A chelating agent, a photovoltaic module cleaning agent and its preparation method
By designing a ternary mixed coordination field with PASP-Cys chelating agent, the selectivity of existing photovoltaic module cleaning agents for Ca, Mg and Si ions is solved, achieving efficient cleaning and protection of photovoltaic modules and maintaining stable module performance.
Patent Information
- Application Number
- CN202611304893.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-17
AI Technical Summary
Existing photovoltaic module cleaning agents lack selectivity for Ca, Mg, and Si ions during the cleaning process, leading to changes in the refractive index of the AR coating and an irreversible decrease in light transmittance. Furthermore, strongly alkaline or acidic cleaning agents corrode photovoltaic glass and aluminum alloy frames.
Using PASP-Cys chelating agent, a ternary mixed coordination field of O, N and S is constructed by introducing cysteine-grafted modified polyaspartic acid to achieve selective chelation of Ca2+/Mg2+, reduce the complexation competition for Si4+, and form an Al-S passivation layer on the aluminum frame surface to protect the AR coating.
While effectively cleaning the surface of photovoltaic modules, it protects the AR coating, maintains stable refractive index and light transmittance, reduces the attack on SiO2, and significantly improves the cleaning effect and module performance.
Smart Images

Figure CN123106492A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of photovoltaic module cleaning agents, and in particular to a chelating agent, a photovoltaic module cleaning agent, and a method for preparing the same. Background Technology
[0002] As global photovoltaic (PV) installed capacity continues to grow, the demand for cleaning and maintenance of PV modules is also increasing. Problems such as hot spot effects caused by dust, bird droppings, oil stains, and inorganic salt deposits on the module surface, leading to a decline in power generation efficiency, are becoming increasingly prominent. Currently, most general-purpose industrial cleaning agents used in PV power plant cleaning are strongly alkaline (pH>12) or strongly acidic formulas. Although they have strong cleaning power, they can corrode the porous SiO2 antireflection film on the surface of PV glass and the aluminum alloy frame.
[0003] To address this, some photovoltaic cleaning agents containing aminocarboxylic acid chelating agents have been developed. For example, existing technology CN103589522A discloses an alkaline photovoltaic silicon wafer cleaning agent, whose formulation includes DTPA (diethylenetriaminepentaacetic acid) as a chelating agent. DTPA belongs to the traditional aminocarboxylic acid chelating agents, and its biodegradability is extremely poor (the 28-day biodegradation rate is usually <20%), which contradicts the green attributes of photovoltaic power plants. Moreover, cleaning agents containing DTPA lack selectivity for Ca, Mg, and Si ions, which can easily lead to changes in the refractive index of AR coatings and an irreversible decrease in light transmittance. Summary of the Invention
[0004] To address the shortcomings of current cleaning agents used for cleaning and maintenance of photovoltaic products, especially in-service photovoltaic modules, which lack selectivity for Ca, Mg, and Si ions and easily lead to changes in the refractive index and irreversible decrease in transmittance of AR coatings, the present invention aims to provide a chelating agent that achieves selective chelation of calcium and magnesium ions while reducing the complexation competition for silicon ions. This effectively cleans the surface of photovoltaic modules while better protecting the AR coating and maintaining stable performance such as refractive index and transmittance.
[0005] Another object of the present invention is to provide a method for preparing a chelating agent.
[0006] Another object of the present invention is to provide a photovoltaic module cleaning agent.
[0007] Another object of the present invention is to provide a method for preparing a photovoltaic module cleaning agent.
[0008] Firstly, this invention protects a chelating agent with the following chemical structural formula: , Where x = 0 - 0.7, y = 0.3 - 0.8, z = 0.3 - 0.8.
[0009] Secondly, the present invention also specifically protects a method for preparing a chelating agent, comprising the following steps: S1. Polysuccinimide of Formula I was prepared by thermal polycondensation of L-aspartic acid; S2. Polysuccinimide was reacted with L-cysteine via a nucleophilic ring-opening reaction to prepare the cysteine-grafted polyaspartic acid intermediate shown in Formula II. S3. Hydrolyze the cysteine-grafted polyaspartic acid intermediate to obtain the chelating agent; Formula I, m / n = 0.3-0.8.
[0010] According to the preparation method of the chelating agent protected by the present invention, preferably, the thermal polycondensation reaction in S1 is carried out under vacuum conditions, the reaction temperature is 185-195°C, and the reaction time is 4-6 hours.
[0011] According to the method for preparing the chelating agent protected by the present invention, preferably, the reaction temperature of the nucleophilic ring-opening reaction in S2 is 40-60°C, the reaction time is 12-18h, and the molar ratio of polysuccinimide to L-cysteine is 1:0.3-0.8.
[0012] According to the method for preparing the chelating agent protected by the present invention, preferably, the hydrolysis reaction temperature in S3 is 50-60°C, the reaction time is 2-3 h, and the reaction pH is 9-10.
[0013] Thirdly, the present invention also specifically protects a photovoltaic module cleaning agent, including the above-mentioned chelating agent.
[0014] According to the photovoltaic module cleaning agent protected by the present invention, preferably, the pH value of the photovoltaic module cleaning agent is 7.8-8.5.
[0015] The photovoltaic module cleaning agent protected according to the present invention preferably comprises, by weight, the following components: 4-11 parts of surfactant, 3-11 parts of composite chelating agent, 2-6 parts of penetrating solvent, and 1-4 parts of pH buffer. The composite chelating agent is a mixture of the chelating agent and the auxiliary chelating agent according to claim 1, with a mass ratio of 1-8:1, preferably 2-3:1; Preferably, the auxiliary chelating agent is selected from any one of sodium citrate, sodium gluconate, sodium polyacrylate, and sodium ethylenediamine di-o-phenylacetate.
[0016] According to the photovoltaic module cleaning agent protected by the present invention, preferably, the surfactant is a mixture of nonionic surfactant and anionic surfactant, and the mass ratio of nonionic surfactant to anionic surfactant is 1-8:1, preferably 2-3:1; More preferably, the nonionic surfactant is selected from any one of fatty alcohol polyoxyethylene ether or alkyl glycoside, and the anionic surfactant is sodium fatty acid methyl ester sulfonate.
[0017] Thirdly, the present invention also specifically protects a method for preparing a photovoltaic module cleaning agent, comprising the following steps: The composite chelating agent was prepared into an aqueous solution and heated to 40-45℃. A surfactant was added while stirring, and the temperature was lowered to 30-35℃. The remaining components were added, and the pH value was adjusted. The solution was allowed to stand and defoam to obtain the photovoltaic module cleaning agent.
[0018] Beneficial effects: This invention provides a PASP-Cys chelating agent that, by introducing cysteine-grafted modified polyaspartic acid, constructs a ternary mixed coordination field of O, N, and S, thereby achieving molecular-level control of Ca. 2+ / Mg 2+ Selective chelation, while significantly reducing Si 4+ Its coordination competition ability allows the thiol group of its cysteine side chain to form an Al-S passivation layer on the aluminum frame surface, providing better protection for photovoltaic modules.
[0019] The photovoltaic module cleaning agent prepared by the PASP-Cys chelating agent of this invention achieves dual protection through selective chelation mechanism and precise control of weak alkalinity, resulting in transmittance damage of AR coating ≤0.3%, H62 brass ≤0.5mg, and LY12 hard aluminum corrosion ≤2.0mg. Furthermore, through the synergistic effect of surfactant system, modified chelating agent and penetrating solvent, it achieves a removal rate of over 95% for simulated bird droppings and a decontamination rate of over 93% for comprehensive stains, demonstrating excellent surface cleaning effect. Attached Figure Description
[0020] To more clearly illustrate the technical solutions in this invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this invention. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.
[0021] Figure 1 This is an infrared characterization diagram of the PASP-Cys chelating agent of the present invention. Detailed Implementation
[0022] To make the objectives, technical solutions, and advantages of this invention clearer, the technical solutions of this invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of this invention, not all embodiments. Based on the embodiments of this invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this invention.
[0023] In a specific embodiment, the present invention provides a chelating agent with the following chemical structural formula: , Where x = 0 - 0.7, y = 0.3 - 0.8, z = 0.3 - 0.8.
[0024] It should be noted that: The above structural formula only shows the types of structural units contained in the polymer, and does not represent that the structural units are arranged in a block manner, nor does it limit the order of arrangement of the units on the polymer chain.
[0025] The chelating agent provided by this invention has a polyaspartic acid backbone as its main chain, with aspartic acid units linked by peptide bonds, providing carboxylic acid groups (-COOH) and amide groups (-CONH-) as coordination sites. The side chain is grafted onto the polyaspartic acid side chain via a ring-opening ammonolysis reaction between the amino group of L-cysteine and polysuccinimide (PSI), introducing thiol (-SH) coordination sites. This design creates a mixed coordination field containing three coordination atoms: O (carboxylic acid), N (amide), and S (thiol / thioether), forming an asymmetric ternary mixed coordination field. 2+ Mg 2+ As a hard acid, it preferentially coordinates with hard bases such as O / N; Si 4+ As a cross-linked acid (leaning towards hard acid), its affinity for S ligands is significantly weaker than its affinity for O ligands. Through the aforementioned asymmetric ternary mixed coordination field, selective chelation of calcium and magnesium ions can be achieved at the molecular level, while reducing the complexation competition for silicon ions.
[0026] The chelating agent of this invention achieves Ca chelation through mixed coordination field design. 2+ Mg 2+ and Si 4+ Its selective recognition can retain the strong chelating ability of calcium and magnesium ions to soften water and break down inorganic dirt, while significantly reducing the coordination attack on SiO2 in AR coating, thus achieving protection of key components of photovoltaic modules while cleaning efficiently.
[0027] In a specific embodiment, the present invention also provides a method for preparing a chelating agent, comprising the following steps: S1. Polysuccinimide of Formula I was prepared by thermal polycondensation of L-aspartic acid; S2. Polysuccinimide was reacted with L-cysteine via a nucleophilic ring-opening reaction to prepare the cysteine-grafted polyaspartic acid intermediate shown in Formula II. S3. Hydrolyze the cysteine-grafted polyaspartic acid intermediate to obtain the chelating agent; Formula I, m / n = 0.3-0.8.
[0028] In some specific exemplary embodiments, in the preparation method of the chelating agent mentioned in this invention, the thermal polycondensation reaction in S1 is carried out under vacuum conditions, the reaction temperature is 185-195℃, and the reaction time is 4-6h.
[0029] Nitrogen gas can be introduced for protection during the thermal polycondensation reaction in S1. After the reaction is completed, the mixture is cooled to room temperature to obtain a pale yellow solid polysuccinimide (PSI) intermediate.
[0030] This invention specifically limits the thermal polycondensation reaction process in step S1 to 185-195℃ and 4-6h, achieving synergistic optimization of both the degree of polymerization (n) and the content of active rings. Within this process range, the number-average molecular weight (Mn) of PSI is stable at 3000-5000 Da (corresponding to n≈30-50). This molecular weight range ensures both the calcium and magnesium chelating capacity of the chelating agent and excellent biodegradability (the degradation rate of polyaspartic acid is negatively correlated with molecular weight; excessively high molecular weight degrades its environmental properties). If only temperature is controlled while time is ignored, for example, reacting at 180℃ for 8h, although a similar yield can be achieved, prolonged heating leads to yellowing of the product, decreased purity, and increased energy consumption, making it uneconomical. If only time is controlled while temperature is ignored, for example, reacting at 200℃ for 3h, the surface yield meets the target, but a large number of branched structures exist internally, severely affecting the selective recognition accuracy of the chelating agent.
[0031] In some specific exemplary embodiments, in the preparation method of the chelating agent mentioned in this invention, the reaction temperature of the nucleophilic ring-opening reaction in S2 is 40-60℃, the reaction time is 12-18h, and the molar ratio of polysuccinimide to L-cysteine is 1:0.3-0.8.
[0032] In the nucleophilic ring-opening reaction of step S2 described above, controlling the reaction temperature provides the activation energy for ring-opening ammonolysis while avoiding high-temperature side cross-linking reactions. Controlling the reaction time ensures the grafting reaction reaches thermodynamic equilibrium, resulting in uniform distribution of grafted units along the molecular chain, while preventing excessive time that could lead to the breakage and degradation of the main chain amide bonds. Through the synergistic control of these process conditions, a grafting rate of at least 30% can be achieved, constructing an effective O, N, S ternary coordination field, while preventing excessive cysteine residue (difficult to remove by dialysis) and intermolecular disulfide cross-linking, which is beneficial for improving product purity.
[0033] Polysuccinimide is soluble in a solvent, such as N,N-dimethylformamide (DMF), and is prepared into a 10-15% (w / w) solution before undergoing a nucleophilic ring-opening reaction with L-cysteine. The preferred concentration of the polysuccinimide solution is 10-15% (w / w) to optimize the degree of polymerization of PSI, the solvation capability of DMF, the nucleophilic reaction kinetics, and the purification efficiency, ensuring a system reaction conversion rate ≥85% and a random distribution of grafted units. Excessively high concentrations may lead to a sudden increase in viscosity, resulting in uneven reaction and intermolecular cross-linking and gelation.
[0034] In some specific exemplary embodiments, in the preparation method of the chelating agent mentioned in this invention, the hydrolysis reaction temperature in S3 is 50-60°C, the reaction time is 2-3 hours, and the reaction pH is 9-10.
[0035] Temperature control during the hydrolysis reaction provides the activation energy required for the reaction, ensuring complete ring-opening within 2-3 hours and guaranteeing ≥99.5% complete hydrolysis of the succinimide ring, thus minimizing exposure time to the alkaline-thermal environment. pH control provides a sufficiently alkaline environment to allow the succinimide ring to completely open and hydrolyze into carboxylate (-COO) groups. - This imparts water solubility and chelating activity to the chelating agent.
[0036] The pH value of the reaction can be controlled by adding an alkali, such as NaOH solution, to the reaction solution where the reaction is complete in S2. By controlling the hydrolysis conditions described above, the remaining succinimide ring can be completely hydrolyzed into carboxylic acid groups.
[0037] In some specific exemplary embodiments, the hydrolyzed product can be further neutralized to pH 7.0-7.5 with hydrochloric acid, dialyzed through a dialysis membrane with a molecular weight cutoff of 500-1000 Da for 24-48 hours to remove unreacted cysteine and small molecule byproducts, concentrated under reduced pressure, and then freeze-dried to obtain the final product PASP-Cys chelating agent, which is a white to pale yellow powder.
[0038] Polyaspartic acid (PASP) is a fully biodegradable polyamino acid whose side-chain carboxyl groups can form stable five- or six-membered chelate rings with metal ions such as calcium and magnesium. Individual PASP-based chelators follow a single carboxylic acid / amide coordination mode, with the carboxylic acid group acting as a hard base, resisting the formation of calcium ions. 2+ Mg 2+ Hard acid ions have strong chelating ability and also affect the SiO2 in glass AR coatings. 4+(Boundary acids / hard acids) also possess competitive coordination ability but lack selective recognition ability. Under weakly alkaline pH conditions, the silanol groups on the glass surface partially dissociate, and the carboxylic acid groups can gradually dissolve silicon atoms in the SiO2 framework through chelation, leading to a change in the refractive index of the AR coating and an irreversible decrease in light transmittance. In a specific embodiment, the present invention also provides a photovoltaic module cleaning agent, which includes the chelating agent provided by the present invention described above.
[0039] The photovoltaic module cleaning agent mentioned in this invention can be applied to the surface cleaning of photovoltaic modules, including crystalline silicon modules and thin-film modules. In particular, it can significantly reduce the damage caused by cleaning to photovoltaic modules and protect the performance of the modules during their service life.
[0040] In some specific embodiments, the pH value of the photovoltaic module cleaning agent provided by the present invention is controlled at 7.8-8.5.
[0041] This pH range ensures that the carboxylic acid groups of the PASP-Cys chelating agent are in a dissociated state (pKa of 4-5) to fully exert its chelating function, while also being non-corrosive to the AR coating on photovoltaic glass and the aluminum alloy frame. The nanoporous AR coating on the photovoltaic glass surface is chemically active; strongly alkaline cleaning agents easily dissolve the SiO2 framework, and the anodized aluminum alloy frame is prone to intergranular corrosion under alkaline conditions. Controlling the pH value of the photovoltaic module cleaning agent can effectively prevent damage to the AR coating and frame during surface cleaning.
[0042] In some specific embodiments, the photovoltaic module cleaning agent provided by the present invention comprises, by weight, the following components: 4-11 parts surfactant, 3-11 parts composite chelating agent, 2-6 parts penetrating solvent, and 1-4 parts pH buffer. The composite chelating agent is a mixture of the chelating agent and the auxiliary chelating agent provided by the present invention, with a mass ratio of 1-8:1, preferably 2-3:1. Preferably, the auxiliary chelating agent is selected from any one of sodium citrate, sodium gluconate, sodium polyacrylate, and sodium ethylenediamine di-o-phenylacetate.
[0043] The O / N coordination sites of the PASP-Cys chelating agent system can efficiently chelate Ca. 2+ / Mg 2+ It softens water and breaks down inorganic salt deposits in scale and bird droppings; S coordination sites support Si 4+With weak affinity, it reduces the attack of SiO2 on the AR coating at the molecular level, achieving cleaning while protecting the substrate. Simultaneously, the carboxylic acid groups in the polymer backbone of the PASP-Cys chelating agent system exhibit excellent suspension and dispersion effects on mud, sand, and dust particles, dispersing and inhibiting scale buildup and preventing secondary fouling. Furthermore, the thiol groups in the cysteine side chains of the PASP-Cys chelating agent system can form an Al-S passivation adsorption layer on the aluminum frame surface, providing additional corrosion inhibition protection.
[0044] In some specific embodiments, the surfactant in the photovoltaic module cleaning agent provided by the present invention is a mixture of nonionic surfactant and anionic surfactant, and the mass ratio of nonionic surfactant to anionic surfactant is 1-8:1, for example, it can be a point value of 1:1, 2:1, 3:1, 4:1, 5:1, 6:1, 7:1, 8:1 or any range of values, preferably 2-3:1.
[0045] In some specific embodiments, the nonionic surfactant of the present invention is selected from either fatty alcohol polyoxyethylene ether (AEO-9) or alkyl glycoside (APG), and the anionic surfactant is sodium fatty acid methyl ester sulfonate (MES).
[0046] Nonionic surfactants have excellent wetting and spreading ability and low foaming properties, making them suitable for rapid spreading on the vertical surface of photovoltaic modules. Anionic surfactants (MES) have excellent hard water resistance. When used in combination with nonionic surfactants at a mass ratio of 1-8:1, they can significantly reduce the critical micelle concentration (CMC). Even at low dosages, they can efficiently remove hydrophobic oil and dust adhering to the glass surface through the "rolling mechanism", significantly improving the surface cleaning effect of photovoltaic modules.
[0047] In some specific embodiments, the penetrating solvent mentioned in this invention is preferably a solvent with low surface tension and a suitable HLB value, such as dipropylene glycol methyl ether or ethylene glycol butyl ether, which can penetrate into the interior of dried bird droppings to swell and soften, thereby improving the removal efficiency of stubborn organic stains.
[0048] In some specific embodiments, the pH buffer of the present invention may be, for example, triethanolamine or DMEA (N,N-dimethylethanolamine), which can precisely stabilize the pH value of a 1 wt% photovoltaic module cleaning agent dilution at 7.8-8.5.
[0049] In some specific embodiments, the photovoltaic module cleaning agent provided by the present invention can also add functional additives according to actual needs. For example, by weight, 0.05-0.2 parts of preservative (MIT (2-methyl-4-isothiazolin-3-one) / CMIT (5-chloro-2-methyl-4-isothiazolin-3-one) mixture, CMIT to MIT by weight ratio of 3:1) and 0.05-0.2 parts of defoamer can be added.
[0050] In the overall photovoltaic module cleaning agent formula, water is used to make up the remaining 100 parts.
[0051] In some specific embodiments, the photovoltaic module cleaning agent of the present invention has the following formula, with a total mass of 100 parts: 3-8 parts nonionic surfactant, 1-3 parts anionic surfactant, 2-8 parts PASP-Cys, 1-3 parts sodium citrate, 2-6 parts penetrating solvent, 1-4 parts pH buffer, 0.05-0.2 parts preservative, 0.05-0.2 parts defoamer, and the balance is water.
[0052] In a specific embodiment, the present invention also provides a method for preparing a photovoltaic module cleaning agent, comprising the following steps: The composite chelating agent was prepared into an aqueous solution and heated to 40-45℃. A surfactant was added while stirring, and the temperature was lowered to 30-35℃. The remaining components were added, and the pH value was adjusted. The solution was allowed to stand and defoam to obtain the photovoltaic module cleaning agent.
[0053] Conventional cleaning agent preparation typically employs a one-pot method at room temperature or a process of complete dissolution at high temperature followed by cooling. However, the three-step progressive process of heating to solubilize, medium-temperature compounding, and cooling to fine-tune the process, specially designed in this invention, is not merely a matter of operational habit. Rather, it is a synergistic temperature window selected through systematic experiments, taking into account the temperature-sensitive properties of the PASP-Cys polymer chain, the cloud point of AEO-9, the solubility behavior of MES, the thermal stability of the preservative, and the pH temperature drift coefficient.
[0054] In some specific embodiments, the preparation method of the photovoltaic module cleaning agent provided by the present invention may include the following steps in detail: Chelating agent pre-dissolution: Add 50%-60% of the formula amount of deionized water to the reaction vessel, add PASP-Cys chelating agent and sodium citrate under stirring at room temperature, and stir for 20-30 minutes until completely dissolved; Surfactant mixing: Heat to 40-45℃, add anionic surfactant MES and nonionic surfactant AEO-9 (or APG) sequentially while stirring at 200-400 rpm, and continue stirring for 15-20 minutes until the system is uniformly mixed; Adding solvents and additives: Cool to 30-35℃, add penetrating solvent, pH buffer, preservative and defoamer, and stir for 10-15 minutes; pH adjustment and water replenishment: Check the pH value and adjust it to 7.8-8.5 with citric acid or sodium hydroxide if necessary. Add the remaining deionized water and continue stirring for 10 minutes; Transfer the product to a settling tank and let it stand for 12-24 hours to eliminate air bubbles; The finished product is obtained by filtering through a microporous filter with a ≤5μm pore size.
[0055] In the pre-dissolving step of the chelating agent mentioned above, the addition rate of PASP-Cys chelating agent and sodium citrate can be controlled to be slow, and then completely added in 5-20 minutes. Slow addition can avoid the powder surface from absorbing water and swelling instantly to form closed clumps that are wet on the outside and dry on the inside (commonly known as fish eyes), which would prevent the active ingredients from dissolving.
[0056] In some specific exemplary embodiments, the nonionic surfactant APG0810 is preferred, which is superior to AEO-9 in terms of surface tension, detergency, mildness and environmental friendliness, and its characteristics of no cloud point and high alkali resistance are more suitable for the medium to weak alkaline (pH 7.8-8.5) photovoltaic cleaning agent system of the present invention.
[0057] The specific raw material information used in the following embodiments and comparative examples of the present invention is shown in Table 1 below.
[0058] Table 1. Raw Material Information Description Material Category Raw material name Manufacturer / Source Chelating agent raw materials L-Aspartic acid Sinopharm Group L-cysteine Sinopharm Group N,N-Dimethylformamide (DMF) Sinopharm Group Maleic anhydride Anaiji Chemical Urea Anaiji Chemical surfactants Fatty alcohol polyoxyethylene ether (AEO-9) BASF Alkyl glycoside (APG 0810) Shanghai Fakai Sodium methyl ester sulfonate of fatty acids (MES) Zanyu Technology auxiliary chelating agents Sodium citrate Weifang Yingxuan Penetrating solvent Dipropylene glycol methyl ether (DPM) Dow Chemicals Ethylene glycol butyl ether Dow Chemicals pH buffer Triethanolamine (TEA) Anaiji Chemical N,N-Dimethylethanolamine (DMEA) Anaiji Chemical preservative MIT / CMIT mixture Rohm and Haas Defoamer silicone defoamer Dow Corning Comparative raw materials DTPA (Diethylenetriaminepentaacetic acid) AkzoNobel GLDA (Tetrasodium glutamate diacetate) AkzoNobel Example 1 A PASP-Cys chelating agent, with the following chemical structural formula: , where x=0-0.7, y=0.3-0.8, z=0.3-0.8.
[0059] This embodiment 1 also specifically provides a method for preparing a PASP-Cys chelating agent: S1. Synthesis of polysuccinimide (PSI): 100g of L-aspartic acid was added to the reactor, heated to 190℃ under nitrogen protection, and reacted under vacuum for 5 hours. After the reaction was completed, it was cooled to room temperature to obtain a pale yellow solid PSI (72g), with a yield of about 85%.
[0060] S2. Cysteine grafting: Dissolve 50g PSI in 350ml LDMF, add 28g L-cysteine (PSI to cysteine molar ratio of about 1:0.5), stir and react at 50℃ for 16 hours to obtain cysteine-grafted polyaspartic acid intermediate. S3. Hydrolysis and purification: Add NaOH solution to adjust pH to 9.5, hydrolyze at 55℃ for 2.5 hours, neutralize with hydrochloric acid to pH 7.2, dialyze through a dialysis membrane with a molecular weight cutoff of 800 Da for 36 hours, concentrate under reduced pressure and freeze dry to obtain 58g of PASP-Cys chelating agent (pale yellow powder).
[0061] Figure 1 The infrared spectrum of the PASP-Cys chelating agent prepared in this invention is shown in the figure. It can be seen from the figure that at 3390 cm⁻¹... -1 A broad and strong NH stretching vibration absorption peak is observed nearby, confirming the presence of numerous secondary amide structures on the polyaspartic acid backbone. (1646 cm⁻¹) -1 and 1549 cm -1 The surrounding area shows characteristic absorption peaks for amide I and amide II bands, further confirming the formation of the peptide backbone. (1398 cm⁻¹) -1 Nearby carboxylate ions (COO) - The symmetric stretching vibration peaks of the succinimide ring are clearly visible, proving that the ring has been completely hydrolyzed and opened into a carboxylate ion, thus endowing the chelating agent with excellent water solubility. (3070 cm⁻¹) -1 The absence of nearby absorption peaks indicates that the five-membered ring imide characteristic structure of the raw material PSI has completely disappeared, meaning that the imide ring has been completely hydrolyzed and opened. Infrared spectroscopy analysis fully demonstrates that this invention successfully synthesized a cysteine-grafted polyaspartic acid (PASP-Cys) chelating agent. Its molecular structure simultaneously contains three coordinating atoms: carboxylic acid oxygen (O), amide nitrogen (N), and mercaptosulfur (S), providing the molecular basis for constructing a ternary mixed coordination field. Example 2 A photovoltaic module cleaning agent, with a pH value of 7.8-8.5, comprises the components shown in Table 2 below by weight.
[0062] Table 2. Components of Photovoltaic Module Cleaning Agent Components Raw material name Number of weights Nonionic surfactants AEO-9 5 Anionic surfactants MES 2 Novel chelating agents PASP-Cys (Prepared in Example 1) 4 auxiliary chelating agent Sodium citrate 2 Penetrating solvent DPM 4 pH buffer Triethanolamine 2 preservative MIT / CMIT 0.1 Defoamer silicone defoamer 0.1 solvent Deionized water Add to 100 This embodiment 1 also specifically provides a method for preparing a photovoltaic module cleaning agent, including the following steps: Chelating agent pre-dissolution: Add 50% of the formula amount of deionized water to the reaction vessel, add PASP-Cys chelating agent and sodium citrate under stirring at room temperature, and stir for 25 minutes until completely dissolved; Surfactant mixing: Heat to 45℃, add anionic surfactant MES and nonionic surfactant AEO-9 sequentially while stirring at 300 rpm, and continue stirring for 15 min until the system is uniformly mixed; Solvent and additive addition: Cool to 35°C, add penetrating solvent, pH buffer, preservative and defoamer, and stir for 15 minutes; pH adjustment and water replenishment: Check the pH value, and adjust it to 7.8-8.5 with citric acid or sodium hydroxide if necessary. Add the remaining deionized water and continue stirring for 10 minutes. The product was transferred to a settling tank and allowed to stand for 20 hours to eliminate air bubbles. It was then filtered through a ≤5μm microporous filter to obtain the finished product.
[0063] Example 3 A photovoltaic module cleaning agent with a pH value of 7.8-8.5, comprising, by weight, essentially the same components and contents as in Example 2, except that the nonionic surfactant AEO-9 is replaced with an equal amount of APG0810 (alkyl glycoside-0810, HLB=14-16, Haisen Chemical).
[0064] The preparation method of the photovoltaic module cleaning agent in Example 3 is the same as that in Example 2.
[0065] Example 4 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that: 8 parts of PASP-Cys chelating agent and 1 part of sodium citrate.
[0066] The preparation method of the photovoltaic module cleaning agent in Example 4 is the same as that in Example 2.
[0067] Example 5 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that: 2 parts of PASP-Cys chelating agent and 3 parts of sodium citrate.
[0068] The preparation method of the photovoltaic module cleaning agent in Example 5 is the same as that in Example 2.
[0069] Example 6 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that: 3 parts of nonionic surfactant and 3 parts of anionic surfactant.
[0070] The preparation method of the photovoltaic module cleaning agent in Example 6 is the same as that in Example 2.
[0071] Example 7 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that: 8 parts of nonionic surfactant and 1 part of anionic surfactant.
[0072] The preparation method of the photovoltaic module cleaning agent in Example 7 is the same as that in Example 2.
[0073] Comparative Example 1 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that PASP-Cys is replaced with an equal amount of chelating agent DTPA (diethylenetriaminepentaacetic acid).
[0074] Comparative Example 2 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that PASP-Cys is replaced with an equal amount of chelating agent GLDA (tetrasodium glutamate-N,N-diacetate).
[0075] Comparative Example 3 A photovoltaic module cleaning agent, by weight, comprises essentially the same components and contents as in Example 2, except that PASP-Cys is replaced with an equal amount of polyaspartic acid (unmodified by cysteine grafting, Sinopharm Group).
[0076] Comparative Example 4 We selected a commercially available photovoltaic-specific cleaning agent (pH 10.5) from a well-known brand.
[0077] Application examples The tests were conducted in accordance with QB / T5826-2023 "Industrial and Public Facility Hard Surface Cleaners" and related self-developed methods. The performance test comparisons of the examples and comparative examples are shown in Table 3.
[0078] QB / T5826-2023 requires that the cleaning agent have a uniform appearance without separation, show no abnormalities after being stored at -5℃±2℃ and 40℃±2℃ for 24 hours respectively, have good stability, a pH value between 8.0 and 13.0, and have a corrosiveness of less than 100mg for both H62 brass and LY12 hard aluminum.
[0079] It should be noted that: The calcium ion chelating capacity (mgCaCO3 / g) in Table 3 was determined using a self-developed method: The detection was performed using the calcium ion selective electrode method. A 500 mg / L Ca solution was prepared. 2+ Standard working solution (in Ca 2+ Measure 100.0 mL of the chelating agent and place it in a 150 mL beaker. Add approximately 0.1 g of the chelating agent sample to be tested. Stir for 10 minutes at a constant temperature of 25 ± 0.5 °C to allow the chelation reaction to reach equilibrium. Measure the free Ca in the solution using a calibrated calcium ion selective electrode. 2+ Concentration C1 (mg / L), and free Ca in the initial standard solution without chelating agent was determined simultaneously. 2+ Concentration C0 (mg / L).
[0080] Calcium ion chelating capacity is calculated using the following formula: Calcium ion chelating capacity (mgCaCO3 / g) = (C0-C1)×V×10 -3 ×2.5 / m, In the formula, C0 is Ca 2+ Initial concentration (mg / L); C1 is Ca 2+ Concentration after reaction (mg / L); V is the volume of the test solution (mL); 2.5 is the Ca... 2+ The coefficient for converting mass to equivalent mass of CaCO3; m is the mass (g) of the chelating agent sample.
[0081] The simulated bird droppings removal rate was determined using a self-developed method: The gravimetric method was used for testing. A simulated bird droppings stain was prepared by uniformly mixing protein powder, cellulose, and vegetable oil in a 2:1:1 mass ratio.
[0082] Simulated bird droppings were evenly coated onto the surface of a pre-weighed photovoltaic glass sheet (5cm×5cm), with a coating amount of approximately 5mg / cm². 2 (On dry weight), after being left at room temperature for 30 minutes, place it in an 80℃ oven for 2 hours to age and fix it. Remove it, cool it to room temperature, weigh it and record m1 (mass of the contaminated glass slide).
[0083] Immerse the contaminated glass slide in a 1% diluted solution of the cleaning agent to be tested, soak at room temperature for 10 minutes, then rinse evenly with a constant flow of water (flow rate 2L / min) for 30 seconds. Place the glass slide in a 105℃ oven to dry for 30 minutes, remove and cool to room temperature, weigh and record m2 (mass of the cleaned glass slide).
[0084] With the original glass slide mass as m0, the simulated bird droppings removal rate is calculated using the following formula: Simulated bird droppings removal rate (%) = (m1-m2) / ((m1-m0)×100%).
[0085] Overall stain removal rate was determined using a self-developed method: The color difference method was used for detection. Carbon black, clay, and vegetable oil were mixed evenly in a mass ratio of 1:2:1 to prepare a comprehensive stain simulant.
[0086] Select a photovoltaic glass sheet with a clean and uniform surface, and measure the initial brightness value L0 (original glass) using a colorimeter.
[0087] The composite stain simulant was uniformly coated onto the surface of the glass slide at a concentration of 3 mg / cm². 2 Allow the glass to sit at room temperature for 24 hours to allow the stain to adhere stably. Measure the brightness value L1 of the contaminated glass slide using a colorimeter.
[0088] Prepare a 1% diluted solution of the cleaning agent to be tested. Soak a clean non-woven fabric in sufficient cleaning solution, apply constant pressure with a 500g weight, and wipe the contaminated area 10 times at a uniform speed. After air drying at room temperature, measure the brightness value L2 of the cleaned glass slide using a colorimeter.
[0089] The overall stain removal rate is calculated using the following formula: Overall stain removal rate (%) = (L2-L1) / (L0-L1)×100%.
[0090] The change in transmittance of AR coating was determined using a self-developed method: Spectrophotometry was used for detection. A photovoltaic glass sample (5cm×5cm) with AR antireflection coating was selected, and its initial average transmittance T0 in the 380-1100nm wavelength range was measured using a UV-Vis spectrophotometer.
[0091] Photovoltaic glass samples were immersed in a 5% diluted solution of the cleaning agent to be tested, and continuously immersed for 72 hours at a constant temperature of 60±5℃ to simulate the cumulative chemical contact during the service life of the module. After removal, the samples were thoroughly rinsed with deionized water and allowed to air dry. The average transmittance T1 was measured again under the same conditions. The change in transmittance of the AR coating was calculated using the following formula: Transmittance change (%) = T1 - T0.
[0092] The specific test results are shown in Table 3.
[0093] Table 3. Test results for each embodiment and comparative example
[0094] As can be seen from the test results in Table 3 above, the photovoltaic cleaning agent prepared by the PASP-Cys chelating agent in this embodiment of the invention differs from the single carboxylic acid coordination mode chelating agents such as DTPA, GLDA, and conventional PASP commonly used in existing formulations. This invention constructs a ternary mixed coordination field of O (carboxylic acid oxygen), N (amide nitrogen), and S (mercaptosulfonium) by introducing cysteine-grafted modified polyaspartic acid, thereby achieving the control of Ca at the molecular level. 2+ / Mg 2+ Selective chelation, while significantly reducing Si 4+ Its coordination competition ability allows the thiol group of its cysteine side chain to form an Al-S passivation layer on the aluminum frame surface, providing better protection for photovoltaic modules.
[0095] The photovoltaic module cleaning agent of this invention achieves dual protection through selective chelation mechanism and precise control of weakly alkaline pH (7.8-8.5), resulting in AR coating transmittance damage ≤0.3%, H62 brass ≤0.5mg, and LY12 hard aluminum corrosion ≤2.0mg.
[0096] Furthermore, the weakly alkaline photovoltaic module cleaning agent of the present invention, through the synergistic effect of surfactant system, modified chelating agent and penetrating solvent, achieves a removal rate of over 95% for simulated bird droppings and a removal rate of over 93% for comprehensive stains, demonstrating excellent surface cleaning effect.
[0097] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A chelating agent, characterized in that, The chemical structural formula is: , where x=0-0.7, y=0.3-0.8, z=0.3-0.
8.
2. A method for preparing a chelating agent, characterized in that, Includes the following steps: S1. Polysuccinimide of Formula I was prepared by thermal polycondensation of L-aspartic acid; S2. Polysuccinimide was reacted with L-cysteine via a nucleophilic ring-opening reaction to prepare the cysteine-grafted polyaspartic acid intermediate shown in Formula II. S3. Hydrolyze the cysteine-grafted polyaspartic acid intermediate to obtain a chelating agent; Formula I, Formula II, m / n = 0.3-0.
8.
3. The method for preparing the chelating agent according to claim 2, characterized in that, The thermal polycondensation reaction described in S1 is carried out under vacuum conditions, with a reaction temperature of 185-195℃ and a reaction time of 4-6 hours.
4. The method for preparing the chelating agent according to claim 2, characterized in that, The nucleophilic ring-opening reaction described in S2 has a reaction temperature of 40-60℃, a reaction time of 12-18h, and a molar ratio of polysuccinimide to L-cysteine of 1:0.3-0.
8.
5. The method for preparing the chelating agent according to claim 2, characterized in that, The hydrolysis reaction described in S3 is carried out at a temperature of 50-60℃, for a reaction time of 2-3 hours, and at a pH of 9-10.
6. A photovoltaic module cleaning agent, characterized in that, The chelating agent includes the chelating agent according to claim 1 or the chelating agent prepared by the preparation method according to any one of claims 2-5.
7. The photovoltaic module cleaning agent according to claim 6, characterized in that, The pH value of the photovoltaic module cleaning agent is 7.8-8.
5.
8. The photovoltaic module cleaning agent according to claim 6 or 7, characterized in that, By weight, it comprises the following components: 4-11 parts surfactant, 3-11 parts complex chelating agent, 2-6 parts penetrating solvent, and 1-4 parts pH buffer. The composite chelating agent is a mixture of the chelating agent and the auxiliary chelating agent, with a mass ratio of 1-8:1, preferably 2-3:1; Preferably, the auxiliary chelating agent is selected from any one of sodium citrate, sodium gluconate, sodium polyacrylate, and sodium ethylenediamine di-o-phenylacetate.
9. The photovoltaic module cleaning agent according to claim 7, characterized in that, The surfactant is a mixture of nonionic surfactant and anionic surfactant, and the mass ratio of nonionic surfactant to anionic surfactant is 1-8:1, preferably 2-3:1; More preferably, the nonionic surfactant is selected from any one of fatty alcohol polyoxyethylene ether or alkyl glycoside, and the anionic surfactant is sodium fatty acid methyl ester sulfonate.
10. A method for preparing the photovoltaic module cleaning agent according to any one of claims 6-9, characterized in that, Includes the following steps: The composite chelating agent was prepared into an aqueous solution and heated to 40-45℃. A surfactant was added while stirring, and the temperature was lowered to 30-35℃. The remaining components were added, and the pH value was adjusted. The solution was allowed to stand and defoam to obtain the photovoltaic module cleaning agent.
Citation Information
Patent Citations
Alkaline photovoltaic battery silicon wafer cleaning agent and preparation method thereof
CN103589522A