Limestone-gypsum wet desulphurization method and system

By using rich liquor heating and flash desorption treatment in the limestone-gypsum wet desulfurization process, combined with the use of surfactants and antioxidants, the problems of unstable gypsum quality and scarce sulfur resources have been solved, realizing the efficient resource utilization of gypsum and the recovery of sulfur resources, and reducing desulfurization costs.

CN121668703APending Publication Date: 2026-03-17GD POWER DEVELOPMENT CO LTD +4
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202511754580.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-11-26
Publication Date
2026-03-17

AI Technical Summary

Technical Problem

In existing limestone-gypsum wet desulfurization technology, the quality of gypsum is unstable and the utilization rate is low, resulting in a large amount of gypsum being wasted. In addition, sulfur resources are scarce, causing pollution to the ecological environment and land resources. At the same time, sulfur resources need to be imported in large quantities.

Method used

The limestone-gypsum wet desulfurization process utilizes a rich liquid heater and a flash desorber for heating and desorption treatment, resulting in flash desorbed vapor which is then purified to obtain desorbed sulfur dioxide gas. Simultaneously, a portion of the desulfurization lean slurry undergoes oxidation treatment to obtain gypsum products. Surfactants and antioxidants are added to the desulfurization absorption tower to enhance the treatment effect.

Benefits of technology

This enables the resource-based recycling and utilization of sulfur, reduces gypsum emissions, improves gypsum quality, alleviates sulfur resource shortages, reduces desulfurization costs, and achieves clean production and circular economy development.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121668703A_ABST
    Figure CN121668703A_ABST
Patent Text Reader

Abstract

The invention relates to a limestone-gypsum wet desulphurization method and system.The method comprises the steps that desulfurized rich slurry is heated through a rich liquid heater and desorbed through a flash desorption device in sequence, obtained flash desorption steam is purified through a purification treatment unit, and desorbed sulfur dioxide gas can be obtained; and treating at least part of the desulfurized lean slurry by a gypsum treatment unit to obtain a gypsum product. By adopting the method disclosed by the invention, the discharge amount of the gypsum can be reduced and the quality of the gypsum can be improved while resource recycling of the sulfur is realized. Besides, the obtained desorbed sulfur dioxide gas can be converted into chemical products through subsequent process treatment, so that the current situation of sulfur resource shortage is relieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of flue gas desulfurization, and more specifically, to a method and system for limestone-gypsum wet desulfurization. Background Technology

[0002] Under the backdrop of ultra-low emission requirements for industrial flue gas, limestone-gypsum wet desulfurization technology accounts for a significant proportion of applications in my country's flue gas desulfurization field. Traditional limestone-gypsum wet desulfurization processes primarily produce gypsum as a byproduct. However, due to the unstable quality of desulfurization gypsum in my country and the utilization rate of less than 50% in most provinces, a large amount of desulfurization gypsum is discarded, causing serious secondary pollution to the ecological environment and land resources. Furthermore, my country's sulfur resources are relatively scarce, requiring the import of large quantities of sulfur and sulfuric acid annually. Therefore, addressing the issue of national sulfur resource imports is of significant practical importance. Summary of the Invention

[0003] The purpose of this disclosure is to provide a method and system for limestone-gypsum wet desulfurization to solve the problems of unstable gypsum quality, large amounts of gypsum being wasted, and sulfur resources being scarce in the prior art.

[0004] To achieve the above objectives, the first aspect of this disclosure provides a method for limestone-gypsum wet desulfurization, the method comprising: The limestone-gypsum wet desulfurization process involves heating the rich slurry in a rich liquid heater and then desorbing it in a flash desorber to obtain flash desorbed vapor and desulfurized lean slurry. The flash-desorbed vapor is fed into a purification unit for purification to obtain desorbed sulfur dioxide gas. At least a portion of the desulfurized lean slurry is fed into a gypsum treatment unit for oxidation treatment to obtain gypsum products.

[0005] Optionally, the operating conditions of the flash desorber include: a temperature of 50-100℃ and a negative pressure of 6-20 kPa (a).

[0006] Optionally, the purification unit includes a desorbed vapor cooler and a gas-liquid separator; the method further includes cooling the flash-desorbed vapor in the desorbed vapor cooler and separating the cooled desorbed vapor in the gas-liquid separator to obtain the desorbed sulfur dioxide gas; the concentration of the desorbed sulfur dioxide gas is 60-80% by volume.

[0007] Optionally, the gypsum processing unit includes an oxidation tank and a centrifugal dewatering machine; the method further includes causing at least a portion of the desulfurized lean slurry to enter the oxidation tank and mix with air for oxidation treatment to obtain gypsum slurry; and causing the gypsum slurry to enter the centrifugal dewatering machine for solid-liquid separation treatment to obtain the gypsum product.

[0008] Optionally, the desulfurization rich slurry comes from the slurry pool of the desulfurization absorption tower of the limestone-gypsum wet desulfurization process; optionally, the method further includes causing the first part of the desulfurization lean slurry to enter the gypsum treatment unit for oxidation treatment, and causing the second part of the desulfurization lean slurry to return to the slurry pool of the desulfurization absorption tower.

[0009] Optionally, a surfactant is added to the desulfurized lean slurry in the second part before it enters the slurry tank; The surfactant includes sodium dodecylbenzenesulfonate and / or calcium dodecylbenzenesulfonate; The ratio of the amount of surfactant added to the weight of the slurry in the slurry tank of the desulfurization absorption tower is (0.00001-0.005):1.

[0010] Optionally, the ratio of the weight of the desulfurized lean slurry returned from the desulfurization absorption tower to the total weight of the desulfurized lean slurry is (0.5-0.85):1.

[0011] Optionally, the method further includes introducing an antioxidant into the slurry pool of the desulfurization absorption tower and mixing it with the slurry in the slurry pool.

[0012] Optionally, the antioxidant includes one or more of the following: aqueous solutions of citric acid, acetic acid, benzoic acid, and oxalic acid; wherein the concentration of the antioxidant is 10-30% by weight.

[0013] The second aspect of this disclosure provides a limestone-gypsum wet desulfurization system, which includes a rich liquid heater, a flash desorber, a purification unit and a gypsum treatment unit. The inlet of the rich liquid heater is connected to the desulfurization rich slurry source; the outlet of the rich liquid heater is connected to the inlet of the flash desorber; the flash desorption steam outlet of the flash desorber is connected to the inlet of the purification unit; and the outlet of the desulfurization lean slurry of the flash desorber is connected to the inlet of the gypsum treatment unit.

[0014] The above technical solution involves sequentially heating the desulfurized rich slurry in a rich liquid heater and then desorbing it in a flash desorber. The resulting flash desorbed vapor is then purified in a purification unit to obtain desorbed sulfur dioxide gas. At least a portion of the obtained desulfurized lean slurry is then treated in a gypsum treatment unit to obtain gypsum products. This method achieves the resource recovery and utilization of sulfur while reducing gypsum emissions and improving gypsum quality. Furthermore, the obtained desorbed sulfur dioxide gas can be further processed into chemical products, which not only alleviates the current sulfur resource shortage but also reduces desulfurization costs, achieving cleaner production and a circular economy.

[0015] Other features and advantages of this disclosure will be described in detail in the following detailed description section. Attached Figure Description

[0016] The accompanying drawings are provided to further illustrate the present disclosure and form part of the specification. They are used together with the following detailed description to explain the present disclosure, but do not constitute a limitation thereof. In the drawings: Figure 1 This is a schematic diagram of a limestone-gypsum wet desulfurization system disclosed herein.

[0017] Figure 2 This is a schematic diagram of the limestone-gypsum wet desulfurization system of Comparative Example 1 of this disclosure.

[0018] Explanation of reference numerals in the attached figures 1. Desulfurization absorption tower; 2. Rich liquor discharge pump; 3. Rich liquor heater; 4. Flash desorber; 5. Desorbed vapor cooler; 6. Gas-liquid separator; 7. Vacuum pump; 8. Lean liquor return pump; 9. Oxidation blower; 10. Oxidation tank; 11. Oxidation tank discharge pump; 12. Centrifugal dehydrator; A. Antioxidant; B. Desulfurized rich slurry; C. Heated rich slurry; D. Flash evaporation desorption steam; E. Cooling desorption steam; F. Desorption of sulfur dioxide gas; G. Desulfurized lean slurry; H. Desulfurized lean slurry; I. First desulfurized lean slurry; J. Second desulfurized lean slurry; K. Air; L. Gypsum slurry; M. Gypsum product. Detailed Implementation

[0019] The specific embodiments of this disclosure will be described in detail below with reference to the accompanying drawings. It should be understood that the specific embodiments described herein are for illustration and explanation only and are not intended to limit this disclosure.

[0020] like Figure 1 As shown, the first aspect of this disclosure provides a method for limestone-gypsum wet desulfurization, the method comprising: The desulfurization rich slurry B from the limestone-gypsum wet desulfurization process is heated in the rich liquid heater 3 and then desorbed in the flash desorber 4 to obtain flash desorbed steam D and desulfurization lean slurry G. The flash desorbed vapor D is fed into a purification unit for purification to obtain desorbed sulfur dioxide gas F. At least a portion of the desulfurized lean slurry G is introduced into a gypsum treatment unit for oxidation treatment to obtain gypsum product M.

[0021] Through the above technical solution, the desulfurized rich slurry B is sequentially heated by the rich liquid heater 3 and desorbed by the flash desorber 4. The resulting flash desorbed gas D is then purified by a purification unit to obtain desorbed sulfur dioxide gas F. At least a portion of the obtained desulfurized lean slurry G is then treated by a gypsum treatment unit to obtain gypsum product M. Using the method disclosed herein, sulfur can be recycled and utilized as a resource while reducing gypsum emissions and improving gypsum quality. Furthermore, the obtained desorbed sulfur dioxide gas F can be further processed to convert it into chemical products, which not only alleviates the current sulfur resource shortage but also reduces desulfurization costs, achieving clean production and circular economy development.

[0022] In one embodiment, the desulfurization-rich slurry B described in this disclosure comes from the slurry pool of the desulfurization absorption tower 1 in the limestone-gypsum wet desulfurization process; wherein, the desulfurization absorption tower 1 is a conventional choice in the art, and this application does not make any special requirements. It should be noted that a spray layer is provided at the upper part of the desulfurization absorption tower 1 for spraying limestone slurry downwards; a slurry pool is provided at the lower part of the desulfurization absorption tower 1 for storing the mixed limestone and gypsum slurry obtained after reacting with sulfur dioxide.

[0023] In one embodiment, the number of spray layers in the desulfurization absorption tower 1 is 2 to 5.

[0024] In one embodiment, the desulfurization absorption tower 1 has a flue gas inlet in the middle and a desulfurization flue gas outlet at the top; the upper part of the slurry pool of the desulfurization absorption tower 1 has a desulfurization rich slurry outlet, the middle part of the slurry pool of the desulfurization absorption tower 1 has an antioxidant inlet, and the lower part of the slurry pool of the desulfurization absorption tower 1 has a desulfurization lean slurry inlet and a circulating slurry outlet.

[0025] In this embodiment, before desulfurization, the slurry at the bottom of the slurry pool in the desulfurization absorption tower 1 is circulated to the inlet of the spray layer via the circulating slurry outlet, so that the slurry is sprayed downwards. During desulfurization, boiler flue gas enters the middle of the desulfurization absorption tower 1 through the flue gas inlet and moves upwards, coming into countercurrent contact with the sprayed slurry, thereby removing sulfur dioxide from the boiler flue gas. The resulting desulfurized flue gas is discharged through the desulfurized flue gas outlet and enters the chimney. It should be noted that the desulfurization absorption tower 1 does not have an inlet for air intake to avoid the oxidation of bisulfite ions caused by the introduction of air, thus improving the desorption rate of sulfur dioxide.

[0026] In one embodiment, the method further includes that the desulfurized rich slurry B located in the upper part of the slurry pool of the desulfurization absorption tower 1 is transported to the rich liquid heater 3 for heating under the action of the rich liquid discharge pump 2 to obtain heated rich slurry C; and the heated rich slurry C is then introduced into the flash desorber 4 for the desorption treatment.

[0027] In this embodiment, the desulfurization-rich slurry B, located at the top of the slurry tank, is the freshest slurry formed after the reaction of limestone slurry and sulfur dioxide. The main product is calcium bisulfite. At this stage, a large portion of the calcium bisulfite has not yet been oxidized to calcium sulfate. Therefore, after the desulfurization-rich slurry B is transported to the rich liquid heater 3 for heating, the bisulfite ions can decompose into sulfur dioxide. The heated rich slurry C is then desorbed by the flash desorber 4. Under negative pressure conditions, as much sulfur dioxide as possible can be separated, improving the resource utilization of sulfur.

[0028] In one embodiment, the rich liquid heater 3 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements, as long as it can raise the temperature of the desulfurized rich slurry B to a suitable temperature. For example, the rich liquid heater 3 includes, but is not limited to, heat exchangers and / or electric heaters.

[0029] In one embodiment, the temperature for heating the rich slurry C is 50-100°C.

[0030] In some embodiments, the temperature at which the rich slurry C is heated is any temperature within the range formed by any one or any two of 55°C, 60°C, 65°C, 70°C, 75°C, 80°C, 85°C, 90°C, and 95°C.

[0031] In this embodiment, the temperature of the heated rich slurry C is raised to a suitable temperature to prepare for subsequent desorption treatment, allowing as many bisulfite ions as possible to decompose into sulfur dioxide, further improving the resource utilization of sulfur. The temperature of the heated rich slurry C can be controlled by adjusting the flow rate of the desulfurized rich slurry B entering the rich slurry heater 3. The flow rate of the desulfurized rich slurry B can be flexibly adjusted according to actual production conditions, as long as the residence time of the desulfurized rich slurry B in the rich slurry heater 3 is guaranteed and the risk of pipe scaling is reduced.

[0032] In one embodiment, the flash desorber 4 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements. For example, the flash desorber 4 includes, but is not limited to, a flash tank.

[0033] In one embodiment, the flash desorber 4 may be equipped with a stirring device. The stirring device can be a conventional choice in the art, and this application does not make any special requirements, as long as it can ensure that the slurry in the flash desorber 4 is fully stirred during the desorption process, and does not affect the sealing performance of the flash desorber 4.

[0034] In one embodiment, the flash desorber 4 of this disclosure includes multiple flash tanks arranged in parallel or in series.

[0035] In one embodiment, the number of flash tanks is 2-10.

[0036] In some implementations, the number of flash tanks is any number within the range of any one or any two of 3, 4, 5, 6, 7, 8, and 9.

[0037] In one embodiment, the flash desorber 4 includes three flash tanks connected in series as an example. These three flash tanks are designated as the first flash tank, the second flash tank, and the third flash tank. The inlet of the first flash tank is connected to the outlet of the rich liquid heater 3; the inlet of the second flash tank is connected to the flash desorption vapor outlet of the first flash tank; the inlet of the third flash tank is connected to the flash desorption vapor outlet of the second flash tank; and the flash desorption vapor outlet of the third flash tank is connected to the inlet of the purification unit. In this embodiment, the flash evaporation process occurs the instant the high-temperature, high-pressure fluid enters the flash tank, where, under negative pressure, gas and slurry are separated, latent heat is released, and sulfur dioxide gas and water vapor are desorbed.

[0038] In one embodiment, to improve the desorption rate of sulfur dioxide gas, the negative pressure of the first flash tank, the second flash tank, and the third flash tank is increased sequentially. The negative pressure of each flash tank can be flexibly adjusted according to actual production needs, which will not be elaborated upon here.

[0039] In another embodiment, taking a flash desorber 4 comprising three flash tanks arranged in parallel as an example, the three flash tanks are designated as the first flash tank, the second flash tank, and the third flash tank, respectively. One of the three flash tanks is in a standby state, meaning one of the three flash tanks is not in operation. Taking the third flash tank as an example, during desorption processing, the pressure of both the first and second flash tanks is adjusted to the negative pressure required for flash tank processing. Then, the heated rich slurry C is introduced into the first and second flash tanks respectively to achieve gas and slurry separation. If either the first or second flash tank experiences insufficient negative pressure or blockage, it can be switched to the third flash tank, allowing for maintenance without shutting down the entire system.

[0040] In one embodiment, the operating temperature of the flash desorber 4 is 50-100°C.

[0041] In some embodiments, the operating temperature of the flash desorber 4 is any temperature within the range formed by any one or any two of 55°C, 60°C, 65°C, 70°C, 75°C, 80°C, 85°C, 90°C, and 95°C.

[0042] In one embodiment, the negative pressure of the flash desorber 4 is 6-20 kPa (a).

[0043] In some embodiments, the negative pressure of the flash desorber 4 is any negative pressure within the range formed by any one or any two of the following: 6.5 kPa(a), 7 kPa(a), 7.5 kPa(a), 8 kPa(a), 8.5 kPa(a), 9 kPa(a), 9.5 kPa(a), 10 kPa(a), 10.5 kPa(a), 11 kPa(a), 11.5 kPa(a), 12 kPa(a), 12.5 kPa(a), 13 kPa(a), 13.5 kPa(a), 14 kPa(a), 14.5 kPa(a), 15 kPa(a), 15.5 kPa(a), 16 kPa(a), 16.5 kPa(a), 17 kPa(a), 17.5 kPa(a), 18 kPa(a), 18.5 kPa(a), 19 kPa(a), and 19.5 kPa(a). In this embodiment, when the operating conditions of the flash desorber 4 are suitable, it can desorb as much sulfur dioxide as possible from the heated slurry C.

[0044] In one embodiment, the purification processing unit of this disclosure includes a desorption vapor cooler 5 and a gas-liquid separator 6.

[0045] In one embodiment, the method further includes: cooling the flash desorbed steam D in a desorbed steam cooler 5 to obtain cooled desorbed steam E; and separating the cooled desorbed steam E in a gas-liquid separator 6 to obtain the desorbed sulfur dioxide gas F and condensate.

[0046] In one embodiment, the desorption vapor cooler 5 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements, as long as it can reduce the temperature of the material entering it.

[0047] In one embodiment, the gas-liquid separator 6 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements, as long as it can fully separate the condensate in the cooling and desorbing vapor E and the desorbed sulfur dioxide gas F.

[0048] In one embodiment, the temperature for cooling the desorbed vapor E is 40-60°C.

[0049] In some embodiments, the temperature for cooling the desorbed vapor E is any temperature within the range formed by any one or any two of 42°C, 44°C, 46°C, 48°C, 50°C, 52°C, 54°C, 56°C, and 58°C.

[0050] In one embodiment, the concentration of desorbed sulfur dioxide gas F is 60-80% by volume.

[0051] In some embodiments, the concentration of desorbed sulfur dioxide gas F is any concentration within the range formed by any one or any two of 61 vol%, 62 vol%, 63 vol%, 64 vol%, 65 vol%, 66 vol%, 67 vol%, 68 vol%, 69 vol%, 70 vol%, 71 vol%, 72 vol%, 73 vol%, 74 vol%, 75 vol%, 76 vol%, 77 vol%, 78 vol%, and 79 vol%.

[0052] In one embodiment, the sulfur dioxide desorption rate of the flash desorber 4 is 20% by weight or more.

[0053] In some embodiments, the sulfur dioxide desorption rate of the flash desorber 4 is any desorption rate within the range formed by any one or any two of the following: 21 wt%, 22 wt%, 23 wt%, 24 wt%, 25 wt%, 26 wt%, 27 wt%, 28 wt%, 29 wt%, 30 wt%, 31 wt%, 32 wt%, 33 wt%, 34 wt%, 35 wt%, 36 wt%, 37 wt%, 38 wt%, 39 wt%, 40 wt%, 41 wt%, 42 wt%, 43 wt%, 44 wt%, 45 wt%, 46 wt%, 47 wt%, 48 wt%, 49 wt%, and 50 wt%.

[0054] In one embodiment, the negative pressure of the flash desorber 4 is provided by the vacuum pump 7. The location of the vacuum pump 7 can be flexibly set according to the actual production situation. For example, the vacuum pump 7 can be set on the flash desorption vapor outlet pipeline of the flash desorber 4, or it can be set on the desorption sulfur dioxide gas outlet pipeline of the gas-liquid separator 6.

[0055] In one embodiment, the method further includes introducing antioxidant A into the slurry pool of the desulfurization absorption tower 1 through an antioxidant inlet, and mixing it with the slurry in the slurry pool. In this embodiment, adding antioxidant A to the slurry pool can, on the one hand, change the ionic form in the limestone slurry and inhibit oxidation, so that the rich solution mainly exists in the form of bisulfite ions; on the other hand, it can also inhibit the conversion of calcium bisulfite to gypsum, thereby improving the desorption rate of sulfur dioxide and the resource utilization rate of sulfur.

[0056] In one embodiment, the antioxidant A described in this disclosure includes, but is not limited to, one or more of the following: aqueous solutions of citric acid, acetic acid, benzoic acid, and oxalic acid.

[0057] In one embodiment, the concentration of antioxidant A described in this disclosure is 10-30% by weight.

[0058] In some embodiments, the concentration of antioxidant A described herein is any concentration within the range formed by any one or any two of 12 wt%, 14 wt%, 16 wt%, 18 wt%, 20 wt%, 22 wt%, 24 wt%, 26 wt%, 28 wt%, 30 wt%, 32 wt%, 34 wt%, 36 wt%, and 38 wt%.

[0059] In some embodiments, the concentrations of the aqueous solutions of citric acid, acetic acid, benzoic acid, and oxalic acid are 10-30 by weight, respectively.

[0060] In some embodiments, the concentrations of the aqueous citric acid solution, aqueous acetic acid solution, aqueous benzoic acid solution, and aqueous oxalic acid solution are any concentrations within the range formed by any one or any two of the following: 12 wt%, 14 wt%, 16 wt%, 18 wt%, 20 wt%, 22 wt%, 24 wt%, 26 wt%, 28 wt%, 30 wt%, 32 wt%, 34 wt%, 36 wt%, and 38 wt%.

[0061] In one embodiment, the weight ratio of the amount of antioxidant A added according to this disclosure to the slurry in the slurry tank of the desulfurization absorption tower 1 is (0.1-0.3):1.

[0062] In some embodiments, the weight ratio of the amount of antioxidant A added to the slurry in the slurry tank of the desulfurization absorption tower 1 is any weight ratio within the range formed by any one or any two of the following: 0.11:1, 0.12:1, 0.13:1, 0.14:1, 0.15:1, 0.16:1, 0.17:1, 0.18:1, 0.19:1, 0.20:1, 0.21:1, 0.22:1, 0.23:1, 0.24:1, 0.25:1, 0.26:1, 0.27:1, 0.28:1, and 0.29:1.

[0063] In one embodiment, the pH value of the slurry in the slurry tank of the desulfurization absorption tower 1 is 3-6.

[0064] In some embodiments, the pH value of the slurry in the slurry tank of the desulfurization absorption tower 1 is any pH value within the range formed by any one or any two of the following: 3, 3.1, 3.2, 3.3, 3.4, 3.5, 3.6, 3.7, 3.8, 3.9, 4.0, 4.1, 4.2, 4.3, 4.4, 4.5, 4.6, 4.7, 4.8, 4.9, 5.0, 5.1, 5.2, 5.3, 5.4, 5.5, 5.6, 5.7, 5.8, and 5.9.

[0065] In a preferred embodiment, the pH value of the slurry in the slurry tank of the desulfurization absorption tower 1 is 3-5.

[0066] In this embodiment, the addition of an acidic antioxidant to the slurry in the slurry tank increases the acidity of the slurry. When the pH of the slurry is within a suitable range, it not only improves the flue gas desulfurization effect but also ensures that the rich liquor mainly exists in the form of bisulfite ions, while inhibiting the oxidation of bisulfite ions to sulfate ions.

[0067] In one embodiment, the method further includes feeding the desorbed sulfur dioxide gas F into a subsequent processing unit for further processing to obtain sulfur-derived products. The subsequent processing unit includes, but is not limited to, a sodium metabisulfite preparation unit and / or a sulfuric acid preparation unit.

[0068] In one embodiment, the method further includes adding 10-30% by weight of antioxidant A to the slurry pool of the desulfurization absorption tower 1 before it is put into operation.

[0069] In one embodiment, the method further includes adding 10-20% by weight of antioxidant A to the slurry tank periodically during the operation of the desulfurization absorption tower 1. The interval between adding antioxidant A can be flexibly set according to actual production conditions, and will not be elaborated further here.

[0070] In one embodiment, the method further includes mixing the condensate obtained from the gas-liquid separator 6 with an antioxidant to form an antioxidant A of a suitable concentration, which is then introduced into the slurry pool of the desulfurization absorption tower 1.

[0071] In one embodiment, the desulfurized lean slurry G is transported via the lean slurry return pump 8, and at least a portion of the desulfurized lean slurry H is processed in the gypsum treatment unit, while another portion of the desulfurized lean slurry H is returned to the slurry pool of the desulfurization absorption tower 1.

[0072] In some embodiments, the desulfurized lean slurry G is transported by the lean slurry return pump 8 and divided into a first desulfurized lean slurry I and a second desulfurized lean slurry J. The first desulfurized lean slurry I is returned to the slurry pool of the desulfurization absorption tower 1, and the second desulfurized lean slurry J is processed in the gypsum treatment unit.

[0073] In one embodiment, the ratio of the weight of the desulfurized lean slurry returned to the desulfurization absorption tower 1 to the total weight of the desulfurized lean slurry H is (0.5-0.85):1.

[0074] In some embodiments, the weight ratio of the desulfurization lean slurry returned to the desulfurization absorption tower 1 to the total weight of the desulfurization lean slurry H is any weight ratio within the range formed by any one or any two of the following: 0.52:1, 0.54:1, 0.56:1, 0.58:1, 0.6:1, 0.62:1, 0.64:1, 0.66:1, 0.68:1, 0.70:1, 0.72:1, 0.74:1, 0.76:1, 0.78:1, 0.80:1, 0.82:1, and 0.84:1.

[0075] In one embodiment, the gypsum treatment unit includes an oxidation blower 9, an oxidation tank 10, and a centrifugal dewatering machine 12. The oxidation blower 9 is used to introduce air K into the oxidation tank 10 to ensure that the desulfurized lean slurry G entering the gypsum treatment unit is fully converted into gypsum; the centrifugal dewatering machine 12 is used to separate the gypsum and water.

[0076] In one embodiment, the oxidation blower 9 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements, as long as it can enable the introduction of air K into the oxidation tank 10.

[0077] In one embodiment, the oxidation tank 10 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements, as long as the material in the oxidation tank 10 can be mixed and stirred with the air K.

[0078] In one embodiment, the oxidation tank 10 may further include a stirring device for thoroughly stirring the slurry therein to enhance the effect of the oxidation reaction.

[0079] In one embodiment, the centrifugal dehydrator 12 described in this disclosure is a conventional choice in the art, and this application does not make any special requirements, as long as it can achieve solid-liquid separation.

[0080] In one embodiment, the method further includes mixing at least a portion of the desulfurized lean slurry G with air K in an oxidation tank 10 for oxidation treatment to obtain gypsum slurry L; and conveying the gypsum slurry L to a centrifugal dewatering machine 12 via an oxidation tank discharge pump 11 for solid-liquid separation treatment to obtain gypsum product M.

[0081] In one embodiment, the air K generated by the oxidation blower 9 has a pressure of 80-120 kPa and a flow rate of 500-5000 m³ / h. 3 / h. In this embodiment, the air K generated by the oxidation blower 9 can be used as a stirring medium for the oxidation tank 10 to improve the oxidation effect.

[0082] In one embodiment, the number of oxidation tanks 10 can be one or more.

[0083] In some embodiments, the number of oxidation tanks 10 is 2-10, wherein the multiple oxidation tanks 10 can be arranged in series or in parallel, preferably in parallel.

[0084] In some embodiments, taking two oxidation tanks 10 as an example, referred to as the first oxidation tank and the second oxidation tank respectively, during the oxidation process, a portion of the desulfurization lean slurry G is first introduced into the first oxidation tank until the desulfurization lean slurry G occupies 50-70% of the volume of the first oxidation tank. The first oxidation tank then begins oxidation treatment, and the process is switched to the second oxidation tank, i.e., slurry supply to the first oxidation tank is stopped, and slurry supply to the second oxidation tank is switched. When the solid content of the slurry in the first oxidation tank reaches 20% by weight, the oxidation reaction endpoint is reached. At this point, the slurry in the first oxidation tank is transferred to a centrifugal dewatering machine 12 for solid-liquid separation. When the desulfurization lean slurry G occupies 50-70% of the volume of the second oxidation tank, the second oxidation tank begins oxidation treatment, and the process is switched back to the first oxidation tank, i.e., slurry supply to the second oxidation tank is stopped, and slurry supply to the first oxidation tank is switched. The endpoint of the oxidation reaction in the second oxidation tank is the same as that in the first oxidation tank. It should be noted that the time for oxidation treatment in the first oxidation tank and the time for all reaction products to be discharged are always shorter than the feeding time of the second oxidation tank. That is, during the oxidation treatment, one oxidation tank is always kept completely empty.

[0085] In one embodiment, the gypsum product M has a purity of 60-90% by weight.

[0086] In some embodiments, the purity of gypsum product M is any purity within the range formed by any one or any two of 62% by weight, 64% by weight, 66% by weight, 68% by weight, 70% by weight, 72% by weight, 74% by weight, 76% by weight, 78% by weight, 80% by weight, 82% by weight, 84% by weight, 86% by weight, and 88% by weight.

[0087] In one embodiment, a surfactant can be added to the slurry circulation or conveying pipeline in the system disclosed herein to prevent pipe and equipment blockage caused by sediment in the slurry. It should be noted that the slurry circulation pipeline refers to the pipeline for slurry recycling, such as the pipeline between the lean liquor return pump 8 and the slurry pool inlet of the desulfurization absorption tower 1; the conveying pipeline refers to the pipeline for transporting material in the system, such as the inlet and outlet pipelines of the rich liquor heater 3 and the inlet and outlet pipelines of the flash desorber 4.

[0088] In some embodiments, a surfactant is added to the desulfurized lean slurry returned to the slurry pool of the desulfurization absorption tower 1.

[0089] In some embodiments, the desulfurized rich slurry B and the surfactant are introduced into the rich slurry heater 3.

[0090] In this embodiment, the addition of surfactants at the appropriate locations in this disclosure can prevent the slurry from scaling and clogging in pipelines and / or devices, thereby improving the system's operating cycle.

[0091] In one embodiment, the surfactant includes, but is not limited to, sodium dodecylbenzenesulfonate and / or calcium dodecylbenzenesulfonate.

[0092] In one embodiment, the amount of surfactant added is in a weight ratio of (0.00001-0.005):1 to the slurry in the slurry tank of the desulfurization absorption tower 1.

[0093] In some embodiments, the amount of surfactant added to the slurry in the slurry tank of the desulfurization absorption tower 1 is any proportion within the range formed by any one or any two of the following: 0.0001:1, 0.0005:1, 0.001:1, 0.0015:1, 0.002:1, 0.0025:1, 0.0030:1, 0.0035:1, 0.0040:1, and 0.0045:1.

[0094] In one implementation, such as Figure 1 As shown, the limestone-gypsum wet desulfurization method includes: Antioxidant A at a concentration of 10-30% by weight is introduced into the slurry tank of the desulfurization absorption tower 1 and mixed with the slurry in the slurry tank to form limestone slurry; wherein the weight ratio of the amount of antioxidant A added to the slurry in the slurry tank of the desulfurization absorption tower 1 is (0.1-0.3):1. The sulfur-containing flue gas enters the desulfurization absorption tower 1 and comes into countercurrent contact with the limestone slurry. The resulting desulfurized rich slurry B flows downward to the slurry pool, and the resulting desulfurized flue gas flows upward out of the device. The desulfurized rich slurry B, located in the upper part of the slurry pool of the desulfurization absorption tower 1, is transported to the rich slurry heater 3 for heating under the action of the rich slurry discharge pump 2, resulting in a heated rich slurry C at a temperature of 50-100℃. The heated rich slurry C then enters the flash desorber 4 for the aforementioned desorption treatment, yielding flash desorbed steam D and desulfurized lean slurry G. The operating conditions of the flash desorber 4 include: a temperature of 50-100℃ and a negative pressure of 6-20 kPa (a). The flash desorbed steam D is cooled by the desorbed steam cooler 5 to obtain cooled desorbed steam E at a temperature of 40-60℃; the cooled desorbed steam E is then processed by the gas-liquid separator 6 to obtain desorbed sulfur dioxide gas F with a concentration of 60-80% by weight and condensate. The desulfurized lean slurry G is transported via lean slurry return pump 8, and at least a portion of the desulfurized lean slurry H is used as the second desulfurized lean slurry J and mixed with air K generated by oxidation fan 9 for oxidation treatment to obtain gypsum slurry L. The gypsum slurry L is then transported via oxidation tank discharge pump 11 to centrifugal dewatering machine 12 for solid-liquid separation treatment to obtain gypsum product M with a purity of 60-90% by weight. Another portion of the desulfurized lean slurry H is returned as the first desulfurized lean slurry I to the slurry pool of the desulfurization absorption tower 1. The ratio of the weight of the desulfurized lean slurry returned to the desulfurization absorption tower 1 to the total weight of the desulfurized lean slurry is (0.5-0.85):1. A surfactant is added to the desulfurized lean slurry returning to the slurry tank of the desulfurization absorption tower 1; and / or, the desulfurized rich slurry B and the surfactant are introduced into the rich liquid heater 3. The amount of surfactant added is in a weight ratio of (0.00001-0.005):1 to the slurry in the slurry tank of the desulfurization absorption tower 1.

[0095] like Figure 1 As shown, the second aspect of this disclosure provides a limestone-gypsum wet desulfurization system, which includes a desulfurization absorption tower 1, a rich liquid heater 3, a flash desorber 4, a purification unit and a gypsum treatment unit. The outlet of the desulfurized rich slurry of the desulfurization absorption tower 1 is connected to the inlet of the rich liquid heater 3; the outlet of the rich liquid heater 3 is connected to the inlet of the flash desorber 4, so that the desulfurized rich slurry B in the slurry pool of the desulfurization absorption tower 1 is heated by the rich liquid heater 3 and then enters the flash desorber 4 for desorption treatment to obtain flash desorbed steam D and desulfurized lean slurry G. The flash desorption vapor outlet of the flash desorber 4 is connected to the inlet of the purification unit so that the flash desorption vapor D can be processed by the purification unit to obtain desorbed sulfur dioxide gas F. The outlet of the desulfurized lean slurry of the flash desorber 4 is connected to the inlet of the gypsum treatment unit, so that at least a portion of the desulfurized lean slurry G enters the gypsum treatment unit for processing to obtain gypsum product M.

[0096] In one embodiment, the purification unit includes a desorbed vapor cooler 5 and a gas-liquid separator 6; the inlet of the desorbed vapor cooler 5 is connected to the flash desorbed vapor outlet of the flash desorber 4, so that the flash desorbed vapor D is cooled by the desorbed vapor cooler 5 to obtain cooled desorbed vapor E; the outlet of the desorbed vapor cooler 5 is connected to the inlet of the gas-liquid separator 6, so that the cooled desorbed vapor E enters the gas-liquid separator 6 for processing to obtain desorbed sulfur dioxide gas F and condensate.

[0097] In one embodiment, the gypsum processing unit includes an oxidation blower 9, an oxidation tank 10, and a centrifugal dewatering machine 12; the inlet of the oxidation blower 9 is connected to an air source, and the outlet of the oxidation blower 9 is connected to the air inlet of the oxidation tank 10; the slurry inlet of the oxidation tank 10 is connected to the outlet of the desulfurized lean slurry of the flash desorber 4, so that at least a portion of the desulfurized lean slurry H enters the oxidation tank 10 as a second desulfurized lean slurry J and mixes with the air K generated by the oxidation blower 9 for oxidation treatment to obtain gypsum slurry L; the outlet of the oxidation tank 10 is connected to the inlet of the centrifugal dewatering machine 12, so that the gypsum slurry L is transported to the centrifugal dewatering machine 12 via the oxidation tank discharge pump 11 for solid-liquid separation treatment to obtain gypsum product M.

[0098] In one embodiment, the slurry inlet of the oxidation tank 10 and the circulating slurry outlet of the desulfurization absorption tower 1 are respectively connected to the desulfurization lean slurry outlet of the flash desorber 4, so that at least part of the desulfurization lean slurry G enters the oxidation tank 10 for oxidation treatment, and another part of the desulfurization lean slurry G is returned to the desulfurization absorption tower 1.

[0099] The present disclosure is further described in detail below through examples. All raw materials used in the examples are commercially available.

[0100] Example 1 limestone-gypsum wet desulfurization systems, such as Figure 1 As shown, this system targets a power plant's flue gas flow rate of 50,000 Nm³. 3 / h, the original SO2 concentration was 2000 mg / Nm³. 3 The emission concentration was 35 mg / Nm³. 3 .

[0101] The limestone-gypsum wet desulfurization method includes: A 20% by weight citric acid aqueous solution is introduced into the slurry tank of the desulfurization absorption tower 1 and mixed with the slurry in the slurry tank to form limestone slurry. The weight ratio of the amount of citric acid aqueous solution added at one time to the slurry in the slurry tank of the desulfurization absorption tower 1 is 0.2:1. The pH value of the limestone slurry fluctuates between 3 and 5. When the pH value reaches 5, citric acid aqueous solution is added. The sulfur-containing flue gas enters the desulfurization absorption tower 1 and comes into countercurrent contact with the limestone slurry. The resulting desulfurized rich slurry B flows downward to the slurry pool, and the resulting desulfurized flue gas flows upward out of the device. The desulfurized rich slurry B, located at the top of the slurry pool in the desulfurization absorption tower 1, is pumped to the rich slurry heater 3 by the rich slurry discharge pump 2 to obtain a heated rich slurry C at a temperature of 50°C. The heated rich slurry C then enters the flash desorber 4 for the desorption treatment to obtain flash desorbed steam D and desulfurized lean slurry G. The operating conditions of the flash desorber 4 include a temperature of 51°C and a negative pressure of 13 kPa (a). The flash desorbed steam D is cooled by the desorbed steam cooler 5 to obtain cooled desorbed steam E at a temperature of 50°C; the cooled desorbed steam E is then processed by the gas-liquid separator 6 to obtain desorbed sulfur dioxide gas F with a concentration of 80% by volume and condensate. The desulfurized lean slurry G is transported via lean slurry return pump 8, and at least a portion of the desulfurized lean slurry H is introduced as second desulfurized lean slurry J into oxidation tank 10 and mixed with air K generated by oxidation blower 9 for oxidation treatment to obtain gypsum slurry L; the gypsum slurry L is then transported via oxidation tank discharge pump 11 to centrifugal dewatering machine 12 for solid-liquid separation treatment to obtain gypsum product M with a purity of 82% by weight; another portion of the desulfurized lean slurry H is returned as first desulfurized lean slurry I to the slurry pool of desulfurization absorption tower 1; the weight ratio of the desulfurized lean slurry returned to desulfurization absorption tower 1 to the total weight of the desulfurized lean slurry is 0.6:1; Sodium dodecylbenzenesulfonate is added to the desulfurization lean slurry returning to the slurry tank of the desulfurization absorption tower 1; and / or, the desulfurization rich slurry B and sodium dodecylbenzenesulfonate are introduced into the rich liquid heater 3. The weight ratio of the amount of sodium dodecylbenzenesulfonate added to the slurry in the slurry tank of the desulfurization absorption tower 1 is 0.0005:1.

[0102] After treatment using the method described in this embodiment, the SO2 desorption rate reaches 30%, reducing gypsum emissions by 501 tons annually and increasing the annual production of desorbed sulfur dioxide gas by 235.8 tons, resulting in considerable economic benefits. The system operates stably within one operating cycle (1 year).

[0103] Example 2 The limestone-gypsum wet desulfurization method is the same as in Example 1, except that the negative pressure of the flash desorber 4 is 30 kPa(a). After treatment by this method, the SO2 desorption rate reaches 32%, the concentration of desorbed sulfur dioxide gas reaches 70% by volume, increasing the annual production of desorbed sulfur dioxide gas by 287.5t; the purity of the gypsum product is 81% by weight, reducing gypsum emissions by 492.8t annually, resulting in considerable economic benefits. The system operates stably within one operating cycle (1 year).

[0104] Example 3 The limestone-gypsum wet desulfurization method is the same as in Example 1, except that the temperature of the flash desorber 4 is 110℃. After treatment by this method, the SO2 desorption rate reaches 38%, the purity of the desorbed sulfur dioxide gas reaches 65% by volume, increasing SO2 production by 367.6t per year; the purity of the gypsum product is 80% by weight, reducing gypsum emissions by 454.9t per year, resulting in considerable economic benefits. The system operates stably within one operating cycle (1 year).

[0105] Example 4 The limestone-gypsum wet desulfurization method is the same as in Example 1, except that the concentration of the citric acid aqueous solution is 5% by weight. After treatment by this method, the SO2 desorption rate reaches 23%, the purity of the desorbed sulfur dioxide gas reaches 60% by volume, increasing the annual production of desorbed sulfur dioxide gas by 241.1 tons; the purity of the gypsum product is 88% by weight, reducing gypsum emissions by 513.6 tons annually, resulting in considerable economic benefits. The system operates stably within one operating cycle (1 year).

[0106] Example 5 The limestone-gypsum wet desulfurization method is the same as in Example 1, except that the weight ratio of the desulfurization lean slurry returned to the desulfurization absorption tower 1 to the total weight of the desulfurization lean slurry is 0.4:1. After treatment by this method, the SO2 desorption rate reaches 30%, the purity of the desorbed sulfur dioxide gas reaches 80% by volume, increasing the annual production of desorbed sulfur dioxide gas by 235.8t; the purity of the gypsum product is 82% by weight, reducing gypsum emissions by 334t annually, resulting in considerable economic benefits. The system operates stably within one operating cycle (1 year).

[0107] Example 6 The limestone-gypsum wet desulfurization method is the same as in Example 1, except that the weight ratio of the surfactant added to the slurry in the slurry tank of the desulfurization absorption tower 1 is 0.000001:1. After treatment by this method, the SO2 desorption rate reaches 30%, the purity of the desorbed sulfur dioxide gas reaches 80% by volume, and the annual production of desorbed sulfur dioxide gas increases by 200.5t; the purity of the gypsum product is 82% by weight, and the annual gypsum emission is reduced by 450.3t, resulting in considerable economic benefits. Pipeline blockage may occur within one operating cycle (1 year).

[0108] Comparative Example 1 limestone-gypsum wet desulfurization systems, such as Figure 2 As shown.

[0109] The limestone-gypsum wet desulfurization method includes: Boiler flue gas enters the desulfurization booster fan through the inlet damper, then passes through the flue gas heat exchanger and enters the absorption tower for SO2 removal. The desulfurized flue gas is then washed and demisted, with small droplets removed by a demister before being discharged from the boiler through the flue gas heat exchanger. Desulfurization byproducts are dehydrated into dehydrated gypsum through a hydrocyclone and a vacuum belt dewatering machine.

[0110] Using a comparative method, no sulfur dioxide desorption and recycling were performed, nor was gypsum emission reduced. The purity of the dehydrated gypsum was 50% by weight. The system requires minor repairs during the year and major repairs at the end of the year within one operating cycle (1 year).

[0111] A comparison of the data from Examples 1-6 and Comparative Example 1 shows that the method of this disclosure can obtain sulfur dioxide gas with higher purity, realizing the recycling and utilization of sulfur resources. Furthermore, the method of this disclosure can reduce gypsum emissions and improve gypsum quality. In addition, the obtained desorbed sulfur dioxide gas can be further processed into chemical products, which can not only alleviate the current shortage of sulfur resources but also reduce desulfurization costs, achieving clean production and circular economy development. A comparison of the data from Examples 1 and 2 shows that when the negative pressure of the flash desorber is 6-20 kPa(a), higher purity sulfur dioxide gas and gypsum products can be obtained, improving the economic efficiency of the system operation. A comparison of the data from Examples 1 and 3 shows that when the temperature of the flash desorber is 50-100℃, higher purity sulfur dioxide gas and gypsum products can be obtained, improving the economic efficiency of the system operation. A comparison of the data from Examples 1 and 4 shows that when the concentration of antioxidant A is 10-30% by weight, higher purity sulfur dioxide gas and gypsum products can be obtained, improving the economic efficiency of the system operation. A comparison of the data from Examples 1 and 5 shows that a weight ratio of the desulfurization lean slurry returned to the desulfurization absorption tower 1 to the total weight of the desulfurization lean slurry is (0.5-0.85):1, which can reduce gypsum emissions and the amount of gypsum requiring waste disposal. A comparison of the data from Examples 1 and 6 shows that a surfactant addition ratio to the weight of the slurry in the slurry tank of (0.00001-0.005):1 can improve the stability of the system operation.

[0112] The preferred embodiments of this disclosure have been described in detail above with reference to the accompanying drawings. However, this disclosure is not limited to the specific details of the above embodiments. Within the scope of the technical concept of this disclosure, various simple modifications can be made to the technical solutions of this disclosure, and these simple modifications all fall within the protection scope of this disclosure.

[0113] It should also be noted that the various specific technical features described in the above embodiments can be combined in any suitable manner without contradiction. To avoid unnecessary repetition, this disclosure will not describe the various possible combinations separately.

[0114] Furthermore, various different embodiments of this disclosure can be combined in any way, as long as they do not violate the spirit of this disclosure, they should also be regarded as the content disclosed in this disclosure.

Claims

1. A method for limestone-gypsum wet desulfurization, characterized by, The method comprises: The desulfurization rich slurry of the limestone-gypsum wet desulfurization process is heated in a rich slurry heater (3) and then enters a flash desorber (4) for desorption treatment to obtain flash desorption gas and desulfurization lean slurry; The flash desorption gas enters a purification treatment unit for purification treatment to obtain desorbed sulfur dioxide gas; At least part of the desulfurization lean slurry enters a gypsum treatment unit for oxidation treatment to obtain gypsum products.

2. The method of claim 1, wherein, The operating conditions of the flash desorber (4) include a temperature of 50-100°C and a negative pressure of 6-20 kPa (a).

3. The method of claim 1, wherein, The purification treatment unit comprises a desorption gas cooler (5) and a gas-liquid separator (6); The method further comprises cooling the flash desorption gas in the desorption gas cooler (5) and gas-liquid separation of the obtained cooled desorption gas in the gas-liquid separator (6) to obtain the desorbed sulfur dioxide gas; The concentration of the desorbed sulfur dioxide gas is 60-80% by volume.

4. The method of claim 1, wherein, The gypsum treatment unit comprises an oxidation tank (10) and a centrifugal dewatering machine (12); The method further comprises mixing the desulfurization lean slurry with air in the oxidation tank (10) for oxidation treatment to obtain gypsum slurry; The gypsum slurry enters the centrifugal dewatering machine (12) for solid-liquid separation treatment to obtain the gypsum products.

5. The method of claim 1, wherein, The desulfurization rich slurry is from the slurry pool of the desulfurization absorption tower (1) of the limestone-gypsum wet desulfurization process; Optionally, the method further comprises that a first part of the desulfurization lean slurry enters the gypsum treatment unit for oxidation treatment and a second part of the desulfurization lean slurry returns to the slurry pool of the desulfurization absorption tower (1).

6. The method of claim 5, wherein, A surfactant is added to the second part of the desulfurization lean slurry before entering the slurry pool; The surfactant comprises sodium dodecyl benzene sulfonate and / or calcium dodecyl benzene sulfonate; The weight ratio of the amount of the surfactant to the slurry in the slurry pool of the desulfurization absorption tower (1) is (0.00001-0.005):

1.

7. The method of claim 5, wherein, The ratio of the weight of the desulfurization lean slurry returning to the desulfurization absorption tower (1) to the total weight of the desulfurization lean slurry is (0.5-0.85):

1.

8. The method of claim 5, wherein, The method further comprises that an antioxidant enters the slurry pool of the desulfurization absorption tower (1) and mixes with the slurry in the slurry pool.

9. The method of claim 8, wherein, The antioxidant comprises one or more of a citric acid aqueous solution, an acetic acid aqueous solution, a benzoic acid aqueous solution and an oxalic acid aqueous solution; The concentration of the antioxidant is 10-30% by weight.

10. A system for limestone-gypsum wet desulphurization, characterized by, The system comprises a rich slurry heater (3), a flash desorber (4), a purification treatment unit and a gypsum treatment unit; The inlet of the rich slurry heater (3) is in communication with a desulfurization rich slurry source; the outlet of the rich slurry heater (3) is in communication with the inlet of the flash desorber (4); the flash desorption gas outlet of the flash desorber (4) is in communication with the inlet of the purification treatment unit; and the desulfurization lean slurry outlet of the flash desorber (4) is in communication with the inlet of the gypsum treatment unit.