A sensory integrated ribbon optical cable with thermally conductive and insulating micro-buffered structure and its fabrication method
By designing a composite sandwich-wrapped cable core architecture and a modified thermally conductive and insulating micro-buffer layer, the problems of inconsistent fiber stress distribution and differences in heat conduction paths in existing ribbon optical cables are solved, enabling high-precision temperature measurement and multi-parameter sensing, which is suitable for complex working conditions.
Patent Information
- Application Number
- CN202611490612.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-23
- Publication Date
- 2026-11-10
AI Technical Summary
Existing ribbon optical cables have problems in the integration of sensing and communication optical fibers, such as excessively large cable outer diameter, complex construction, inconsistent fiber stress distribution, large differences in heat conduction paths, poor temperature measurement synchronization, errors introduced by mechanical strain, slow heat diffusion, and insufficient anti-aging performance. They cannot effectively identify the true temperature of the optical cable and the false temperature signal caused by external pressure.
It adopts a composite sandwich-clad cable core architecture, integrating communication and Raman temperature measurement optical fibers. It uses a gradient modified thermally conductive and insulating micro-buffer layer and a thermally controlled water-blocking composite transition layer, combined with a modified thermally conductive non-metallic composite reinforcement layer, to achieve coplanar arrangement of optical fibers and strain-assisted sensing, taking into account both heat conduction and stress isolation, and adapting to strong electromagnetic interference scenarios.
It simplifies the construction process, reduces engineering costs, improves temperature measurement accuracy and multi-parameter sensing capabilities, can distinguish between real and pseudo temperature signals, enhances the heat diffusion capacity and anti-aging performance of optical cables, and is suitable for complex working conditions.
Smart Images

Figure CN123066941A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of optical cable technology, specifically relating to an integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure and its preparation method. Background Technology
[0002] Ribbon optical cables have high fiber density and high splicing efficiency, and are widely used in access networks, data centers, utility tunnels, and power supply communication projects. There are currently two main solutions for distributed temperature monitoring: the first is to lay independent DTS temperature measurement optical cables in parallel with ordinary communication optical cables; the second is to simultaneously place independent communication fiber ribbons and independent sensing fiber units inside the cable core.
[0003] The existing technology has several drawbacks: 1) The cable is made of two independent optical fiber units, resulting in a large outer diameter that is incompatible with existing ribbon optical cable duct routes and junction boxes; construction requires separate splicing of communication and sensing optical fibers, which is cumbersome and costly. 2) The communication and sensing optical fibers belong to different fiber bands, leading to inconsistent stress distributions when the cable is bent or compressed; the heat conduction paths of the sensing and communication optical fibers differ significantly, resulting in a deviation between the sensed temperature and the actual ambient temperature, and poor temperature synchronization. 3) The sensing optical fiber is directly subjected to mechanical strain from cabling, laying bends, and external pressure; the strain signal is superimposed with the Raman scattering demodulated signal, introducing temperature drift error and distorting the temperature measurement. 4) Existing integrated sensing ribbon optical cables only achieve single-temperature acquisition and cannot distinguish between a genuine temperature rise and a false temperature signal caused by external pressure; traditional all-dry non-metallic optical cables are prone to thermal delamination at the sheath-reinforcement interface under high-temperature conditions, and their thermal conductivity efficiency decreases year by year with aging; ordinary thermally conductive buffer layers only focus on stress buffering and do not take into account controllable thermal impedance, anti-aging, and pressure recognition capabilities. 5) Traditional non-metallic reinforcing braided layers only provide tensile strength and have no thermal conductivity regulation function. The heat transfer path from the sheath to the cable core is uncontrollable, and when local hot spots occur, heat diffusion is slow, resulting in a lag in sensing response.
[0004] Therefore, there is an urgent need to develop an innovative layered formulation structure for an integrated sensing ribbon optical cable that breaks away from the conventional cable core layout of bundled tubes and filler ropes. This cable integrates communication and temperature sensing within a single optical fiber ribbon, while simultaneously achieving graded control of thermal impedance, decoupling and identification of stress-temperature signals, and high-temperature delamination resistance. It is also compatible with existing ribbon fusion splicing equipment and improves temperature measurement accuracy and multi-parameter sensing capabilities. Summary of the Invention
[0005] To address the problems in existing technologies, the present invention aims to provide an integrated sensing ribbon optical cable with a thermally conductive and insulating micro-buffered structure and its fabrication method. This invention abandons the conventional cable core arrangement of multiple bundle tubes + filler ropes, adopting a composite sandwich-wrapped cable core architecture. A gradient-modified thermally conductive and insulating micro-buffered composite layer is set at the Raman temperature measurement multimode sensing fiber at the edge of the planar integrated fiber ribbon unit. A thermally controlled water-blocking composite transition layer is added between the planar integrated fiber ribbon unit and the modified thermally conductive non-metallic composite reinforcement layer. A thermally modified formula is designed for the modified thermally conductive non-metallic composite reinforcement layer. This achieves integration of communication, Raman temperature measurement, and strain-assisted sensing, decoupling temperature and strain signals, and avoiding spurious temperature signals caused by mechanical stress. It balances thermal conductivity and stress isolation, resists high-temperature aging and delamination, is suitable for strong electromagnetic interference scenarios, and is compatible with existing ribbon fusion splicing fixtures and junction boxes.
[0006] To achieve the above objectives and technical effects, the technical solution adopted by this invention is as follows: A transducer-integrated ribbon optical cable with a thermally conductive and insulating micro-buffered structure includes, from the inside out: a planar integrated fiber ribbon unit, a thermally modulated water-blocking composite transition layer, a modified thermally conductive non-metallic composite reinforcing layer, and a low-smoke, halogen-free, and temperature-resistant outer sheath.
[0007] Furthermore, the planar integrated fiber ribbon unit is a single integrated planar fiber ribbon, and the fibers in the planar integrated fiber ribbon unit are arranged coplanarly and are integrally solidified into one piece by the ribbon base encapsulation layer.
[0008] Furthermore, the optical fibers within the planar integrated fiber ribbon unit include multiple single-mode communication fibers and Raman temperature measurement multimode sensing fibers, with all fibers maintaining a standard fiber ribbon pitch of 250μm. The single-mode optical fiber for communication is arranged in the middle of the planar integrated fiber optic ribbon unit; The Raman temperature measurement multimode sensing fiber is arranged at the two edges of the planar integrated fiber ribbon unit; a gradient modified thermally conductive and insulating micro-buffer composite layer is provided between the outer side of each Raman temperature measurement multimode sensing fiber and the ribbon base encapsulation layer. A Brillouin scattering strain-assisted sensing fiber may or may not be provided between the Raman temperature measurement multimode sensing fiber and the communication single-mode fiber at one edge of the planar integrated fiber ribbon unit.
[0009] Furthermore, the planar integrated fiber ribbon unit employs differentiated excess length control: The excess length of single-mode communication fiber in the middle is 0.02%-0.05%, and the excess length of Raman temperature measurement multimode sensing fiber on both sides is 0.05%-0.08%.
[0010] Furthermore, the total thickness of the gradient-modified thermally conductive and insulating micro-buffered composite layer is 25-60 μm, and it is a two-layer composite structure, including a first buffer sub-layer and a second impedance-regulating sub-layer arranged sequentially from the inside to the outside. The first buffer sublayer is attached to the Raman temperature measurement multimode sensing fiber, which is made of an organosilicon elastomer doped with 5-8wt% and 50-200nm nano-hexagonal boron nitride, with a Shore A hardness of 25-35. The second impedance control sublayer is made of an organosilicon-acrylic blend elastomer doped with 2-4 wt% hollow glass microspheres with a particle size of 10-50 μm, and has a Shore A hardness of 45-55.
[0011] Furthermore, the substrate encapsulation layer is made of UV-curable acrylic resin with 1-3 wt% nano-silica filler with a particle size of 20-100 nm, and the overall thickness is 0.4-0.6 mm.
[0012] Furthermore, the thickness of the thermally controlled water-blocking composite transition layer is 0.25-0.4 mm, and it is a co-extruded semi-dense microporous structure. The matrix is modified EVA, compounded with superabsorbent polymer (SAP) powder and sheet-like boron nitride thermally conductive filler.
[0013] Furthermore, the modified thermally conductive non-metallic composite reinforcing layer is made of glass fiber yarn and high thermally conductive aramid chopped fiber, with a weaving coverage of 80%-92%.
[0014] Furthermore, the low-smoke halogen-free, heat-resistant outer sheath is made of heat-resistant, low-smoke halogen-free, flame-retardant polyolefin sheath material with a total thickness of 1.4-1.8 mm.
[0015] This invention also discloses a method for fabricating an integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure, comprising the following steps: S1. Fabrication of planar integrated fiber ribbon units; S2. A thermally modulated water-blocking composite transition layer is formed by coating the outer periphery of the planar integrated fiber ribbon unit. S3. A modified thermally conductive non-metallic composite reinforcing layer is woven around the outer periphery of the thermally controlled water-blocking composite transition layer; S4. A low-smoke, halogen-free, and temperature-resistant outer sheath is formed by extruding and coating the modified thermally conductive non-metallic composite reinforcing layer to obtain the integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure.
[0016] Compared with the prior art, the beneficial effects of the present invention are as follows: (1) The cable core structure is innovative. The conventional structure of PBT bundle tube + filler rope is eliminated. The planar integrated optical fiber ribbon unit is directly covered by a heat-controlled water-blocking composite transition layer, which simplifies the cable core structure. The overall outer diameter of the optical cable is smaller than that of the traditional multi-unit ribbon optical cable. It is compatible with existing pipeline routes, 12 / 13 core ribbon junction boxes and fusion splicing equipment. The original construction process does not need to be significantly modified, reducing the project cost. (2) The planar integrated fiber ribbon unit integrates multiple communication single-mode fibers and at least two Raman temperature measurement multimode sensing fibers. The Raman temperature measurement multimode sensing fibers are placed at the edge, resulting in a short thermal path. All fibers are coplanarly cured, and the communication single-mode fibers and the Raman temperature measurement multimode sensing fibers are in the same environment, resulting in high temperature measurement synchronization. The two Raman temperature measurement multimode sensing fibers serve as hardware backups for each other. (3) A gradient-modified thermally conductive and insulating micro-buffered composite layer is adopted, which is no longer a single material buffer layer; the inner layer focuses on thermal conductivity and flexible buffering, while the outer layer controls thermal impedance and filters out high-frequency impact stress; in conjunction with Brillouin scattering strain-assisted sensing fiber to collect the actual strain of the optical cable, it can distinguish between the pseudo temperature signal of external force extrusion and the real environmental temperature rise, and significantly reduce the temperature drift error introduced by strain. (4) A new thermally controlled water-blocking composite transition layer with a semi-dense microporous composite formula is added to achieve dry water blocking, deformation buffering and heat conduction channel establishment, while solving the defects of interlayer delamination and heat conduction failure after high temperature aging of traditional optical cables. (5) A modified thermally conductive non-metallic composite reinforcing layer is made of multiple strands of glass fiber yarn and a small amount of high thermal conductivity aramid short-cut fiber. It takes into account tensile strength and electromagnetic interference resistance, while improving radial heat diffusion capability. Local hot spot heat is rapidly diffused, and the sensing fiber response speed is faster. The whole is dry and metal-free, which is suitable for strong electromagnetic and high temperature complex working conditions such as pipe gallery, power tunnel, and energy storage compartment. (6) This optical cable not only realizes simple distributed temperature measurement, but also has communication + temperature monitoring + strain event recognition capabilities. It can identify abnormal events such as squeezing, impact, and excessive stretching, thus expanding the sensing capabilities of the optical cable. Attached Figure Description
[0017] Figure 1 This is a schematic diagram of the structure of the present invention. Detailed Implementation
[0018] The present invention will now be described in detail so that its advantages and features can be more easily understood by those skilled in the art, thereby providing a clearer and more explicit definition of the scope of protection of the present invention.
[0019] The following provides a brief overview of one or more aspects to offer a basic understanding of them. This overview is not an exhaustive summary of all conceived aspects, nor is it intended to identify key or decisive elements of all aspects, nor to define the scope of any or all aspects. Its sole purpose is to present some concepts of one or more aspects in a simplified form to prepare for the more detailed descriptions that follow.
[0020] like Figure 1 As shown, this invention discloses an integrated optical fiber ribbon cable with a thermally conductive and insulating micro-buffered structure, comprising: a planar integrated optical fiber ribbon unit 1, a thermally controlled water-blocking composite transition layer 2, a modified thermally conductive non-metallic composite reinforcing layer 3, and a low-smoke halogen-free and temperature-resistant outer sheath 4. The planar integrated optical fiber ribbon unit 1 is completely covered by the thermally controlled water-blocking composite transition layer 2, the modified thermally conductive non-metallic composite reinforcing layer 3 is wrapped around the outer periphery of the thermally controlled water-blocking composite transition layer 2, and the low-smoke halogen-free and temperature-resistant outer sheath 4 is extruded and wrapped around the outer side of the modified thermally conductive non-metallic composite reinforcing layer 3.
[0021] Unlike the traditional structure of the original design with bundle tube and filler rope, this invention eliminates the independent PBT bundle tube and filler rope. The planar integrated optical fiber ribbon unit 1 of this invention is directly and tightly wrapped by the thermally controlled water-blocking composite transition layer 2, and no longer adopts the round cable core mode with loose filler ropes.
[0022] In some embodiments, the planar integrated fiber ribbon unit 1 is a single integrated planar fiber ribbon. The fibers within the planar integrated fiber ribbon unit 1 are arranged coplanarly and are integrally solidified by the ribbon base encapsulation layer.
[0023] In some specific implementations, the planar integrated fiber optic ribbon unit 1 includes multiple single-mode communication fibers and at least two Raman temperature measurement multimode sensing fibers. The planar integrated fiber optic ribbon unit 1 may also optionally include a Brillouin scattering strain-assisted sensing fiber, depending on actual requirements.
[0024] In some specific implementations, the fiber arrangement rules within the planar integrated fiber ribbon unit 1 are as follows: The single-mode optical fiber for communication is arranged in the middle of the planar integrated optical fiber strip unit 1; Raman temperature measurement multimode sensing fiber is arranged at the two edges of the planar integrated fiber ribbon unit 1; The Brillouin scattering strain-assisted sensing fiber is positioned between the Raman temperature measurement multimode sensing fiber and the communication single-mode fiber on one side.
[0025] In some specific implementations, a gradient-modified thermally conductive and insulating micro-buffered composite layer is provided between the outer side of each Raman temperature measurement multimode sensing fiber and the base-encapsulated layer.
[0026] In some specific implementations, the planar integrated fiber ribbon unit 1 has a total of 13 cores. Ten G.652D communication single-mode fibers are arranged in the center, and one 50 / 125μm Raman thermometry multimode sensing fiber is arranged on each of the left and right edges. A 9 / 125μm Brillouin scattering strain-assisted sensing fiber is added between the Raman thermometry multimode sensing fiber and the communication single-mode fiber on one side. All fibers maintain a standard 250μm fiber ribbon pitch, compatible with conventional ribbon fusion splicer fixtures.
[0027] In some specific implementations, the planar integrated fiber ribbon unit 1 employs differentiated excess length control: The excess length of single-mode fiber in the central communication section is 0.02%-0.05%, while the excess length of multimode Raman thermometry fiber on both sides is 0.05%-0.08%. The edge fibers are given a larger excess length to preferentially offset the tensile strain caused by bending and compression.
[0028] In some specific implementations, the gradient-modified thermally conductive and insulating micro-buffered composite layer no longer uses a single-thickness, single-formulation elastomer. With a total thickness of 25-60 μm, it is a two-layer composite structure, including a first buffer sub-layer and a second impedance-regulating sub-layer arranged sequentially from the inside out. The two layers work together to achieve steady-state heat conduction to the Raman temperature-sensing multimode optical fiber, enabling temperature sensing, while simultaneously filtering out high-frequency transient mechanical shocks caused by cabling and laying. Combined with a Brillouin scattering strain-assisted sensing optical fiber to collect actual strain data of the optical cable, the strain data is then used to compensate and decouple the Raman temperature measurement results, distinguishing between true temperature rise and spurious temperature signals caused by external pressure.
[0029] In some specific implementations, the inner side of the Raman thermometric multimode sensing fiber serves as the first buffer sublayer, made of an organosilicon elastomer doped with 5-8 wt% hexagonal boron nitride with a particle size of 50-200 nm and a Shore A hardness of 25-35. This provides stress buffering while also possessing lateral thermal conductivity.
[0030] In some specific embodiments, the outer mating tape encapsulation layer is a second impedance-tuning sublayer, made of an organosilicon-acrylic blend elastomer doped with 2-4 wt% hollow glass microspheres with a particle size of 10-50 μm, and a Shore A hardness of 45-55. This moderately regulates the longitudinal thermal impedance, filtering high-frequency transient mechanical shocks while allowing steady-state environmental heat to penetrate and reach the sensing optical fiber.
[0031] In some embodiments, the substrate encapsulation layer is made of UV-curable acrylic resin compounded with 1-3 wt% nano-silica filler with a particle size of 20-100 nm, and has an overall thickness of 0.4-0.6 mm. The nano-silica improves the dimensional stability of the substrate and reduces fiber ribbon warping under high and low temperature cycling.
[0032] In some embodiments, the thickness of the thermally controlled water-blocking composite transition layer 2 is 0.25-0.4 mm. It is a co-extruded semi-dense microporous structure with a modified EVA matrix and is compounded with superabsorbent polymer (SAP) powder and sheet-like boron nitride thermally conductive filler. Its functions are: to achieve completely dry water blocking without fiber paste; the microporous structure can absorb local minor extrusion deformation of the optical cable; the boron nitride thermally conductive filler establishes a low thermal resistance heat conduction channel from the sheath to the optical fiber ribbon; and it inhibits interlayer delamination at high temperatures to prevent gaps from appearing after long-term thermal aging, which would cause thermal conduction failure.
[0033] In some embodiments, the modified thermally conductive non-metallic composite reinforcing layer 3 is made of multi-strand glass fiber yarn mixed with a small amount of high thermal conductivity aramid chopped fibers (8-12 wt%), with a weaving coverage of 80%-92%. No metal components are used, thus avoiding eddy current interference in strong electromagnetic environments. After weaving, the high tensile modulus of glass fiber is retained, while the radial thermal conductivity of the reinforcing layer is improved. Heat can be rapidly diffused laterally along the reinforcing layer, avoiding heat accumulation in local hot spots. The weaving gaps are slightly interlocked by the outer surface of the thermally controlled water-blocking composite transition layer 2, improving the interlayer bonding force and preventing thermal delamination and slippage.
[0034] In some implementations, the low-smoke halogen-free heat-resistant outer sheath 4 is made of heat-resistant low-smoke halogen-free flame-retardant polyolefin sheath material with a total thickness of 1.4-1.8mm and a long-term working temperature range of -40℃ to 115℃, which is suitable for high-temperature working conditions in energy storage compartments and power tunnels.
[0035] This invention also discloses a method for fabricating an integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure, comprising the following steps: S1. Fabrication of planar integrated fiber ribbon unit 1: Select multiple single-mode communication fibers and at least two Raman multimode sensing fibers; arrange the single-mode communication fibers side-by-side in the center, and arrange the Raman multimode sensing fibers at the left and right edges of the planar integrated fiber ribbon unit 1; a Brillouin scattering strain auxiliary sensing fiber may or may not be added between the Raman multimode sensing fiber and the single-mode communication fiber on one side; all fibers maintain a standard fiber ribbon pitch of 250μm and are coplanarly arranged; control the excess length of the central single-mode communication fiber to 0.02%-0.05. The excess length of the Raman temperature measurement multimode sensing fiber on both sides is controlled to be 0.05%-0.08%. A gradient-modified thermally conductive and insulating micro-buffered composite layer is formed by locally coating the outer side of each Raman temperature measurement multimode sensing fiber and the base-encapsulated layer in two steps: first, a first buffer sub-layer is coated with a thickness of 10-25 μm and thermally cured at 80-120℃ for 30-60 s; then, a second impedance-modifying sub-layer is coated on the outer side of the first buffer sub-layer with a thickness of 15-35 μm and cured at 0.5-1.5 J / cm². 2UV curing is performed; then, a UV-curable acrylic resin with 1-3 wt% and 20-100 nm nano-silica filler is used as the substrate encapsulation layer to integrally cure all coplanarly arranged optical fibers. The thickness of the substrate encapsulation layer is 0.4-0.6 mm, and a two-stage UV curing process is employed. The first-stage UV curing dose is 0.3-0.6 J / cm². 2 The second-stage UV curing dose is 0.8-1.2 J / cm². 2 ; S2, Formation of thermally regulated water-blocking composite transition layer 2: Using modified EVA with a VA content of 15-20wt% as the matrix, it is compounded with 5-10wt% superabsorbent polymer (SAP) powder with a particle size of 10-50μm, 3-8wt% lamellar boron nitride thermally conductive filler with a particle size of 1-10μm, 1-2wt% coupling agent, and 0.5-1wt% antioxidant. The mixture is plasticized and extruded using a twin-screw extruder. The extrusion temperature is controlled as follows: Zone 1 140-150℃, Zone 2 155-165℃, Zone 3 165-175℃, and die head 170-180℃. ℃; During the extrusion process, a supercritical carbon dioxide foaming agent with a pressure of 8-12MPa is injected to control the micropore diameter to be 5-30μm and the porosity to be 15%-35%; The planar integrated fiber ribbon unit 1 obtained in step S1 is passed through the central channel of the co-extrusion die, so that the thermally controlled water-blocking composite transition layer 2 is directly wrapped around the outer periphery of the planar integrated fiber ribbon unit 1 with a coating thickness of 0.25-0.4mm, and no PBT bundle tube and filler rope are set. It is then cooled and shaped in a water bath at 20-30℃. S3, Forming a modified thermally conductive non-metallic composite reinforcing layer 3: Glass fiber yarn with a linear density of 600-1200 tex is blended with 8-12 wt% high thermal conductivity aramid chopped fibers with a linear density of 200-400 tex and a length of 3-6 mm. The blended yarn is then woven onto the outer periphery of the heat-controlled water-blocking composite transition layer 2 obtained in step S2 using a high-speed braiding machine. The braiding coverage is 80%-92%, the braiding pitch is 5-15 mm, and the braiding tension is 2-4 N / spindle, so that the braiding gap is 5-15 μm in place with the outer surface of the heat-controlled water-blocking composite transition layer 2. S4. Forming a low-smoke, halogen-free, heat-resistant outer sheath: A heat-resistant, low-smoke, halogen-free, flame-retardant polyolefin sheath material is selected and compounded with 0.5-1.5wt% of anti-thermal-oxidative aging agent. After drying at 80-90℃ for 2-3 hours, it is extruded and coated onto the outside of the modified thermally conductive non-metallic composite reinforcing layer 3 obtained in step S3 using an extruder. The extrusion temperature is controlled as follows: Zone 1 130-140℃, Zone 2 145-155℃, Zone 3 155-165℃, and die head 160-170℃. The sheath thickness is 1.4-1.8mm. After cooling and shaping in three cooling water tanks at 40-50℃, 25-35℃, and 15-25℃, the cable is wound up to obtain an integrated inductive ribbon optical cable with a thermally conductive, insulating, and micro-buffered structure.
[0036] Example 1
[0037] like Figure 1 As shown, an integrated optical fiber ribbon cable with a thermally conductive and insulating micro-buffered structure includes: a planar integrated optical fiber ribbon unit 1, a thermally controlled water-blocking composite transition layer 2, a modified thermally conductive non-metallic composite reinforcing layer 3, and a low-smoke halogen-free and temperature-resistant outer sheath 4. The planar integrated optical fiber ribbon unit 1 is completely covered by the thermally controlled water-blocking composite transition layer 2, the modified thermally conductive non-metallic composite reinforcing layer 3 is wrapped around the outer periphery of the thermally controlled water-blocking composite transition layer 2, and the low-smoke halogen-free and temperature-resistant outer sheath 4 is extruded and wrapped around the outer side of the modified thermally conductive non-metallic composite reinforcing layer 3.
[0038] Planar integrated fiber ribbon unit 1 is a single integrated planar fiber ribbon. The fibers within planar integrated fiber ribbon unit 1 are arranged coplanarly and are integrally solidified by the ribbon base encapsulation layer.
[0039] The planar integrated fiber ribbon unit 1 includes multiple single-mode communication fibers and two Raman temperature measurement multimode sensing fibers.
[0040] The fiber arrangement rules within the planar integrated fiber ribbon unit 1 are as follows: The single-mode optical fiber for communication is arranged in the middle of the planar integrated optical fiber strip unit 1; Two Raman temperature measurement multimode sensing fibers are respectively arranged at the left and right edges of the planar integrated fiber ribbon unit 1. A Brillouin scattering strain-assisted sensing fiber is arranged between a Raman temperature measurement multimode sensing fiber and a communication single-mode fiber on one side.
[0041] A gradient-modified thermally conductive and insulating micro-buffered composite layer is set between the outer side of each Raman temperature measurement multimode sensing fiber and the base-encapsulated layer.
[0042] The planar integrated fiber ribbon unit 1 has a total of 13 cores. Ten G.652D communication single-mode fibers are placed in the center, and one 50 / 125μm Raman thermometry multimode sensing fiber is placed on each of the left and right edges. A 9 / 125μm Brillouin scattering strain-assisted sensing fiber is added between the Raman thermometry multimode sensing fiber and the communication single-mode fiber on one side. All fibers maintain a standard 250μm fiber ribbon pitch, compatible with conventional ribbon fusion splicer fixtures.
[0043] Planar integrated fiber ribbon unit 1 employs differentiated excess length control: The central communication single-mode fiber has a surplus length of 0.02%, while the Raman temperature measurement multimode sensing fiber on both sides has a surplus length of 0.08%. The edge fibers are given a larger surplus length to preferentially offset the tensile strain caused by bending and compression.
[0044] The gradient-modified thermally conductive and insulating micro-buffered composite layer no longer uses a single-thickness, single-formulation elastomer. With a total thickness of 50 μm, it is a two-layer composite structure, comprising a first buffer sublayer and a second impedance-modulating sublayer arranged sequentially from the inside out. The two layers work together to achieve steady-state heat conduction to the Raman temperature-sensing multimode optical fiber, enabling temperature sensing, while simultaneously filtering out high-frequency transient mechanical shocks from cabling and installation. Combined with a Brillouin scattering strain-assisted sensing optical fiber to collect actual strain data from the optical cable, the strain data is then used to compensate and decouple the Raman temperature measurement results, distinguishing between true temperature rise and spurious temperature signals caused by external pressure.
[0045] The inner side is attached to the Raman temperature measurement multimode sensing fiber as the first buffer sublayer, with a Shore A hardness of 25.
[0046] The outer mating strip base encapsulation layer is the second impedance control sublayer, with a Shore A hardness of 55.
[0047] The thermally controlled water-blocking composite transition layer 2 has a thickness of 0.4 mm and is a co-extruded semi-dense microporous structure. The matrix is modified EVA, compounded with superabsorbent polymer (SAP) powder and sheet-like boron nitride thermally conductive filler. Its functions are: to achieve completely dry water blocking without fiber paste; the microporous structure can absorb local minor extrusion deformation of the optical cable; the boron nitride thermally conductive filler establishes a low thermal resistance heat conduction channel from the sheath to the optical fiber ribbon; and it inhibits interlayer delamination at high temperatures, preventing gaps from appearing after long-term thermal aging and causing thermal conduction failure.
[0048] The modified thermally conductive non-metallic composite reinforcing layer 3 is made of multi-strand glass fiber yarn mixed with a small amount of high thermal conductivity aramid chopped fibers, with a weaving coverage of 92%. It does not use any metal components and avoids eddy current interference in strong electromagnetic environments. After weaving, it retains the high tensile modulus of glass fiber and improves the radial thermal conductivity of the reinforcing layer. Heat can be rapidly diffused laterally along the reinforcing layer, avoiding heat accumulation in local hot spots. The weaving gaps are slightly embedded on the outer surface of the thermally controlled water-blocking composite transition layer 2, which improves the interlayer bonding force and prevents thermal delamination and slippage.
[0049] The low-smoke halogen-free, high-temperature resistant outer sheath 4 is made of high-temperature resistant, low-smoke halogen-free, flame-retardant polyolefin sheath material with a total thickness of 1.4mm. Its long-term working temperature range is -40℃ to 115℃, making it suitable for high-temperature conditions in energy storage compartments and power tunnels.
[0050] A method for fabricating an integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure includes the following steps: S1. Fabrication of planar integrated fiber ribbon unit 1: Multiple single-mode communication fibers and two Raman multimode sensing fibers were selected. The single-mode communication fibers were arranged side-by-side in the center, and the two Raman multimode sensing fibers were arranged at the left and right edges of the planar integrated fiber ribbon unit 1, respectively. A Brillouin scattering strain-assisted sensing fiber was added between the Raman multimode sensing fiber and the single-mode communication fiber on one side. All fibers were arranged coplanarly with a standard fiber ribbon pitch of 250 μm. The excess length of the single-mode communication fiber in the middle was controlled to 0.02%, and the excess length of the Raman multimode sensing fibers on both edges was controlled to 0.08%. A gradient-modified thermally conductive and insulating micro-buffered composite layer was formed by local coating in two steps between the outer side of each Raman multimode sensing fiber and the base layer: first, a first buffer sublayer was coated with a thickness of 25 μm and heat-cured at 120℃ for 30 s; then, a second impedance-modifying sublayer was coated with a thickness of 25 μm on the outer side of the first buffer sublayer and cured at 1.5 J / cm. 2 UV curing was then performed; subsequently, a UV-curable acrylic resin with 3 wt% and 50 nm nano-sized silica filler was used as the substrate encapsulation layer to integrally cure all coplanarly arranged optical fibers. The thickness of the substrate encapsulation layer was 0.4 mm, and a two-stage UV curing process was employed, with the first stage UV curing dose being 0.3 J / cm². 2 The second-stage UV curing dose is 0.8 J / cm². 2 ; S2, Formation of thermally regulated water-blocking composite transition layer 2: Using modified EVA with a VA content of 15wt% as the matrix, 10wt% superabsorbent polymer (SAP) powder with a particle size of 50μm, 8wt% sheet-like boron nitride thermally conductive filler with a particle size of 10μm, 2wt% coupling agent, and 1wt% antioxidant were compounded and plasticized by a twin-screw extruder. The extrusion temperature was controlled as follows: 140℃ in zone 1, 155℃ in zone 2, 165℃ in zone 3, and 170℃ at the die head. During the extrusion process, a supercritical carbon dioxide foaming agent with a pressure of 8MPa was injected to control the micropore diameter to 5μm and the porosity to 15%. The planar integrated fiber ribbon unit 1 obtained in step S1 was passed through the central channel of the co-extrusion die, so that the thermally controlled water-blocking composite transition layer 2 was directly coated on the outer periphery of the planar integrated fiber ribbon unit 1 with a coating thickness of 0.4mm. No PBT bundle tube or filler rope was set. The unit was then cooled and shaped in a 20℃ water bath. S3, Forming a modified thermally conductive non-metallic composite reinforcing layer 3: Glass fiber yarn with a linear density of 600 tex is blended with 12 wt% high thermal conductivity aramid chopped fiber with a linear density of 200 tex and a length of 6 mm. The blended yarn is then woven onto the outer periphery of the heat-controlled water-blocking composite transition layer 2 obtained in step S2 using a high-speed braiding machine. The braiding coverage is 92%, the braiding pitch is 15 mm, and the braiding tension is 4 N / spindle, so that the braiding gap is 5 μm in place with the outer surface of the heat-controlled water-blocking composite transition layer 2. S4. Forming a low-smoke, halogen-free, heat-resistant outer sheath: A heat-resistant, low-smoke, halogen-free, flame-retardant polyolefin sheath material was selected and compounded with 1.5wt% of anti-thermal-oxidative aging agent. After drying at 80℃ for 3 hours, it was extruded and coated onto the outside of the modified thermally conductive non-metallic composite reinforcing layer 3 obtained in step S3 using an extruder. The extrusion temperature was controlled as follows: 130℃ in zone 1, 145℃ in zone 2, 155℃ in zone 3, and 160℃ at the die head. The sheath thickness was 1.4 mm. After cooling and shaping in three cooling water tanks at 50℃, 35℃, and 25℃, the cable was wound up to obtain an integrated inductive ribbon optical cable with a thermally conductive, insulating, and micro-buffered structure.
[0051] Any parts or structures not specifically described in this invention can be made using existing technologies or products, and will not be elaborated upon here.
[0052] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural or procedural transformations made based on the content of the present invention specification, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.
Claims
1. A transducer-integrated ribbon optical cable with a thermally conductive and insulating micro-buffered structure, characterized in that, It includes, from the inside out, the following components arranged sequentially: a planar integrated fiber optic ribbon unit, a thermally modulated water-blocking composite transition layer, a modified thermally conductive non-metallic composite reinforcing layer, and a low-smoke, halogen-free, and temperature-resistant outer sheath.
2. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 1, characterized in that, The planar integrated fiber ribbon unit is a single integrated planar fiber ribbon, in which the fibers are arranged coplanarly and are integrally solidified by the ribbon base encapsulation layer.
3. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 2, characterized in that, The optical fibers in the planar integrated fiber ribbon unit include multiple single-mode communication fibers and Raman temperature measurement multimode sensing fibers, and all fibers maintain a standard fiber ribbon pitch of 250μm. The single-mode optical fiber for communication is arranged in the middle of the planar integrated fiber optic ribbon unit; The Raman temperature measurement multimode sensing fiber is arranged at the two edges of the planar integrated fiber ribbon unit; a gradient modified thermally conductive and insulating micro-buffer composite layer is provided between the outer side of each Raman temperature measurement multimode sensing fiber and the ribbon base encapsulation layer. A Brillouin scattering strain-assisted sensing fiber may or may not be provided between the Raman temperature measurement multimode sensing fiber and the communication single-mode fiber at one edge of the planar integrated fiber ribbon unit.
4. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 3, characterized in that, The planar integrated fiber optic strip unit employs differentiated excess length control: The excess length of single-mode communication fiber in the middle is 0.02%-0.05%, and the excess length of Raman temperature measurement multimode sensing fiber on both sides is 0.05%-0.08%.
5. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 3, characterized in that, The gradient-modified thermally conductive and insulating micro-buffered composite layer has a total thickness of 25-60 μm and is a two-layer composite structure, including a first buffer sub-layer and a second impedance control sub-layer arranged sequentially from the inside to the outside. The first buffer sublayer is attached to the Raman temperature measurement multimode sensing fiber, which is made of an organosilicon elastomer doped with 5-8wt% and 50-200nm nano-hexagonal boron nitride, with a Shore A hardness of 25-35. The second impedance control sublayer is made of an organosilicon-acrylic blend elastomer doped with 2-4 wt% hollow glass microspheres with a particle size of 10-50 μm, and has a Shore A hardness of 45-55.
6. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 2, characterized in that, The substrate encapsulation layer is made of UV-curable acrylic resin with 1-3 wt% nano-silica filler with a particle size of 20-100 nm, and the overall thickness is 0.4-0.6 mm.
7. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 1, characterized in that, The thickness of the thermally regulated water-blocking composite transition layer is 0.25-0.4 mm. It is a co-extruded semi-dense microporous structure with modified EVA as the matrix and compounded with superabsorbent polymer (SAP) powder and sheet-like boron nitride thermally conductive filler.
8. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 1, characterized in that, The modified thermally conductive non-metallic composite reinforcing layer is made of glass fiber yarn and high thermally conductive aramid chopped fiber, with a weaving coverage of 80%-92%.
9. The integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure according to claim 1, characterized in that, The low-smoke halogen-free, heat-resistant outer sheath is made of heat-resistant, low-smoke halogen-free, flame-retardant polyolefin sheath material with a total thickness of 1.4-1.8 mm.
10. A method for preparing an integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure as described in any one of claims 1-9, characterized in that, Includes the following steps: S1. Fabrication of planar integrated fiber ribbon units; S2. A thermally modulated water-blocking composite transition layer is formed by coating the outer periphery of the planar integrated fiber ribbon unit. S3. A modified thermally conductive non-metallic composite reinforcing layer is woven around the outer periphery of the thermally controlled water-blocking composite transition layer; S4. A low-smoke, halogen-free, and temperature-resistant outer sheath is formed by extruding and coating the modified thermally conductive non-metallic composite reinforcing layer to obtain the integrated inductive ribbon optical cable with a thermally conductive and insulating micro-buffered structure.