A method for processing microstructures of hard and brittle materials and structural components
By employing a three-dimensional collaborative method involving buffered entry structure, continuous smooth trajectory, and smooth feed rate control in the microstructure machining of hard and brittle materials, the problems of edge chipping and dimensional deviation caused by dynamic cutting impact in the microstructure machining of hard and brittle materials have been solved, achieving high-quality and high-precision machining results.
Patent Information
- Application Number
- CN202611385030.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-08
- Publication Date
- 2026-11-17
AI Technical Summary
In the manufacturing of core components for high-end equipment such as semiconductor etching machines, hard and brittle materials such as silicon are prone to edge chipping, hidden cracks and dimensional deviations during the microstructure processing. Existing processing technology lacks systematic control over the dynamic mechanical behavior during the cutting process, resulting in unstable surface quality and difficulty in guaranteeing dimensional accuracy.
A cutting tool with a buffered entry structure is used to cut hard and brittle materials along a continuous and smooth trajectory. The feed rate is smoothly controlled in the curvature change region. Combined with high-order kinematic curve planning and micro-lubrication and cooling, a three-dimensional synergistic anti-impact system is constructed to suppress dynamic cutting impact.
It significantly improves the surface quality and dimensional consistency of microstructures, ensuring the processing integrity and precision of hard and brittle materials, and meeting the performance requirements of high-end equipment.
Smart Images

Figure CN123103887A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor precision manufacturing technology, specifically to a method for processing microstructures of hard and brittle materials and structural components. Background Technology
[0002] In the manufacturing of core components for high-end equipment such as semiconductor etching machines, hard and brittle materials like silicon, due to their high hardness and low toughness, are prone to defects such as edge chipping, hidden cracks, and dimensional deviations during the machining of microstructures (such as narrow grooves and grids). Existing machining processes typically focus on single-dimensional optimization, such as only considering the wear resistance of the tool material or only adjusting cutting parameters, lacking systematic control over the dynamic mechanical behavior during cutting. Specifically, when the tool cuts into hard and brittle materials or runs in areas of abrupt curvature change (such as corners), the local stress concentration caused by the tool geometry, the step of cutting force caused by the discontinuity of the cutting trajectory, and the motion overshoot caused by the inertia of the machine tool feed mechanism combine to form a strong dynamic cutting impact. This impact exceeds the fracture toughness threshold of hard and brittle materials, resulting in unstable surface quality and difficulty in ensuring contour accuracy, severely restricting the yield and reliability of high-performance semiconductor silicon components. Therefore, there is an urgent need for a machining method for hard and brittle materials that can effectively suppress dynamic cutting impact while maintaining surface integrity and dimensional accuracy. Summary of the Invention
[0003] To address the problems of edge chipping, hidden cracks, and dimensional deviations caused by dynamic cutting impact in the machining of microstructures of hard and brittle materials in existing technologies, this application proposes a machining method and structural component for microstructures of hard and brittle materials. This method achieves the combined suppression of micro-stress, macro-cutting force, and motion inertia during the cutting process, thereby improving the surface quality and dimensional consistency of the microstructure.
[0004] To achieve the above objectives, this application adopts the following technical solution: A method for machining microstructures of hard and brittle materials includes: using a cutting tool with a buffered entry structure to cut the microstructures of the hard and brittle material along a continuous smooth trajectory, so that the cutting tool smoothly enters the hard and brittle material and maintains continuous cutting contact; and in the curvature abrupt change region of the continuous smooth trajectory, smoothly controlling the feed rate of the cutting tool to suppress the inertial overcutting and cutting force step of the cutting tool in the curvature abrupt change region.
[0005] The above solution weakens the transient impact load acting on hard and brittle materials from the source through the three-dimensional coordination of tool geometry buffering, continuous trajectory transition and kinematic smooth control, and avoids material damage and contour distortion caused by stress concentration and inertial overshoot.
[0006] In one implementation, the buffered entry structure includes a preset rounded corner or blunt edge on the cutting edge of the cutting tool; the continuous smooth trajectory includes a helical entry trajectory or a tangential transition trajectory, so that the cutting tool smoothly enters the machining boundary of the microstructure along the helical entry trajectory or the tangential transition trajectory.
[0007] This implementation transforms point contact into surface contact by modifying the geometry of the cutting edge, thus dispersing the local pressure at the moment of entry. Combined with a spiral or tangential trajectory, it achieves a gradual increase in cutting thickness, eliminating the rigid impact during vertical entry and further reducing the risk of edge chipping.
[0008] In one implementation, the radius of the pre-set fillet is in the range of 0.05 mm to 0.2 mm, and the surface roughness Ra value of the cutting tool is less than 0.2 μm; the helix angle of the helical entry trajectory is in the range of 10° to 30°, and the ratio of the single-turn cutting depth of the helical entry trajectory to the diameter of the cutting tool is in the range of 5% to 15%; during the cutting process along the helical entry trajectory, the axial feed of the cutting tool remains constant, and the radial depth of cut of the cutting tool decreases layer by layer according to a pre-set decreasing ratio; when the cutting tool cuts to the bottom surface of the microstructure, the radial depth of cut decreases to zero, so as to form a smooth transition cutting texture at the junction of the sidewall and the bottom surface of the microstructure.
[0009] This implementation method ensures the effectiveness of the buffering effect by matching the fracture mechanical properties of hard and brittle materials through a refined parameter window; in particular, the strategy of decreasing the radial depth of cut to zero avoids residual stress and step marks at the bottom interface, ensuring the geometric integrity and surface smoothness of the bottom of the microstructure.
[0010] As one implementation method, the feed rate of the cutting tool is smoothly controlled in the curvature abrupt region of a continuous smooth trajectory, including: obtaining the real-time curvature radius of the continuous smooth trajectory; when the real-time curvature radius is less than a preset curvature threshold, reducing the feed rate of the cutting tool according to a preset deceleration strategy; when the real-time curvature radius is greater than or equal to the preset curvature threshold, restoring the feed rate of the cutting tool according to a preset acceleration strategy.
[0011] This implementation establishes an adaptive speed adjustment mechanism based on trajectory geometry features, which dynamically matches the feed speed with the path curvature, preventing trajectory deviation and overcutting caused by insufficient centripetal force or servo lag at sharp turns.
[0012] As one implementation method, reducing the feed rate of the cutting tool according to a preset deceleration strategy includes: determining a target deceleration ratio based on the difference between the real-time radius of curvature and a preset curvature threshold; generating a smooth speed planning curve using an S-shaped acceleration / deceleration curve or an exponential acceleration / deceleration curve according to the target deceleration ratio; controlling the feed mechanism of the cutting tool to perform a deceleration action according to the smooth speed planning curve so that the rate of change of acceleration of the feed rate remains within a preset impact threshold range; and restoring the feed rate of the cutting tool according to a preset acceleration strategy, including: when the real-time radius of curvature recovers to a value greater than or equal to the preset curvature threshold, and the current position of the cutting tool deviates from the curvature abrupt change region by a distance greater than a preset safety distance, performing an acceleration action according to the smooth speed planning curve to restore the initial feed rate.
[0013] This implementation method limits the abrupt rate of acceleration through high-order kinematic curve planning, eliminating the flexible impact during speed switching; at the same time, it introduces a safety distance criterion to ensure the stability of the speed recovery phase and avoid damage to the processed surface by secondary vibration.
[0014] In one implementation, the base material of the cutting tool is tungsten steel, and the surface of the cutting tool is coated with a diamond coating or a titanium nitride coating; the spindle speed of the cutting tool ranges from 15,000 r / min to 30,000 r / min, and the cutting depth ranges from 0.01 mm to 0.1 mm; during the cutting process, a micro-lubrication cooling method is used to cool the contact area between the cutting tool and the hard and brittle material, and the lubricating oil flow rate of the micro-lubrication cooling method ranges from 5 ml / h to 20 ml / h.
[0015] This implementation creates a physical environment suitable for high-speed precision machining of hard and brittle materials. The combination of high wear-resistant coating and high rotation speed suppresses abrasive wear, while micro-lubrication removes cutting heat and avoids thermal shock damage to silicon materials caused by traditional liquid cooling, ensuring the long-term stability of the process system.
[0016] In addition, this application also provides a microstructure of a hard and brittle material, including a microgrid structure, which is formed by processing the microstructure of a hard and brittle material using the processing method described above; the surface roughness Ra value of the sidewall of the microgrid structure is less than 0.4 μm, and the edge of the microgrid structure is free from chipping and hidden crack defects.
[0017] Thanks to the comprehensive suppression of dynamic cutting impact by the aforementioned processing method, the above-mentioned structural components possess excellent surface integrity and dimensional accuracy, and can meet the stringent performance requirements of high-end equipment such as semiconductor etching machines for core silicon components. Beneficial effects
[0018] The method and structural components for machining microstructures of hard and brittle materials provided in this application effectively solve the dynamic damage problem in the micromachining of hard and brittle materials by constructing a three-dimensional collaborative anti-impact system of "tool micro-geometry - macro-toolpath trajectory - machine tool kinematic control". Specifically, the tool with a buffered entry structure disperses the stress concentration in the contact area between the cutting edge and the workpiece at the micro level, reducing the driving force for brittle fracture; the continuous smooth trajectory ensures the continuous transition of cutting force at the macro level, avoiding the force step impact caused by abrupt changes in cutting thickness; and the smooth control of the feed rate in the curvature change region suppresses the inertial overcut and servo oscillation of the machine tool feed mechanism at the kinematic level, eliminating the additional dynamic load caused by the speed change. The three are closely coupled in the spatiotemporal dimension, jointly controlling the transient impact energy during the machining process within the safe threshold of hard and brittle materials, thereby significantly improving the sidewall surface quality, edge integrity, and dimensional consistency of the microstructure, providing a reliable process guarantee for the high-yield manufacturing of high-performance semiconductor silicon components. Attached Figure Description
[0019] Figure 1 This is a flowchart of a method for processing microstructures of hard and brittle materials according to an embodiment of this application. Detailed Implementation
[0020] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this application. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.
[0021] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application.
[0022] Example 1
[0023] like Figure 1 As shown, this embodiment provides a method for processing microstructures of hard and brittle materials. This method achieves comprehensive suppression of dynamic cutting impacts during processing by constructing a three-dimensional collaborative mechanism of micro-geometry, macro-trajectory, and kinematic control. The processing method mainly includes the following steps.
[0024] In step S100, a cutting tool 1 with a buffered entry structure is used to cut the fine structure of the hard and brittle material along a continuous and smooth trajectory, so that the cutting tool 1 smoothly enters the hard and brittle material and maintains continuous cutting contact.
[0025] Specifically, a buffered entry structure refers to a non-sharp transition shape formed by specific geometric modification or blunting of the cutting edge of the cutting tool 1. Its core function is to change the mechanical boundary conditions at the moment of contact between the tool and the workpiece. In the machining of hard and brittle materials, sharp cutting edges are prone to generating extremely high local stress concentration at the moment of entry, inducing brittle fracture. The buffered entry structure effectively disperses the entry load and reduces the peak pressure per unit area by transforming point or line contact into surface contact with a certain area, thereby weakening the driving force of edge chipping and hidden cracks from the source. At the same time, a continuous and smooth trajectory means that the movement path of the cutting tool 1 relative to the workpiece remains geometrically continuous and differentiable, without any tangential abrupt change or normal step. This trajectory design ensures the gradual loading of cutting thickness and cutting force, avoiding the rigid impact caused by the instantaneous switching of cutting states in traditional vertical entry or broken line paths. It should be understood that the buffered entry structure and the continuous smooth trajectory constitute a spatiotemporal coupling relationship in this step: the former alleviates the contact stress at the microscale, while the latter ensures the continuity of load transmission at the macroscale. The two work together to enable the cutting tool 1 to enter the interior of the hard and brittle material in a flexible manner and maintain a stable cutting contact state.
[0026] In step S200, the feed rate of the cutting tool 1 is smoothly controlled in the curvature abrupt region of the continuous smooth trajectory to suppress the inertial overcut and cutting force step of the cutting tool 1 in the curvature abrupt region.
[0027] Specifically, curvature abrupt change regions refer to sections in a continuous smooth trajectory where the radius of curvature changes significantly and the rate of change exceeds a preset threshold, such as corner transitions or narrow slot ends in micro-grid structures. In these regions, if the machine tool feed mechanism maintains a constant speed, the actual trajectory will deviate from the theoretical trajectory due to the lag in the servo system's response and the inertia of the mechanical transmission chain—a phenomenon known as inertial overcutting. This is fatal for micro-structures with extremely high dimensional accuracy requirements. Furthermore, the abrupt change in curvature itself can cause a rapid deflection between the cutting direction and the force direction; if the speeds are mismatched, it will trigger severe fluctuations in cutting force. The feed speed smoothing control in this step is not a simple deceleration or pause, but an adaptive adjustment mechanism based on trajectory geometry and machine tool dynamics. This mechanism intervenes in speed planning before the curvature abrupt change, keeping the rate of change of feed speed (i.e., the rate of change of acceleration) within a safe threshold that both the hard, brittle material and the machine tool system can withstand, thereby eliminating the soft impact during speed switching. In this way, not only is the precise tracking capability of the cutting tool 1 at complex contours guaranteed, but secondary damage to the machined surface caused by sudden changes in motion state and fluctuations in cutting force is also avoided.
[0028] Through the coordinated execution of steps S100 and S200, this embodiment establishes a complete dynamic cutting impact suppression system. The buffered entry structure solves the micro-stress problem of "difficult entry," the continuous smooth trajectory solves the macro-load problem of "stable cutting," and the smooth control of the feed rate in the curvature abrupt change region solves the kinematic inertia problem of "accurate steering." The three work closely together throughout the machining process to control the transient impact energy acting on the microstructure of hard and brittle materials within a safe range, thereby significantly improving the integrity and dimensional accuracy of the machined surface and effectively overcoming the shortcomings of existing technologies where a single method cannot simultaneously achieve both quality and efficiency.
[0029] Example 2
[0030] Based on Example 1, this embodiment further defines the specific form and parameters of the buffered entry structure and the continuous smooth trajectory. As one implementation, the buffered entry structure includes a preset rounded corner or blunted edge on the cutting edge of the cutting tool 1; the continuous smooth trajectory includes a helical entry trajectory or a tangential transition trajectory, so that the cutting tool 1 smoothly enters the machining boundary of the microstructure along the helical entry trajectory or tangential transition trajectory. Specifically, considering the characteristics of hard and brittle materials—low fracture toughness and extreme sensitivity to stress concentration—the cutting edge of the cutting tool 1 is designed with a preset rounded corner or blunted edge, which can geometrically change the contact state between the cutting edge and the workpiece. Compared to the extremely high local pressure generated by a sharp cutting edge, the rounded corner or blunted edge transforms instantaneous point or line contact into surface contact with a certain width, effectively dispersing the impact load at the moment of entry and reducing the driving force that induces brittle fracture. Simultaneously, using a helical entry trajectory or tangential transition trajectory instead of the traditional vertical entry method allows the cutting thickness to gradually increase from zero, avoiding rigid impacts caused by sudden changes in cutting force and ensuring the mechanical stability of the cutting tool 1 when entering the machining boundary. It should be understood that although this embodiment lists two forms, helical entry and tangential transition, in other embodiments, any continuous curved trajectory that can achieve gradual loading of cutting load can be used as an equivalent substitute, as long as it meets the functional requirements of smooth entry.
[0031] To further adapt to the precision machining requirements of hard and brittle materials, this embodiment also refines the above-mentioned geometric and trajectory parameters. As one implementation method, the preset fillet radius ranges from 0.05mm to 0.2mm, and the surface roughness Ra value of the cutting tool 1 is less than 0.2μm; the helix angle of the helical entry trajectory ranges from 10° to 30°, and the ratio of the single-turn cutting depth of the helical entry trajectory to the diameter of the cutting tool 1 ranges from 5% to 15%. Within this parameter window, the selection of the preset fillet radius is based on a balance between buffering effect and cutting resistance: when the radius is less than 0.05mm, the cutting edge is still too sharp, making it difficult to effectively alleviate the risk of edge chipping in hard and brittle materials; while when the radius is greater than 0.2mm, the wedging effect of the cutting edge weakens, and the squeezing effect strengthens, which can easily lead to squeezing and crushing or subsurface damage to the material surface. Controlling the surface roughness Ra value of the cutting edge below 0.2μm aims to reduce the coefficient of friction and heat accumulation during the cutting process, and reduce the initiation of microcracks induced by the thermo-mechanical coupling effect. For helical entry trajectories, a helix angle range of 10° to 30° ensures sufficient axial force for chip removal while avoiding a decrease in tool radial rigidity due to excessive helix angle. Limiting the ratio of single-turn cutting depth to diameter to 5% to 15% ensures that the cutting load per revolution is within the safe removal threshold for hard and brittle materials, preventing macroscopic cracking caused by excessive single-turn cutting depth.
[0032] Furthermore, to address the issue of residual stress and chipping at the junction of the bottom and sidewalls of microstructures, this embodiment employs a special depth-of-cut control strategy. As one implementation method, during cutting along the helical entry trajectory, the axial feed of the cutting tool 1 remains constant, and the radial depth of cut of the cutting tool 1 decreases layer by layer according to a preset decreasing ratio. When the cutting tool 1 reaches the bottom surface of the microstructure, the radial depth of cut decreases to zero, thus forming a smooth transition cutting texture at the junction of the sidewall and bottom surface of the microstructure. Specifically, this radial depth-of-cut decreasing strategy is essentially a "soft landing" machining mechanism. In traditional constant depth-of-cut machining, when the tool approaches the bottom end point, a small residual triangular area is often left at the junction of the sidewall and bottom surface. The material in this area is highly susceptible to chipping due to uneven stress release during subsequent machining or tool retraction. By proportionally decreasing the radial depth of cut with the axial feed, the radial cutting allowance of the cutting tool 1 approaches zero at the instant it reaches the bottom elevation, thus geometrically eliminating residual steps and mechanically achieving smooth unloading of cutting forces. This treatment not only ensures the dimensional accuracy and contour integrity of the bottom of the microstructure but also significantly improves the continuity of surface texture at the interface, preventing abrupt changes in machining marks from becoming sources of crack propagation in subsequent use.
[0033] Example 3
[0034] Based on Example 1, this example further defines the specific implementation logic for smooth control of feed rate in the curvature abrupt change region of a continuous smooth trajectory. As one implementation method, smooth control of the feed rate of the cutting tool 1 in the curvature abrupt change region of a continuous smooth trajectory includes: acquiring the real-time curvature radius of the continuous smooth trajectory; when the real-time curvature radius is less than a preset curvature threshold, reducing the feed rate of the cutting tool 1 according to a preset deceleration strategy; when the real-time curvature radius is greater than or equal to the preset curvature threshold, restoring the feed rate of the cutting tool 1 according to a preset acceleration strategy. Specifically, this control strategy constructs an adaptive speed adjustment closed loop based on trajectory geometry features. In the machining of microstructures of hard and brittle materials, the curvature radius of the trajectory directly reflects the degree of drastic change in the cutting direction. By obtaining the real-time curvature radius through real-time calculation or pre-reading of trajectory data and comparing it with a preset curvature threshold, the system can identify high-risk sections that may cause inertial overcutting or a surge in cutting force in advance. When the real-time radius of curvature is less than the preset curvature threshold, it indicates that the tool is about to enter or is in a region of sudden curvature change, such as a sharp turn or a small arc. If the original speed is maintained at this time, the servo lag and mechanical inertia of the machine tool feed mechanism will cause the actual motion trajectory to deviate from the theoretical path, resulting in overcutting or contour distortion. Therefore, the system automatically triggers a deceleration strategy to match the feed speed with the current path's throughput capacity. Conversely, when the tool leaves the high-risk section and the real-time radius of curvature returns to a safe range, the system triggers an acceleration strategy to restore machining efficiency. This dynamic speed regulation mechanism based on geometric features fundamentally solves the problem that constant feed or simple segmented speed changes cannot adapt to complex and fine contours, ensuring the mechanical stability and geometric accuracy of the cutting process.
[0035] To further eliminate transient shocks during speed switching, this embodiment employs high-order kinematic planning for the execution of deceleration and acceleration strategies. As one implementation method, reducing the feed rate of the cutting tool 1 according to a preset deceleration strategy includes: determining a target deceleration ratio based on the difference between the real-time radius of curvature and a preset curvature threshold; generating a smooth speed planning curve using an S-shaped or exponential acceleration / deceleration curve according to the target deceleration ratio; and controlling the feed mechanism of the cutting tool 1 to perform a deceleration action according to the smooth speed planning curve, so that the rate of change of acceleration of the feed rate remains within a preset impact threshold range. Specifically, the target deceleration ratio is not a fixed value, but a variable that dynamically changes with the degree of curvature deviation. The smaller the radius of curvature, the greater the deceleration amplitude, thereby achieving a precise speed response to path difficulty. More importantly, this application abandons the abrupt acceleration pattern in traditional trapezoidal acceleration / deceleration and instead adopts an S-shaped or exponential acceleration / deceleration curve. The S-curve, by introducing a finite constraint on jerk (i.e., the rate of change of acceleration, Jerk), ensures that the acceleration itself is continuously changing, avoiding the soft impact caused by acceleration abrupt changes. The exponential curve, on the other hand, utilizes its natural decay characteristics to make the velocity transition more rounded. For hard and brittle materials, even a small abrupt change in acceleration can excite high-frequency vibration modes in the machine tool structure, thereby leaving vibration marks on the working surface or inducing subsurface cracks. By strictly limiting the rate of change of acceleration within a preset impact threshold range, this embodiment cuts off the transmission path of vibration excitation at the kinematic source, ensuring the extreme smoothness of the cutting tool 1 during speed change.
[0036] Furthermore, to address the risk of secondary damage that may occur during the speed recovery phase, this embodiment introduces a spatial position criterion as a safety barrier. As one implementation method, the feed rate of the cutting tool 1 is restored according to a preset acceleration strategy, including: when the real-time radius of curvature recovers to a value greater than or equal to a preset curvature threshold, and the current position of the cutting tool 1 deviates from the curvature abrupt change region by a distance greater than a preset safety distance, an acceleration action is performed according to a smooth speed planning curve to restore the initial feed rate. Specifically, relying solely on the recovery of the radius of curvature as an acceleration trigger condition is insufficient, because after the machine tool system has just completed deceleration and turning, its mechanical transmission chain may still retain incompletely dissipated elastic potential energy or minor vibrations. If acceleration is immediately performed at this time, the new driving force will be superimposed with the residual vibrations, easily forming visible tool marks or ripples on the machined surface. The preset safety distance essentially provides a physical "calming buffer" for the system, ensuring that the tool is completely removed from the curvature abrupt change region and the system's dynamic response tends to a steady state before the speed is smoothly increased. This design effectively avoids secondary vibration damage caused by premature acceleration, ensuring consistent surface quality across the entire contour of the microstructure.
[0037] To more clearly illustrate the actual operation of the above control strategy, the following example is taken for machining a micro-grid corner. In this scenario, when the cutting tool 1 approaches the grid corner along a straight line, the system monitors in real time that the radius of curvature of the trajectory gradually decreases. When the radius of curvature drops below a preset curvature threshold (e.g., 0.05 mm), the control system calculates the need to reduce the feed rate from 2000 mm / min to 400 mm / min based on the difference between the current radius of curvature and the threshold, and then generates an S-shaped speed planning curve. The feed mechanism of the cutting tool 1 strictly follows this curve to reduce the speed. The acceleration changes continuously throughout the deceleration process without any abrupt changes, thus avoiding tool chatter caused by rapid deceleration. When the cutting tool 1 completes the corner transition and continues to travel along the straight line, although the radius of curvature of the trajectory has returned to infinity (straight line), the system does not accelerate immediately. Instead, it waits for the tool to move forward beyond a preset safety distance (e.g., 0.2 mm) before smoothly restoring the feed rate to 2000 mm / min again according to the S-shaped curve. It should be understood that although this example uses an S-curve and specific values, in other implementations, exponential curves or other higher-order polynomial curves may also be used. The specific values of the preset curvature threshold and safety distance may also be adaptively adjusted according to the type of hard and brittle material, the stiffness of the tool and the dynamic performance of the machine tool. As long as it can achieve smooth speed planning with controlled acceleration change rate and safety buffer function, it falls within the protection scope of this application.
[0038] Example 4
[0039] Based on Examples 1 to 3, this example further defines the process environment configuration supporting the above-mentioned dynamic cutting impact suppression method. As one implementation, the base material of the cutting tool 1 is cemented carbide or tungsten steel, and the surface of the cutting tool 1 is coated with a diamond coating or a titanium nitride coating; the spindle speed of the cutting tool 1 ranges from 15000 r / min to 30000 r / min, and the cutting depth ranges from 0.01 mm to 0.1 mm; during the cutting process, a micro-lubrication cooling method is used to cool the contact area between the cutting tool 1 and the hard and brittle material, and the lubricating oil flow rate of the micro-lubrication cooling method ranges from 5 ml / h to 20 ml / h.
[0040] Specifically, the effective execution of the buffered entry structure and feed rate smoothing control strategy in the aforementioned embodiments highly depends on a stable physical machining environment. Considering the high hardness and poor thermal conductivity of brittle materials, the cutting tool 1 is made of cemented carbide or tungsten carbide as the base material, providing sufficient elastic modulus and bending strength to ensure that the tool body does not undergo significant tool deformation at high speeds, thereby maintaining the shape accuracy of the micro-geometric buffer structure. Furthermore, the surface-coated diamond or titanium nitride layer not only significantly improves the wear resistance of the cutting edge and extends the effective life of the tool in microstructure machining, but more importantly, it improves the tribological properties and thermal conductivity of the tool surface, reducing the penetration of cutting heat into the workpiece and lowering the risk of subsurface damage due to heat accumulation. It should be understood that although this embodiment lists diamond and titanium nitride as two preferred coatings, in other embodiments, any coating system with high hardness, low coefficient of friction, and low chemical affinity to brittle materials can be used as an equivalent substitute.
[0041] Regarding motion parameters, setting the spindle speed within the high-speed range of 15,000 r / min to 30,000 r / min, combined with a micro-cutting depth of 0.01 mm to 0.1 mm, is a key combination for suppressing abrasive wear and brittle fracture in hard and brittle materials. High spindle speeds significantly increase the number of cuts per unit time. While maintaining the same material removal rate, the thickness of a single cut is extremely compressed, resulting in a cutting force peak below the critical fracture load of hard and brittle materials. This promotes a shift in the material removal mechanism from brittle fragmentation to plastic shear or quasi-ductile modes. Simultaneously, the small cutting depth limits the spatial scale of crack initiation and propagation, preventing macroscopic edge chipping. If the spindle speed is below 15,000 r / min, the single-tooth cutting load increases, easily inducing low-frequency vibration and edge breakage; if the cutting depth exceeds 0.1 mm, it exceeds the rigidity limit of the micro-tool and the ductile removal threshold of hard and brittle materials, leading to a sharp deterioration in machining quality.
[0042] Furthermore, considering the extreme sensitivity of hard and brittle materials to temperature gradients, this embodiment employs a specific micro-volume lubrication cooling strategy. The lubricating oil flow rate is strictly controlled within the range of 5 ml / h to 20 ml / h, forming a high-pressure, two-phase gas mist that is precisely sprayed onto the cutting zone. Compared to traditional high-flow-rate liquid cooling, this micro-volume lubrication method avoids thermal shock cracks caused by drastic temperature differences in the coolant on hard and brittle materials such as silicon, and overcomes the problems of rapid tool wear and workpiece thermal burns caused by poor heat dissipation in dry cutting. The flow rate window of 5 ml / h to 20 ml / h is a balance point determined based on extensive process verification: too low a flow rate is insufficient to remove cutting heat and establish an effective lubricating film, while too high a flow rate will cause localized cold sources due to excessively rapid droplet impact and evaporation heat absorption, introducing new thermal stress risks. Through the synergistic configuration of the tool material, motion parameters, and cooling method, this embodiment constructs a robust physical environment suitable for high-speed precision machining of hard and brittle materials, providing the necessary material basis and process guarantee for the implementation of the aforementioned dynamic cutting impact suppression strategy.
[0043] Example 5
[0044] This embodiment provides a microstructure of a hard and brittle material, comprising a microgrid structure, which is formed by processing the microstructure of a hard and brittle material using the processing method described in any one of embodiments 1 to 4 above. Specifically, this embodiment extends the protected object from the processing method to the end product directly obtained by the method. In the field of semiconductor precision manufacturing, simple method patents often face difficulties in obtaining evidence when determining infringement, because the processing is usually completed in a closed factory and leaves no trace; while product patents can be asserted by reverse engineering commercially available or competing components. By establishing a direct causal link between the aforementioned processing method, which includes a buffered cutting structure, a continuous smooth trajectory, and smooth control of the feed speed in the curvature abrupt region, and the final product, this embodiment constructs a complete closed loop for supply chain protection. It should be understood that although this embodiment uses a microgrid structure as an example, in other embodiments, any hard and brittle material component with microchannels, arrayed holes, or thin-walled features prepared using the above processing method falls within the scope of protection of this application, and is not limited to a specific geometric shape or application carrier.
[0045] As a key performance characteristic, the Ra value of the sidewall surface roughness of the micro-grid structure is less than 0.4 μm. This quantitative indicator is not simply a numerical limitation, but a direct mapping of the aforementioned three-dimensional collaborative anti-impact processing mechanism to the micro-morphology. In the actual working conditions of high-end equipment such as semiconductor etching machines, the micro-smoothness of the silicon component surface directly affects the uniformity of the plasma flow field and particle adsorption behavior. If the sidewall roughness is too large, it will not only aggravate the local electric field distortion, leading to uneven etching rate, but also become a source of accumulation of reaction byproducts, thereby contaminating the wafer. In the prior art, due to the processing characteristics of hard and brittle materials, even with subsequent polishing, the Ra value of the sidewall in conventional milling or grinding processes is usually maintained in the range of 0.6 μm to 1.0 μm, and it is difficult to guarantee the uniformity of areas with large depth-to-width ratios. This application achieves the removal of the quasi-ductile domain from the source by using tool geometry to buffer and disperse contact stress, helical trajectory to eliminate cutting force steps, and S-shaped speed planning to suppress inertial vibration, resulting in a mirror-like smooth texture on the processed surface. Actual test data show that the Ra value of the sidewall of the microgrid processed by the method of this application is stably controlled below 0.4 μm, and some preferred samples can even reach the 0.2 μm level, which is significantly better than the traditional process level, thus meeting the stringent requirements of advanced processes for the surface integrity of core components.
[0046] Furthermore, the edges of the micro-grid structure are free from chipping and microcracks. Edge integrity is another core dimension for evaluating the quality of micro-machining of hard and brittle materials, and a key factor determining the service life and reliability of components. Specifically, "free from chipping" means that under optical or scanning electron microscopy, the edge contours of the micro-grid are continuous and smooth, without any serrated defects, conchoidal fractures, or macroscopic peeling visible to the naked eye or at low magnification; "free from microcracks" means that, as confirmed by staining penetration or ultrasonic non-destructive testing, no microcrack network induced by processing stress remains in the edge region and subsurface. In traditional machining methods, due to the lack of systematic suppression of dynamic cutting impacts, stress concentration at the moment of tool entry and inertial overcutting at corners can easily induce damage at the edges of brittle materials. These damages are often hidden, gradually expanding and failing only during subsequent cleaning, assembly, or thermal cycling. The product of this application benefits from the fact that the transient impact energy during processing is strictly limited within the material's fracture toughness threshold, and its edge region maintains an intact lattice structure and mechanical strength. This superior edge integrity not only improves the appearance yield of products, but more importantly, it eliminates potential fatigue crack sources, ensuring the dimensional stability and functional reliability of hard and brittle microstructures under long-term harsh operating conditions, providing a solid material foundation for the high-performance operation of semiconductor equipment.
[0047] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.
Claims
1. A method for processing the microstructure of a hard and brittle material, characterized in that, include: A cutting tool with a buffered entry structure is used to cut the fine structure of a hard and brittle material along a continuous and smooth trajectory, so that the cutting tool smoothly enters the hard and brittle material and maintains continuous cutting contact; In the curvature abrupt change region of the continuous smooth trajectory, the feed rate of the cutting tool is smoothly controlled to suppress the inertial overcutting and cutting force step of the cutting tool in the curvature abrupt change region.
2. The method for processing the microstructure of hard and brittle materials according to claim 1, characterized in that, The buffer cutting structure includes a preset rounded corner or blunted edge on the cutting edge of the cutting tool; The continuous smooth trajectory includes a helical infeed trajectory or a tangential transition trajectory, so that the cutting tool smoothly cuts into the machining boundary of the microstructure along the helical infeed trajectory or the tangential transition trajectory.
3. The method for processing the microstructure of hard and brittle materials according to claim 2, characterized in that, The radius of the preset fillet is in the range of 0.05mm to 0.2mm, and the surface roughness Ra value of the cutting tool is less than 0.2μm; The helix angle of the helical entry trajectory ranges from 10° to 30°, and the ratio of the single-turn cutting depth of the helical entry trajectory to the diameter of the cutting tool ranges from 5% to 15%. During the cutting process along the spiral cutting trajectory, the axial feed of the cutting tool remains constant, and the radial depth of cut of the cutting tool decreases layer by layer according to a preset decreasing ratio; when the cutting tool cuts to the bottom surface of the microstructure, the radial depth of cut decreases to zero, so as to form a smooth transition cutting texture at the junction of the sidewall and the bottom surface of the microstructure.
4. The method for processing the microstructure of hard and brittle materials according to claim 1, characterized in that, The step of smoothly controlling the feed rate of the cutting tool in the curvature abrupt change region of the continuous smooth trajectory includes: Obtain the real-time radius of curvature of the continuous smooth trajectory; When the real-time radius of curvature is less than the preset curvature threshold, the feed rate of the cutting tool is reduced according to the preset deceleration strategy; When the real-time radius of curvature is greater than or equal to the preset curvature threshold, the feed rate of the cutting tool is restored according to the preset acceleration strategy.
5. The method for processing the microstructure of hard and brittle materials according to claim 4, characterized in that, The step of reducing the feed rate of the cutting tool according to a preset deceleration strategy includes: The target deceleration ratio is determined based on the difference between the real-time radius of curvature and the preset curvature threshold. Based on the target deceleration ratio, a smooth speed planning curve is generated using an S-shaped acceleration / deceleration curve or an exponential acceleration / deceleration curve. The feed mechanism of the cutting tool is controlled to perform a deceleration action according to the smooth speed planning curve, so that the rate of change of the acceleration of the feed speed is kept within a preset impact threshold range; The step of restoring the feed rate of the cutting tool according to the preset acceleration strategy includes: when the real-time radius of curvature is restored to a value greater than or equal to the preset curvature threshold, and the current position of the cutting tool is deviated from the curvature abrupt change region by a distance greater than the preset safety distance, performing an acceleration action according to the smooth speed planning curve to restore the initial feed rate.
6. The method for processing the microstructure of hard and brittle materials according to claim 1, characterized in that, The base material of the cutting tool is cemented carbide or tungsten steel, and the surface of the cutting tool is coated with a diamond coating or a titanium nitride coating. The spindle speed range of the cutting tool is 15,000 r / min to 30,000 r / min, and the cutting depth range is 0.01 mm to 0.1 mm. During the cutting process, a micro-lubrication cooling method is used to cool the contact area between the cutting tool and the hard and brittle material. The flow rate of the lubricating oil in the micro-lubrication cooling method ranges from 5 ml / h to 20 ml / h.
7. A microstructure component made of a hard and brittle material, characterized in that, It includes a micro-grid structure, which is formed by processing a micro-structure of a hard and brittle material using the processing method described in any one of claims 1 to 6; The surface roughness Ra of the sidewall of the microgrid structure is less than 0.4 μm, and the edges of the microgrid structure are free from chipping and hidden cracks.