Chemical deposition methods and vertical chemical deposition equipment
By monitoring film thickness growth data and adjusting the rotation speed in stages, combined with temperature control of internal and external heating components, the problem of film thickness non-uniformity in LPCVD equipment was solved, achieving uniformity and consistency in the silicon wafer deposition process.
Patent Information
- Application Number
- CN202611466706.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-20
- Publication Date
- 2026-11-17
AI Technical Summary
Existing LPCVD equipment suffers from film thickness inhomogeneity during silicon wafer deposition, particularly due to cross-sectional and radial thermal hysteresis caused by hot gas rising and cold gas sinking, which affects film uniformity.
By monitoring the film thickness growth data of silicon wafers, the rotation speed of the wafer carrier assembly is adjusted in stages, and combined with the temperature control of the internal and external heating components, the rotation uniformity and temperature consistency of the silicon wafers at different deposition stages are ensured, and the vertical and radial concentration differences are compensated by using independent heating temperature zones.
It significantly reduces the film thickness non-uniformity within silicon wafers, improves the overall uniformity of the film layer, reduces the film thickness difference between wafers, and enhances the uniformity of deposition.
Smart Images

Figure CN123108538A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of solar cell manufacturing technology, and more particularly to a chemical deposition method and a vertical chemical deposition apparatus. Background Technology
[0002] With the rapid mass production of high-efficiency crystalline silicon solar cells (HJT, TOPCon, BC, etc.), LPCVD (low-pressure chemical vapor deposition) for tunneling oxide layers and doped polycrystalline silicon layers has become a key process for improving cell conversion efficiency. LPCVD equipment, with its advantages of dense and uniform films and suitability for mass production, has become the mainstream equipment for amorphous / polycrystalline silicon thin film deposition and is widely used in the large-scale manufacturing of crystalline silicon cells.
[0003] Currently, the LPCVD deposition process for crystalline silicon solar cells in the industry generally uses horizontal LPCVD equipment. The cavity is usually tubular, with heating elements on the outer wall, which are wound around the outside of the tube in the form of heating wires to provide the most uniform thermal environment possible. The silicon wafer is supported by a quartz boat and inserted vertically into the quartz boat, and is left to stand in the cavity to complete the entire deposition process. Although the technology is mature, it has a fatal flaw: due to the natural convection effect of hot gas rising and cold gas sinking, there is a significant "hot at the top and cold at the bottom" phenomenon in the cross-section of the furnace tube, resulting in significant differences in film thickness between the upper and lower regions of the same silicon wafer; moreover, the heat dissipates quickly at both ends of the furnace tube, while the temperature in the middle is high, leading to large differences in film thickness uniformity. To address this issue, some LPCVD deposition processes employ vertical LPCVD equipment with internal and external heating to avoid the top-heating and bottom-cooling phenomenon of horizontal LPCVD equipment. This also avoids the problem of the cavity wall temperature being much higher than the center due to the heating wire wrapped around the outside of the tube, resulting in severe radial thermal hysteresis. However, while this vertical LPCVD equipment improves the uniformity of deposition to some extent, the silicon wafer also undergoes dynamic changes during the deposition process. Current technologies do not address these changes to control the uniformity of deposition, leaving room for further improvement in film thickness uniformity.
[0004] Therefore, how to eliminate the film thickness difference caused by the dynamic changes of the deposited film during the deposition process is a technical problem that urgently needs to be solved in this field. Summary of the Invention
[0005] To address the technical problem of uneven film thickness caused by neglecting dynamic changes during the deposition process in existing silicon wafer deposition technologies, this invention proposes a chemical deposition method and a vertical chemical deposition apparatus.
[0006] The first aspect of the present invention provides a chemical deposition method, comprising:
[0007] The wafer carrier assembly containing the silicon wafer is fed into the deposition chamber, and the deposition chamber is evacuated.
[0008] Deposition gas is introduced into the air inlet of the deposition chamber, and the deposition chamber is heated so that the temperature and pressure inside the deposition chamber reach the deposition conditions.
[0009] The film thickness growth data of the silicon wafer is monitored, the deposition stage of the silicon wafer is determined based on the film thickness growth data, and the wafer carrier assembly is controlled to rotate at different speeds according to different deposition stages.
[0010] Furthermore, the deposition stages of the silicon wafer include a nucleation stage, a rapid growth stage, and a densification stage; the rotation speed of the wafer carrier assembly is: rapid growth stage > densification stage > nucleation stage.
[0011] Furthermore, the air inlet of the deposition chamber includes multiple sets evenly distributed around the deposition chamber, and each set of air inlets includes at least one air inlet corresponding to each layer of the wafer assembly loading boat; the air outlet of the deposition chamber is located at the center of the bottom and / or top of the deposition chamber.
[0012] Further, determining the deposition stage of the silicon wafer based on the film thickness growth data includes: obtaining a film thickness versus time curve through optical monitoring or historical sampling data; calculating the film thickness growth rate and the rate of change of the growth rate based on the curve; using the inflection point where the rate of change changes from positive to negative, or the inflection point when it approaches zero, as the boundary point between the nucleation stage and the rapid growth stage; and using the inflection point where the negative amplitude of the rate of change is greater than a preset amplitude as the boundary point between the rapid growth stage and the densification stage.
[0013] Furthermore, the rotational speed of the wafer assembly in each deposition stage is determined as follows: any plane perpendicular to the rotational axis of the wafer assembly is defined as the rotational plane; the rotational plane is divided into multiple dense sector regions and multiple sparse sector regions according to the position of the air inlet, wherein the central angles of each dense sector region and each sparse sector region are equal; the rotational speed of each deposition stage is determined according to the duration of each deposition stage and the number of air inlets, such that the duration of each deposition stage is an integer multiple of the rotational period of the wafer assembly in that deposition stage, and within the same deposition stage, the cumulative residence time of each silicon wafer in the dense sector region is equal, and the cumulative residence time in the sparse sector region is equal, thereby ensuring that the deposition of each silicon wafer is uniform in each deposition stage, and thus ensuring that the overall deposition of each silicon wafer is uniform.
[0014] Furthermore, the rotational speed of the slide assembly during the rapid growth phase is 5-8 rpm; and / or, the rotational speed of the slide assembly during the densification phase is 3-4 rpm; and / or, the rotational speed of the slide assembly during the nucleation phase is 1-2 rpm.
[0015] Further, heating the deposition chamber includes: heating the deposition chamber by means of multiple independent heating temperature zones segmented along the axial direction of the deposition chamber, each of the independent heating temperature zones corresponding to the silicon wafer bearing areas of different height layers on the wafer carrier assembly; during the deposition process, the temperature setpoint of each of the independent heating temperature zones is independently adjusted to compensate for the influence of the vertical gas concentration difference in the deposition chamber on the deposition rate of the silicon wafers of each height layer.
[0016] Furthermore, each of the independent heating temperature zones includes an internal heating component and an external heating component with independent temperature control. The carrier assembly is located between the internal heating component and the external heating component, with the side closer to the internal heating component being the central region and the side closer to the external heating component being the edge region. The method further includes: using the effective average value of multiple temperature points collected within a complete rotation cycle as the temperature feedback value for the corresponding independent heating temperature zone; when the deviation between the temperature feedback value and the preset target temperature value exceeds a set threshold, adjusting the power ratio of the internal heating component and the external heating component in the independent heating temperature zone to compensate for the temperature difference between the edge region and the central region.
[0017] A second aspect of the present invention provides a vertical chemical deposition apparatus, comprising:
[0018] The sedimentation chamber has an air inlet and an air outlet;
[0019] A gas system for supplying deposition gas to the inlet of the deposition chamber and recovering deposition gas from the outlet;
[0020] The wafer carrier assembly has multiple loading boats along the axial direction of the deposition chamber for holding the silicon wafers to be deposited;
[0021] A driving component that drives the wafer assembly to rotate about its rotation center;
[0022] Temperature control unit for controlling the temperature of the deposition chamber;
[0023] A film thickness monitoring component is used to monitor the film thickness growth data of the silicon wafer;
[0024] The controller controls the gas system, drive components, and temperature components based on the film thickness growth data monitored by the film thickness monitoring component.
[0025] Compared with the prior art, the present invention has the following beneficial effects:
[0026] By monitoring the film thickness growth data of silicon wafers, the deposition stage of the wafer is determined, and the rotation speed is adjusted accordingly. The staged variable-speed rotation flexibly adjusts the rotation speed based on the uniformity requirements of different stages of film growth, balancing nucleation uniformity and deposition homogenization, resulting in more uniform film thickness growth at each stage. Furthermore, this invention utilizes the time averaging effect to transform the spatially fixed thermal and flow field differences of the silicon wafer into a process quantity that homogenizes over time. The wafer rotation causes it to periodically pass through regions with higher or lower temperatures and higher or lower gas concentrations, making the cumulative deposition amount within the equivalent process time tend to be equal, significantly reducing intra-wafer film thickness non-uniformity. For example, each silicon wafer traverses the deposition chamber angularly with the carrier assembly, eliminating systematic film thickness deviations at different boat positions, making the deposition environment of all silicon wafers more consistent. Moreover, layer temperature compensation and internal / external power ratio adjustment address systematic differences in the vertical and radial directions respectively, working in conjunction with the angular homogenization of rotation to achieve uniform deposition across the entire region. Attached Figure Description
[0027] The present invention will now be described in detail with reference to the embodiments and accompanying drawings, wherein:
[0028] Figure 1 This is a top view of a vertical chemical deposition apparatus provided in an embodiment of the present invention;
[0029] Figure 2 This is a flowchart of a deposition method according to an embodiment of the present invention.
[0030] Explanation of reference numerals in the attached figures:
[0031] 1. Deposition chamber; 2. Heating assembly; 3. Boat support; 4. Rotating base. Detailed Implementation
[0032] To make the technical problems to be solved, the technical solutions, and the beneficial effects of the present invention clearer, the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0033] like Figure 1As shown, an embodiment of the present invention provides a vertical chemical deposition apparatus, including a deposition chamber 1, a gas system, a wafer carrier assembly, a drive assembly, a temperature assembly, a film thickness monitoring assembly, and a controller. The deposition chamber adopts an annular cavity, and heating assemblies 2 are provided on both its inner and outer walls. Six sets of boat supports 3 are arranged in a ring evenly inside the cavity. Each set of boat supports 3 carries a wafer carrier assembly. Each wafer carrier assembly has three loading boats (upper, middle, and lower) placed vertically. The loading boats are used to carry the solar cell silicon wafers (also referred to as silicon wafers) to be deposited. All boat supports 3 are fixedly mounted on an integral rotating base 4. The rotating base 4 is driven by the drive assembly at the bottom of the cavity, causing all boat supports 3 and silicon wafers to rotate smoothly around the central axis of the cavity.
[0034] The air inlets of the sedimentation chamber 1 are located around the outer wall of the chamber, in multiple groups and evenly distributed. The opening height of each group of air inlets corresponds to the upper, middle, and lower layers of small boats, ensuring that each layer of small boats receives a direct and equal amount of gas supply. The air outlets are located at the center of the top and / or bottom of the sedimentation chamber 1. The reaction gas is transported into the sedimentation chamber by the gas system through the air inlets and recovered through the air outlets. The gas diffuses and flows from the periphery to the center within the chamber.
[0035] The wafer carrier assembly is provided with a multi-layer loading boat along the axial direction of the deposition chamber to hold the silicon wafer to be deposited; the drive assembly drives the wafer carrier assembly to rotate around its rotation center, that is, around the center of the cavity.
[0036] The temperature component controls the temperature of the deposition chamber, specifically including multiple independent heating zones segmented along the axial direction of the deposition chamber. Each independent heating zone corresponds to the silicon wafer bearing area of a different height layer on the wafer carrier assembly, and each independent heating zone includes an internal heating component and an external heating component with independent temperature control.
[0037] Film thickness monitoring components are used to monitor film thickness growth data of silicon wafers, for example, by employing online optical monitoring devices.
[0038] The controller controls the gas system, drive components, and temperature components based on the film thickness growth data monitored by the film thickness monitoring component.
[0039] like Figure 2 As shown, based on the above-described vertical chemical deposition equipment, a chemical deposition method according to an embodiment of the present invention includes the following steps:
[0040] Step S1: The wafer carrier assembly containing the silicon wafer is fed into the deposition chamber, and the deposition chamber is evacuated to achieve the required vacuum level. The drive assembly can be started first to rotate the wafer carrier assembly to a preset starting position, such as a wafer carrier assembly being positioned in the furnace opening alignment area, to establish a reference orientation for the rotational movement in the subsequent deposition stage.
[0041] Step S2: Introduce deposition gas into the air inlet of the deposition chamber and heat the deposition chamber to bring the temperature and pressure inside the deposition chamber to the deposition conditions, such as a deposition temperature of 560℃-620℃ and maintaining the deposition pressure required for the process inside the chamber.
[0042] Step S3: Monitor the film thickness growth data of the silicon wafer, determine the deposition stage of the silicon wafer based on the film thickness growth data, and control the wafer carrier assembly to rotate at different speeds according to different deposition stages. Thin film deposition is performed while the silicon wafer is rotating, so that the silicon wafer periodically traverses different positions in the cavity, and the local differences in the thermal field and airflow field are homogenized in a time-averaged manner.
[0043] This invention improves the uniformity of deposition on silicon wafers by using different rotation speeds at different deposition stages.
[0044] Specifically, the deposition stages of a silicon wafer include the nucleation stage, the rapid growth stage, and the densification stage, which are objectively divided based on the film thickness growth curve. The rotation speed of the wafer carrier assembly is: rapid growth stage > densification stage > nucleation stage.
[0045] Specifically, the film thickness-time curve d(t) is obtained through online optical monitoring or offline sampling, and the growth rate v(t) of the film thickness and the rate of change of the growth rate a(t) are calculated.
[0046] The inflection point where a(t) changes from positive to negative, or the inflection point when it approaches zero, is taken as the dividing point between the nucleation period and the rapid growth period.
[0047] The inflection point where the negative amplitude of a(t) exceeds a preset amplitude is used as the boundary between the rapid growth phase and the densification phase. This objectively divides the deposition process into three physical stages, rather than artificially setting the duration.
[0048] Different rotation speeds are used in each deposition stage, and the configuration logic is as follows:
[0049] The nucleation stage is sensitive to microscopic temperature and concentration fluctuations; high-frequency disturbances can interfere with uniform nucleus formation, so low-speed rotation is used to maintain environmental stability. The rapid growth stage is mainly affected by macroscopic thermal and gas field distributions, requiring high-frequency traversal of orientations to eliminate macroscopic differences through time averaging, thus employing high-speed rotation. The densification stage requires a stable surface atomic migration environment, so medium-speed rotation is used to reduce mechanical disturbances. In a specific example, the rotation speed during the nucleation stage is 1-2 rpm, during the rapid growth stage it is 5-8 rpm, and during the densification stage it is 3-4 rpm. The duration of each stage is estimated based on the target film thickness and deposition rate, and fine-tuned through orthogonal experiments within the determined inflection point range to lock in the combination of duration and rotation speed that minimizes film thickness non-uniformity.
[0050] Furthermore, the reactant gas diffuses from the surrounding inlets toward the center and is then extracted from the outlets located at the top or bottom of the deposition chamber. This creates three types of inhomogeneities within the deposition chamber: angular concentration difference, where the concentration is high near the inlets and low away from them; radial concentration difference, where the concentration is high at the periphery and low at the center; and vertical concentration difference, where there are systematic differences in gas concentration at different heights.
[0051] This invention utilizes a rotating wafer carrier assembly to traverse all angular positions in the horizontal plane, primarily focusing on homogenization in the angular dimensions. Assuming N groups of air inlets, each rotation of the silicon wafer will experience N concentration peaks and valleys corresponding to the air inlets. Over the total deposition time, the cumulative residence time of each silicon wafer at all angular positions tends to be consistent, resulting in all silicon wafers at the same height layer obtaining the same angular integral concentration, thus eliminating inter-wafer differences.
[0052] Furthermore, any plane perpendicular to the rotation axis of the wafer assembly is defined as the rotation plane. Based on the location of the air inlet, the rotation plane is divided into multiple dense and dilute sectors. The dense sector is an angular region near the air inlet with a high gas concentration, while the dilute sector is an angular region far from the air inlet with a low gas concentration. The central angles of all dense and dilute sectors are equal, although the central angles of the dense and dilute sectors may or may not be equal. Based on the duration of each deposition stage and the number of air inlets, the rotation speed of each deposition stage is determined, ensuring that the duration of each deposition stage is an integer multiple of the rotation cycle of the wafer assembly within that deposition stage. Because each silicon wafer is mounted at a different angular position on the carrier assembly, the cumulative dwell time of each silicon wafer in the dense sector and the cumulative dwell time in the sparse sector will be equal only when each silicon wafer completes an integer number of rotation cycles in a single deposition stage. Therefore, the deposition of each silicon wafer is uniform in a single deposition stage, and this is true for each deposition stage, resulting in uniform deposition of each silicon wafer as a whole.
[0053] Rotation cannot directly eliminate the concentration difference in the vertical direction. In a further embodiment, this is addressed through a layered design.
[0054] On the one hand, the air inlet opening height precisely corresponds to the upper, middle, and lower layers of small boats, ensuring that each layer of small boats receives a direct and equal amount of gas supply. On the other hand, multiple independent heating temperature zones are segmented along the axial direction of the deposition chamber. Each temperature zone is radially aligned with the silicon wafer bearing area of the corresponding height layer on the wafer carrier assembly. In one embodiment, three independent heating temperature zones (upper, middle, and lower) are segmented along the axial direction, with each independent heating temperature zone corresponding one-to-one with a layer of small boats. During the deposition process, the temperature setpoint of each temperature zone is independently adjusted to compensate for the influence of vertical concentration differences on the deposition rate of silicon wafers at each height layer. Vertical differences are systematic errors. Rotation ensures that all silicon wafers within the same layer have consistent conditions. Vertical differences are only manifested as uniform interlayer offset and can be eliminated through the aforementioned layering temperature compensation.
[0055] For radial temperature difference, each independent heating zone includes an internal heating component and an external heating component with independent temperature control. The controlled objects are the internal and external heating components at the same axial height (same temperature zone), and the power ratio is calculated independently for each axial temperature zone. Because the wafer assembly rotates continuously during the process while the thermocouple position remains fixed, the rotating boat support blades, wafer edges, or support structures periodically pass through the thermocouple detection area, causing momentary obstruction of thermal radiation or local airflow disturbances, resulting in periodic noise in the single-point instantaneous temperature data. Therefore, the controller's data sampling period is set to be synchronized with the wafer assembly's rotation period, i.e., the sampling period is an integer multiple of the rotation period. The controller does not directly use the instantaneous temperature measurement value at a certain moment, but instead performs digital filtering on multiple temperature points collected within an integer number of complete rotation cycles, using the effective average of the periods as the true feedback of the current circumferential average temperature (in other embodiments, an arithmetic average can also be used).
[0056] Based on this, the power ratio adjustment of the inner and outer heating components in the corresponding temperature zone is triggered only when the deviation between the effective average value of the aforementioned rotation cycle and the preset target temperature value exceeds the set control dead zone (e.g., ±0.5℃). If the central area is too cold, the power of the inner heating component is increased; if the edge area is too cold, the power of the outer heating component is increased. The power ratio is not directly set, but is the result of the voltage / current ratio dynamically calculated by the PID algorithm. This mechanism ensures that each adjustment of the power ratio is based on the global average thermal field deviation over the entire circumferential space, rather than spurious deviations caused by local obstruction or instantaneous airflow interference, thereby effectively eliminating feedback noise caused by rotation and improving the stability and deposition uniformity of radial temperature control.
[0057] In a further embodiment, after deposition is completed, the reaction gas supply is stopped, but the drive assembly can continue to run for a period of time before stopping, for example, for 1-3 minutes, so that the silicon wafer continues to rotate during the initial cooling phase to ensure uniform heat dissipation. Afterward, the drive assembly is shut down, and subsequent operations such as vacuuming, gas backfilling, cooling, and unloading are performed. This achieves directional homogenization throughout the entire process from material feeding and alignment to deposition and cooling.
[0058] Referring to Tables 1 and 2 below, experiments show that, compared with static deposition on silicon wafers, the rotating homogenization deposition method of this invention, after the silicon wafer periodically passes through regions with higher or lower temperatures and higher or lower gas concentrations, tends to have equal cumulative deposition amounts within the equivalent process time. The intra-wafer film thickness uniformity can be reduced by more than 50% compared with the traditional horizontal equipment deposition method. Specifically, in terms of overall intra-wafer uniformity, the overall intra-wafer uniformity of this invention is reduced by 78.7%. Even when comparing the worst results, the uniformity within a single wafer is reduced by about 75%, and when comparing the best results, the uniformity within a single wafer is reduced by about 91.5%. The inter-wafer uniformity is reduced by 42.86%. As each silicon wafer traverses the deposition chamber along the angular orientation of the carrier assembly, the systematic film thickness deviation between silicon wafers in different boat positions is basically eliminated, and the inter-wafer consistency is significantly improved.
[0059]
[0060] Table 1 Film thickness data of the present invention
[0061]
[0062] Table 2 Film thickness data for horizontal LPCVD equipment
[0063] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A method of electroless deposition, characterized in that, include: The wafer carrier assembly containing the silicon wafer is fed into the deposition chamber, and the deposition chamber is evacuated. Deposition gas is introduced into the air inlet of the deposition chamber, and the deposition chamber is heated so that the temperature and pressure inside the deposition chamber reach the deposition conditions. The film thickness growth data of the silicon wafer is monitored, the deposition stage of the silicon wafer is determined based on the film thickness growth data, and the wafer carrier assembly is controlled to rotate at different speeds according to different deposition stages.
2. The electroless deposition method of claim 1, wherein, The deposition stages of the silicon wafer include the nucleation stage, the rapid growth stage, and the densification stage; the rotation speed of the wafer carrier assembly is: rapid growth stage > densification stage > nucleation stage.
3. The electroless deposition method according to claim 2, wherein The air inlet of the deposition chamber includes multiple sets evenly distributed around the deposition chamber, and each set of air inlets includes at least one air inlet corresponding to each layer of the substrate loading boat; the air outlet of the deposition chamber is located at the center of its bottom and / or top.
4. The electroless deposition method according to claim 3, wherein The deposition stages of the silicon wafer are determined based on the film thickness growth data, including: The relationship curve between film thickness and time can be obtained by optical monitoring or historical sampling data; The growth rate of film thickness and the rate of change of growth rate are calculated based on the relationship curve. The inflection point where the rate of change turns from positive to negative, or the inflection point when it approaches zero, is taken as the dividing point between the nucleation period and the rapid growth period. The inflection point where the negative amplitude of the rate of change is greater than a preset amplitude is taken as the dividing point between the rapid growth period and the densification period.
5. The electroless deposition method according to claim 4, wherein The rotational speed of the wafer assembly at each deposition stage is determined as follows: Any plane perpendicular to the rotation center axis of the slide assembly is defined as the rotation plane. According to the position of the air inlet, the rotation plane is divided into multiple rich sector regions and multiple poor sector regions, wherein the central angle of each rich sector region is equal and the central angle of each poor sector region is equal. Based on the duration of each deposition stage and the number of air inlets, the rotation speed of each deposition stage is determined, such that the duration of each deposition stage is an integer multiple of the rotation cycle of the wafer assembly within that deposition stage, and within the same deposition stage, the cumulative dwell time of each silicon wafer in the dense sector is equal, and the cumulative dwell time in the sparse sector is equal.
6. The electroless deposition method according to any one of claims 1 to 5, wherein The rotational speed of the slide assembly during the rapid growth phase is 5-8 rpm; and / or, the rotational speed of the slide assembly during the densification phase is 3-4 rpm; and / or, the rotational speed of the slide assembly during the nucleation phase is 1-2 rpm.
7. The electroless deposition method of claim 1, wherein, Heating the deposition chamber includes: heating the deposition chamber by means of multiple independent heating temperature zones segmented along the axial direction of the deposition chamber, each of the independent heating temperature zones corresponding to the silicon wafer bearing area of different height layers on the wafer carrier assembly; during the deposition process, the temperature set value of each of the independent heating temperature zones is independently adjusted to compensate for the influence of the vertical gas concentration difference in the deposition chamber on the deposition rate of the silicon wafers of each height layer.
8. The chemical deposition method as described in claim 7, characterized in that, Each of the independent heating temperature zones includes an internal heating component and an external heating component with independent temperature control. The substrate assembly is located between the internal heating component and the external heating component, with the side closer to the internal heating component being the central region and the side closer to the external heating component being the edge region. The chemical deposition method further includes: using the effective average value of multiple temperature points collected within a complete rotation cycle as the temperature feedback value for the corresponding independent heating temperature zone; when the deviation between the temperature feedback value and the preset target temperature value exceeds a set threshold, adjusting the power ratio of the internal heating component and the external heating component in the independent heating temperature zone to compensate for the temperature difference between the edge region and the central region.
9. A vertical chemical deposition apparatus, characterized in that, include: The sedimentation chamber has an air inlet and an air outlet; A gas system for supplying deposition gas to the inlet of the deposition chamber and recovering deposition gas from the outlet; The wafer carrier assembly has multiple loading boats along the axial direction of the deposition chamber for holding the silicon wafers to be deposited; A driving component that drives the wafer assembly to rotate about its rotation center; Temperature control unit for controlling the temperature of the deposition chamber; A film thickness monitoring component is used to monitor the film thickness growth data of the silicon wafer; The controller, according to any one of claims 1 to 8, controls the gas system, the drive component, and the temperature component based on the film thickness growth data monitored by the film thickness monitoring component.