A quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate and its preparation method
By preparing a sulfur-doped carbon quantum dot-based percolation displacement agent based on corn cob and sodium lignin sulfonate, the problems of high cost and difficulty in reducing particle size of nano-displacement materials in the prior art have been solved, achieving low-cost and high-efficiency percolation displacement effect and improving the recovery rate of tight oil reservoirs.
Patent Information
- Application Number
- CN202611487258.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-23
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies struggle to effectively utilize nanomaterials to enhance oil recovery in tight reservoirs. Furthermore, the high cost of these materials, complex synthesis processes, and difficulty in further reducing particle size limit the release of structural separation pressure effects.
Sulfur-doped carbon quantum dots were prepared using biomass corn cobs and sodium lignin sulfonate. A highly active quantum dot-based oil displacement agent was constructed through solid-state calcination and redox polymerization. The agent has small particle size, is temperature and salt resistant, and can be stably dispersed in high-temperature and high-salt environments. Furthermore, it was modified by copolymerization with polymers to enhance the oil displacement effect.
This low-cost, large-scale application of the percolation oil displacement agent significantly improves the percolation recovery rate of tight oil reservoirs. It is suitable for the later stages of water injection development in tight oil reservoirs, utilizing residual oil, reducing oil-water interfacial tension, and enhancing the spontaneous percolation capacity of the core matrix.
Smart Images

Figure CN123107650A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of oilfield chemical technology, specifically to a quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate and its preparation method. Background Technology
[0002] Tight oil reservoirs have complex pore structures, generally low reservoir properties, prominent intra-layer heterogeneity, and pore throat sizes mostly in the micro-nano range. They generally face development challenges such as difficulty in water injection and high fluid displacement resistance, resulting in low reserve utilization and limited oilfield development benefits. There is an urgent need to develop oil recovery technologies adapted to the pore throat characteristics of tight reservoirs.
[0003] Small-molecule surfactant systems, characterized by ultra-low interfacial tension, can improve oil washing efficiency by reducing the oil-water-rock interfacial energy, and are currently a common technique for percolation-driven oil displacement in tight oil. However, the mechanism of action of these systems is relatively simple, relying solely on interfacial tension regulation to achieve crude oil stripping, resulting in limited recovery and difficulty in fully utilizing the crude oil retained in the tight matrix. The Nikolov-Wasan model reported in *Nature* reveals a unique oil washing mechanism using nanofluids: nanofluids and spherical micelle systems can generate additional osmotic pressure within the narrow wedge-shaped space of the oil-water-solid three-phase contact, forming a structural separation pressure that drives the fluid to expand into the pore throat wedge region, efficiently stripping the oil film from the rock surface. This opens up new avenues for the development of next-generation tight oil displacement materials. According to this theory, maintaining the ultra-dispersed state and ultra-small particle size of the displacement material is a core prerequisite for maximizing the structural separation pressure and enhancing oil washing efficiency.
[0004] Current nanomaterials for oil displacement primarily employ modified inorganic nanoparticles, nanomicelles, and spherical polymers. While chemical modification can optimize dispersion and regulate rock wettability, limitations in the synthesis process restrict the continuous reduction of particle size, hindering the further release of structural separation pressure effects and creating a bottleneck in improving oil washing and percolation displacement efficiency. Carbon quantum dots, as zero-dimensional nanomaterials with generally smaller than 10 nm in three dimensions, possess advantages such as ultra-small particle size, high specific surface area, and easy surface functionalization, making them an important candidate for high-performance percolation and displacement materials.
[0005] Currently, the cost of chemically synthesized carbon quantum dots is relatively high, which is not conducive to large-scale on-site injection in oil fields. Therefore, developing quantum dot percolation displacement agents that use agricultural and forestry waste biomass as a carbon source and construct them through compounding, possessing ultra-small particle size, excellent temperature and salt resistance, and strong percolation and oil washing capabilities, is of great practical significance for solving the problem of utilizing reserves in tight oil reservoirs. Summary of the Invention
[0006] In view of the shortcomings of existing technologies, this invention proposes a carbon quantum dot-based percolation displacement agent based on corn cob and sodium lignin sulfonate, and its preparation method. This invention utilizes biomass corn cob and sodium lignin sulfonate to dry-process sulfur-doped carbon quantum dots; these are then compounded with specific monomers to construct a bio-based, highly active quantum dot percolation displacement agent. The preparation process is mild, using inexpensive and readily available raw materials; the product has small particle size, strong dispersion stability under high temperature and high salt conditions, and also exhibits wetting reversal, reduces oil-water interfacial tension, enhances spontaneous percolation of the core matrix, and improves percolation and oil recovery rates in tight oil reservoirs.
[0007] To achieve the above objectives, the present invention adopts the following technical solution: A method for preparing a quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate includes the following steps: S1. Mix corn cob powder with sodium lignosulfonate at a mass ratio of 3:1 to 1:3, and prepare corn cob-sodium lignosulfonate-based sulfur-doped carbon quantum dots by solid-phase calcination. S2. Mix corn cob-lignosulfonate sodium sulfur-doped carbon quantum dots with 3-methacryloyloxypropyltrimethoxysilane (γ-MPS) at a mass ratio of 3:1 to 1:1.3 to prepare γ-MPS-modified corn cob-lignosulfonate sodium sulfur-doped carbon quantum dots. S3. Acrylamide, 1-(3-sulfopropyl)-4-vinylpyridine inner salt or sodium 3-allyloxy-2-hydroxy-1-propanesulfonate, sodium tridecyl alcohol polyoxyethylene ether sulfate, and modified corn cob-lignin sulfonate-based sulfur-doped carbon quantum dots are dispersed and dissolved in deionized water at a mass ratio of 1:0.5-1:0.2-0.6:0.05-0.3. The corn cob is then prepared by redox-initiated polymerization. Sodium lignosulfonate-based carbon quantum dot percolation oil displacement agent.
[0008] In this invention, in step S1, corn cob is used as the main carbon source, while sodium lignosulfonate serves as an auxiliary carbon source, a solid-phase in-situ sulfur dopant, and a surface modification agent. The size of the corn cob powder can be selected as needed, for example, corn cob powder pulverized through an 80-120 mesh sieve. In step S2, 3-methacryloyloxypropyltrimethoxysilane (γ-MPS) can undergo a covalent chemical reaction with the corn cob-sodium lignosulfonate-based sulfur-doped carbon quantum dots prepared by the solid-phase method. The sulfur-doped carbon quantum dots have a large number of hydroxyl active sites on their surface. Under the influence of trace amounts of water in the reaction system, the trimethoxy group of the γ-MPS molecule undergoes hydrolysis to generate silanol. The silanol first forms hydrogen bonds with the hydroxyl groups on the carbon quantum dot surface, and then further dehydrates and condenses under heating conditions to form stable Si-OC covalent bonds, thereby grafting polymerizable methacrylate carbon-carbon double bonds onto the sulfur-doped carbon quantum dot surface. The modified carbon quantum dots carry polymerizable double bonds, and the sulfonic acid groups on the surface of the carbon quantum dots are retained, maintaining the material's excellent salt resistance and hydrophilicity. In the redox radical polymerization system of step S3, 1 (3 sulfopropyl) 4 Vinylpyridine inner salt, 3 Allyloxy 2 hydroxyl 1 Sodium propanesulfonate is a polymerizable monomer, while sodium tridecyl alcohol polyoxyethylene ether sulfate is a non-polymerizable functional additive. γ-MPS-modified sulfur-doped carbon quantum dots carry carbon-carbon double bonds grafted from silane on their surface, enabling them to undergo free radical copolymerization with the vinyl / allyl double bonds of acrylamide, 1-(3-sulfopropyl)-4-vinylpyridine inner salt, and sodium 3-allyloxy-2-hydroxy-1-propanesulfonate. This allows the sulfur-doped carbon quantum dots to covalently integrate into the polymer backbone, preventing desorption and aggregation of nanoparticles in high-temperature, high-salt environments. The sodium tridecyl alcohol polyoxyethylene ether sulfate added in this system is a surfactant with a molecular structure entirely composed of saturated chemical bonds, lacking free radical polymerization activity and not participating in covalent polymerization. After polymerization, the sodium tridecyl alcohol polyoxyethylene ether sulfate is physically dispersed within the polymer network through hydrogen bonding and hydrophobic interactions.
[0009] In one specific embodiment of the present invention, the corn cob-sodium lignin sulfonate-based sulfur-doped carbon quantum dots are prepared by solid-phase calcination, comprising the following steps: grinding and mixing corn cob powder and sodium lignin sulfonate solid powder, calcining at a constant temperature of 240℃-320℃ for 1.5-4h under an inert protective atmosphere; naturally cooling the calcined product to room temperature and grinding it, then adding ultrapure water for ultrasonic extraction, and centrifuging to remove uncarbonized solid residue; filtering the supernatant through a 0.22μm filter membrane; dialyzing the filtrate in a dialysis bag with a molecular weight cutoff of 1000Da to remove small molecule salt impurities, and then freeze-drying to obtain brownish-yellow corn cob-sodium lignin sulfonate-based sulfur-doped carbon quantum dots. The present invention employs a solid-phase synthesis process, which does not require a high-pressure hydrothermal reactor, resulting in a simple process and large throughput; sodium lignin sulfonate decomposes during solid-phase high-temperature pyrolysis, introducing sulfonic acid functional groups into the carbon quantum dot framework and surface, eliminating the need for additional exogenous sulfur sources and directly obtaining highly hydrophilic sulfur-doped carbon quantum dots.
[0010] As a specific embodiment of the present invention, step S2 includes: adding sulfur-doped carbon quantum dots and 3-methacryloxypropyltrimethoxysilane into anhydrous ethanol and dispersing them uniformly; stirring the mixture in a closed container at 400-700 r / min for 3-6 h at 65℃-85℃; and removing the solvent by rotary evaporation after the reaction is completed to obtain γ-MPS modified sulfur-doped carbon quantum dots.
[0011] In one specific embodiment of the present invention, the reaction system in step S3 has a total solute mass fraction of 10%-30% and a pH value of 6-9; the reaction temperature is controlled at 10-40℃; the amount of initiator (oxidant-reducant system) added accounts for 0.1%-0.6% of the total mass of all organic monomers; the redox polymerization reaction time is 4-8h; after the reaction is completed, the product is vacuum dried to obtain a solid percolation displacement agent.
[0012] Furthermore, in the initiator, the oxidant is ammonium persulfate, and the reducing agent is sodium bisulfite or sodium formaldehyde sulfoxylate; when the reducing agent is sodium bisulfite, the mass ratio of oxidant to reducing agent is 1:1; when the reducing agent is sodium formaldehyde sulfoxylate, the mass ratio of oxidant to reducing agent is 2:1.
[0013] A bio-based highly active quantum dot-based oil displacement agent is prepared using the above-described preparation method.
[0014] The present invention has the following beneficial effects: (1) The carbon source of this invention is agricultural waste corn cob, and sodium lignin sulfonate is an industrial by-product. The raw materials are widely available and inexpensive, realizing the resource utilization of solid waste. Solid phase calcination to prepare carbon quantum dots does not require a high-pressure hydrothermal reactor. The polymerization reaction is completed in the aqueous phase. It does not use a large amount of organic solvent, is environmentally friendly, and is suitable for large-scale injection in oil fields.
[0015] (2) Sulfur-doped carbon quantum dots participate in free radical copolymerization after covalent grafting with γ-MPS, and are anchored to the polymer framework, effectively inhibiting the aggregation of nanoparticles under high temperature and high salt conditions, maintaining a nanoscale size of less than 10 nm, and can enter the micro-nano pore throat of dense reservoirs, ensuring the performance of the Nikolov-Wasan model structure separation pressure effect. The carbon quantum dot surface retains a large number of sulfonic acid groups, which can chelate divalent Ca in the formation. 2+ Mg 2+ Ions enhance the system's temperature and salt resistance stability.
[0016] (3) The present invention is a composite synergistic system. The copolymer polymer realizes the reversal of rock wettability and stabilizes the nanoparticles. The physical doping of sodium tridecyl alcohol polyoxyethylene ether sulfate realizes the reduction of oil-water interfacial tension. The two work together to enhance the spontaneous absorption capacity of the tight oil matrix. Core absorption experiments have confirmed that the absorption recovery rate is significantly improved. It is suitable for the utilization of the residual oil in the matrix during the later stage of water injection development of tight oil reservoirs. Attached Figure Description
[0017] Figure 1 The static permeation T2 spectra of the oil displacement system corresponding to Example 2 under different permeation times are shown in the core. The core length is 5.0 cm, the diameter is 2.50 cm, the gas permeability is 0.087 mD, and the porosity is 3.36%. Detailed Implementation
[0018] The present invention will be further described in detail below with reference to embodiments, but the embodiments of the present invention are not limited thereto. Unless otherwise specified, the experimental methods used in the following embodiments are conventional methods; the materials and reagents used are commercially available unless otherwise specified.
[0019] Example 1 (1) Preparation of corn cob-sodium lignosulfonate-based sulfur-doped carbon quantum dots by solid-phase method: Corn cob powder was crushed and passed through a 100-mesh sieve; 5g of corn cob powder and 2g of sodium lignosulfonate were taken, ground and mixed thoroughly, and placed in a ceramic boat in a tube furnace; nitrogen gas was introduced as a protective gas, and the temperature was raised to 280℃ for constant-temperature solid-phase calcination for 2.5h; after natural cooling to room temperature, the solid product was taken out and ground thoroughly, and 120mL of ultrapure water was added for ultrasonic extraction for 2h to dissolve the generated carbon quantum dots into the aqueous phase; centrifugation at 8000r / min for 20min was used to remove uncarbonized solid residue; the supernatant was filtered through a 0.22μm filter membrane; the filtrate was placed in a dialysis bag with a molecular weight cutoff of 1000Da for dialysis to remove small molecule salt impurities (dialysis time 48h); freeze-drying (temperature -60℃, time 48h) was used to obtain brownish-yellow corn cob. Sodium lignosulfonate-based sulfur-doped carbon quantum dots retain sulfonic acid groups, giving them excellent salt resistance and hydrophilicity.
[0020] (2) Preparation of γ-MPS modified corn cob-lignosulfonate-based sulfur-doped carbon quantum dots: Weigh 2.0g of the above sulfur-doped carbon quantum dots and 2.2g of γ-MPS, add 150mL of anhydrous ethanol and disperse thoroughly by ultrasonication; react at 70℃ with sealed stirring (550r / min) for 4h; remove ethanol by rotary evaporation to obtain γ-MPS modified corn cob-lignosulfonate-based sulfur-doped carbon quantum dots with a particle size of 2-5nm.
[0021] (3) Preparation of quantum dot percolation displacement agent: Weigh 10.0g acrylamide and 6.0g 1-(3-sulfopropyl)-4 Vinylpyridine inner salt, 2.0 g of tridecyl alcohol polyoxyethylene ether sulfate, and 1.0 g of γ-MPS-modified corn cob-lignin sulfonate-based sulfur-doped carbon quantum dots were dispersed in 80 g of deionized water. The pH of the system was adjusted to 7 using sodium hydroxide solution. Ammonium persulfate and sodium bisulfite in a 1:1 mass ratio were added as initiators, with the total amount of initiator added being 0.3% of the total mass of all organic monomers. The system was kept at 30 °C for 5 h for polymerization. The product was collected, washed with ethanol, and extracted to remove residual water, monomers, and initiators. It was then vacuum dried at 60 °C for 24 h to obtain a corn cob-lignin sulfonate-based carbon quantum dot percolation oil displacement agent, designated CC-NE-1.
[0022] Example 2 The implementation method of this embodiment is basically the same as that of Example 1, except that the amount of sodium tridecane alcohol polyoxyethylene ether sulfate added when preparing the quantum dot percolation displacement agent is changed to 6g, and the resulting displacement agent is numbered CC-NE-2.
[0023] Example 3 The implementation method of this embodiment is basically the same as that of Example 1, except that the amount of γ-MPS modified corn cob-lignosulfonate sodium sulfur-doped carbon quantum dots is increased to 3g, and the resulting oil displacement agent is numbered CC-NE-3.
[0024] Comparative Example 1 The implementation method of Comparative Example 1 is basically the same as that of Example 1, except that γ-MPS-modified corn cob-lignosulfonate sodium sulfur-doped carbon quantum dots are not added in Comparative Example 1 to prepare the final product, while the proportions of other materials remain unchanged. The product obtained in Comparative Example 1 is numbered NE-1.
[0025] Comparative Example 2 The implementation method of Comparative Example 2 is basically the same as that of Example 1, except that the sulfur-doped carbon quantum dots are not modified by γ-MPS grafting, but are directly added to the reaction system by physical blending, while the proportions of other materials remain unchanged. The product obtained in Comparative Example 2 is numbered NE-2.
[0026] Test Example 1 (Interface Tension Test) The oil displacement agents prepared in each example and comparative example were used to... 4 A 0.2% (w / w) percolation displacement agent system was prepared using mg / L NaCl brine. The system's ability to reduce the interfacial tension between crude oil and formation water in the Xinjiang oilfield was tested at 80°C. The experimental results are shown in Table 1, where the blank sample was 20 × 10⁻⁶ mg / L NaCl. 4 The interfacial tension between mg / L NaCl brine and crude oil. Table 1 shows that the oil displacement system based on Examples 1-3 can reduce the oil-water interfacial tension from 10 mg / L. 1 The mN / m order of magnitude is reduced to 10. -2 On the order of mN / m, it is superior to systems without quantum dots or physical mixtures of quantum dots.
[0027] Table 1. Ability of different systems to reduce interfacial tension Test Example 2 (Wettability Improvement Performance Test) The ability of different systems to improve wettability was tested using a shape analyzer. The experimental steps are as follows: 1) Soak the core slides in a mixed solution of toluene and anhydrous ethanol for 48 hours and clean them. After cleaning, place them in a vacuum drying oven at 70°C and dry them for later use. 2) The dried core sections were soaked in crude oil from Xinjiang Oilfield and placed in a vacuum drying oven at 70°C for 48 hours to simulate formation aging and make them oleophilic. 3) Mount the core section on two supports, using a 20×10... 4 The chamber was filled with mg / L NaCl brine, immersing the core slide in the water. A drop of oil was injected under the core slide using a microsyringe, and the shape of the oil droplet could be clearly observed through the transparent glass of the chamber. 4) After the crude oil has reached equilibrium with the water level for a period of time, the contact angle will slowly change. The droplet's angle is then measured using the instrument's optical lens and scale until it remains constant; the original contact angle of the rock slice is then obtained. 5) Take the oil displacement agents prepared in each example and comparative example, and place the rock slices in a 20×10 inch quartz tank. 4 An oil displacement system with an oil displacement agent concentration of 0.2% prepared by mg / L NaCl brine was aged at 80°C for 2 days. Then, steps 3) and 4) were repeated to obtain the contact angle after improved wettability.
[0028] The ability of the system to improve wettability was determined by the change in contact angle, and the experimental results are shown in Table 2. The oil displacement agent system based on Examples 1-3 can reduce the contact angle from 134°-137° to 37°-42°, which is better than the system without quantum dots or the physical mixture of quantum dots.
[0029] Table 2. The ability of different systems to improve wettability Test Example 3 (Percolation Efficiency Test) Prepare 20×10 using heavy water 4 A mg / L NaCl brine solution was used to prepare a CC-NE-2 system with a displacement agent concentration of 0.2%, which was then placed in an adsorption bottle. The T2 spectra of the test cores were taken at intervals, and the adsorption recovery rate was calculated based on the changes in the T2 spectra. The specific experimental steps are as follows: 1) Dry the core sample in an oven at 100℃ for 24 hours. Weigh the dry weight of the core and measure the size of the core sample before the experiment. 2) Determine core porosity and permeability using the nitrogen method; 3) Vacuum pressurize the treated core to saturate it with oil, wipe off the surface oil, and weigh its wet weight; 4) T2 spectrum analysis of saturated good oil cores was performed using a high-temperature and high-pressure online NMR displacement system; 5) A quantum dot nano-permeable agent system (i.e., a CC-NE-2 system with an oil displacement agent mass concentration of 0.2%) was prepared using heavy water. The core sample saturated with good oil was immersed in the quantum dot nano-permeable agent system to conduct a static permeation experiment. 6) Every so often, the core is removed, the surface liquid is wiped off, and T2 spectrum analysis is performed using a high-temperature and high-pressure online NMR displacement system.
[0030] Experimental results are as follows Figure 1 As shown, the quantum dot-based oil displacement agent first utilizes the movable oil in macropores during the permeation process, and then significantly enhances the utilization of micropores (bound oil). The recovery rate can reach 36.5% after 6 days of permeation, demonstrating significant permeation efficiency.
[0031] The same experimental method was used to test the permeation efficiency of other examples and comparative systems, as well as conventional sulfonic acid-modified carbon quantum dots (preparation process referred to Example 2 in CN 111234818 A). The experimental core length was 5.0 cm, the diameter was 2.50 cm, the gas permeability was 1.0 mD, and the porosity was 4.5%. The experimental results are shown in Table 3. It can be seen that the system constructed in this invention is superior to the system without quantum dots or the physical mixture of quantum dots, with a recovery rate more than 10% higher. Compared with the currently reported sulfonic acid-modified carbon quantum dots, the recovery rate is more than 7% higher.
[0032] Table 3. Oil recovery rates of different systems The above description is merely a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in the present invention should be included within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the scope of the claims.
Claims
1. A method for preparing a quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate, characterized in that, Includes the following steps: S1. Mix corn cob powder with sodium lignosulfonate at a mass ratio of 3:1 to 1:3, and prepare corn cob-sodium lignosulfonate-based sulfur-doped carbon quantum dots by solid-phase calcination. S2. Prepare modified corn cob-lignosulfonate sodium sulfur-doped carbon quantum dots by mixing and reacting them with 3-methacryloyloxypropyltrimethoxysilane at a mass ratio of 3:1 to 1:1.
3. S3. Acrylamide, 1-(3-sulfopropyl)-4-vinylpyridine inner salt or sodium 3-allyloxy-2-hydroxy-1-propanesulfonate, sodium tridecyl alcohol polyoxyethylene ether sulfate, and modified corn cob-lignin sulfonate-based sulfur-doped carbon quantum dots are dispersed and dissolved in deionized water at a mass ratio of 1:0.5-1:0.2-0.6:0.05-0.
3. The corn cob is then prepared by redox-initiated polymerization. Sodium lignosulfonate-based carbon quantum dot percolation oil displacement agent.
2. The preparation method of the quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate according to claim 1, characterized in that, The corn cob-sodium lignin sulfonate-based sulfur-doped carbon quantum dots were prepared by solid-phase calcination, including the following steps: corn cob powder and sodium lignin sulfonate solid powder were ground and mixed, and calcined at 240℃-320℃ for 1.5-4h under an inert protective atmosphere; the calcined product was naturally cooled to room temperature and ground, then ultrapure water was added for ultrasonic extraction, and the uncarbonized solid residue was removed by centrifugation; the supernatant was filtered through a 0.22μm filter membrane; the filtrate was placed in a dialysis bag with a molecular weight cutoff of 1000Da for dialysis to remove small molecule salt impurities, and then freeze-dried to obtain brownish-yellow corn cob-sodium lignin sulfonate-based sulfur-doped carbon quantum dots.
3. The preparation method of the quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate according to claim 1, characterized in that, Step S2 includes: adding sulfur-doped carbon quantum dots and 3-methacryloxypropyltrimethoxysilane into anhydrous ethanol and dispersing them uniformly; stirring the mixture in a closed container at 400-700 r / min for 3-6 h at 65℃-85℃; and removing the solvent by rotary evaporation after the reaction is complete to obtain modified corn cob-lignin sulfonate-based sulfur-doped carbon quantum dots.
4. The preparation method of the quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate according to claim 1, characterized in that, In step S3, the total solute mass fraction in the reaction system is 10%-30%, the pH value is 6-9, the reaction temperature is 10-40℃, the reaction time is 4-8h, and the amount of initiator added accounts for 0.1%-0.6% of the total mass of all organic monomers.
5. The preparation method of the quantum dot-based oil displacement agent based on corn cob and sodium lignin sulfonate according to claim 4, characterized in that, In the initiator, the oxidant is ammonium persulfate, and the reducing agent is sodium bisulfite or sodium formaldehyde sulfoxylate. When the reducing agent is sodium bisulfite, the mass ratio of oxidant to reducing agent is 1:1; when the reducing agent is sodium formaldehyde sulfoxylate, the mass ratio of oxidant to reducing agent is 2:
1.
6. A quantum dot-based oil displacement agent based on corn cob and sodium lignosulfonate, characterized in that, It is prepared by any one of the preparation methods described in claims 1-5.
Citation Information
Patent Citations
Method for synthesizing surface functional group modified carbon quantum dots and application to nano oil displacement
CN111234818A