with an anti-reflective layer and an anti-fingerprint layer, it is formed by a mold imprinting process.
It effectively avoids cracking of the optical functional layer, improves wear resistance and service life, reduces light interference with vision, and is suitable for foldable display devices.
Smart Images

Figure CN119001930A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of optical devices, and in particular to an optical functional layer and a manufacturing method thereof, and a display device. Background Art
[0002] When an external light source shines on the display screen of a display device, the light is reflected by a mirror on the display screen, thereby generating strong reflected light, which is glare. Glare can interfere with the user's vision, causing the user to be unable to see the screen clearly, affecting the visual health of the display device. In related technologies, display screens usually have anti-glare glass (AG glass for short) on the outermost layer to reduce glare. However, AG glass is prone to cracking and failure during use, and cannot meet the higher requirements of display devices. Summary of the invention
[0003] The present application provides an optical functional layer and a manufacturing method thereof, and a display device. The optical functional layer can effectively avoid the problem of cracking and has good bending ability and wear resistance.
[0004] In a first aspect, the present application provides an optical functional layer, which is used to be arranged on a display screen, and the optical functional layer includes a light-transmitting base layer and an anti-glare layer, wherein the anti-glare layer is arranged on a first surface of the light-transmitting substrate, and the anti-glare layer includes a plurality of protrusions, and the surfaces of the plurality of protrusions facing away from the light-transmitting base layer together constitute an anti-glare surface. With the first surface of the light-transmitting base layer as a reference plane, the absolute value of the tangent slope at any position on the anti-glare surface is less than or equal to 0.1.
[0005] It should be noted that, with the first surface of the light-transmitting base layer as the reference plane, the tangent slope at any position on the anti-glare surface specifically refers to: the tangent value of the angle between the tangent at any position on the anti-glare surface and the reference plane. The tangent slope at any position on the anti-glare surface can reflect the degree of inclination of the anti-glare surface at that position.
[0006] The optical functional layer provided in the above embodiment has an anti-glare surface. It is difficult for the external light to be totally reflected after entering the anti-glare surface, thereby achieving an anti-glare effect. Moreover, any position on the anti-glare surface has a small inclination, so that the multiple protrusions will not be squeezed against each other when the optical functional layer is bent, which can effectively avoid the problem of cracking of the optical functional layer. Moreover, the anti-glare surface has good mechanical properties, which can reduce the stress concentration generated by the protrusions when subjected to force, and improve the wear resistance and service life of the anti-glare surface. The optical functional layer in the above embodiment has good bending ability and wear resistance.
[0007] In conjunction with the first aspect, in some possible implementations, the absolute value of the slope change rate at any position on the anti-glare surface is less than or equal to 0.5. The slope change rate is a quantity that describes the speed of change of the slope at each position on the curve. From a mathematical point of view, the slope change rate of a point on the curve is equal to the second-order derivative of the curve at that point.
[0008] In the above embodiment, the slope of each point on the anti-glare surface changes slowly, and there is a smooth transition between each position of the anti-glare surface, without sharp positions with sudden changes in inclination. Taking the vertex of the protrusion as an example, the smooth transition of the protrusion at the vertex can increase the contact area between the protrusion and the outside, thereby reducing the stress concentration of the protrusion at the vertex and improving the wear resistance of the anti-glare surface. Taking the valley point of the protrusion as an example, adjacent protrusions can smoothly transition and border each other. When the optical functional layer is bent, the bending stress of the adjacent protrusions near the valley point can be effectively reduced, and the optical functional layer is not easy to break, thereby improving the bending ability of the optical functional layer.
[0009] In combination with the first aspect, in some possible implementations, the position on each protrusion where the distance from the reference plane is the largest is the vertex of the protrusion, and among the plurality of protrusions, the height difference between the vertices of any two protrusions in the height direction is less than or equal to 1 um, where the height direction refers to the direction perpendicular to the reference plane. In this way, the heights of the plurality of protrusions have good consistency, and the number of protrusions in contact with the external structure can be increased, thereby increasing the contact area under force, reducing stress concentration, and improving the wear resistance and service life of the anti-glare surface.
[0010] In combination with the first aspect, in some possible implementations, the position on each protrusion where the distance from the reference plane is the largest is the vertex of the protrusion, the position on each protrusion where the distance from the reference plane is the smallest is the valley of the protrusion, and the distance between the vertex on each protrusion and the valley of the protrusion in the height direction is 0.1um-10um, and the height direction refers to the direction perpendicular to the reference plane. The protrusion in this embodiment can achieve good light dispersion performance, so that the optical functional layer has good anti-glare ability, the protrusion has a small thickness dimension, can have good mechanical properties, and reduce the influence of the optical functional layer on the display optics of the display screen.
[0011] In combination with the first aspect, in some possible implementations, the maximum size of each protrusion in a direction parallel to the reference plane is 5-100 um. The protrusion in this embodiment has a size much smaller than the visible size of the human eye, which can reduce the impact of the optical functional layer on the display optics of the display screen.
[0012] In conjunction with the first aspect, in some possible embodiments, the protrusions are formed into non-spherical particles such as ellipsoidal particles, convex lens-shaped particles, disc-shaped particles, etc. Exemplarily, the edges of the protrusions used to border the adjacent protrusions are formed into irregular shapes. The shape of the protrusions in this embodiment is more disordered, and has a better anti-glare effect.
[0013] In combination with the first aspect, in some possible implementations, the light transmittance of the anti-glare layer is greater than or equal to 90%. The anti-glare layer can have good light transmittance to the light emitted from the inside of the display screen, reducing the influence of the optical functional layer on the display light of the display screen.
[0014] In combination with the first aspect, in some possible implementations, the haze of the anti-glare layer is less than or equal to 5%. The anti-glare layer has good gloss, transparency and imaging quality.
[0015] In combination with the first aspect, in some possible implementations, the hardness of the anti-glare layer is greater than or equal to 1H, so as to improve the wear resistance of the anti-glare surface and increase the service life of the optical functional layer.
[0016] In conjunction with the first aspect, in some possible implementations, the tensile modulus of the anti-glare layer is greater than or equal to 5 GPa. The anti-glare layer in this embodiment has a large tensile modulus and is not easily deformed during use (for example, when a user touches the display screen), thereby ensuring a stable display function of the display screen.
[0017] In combination with the first aspect, in some possible implementations, the elongation at break of the anti-glare layer is greater than or equal to 3%. The anti-glare layer has a large elongation at break, good softness and elasticity, and thus has good bending performance.
[0018] In combination with the first aspect, in some possible embodiments, the material of the light-transmitting base layer is any one of polyethylene terephthalate (PET), polycarbonate (PC), colorless polyimide (CPI), or ultra-thin flexible glass (UTG).
[0019] In combination with the first aspect, in some possible implementations, the anti-glare layer is made of acrylic resin material or epoxy resin material.
[0020] In combination with the first aspect, in some possible implementations, the optical functional layer further includes an anti-reflection layer, which covers the anti-glare surface and can reduce the reflectivity of light incident on the anti-glare layer, so that external light enters the anti-glare layer to be absorbed by the plurality of protrusions in the anti-glare layer, thereby improving the anti-glare performance. Exemplarily, the thickness of the anti-reflection layer is less than or equal to 500 nm, so as to reduce the overall thickness of the optical functional layer and facilitate the bending of the optical functional layer.
[0021] In combination with the first aspect, in some possible implementations, the anti-reflection layer includes a high-fold layer and a low-fold layer stacked on each other, the refractive index of the high-fold layer is greater than 1.65, and the refractive index of the low-fold layer is less than 1.55. The high-fold layer and the low-fold layer stacked on each other can reduce the reflectivity of light incident on the anti-glare layer. Exemplarily, the high-fold layer includes high-fold particles, such as zirconium oxide or aluminum oxide. Exemplarily, the low-fold layer includes hollow silica particles.
[0022] In combination with the first aspect, in some possible implementations, the optical functional layer further includes an anti-fingerprint layer, and the anti-fingerprint layer covers the anti-glare surface. In other possible implementations, the optical functional layer includes an anti-reflection layer and an anti-fingerprint layer, and the anti-reflection layer covers the anti-glare surface, and the anti-fingerprint layer is located on the side of the anti-reflection layer away from the anti-glare layer. The anti-fingerprint layer can reduce the adhesion of fingerprints, making it easy to clean the dirt on the surface of the display screen.
[0023] In some possible implementations, the thickness of the anti-fingerprint layer is less than 50 nm, so as to reduce the overall thickness of the optical functional layer and facilitate bending of the optical functional layer.
[0024] In a second aspect, the present application provides a method for manufacturing an optical functional layer, which is used for the optical functional layer in any of the above possible implementations, and the manufacturing method comprises:
[0025] A layered gelatin material is arranged on the surface of the light-transmitting base layer, and a mold is used to emboss the gelatin material to form a protrusion.
[0026] The above-mentioned manufacturing method can simply and quickly manufacture the optical functional layer provided in the embodiment of the present application.
[0027] In some possible implementations, the above manufacturing method specifically includes: arranging a layered colloid material (e.g., UV curing glue or thermoplastic curing glue) on the surface of a light-transmitting base layer (e.g., made of any of PET, PC, CPI, or UTG), then arranging the layered colloid material toward a mold formed with a recessed portion so that the mold squeezes the layered colloid material, and then irradiating light from the opposite side of the light-transmitting base layer where the layered colloid material is arranged to cure the colloid material, or baking the layered colloid material to cure the colloid material. Finally, the mold is removed, and thus, the manufacturing method forms an anti-glare surface with a specific shape and size on the colloid material through a mold embossing process. .
[0028] In conjunction with the second aspect, in some possible implementations, the manufacturing method further includes:
[0029] Depositing multiple layers of inorganic materials at least on the anti-glare surface in a vacuum environment by evaporation or sputtering to form an anti-reflection layer; or
[0030] Hollow silica sphere coating is applied to the anti-glare surface to form an anti-reflection layer.
[0031] In conjunction with the second aspect, in some possible implementations, the manufacturing method further includes:
[0032] The anti-fingerprint layer is formed on the side of the anti-reflection layer away from the anti-fingerprint layer by vacuum coating or wet spraying.
[0033] In a third aspect, the present application provides a display device, comprising a display screen and an optical functional layer in any possible implementation manner described above, wherein the optical functional layer is disposed on the display screen. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0035] Figure 1 is a schematic structural diagram of a display device provided by an exemplary embodiment of the present application;
[0036] Figure 2 is a cross-sectional view of an optical functional layer provided by an exemplary embodiment of the present application after being cut along a direction perpendicular to the first surface;
[0037] Figure 3 is a cross-sectional view of an optical functional layer provided by another exemplary embodiment of the present application, cut along a direction perpendicular to the first surface;
[0038] Figure 4 is a top view of an optical functional layer provided by another exemplary embodiment of the present application;
[0039] Figure 5 is a curve schematic diagram of the anti-glare surface of the optical functional layer provided by another exemplary embodiment of the present application after being cut along a direction perpendicular to the first surface;
[0040] Figure 6 is a cross-sectional view of the optical function layer provided by another exemplary embodiment of the present application after being cut along a direction perpendicular to the first surface;
[0041] Figure 7 is a flow chart of a method for manufacturing an optical functional layer provided by an exemplary embodiment of the present application;
[0042] Figure 8 4 is a flow chart of a method for manufacturing an optical functional layer provided in another exemplary embodiment of the present application. DETAILED DESCRIPTION
[0043] In order to make the objectives, technical solutions and advantages of the present invention more clear, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings.
[0044] In the following, the terms "first", "second", etc. are used only for convenience of description and are not to be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise specified, "plurality" means two or more.
[0045] In the embodiments of the present application, unless otherwise clearly specified and limited, the term "electrical connection" can be a direct electrical connection or an indirect electrical connection through an intermediate medium. The words "exemplary" or "for example" are used to indicate examples, illustrations or explanations. Any embodiment or design described as "exemplary" or "for example" in the embodiments of the present application should not be interpreted as being more preferred or more advantageous than other embodiments or designs. Specifically, the use of words such as "exemplary" or "for example" is intended to present related concepts in a concrete way. "And / or" describes the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone, where A and B can be singular or plural. The character " / " generally indicates that the objects associated before and after are in an "or" relationship.
[0046] In the embodiments of the present application, the directional indications such as up, down, left, right, front and back used to explain the structure and movement of different components in the present application are relative. These indications are appropriate when the components are in the positions shown in the figures. However, if the description of the component position changes, these directional indications will also change accordingly. It should also be noted that in the embodiments of the present application, the same reference numerals are used to represent the same component or the same component. For the same components in the embodiments of the present application, the figure may only be marked with a reference numeral for one of the components or components as an example. It should be understood that the reference numerals are also applicable to other identical components or components.
[0047] First, a unified explanation is given for terms that may be involved in the embodiments of the present invention.
[0048] Slope: The slope is a measure of the inclination of a straight line (or the tangent of a curve) with respect to the (horizontal) coordinate axis, usually expressed as the tangent of the angle between the straight line (or the tangent of the curve) and the (horizontal) coordinate axis. From a mathematical point of view, the slope of a point on a straight line (or curve) is equal to the first-order derivative of the straight line (or curve) at that point.
[0049] Slope change rate: The slope change rate is a quantity that describes the speed of change of the slope at each position on the curve. From a mathematical point of view, the slope change rate of a point on the curve is equal to the second-order derivative of the curve at that point.
[0050] Diffuse reflection: When a beam of parallel light is projected onto an object with a rough surface, the reflected light is no longer parallel, but is emitted in all directions. This reflection phenomenon is called diffuse reflection. The reflected light of diffuse reflection is emitted in all directions, and the reflected light is softer and less dazzling.
[0051] Light transmittance: Light transmittance indicates the ability of light to pass through a medium. It is the percentage of the luminous flux passing through a transparent or translucent body to the incident luminous flux. When a parallel monochromatic light beam passes through a uniform, non-scattering medium, part of the light is absorbed, part of it passes through the medium, and part of it is reflected by the surface of the medium. Light transmittance can indicate the efficiency of light transmission of display devices, etc., which directly affects the visual effect of the touch screen.
[0052] Haze: Haze is the percentage of the transmitted light intensity that deviates from the incident light by more than 2.5° to the total transmitted light intensity. Specifically, a beam of parallel light from a standard light source is vertically irradiated onto a transparent or translucent film, sheet, plate or other material. The parallel light is scattered inside and on the surface of the material. The haze is the percentage of the luminous flux of the scattered light that deviates from the incident direction by more than 2.5° to the luminous flux that passes through the material. The greater the haze, the lower the gloss, transparency and imaging of the film. Haze is an important parameter for describing the optical transparency of transparent or translucent materials.
[0053] Hardness: The ability of a material to locally resist the penetration of a hard object into its surface is called hardness. The local resistance of a solid to the invasion of foreign objects is an indicator for comparing the softness and hardness of various materials.
[0054] Tensile modulus: Tensile modulus refers to the elasticity of a material when stretched. The value of the tensile modulus is the ratio of the force required to stretch the material per unit length along the central axis to the cross-sectional area of the material. The tensile modulus is a physical quantity that describes the ability of a solid material to resist deformation.
[0055] Elongation at break: Elongation at break refers to the ratio of the displacement value of a material when it is broken to its original length, expressed as a percentage. Elongation at break is an indicator of the softness and elasticity of a material. The greater the elongation at break, the better the softness and elasticity of the material.
[0056] Steel wool wear test: It is a method used to test the wear resistance of the material surface. The test method is to use steel wool to rub back and forth on the surface of the material under a specific load, and to evaluate the wear resistance of the material by testing the difference in the water drop angle on the surface of the material before and after the friction.
[0057] The optical functional layer and its manufacturing method, and the specific structure of the display device provided by the embodiments of the present application will be described in detail below in conjunction with the relevant drawings.
[0058] The embodiment of the present application provides a display device 1000, which can be a mobile phone, a tablet personal computer, a laptop computer, a personal digital assistant (PDA), a camera, a personal computer, a notebook computer, a vehicle-mounted device, a wearable device, a watch, augmented reality (AR) glasses, an AR helmet, virtual reality (VR) glasses or a VR helmet, etc. Exemplarily, the display device 1000 can be a portable display device 1000.
[0059] refer to Figure 1 As shown, Figure 1 1 is a schematic diagram of the structure of a display device 1000 provided in an embodiment of the present application. Figure 1In the illustrated embodiment, the display device 1000 is a mobile phone. In some embodiments, the display device 1000 includes a display screen 1001, which is used to receive electrical signals and optically display information for the user to view. The display screen 1001 in the display device 1000 may be used only for optical display, or the display screen 1001 may also be integrated with a touch module, and the user may input information or implement a specific function by performing a touch operation on the display screen 1001. In some embodiments, the display device 1000 is a foldable mobile phone, and the foldable mobile phone has a first screen and a second screen, and the first screen and the second screen can be close to or away from each other through a rotating shaft 1006, so that the foldable mobile phone has a folded state and an unfolded state.
[0060] The display device 1000 may also include a back shell 1002, a control circuit board (not shown), a battery (not shown), a camera and other components. For example, the display screen 1001 can be combined with the back shell 1002 to jointly form the outer contour of the display device 1000. The back shell 1002 can be used to protect the internal electronic devices (such as circuit boards, batteries, etc.) of the display device 1000. In some embodiments, the back shell 1002 may include a back cover and a middle frame, and the middle frame is fixed to the back cover. Exemplarily, the middle frame can be fixedly connected to the back cover by adhesive. The middle frame can also be an integrally formed structure with the back cover, that is, the middle frame and the back cover are an integral structure. The display screen 1001 can be connected to the middle frame by, for example, bonding. The aforementioned circuit board, battery and other components can be accommodated in the space formed by the display screen 1001, the middle frame and the back cover. The circuit board may include a flexible circuit board, a rigid circuit board, etc. Power devices such as chips and controllers may be provided on the circuit board.
[0061] For another example, the display device 1000 may further include a front camera 1003, and a camera hole may be provided on the display screen 1001, through which the front camera 1003 can obtain image information of the light-emitting side of the display screen 1001. In some other examples, the display device 1000 may also not include a battery, for example, it may be directly connected to an external power source for use. It is understandable that Figure 1 Only some components of the display device 1000 are schematically shown, and the actual shapes, actual sizes, actual positions and actual structures of these components are not subject to the present invention. Figure 1 and the limitations of the following drawings.
[0062] In some embodiments, the display device 1000 is a foldable display device, such as a foldable mobile phone or a foldable tablet computer. Exemplarily, the foldable display device includes a first part 1004, a second part 1005, a display screen 1001, and a hinge 1006. The first part 1004 and the second part 1005 are movably connected through the hinge 1006, and the display screen 1001 is carried on the first part 1004 and the second part 1005. The foldable display device 1000 has an unfolded state and a folded state. In the unfolded state, the first part 1004, the hinge 1006, and the second part 1005 are located or approximately located in the same plane, and the display screen 1001 is carried on the first part 1004, the hinge 1006, and the second part 1005, and the display screen 1001 is in a flat unfolded state. In the folded state, the first part 1004 and the second part 1005 are close to each other through the hinge 1006, so that the first part 1004 and the second part 1005 are overlapped, and the display screen 1001 is bent. In some embodiments, the display screen 1001 is located between the first portion 1004 and the second portion 1005. In other embodiments, the display screen 1001 covers the first portion 1004, the hinge 1006 and the outer side of the second portion 1005. It can be seen that the display screen 1001 used in the foldable display device 1000 needs to have a certain bending ability and elasticity to adapt to the unfolded state and the folded state.
[0063] In some embodiments, the display device 1000 includes a display screen 1001 and a flexible circuit board (not shown), and the flexible circuit board is electrically connected to the display screen 1001 to provide an electrical signal to the display screen 1001. Exemplarily, a first end of the flexible circuit board can be electrically connected to the display screen 1001, and the other end of the flexible circuit board can be provided with a connector, and the connector is used to be plugged into an external controller or power supply, so that the display screen 1001 is easy to install and remove. In an embodiment where the display screen 1001 is applied to the display device 1000, the flexible circuit board of the display screen 1001 module can be connected between the display screen 1001 and the control circuit board of the display device 1000 to play a role in signal transmission.
[0064] The display screen 1001 in the embodiment of the present application can be a flexible display screen or a rigid display screen. Exemplarily, the display screen 1001 can be any one of an organic light-emitting diode (OLED) display screen, an active-matrix organic light-emitting diode or an active-matrix organic light-emitting diode (AMOLED) display screen, a mini organic light-emitting diode (Mini organic light-emitting diode) display screen, a micro organic light-emitting diode (micro organic light-emitting diode) display screen, a quantum dot light-emitting diode (QLED) display screen, and a liquid crystal display (LCD).
[0065] In some usage scenarios, external ambient light enters the display screen 1001, and is reflected and emitted from the display screen 1001. The reflected light may cause the user to be unable to clearly view the content on the display screen 1001. In some embodiments, a polarizer is provided in the display screen 1001 to absorb the reflected ambient light. However, since the polarizer is an absorption polarizer, the light emitted from the display screen 1001 will also be absorbed by the polarizer, thereby reducing the light extraction efficiency of the display screen 1001. In other words, although the polarizer can enable the display screen 1001 to achieve visual function under ambient light, it also brings about the problem of low light extraction efficiency. In other embodiments, the industry has proposed a technology of forming a color filter on a thin film encapsulation structure (color filter on thin film encapsulation, CF on TFE, COE). COE technology is a new technology that can replace polarizers. By making the color filter on the thin film encapsulation (thin film encapsulation, TFE) layer, the color filter can be used to transmit specific spectrum light and absorb other spectrum light. The characteristics of light, can achieve the suppression of ambient light, so that the display screen 1001 can also clearly show the content in strong light environments such as outdoors. Furthermore, compared with the technical solution using polarizers, the color film has a thinner structure, which is conducive to making the display screen 1001 lighter and thinner and achieving flexible display characteristics.
[0066] In some usage scenarios, the light from an external light source is irradiated onto the display screen 1001 of the display device 1000, and the light is easily totally reflected on the panel of the display screen 1001 to produce strong reflected light, which is also called glare. Glare can interfere with the user's line of sight, causing the user to be unable to see the screen clearly, affecting the visual health of the display device 1000. In some embodiments, the display screen 1001 includes anti-glare glass (AG glass for short). AG glass specifically refers to a disordered random structure of glass formed on the glass by a frosting etching process, so that light is diffusely reflected between multiple random structures of glass, and it is difficult for light to be totally reflected regularly on the surface of the random structure of glass, thereby reducing the interference of light on the user's line of sight and achieving an anti-glare effect. However, the random structure of glass on AG glass usually has the problem of sharp transition of surface structure, which causes AG glass to crack easily when bent. In addition, the wear resistance of AG glass is poor, and its anti-glare surface fails in about 50 times in the steel wool wear test.
[0067] Based on this, an embodiment of the present application provides an optical function layer 100, which is used to be arranged on a display screen 1001, replacing the conventional AG glass mentioned above, so as to achieve an anti-glare function for the display screen 1001. Exemplarily, the optical function layer 100 is located on the light-emitting side of the display screen 1001, for example, the optical function layer 100 covers the polarizer or color filter layer of the display screen 1001. In other embodiments, the optical function layer 100 is used to cover the glass cover plate of the display screen 1001.
[0068] Figure 2 A cross-sectional view of an optical functional layer 100 provided by an exemplary embodiment of the present application is shown. It should be noted that the structural dimensions shown in the drawings of the present application do not represent the structural dimensions in actual applications. For the convenience of the drawings, the structures shown in the drawings of the present application have certain deformations in size ratios, which do not constitute any limitation to the present application.
[0069] like Figure 2 As shown, the optical functional layer 100 includes a light-transmitting base layer 1 and an anti-glare layer 2. The anti-glare layer 2 is disposed on the first surface 11 of the light-transmitting substrate. The anti-glare layer 2 includes a plurality of protrusions 21. The surfaces of the plurality of protrusions 21 facing away from the light-transmitting base layer 1 together constitute the anti-glare surface G. With the first surface 11 of the light-transmitting base layer 1 as the reference plane F, the absolute value of the tangent slope k at any position on the anti-glare surface G is less than or equal to 0.1, that is, |k|≥0.01 is satisfied. In some embodiments, the tangent slope k at any position on the anti-glare surface G satisfies the relationship of 0.01≤|k|≤0.05.
[0070] Taking the first surface 11 of the light-transmitting base layer 1 as the reference plane F, the tangent slope at any position on the anti-glare surface G specifically refers to: the tangent value of the angle between the tangent at any position on the anti-glare surface G and the reference plane F. For example, refer to Figure 2 As shown in FIG. 1 , the tangent line aa at point A on the anti-glare surface G intersects the first surface 11 as the reference plane F and forms an angle α, and the slope of point A is the tangent value of the angle α. In addition, from a mathematical point of view, the slope of any position on the anti-glare surface G is equal to the first-order derivative of the anti-glare surface G at that position. Figure 2 In the cross-sectional view shown, the anti-glare surface G can be regarded as a curve on the cross-sectional view, and the slope of point A on the anti-glare surface G can be obtained by calculating the first-order derivative of the curve of the anti-glare surface G on the cross-sectional view at point A. In addition, the slope of the tangent line at any position on the anti-glare surface G can also be obtained by any other method, and the present application does not impose any specific limitation on this.
[0071] In the above embodiment, the anti-glare layer 2 includes a plurality of protrusions 21, and the surfaces of the plurality of protrusions 21 facing away from the light-transmitting base layer 1 together constitute an anti-glare surface G. External light is diffusely reflected when entering the anti-glare surface G, that is, it is difficult to have regular total reflection. The light is refracted and absorbed between the plurality of protrusions 21, thereby reducing the interference of light on the user's line of sight and achieving a good anti-glare effect.
[0072] The tangent slope at any position on the anti-glare surface G can reflect the degree of inclination of the anti-glare surface G at that position. In the optical functional layer 100, the first surface 11 of the light-transmitting base layer 1 is taken as the reference plane F, and the absolute value of the tangent slope at any position on the anti-glare surface G is less than or equal to 0.1. In this way, any position on the anti-glare surface G has a smaller inclination than the first surface 11, so that the protrusion 21 of the anti-glare surface G transitions at a relatively gentle angle. Compared with the solution in the related art in which there are sharp protrusions on the anti-glare surface, when the anti-glare surface is folded, the sharp protrusions are easy to interfere with other protrusions and thus damage the anti-glare surface. The inclination of each position on the anti-glare surface G in the embodiment of the present application is low. Even if the optical functional layer 100 is bent, the adjacent protrusions 21 will not be squeezed against each other, which can effectively avoid the problem of cracking of the optical functional layer 100.
[0073] On the other hand, any position on the anti-glare surface G has a smaller inclination than the first surface 11, which can improve the mechanical properties of the protrusion 21, increase the force contact area of the protrusion 21, thereby reducing the stress concentration generated by the protrusion 21 when it is subjected to force, and improving the wear resistance and service life of the anti-glare surface G. Exemplarily, in the steel wool wear test of the anti-glare surface G, since any position on the anti-glare surface G has a smaller inclination, the steel wool and the anti-glare surface can have a larger actual contact area, and the anti-glare surface can disperse the stress, reduce the local force of the protrusion 21, and thus have good wear resistance.
[0074] It can be seen that the optical functional layer 100 provided in the above embodiment has an anti-glare surface G, and the protrusions 21 of the anti-glare surface G all have a small inclination, so that the multiple protrusions 21 will not squeeze each other when the optical functional layer 100 is bent, which can effectively avoid the problem of cracking of the optical functional layer 100. In addition, the anti-glare surface G has good mechanical properties, which can reduce the stress concentration generated by the protrusions 21 when subjected to force, and improve the wear resistance and service life of the anti-glare surface G. The optical functional layer 100 in the above embodiment has good bending ability and wear resistance, and has good application prospects. For example, the optical functional layer 100 can be used in a foldable display device 1000, such as a foldable mobile phone or a foldable tablet computer.
[0075] like Figure 2 and Figure 3 As shown, each protrusion 21 has a position where the distance from the reference plane F is the largest, that is, the vertex T of the protrusion 21. Each protrusion 21 has a position where the distance from the reference plane F is the smallest, that is, the valley point B of the protrusion 21. It should be noted that each protrusion 21 may have more than one vertex T and more than one valley point B, but the distance between each protrusion 21 and the reference plane F has a certain maximum value and a certain minimum value.
[0076] refer to Figure 4 As shown, two adjacent protrusions 21 border each other at the valley point B, and the same protrusion 21 can border multiple different protrusions 21 in the circumferential direction, and multiple protrusions 21 border each other, so that the surfaces of the multiple protrusions 21 facing away from the light-transmitting base layer 1 can together form an integral anti-glare surface G.
[0077] In some embodiments, the protrusions 21 are formed as non-spherical particles such as ellipsoidal particles, convex lens-shaped particles, and disc-shaped particles. Figure 4The top view of the optical functional layer 100 is shown. In some embodiments, the edges of the protrusions 21 bordering the adjacent protrusions 21 are formed into irregular shapes. In this way, the protrusions 21 have disordered irregular shapes, which can improve the anti-glare effect of the anti-glare surface G.
[0078] In some embodiments, the absolute value of the slope change rate at any position on the anti-glare surface G is less than or equal to 0.5. The slope change rate is a quantity that describes the speed of change of the slope at each position on the curve. From a mathematical point of view, the slope change rate of a point on the curve is equal to the second-order derivative of the curve at that point. In this embodiment, the absolute value of the slope change rate at any position on the anti-glare surface G is less than or equal to 0.5. The slope change rate of each point on the anti-glare surface G that satisfies this relationship is relatively gentle, and there is a gentle transition between each position of the anti-glare surface G, without a sharp position with a sudden change in inclination.
[0079] Especially at the position where the bending direction of the protrusion 21 changes, for example, the bending direction of the protrusion 21 on both sides of the vertex T / valley point B changes, and its slope undergoes a sudden change in positive and negative values. The absolute value of the slope change rate of the vertex T of the protrusion 21 is less than or equal to 0.5. For example, the absolute value of the slope change rate of the vertex T of the protrusion 21 is 0.05-0.3. In this way, the transition of the protrusion 21 at the vertex T is smooth, which can increase the contact area between the protrusion 21 and the outside, thereby reducing the stress concentration of the protrusion 21 at the vertex T and improving the wear resistance of the anti-glare surface G. The absolute value of the slope change rate of the valley point B of the protrusion 21 is less than or equal to 0.5. For example, the absolute value of the slope change rate of the valley point B of the protrusion 21 is 0.05-0.3. In this way, adjacent protrusions 21 can smoothly transition and border each other. When the optical functional layer 100 is bent, the bending stress exerted on the adjacent protrusions 21 near the valley point B can be effectively reduced, and the optical functional layer 100 is not prone to breakage, thereby improving the bending ability of the optical functional layer 100.
[0080] In some embodiments, the distance between the vertex T on each protrusion 21 and the valley point B of the protrusion 21 in the height direction is 0.1um-10um, and the height direction refers to the direction perpendicular to the reference plane F (ie, the first surface 11). Figure 2 As shown, the distance H between the vertex T on the protrusion 21 and the valley point B of the protrusion 21 in the height direction is 0.05um-3um. In the above embodiment, the protrusion 21 can achieve good light dispersion performance, so that the optical function layer 100 has good anti-glare ability, the protrusion 21 has a small thickness, can have good mechanical properties, and reduce the influence of the optical function layer 100 on the display optics of the display screen 1001.
[0081] In some embodiments, among the plurality of protrusions 21, the height difference between the vertices T of any two protrusions 21 in the height direction is less than or equal to 1 um. Figure 3 As shown, a height difference h between the vertex T1 of the first protrusion 21 and the vertex T2 of the second protrusion 21 in the height direction is less than or equal to 1 um, for example, the height difference h is 0.01 um-0.5 um.
[0082] The heights of the multiple protrusions 21 in the above embodiment have good consistency. When in contact with an external structure, the number of protrusions 21 in contact with the external structure can be increased, thereby increasing the force contact area, reducing stress concentration, and improving the wear resistance and service life of the anti-glare surface G. For example, in the steel wool wear test of the anti-glare surface G, since the heights of the multiple protrusions 21 are close to each other, the steel wool can contact different protrusions 21 at the same time when in contact with the anti-glare surface, thereby having a larger actual contact area, and the anti-glare surface can disperse stress, reduce the local force of the protrusion 21, and thus have good wear resistance.
[0083] In some embodiments, the maximum size of each protrusion 21 in the direction parallel to the reference plane F is 5um-100um. It should be noted that the direction parallel to the reference plane F here can also be understood as a direction perpendicular to the aforementioned height direction. In other words, the maximum size of each protrusion 21 in the direction perpendicular to the height direction is 5um-100um. The protrusion 21 that satisfies this relationship has a size that is much smaller than the visible size of the human eye, which can reduce the impact of the optical functional layer 100 on the display optics of the display screen 1001.
[0084] Figure 4 is a top view of an optical functional layer 100 provided in an exemplary embodiment of the present application, wherein the ordinate and abscissa are respectively marked with the dimensions in the direction (in um), with reference to Figure 4 As shown, the maximum dimension of each protrusion 21 in a direction parallel to the reference plane F is the maximum dimension of the edge of each protrusion 21 bordering the adjacent protrusion 21 . Figure 5 1 is a schematic diagram of a curve of the anti-glare surface G of the optical functional layer 100 provided by an exemplary embodiment of the present application after being cut along a direction perpendicular to the first surface 11, wherein the ordinate marks the dimension in the thickness direction perpendicular to the reference plane F (in um), and the abscissa marks the dimension in the direction parallel to the reference plane F (in um). Figure 5As shown, the dimension of the protrusion 21 where the first vertex T on the curve is located in the thickness direction perpendicular to the reference plane F is 1.456um, the dimension of the protrusion 21 where the second vertex T on the curve is located in the thickness direction perpendicular to the reference plane F is 1.500um, and the height difference between the second vertex T and the first vertex T in the thickness direction perpendicular to the reference plane F is 0.044. In addition, the distance between the two valley points B of the protrusion 21 where the first vertex T on the curve is located in the horizontal coordinate direction is less than 50um.
[0085] Figure 4 and Figure 5 The optical function layer 100 shown can maintain anti-glare performance after being rubbed 2000 times in a steel wool abrasion test, and the optical function layer 100 can be bent at a bending radius R greater than or equal to 0.8 mm without breaking.
[0086] In some embodiments, the transmittance of the anti-glare layer 2 is greater than or equal to 90%. The transmittance indicates the ability of light to pass through a medium. The anti-glare layer 2 meeting this transmittance can have good light transmittance performance for the light emitted from the inside of the display screen 1001, thereby reducing the influence of the optical functional layer 100 on the display light of the display screen 1001.
[0087] In some embodiments, the haze of the anti-glare layer 2 is less than or equal to 5%. Haze is an important parameter for describing the optical transparency of transparent or translucent materials. The anti-glare layer 2 that satisfies this relationship has good gloss, transparency and imaging, so as to improve the optical performance of the display device 1000.
[0088] In some embodiments, the hardness of the anti-glare layer 2 is greater than or equal to 1H, so as to improve the wear resistance of the anti-glare surface G and increase the service life of the optical function layer 100 .
[0089] In some embodiments, the tensile modulus of the anti-glare layer 2 is greater than or equal to 5 GPa. The tensile modulus is a physical quantity used to describe the ability of a solid material to resist deformation. The anti-glare layer 2 in this embodiment has a large tensile modulus and is not easily deformed during use, thereby ensuring the stable display function of the display screen 1001. In an embodiment in which the display screen 1001 includes a touch module, the user performs a touch operation on the display screen 1001, and the anti-glare layer 2 has a large tensile modulus, which can resist deformation or damage to the optical functional layer 100 caused by the user touching the display screen 1001.
[0090] In some embodiments, the elongation at break of the anti-glare layer 2 is greater than or equal to 3%. The elongation at break is an indicator of the softness and elasticity of the material. The anti-glare layer 2 in this embodiment has a large elongation at break, good softness and elasticity, and is not prone to breakage when the optical functional layer 100 is bent, thereby having good bending performance and being suitable for a foldable display device 1000 (such as a foldable mobile phone or a foldable tablet, etc.).
[0091] In some embodiments, the anti-glare layer 2 is made of acrylic resin material or epoxy resin material. Taking acrylic resin material as an example, acrylic resin material has good light transmittance, haze, hardness and crack resistance, so that the optical function layer 100 can have good optical properties and is not easy to break in a bent state.
[0092] The light-transmitting base layer 1 is made of a material having good light-transmitting properties. Exemplarily, the material of the light-transmitting base layer 1 is any one of polyethylene terephthalate (PET), polycarbonate (PC), colorless polyimide (CPI), or ultra-thin flexible glass (UTG).
[0093] like Figure 6 As shown, in some embodiments, the optical functional layer 100 further includes an anti-reflection layer 3, and the anti-reflection layer 3 covers the anti-glare surface G of the anti-glare layer 2. The anti-reflection layer 3 can reduce the reflectivity of the light incident on the anti-glare layer, so that the external light enters the anti-glare layer to be absorbed by the plurality of protrusions 21 in the anti-glare layer, thereby improving the anti-glare performance and enhancing the visibility of the display screen 1001. In some embodiments, the thickness of the anti-reflection layer 3 is less than or equal to 500nm, so as to reduce the overall thickness of the optical functional layer 100, which is conducive to the bending of the optical functional layer 100. It should be noted that the direction of the thickness mentioned here is parallel to the aforementioned height direction.
[0094] In some embodiments, the anti-reflection layer 3 includes a high-fold layer and a low-fold layer stacked on each other. The high-fold layer and the low-fold layer stacked on each other can reduce the reflectivity of the light incident on the anti-glare layer. The refractive index of the high-fold layer is greater than 1.65. For example, the high-fold layer includes high-fold particles, such as zirconium oxide or aluminum oxide. The refractive index of the low-fold layer is less than 1.55. For example, the low-fold layer includes hollow silica particles.
[0095] In some embodiments, the optical functional layer 100 further includes an anti-fingerprint layer 4. Exemplarily, the anti-fingerprint layer 4 covers the side of the anti-glare layer away from the transparent substrate. In an embodiment where the optical functional layer 100 includes an anti-reflection layer 3, the anti-fingerprint layer 4 is located on the side of the anti-reflection layer 3 away from the anti-glare layer. The anti-fingerprint layer 4 can reduce the adhesion of fingerprints, making it easy to clean the dirt on the surface of the display screen 1001.
[0096] In some embodiments, the thickness of the anti-fingerprint layer 4 is less than 50 nm to reduce the overall thickness of the optical functional layer 100 and facilitate bending of the optical functional layer 100. Exemplarily, the thickness of the anti-fingerprint layer 4 is 10 nm. In some embodiments, the anti-fingerprint layer 4 is made of perfluoropolyether material.
[0097] like Figure 7 In a second aspect, the present application provides a method for manufacturing an optical functional layer 100, which is used for the optical functional layer 100 in any of the above possible implementations, and the manufacturing method includes:
[0098] S101 , arranging a layered colloid material on the surface of the light-transmitting base layer 1 , and forming a protrusion 21 on the colloid material by embossing with a mold.
[0099] The above-mentioned manufacturing method can simply and quickly manufacture the optical functional layer 100 provided in the embodiment of the present application. Specifically, in some embodiments, the manufacturing method arranges a layered colloid material (e.g., a UV curing glue or a thermoplastic curing glue) on the surface of a light-transmitting base layer 1 (e.g., made of any of PET, PC, CPI, or UTG), and then arranges the layered colloid material toward a mold formed with a recessed portion so that the mold extrude the layered colloid material, and then irradiates light from the opposite side of the light-transmitting base layer 1 where the layered colloid material is arranged to cure the colloid material, or bakes the layered colloid material to cure the colloid material. Finally, the mold is removed, and thus, the manufacturing method forms an anti-glare surface G having a specific shape and size on the colloid material through a mold embossing process.
[0100] In some embodiments, the colloid material is a thermoplastic curing glue, such as an acrylic resin solvent. In some embodiments, the viscosity of the acrylic resin solvent before baking is less than 100 cgs to meet the processing requirements of the mold imprinting process.
[0101] In the embodiment where the optical functional layer 100 further includes an anti-reflection layer 3, the anti-reflection layer 3 is exemplarily disposed on the side of the anti-glare layer 2 away from the light-transmitting substrate. Figure 8 As shown, the method for manufacturing the optical functional layer 100 further includes:
[0102] S201 , depositing multiple layers of inorganic materials on the anti-glare surface G in a vacuum environment by evaporation or sputtering to form an anti-reflection layer 3 , or coating the anti-glare surface G with hollow silica sphere coating to form an anti-reflection layer 3 .
[0103] In an embodiment where the optical functional layer 100 further includes an anti-fingerprint layer 4, exemplarily, the anti-fingerprint layer 4 is disposed on a side of the anti-reflection layer 3 away from the anti-fingerprint layer 4. Corresponding to this embodiment, exemplarily, the method for manufacturing the optical functional layer 100 further includes:
[0104] S202 , forming the anti-fingerprint layer 4 on the side of the anti-reflection layer 3 facing away from the anti-fingerprint layer 4 by vacuum coating or wet spraying.
[0105] The above are only some embodiments and implementation methods of the present application, and the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by any person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the protection scope of the claims.
Claims
1. An optical functional layer (100), the optical functional layer (100) being used to be arranged on a display screen (1001), characterized in that: include: Light-transmitting base layer (1); An anti-glare layer (2) is arranged on the first surface (11) of the light-transmitting substrate, the anti-glare layer (2) comprises a plurality of protrusions (21), and surfaces of the plurality of protrusions (21) facing away from the light-transmitting base layer (1) together constitute an anti-glare surface (G); Wherein, taking the first surface (11) of the light-transmitting base layer (1) as the reference plane (F), the absolute value of the tangent slope at any position on the anti-glare surface (G) is less than or equal to 0.
1.
2. The optical functional layer (100) according to claim 1, characterized in that: The absolute value of the slope change rate at any position on the anti-glare surface (G) is less than or equal to 0.
5.
3. The optical functional layer (100) according to claim 1 or 2, characterized in that: The position on each protrusion (21) at the maximum distance from the reference plane (F) is the vertex (T) of the protrusion (21); among the plurality of protrusions (21), the height difference between the vertices of any two protrusions (21) in the height direction is less than or equal to 1 um, and the height direction is a direction perpendicular to the reference plane (F).
4. The optical functional layer (100) according to any one of claims 1 to 3, characterized in that: The position on each protrusion (21) at which the distance from the reference plane (F) is the largest is the vertex (T) of the protrusion (21), the position on each protrusion (21) at which the distance from the reference plane (F) is the smallest is the valley point (B) of the protrusion (21), and the distance between the vertex (T) on each protrusion (21) and the valley point (B) of the protrusion (21) in the height direction is 0.1um-10um, and the height direction is a direction perpendicular to the reference plane (F).
5. The optical functional layer (100) according to any one of claims 1 to 4, characterized in that: The maximum dimension of each protrusion (21) in a direction parallel to the reference plane (F) is 5-100 um.
6. The optical functional layer (100) according to any one of claims 1 to 5, characterized in that: The light transmittance of the anti-glare layer (2) is greater than or equal to 90%; and / or, The haze of the anti-glare layer (2) is less than or equal to 5%.
7. The optical functional layer (100) according to any one of claims 1 to 6, characterized in that: The hardness of the anti-glare layer (2) is greater than or equal to 1H; and / or, The tensile modulus of the anti-glare layer (2) is greater than or equal to 5 GPa; and / or, The elongation at break of the anti-glare layer (2) is greater than or equal to 3%.
8. The optical functional layer (100) according to any one of claims 1 to 7, characterized in that: The light-transmitting base layer (1) is made of any one of a polyester terephthalate material, a polycarbonate material, a transparent polyimide material, or an ultra-thin flexible glass material.
9. The optical functional layer (100) according to any one of claims 1 to 8, characterized in that: The anti-glare layer (2) is made of acrylic resin material or epoxy resin material.
10. The optical functional layer (100) according to any one of claims 1 to 9, characterized in that: The optical functional layer (100) further comprises an anti-reflection layer (3), wherein the anti-reflection layer (3) covers the anti-glare surface (G).
11. The optical functional layer (100) according to claim 10, characterized in that: The thickness of the anti-reflection layer (3) is less than or equal to 500 nm.
12. The optical functional layer (100) according to claim 10, characterized in that: The optical functional layer (100) further comprises an anti-fingerprint layer (4), wherein the anti-fingerprint layer (4) covers a side of the anti-reflection layer (3) away from the anti-glare layer.
13. The optical functional layer (100) according to claim 12, characterized in that: The thickness of the anti-fingerprint layer (4) is less than or equal to 50 nm.
14. A method for manufacturing an optical functional layer, for manufacturing the optical functional layer (100) according to any one of claims 1 to 13, characterized in that: The manufacturing method comprises: A layered colloid material is arranged on the surface of the light-transmitting base layer (1), and the protrusion (21) is formed by pressing the colloid material with a mold.
15. A display device (1000), characterized in that: The display device (1000) comprises a display screen (1001) and an optical functional layer (100) according to any one of claims 1 to 13, wherein the optical functional layer (100) is arranged on the display screen (1001).
Citation Information
Patent Citations
Anti-glare film, method of manufacturing the same, and display device
CN101251608A
Method for producing anti-glare film
CN101324677A
Optical film and manufacturing method therefor, anti-glare film, polarizing element with optical layer, and display device
CN101815958A
Anti-glare sheet for image display device
CN103975258A
Anti-glare hard coat laminated film
CN110358343A
Cited By
Optical component, display screen module and foldable electronic equipment
CN120255037A
Optical component, display screen module and foldable electronic equipment
CN120539856A
Optical component, display screen module and foldable electronic device
CN120539856B
Optical functional layer and manufacturing method therefor, and display device
WO2026020803A1
Anti-glare film and preparation method therefor
WO2026137870A1