A high-precision closed-loop controlled laser cutting system and cutting process for tempered glass films

By coordinating the common optical path coaxial sensing module and the closed-loop control module, the problem of insufficient real-time monitoring of thickness and stress in existing tempered film laser cutting systems is solved, realizing dynamic control of stress and thickness, and improving the stability and consistency of cutting quality.

CN123103206APending Publication Date: 2026-11-17JIANGXI WEIDU TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611391255.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-09
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing tempered glass laser cutting systems lack a collaborative sensing mechanism for online thickness detection and real-time stress monitoring. This makes it impossible to dynamically control stress and thickness during the cutting process, leading to edge chipping and micro-cracks in stress concentration areas. Furthermore, the lack of coordinated adjustment between feedforward and feedback control in laser parameter adjustment reduces the stability and consistency of cutting quality.

Method used

A common-path coaxial sensing module is used to measure thickness in front of the focal point and stress behind it. Combined with a thermo-mechanical coupling database module and a closed-loop control module, the thermal parameters of the laser and the focal position of the cutting head are adjusted through a thermo-mechanical coupling mapping model to achieve coordinated closed-loop control of stress and thickness, including coordinated adjustment of feedforward control, feedback control and coupled decision.

Benefits of technology

This method achieves stress gradient convergence within the target range, significantly reducing edge chipping and cracking defects caused by stress concentration, improving the stability and consistency of cutting quality, and increasing cutting yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123103206A_ABST
    Figure CN123103206A_ABST
Patent Text Reader

Abstract

This invention discloses a high-precision closed-loop control laser cutting system and process for tempered glass films, belonging to the field of laser precision machining technology. The system includes a laser cutting module, a coaxial sensing module with a common optical path, a thermo-mechanical coupling database module, and a closed-loop control module. The sensing module collects thickness data in front of the laser focal point and residual stress data behind it. The database module outputs the corresponding stress safety tolerance value based on the thickness. The closed-loop control module adjusts the thermal parameters of the laser and the focal position of the cutting head based on the difference between the residual stress and the safety tolerance value through a thermo-mechanical coupling mapping model, so that the stress gradient converges to the target range determined by the current thickness. This invention achieves coordinated real-time monitoring and look-ahead pre-compensation of thickness and stress, effectively avoiding edge chipping and cracking defects caused by stress concentration, significantly improving cutting accuracy and yield, and is suitable for precision laser cutting of tempered glass films of various thicknesses.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of laser precision machining technology, specifically to a high-precision closed-loop controlled tempered glass film laser cutting system and cutting process. Background Technology

[0002] Laser cutting of tempered glass screen protectors is a crucial process in the production of screen protectors for consumer electronics such as mobile phones and tablets. Currently, tempered glass laser cutting systems typically include a laser, a cutting head, and a motion platform. During the cutting process, the laser outputs a laser beam with specific power and frequency, which is focused by the cutting head and applied to the surface of the tempered glass workpiece. Through the laser's thermal effect, the material vaporizes and separates along a preset trajectory, completing the cutting of irregular contours. To improve cutting quality, some existing systems perform offline thickness sampling inspections on the incoming tempered glass before cutting and manually adjust the focal point position based on the inspection results. Other systems use offline stress testing equipment to sample and inspect the finished product after cutting to evaluate the rationality of the cutting process. Furthermore, a few high-end systems have introduced vision-based cutting trajectory tracking technology and temperature monitoring technology for the cutting area based on temperature sensors, used to assist in adjusting process parameters during the cutting process.

[0003] However, the existing technologies still have the following shortcomings: First, the existing systems lack a collaborative sensing mechanism for online thickness detection and real-time stress monitoring. Thickness detection is limited to offline sampling before cutting, failing to detect thickness tolerance fluctuations in individual tempered film and compensate for focal positions in a timely manner. Stress detection is limited to offline sampling after cutting, unable to acquire residual stress data in real time during the cutting process and dynamically adjust stress safety tolerance values ​​accordingly, resulting in the inability to achieve dynamic control in areas of thickness fluctuation and stress concentration. Second, the existing systems lack a forward-looking pre-compensation function based on the stress distribution of the cut area. Laser parameter adjustments during the cutting process rely solely on the feedback signal at the current moment. When encountering local stress abrupt changes, real-time feedback cannot intervene in advance due to inherent delays, leading to edge chipping and microcrack propagation in stress peak areas. Third, in the existing systems, the thermal parameters of the laser and the adjustment of the cutting head focal position are independent of each other, lacking a collaborative adjustment mechanism of feedforward control and feedback control. Furthermore, the impact of temperature changes in the cutting area on the accuracy of the control model is not considered, reducing the stability and consistency of the cutting quality of tempered film of different thicknesses. Summary of the Invention

[0004] (a) Technical problems to be solved

[0005] To address the shortcomings of existing technologies, this invention provides a high-precision closed-loop control system and process for laser cutting of tempered glass films. The system includes a laser cutting module, a coaxial sensing module with a common optical path, a thermo-mechanical coupling database module, and a closed-loop control module. The sensing module measures the thickness in front of the focal point and the stress behind it. The database module outputs a dynamic stress safety tolerance value based on the thickness. The closed-loop control module adjusts the thermal parameters of the laser and the focal position of the cutting head through a thermo-mechanical coupling mapping model, causing the stress gradient to converge to the target range determined by the current thickness, thus achieving coordinated closed-loop control of stress and thickness during the cutting process.

[0006] (II) Technical Solution

[0007] To achieve the above objectives, the present invention provides the following technical solution: a high-precision closed-loop controlled tempered glass film laser cutting processing system, including a laser cutting module, comprising a laser and a cutting head, for cutting tempered glass film workpieces;

[0008] The coaxial sensing module with a common optical path is fixed in relative position to the cutting head, and includes, along the cutting direction, a thickness detection position located in front of the laser focus and a stress detection position located behind the laser focus; the thickness detection position is used to collect and output the tempered film thickness data of the current cutting area; the stress detection position is used to collect and output the residual stress data of the current cutting area at the moment of cutting completion.

[0009] The thermo-mechanical coupling database module stores thermoelastic mechanical parameters and stress safety tolerance values ​​corresponding to different thicknesses of tempered film, and is used to output the corresponding stress safety tolerance value based on the received thickness data;

[0010] A closed-loop control module, connected to the sensing module, the database module, and the laser cutting module, is used to obtain the corresponding stress safety tolerance value from the database module based on the thickness data, and output a deviation signal based on the difference between the residual stress data and the stress safety tolerance value. The closed-loop control module is also used to adjust the thermal parameters of the laser and the focal position of the cutting head based on the deviation signal using a preset thermo-mechanical coupling mapping model. The thermo-mechanical coupling mapping model takes the thickness data and the deviation signal as input, and outputs the adjustment amounts of the thermal parameters and the focal position. The thermal parameters are the output power of the laser and / or the moving speed of the cutting head.

[0011] Preferably, the thickness detection position is equipped with a laser confocal thickness sensor, and the stress detection position is equipped with a polarized light imaging sensor or a photoelastic sensor; the thickness detection position and the stress detection position share the same optical path, and the distance between them is 0.2 mm to 3 mm.

[0012] Preferably, the thermoelastic mechanical parameters stored in the thermo-mechanical coupling database module include the thermal diffusivity, heat-affected zone width, critical stress intensity factor, and stress relaxation time constant of tempered films of different thicknesses under laser cutting conditions; the stress safety tolerance value is negatively correlated with the thickness data.

[0013] Preferably, the feedforward control submodule is used to determine the basic thermal parameters and reference focus position of the current cutting area through the database module based on the thickness data;

[0014] The feedback control submodule is used to determine the stress deviation ratio based on the residual stress data and the stress safety tolerance value, wherein the stress deviation ratio is the difference between the residual stress data and the stress safety tolerance value divided by the stress safety tolerance value.

[0015] The coupling decision submodule is used to output the adjustment amount of the thermal effect parameter and the adjustment amount of the focal position through the thermo-mechanical coupling mapping model based on the stress deviation ratio.

[0016] Preferably, when the stress deviation ratio is positive, the coupling decision submodule outputs an adjustment command to decrease the thermal effect parameter and move the focal position downward; when the stress deviation ratio is negative, the coupling decision submodule outputs an adjustment command to increase the thermal effect parameter and move the focal position upward; the adjustment amount of the thermal effect parameter and the adjustment amount of the focal position satisfy the mapping relationship of the thermo-mechanical coupling mapping model.

[0017] Preferably, the closed-loop control module further includes a stress field thermal memory unit, which is used to receive continuous stress data collected along the cutting trajectory at the stress detection position and construct stress field distribution data of the cut area. The stress field thermal memory unit predicts the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the thickness data collected at the thickness detection position, and outputs a pre-adjustment command before the laser cutting module reaches the position.

[0018] Preferably, the coaxial sensing module further includes a temperature sensor disposed on the side of the cutting head, used to collect temperature data of the cutting area and output it to the closed-loop control module, wherein the closed-loop control module corrects the thermo-mechanical coupling mapping model based on the temperature data.

[0019] Preferably, the system used as described in any one of claims 1 to 7 includes the following steps:

[0020] S1: Place the tempered glass workpiece on the processing platform and activate the sensing module;

[0021] S2: The closed-loop control module loads the reference parameters from the database module and performs initial calibration on the sensing module;

[0022] S3: Drive the cutting head to move along the preset cutting trajectory, obtain the thickness data in front of the laser focus through the thickness detection position, and obtain the residual stress data behind the laser focus through the stress detection position;

[0023] S4: The closed-loop control module obtains the corresponding stress safety tolerance value from the database module based on the thickness data, and determines the stress deviation ratio based on the residual stress data and the stress safety tolerance value;

[0024] S5: The closed-loop control module adjusts the thermal parameters of the laser and the focal position of the cutting head according to the stress deviation ratio through the thermo-mechanical coupling mapping model;

[0025] S6: Repeat steps S3 to S5 until the cutting trajectory is completed.

[0026] Preferably, step S5 further includes: the closed-loop control module constructs stress field distribution data of the cut area based on the continuous stress data collected along the cutting trajectory from the stress detection position, and predicts the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the forward thickness data collected from the thickness detection position, and outputs a pre-adjustment command before the cutting head reaches the position.

[0027] Preferably, the sampling frequency of the thickness detection position is the same as that of the stress detection position. The sampling data of the two are aligned according to spatial coordinates and then input into the closed-loop control module. The signal delay between the thickness detection position and the stress detection position is equal to the distance between the two divided by the current cutting speed.

[0028] Compared with the prior art, the present invention provides a high-precision closed-loop control tempered glass film laser cutting system and cutting process, which has the following beneficial effects:

[0029] First, this invention collects thickness data in front of the laser focal point and residual stress data behind it using a coaxial sensing module with a common optical path. It then uses a thermo-mechanical coupling database module to output a dynamic stress safety tolerance value based on the thickness. The closed-loop control module adjusts the thermal parameters and focal point position based on the difference between the residual stress and the safety tolerance value, thus achieving coordinated closed-loop control of thickness and stress. This ensures that the stress gradient always converges to the target range determined by the current thickness, effectively avoiding edge chipping and cracking defects caused by stress concentration.

[0030] Secondly, the present invention uses a stress field thermal memory unit to predict the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the thickness data in front, and outputs pre-adjustment instructions in advance to achieve forward-looking pre-compensation. This eliminates the lag defects of traditional real-time feedback and significantly reduces the risk of crack propagation in the cutting of thick tempered film.

[0031] Third, the present invention determines the basic thermal parameters and reference focus position based on the thickness data through the feedforward control submodule, and achieves coordinated adjustment of feedforward and feedback by combining feedback control and coupled decision-making. At the same time, the temperature data collected by the temperature sensor is corrected by mapping model, which effectively suppresses the heat accumulation effect during the cutting process and ensures the stability and consistency of the cutting quality of tempered film of different thicknesses. Attached Figure Description

[0032] Figure 1 This is a schematic diagram of the method steps of the present invention. Detailed Implementation

[0033] The present invention will now be described in detail with reference to the accompanying drawings. It should be understood that the specific embodiments described herein are for illustrative purposes only and are not intended to limit the scope of the invention.

[0034] like Figure 1 As shown, the high-precision closed-loop control tempered glass film laser cutting processing system provided by the present invention mainly includes a laser cutting module, a common optical path coaxial sensing module, a thermo-mechanical coupling database module, and a closed-loop control module.

[0035] The laser cutting module includes a laser and a cutting head. The laser is preferably a nanosecond ultraviolet solid-state laser with a wavelength of 355 nanometers and a beam quality M. 2 The laser beam has a pulse width of less than 25 nanoseconds and a photon energy of less than 1.2 ppm. The high energy of the ultraviolet laser photons allows for direct detachment of molecules from the surface of the tempered glass film, resulting in low thermal effects and minimizing the formation of microcracks during cutting. The cutting head is equipped with a focusing lens assembly to focus the laser beam onto the surface of the tempered glass workpiece. The cutting head can move along three axes: X, Y, and Z.

[0036] The coaxial sensing module with a common optical path is fixed in relative position to the cutting head. Along the cutting direction, it includes a thickness detection position positioned in front of the laser focal point and a stress detection position positioned behind the laser focal point. The thickness detection position is equipped with a laser confocal thickness sensor, and the stress detection position is equipped with a polarized light imaging sensor or a photoelastic sensor. The thickness detection position and the stress detection position share the same optical path, with a distance of 0.2 mm to 3 mm between them. The thickness detection position is used to acquire and output the tempered film thickness data of the current cutting area; the stress detection position is used to acquire and output the residual stress data of the current cutting area at the moment of cutting completion.

[0037] The thermo-mechanical coupling database module stores thermoelastic mechanical parameters and stress safety tolerance values ​​corresponding to different thicknesses of tempered glass films. It is used to output the corresponding stress safety tolerance value based on the received thickness data. The thermoelastic mechanical parameters include the thermal diffusivity, heat-affected zone width, critical stress intensity factor, and stress relaxation time constant of tempered glass films of different thicknesses under laser cutting conditions. The stress safety tolerance value is negatively correlated with the thickness data; that is, the greater the thickness, the smaller the allowable stress safety tolerance value.

[0038] The closed-loop control module is connected to the common-path coaxial sensing module, the thermo-mechanical coupling database module, and the laser cutting module. It retrieves the corresponding stress safety tolerance value from the database module based on the thickness data and outputs a deviation signal based on the difference between the residual stress data and the stress safety tolerance value. The closed-loop control module also adjusts the laser's thermal parameters and the cutting head's focal position based on the deviation signal using a preset thermo-mechanical coupling mapping model. The thermo-mechanical coupling mapping model takes the thickness data and deviation signal as input and outputs the adjustment amounts of the thermal parameters and the focal position. The thermal parameters are the laser's output power and / or the cutting head's moving speed.

[0039] The closed-loop control module comprises a feedforward control submodule, a feedback control submodule, and a coupled decision submodule. The feedforward control submodule determines the basic thermal parameters and reference focal position of the current cutting area based on thickness data via a database module. The feedback control submodule determines the stress deviation ratio based on residual stress data and the stress safety tolerance value; the stress deviation ratio is the difference between the residual stress data and the stress safety tolerance value divided by the stress safety tolerance value. The coupled decision submodule outputs adjustments to the thermal parameters and focal position based on the stress deviation ratio using a thermo-mechanical coupling mapping model. When the stress deviation ratio is positive, the coupled decision submodule outputs an adjustment command to decrease the thermal parameters and move the focal position downwards; when the stress deviation ratio is negative, the coupled decision submodule outputs an adjustment command to increase the thermal parameters and move the focal position upwards. The adjustment amounts of the thermal parameters and the focal position satisfy the mapping relationship of the thermo-mechanical coupling mapping model.

[0040] The closed-loop control module also includes a stress field thermal memory unit, which receives continuous stress data collected along the cutting trajectory from the stress detection position and constructs stress field distribution data of the cut area. The stress field thermal memory unit predicts the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the thickness data collected from the thickness detection position, and outputs a pre-adjustment command before the laser cutting module reaches that position.

[0041] The coaxial sensing module also includes a temperature sensor located on the side of the cutting head, which is used to collect temperature data of the cutting area and output it to the closed-loop control module; the closed-loop control module corrects the thermo-mechanical coupling mapping model based on the temperature data.

[0042] The construction method of the thermo-mechanical coupling mapping model;

[0043] Thermo-mechanical coupling mapping models can be implemented in various ways, including but not limited to lookup table methods, analytical formula methods, or machine learning model methods. The following uses the lookup table method as an example to illustrate its construction process:

[0044] First, cutting experiments were conducted on tempered glass film samples of different thicknesses, including 0.15 mm, 0.20 mm, 0.25 mm, 0.30 mm, 0.33 mm, and 0.40 mm, under fixed baseline process parameters: laser power of 10 watts, cutting speed of 100 mm per second, and focal point set at 0.0 mm. The optimal compensation parameter combination for each thickness sample under different stress deviation ratios was measured through experiments. Based on extensive experimental data, a multidimensional mapping table was established between thickness data, stress deviation ratio, thermal parameter adjustments, and focal point position adjustments.

[0045] The core logic of the mapping table is as follows: When the stress deviation ratio is positive, meaning the measured residual stress is higher than the safety tolerance value for the current thickness, it indicates that excessive heat input has led to stress accumulation. In this case, the thermal parameters need to be reduced and the focal position moved downwards. When the stress deviation ratio is negative, meaning the measured residual stress is lower than the safety tolerance value, it indicates that insufficient heat input may affect the cutting quality. In this case, the thermal parameters need to be increased and the focal position moved upwards. The adjustment amount of the thermal parameters and the adjustment amount of the focal position satisfy the non-linear correspondence in the mapping table.

[0046] During the actual cutting process, the system acquires thickness data and residual stress data in real time, calculates the stress deviation ratio, and then uses the thickness data and stress deviation ratio as an index to look up the corresponding thermal parameter adjustment amount and focal position adjustment amount, thereby driving the laser and cutting head to perform adjustments.

[0047] Example 1

[0048] Purpose of implementation:

[0049] The purpose of this embodiment is to verify the closed-loop control effect of the system of the present invention in the cutting and processing of tempered film of conventional thickness. Specifically, it verifies the collaborative working capability of the thickness detection and stress detection of the coaxial sensing module in the common optical path, and the effectiveness of the closed-loop control module in adjusting the thermal parameters of the laser and the focal position of the cutting head according to the stress deviation ratio through the thermo-mechanical coupling mapping model.

[0050] Implementation System:

[0051] The system configuration used in this embodiment is as follows: The laser cutting module uses a nanosecond ultraviolet solid-state laser with a wavelength of 355 nanometers, a pulse width of 20 nanoseconds, and a beam quality M² of 1.1. The initial focal position of the cutting head is set to 0.10 millimeters below the upper surface of the tempered film. In the coaxial sensing module, the distance between the thickness detection position and the stress detection position is set to 1.0 millimeters. The thickness detection position uses a spectral confocal displacement sensor with a range of 0 to 2 millimeters, an accuracy of ±0.8 micrometers, and a sampling frequency of 40 kHz. The stress detection position uses a pixel polarization camera. The thermo-mechanical coupling database module stores the thermoelastic mechanical parameters and stress safety tolerance value of 85 MPa corresponding to the 0.20 millimeter thickness tempered film. The closed-loop control module is connected to each of the above modules and has a built-in thermo-mechanical coupling mapping model with thickness data and deviation signals as inputs and thermal effect parameter adjustment and focal position adjustment as outputs. The closed-loop control module includes a feedforward control submodule, a feedback control submodule, and a coupling decision submodule.

[0052] In this embodiment, a tempered glass workpiece with a thickness of 0.20 mm is placed on the processing platform. After the system starts, the closed-loop control module loads the reference parameters from the database module and completes the initial calibration of the coaxial sensing module. The cutting head moves along the preset cutting trajectory. The thickness detection position collects the thickness data in front of the laser focus in real time, and the stress detection position collects the residual stress data behind the laser focus in real time. During the cutting process, the thickness detection position measures the current thickness data as 0.198 mm, and the stress detection position measures the residual stress data as 92 MPa. The closed-loop control module obtains the corresponding stress safety tolerance value of 85 MPa from the database module based on the thickness data of 0.198 mm. The difference between the residual stress data of 92 MPa and the stress safety tolerance value of 85 MPa is 7 MPa. The feedback control submodule divides this difference by the stress safety tolerance value of 85 MPa to obtain a stress deviation ratio of approximately 0.082, which is a positive value. The coupling decision submodule, based on the positive stress deviation ratio, outputs an adjustment command through the thermo-mechanical coupling mapping model: reducing the laser power from 10 watts to 9.2 watts, and simultaneously moving the focal point position from 0.10 mm below the upper surface of the tempered film to 0.13 mm. After adjustment, the residual stress in the next set of detection data drops to 84 MPa. The difference between the residual stress data of 84 MPa and the stress safety tolerance value of 85 MPa is -1 MPa. The feedback control submodule divides this difference by the stress safety tolerance value of 85 MPa to obtain a stress deviation ratio of approximately -0.012, and the system enters a stable cutting state. Throughout the cutting process, the system continuously collects thickness and stress data at a sampling frequency of 40 kHz. The signal delay between the thickness detection position and the stress detection position is equal to the distance between them of 1.0 mm divided by the current cutting speed of 100 mm per second, i.e., 10 milliseconds. The sampled data is input into the closed-loop control module after being aligned according to spatial coordinates.

[0053] Implementation results:

[0054] After cutting, microscopic inspection revealed that the chipped edge size of the cut surface was less than 15 micrometers, with no visible microcracks, achieving a cutting yield of 98.5%. This embodiment verifies the effectiveness of the collaborative operation of thickness detection and stress detection in the coaxial sensing module with the common optical path. It also confirms the feasibility of the closed-loop control module adjusting the thermal parameters of the laser and the focal position of the cutting head based on the stress deviation ratio through a thermo-mechanical coupling mapping model. This demonstrates that the system of this invention can effectively suppress chipping and cracking defects in the cutting of tempered glass films of conventional thicknesses through collaborative closed-loop control of thickness detection and stress detection.

[0055] Example 2

[0056] Purpose of implementation:

[0057] The purpose of this embodiment is to verify the effect of the look-ahead pre-compensation function of the stress field thermal memory unit in the system of the present invention on the cutting quality of tempered film with a large thickness. Specifically, it verifies the effectiveness of the stress field thermal memory unit in predicting the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the thickness data collected at the thickness detection position, and outputting a pre-adjustment command before the cutting head reaches the position.

[0058] Implementation System:

[0059] The system configuration used in this embodiment is as follows: the laser cutting module is the same as in embodiment 1; in the coaxial sensing module with common optical path, the distance between the thickness detection position and the stress detection position is set to 2.5 mm; the thermo-mechanical coupling database module stores the thermoelastic mechanical parameters and stress safety tolerance value of 65 MPa corresponding to the 0.33 mm thick tempered film; in addition to the feedforward control submodule, feedback control submodule and coupling decision submodule, the closed-loop control module also includes a stress field thermal memory unit.

[0060] In this embodiment, a tempered glass workpiece with a thickness of 0.33 mm is placed on a processing platform. The initial laser power is 14 watts, the cutting speed is 80 mm per second, and the initial focal position is set to 0.16 mm below the upper surface of the tempered glass. During the cutting process, the thickness detection position measures the preceding thickness sequence data as follows: 0.332 mm, 0.335 mm, 0.328 mm, and 0.330 mm. The stress detection position collects continuous stress data along the cutting trajectory and outputs it to the stress field thermal memory unit. Based on the stress field distribution data of the cut area and the preceding thickness sequence data, the stress field thermal memory unit predicts that a stress peak may occur in the subsequent approximately 2 mm path. The predicted stress value is approximately 78 MPa, exceeding the safety tolerance of 65 MPa by approximately 20%. The closed-loop control module outputs a pre-adjustment command approximately 1.5 mm before the cutting head reaches the predicted position: gradually reducing the laser power from 14 watts to 12.5 watts, and simultaneously moving the focal position from 0.16 mm below the upper surface of the tempered glass to 0.20 mm. When the cutting head reached the predicted position, the measured peak residual stress was 67 MPa, close to the safety tolerance of 65 MPa, and no edge chipping or crack propagation occurred.

[0061] Implementation results:

[0062] The chipping size of the cut surface was controlled within 18 micrometers, and the cutting yield reached 97.8%. In contrast, if the system lacked a stress field thermal memory unit, relying solely on real-time feedback without look-ahead pre-compensation, the adjustment was only triggered after the measured stress reached 79 MPa at the stress peak position, and microcracks approximately 35 micrometers wide had already appeared on the cut surface. This embodiment verifies the effectiveness of the look-ahead pre-compensation function of the stress field thermal memory unit, demonstrating that predicting the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the preceding thickness data, and outputting pre-adjustment commands in advance, significantly improves the cutting quality of thicker tempered glass films.

[0063] Example 3

[0064] Purpose of implementation:

[0065] The purpose of this embodiment is to verify the adaptive capability of the system of the present invention to thickness fluctuations in the cutting and processing of thin tempered glass films. Specifically, it verifies that the feedforward control submodule determines the basic thermal parameters and reference focus position of the current cutting area through the database module based on the thickness data, as well as the collaborative control effect of the feedback control submodule and the coupled decision submodule.

[0066] Implementation System:

[0067] The system configuration used in this embodiment is as follows: the laser cutting module is the same as in embodiment 1; in the coaxial sensing module with common optical path, the distance between the thickness detection position and the stress detection position is set to 0.3 mm; the thermo-mechanical coupling database module stores the thermoelastic mechanical parameters and stress safety tolerance value of 105 MPa corresponding to the 0.15 mm thick tempered film; in the closed-loop control module, the feedforward control submodule determines the basic thermal parameters and reference focal position of the current cutting area through the database module based on the thickness data, the feedback control submodule determines the stress deviation ratio based on the residual stress data and the stress safety tolerance value, and the coupling decision submodule outputs the thermal parameter adjustment amount and the focal position adjustment amount through the thermo-mechanical coupling mapping model based on the stress deviation ratio.

[0068] In this embodiment, a tempered glass workpiece with a thickness of 0.15 mm is placed on a processing platform. The initial laser power is 6 watts, the cutting speed is 150 mm per second, and the initial focal position is set to 0.07 mm below the upper surface of the tempered glass. During the cutting process, the system detects fluctuations in the thickness data, varying between 0.148 mm and 0.153 mm. The feedforward control submodule dynamically adjusts the basic thermal parameters based on the real-time thickness data: when the thickness is 0.148 mm, the basic power is adjusted to 5.8 watts; when the thickness is 0.153 mm, the basic power is adjusted to 6.3 watts. Simultaneously, the feedback control submodule continuously calculates the stress deviation ratio based on the residual stress data, and the coupled decision submodule outputs fine-tuning instructions based on this. Due to the thinness of the tempered glass, the thermal accumulation effect is significant. In the region where the thickness jumps from 0.148 mm to 0.153 mm, the system detects that the stress deviation ratio increases from -0.05 to +0.09. The coupled decision submodule, based on the stress deviation ratio of +0.09, outputs a linkage adjustment through the thermo-mechanical coupling mapping model: the power is reduced from 6.3 watts to 5.6 watts, and the focal position is moved from 0.07 mm below the upper surface of the tempered film to 0.09 mm. After adjustment, the stress deviation ratio returns to +0.02. The sampling frequency of the thickness detection position and the stress detection position remains the same, both at 40 kHz. The sampling data from both are aligned according to spatial coordinates and input into the closed-loop control module. The signal delay is equal to the distance between the two positions of 0.3 mm divided by the current cutting speed of 150 mm per second, i.e., 2 milliseconds.

[0069] Implementation results:

[0070] After cutting, the tempered glass film with a thickness of 0.15 mm was inspected, and the chipped edge size of the cut surface was less than 12 micrometers, with no cracks, and the cutting yield reached 99.2%. This embodiment verifies the effectiveness of the feedforward control submodule in determining the basic thermal parameters and reference focal position based on the thickness data through the database module, indicating that the synergistic effect of feedforward control and feedback control enables the system of this invention to have good adaptability to thickness fluctuations in the cutting of thin tempered glass films.

[0071] Comparative example;

[0072] The comparative example uses the same tempered glass workpiece as in Example 1, with a thickness of 0.20 mm, and employs the same laser as in Example 1. However, the cutting system used lacks the common-path coaxial sensing module, thermo-mechanical coupling database module, and closed-loop control module described in this invention. Specifically, the missing technical features of this cutting system are reflected in the following three aspects:

[0073] Firstly, it lacks online thickness detection and adaptive focus compensation. This cutting system only performs an offline thickness check before cutting, and the focus position remains fixed during the cutting process. It cannot detect thickness fluctuations in the tempered glass film material between 0.195 mm and 0.205 mm and adjust the focus position accordingly.

[0074] Secondly, it features stress-free real-time monitoring and feedback control. This cutting system does not collect residual stress data during the cutting process, does not make any parameter adjustments based on the stress state, and cannot detect or intervene in stress concentrations generated during the cutting process.

[0075] Third, a non-thermal-mechanical coupling mapping model. The laser power and cutting speed of this cutting system are set empirically before cutting and remain unchanged during the cutting process. The laser power is fixed at 10 watts, the cutting speed is fixed at 100 millimeters per second, and the focal position is fixed at 0.10 millimeters below the upper surface of the tempered film.

[0076] The comparative cutting process is as follows: the tempered glass workpiece is placed on the processing platform, the cutting head moves along the preset cutting trajectory, and the laser cuts the tempered glass film with a fixed power and a fixed focal position until the entire cutting trajectory is completed. There is no real-time detection or parameter adjustment during the entire process.

[0077] The results of the comparative study were as follows: In the thinner region, specifically at a thickness of 0.195 mm, the fixed focal point position resulted in a relatively lower focal point, increasing the heat-affected zone and causing slight overheating on the cut surface; in the thicker region, specifically at a thickness of 0.205 mm, the fixed focal point position resulted in a relatively higher focal point, insufficient cutting depth, and burrs on the cut surface. More seriously, due to the lack of real-time stress monitoring, the system could not intervene in time when local stress concentration exceeded the material's critical value. Microscopic examination after cutting revealed that the chipped edges of the cut samples ranged from 35 to 60 micrometers, and some samples showed obvious microcracks at the corners of the cutting trajectory, with crack lengths ranging from 50 to 120 micrometers. The cutting yield was only 82.3%.

[0078] A comparison of Example 1 and the comparative example shows that, under the same tempered glass workpiece and laser conditions, the present invention achieves online thickness detection and real-time stress monitoring through a coaxial sensing module with a common optical path, provides dynamic stress safety tolerance values ​​through a thermo-mechanical coupling database module, and achieves correlation adjustment between thermal parameters and focal point position through a closed-loop control module. This reduces the chipping size from 35-60 micrometers in the comparative example to below 15 micrometers, and increases the cutting yield from 82.3% to over 98.5%, while effectively preventing the generation and propagation of microcracks. The above comparative results fully demonstrate the significant advancement and practical value of the present invention.

[0079] System working process;

[0080] The working process of the high-precision closed-loop control tempered glass film laser cutting processing system of the present invention will be described in detail below with reference to the accompanying drawings.

[0081] After the tempered glass workpiece is placed on the processing platform, the platform uses vacuum adsorption to fix the workpiece, ensuring that it does not shift during the cutting process. The coaxial sensing module enters standby mode after power-on, while the laser confocal thickness sensor at the thickness detection position and the polarized light imaging sensor at the stress detection position begin preheating and enter preparation mode.

[0082] The closed-loop control module loads the reference parameters from the thermo-mechanical coupling database module and performs initial calibration on the common-path coaxial sensing module. Specifically, the closed-loop control module reads the theoretical thickness value of the current batch of tempered glass film and corresponding thermoelastic mechanical parameters, stress safety tolerance values, and other reference data from the database module. Subsequently, the thickness detection position and stress detection position are zeroed: background signals are collected as a zero-point reference in the absence of a workpiece, and range calibration is performed in the presence of a standard thickness sample to ensure the accuracy of the detection data.

[0083] The cutting head moves along a preset cutting trajectory, acquiring thickness data in front of the laser focus at the thickness detection position and residual stress data behind the laser focus at the stress detection position. The cutting head moves in the XY plane according to the preset cutting trajectory, which can be rectangular, rounded rectangular, or irregularly shaped opening trajectory. The thickness detection position is located in front of the laser focus, completing the thickness measurement at that position before the laser reaches it; the stress detection position is located behind the laser focus, completing the residual stress measurement at that position immediately after the laser leaves it. The spatial distance between the thickness detection position and the stress detection position is known, and the time delay between them can be calculated using the current cutting speed, ensuring strict temporal alignment of the sampled data.

[0084] The closed-loop control module retrieves the corresponding stress safety tolerance value from the thermo-mechanical coupling database module based on the thickness data, and determines the stress deviation ratio based on the residual stress data and the stress safety tolerance value. Specifically, after receiving the thickness data, the closed-loop control module queries the database module using the thickness data as an index to obtain the stress safety tolerance value for the current thickness. Subsequently, it compares the measured residual stress data with the stress safety tolerance value and calculates the stress deviation ratio, which is the difference between the residual stress data and the stress safety tolerance value divided by the stress safety tolerance value.

[0085] The closed-loop control module adjusts the laser's thermal parameters and the cutting head's focal position based on the stress deviation ratio using a thermo-mechanical coupling mapping model. A positive stress deviation ratio indicates that the measured residual stress exceeds the safety tolerance, posing a risk of edge chipping or crack propagation. In this case, the system outputs an adjustment command to reduce the thermal parameters and lower the focal position. Conversely, a negative stress deviation ratio indicates insufficient heat input, potentially affecting cutting quality. In this case, the system outputs an adjustment command to increase the thermal parameters and raise the focal position. The adjustment amounts of the thermal parameters and the focal position satisfy a nonlinear mapping relationship within the thermo-mechanical coupling mapping model.

[0086] At the same time, the stress field thermal memory unit constructs stress field distribution data of the cut area based on the continuous stress data collected along the cutting trajectory from the stress detection position, and predicts the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the thickness data collected from the thickness detection position. Before the cutting head reaches the position, it outputs a pre-adjustment command to achieve look-ahead pre-compensation.

[0087] The above process continues in a loop until all cutting trajectories are completed. During the cutting process, the sampling frequency of the thickness detection position and the sampling frequency of the stress detection position remain the same. The sampling data from both are strictly aligned according to spatial coordinates before being input into the closed-loop control module. The entire cutting process forms a complete closed loop of detection, comparison, decision-making, adjustment, and re-detection, ensuring that each cutting trajectory is completed under optimal process parameters.

[0088] After cutting, the processing platform releases vacuum adsorption, removes the cut tempered glass film, and moves it to the next station for further processing.

[0089] The high-precision closed-loop control tempered glass screen protector laser cutting system and cutting process provided by this invention can be widely applied to precision laser cutting of tempered glass screen protectors for mobile phones, tablets, and smart wearable devices. Compared with existing technologies, this invention achieves online thickness detection and real-time stress monitoring through a common-path coaxial sensing module, provides dynamic stress safety tolerance values ​​through a thermo-mechanical coupling database module, and realizes the correlation adjustment and look-ahead pre-compensation of thermal parameters and focal position through a closed-loop control module. This significantly improves cutting accuracy and yield, effectively reduces cutting defects such as edge chipping and micro-cracks, and has broad industrial application prospects and significant economic benefits.

[0090] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A high-precision closed-loop control system for laser cutting of tempered glass films, characterized in that, Includes a laser cutting module, comprising a laser and a cutting head, for cutting tempered glass workpieces; The coaxial sensing module with a common optical path is fixed in relative position to the cutting head, and includes, along the cutting direction, a thickness detection position located in front of the laser focus and a stress detection position located behind the laser focus; the thickness detection position is used to collect and output the tempered film thickness data of the current cutting area; the stress detection position is used to collect and output the residual stress data of the current cutting area at the moment of cutting completion. The thermo-mechanical coupling database module stores thermoelastic mechanical parameters and stress safety tolerance values ​​corresponding to different thicknesses of tempered film, and is used to output the corresponding stress safety tolerance value based on the received thickness data; A closed-loop control module, connected to the sensing module, the database module, and the laser cutting module, is used to obtain the corresponding stress safety tolerance value from the database module based on the thickness data, and output a deviation signal based on the difference between the residual stress data and the stress safety tolerance value; the closed-loop control module is also used to adjust the thermal parameters of the laser and the focal position of the cutting head based on the deviation signal through a preset thermo-mechanical coupling mapping model. The thermo-mechanical coupling mapping model takes the thickness data and the deviation signal as inputs, and the adjustment amount of the thermal effect parameters and the adjustment amount of the focal position as outputs; the thermal effect parameters are the output power of the laser and / or the moving speed of the cutting head.

2. The high-precision closed-loop control tempered glass film laser cutting system according to claim 1, characterized in that: The thickness detection position is equipped with a laser confocal thickness sensor, and the stress detection position is equipped with a polarized light imaging sensor or a photoelastic sensor; the thickness detection position and the stress detection position share the same optical path, and the distance between them is 0.2 mm to 3 mm.

3. The high-precision closed-loop control tempered glass film laser cutting system according to claim 1, characterized in that: The thermoelastic mechanical parameters stored in the thermo-mechanical coupling database module include the thermal diffusivity, heat-affected zone width, critical stress intensity factor, and stress relaxation time constant of tempered films of different thicknesses under laser cutting conditions; the stress safety tolerance value is negatively correlated with the thickness data.

4. The high-precision closed-loop control tempered glass film laser cutting system according to claim 1, characterized in that: The feedforward control submodule is used to determine the basic thermal parameters and reference focus position of the current cutting area based on the thickness data through the database module. The feedback control submodule is used to determine the stress deviation ratio based on the residual stress data and the stress safety tolerance value, wherein the stress deviation ratio is the difference between the residual stress data and the stress safety tolerance value divided by the stress safety tolerance value. The coupling decision submodule is used to output the adjustment amount of the thermal effect parameter and the adjustment amount of the focal position through the thermo-mechanical coupling mapping model based on the stress deviation ratio.

5. The high-precision closed-loop control tempered glass film laser cutting system according to claim 4, characterized in that: When the stress deviation ratio is positive, the coupling decision submodule outputs an adjustment command to reduce the thermal effect parameter and move the focal position downward; When the stress deviation ratio is negative, the coupled decision submodule outputs an adjustment command to increase the thermal effect parameter and move the focal position upward; the adjustment amount of the thermal effect parameter and the adjustment amount of the focal position satisfy the mapping relationship of the thermo-mechanical coupling mapping model.

6. The high-precision closed-loop control tempered glass film laser cutting system according to claim 1, characterized in that: The closed-loop control module also includes a stress field thermal memory unit, which is used to receive continuous stress data collected along the cutting trajectory at the stress detection position and construct stress field distribution data of the cut area. The stress field thermal memory unit predicts the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the thickness data collected at the thickness detection position, and outputs a pre-adjustment command before the laser cutting module reaches the position.

7. The high-precision closed-loop controlled tempered glass film laser cutting system according to claim 1, characterized in that: The coaxial sensing module with common optical path also includes a temperature sensor disposed on the side of the cutting head, used to collect temperature data of the cutting area and output it to the closed-loop control module, and the closed-loop control module corrects the thermo-mechanical coupling mapping model based on the temperature data.

8. A high-precision closed-loop controlled laser cutting process for tempered glass films, characterized in that: The system as described in any one of claims 1 to 7 comprises the following steps: S1: Place the tempered glass workpiece on the processing platform and activate the sensing module; S2: The closed-loop control module loads the reference parameters from the database module and performs initial calibration on the sensing module; S3: Drive the cutting head to move along the preset cutting trajectory, obtain the thickness data in front of the laser focus through the thickness detection position, and obtain the residual stress data behind the laser focus through the stress detection position; S4: The closed-loop control module obtains the corresponding stress safety tolerance value from the database module based on the thickness data, and determines the stress deviation ratio based on the residual stress data and the stress safety tolerance value; S5: The closed-loop control module adjusts the thermal parameters of the laser and the focal position of the cutting head according to the stress deviation ratio through the thermo-mechanical coupling mapping model; S6: Repeat steps S3 to S5 until the cutting trajectory is completed.

9. The high-precision closed-loop controlled tempered glass film laser cutting process according to claim 8, characterized in that: Step S5 further includes: the closed-loop control module constructs stress field distribution data of the cut area based on the continuous stress data collected along the cutting trajectory at the stress detection position, and predicts the stress peak position on the subsequent cutting path based on the stress field distribution data of the cut area and the forward thickness data collected at the thickness detection position, and outputs a pre-adjustment command before the cutting head reaches the position.

10. The high-precision closed-loop controlled laser cutting process for tempered glass films according to claim 9, characterized in that: The sampling frequency of the thickness detection position is the same as that of the stress detection position. The sampling data of the two are input into the closed-loop control module after being aligned with spatial coordinates. The signal delay between the thickness detection position and the stress detection position is equal to the distance between the two divided by the current cutting speed.