High-strength aluminum alloy sheet metal part hot forming parameter automatic control framework and method

By using an automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts, and by optimizing forming parameters using sensors and multi-physical quantity models, the problem of rigid parameters in hot forming equipment has been solved. This has enabled high-quality and efficient multi-variety, small-batch production, while reducing energy consumption and equipment wear.

CN121467533AActive Publication Date: 2026-02-06DALIAN UNIV OF TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202610024913.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-01-09
Publication Date
2026-02-06
Estimated Expiration
2046-01-09

AI Technical Summary

Technical Problem

The existing high-strength aluminum alloy sheet metal hot forming equipment has rigid parameter settings, making it difficult to respond to temperature fluctuations and environmental changes in real time, resulting in forming defects such as cracking and local thinning.

Method used

An automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts is adopted, including a hot stamping forming device and a control system based on a multi-physical quantity model. The system monitors temperature and pressure in real time through sensors, dynamically adjusts parameters such as forming speed and clamping force, and optimizes them by combining the constitutive model, forming limit model and TTT model of the alloy.

Benefits of technology

It enables automated forming of workpieces of different types and geometries, improving forming quality and yield, reducing energy waste, and extending equipment life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121467533A_ABST
    Figure CN121467533A_ABST
Patent Text Reader

Abstract

The invention discloses an automatic control framework and method for hot forming parameters of a high-strength aluminum alloy sheet metal part, and relates to the technical field of sheet metal forming, and the automatic control framework comprises a hot stamping forming device and a control system based on a multi-physical-quantity model; the hot stamping forming device comprises a hot stamping press, a hot stamping die arranged in the hot stamping press, a sensor unit arranged on the hot stamping die and a temperature control element arranged on the hot stamping die. The control system comprises a built-in model, and the built-in model comprises a constitutive model of the alloy, a forming limit model of the alloy and a TTT model of the alloy; the control system receives information acquired by the sensor unit and performs data analysis; according to the automatic control framework and method for the hot forming parameters of the high-strength aluminum alloy sheet metal part, the problem that in the prior art, parameter setting of a hot forming device is rigid is solved.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The application relates to the sheet metal forming technical field, in particular to a high-strength aluminum alloy sheet metal part hot forming parameter automatic control architecture and method. BACKGROUND

[0002] In recent years, metal thin-walled components with large-scale, long-life, high-performance and high-reliability are increasingly used in new-generation aerospace vehicles and ships and other cutting-edge equipment, and the ability to manufacture precise light thin-walled parts is one of the core technologies for the development of high-end transportation equipment such as aerospace. Based on the characteristics of lightweight, large-scale, long-life, high-performance and high-reliability of components, it is necessary to use as many integral structural parts as possible. High-strength aluminum alloy sheet metal part non-isothermal hot forming is an important way of forming integral structural parts.

[0003] However, the existing high-strength aluminum alloy sheet metal part hot forming device mainly relies on preset constant parameters or simple empirical adjustment, and it is difficult to respond to temperature fluctuations in real time. However, during the forming process, due to the non-constant external environment, such as temperature difference at different times and regions in the workshop, different air circulation conditions and the like, these environmental factors will make it difficult to unify the temperature of the blank during forming. Moreover, it is also difficult to ensure that the time of the blank from one processing link to the hot forming device is completely consistent, which will also cause the temperature of the blank to be different when entering the hot forming. When running according to fixed forming pressure and speed parameters, if the actual temperature of the blank is lower than the target value, the material plasticity is insufficient and cracking is easily caused; if the temperature is too high, the local excessive thinning or rebound exceeding the standard may be caused due to the excessively low deformation resistance. Although some existing systems attempt to preliminarily monitor the temperature through infrared temperature measurement, there is a lack of deep coupling with the forming parameters, and the parameter adjustment still relies on manual experience, which has problems such as response lag and insufficient compensation accuracy, and it is difficult to fundamentally solve the forming defects caused by uneven temperature. SUMMARY

[0004] The purpose of the present application is to provide a high-strength aluminum alloy sheet metal part hot forming parameter automatic control architecture and method, which solves the problem of rigid parameter setting of the existing hot forming device.

[0005] To achieve the above-mentioned purpose, the present application provides a high-strength aluminum alloy sheet metal part hot forming parameter automatic control architecture, which comprises a hot stamping forming device and a control system based on a multi-physical quantity model. The hot stamping forming device comprises a hot stamping press, a hot stamping die arranged in the hot stamping press, a sensor unit arranged on the hot stamping die and a temperature control element arranged on the hot stamping die. The control system comprises an embedded model, which comprises a constitutive model of the alloy, a forming limit model of the alloy and a TTT model of the alloy; the control system receives information collected by the sensor unit and performs data analysis.

[0006] Preferably, the hot stamping press comprises a slide, and the hot stamping die is arranged below the slide; The hot stamping die comprises an upper die, a lower die, a blank holder and a blank; the upper die is arranged above the lower die, the blank is arranged between the upper die and the lower die, and the blank holder is arranged on the outer circumferential side of the upper die and cooperates with the lower die to press the blank; the upper die comprises a first forming surface, the first forming surface is arranged at the lower end of the upper die and protrudes downward, the lower die comprises a second forming surface, the second forming surface is arranged at the upper end of the lower die and is recessed downward, and the first forming surface and the second forming surface are appropriately sized; The sensor unit comprises a temperature sensor, a first pressure sensor and a second pressure sensor; the temperature sensor and the first pressure sensor are both arranged at the bottom of the first forming surface, and the second pressure sensor is arranged at the bottom of the second forming surface; the temperature sensor is used to measure the temperature of the blank in real time; the first pressure sensor is used to determine the time when the blank enters the forming stage and simultaneously collect the information of the closing pressure of the hot stamping die during the quenching process; and the second pressure sensor is used to determine the time when the blank ends the forming stage and starts the quenching; The temperature control elements are arranged at equal intervals on the first forming surface and the second forming surface.

[0007] Preferably, the sensor unit transmits the collected temperature and pressure information to the control system, and the control system adjusts the parameters of the hot stamping forming device according to the information collected by the sensor unit to ensure the forming quality and mechanical properties of the workpiece.

[0008] Preferably, the range of the temperature sensor includes the solution treatment temperature and the first aging temperature of the aluminum alloy; if a contact temperature sensor is used, a platinum resistance temperature sensor or a thermocouple sensor is preferred; and if a non-contact temperature sensor is used, a thin-film optical temperature sensor is preferred. The range of the first pressure sensor and the second pressure sensor includes the closing force range of the hot stamping die, and the first pressure sensor and the second pressure sensor are preferably piezoelectric sensors.

[0009] The application also provides a method for automatically controlling the parameters of a high-strength aluminum alloy sheet metal part hot forming architecture, which comprises the following steps: Step 1, system initialization; Step 2, first stage data acquisition and analysis; Step 3, calculation of forming speed; Step 4, second stage data acquisition and analysis; Step 5, calculation of closing force; Step 6, quenching: the control system feeds back the closing force to the hot stamping press, and the hot stamping press performs in-die quenching on the blank; Step 7, when the temperature of the blank decreases to the temperature of the die At that time, the mold is opened and samples are taken; the mold temperature is the first aging temperature.

[0010] Preferably, in step 1: initial information is input into the control system, including the maximum strain of the billet deformation. Strain path and billet material; the maximum strain of billet deformation is determined by the target geometry; maximum strain Obtained through finite element simulation or empirical formulas.

[0011] Preferably, in step 2: when the upper die contacts the billet and triggers the first pressure sensor, the temperature sensor simultaneously collects the billet temperature in the first stage. ,Will Input control system, through and Obtain the strain rate ; The strain rate was determined by the following method: For the billet at the target temperature, the upper limit of strain rate is calculated using the built-in forming limit model. ,in This is the maximum strain rate corresponding to the FLD safety zone, i.e., the critical value that does not trigger necking; A safety margin of ≥10%~15% is typically required to avoid fracture caused by edge effects; a strain rate with a safety margin of not less than 15% is selected for the FLD (Fluorescent Diode); the formula for calculating the safety margin is: ; In the formula, This represents the critical strain under the corresponding strain rate conditions.

[0012] Preferably, in step 3: the control system obtains the forming time through the strain rate and the maximum strain. Through forming time and the maximum depth of the part Obtain forming speed The control system will control the forming speed. The output is given to the hot stamping forming device; the calculation expressions are as follows: ; .

[0013] Preferably, in step 4: when the billet contacts the lower die and triggers the second pressure sensor, the temperature sensor simultaneously collects the second stage temperature of the billet. ,Will The input is processed by the control system, which obtains the results through the built-in TTT model. Critical cooling rate ,in Mold temperature; The critical cooling rate is tangent to the nose point of the TTT model curve, and is determined by the following method: Let the coordinates of the nose tip point of the TTT model be... ,in Temperature of the tip of the nose. The shortest phase transition time from the start of cooling to the nose tip temperature; when the cooling curve satisfies the condition that the temperature drops to... At that time, the time taken was exactly equal to If the cooling curve is tangent to the phase transition initiation curve at the nose tip on the TTT model, then the cooling rate... .

[0014] Preferably, in step 5: the relationship between cooling rate and mold closing pressure is obtained experimentally; different pressures are selected for quenching the material, the cooling rate is measured, and a pressure-cooling rate curve is plotted by fitting the formula; the relationship between cooling rate and mold closing pressure is then analyzed. The relationship is used to obtain the required mold closing pressure. The clamping force is calculated from the clamping pressure, and the expression is: ; In the formula, This represents the contact area between the blank and the mold.

[0015] Therefore, the present invention, employing the above-mentioned automatic control architecture and method for hot forming parameters of high-strength aluminum alloy sheet metal parts, has the following beneficial effects: (1) Strong adaptability: No need to rely on fixed parameters. After initial input of information such as part strain and material, the system can automatically adapt to the forming requirements of different types of high-strength aluminum alloys and workpieces with different geometric shapes, and meet the needs of multi-variety and small-batch production. (2) High quality and yield: The blank temperature and mold closing pressure are monitored in real time by sensors, and the forming speed, mold closing force and other parameters are dynamically adjusted by combining multi-physical quantity models to avoid defects such as cracking and excessive thinning caused by temperature fluctuations, thereby improving the forming quality and yield of parts. (3) Low energy consumption and equipment wear: Dynamically adjust process parameters to avoid redundant energy consumption and excessive equipment load caused by fixed parameters. While ensuring quality, reduce energy waste and extend equipment service life.

[0016] The technical solution of the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description

[0017] Figure 1 This is a schematic diagram of the automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts according to the present invention. Figure 2 This is a partial structural schematic diagram of an embodiment of the present invention; Figure 3This is an overall flowchart of a method for an automatic control architecture of hot forming parameters for high-strength aluminum alloy sheet metal parts according to the present invention. Figure 4 This is the hot forming process of high-strength aluminum alloy sheet metal parts according to an embodiment of the present invention; Figure 5 This is a curve showing the relationship between the mold clamping pressure and cooling rate of the high-strength aluminum alloy according to an embodiment of the present invention; Figure 6 This is a schematic diagram illustrating the relationship between molding temperature and time in an embodiment of the present invention.

[0018] Figure Labels 1. Hot stamping press; 11. Slider; 2. Hot stamping die; 21. Upper die; 22. Lower die; 23. Blanking ring; 24. Blank; 25. First forming surface; 26. Second forming surface; 3. Temperature sensor; 4. First pressure sensor; 5. Second pressure sensor; 6. Temperature control element; 7. Control system. Detailed Implementation

[0019] The following detailed description of embodiments of the invention provided in the accompanying drawings is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention. All other embodiments obtained by those skilled in the art based on the embodiments of the invention without inventive effort are within the scope of protection of the invention.

[0020] Please see Figures 1-2 An automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts, including a hot stamping forming device and a control system based on a multi-physical quantity model 7. The hot stamping forming apparatus includes a hot stamping press 1, a hot stamping die 2 disposed in the hot stamping press 1, a sensor unit disposed on the hot stamping die 2, and a temperature control element 6 disposed on the hot stamping die 2; Hot stamping press 1 includes a slide block 11, and hot stamping die 2 is disposed below the slide block 11; The hot stamping die 2 includes an upper die 21, a lower die 22, a blank holder 23, and a blank 24. The upper die 21 is positioned above the lower die 22, and the blank 24 is positioned between the upper die 21 and the lower die 22. The blank holder 23 is positioned on the outer periphery of the upper die 21 and cooperates with the lower die 22 to press the blank 24. The upper die 21 includes a first forming surface 25, which is positioned at the lower end of the upper die 21 and protrudes downward. The lower die 22 includes a second forming surface 26, which is positioned at the upper end of the lower die 22 and is recessed downward. The first forming surface 25 and the second forming surface 26 are adapted to each other in size. The sensor unit includes a temperature sensor 3, a first pressure sensor 4, and a second pressure sensor 5. The temperature sensor 3 and the first pressure sensor 4 are both located at the bottom of the first forming surface 25, and the second pressure sensor 5 is located at the bottom of the second forming surface 26. The temperature sensor 3 is used to measure the temperature of the blank 24 in real time. The first pressure sensor 4 is used to determine the time when the blank 24 enters the forming stage, and at the same time collects the mold closing pressure information of the hot stamping die 2 during the quenching process. The second pressure sensor 5 is used to determine the time when the blank 24 ends the forming stage and begins quenching. Temperature control elements 6 are equally spaced on the first forming surface 25 and the second forming surface 26; The control system 7 includes a built-in model, which includes the constitutive model of the alloy, the forming limit model of the alloy, and the TTT model of the alloy; the control system 7 receives information collected by the sensor unit and performs data analysis. The sensor unit transmits the collected temperature and pressure information to the control system 7. The control system 7 adjusts the parameters of the hot stamping forming device according to the information collected by the sensor unit to ensure the forming quality and mechanical properties of the workpiece. The temperature sensor 3 has a range that includes the solution treatment temperature and the first aging temperature of the aluminum alloy. If a contact temperature sensor 3 is used, a platinum resistance temperature sensor 3 or a thermocouple sensor is preferred. If a non-contact temperature sensor 3 is used, a thin-film optical temperature sensor 3 is preferred. The measuring range of the first pressure sensor 4 and the second pressure sensor 5 includes the clamping force range of the hot stamping die 2, and the first pressure sensor 4 and the second pressure sensor 5 are preferably piezoelectric sensors.

[0021] Please see Figures 3-4 A method for automatically controlling the hot forming parameters of high-strength aluminum alloy sheet metal parts includes the following steps: Step 1, System Initialization: Input initial information into control system 7, including the maximum strain of billet 24 deformation. Strain path and billet 24 material; the maximum strain of billet 24 deformation is determined by the target geometry; maximum strain Obtained through finite element simulation or empirical formulas; Step 2, First Stage Data Collection and Analysis: When the upper mold 21 contacts the billet 24 and triggers the first pressure sensor 4, the temperature sensor 3 simultaneously collects the temperature of the billet 24 in the first stage. ,Will Input control system 7, through and Obtain the strain rate ; The strain rate was determined by the following method: For the billet 24 at the target temperature, the upper limit of strain rate is calculated using the built-in forming limit model. ,in This is the maximum strain rate corresponding to the FLD safety zone, i.e., the critical value that does not trigger necking; A safety margin of ≥10%~15% is typically required to avoid fracture caused by edge effects; a strain rate with a safety margin of not less than 15% is selected for the FLD (Fluorescent Diode); the formula for calculating the safety margin is: ; In the formula, The critical strain under the corresponding strain rate condition; Step 3: Calculate the forming speed; Control system 7 obtains the forming time through strain rate and maximum strain. Through forming time and the maximum depth of the part Obtain forming speed The control system 7 will control the forming speed The output is given to the hot stamping forming device; the calculation expressions are as follows: ; ; Step 4: Second stage data collection and analysis; When the billet 24 contacts the lower die 22, triggering the second pressure sensor 5, the temperature sensor 3 simultaneously collects the second-stage temperature of the billet 24. ,Will Input to control system 7, which obtains the result through the built-in TTT model. Critical cooling rate ,in Mold temperature; The critical cooling rate is tangent to the nose point of the TTT model curve, and is determined by the following method: Let the coordinates of the nose tip point of the TTT model be... ,in Temperature of the tip of the nose. The shortest phase transition time from the start of cooling to the nose tip temperature; when the cooling curve satisfies the condition that the temperature drops to... At that time, the time taken was exactly equal to The cooling curve on the TTT model is tangent to the phase transition initiation curve at the nose tip. Please refer to [link / reference]. Figure 6 Then the cooling rate ; Step 5: Calculate the clamping force; The relationship between cooling rate and mold closing pressure was obtained experimentally. Different pressures were selected for material quenching, and the cooling rate was measured. The pressure-cooling rate curve was plotted by fitting the formula. (See also...) Figure 5 By cooling rate and mold closing pressure The relationship is used to obtain the required mold closing pressure. The clamping force is calculated from the clamping pressure, and the expression is: ; In the formula, This represents the contact area between the blank 24 and the mold; Step 6, Quenching: The control system 7 feeds back the clamping force to the hot stamping press 1, and the hot stamping press 1 performs in-mold quenching on the blank 24; Step 7: When the slab temperature drops to the mold temperature At that time, the mold is opened and samples are taken; the mold temperature is the first aging temperature.

[0022] Therefore, this invention adopts the above-mentioned automatic control architecture and method for hot forming parameters of high-strength aluminum alloy sheet metal parts. By using sensors to monitor the blank temperature and mold closing pressure in real time, and combining a multi-physical quantity model to dynamically adjust parameters such as forming speed and mold closing force, it avoids defects such as cracking and excessive thinning caused by temperature fluctuations, thereby improving the forming quality and yield of parts. It does not rely on fixed parameters. After initial input of information such as part strain and material, the system can automatically adapt to the forming requirements of different types of high-strength aluminum alloys and workpieces with different geometric shapes, meeting the needs of multi-variety, small-batch production. Dynamically adjusting process parameters avoids redundant energy consumption and excessive equipment load caused by fixed parameters, thereby reducing energy waste and extending equipment service life while ensuring quality.

[0023] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and not to limit them. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can still be made to the technical solutions of the present invention, and these modifications or equivalent substitutions cannot cause the modified technical solutions to deviate from the spirit and scope of the technical solutions of the present invention.

Claims

1. An automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts, characterized in that: This includes a hot stamping forming device and a control system based on a multi-physical model; The hot stamping forming apparatus includes a hot stamping press, a hot stamping die disposed in the hot stamping press, a sensor unit disposed on the hot stamping die, and a temperature control element disposed on the hot stamping die; The control system includes a built-in model, which includes the constitutive model of the alloy, the forming limit model of the alloy, and the TTT model of the alloy; the control system receives information collected by the sensor unit and performs data analysis.

2. The automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 1, characterized in that: Hot stamping press includes a slide block, and hot stamping die is located below the slide block; The hot stamping die includes an upper die, a lower die, a blank holder, and a blank. The upper die is positioned above the lower die, and the blank is placed between the upper and lower dies. The blank holder is positioned on the outer periphery of the upper die and cooperates with the lower die to clamp the blank. The upper die includes a first forming surface, which is located at the lower end of the upper die and protrudes downward. The lower die includes a second forming surface, which is located at the upper end of the lower die and is recessed downward. The sizes of the first forming surface and the second forming surface are matched. The sensor unit includes a temperature sensor, a first pressure sensor, and a second pressure sensor; both the temperature sensor and the first pressure sensor are located at the bottom of the first forming surface, and the second pressure sensor is located at the bottom of the second forming surface; the temperature sensor is used to measure the temperature of the billet in real time; the first pressure sensor is used to determine the time when the billet enters the forming stage, and at the same time collects the mold closing pressure information of the hot stamping die during the quenching process; the second pressure sensor is used to determine the time when the billet ends the forming stage and begins quenching. Temperature control elements are evenly spaced on the first forming surface and the second forming surface.

3. The automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 2, characterized in that: The sensor unit transmits the collected information to the control system, which then adjusts the parameters of the hot stamping forming device based on the information collected by the sensor unit.

4. The automatic control architecture for hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 3, characterized in that: The temperature sensor's range includes the solution treatment temperature and the first aging temperature of the aluminum alloy. The measuring ranges of the first and second pressure sensors include the clamping force range of hot stamping dies.

5. A method for an automatic control architecture of hot forming parameters for high-strength aluminum alloy sheet metal parts as described in any one of claims 1-4, characterized in that, Includes the following steps: Step 1: System initialization; Step 2: First-stage data collection and analysis; Step 3: Calculate the forming speed; Step 4: Second stage data collection and analysis; Step 5: Calculate the clamping force; Step 6, Quenching: The control system feeds back the clamping force to the hot stamping press, which performs in-mold quenching on the blank. Step 7: When the slab temperature drops to the mold temperature At that time, the mold is opened and samples are taken; the mold temperature is the first aging temperature.

6. The method for automatic control architecture of hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 5, characterized in that, In step 1: Initial information is input into the control system, including the maximum strain of the billet deformation. Strain path and billet material; The maximum strain of the billet deformation is determined by the target geometry; maximum strain Obtained through finite element simulation or empirical formulas.

7. The method for automatic control architecture of hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 6, characterized in that, In step 2: When the upper die contacts the billet and triggers the first pressure sensor, the temperature sensor simultaneously collects the billet temperature in the first stage. ,Will Input control system, through and Obtain the strain rate ; The strain rate was determined by the following method: For the billet at the target temperature, the upper limit of strain rate is calculated using the built-in forming limit model. ,in The maximum strain rate in the FLD safety zone; Select a strain rate with a safety margin of not less than 15% for the FLD; the formula for calculating the safety margin is: ; In the formula, This represents the critical strain under the corresponding strain rate conditions.

8. The method for automatic control architecture of hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 7, characterized in that, In step 3: the control system obtains the forming time through strain rate and maximum strain. Through forming time and the maximum depth of the part Obtain forming speed The control system will control the forming speed. The output is given to the hot stamping forming device; the calculation expressions are as follows: ; 。 9. The method for automatic control architecture of hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 8, characterized in that, In step 4: When the billet contacts the lower die and triggers the second pressure sensor, the temperature sensor simultaneously collects the billet's second-stage temperature. ,Will The input is processed by the control system, which obtains the results through the built-in TTT model. Critical cooling rate ,in Mold temperature; The critical cooling rate is tangent to the nose point of the TTT model curve, and is determined by the following method: Let the coordinates of the nose tip point of the TTT model be... ,in Temperature of the tip of the nose. The shortest phase transition time from the start of cooling to the nose tip temperature; when the cooling curve satisfies the condition that the temperature drops to... When, the time taken is equal to If the cooling curve is tangent to the phase transition initiation curve at the nose tip on the TTT model, then the cooling rate... .

10. The method for automatic control architecture of hot forming parameters of high-strength aluminum alloy sheet metal parts according to claim 9, characterized in that, In step 5: the cooling rate and the mold closing pressure are controlled. The relationship is used to obtain the mold closing pressure. The clamping force is calculated from the clamping pressure, and the expression is: ; In the formula, This represents the contact area between the blank and the mold.

Citation Information

Patent Citations

  • Hot stamping forming method of lightweight aluminum alloy vehicle body component

    CN108380722A

  • Hot forming method and device for large-size high-strength aluminum alloy aviation thin-wall part

    CN114318182A

  • Aluminum alloy sheet metal part hot forming production line based on multiple sensors and control method

    CN117463857A

  • Method for press-working aluminum alloy sheet, and aluminum alloy sheet

    JP2003117614A

  • Hot-stamping forming method for lightweight aluminum alloy vehicle body component

    WO2019205768A1