Flue gas desulfurization additive and preparation method thereof
By using specific combinations of flue gas desulfurization additives in wet flue gas desulfurization equipment, the problem of insufficient efficiency and high operating costs in the face of strict SO2 emission standards is solved, and more efficient desulfurization and nitrogen removal effects are achieved, while reducing the efficiency of reducing the number of The equipment is scaled and the system reliability is improved.
Patent Information
- Application Number
- CN202411451541.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-17
- Publication Date
- 2024-11-26
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
When existing wet flue gas desulfurization equipment faces increasingly strict SO2 emission standards, it is difficult to meet the design desulfurization efficiency, and the operating costs are high and the equipment is prone to scale, resulting in the equipment being unable to be effectively upgraded.
Using a flue gas desulfurization additive, including diammonium hydroxide, sodium formate, volcanic rock powder, platinum powder, copper powder, disodium EDTA, iron oxide, calcium formate, activated soil and polyaspartic acid, through a specific combination and treatment methods, form a mixture with adsorption and catalytic effects, improve desulfurization efficiency and prevent scaling.
It improves the flue gas desulfurization efficiency, reduces operating costs, slows down calcium scale rate, enhances system reliability, and meets stricter SO2 emission standards without renovating the equipment.
Smart Images

Figure CN119015855A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of preparation of desulfurization additives, and more specifically discloses a flue gas desulfurization additive and a preparation method thereof. Background Art
[0002] Among the many flue gas desulfurization technologies, wet flue gas desulfurization has been the most widely used desulfurization technology as a relatively mature and efficient desulfurization technology. However, it also has the disadvantages of large initial investment, high operating costs and easy scaling of equipment. With the gradual increase in the sulfur content of flue gas from pulverized coal boilers in power plants and the implementation of increasingly stringent environmental emission standards in 2012, some desulfurization equipment that has been put into operation is difficult to meet the increasingly stringent SO2 emission standards even at its designed desulfurization efficiency. Studies have shown that in wet desulfurization technology, adding a certain amount of appropriate additives can not only improve its desulfurization efficiency and the utilization rate of desulfurizers, thereby reducing operating costs, but also slow down the scaling rate of calcium, thereby improving the reliability of the system. Without upgrading the original desulfurization equipment, the study of using desulfurization additives to improve the designed desulfurization rate of the equipment has practical significance. Summary of the invention
[0003] The main technical problem solved by the present invention is to provide a flue gas desulfurization additive and a preparation method thereof, which can solve the problem that the desulfurization equipment already in use cannot meet the increasingly stringent SO2 emission standards.
[0004] The present invention provides a flue gas desulfurization additive, comprising the following components in parts by weight: The invention comprises 6-10 parts of diammine silver hydroxide, 6-10 parts of sodium formate, 25-30 parts of volcanic rock powder, 0.1-0.2 parts of platinum powder, 4-6 parts of copper powder, 10-12 parts of disodium EDTA, 3-5 parts of iron oxide, 3-5 parts of calcium formate, 15-20 parts of active soil and 12-15 parts of polyaspartic acid.
[0005] Preferably, the silver diammine hydroxide is an aqueous ammonia solution of reagent grade silver diammine hydroxide.
[0006] The sodium formate is industrial grade sodium formate powder.
[0007] The volcanic rock powder is 320 mesh ultra-fine volcanic rock powder The platinum powder is ultrafine platinum powder with an average particle size of less than 0.5 μm.
[0008] The calcium formate is chemical grade calcium formate powder; The iron oxide is iron oxide powder with a particle size of 1 μm; The copper powder is an ultrafine copper powder with a particle size of 500 mesh; The disodium EDTA is industrial grade disodium EDTA powder; The activated soil is ordinary activated clay powder; The polyaspartic acid is industrial grade polyaspartic acid.
[0009] The present invention also provides a method for preparing a flue gas desulfurization additive, comprising the following steps: S1. Dissolve diammine silver hydroxide and sodium formate in water, add ultrafine platinum powder, add volcanic rock powder and activated soil while stirring, mix and filter, and dry to obtain adsorption mixed soil; S2. The adsorption mixed soil is mixed with calcium formate, iron oxide, copper powder, disodium EDTA and polyaspartic acid and stirred evenly to obtain a flue gas desulfurization additive.
[0010] Preferably, in step S1, the amount of water used to dissolve diammine silver hydroxide and sodium formate is 500wt% of the total amount of volcanic rock powder and active soil, the mixing time is 30min, the mixing temperature is room temperature, and the drying condition is 25°C forced air drying.
[0011] Preferably, in step S2, the mixing method is mechanical stirring, and the mixing time is 1 hour.
[0012] The present invention has the following beneficial effects: (1) The present invention adsorbs silver diammine hydroxide, sodium formate and platinum powder into the pores of volcanic rock powder and activated soil. By virtue of the adsorption capacity of the pores of the volcanic rock powder and activated soil, while adsorbing sulfur dioxide, the silver diammine hydroxide and sodium formate in the pores undergo a silver mirror reaction under flue gas heating conditions to generate ammonia and silver. The ammonia reacts with the adsorbed nitrogen dioxide and nitrogen monoxide under the catalysis of platinum powder to generate harmless nitrogen. The generated silver reacts with hydrogen sulfide to generate silver sulfide, thereby removing nitrogen while removing sulfur.
[0013] (2) The volcanic rock powder and activated soil added in the present invention have both adsorption and decolorization functions, thereby further removing harmful components in the flue gas.
[0014] (3) The disodium EDTA added in the present invention has a complexing effect on the metal ions after the dereaction, which can prevent the metal ions from adhering to the metal surface after the reaction, and is conducive to ensuring the subsequent reaction.
[0015] (4) The copper powder added in the present invention can react with sulfur dioxide or nitrogen dioxide, and the iron oxide added in the present invention can directly react with sulfur dioxide and sulfur trioxide.
[0016] (5) The polyaspartic acid added in the present invention can prevent the flue gas desulfurization additive from scaling and agglomerating during use, thereby making it more fully utilized. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The present invention is further described in detail below with reference to the accompanying drawings and specific implementation methods.
[0018] Figure 1 It is the chemical reaction principle diagram of the present invention. DETAILED DESCRIPTION
[0019] The present invention will be described in detail below with reference to the accompanying drawings and in combination with embodiments. It should be noted that the embodiments and features in the embodiments of the present application can be combined with each other without conflict.
[0020] The wet flue gas desulfurization additive provided by the present invention is applied to the inlet flue gas SO2 design concentration of 2100mg / Nm 2 In the desulfurization system, the specific embodiments are as follows: Example 1
[0021] The components of the desulfurization additive and the weight proportions of each component are: 8 parts of diammine silver hydroxide 8 parts of sodium formate 27 parts volcanic rock powder 0.15 parts of platinum powder 0.5 parts of copper powder EDTA disodium 11 parts 4 parts of iron oxide Calcium formate 4 parts 17 parts of active soil 13 parts of polyaspartic acid (1) Dissolve 8 kg of silver diammine hydroxide ammonia solution and 8 kg of ammonium formate in 220 kg of water at room temperature, add 0.15 kg of ultrafine platinum powder, add 27 kg of volcanic rock powder and 17 kg of active soil while stirring, mix for 30 minutes, filter, and dry with air at 25°C to obtain adsorption mixed soil.
[0022] (2) Add the adsorption mixed soil into a solid mixer, add 11 kg of disodium EDTA, 4 kg of calcium formate, 0.5 kg of copper powder, 4 kg of iron oxide and 13 kg of polyaspartic acid, mix and stir evenly to obtain a flue gas desulfurization additive.
[0023] Example 2
[0024] The components of the desulfurization additive and the weight proportions of each component are: 6 parts of diammine silver hydroxide 6 parts of sodium formate 25 parts volcanic rock powder Platinum powder 0.1 part 0.4 parts of copper powder 10 parts of disodium EDTA 3 parts of iron oxide Calcium formate 3 parts 15 parts of active soil 12 parts of polyaspartic acid (1) Dissolve 6 kg of silver diammine hydroxide ammonia solution and 6 kg of ammonium formate in 200 kg of water at room temperature, add 0.1 kg of ultrafine platinum powder, add 25 kg of volcanic rock powder and 15 kg of active soil while stirring, mix for 30 minutes, filter, and dry at 25°C to obtain adsorption mixed soil.
[0025] (2) Add the adsorption mixed soil into a solid mixer, add 10 kg of disodium EDTA, 3 kg of calcium formate, 0.4 kg of copper powder, 3 kg of iron oxide and 12 kg of polyaspartic acid, mix and stir evenly to obtain a flue gas desulfurization additive.
[0026] Example 3
[0027] The components of the desulfurization additive and the weight proportions of each component are: 10 parts of diammine silver hydroxide 10 parts of sodium formate 30 parts volcanic rock powder 0.2 parts of platinum powder 0.6 parts of copper powder 12 parts of disodium EDTA 5 parts of iron oxide 5 parts calcium formate 20 parts of active soil 15 parts of polyaspartic acid (1) Dissolve 10 kg of silver diammine hydroxide ammonia solution and 10 kg of ammonium formate in 250 kg of water at room temperature, add 0.2 kg of ultrafine platinum powder, add 30 kg of volcanic rock powder and 20 kg of active soil while stirring, mix for 30 minutes, filter, and dry at 25°C to obtain adsorption mixed soil.
[0028] (2) Add the adsorption mixed soil into a solid mixer, add 12 kg of disodium EDTA, 5 kg of calcium formate, 0.6 kg of copper powder, 5 kg of iron oxide and 15 kg of polyaspartic acid, mix and stir evenly to obtain a flue gas desulfurization additive.
[0029] Example 4
[0030] The components of the desulfurization additive and the weight proportions of each component are: 6 parts of diammine silver hydroxide 6 parts of sodium formate 30 parts volcanic rock powder Platinum powder 0.1 part 0.4 parts of copper powder 10 parts of disodium EDTA 3 parts of iron oxide Calcium formate 3 parts 20 parts of active soil 12 parts of polyaspartic acid (1) Dissolve 6 kg of silver diammine hydroxide ammonia solution and 6 kg of ammonium formate in 250 kg of water at room temperature, add 0.1 kg of ultrafine platinum powder, add 30 kg of volcanic rock powder and 20 kg of active soil while stirring, mix for 30 minutes, filter, and dry at 25°C to obtain adsorption mixed soil.
[0031] (2) Add the adsorption mixed soil into a solid mixer, add 10 kg of disodium EDTA, 3 kg of calcium formate, 0.4 kg of copper powder, 3 kg of iron oxide and 12 kg of polyaspartic acid, mix and stir evenly to obtain a flue gas desulfurization additive.
[0032] Example 5
[0033] The components of the desulfurization additive and the weight proportions of each component are: 10 parts of diammine silver hydroxide 10 parts of sodium formate 25 parts volcanic rock powder 0.2 parts of platinum powder 0.6 parts of copper powder 12 parts of disodium EDTA 5 parts of iron oxide 5 parts calcium formate 15 parts of active soil 15 parts of polyaspartic acid (1) Dissolve 10 kg of silver diammine hydroxide ammonia solution and 10 kg of ammonium formate in 200 kg of water at room temperature, add 0.2 kg of ultrafine platinum powder, add 25 kg of volcanic rock powder and 15 kg of active soil while stirring, mix for 30 minutes, filter, and dry at 25°C to obtain adsorption mixed soil.
[0034] (2) Add the adsorption mixed soil into a solid mixer, add 12 kg of disodium EDTA, 5 kg of calcium formate, 0.6 kg of copper powder, 5 kg of iron oxide and 15 kg of polyaspartic acid, mix and stir evenly to obtain a flue gas desulfurization additive.
[0035] Comparative Example 1 Same as Example 1, except that no ultrafine platinum powder is added.
[0036] Comparative Example 2 Same as Example 1, except that copper powder and iron oxide are not added.
[0037] Comparative Example 3 Same as Example 1, except that polyaspartic acid is not added.
[0038] Comparative Example 4 Same as Example 1, except that disodium EDTA was not added.
[0039] Comparative Example 5 Same as Example 1, except that silver diammine hydroxide and sodium formate are not added.
[0040] Comparative Example 6 Same as Example 1, except that no active soil is added.
[0041] The flue gas desulfurization additives prepared in the examples and comparative examples were applied to the inlet flue gas with an initial SO2 concentration of 1584 mg / Nm 2 In the desulfurization system, the addition amount is 1% of the weight of the limestone slurry. The specific data of the concentrations of SO2, H2S and nitrogen dioxide in the outlet flue gas, the liquid-gas ratio, the calcium-sulfur ratio and the desulfurization efficiency are shown in Table 1.
[0042] Table 1 Test results of flue gas desulfurization additives of examples and comparative examples
[0043] Note: nd means not detected.
[0044] As shown in Table 1, the desulfurization additive can desulfurize to a greater extent through the cooperation of various components, and it also has a good effect on denitrification and dust adsorption.
[0045] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by ordinary technicians in this technical field within the essential scope of the present invention also fall within the protection scope of the present invention.
Claims
1. A flue gas desulfurization additive, It is characterized in that It includes the following components by weight: 6-10 parts of diammine silver hydroxide, 6-10 parts of sodium formate, 25-30 parts of volcanic rock powder, 0.1-0.2 parts of platinum powder, 0.4-0.6 parts of copper powder, 10-12 parts of disodium EDTA, 3-5 parts of iron oxide, 3-5 parts of calcium formate, 15-20 parts of active soil and 12-15 parts of polyaspartic acid.
2. The flue gas desulfurization additive according to claim 1, It is characterized in that The diammine silver hydroxide is a reagent grade ammonia solution of diammine silver hydroxide; The sodium formate is industrial grade sodium formate powder; The volcanic rock powder is 320 mesh ultra-fine volcanic rock powder; The platinum powder is an ultrafine platinum powder with an average particle size of less than 0.5 μm; The calcium formate is chemical grade calcium formate powder; The iron oxide is iron oxide powder with a particle size of 1 μm; The copper powder is an ultrafine copper powder with a particle size of 500 mesh; The disodium EDTA is industrial grade disodium EDTA powder; The activated soil is ordinary activated clay powder; The polyaspartic acid is industrial grade polyaspartic acid.
3. A method for preparing the flue gas desulfurization additive according to any one of claims 1 to 2, It is characterized in that The steps include: S1. Dissolve diammine silver hydroxide and sodium formate in water, add ultrafine platinum powder, add volcanic rock powder and activated soil while stirring, mix and filter, and dry to obtain adsorption mixed soil; S2. The adsorption mixed soil is mixed with calcium formate, iron oxide, copper powder, disodium EDTA and polyaspartic acid and stirred evenly to obtain a flue gas desulfurization additive.
4. The method for preparing the flue gas desulfurization additive according to claim 3, It is characterized in that In the step S1, the amount of water used to dissolve diammine silver hydroxide and sodium formate is 500wt% of the total amount of volcanic rock powder and active soil, the mixing time is 30min, the mixing temperature is room temperature, and the drying condition is 25°C forced air drying.
5. The method for preparing the flue gas desulfurization additive according to claim 3, It is characterized in that In step S2, the mixing method is mechanical stirring, and the mixing time is 1 hour.