Air-cooled fuel cell stack
By introducing a metal porous transport layer into the air-cooled fuel cell stack, the problem of unstable stack structure under high power density is solved, and sealing, gas transmission stability and stack performance are improved.
Patent Information
- Application Number
- CN202511028461.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-25
- Publication Date
- 2025-08-22
- Estimated Expiration
- 2045-07-25
AI Technical Summary
The existing air-cooled fuel cell stacks have problems such as reduced contact area between the cathode gas diffusion layer and the bipolar plate, increased contact resistance, carbon fiber breakage, and seal failure caused by the sealing line trapped in the flow channel under high power density, which affects the stability and life of the stack.
A metal porous transport layer is added between the bipolar plate and the membrane electrode. One side of the metal porous transport layer is in close contact with the membrane electrode to reduce contact resistance, and a raised structure is provided on the other side to disturb the flow of gas and is embedded in the bipolar plate to support the sealing line to ensure uniform stress.
It improves the sealing and stability of the stack, reduces contact resistance, enhances gas transmission stability, expands the cathode flow channel structure design space, and improves the overall performance of the stack.
Smart Images

Figure CN120527408A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of battery stacks, and in particular relates to an air-cooled fuel cell stack. Background Art
[0002] Air-cooled proton exchange membrane fuel cell stacks are primarily categorized as area-air-cooling and open-cathode stacks, depending on how air acts on them. Area-air-cooled stacks utilize only air as a coolant, and without specialized cooling channels, they struggle to meet heat dissipation requirements. Adding cooling channels complicates the stack structure, but the cooling efficiency remains lower than that of a water-cooled system, making it difficult for the battery to operate under optimal conditions. In contrast, open-cathode stacks utilize air for both cooling and cathode oxygen supply, resulting in a simpler structure, eliminating the need for a water-cooling system and oxygen storage tanks, and significantly reducing the stack's mass and volume. Consequently, they have become the mainstream direction of current air-cooled fuel cell research.
[0003] An air-cooled fuel cell stack is usually composed of an end plate, a current collecting plate, a bipolar plate, and a membrane electrode. Its power generally does not exceed 5kW and is suitable for scenarios such as backup power supplies and drones. However, different applications have different requirements for stack performance (such as durability and weight-to-power ratio). In a typical structure, the cathode adopts a straight-through flow field, and a fan drives air through the flow channel, which not only supplies the oxygen required for the reaction but also removes waste heat. However, with the increase in membrane electrode power density, the heat generation and oxygen consumption per unit volume of the stack increase significantly, and the gas channel needs to be expanded to enhance heat dissipation and gas transmission. However, the increase in flow channel width will lead to the following problems: (1) The contact area between the cathode gas diffusion layer (GDL) and the bipolar plate ridge decreases, and the contact resistance increases; (2) The GDL carbon fiber breaks due to local pressure overload, affecting the life of the stack; (3) The sealing line may sink into the flow channel, causing seal failure and threatening the stability of the stack.
[0004] In existing technologies, the bipolar plate flow field design is not well matched with the mechanical and electrochemical properties of the gas diffusion layer, limiting the development of high-power density air-cooled fuel cell stacks. Therefore, a new structure is urgently needed that can optimize current collection capabilities and improve fuel cell stack reliability while ensuring efficient mass transfer and heat dissipation. Summary of the Invention
[0005] The present invention provides an air-cooled fuel cell stack to solve the technical problem of unstable stack structure in the prior art.
[0006] The technical solutions provided by the present invention are as follows: An air-cooled fuel cell stack comprises: a bipolar plate (7), a membrane electrode (9) and a metal porous transmission layer (8); wherein: The cathode side (7-1) of the bipolar plate (7) is provided with a cathode flow field, and the anode side (7-2) of the bipolar plate (7) is provided with an anode flow field; The membrane electrode (9) comprises a membrane electrode cathode side (9-1) and a membrane electrode anode side (9-2), and both the anode and cathode sides of the membrane electrode have gas diffusion layers; A metal porous transport layer (8), the metal porous transport layer is arranged between the cathode side (7-1) of the bipolar plate and the cathode side (9-1) of the membrane electrode; one side of the metal porous transport layer is a plane, the plane is in close contact with the membrane electrode to reduce contact resistance; the other side of the metal porous transport layer is provided with a protrusion structure, the protrusion structure is in contact with the cathode flow field ridge of the bipolar plate to disturb gas flow.
[0007] Optionally, the metal porous transport layer (8) is embedded in the bipolar plate, the thickness of the metal porous transport layer (8) is equal to the depth of the cathode groove of the bipolar plate, and the length and width of the metal porous transport layer match the cathode groove of the bipolar plate, so that the upper coating (8-1) of the metal porous transport layer is flush with the upper surface of the cathode plate of the bipolar plate.
[0008] Optionally, the metal porous transmission layer (8) has a porosity of 30% to 85% and a thickness of 0.05 mm to 0.3 mm; The material of the metal porous transmission layer (8) is at least one of titanium, stainless steel, nickel or aluminum, and the surface is plated, the plated material is carbon, platinum or nickel, and the thickness of the plated layer is 0.05 μm to 0.5 μm.
[0009] Optionally, the protrusion structure of the metal porous transport layer (8) is fish-scale-shaped, triangular-shaped or arc-shaped, and the protrusion height is less than or equal to 1 / 2 of the thickness of the metal porous transport layer (8), which is used to generate turbulence when the gas flows through and promote gas diffusion to the membrane electrode.
[0010] Optionally, the pore structure of the metal porous transmission layer (8) is diamond-shaped, circular or square; When the hole structure is diamond-shaped, the two diagonal dimensions of the diamond-shaped hole are 0.5 mm to 3 mm and 0.3 mm to 1.5 mm respectively, and the long diagonal is perpendicular to the flow channel ridge, and the dimension of the long diagonal is greater than the width of the flow channel ridge; When the hole structure is circular, the diameter of the circular hole is 0.6 mm to 2 mm, and the diameter is larger than the width of the flow channel ridge; When the hole structure is square, the side length of the square hole is 0.5 mm to 2 mm, one side is perpendicular to the flow channel ridge, and the side length is greater than the flow channel ridge width.
[0011] Optionally, when the pore structure is diamond-shaped, the protrusions of the protrusion structure are located on two adjacent sides of the diamond mesh, and the two sides form a triangle with the long diagonal line. The gas flows from the vertical direction of the long diagonal line to the protrusion area of the metal porous transport layer, and is blocked by the protrusions, generating turbulence, thereby accelerating diffusion to the membrane electrode; When the hole structure is square, the protrusion of the protrusion structure is located on an edge of the square hole perpendicular to the flow channel ridge, and the edge is located on the edge after the gas flows through the square hole. After the gas flows through the square hole, it is blocked by the protrusion, generating turbulence and accelerating diffusion to the membrane electrode; When the hole structure is circular, the convex position of the convex structure is located on a semicircle perpendicular to the flow channel ridge. The semicircle is located on the semicircular arc after the gas flows through the circular hole. The line connecting the two points on the edge passes through the center of the circle and is perpendicular to the flow channel ridge.
[0012] Optionally, the groove-land ratio of the cathode flow field of the bipolar plate is 2:1-4:1, and the groove width is 2 mm-4.5 mm; The flow grooves of the cathode flow field are point-shaped or line-segment-shaped, the groove-ridge ratio of adjacent flow field line segments is 1:1~3:1, and the groove width is 1.5mm~4mm.
[0013] Optionally, the frame of the membrane electrode (9) contacts the bipolar plate sealing line (10), and the metal porous transmission layer (8) evenly supports the sealing line to prevent it from sinking into the cathode flow channel, thereby ensuring the sealing of the stack.
[0014] Optionally, flow grooves are provided on the cathode surface and the anode surface of the bipolar plate, and air inlets and air outlets are provided at both ends of the flow grooves; the membrane electrode is composed of a catalytic layer, a proton exchange membrane and a gas diffusion layer, the catalytic layer is coated on both sides of the proton exchange membrane, and the gas diffusion layer is covered on both sides of the proton exchange membrane coated with the catalytic layer.
[0015] Optionally, the metal porous transmission layer (8) is prepared by any of the following methods: The metal sheet is punched by a rolling mill, and the hole area is 0.1mm 2 ~4mm 2 , the hole spacing is 0.2mm~1mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge; The metal fiber is felted and hot pressed and sintered, and then punched by a rolling mill with a hole area of 0.1mm 2 ~2mm 2 , the hole spacing is 0.4mm~3mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge; The metal powder is spread flat in the forming mold, hot pressed and vacuum sintered, and then punched by a rolling mill with a hole area of 0.1mm 2 ~2mm 2The hole spacing is 0.4mm~3mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge.
[0016] The beneficial effects of the present invention are: The technical solution provided by the embodiments of the present invention adds a porous metal transport layer between the bipolar plate and the membrane electrode. The porous metal transport layer has a stable structure and is not easily compressed or deformed, thereby ensuring uniform force on the sealing line. This eliminates the risk of the sealing line in traditional structures being trapped in the flow field. The sealing line is evenly compressed, reducing the risk of uneven compression leading to poor sealing and unstable stack structure. In addition, one side of the porous metal transport layer is flat, in close contact with the membrane electrode to reduce contact resistance; the other side is provided with a raised structure, which contacts the cathode flow field ridge of the bipolar plate to disturb the gas flow, enhance gas dispersion, and improve overall gas transmission stability. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0018] Figure 1 A schematic structural diagram of an air-cooled fuel cell stack provided in one embodiment of the present invention; Figure 2 A schematic diagram of a metal porous transport layer, bipolar plate and membrane electrode structure provided in one embodiment of the present invention; FIG3(a) is a front view of a schematic diagram of a metal porous transport layer and a bipolar plate attached together according to one embodiment of the present invention, and FIG3(b) is a top view of a schematic diagram of a metal porous transport layer and a bipolar plate attached together according to one embodiment of the present invention; FIG4( a ) is a schematic diagram of a metal porous transmission layer structure provided in one embodiment of the present invention, and FIG4( b ) is a partially enlarged schematic diagram of region 41 in FIG4( a ); Figure 5 A schematic diagram of a bipolar plate structure provided by one embodiment of the present invention; FIG6( a ) is a schematic diagram of another metal porous transmission layer structure provided in one embodiment of the present invention, and FIG6( b ) is a partially enlarged schematic diagram of area 61 in FIG6( a ); Figure 7 A schematic diagram of another bipolar plate structure provided by an embodiment of the present invention; FIG8( a ) is a schematic diagram of another metal porous transmission layer structure provided in one embodiment of the present invention, and FIG8( b ) is a partially enlarged schematic diagram of area 81 in FIG8( a ); Figure 9 A schematic diagram of another bipolar plate structure provided by an embodiment of the present invention; Among them, 1-hydrogen inlet; 2-hydrogen outlet; 3-upper end plate; 4-end plate air outlet sealing gasket; 5-upper insulating gasket; 6-upper current collecting plate; 7-bipolar plate; 7-1-cathode side; 7-2-anode side; 8-metal porous transport layer; 8-1-metal porous transport layer upper plating layer; 8-2-metal porous transport layer lower plating layer; 9-membrane electrode; 9-1-membrane electrode cathode; 9-2-membrane electrode anode; 10-bipolar plate sealing line; 10-1-bipolar plate cathode sealing line; 10-2-bipolar plate anode sealing line; 11-lower current collecting plate; 12-lower insulating gasket; 13-lower end plate. DETAILED DESCRIPTION
[0019] To make the objectives, technical solutions, and advantages of the present invention more apparent, the technical solutions of the present invention will be described in detail below. Obviously, the embodiments described are only some of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other implementations obtained by those of ordinary skill in the art without inventive effort are within the scope of protection of the present invention.
[0020] As described in the background technology, increasing the slot width will lead to the following problems: (1) the contact area between the cathode gas diffusion layer (GDL) and the bipolar plate ridge is reduced, and the contact resistance is increased; (2) the GDL carbon fibers are broken due to local pressure overload, affecting the life of the fuel cell stack; (3) the sealing wire may sink into the flow groove, causing the seal to fail and threatening the stability of the fuel cell stack.
[0021] In the existing technology, the flow field design of the bipolar plate is not well matched with the mechanical and electrochemical properties of the gas diffusion layer, which limits the development of high power density of air-cooled fuel cells.
[0022] That is, in the prior art, the anode and cathode sealing grooves of air-cooled fuel cell stacks are asymmetrical. The uneven compression of the anode sealing line by the cathode ridges can cause the membrane electrode frame to bend and deform, leading to anode seal failure. Air-cooled fuel cell stacks have an open cathode structure, and both oxygen supply and heat dissipation require the infiltration of the cathode troughs. To provide good thermal management performance and sufficient reactant gas, the cathode groove width or groove-ridge ratio must be increased. However, a high cathode groove width or groove-ridge ratio can easily cause fracture damage to the cathode diffusion layer carbon fiber layer after stacking, thereby affecting the life of the fuel cell stack. A low groove width or groove-ridge ratio is not conducive to the entry of reactant gas and heat dissipation, which can affect the performance of the membrane electrode.
[0023] Based on this, an embodiment of the present invention provides an air-cooled fuel cell stack to improve the structural stability of the stack.
[0024] Figure 1 This is a schematic structural diagram of an air-cooled fuel cell stack provided by one embodiment of the present invention. Figure 2 A schematic diagram of a metal porous transport layer, a bipolar plate and a membrane electrode structure provided in one embodiment of the present invention; FIG3 (a) is a main view of a metal porous transport layer and a bipolar plate provided in one embodiment of the present invention in a main view and a top view schematic diagram, and FIG3 (b) is a top view of a metal porous transport layer and a bipolar plate provided in one embodiment of the present invention in a main view and a top view schematic diagram.
[0025] See Figure 1 、 Figure 2 3 (a), FIG3 (b), the air-cooled fuel cell stack provided by the embodiment of the present invention may include the following structures: a bipolar plate 7, a membrane electrode 9 and a metal porous transmission layer 8; wherein, The cathode side 7-1 of the bipolar plate 7 is provided with a cathode flow field, and the anode side 7-2 of the bipolar plate 7 is provided with an anode flow field; The membrane electrode 9 includes a membrane electrode cathode side 9-1 and a membrane electrode anode side 9-2, and the membrane electrode cathode side is in contact with the gas diffusion layer; A metal porous transport layer 8, which is arranged between the cathode side 7-1 of the bipolar plate and the cathode side 9-1 of the membrane electrode; one side of the metal porous transport layer is a plane, which is in close contact with the membrane electrode to reduce contact resistance; the other side of the metal porous transport layer is provided with a protruding structure, which is in contact with the cathode flow field ridge of the bipolar plate to disturb the gas flow.
[0026] Specifically, the metal porous transport layer has a flat surface on one side and tiny protrusions similar to fish scales on the other side. The flat surface is in direct contact with the membrane electrode, while the protrusions are in contact with the cathode.
[0027] It is understood that the technical solution provided by this embodiment, by adding a porous metal transport layer between the bipolar plate and the membrane electrode, has a stable structure and is not easily compressed and deformed, thereby ensuring uniform force on the sealing line. This eliminates the risk of the sealing line in traditional structures being trapped in the flow field. The sealing line is evenly compressed, reducing the risk of uneven compression leading to poor sealing and unstable stack structure. In addition, one side of the porous metal transport layer is flat, in close contact with the membrane electrode to reduce contact resistance; the other side is provided with a raised structure, which contacts the cathode flow field ridge of the bipolar plate to disturb the gas flow, enhance the gas dispersion effect, and help improve the overall gas transmission stability.
[0028] See attached Figure 1 、 Figure 2 3(a) and 3(b), the stack consists of, from top to bottom, a hydrogen inlet 1, a hydrogen outlet 2, an upper end plate 3, an end plate gasket 4, an upper insulating gasket 5, an upper current collector 6, a bipolar plate 7, a porous metal transport layer 8, a membrane electrode 9, a lower current collector 11, a lower insulating gasket 12, and a lower end plate 13. The bipolar plate seal lines 10 are located around the gas outlets on both sides of the bipolar plate 7 and around the anode flow field.
[0029] In some embodiments, the metal porous transport layer 8 is embedded in the bipolar plate, the thickness of the metal porous transport layer 8 is equal to the depth of the cathode groove of the bipolar plate, and the length and width of the metal porous transport layer match the cathode groove of the bipolar plate, so that the upper coating 8-1 of the metal porous transport layer is flush with the upper surface of the cathode plate of the bipolar plate.
[0030] For example, the upper and lower surfaces of the metal porous transport layer 8 include a metal porous transport layer upper coating 8-1 and a metal porous transport layer lower coating 8-2. The metal porous transport layer upper coating 8-1 is connected to the cathode of the membrane electrode, and the metal porous transport layer lower coating 8-2 is connected to the cathode flow channel of the bipolar plate and is embedded in the bipolar plate.
[0031] For example, a porous metal transport layer 8 is embedded in the cathode side of the bipolar plate, with the coating on the porous metal transport layer flush with the raised structure on the cathode side of the bipolar plate. The cathode side 9-1 of the membrane electrode is connected to the porous metal transport layer, while the anode side 9-2 of the membrane electrode is connected to the anode side of the bipolar plate. The membrane electrode anode is sealed to prevent air by a bipolar plate anode seal line 10-2 (e.g., a gasket), while the membrane electrode cathode is sealed to prevent hydrogen leakage by a bipolar plate cathode seal line 10-1 (e.g., a gasket).
[0032] Specifically, the porous metal transport layer is embedded within the bipolar plate cathode, with one side aligned with the bipolar plate cathode flow field ridge and the other with the membrane electrode cathode. The thickness H of the porous metal transport layer is equal to the depth h of the bipolar plate cathode groove. The porous metal transport layer's dimensions (a and b) are aligned with the bipolar plate cathode, and the length and width dimensions (A and B) of the porous metal transport layer are equal to the length and width dimensions (A and B) of the bipolar plate step surface. The porous metal transport layer is embedded within the bipolar plate, ensuring that the upper coating 8-1 of the porous metal transport layer is flush with the upper surface of the bipolar plate cathode.
[0033] It can be understood that the embedding and lamination are achieved by embedding the metal porous transport layer into the bipolar plate and arranging the metal porous transport layer to match the grooves of the bipolar plate.
[0034] In some embodiments, the metal porous transmission layer 8 has a porosity of 30% to 85% and a thickness of 0.05 mm to 0.3 mm; The material of the metal porous transmission layer 8 is at least one of titanium, stainless steel, nickel or aluminum, and the surface is plated with carbon, platinum or nickel, and the thickness of the plated layer is 0.05 μm to 0.5 μm.
[0035] It can be understood that such a setting improves the strength of the metal porous transmission layer.
[0036] In some embodiments, the raised structure of the metal porous transport layer 8 is fish-scale, triangular or arc-shaped, and the raised height is less than or equal to 1 / 2 of the thickness of the metal porous transport layer 8, which is used to generate turbulence when the gas flows through and promote the diffusion of gas to the membrane electrode.
[0037] FIG4( a ) is a schematic diagram of a metal porous transmission layer structure provided in one embodiment of the present invention, and FIG4( b ) is a partially enlarged schematic diagram of region 41 in FIG4( a ); Figure 5 FIG6 is a schematic diagram of a bipolar plate structure according to an embodiment of the present invention; FIG6(a) is a schematic diagram of another metal porous transport layer structure according to an embodiment of the present invention; FIG6(b) is a partially enlarged schematic diagram of area 61 in FIG6(a); Figure 7 FIG8( a ) is a schematic diagram of another bipolar plate structure according to an embodiment of the present invention; FIG8( a ) is a schematic diagram of another porous metal transport layer structure according to an embodiment of the present invention; FIG8( b ) is a partially enlarged schematic diagram of region 81 in FIG8( a ); Figure 9 A schematic diagram of another bipolar plate structure provided by an embodiment of the present invention.
[0038] In some embodiments, the pore structure of the metal porous transmission layer 8 is diamond-shaped, circular, or square; When the hole structure is diamond-shaped, the two diagonal dimensions of the diamond-shaped hole are 0.5 mm to 3 mm and 0.3 mm to 1.5 mm respectively, and the long diagonal is perpendicular to the flow channel ridge, and the dimension of the long diagonal is greater than the width of the flow channel ridge; When the hole structure is circular, the diameter of the circular hole is 0.6 mm to 2 mm, and the diameter is larger than the width of the flow channel ridge; When the hole structure is square, the side length of the square hole is 0.5 mm to 2 mm, one side is perpendicular to the flow channel ridge, and the side length is greater than the flow channel ridge width.
[0039] In some embodiments, when the pore structure is diamond-shaped, the protrusion position of the protrusion structure is located on two adjacent sides of the diamond mesh, and the two sides form a triangle with the long diagonal line. The gas flows from the vertical direction of the long diagonal line to the protrusion area of the metal porous transport layer, is blocked by the protrusion, generates turbulence, and accelerates diffusion to the membrane electrode.
[0040] Specifically, the diamond-shaped porous metal transport layer has protrusions located on two adjacent sides of the diamond mesh, forming a triangle with the long diagonal. Gas flows perpendicular to the long diagonal toward the protrusions of the porous metal transport layer, where it is blocked by the protrusions, generating turbulence and accelerating diffusion to the membrane electrode, improving transport capacity. The height of the highest point D of the diamond-shaped porous metal transport layer is less than 1 / 2 of the thickness of the porous metal transport layer. The starting points C and E on both sides of the protrusion gradually increase in height from C to D and gradually decrease from D to E to the plane of the thickness of the porous metal transport layer. This ensures a certain disturbance and dispersion effect on the gas without hindering gas transmission.
[0041] In some embodiments, when the hole structure is square, the protrusion position of the protrusion structure is located on an edge of the square hole perpendicular to the flow channel ridge, and the edge is located on the edge after the gas flows through the square hole. After the gas flows through the square hole, it is blocked by the protrusion, generating turbulence and accelerating diffusion to the membrane electrode.
[0042] Specifically, the metal porous transport layer has a square pore structure, with two sides x and y, where x is 0.5-2mm and y is 0.5-2mm, with y being larger than x. One side y of the square pore is perpendicular to the flow channel ridge, and y is larger than the flow channel ridge width. The metal porous transport layer has a square pore structure, with a protrusion located on one side of the square pore perpendicular to the flow channel ridge. This side is located on side y after the gas flows through the square pore. Two points F and G on the side are equidistant from the plane of the metal porous transport layer. The height of the protrusion is less than 1 / 2 of the thickness of the metal porous transport layer. After the gas flows through the square pore, it is blocked by the protrusion, generating turbulence, which accelerates diffusion to the membrane electrode and improves the transport capacity.
[0043] In some embodiments, when the hole structure is circular, the raised position of the raised structure is located on a semicircle perpendicular to the flow channel ridge. The semicircle is located on the semicircular arc after the gas flows through the circular hole. The line connecting the two points on the edge passes through the center of the circle and is perpendicular to the flow channel ridge.
[0044] Specifically, the circular pore structure of the metal porous transport layer has a radius of r, a size of 0.3-1mm, and the diameter of the circular pore is larger than the width of the flow channel ridge. The circular pore structure of the metal porous transport layer has a convex position located on a semicircle perpendicular to the flow channel ridge. The arc is located on the semicircular arc after the gas flows through the circular hole. The line connecting the two points M and N on the edge passes through the circle and is perpendicular to the flow channel ridge. The highest point O of the convexity is located at the midpoint of the MN arc, and its height is less than 1 / 2 of the thickness of the metal porous transport layer. After the gas flows through the circular hole, it is blocked by the convexity, generating turbulence, which accelerates the diffusion to the membrane electrode and improves the transmission capacity.
[0045] Three different hole shapes are described in detail: Example 1: For example, see Figures 4(a), 4(b) and Figure 5 The porous metal transport layer is embedded in the cathode side of the bipolar plate. The upper coating of the porous metal transport layer is flush with the cathode protrusion structure (eg, boss) of the bipolar plate.
[0046] The metal porous transmission layer is a diamond mesh made of 0.125mm thick titanium mesh punched by a rolling mill, with a porosity of 50%. The surface of the metal porous transmission layer is carbon-plated, and the thickness of the carbon plating is 0.2 μm.
[0047] The cathode flow field of the bipolar plate is a straight-through flow field with a groove depth of 1.5 mm and a groove-ridge ratio of 4.
[0048] Example 2: For example, see Figures 6(a), 6(b) and Figure 7 The porous metal transport layer is embedded in the cathode side of the bipolar plate. The upper coating of the porous metal transport layer is flush with the cathode boss of the bipolar plate.
[0049] The metal porous transmission layer is a titanium fiber felt with a thickness of 0.25 mm and a porosity of 60%. The titanium fiber felt is then punched into a circular mesh through a rolling mill, with a final porosity of 70%.
[0050] The surface of the metal porous transmission layer is carbon-plated, and the thickness of the carbon plating is 0.2 μm.
[0051] The cathode flow field of the bipolar plate is a rod-shaped flow field with a groove depth of 1.5 mm.
[0052] Example 3: For example, see Figures 8(a), 8(b) and Figure 9 The porous metal transport layer is embedded in the cathode side of the bipolar plate. The upper coating of the porous metal transport layer is flush with the cathode boss of the bipolar plate.
[0053] The metal porous transmission layer is 0.2mm thick sintered titanium with a porosity of 50%. The porous sintered titanium is then punched into square meshes through a rolling mill, with a final porosity of 65%.
[0054] The surface of the metal porous transmission layer is carbon-plated, and the thickness of the carbon plating is 0.2 μm.
[0055] The cathode flow field of the bipolar plate is a point flow field with a groove depth of 1.5 mm.
[0056] It is understandable that the stability of the battery stack can be improved by setting the holes in different shapes.
[0057] In some embodiments, The cathode flow field of the bipolar plate has a groove-land ratio of 2:1 to 4:1 and a groove width of 2 mm to 4.5 mm; The cathode flow channel is point-shaped or line-segment-shaped, the ratio of grooves and ridges of adjacent flow field line segments is 1:1-3:1, and the groove width is 1.5mm-4mm.
[0058] In some embodiments, the frame of the membrane electrode 9 contacts the bipolar plate sealing line 10, and the metal porous transmission layer 8 evenly supports the sealing line to prevent it from sinking into the flow channel, thereby ensuring the sealing of the stack.
[0059] In some embodiments, flow grooves are provided on the cathode surface and the anode surface of the bipolar plate, and air inlets and air outlets are provided at both ends of the flow grooves; the membrane electrode is composed of a catalytic layer, a proton exchange membrane and a gas diffusion layer, the catalytic layer is coated on both sides of the proton exchange membrane, and the gas diffusion layer is covered on both sides of the proton exchange membrane coated with the catalytic layer.
[0060] Specifically, the bipolar plates have flow channels on the anode and cathode surfaces, with inlets and outlets at both ends. Sealing grooves are provided around the inlets and outlets on both sides of the bipolar plates and around the anode flow field. The anode of the bipolar plate utilizes a straight flow channel, a wavy flow channel, or a multi-channel serpentine flow channel. The cathode flow channel can be a straight-through flow field with a groove-ridge ratio of 2:1 to 4:1 and a groove width of 2 to 4.5 mm. The cathode flow channel can also be a point-shaped or line-shaped flow field, with a groove-ridge ratio of 1:1 to 3:1 between adjacent flow field segments and a groove width of 1.5 to 4 mm.
[0061] In some embodiments, The metal porous transmission layer 8 is prepared by any of the following methods: The metal sheet is punched by a rolling mill, and the hole area is 0.1mm 2 ~4mm 2 , the hole spacing is 0.2mm~1mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge; The metal fiber is felted and hot pressed and sintered, and then punched by a rolling mill with a hole area of 0.1mm 2 ~2mm 2 , the hole spacing is 0.4mm~3mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge; The metal powder is spread flat in the forming mold, hot pressed and vacuum sintered, and then punched by a rolling mill with a hole area of 0.1mm 2 ~2mm 2 The hole spacing is 0.4mm~3mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge.
[0062] Compared with the prior art, the present invention has the following beneficial effects: 1. The stack has good sealing, high support strength and stable structure. In the traditional air-cooled fuel cell stack structure, the sealing line is easily squeezed and pressed into the cathode flow channel, resulting in a risk of leakage at the channel position; a metal porous transmission layer is added between the bipolar plate and the membrane electrode. The metal porous transmission layer acts as a reinforcement layer, and its structure is stable and not easily compressed and deformed; the sealing line is subjected to uniform force at all locations, solving the risk of the sealing line of the traditional structure falling into the flow field, and the sealing line will be evenly compressed, reducing the uneven compression that results in poor sealing effect and unstable fuel cell structure.
[0063] 2. Good contact, uniform compression of the diffusion layer, good drainage and good stability.
[0064] In the traditional structure, the membrane electrode and the bipolar plate are in direct contact. The gas diffusion layer will be squeezed by the cathode ridge of the bipolar plate, causing the carbon fibers to break, resulting in an unstable membrane electrode structure and affecting stability. The metal porous transmission layer has strong rigidity and fits perfectly with the gas diffusion layer, dispersing the squeezing force of the flow channel ridge on the diffusion layer, ensuring that the force at each position of the diffusion layer is relatively uniform, and each part of the diffusion layer is evenly compressed, thus solving the problems of uneven pressure on the carbon paper of the diffusion layer in the existing structure, insufficient water vapor channels at the flow field ridge position, high contact resistance, and stress damage of the carbon fibers. In addition, the presence of the metal porous transmission layer can make the force uniform across the gas diffusion layer, the diffusion layer is evenly compressed, and the pore structure of the diffusion layer is evenly distributed, which is conducive to the transmission of water vapor and can ensure that the water generated by the reaction has enough space to discharge.
[0065] 3. The cathode flow channel structure has a large adjustable space, good water and heat management, and high fuel cell performance.
[0066] The sealed structure of traditional air-cooled fuel cell stacks limits the anode hydrogen pressure to a relatively low level, typically between 0.04 and 0.06 MPa. This is because uneven compression between the cathode ridges and the sealing line affects the seal, and excessively high pressure exacerbates leakage. However, low pressure hinders gas diffusion, so the anode flow field typically uses a simple flow process, such as a DC field, and the single electrode area is limited. The high strength of the metal porous transport layer provides uniform support for the sealing line, improves the sealing effect, and can increase the anode hydrogen pressure to 0.1MPa or even higher without causing sealing problems in the stack. It also provides a wide space for the cathode flow field design. Generally, the cathode flow channel width is 1-2.5mm. A flow channel that is too wide can easily cause the membrane electrode to bend due to insufficient rigidity, resulting in increased contact resistance, seriously affecting performance and stability. The metal porous transport layer has high rigidity and is not easy to bend and deform. It can ensure that the membrane electrode is evenly compressed and does not bend and deform, and the restriction on the cathode flow field channel width can be relaxed. The cathode flow channel width can be increased to 4.5mm, the groove-ridge ratio can be increased, and the air flow rate can be increased to meet the demand for reaction oxygen and the control of stack temperature under high electrical density conditions, and give full play to the positive impact of cathode structure optimization on performance.
[0067] The above description is merely a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any modifications or substitutions that can be easily conceived by a person skilled in the art within the technical scope disclosed in the present invention should be included within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be based on the scope of protection of the claims.
[0068] It can be understood that the same or similar parts of the above embodiments can be referenced to each other, and the contents not described in detail in some embodiments can refer to the same or similar contents in other embodiments.
[0069] It should be noted that, in the description of the present invention, the terms "first", "second", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance. In addition, in the description of the present invention, unless otherwise specified, the meaning of "plurality" is at least two.
[0070] Any process or method description in a flowchart or otherwise described herein may be understood to represent a module, segment or portion of code comprising one or more executable instructions for implementing the steps of a specific logical function or process, and the scope of the preferred embodiments of the present invention includes alternative implementations in which functions may be performed out of the order shown or discussed, including performing functions in a substantially simultaneous manner or in the reverse order depending on the functions involved, which should be understood by those skilled in the art to which the embodiments of the present invention pertain.
[0071] It should be understood that various components of the present invention may be implemented using hardware, software, firmware, or a combination thereof. In the above-described embodiments, multiple steps or methods may be implemented using software or firmware stored in a memory and executed by a suitable instruction execution system. For example, if implemented using hardware, as in another embodiment, any one of the following technologies known in the art or a combination thereof may be used: a discrete logic circuit having logic gate circuits for implementing logic functions on data signals, an application-specific integrated circuit having suitable combinational logic gate circuits, a programmable gate array (PGA), a field-programmable gate array (FPGA), etc.
[0072] Those skilled in the art will understand that all or part of the steps in the method of the above embodiment can be completed by instructing related hardware through a program, and the program can be stored in a computer-readable storage medium. When the program is executed, it includes one or a combination of the steps of the method embodiment.
[0073] In addition, the functional units in the various embodiments of the present invention may be integrated into a single processing module, or each unit may exist physically separately, or two or more units may be integrated into a single module. The aforementioned integrated modules may be implemented in the form of hardware or in the form of software functional modules. If the integrated modules are implemented in the form of software functional modules and sold or used as independent products, they may also be stored in a computer-readable storage medium.
[0074] The storage medium mentioned above can be a read-only memory, a magnetic disk or an optical disk, etc.
[0075] Throughout this specification, reference to terms such as "one embodiment," "some embodiments," "examples," "specific examples," or "some examples" means that a specific feature, structure, material, or characteristic described in conjunction with that embodiment or example is included in at least one embodiment or example of the present invention. In this specification, schematic representations of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in any one or more embodiments or examples.
[0076] Although the embodiments of the present invention have been shown and described above, it will be understood that the above embodiments are illustrative and are not to be construed as limitations on the present invention. A person skilled in the art may change, modify, replace and modify the above embodiments within the scope of the present invention.
Claims
1. An air-cooled fuel cell stack, characterized in that: include: Bipolar plate (7), membrane electrode (9) and metal porous transport layer (8); wherein, The cathode side (7-1) of the bipolar plate (7) is provided with a cathode flow field, and the anode side (7-2) of the bipolar plate (7) is provided with an anode flow field; The membrane electrode (9) comprises a membrane electrode cathode side (9-1) and a membrane electrode anode side (9-2), and both the anode and cathode sides of the membrane electrode have gas diffusion layers; A metal porous transport layer (8), the metal porous transport layer is arranged between the cathode side (7-1) of the bipolar plate and the cathode side (9-1) of the membrane electrode; one side of the metal porous transport layer is a plane, the plane is in close contact with the membrane electrode to reduce contact resistance; the other side of the metal porous transport layer is provided with a protrusion structure, the protrusion structure is in contact with the cathode flow field ridge of the bipolar plate to disturb gas flow.
2. The air-cooled fuel cell stack according to claim 1, characterized in that: The metal porous transport layer (8) is embedded in the bipolar plate, the thickness of the metal porous transport layer (8) is equal to the depth of the cathode groove of the bipolar plate, and the length and width of the metal porous transport layer match the cathode groove of the bipolar plate, so that the upper coating (8-1) of the metal porous transport layer is flush with the upper surface of the cathode plate of the bipolar plate.
3. The air-cooled fuel cell stack according to claim 1, characterized in that: The metal porous transmission layer (8) has a porosity of 30% to 85% and a thickness of 0.05 mm to 0.3 mm; The material of the metal porous transmission layer (8) is at least one of titanium, stainless steel, nickel or aluminum, and the surface is plated, the plated material is carbon, platinum or nickel, and the thickness of the plated layer is 0.05 μm to 0.5 μm.
4. The air-cooled fuel cell stack according to any one of claims 1 to 3, characterized in that: The protrusion structure of the metal porous transmission layer (8) is fish-scale-shaped, triangular-shaped or arc-shaped, and the protrusion height is less than or equal to 1 / 2 of the thickness of the metal porous transmission layer (8), and is used to generate turbulence when the gas flows through, thereby promoting the diffusion of the gas to the membrane electrode.
5. The air-cooled fuel cell stack according to any one of claims 1 to 3, characterized in that: The pore structure of the metal porous transmission layer (8) is diamond-shaped, circular or square; When the hole structure is diamond-shaped, the two diagonal dimensions of the diamond-shaped hole are 0.5 mm to 3 mm and 0.3 mm to 1.5 mm respectively, and the long diagonal is perpendicular to the flow channel ridge, and the dimension of the long diagonal is greater than the width of the flow channel ridge; When the hole structure is circular, the diameter of the circular hole is 0.6 mm to 2 mm, and the diameter is larger than the width of the flow channel ridge; When the hole structure is square, the side length of the square hole is 0.5 mm to 2 mm, one side is perpendicular to the flow channel ridge, and the side length is greater than the flow channel ridge width.
6. The air-cooled fuel cell stack according to claim 5, characterized in that: When the pore structure is rhombus-shaped, the protrusions of the protrusion structure are located on two adjacent sides of the rhombus mesh, and the two sides form a triangle with the long diagonal line. The gas flows from the vertical direction of the long diagonal line to the protrusion area of the metal porous transport layer, and is blocked by the protrusion, generating turbulence, thereby accelerating diffusion to the membrane electrode; When the hole structure is square, the protrusion of the protrusion structure is located on an edge of the square hole perpendicular to the flow channel ridge, and the edge is located on the edge after the gas flows through the square hole. After the gas flows through the square hole, it is blocked by the protrusion, generating turbulence and accelerating diffusion to the membrane electrode; When the hole structure is circular, the convex position of the convex structure is located on a semicircle perpendicular to the flow channel ridge. The semicircle is located on the semicircular arc after the gas flows through the circular hole. The line connecting the two points on the edge passes through the center of the circle and is perpendicular to the flow channel ridge.
7. The air-cooled fuel cell stack according to claim 1, characterized in that: The cathode flow field of the bipolar plate has a groove-land ratio of 2:1 to 4:1 and a groove width of 2 mm to 4.5 mm; The flow grooves of the cathode flow field are point-shaped or line-segment-shaped, the groove-ridge ratio of adjacent flow field line segments is 1:1~3:1, and the groove width is 1.5mm~4mm.
8. The air-cooled fuel cell stack according to claim 1, characterized in that: The frame of the membrane electrode (9) contacts the bipolar plate sealing line (10), and the metal porous transmission layer (8) evenly supports the sealing line to prevent it from sinking into the cathode flow channel, thereby ensuring the sealing of the stack.
9. The air-cooled fuel cell stack according to claim 1, characterized in that: The cathode surface and the anode surface of the bipolar plate are both provided with flow grooves, and an air inlet and an air outlet are provided at both ends of the flow groove; the membrane electrode is composed of a catalytic layer, a proton exchange membrane and a gas diffusion layer, the catalytic layer is coated on both sides of the proton exchange membrane, and the gas diffusion layer is covered on both sides of the proton exchange membrane coated with the catalytic layer.
10. The air-cooled fuel cell stack according to claim 1, characterized in that: The metal porous transmission layer (8) is prepared by any of the following methods: The metal sheet is punched by a rolling mill, and the hole area is 0.1mm 2 ~4mm 2 , the hole spacing is 0.2mm~1mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge; The metal fiber is felted and hot pressed and sintered, and then punched by a rolling mill with a hole area of 0.1mm 2 ~2mm 2 , the hole spacing is 0.4mm~3mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge; The metal powder is spread flat in the forming mold, hot pressed and vacuum sintered, and then punched by a rolling mill with a hole area of 0.1mm 2 ~2mm 2 The hole spacing is 0.4mm~3mm, and the minimum diagonal dimension of the hole is larger than the width of the cathode flow channel ridge.
Citation Information
Patent Citations
Membrane electrode with low internal resistance and fuel cell including membrane electrode
CN109449455A
Fuel cell electrode plate, bipolar plate, and hydrogen fuel cell
CN110474065A
Air-cooled fuel cell stack and metal bipolar plate thereof
CN114583204A
Reactor core of air-cooled fuel cell stack, stack and thermal management design method thereof
CN120221698A
Fuel battery
JP2017084737A