A fabrication apparatus and layer-by-layer fabrication method for a microchannel array
By using a fabrication device with a transparent conductive substrate and a cutout template, the layer-by-layer fabrication of photoresist and electroforming solution was achieved, solving the problems of low efficiency and poor precision in the existing technology. This resulted in the fabrication of a microchannel array with a high aspect ratio, suitable for heat dissipation of high-performance computing chips.
Patent Information
- Application Number
- CN202611402647.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-10
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies make it difficult to integrate photoresist patterning and electroforming metal filling processes in the same workstation, resulting in low efficiency and poor performance in microchannel array fabrication. Furthermore, the transfer process of photoresist and electroforming solution can easily introduce mechanical damage and positional deviations.
A fabrication apparatus employing a transparent conductive substrate and a perforated template is used to achieve layer-by-layer fabrication of photoresist and electroforming solution through the lifting and lowering movement of the perforated template. Passive isolation and self-pumping liquid exchange of the liquid are achieved by utilizing isolation gaps to keep the substrate fixed. The channel wall structure is optimized by combining different electroforming parameters.
It improves the fabrication efficiency and effectiveness of microchannel arrays, reduces mechanical damage and positional deviations, achieves high-precision interlayer alignment, and has an aspect ratio of over 15:1, meeting the heat dissipation requirements of high-performance computing chips.
Smart Images

Figure CN123108670A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of microchannel array fabrication technology, and in particular to a fabrication apparatus and layer-by-layer fabrication method for microchannel arrays. Background Technology
[0002] As the thermal design power (TDP) of high-performance computing chips (such as GPUs and AI accelerator chips) continues to rise, liquid cooling solutions have become the mainstream thermal management method for data centers and high-power electronic devices. As the core heat exchange component in a liquid cooling system, the heat dissipation capacity of the liquid cooler plate largely depends on the structural parameters of its internal microchannels, especially the aspect ratio (the ratio of channel depth to width). A larger aspect ratio results in a larger heat exchange area, a higher heat transfer coefficient under the same flow rate conditions, and a lower overall thermal resistance of the liquid cooler plate.
[0003] For microchannel arrays made of metals (such as copper), existing fabrication methods mainly include three categories: precision mechanical milling, laser processing, and photoresist-masked electroforming. Mechanical milling is limited by tool size, and the processing difficulty increases sharply when the channel width is less than about 0.3 mm. Laser processing has heat-affected zones and recasting layer problems at the bottom of deep holes. The principle of photoresist-masked electroforming is as follows: first, photoresist masking walls (defining the wall positions of the microchannels) are formed on a conductive substrate by photolithography; then, metal is electroformed and deposited in the gaps between the photoresist masking walls; finally, the photoresist is removed to obtain the metal microchannel array. This method can theoretically achieve arbitrary channel geometry, and the dimensional accuracy of the channel walls is guaranteed by the photolithography process.
[0004] Integrating photoresist patterning and electroforming metal filling processes at the same workstation while maintaining substrate stability throughout the multilayer fabrication process remains a technical challenge with no mature solution yet. In conventional operations, photoresist patterning requires applying liquid photoresist to the work surface and curing it using UV exposure. During this process, the work surface should avoid contact with the acidic electroforming solution; otherwise, metal ions and acids in the solution will interfere with the photoresist's cross-linking reaction and contaminate the photoresist bath. Electroforming metal filling requires immersing the work surface in the acidic electroforming solution and electrodepositing metal. During this process, it is crucial to prevent photoresist contamination of the electroforming solution and uncured photoresist from covering the deposited metal surface. Alternating between these two processes means the liquid environment of the work surface needs to be rotated accordingly, which can easily lead to poor fabrication results and low work efficiency.
[0005] Therefore, there is an urgent need in the field for a microchannel array fabrication device and a layer-by-layer fabrication method to solve the above problems. Summary of the Invention
[0006] The purpose of this invention is to provide a microchannel array fabrication apparatus and a layer-by-layer fabrication method to solve the problems existing in the prior art and improve work efficiency and fabrication effect.
[0007] To achieve the above objectives, the present invention provides the following solution: This invention discloses a fabrication apparatus for a microchannel array, comprising: A transparent substrate, on which a transparent conductive substrate is placed; A cutout template is located above the transparent conductive substrate. The cutout template has a cutout pattern and is connected to a lifting drive device. The lifting drive device is used to move the cutout template closer to or away from the transparent conductive substrate. A photoresist supply source, which is capable of introducing liquid photoresist into the hollowed-out pattern; A photoresist curing apparatus, wherein the photoresist curing apparatus is used to cure liquid photoresist on the transparent conductive substrate; An electroforming solution supply source, wherein the electroforming solution supply source is used to supply electroforming solution to the electroforming space on the transparent conductive substrate; Electroforming apparatus, the electroforming apparatus being used to deposit metal ions in the electroforming liquid within the electroforming space; and A residual medium treatment device includes an electroforming liquid discharge channel, through which the electroforming liquid in the electroforming space can be discharged.
[0008] Preferably, the electroforming apparatus includes an electroforming power source, the positive electrode of which is electrically connected to the electroforming anode, the electroforming anode being fixed on the hollow template, the electroforming anode being able to move closer to or further away from the transparent conductive substrate synchronously with the hollow template, and the negative electrode of the electroforming power source being electrically connected to the transparent conductive substrate.
[0009] Preferably, the residual medium treatment device can also discharge uncured liquid photoresist.
[0010] Preferably, it further includes a vibration device for applying vibration to at least one of the cutout template, the transparent conductive substrate, or the liquid photoresist when supplying liquid photoresist to the cutout pattern.
[0011] Preferably, it also includes a pressure detection device and a control unit, wherein the pressure detection device is used to measure the pressure within the electroforming space; The control unit is connected to the pressure detection device and the lifting drive device respectively. The control unit determines the fluid isolation state of the isolation gap based on the pressure detection signal obtained by the pressure detection device, and controls the lifting drive device to adjust the position of the hollow template when the fluid isolation state does not meet the preset conditions.
[0012] Preferably, the inner wall of the hollow pattern has a stronger wettability to the liquid photoresist than the upper surface of the hollow template.
[0013] Preferably, it further includes a temperature regulating device for regulating the temperature of the liquid photoresist and / or the electroforming solution.
[0014] This invention discloses a layer-by-layer fabrication method for microchannel arrays, based on the aforementioned fabrication apparatus for microchannel arrays, comprising the following steps: S1. Photoresist patterning process: The cutout template is moved in a direction close to the transparent conductive substrate until the bottom surface of the cutout template abuts the transparent conductive substrate or the top surface of the formed structure; liquid photoresist is supplied into the cutout pattern; the photoresist curing device is started to cure the photoresist to form a masking wall attached to the transparent conductive substrate or the formed structure. S2, Electroforming Metal Filling Process: The cutout template is moved away from the transparent conductive substrate until the bottom surface of the cutout template is lower than the top surface of the newly cured masking wall, so that the upper end of the masking wall is embedded in the interior of the cutout pattern near the transparent conductive substrate. An isolation gap is formed between the inner wall of the cutout pattern and the outer wall of the masking wall. The isolation gap can prevent the electroforming liquid in the electroforming space from flowing into the cutout pattern. During the movement of the cutout template away from the transparent conductive substrate, the electroforming liquid in the electroforming liquid supply source can be drawn into the electroforming space. The electroforming power supply is turned on to deposit metal in the electroforming space. After the metal is deposited to a preset thickness, the cutout template is moved closer to the transparent conductive substrate, and the residual electroforming liquid in the electroforming space is discharged through the electroforming liquid discharge channel. S3. Repeat steps S1-S2 until the formed metal structure reaches the predetermined number of layers or the predetermined height. S4. Remove the masking walls formed by the stacking of each layer to complete the fabrication of the entire microchannel array.
[0015] Preferably, after each step S2 is completed, the top of the electroformed metal formed in this step is lower than the top surface of the shielding wall formed in step S1.
[0016] Preferably, different electroforming parameters are used in at least two steps S2, the electroforming parameters including at least one of current density and electroforming solution temperature.
[0017] The present invention achieves the following technical effects compared to the prior art: The transparent conductive substrate in this invention is fixed throughout the entire fabrication process: the transparent conductive substrate remains in the same position throughout the layer-by-layer fabrication process, eliminating the need for repeated transfers between the photoresist bath and the electroforming bath. This fundamentally eliminates the risk of mechanical damage to the masking wall caused by transfers and the cumulative interlayer positional deviation introduced by realignment. The interlayer alignment accuracy is no greater than 1 micrometer, far superior to the ±5 to 12 micrometer accuracy of repeated transfer schemes.
[0018] The hollow template in this invention can be used for multiple purposes: the hollow template can realize four functions in one reciprocating motion: pattern definition, electroforming space enclosure, passive isolation of two liquids and pumping drainage, which greatly simplifies the device structure and eliminates the need for independent valve group switching, liquid circuit switching system and cleaning system.
[0019] Overlapping seal: The high flow resistance generated by the narrow annular isolation gap between the shielding wall and the hollow pattern is used to achieve passive fluid isolation between the electroforming solution and the photoresist.
[0020] Self-pumping liquid replacement: The reciprocating motion of the hollow template drives the intake and discharge of liquid. When it moves away from the transparent conductive substrate, the electroforming space volume expands to generate negative pressure to draw in new liquid. When it approaches the transparent conductive substrate, the volume shrinks to discharge waste liquid. It works in conjunction with a one-way valve to achieve liquid flow direction.
[0021] Improved heat dissipation: Different electroforming parameters can be used in different layers during layer-by-layer electroforming to create a grain size gradient along the channel wall height direction, optimizing the thermal conductivity distribution of the channel walls. The resulting microchannel arrays can achieve aspect ratios of 15:1 or higher, meeting the heat dissipation requirements of high-performance computing chips. Attached Figure Description
[0022] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0023] Figure 1 This is a schematic diagram of the fabrication apparatus for the microchannel array in Example 1; Figure 2 This is a schematic diagram of photoresist being injected onto a transparent conductive substrate and formed into a masking wall in the layer-by-layer fabrication method of the microchannel array in Example 2. Figure 3 This is a schematic diagram of injecting electroforming liquid into the electroforming space in the layer-by-layer preparation method of the microchannel array in Example 2; Figure 4This is a schematic diagram of the electroforming solution deposition of electroformed metal in the layer-by-layer fabrication method of microchannel array in Example 2; Figure 5 This is a schematic diagram showing the process after removing residual electroforming solution in the layer-by-layer fabrication method of the microchannel array in Example 2; Figure 6 In the layer-by-layer fabrication method of the microchannel array in Example 2, photoresist is applied to the already formed structure. Figure 7 In the layer-by-layer fabrication method of microchannel array in Example 2, electroforming solution is injected again onto the electroformed metal; In the figure: 1-Transparent substrate; 2-Transparent conductive substrate; 3-Knurled template; 301-Knurled pattern; 4-Lifting drive device; 5-Photoresist supply source; 6-Electroforming solution supply source; 7-Mask wall; 8-Enclosure plate; 9-Electroforming metal. Detailed Implementation
[0024] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0025] The purpose of this invention is to provide a microchannel array fabrication apparatus and a layer-by-layer fabrication method to solve the problems existing in the prior art and improve work efficiency and fabrication effect.
[0026] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, the present invention will be further described in detail below with reference to the accompanying drawings and specific embodiments.
[0027] Example 1 like Figure 1 As shown, this embodiment provides a fabrication apparatus for a microchannel array, comprising: A transparent substrate 1 is provided, and a transparent conductive substrate 2 is placed on the transparent substrate 1. The transparent substrate 1 is made of quartz glass; however, those skilled in the art can also use borosilicate glass, sapphire, or other hard transparent materials that allow the corresponding exposure light to pass through. In this embodiment, the transparent conductive substrate 2 is made of FTO conductive glass, i.e., a fluorine-doped tin oxide conductive layer is formed on the surface of the transparent glass substrate. Alternatively, the transparent conductive substrate 2 can also be made of ITO conductive glass, AZO conductive glass, etc. It should be noted that the transparency referred to in this embodiment means that the corresponding components (the central areas of the transparent substrate 1 and the transparent conductive substrate 2) can transmit light of the wavelength required for curing the liquid photoresist; it does not require that the components be transparent to all visible light.
[0028] A perforated template 3 is located above the transparent conductive substrate 2, and a perforated pattern 301 is provided on the perforated template 3. The cutout pattern 301 extends through the entire cutout template 3 along its thickness direction, and the planar outline of the cutout pattern 301 corresponds to the planar outline of the photoresist mask 7 to be formed. Specifically, this means that after the liquid photoresist enters the cutout pattern 301 and solidifies, it can form a photoresist mask 7 that matches the shape defined by the cutout pattern 301. The two can have basically the same planar outline, or the dimensions can be set according to the curing shrinkage of the photoresist, the demolding gap, or the processing tolerance. The planar layout of the cutout pattern 301 is the common equal-spacing strip, but in addition, it can be designed as a variable-spacing pattern (such as a higher channel density in the hot spot area of the chip), a radial pattern, or other non-uniform patterns according to heat dissipation requirements. In addition to rectangles, the cross-sectional shape of the cutout pattern 301 can be a trapezoid (narrower at the top and wider at the bottom), an inverted trapezoid (wider at the top and narrower at the bottom), or a rounded rectangle. The material of the cutout template 3 is monocrystalline silicon. However, those skilled in the art can also choose electroformed nickel (more wear-resistant, suitable for mass production), PDMS (suitable for curved or non-planar substrates), or amorphous alloys (nanoscale surface precision and excellent demolding properties). The cutout pattern 301 can be processed using the DRIE process, or laser cutting, precision electroforming, or LIGA processes. The cutout template 3 is connected to a lifting drive device 4, which moves the cutout template 3 closer to or further away from the transparent conductive substrate 2. The lifting drive device 4 can be a common ball screw module, including a rotary motor. The output shaft of the rotary motor is connected to a lead screw, and a nut seat is threaded onto the lead screw. The ball screw module also includes a slide rail. When the rotary motor is started, it drives the nut seat to move reciprocally linearly along the slide rail. The cutout template 3 is then mounted on the nut seat. Of course, those skilled in the art can also replace the lifting drive device 4 with a nano-displacement stage (higher precision), a voice coil motor direct drive (higher response speed), or a pneumatic actuator (i.e., a cylinder) to meet different precision and speed requirements.
[0029] The photoresist supply source 5 is a container filled with liquid photoresist. It allows liquid photoresist to be introduced into the cutout pattern 301. Specifically, the outlet of the photoresist supply source 5 is connected to a photoresist delivery tube, which is equipped with a micro-pump. Driven by the micro-pump, the photoresist in the photoresist supply source 5 is delivered to the cutout pattern 301 through the photoresist delivery tube. Since the cutout template 3 moves up and down during operation, to prevent changes in the relative position between the photoresist delivery tube and the cutout pattern 301 due to changes in the position of the cutout template 3, the photoresist supply source 5 can be fixed to the lifting drive device 4, thus fixing their relative positions. Alternatively, the photoresist supply source 5 can be an inkjet printer, using inkjet printing to fill the photoresist. The photoresist used is the existing SU-8 2050 photoresist. Of course, other options include the KMPR 1000 series, THB-151N series, or other negative photoresists that can be cured by UV. Alternatively, a visible light curable resin can be used in conjunction with a corresponding visible light source.
[0030] A photoresist curing apparatus is used to cure liquid photoresist on a transparent conductive substrate 2. The photoresist curing apparatus can be located on the side of the transparent substrate 1 opposite to the transparent conductive substrate 2, or it can be located in other positions, and the curing light is guided to the transparent substrate 1 through a reflector, a light guide, or an optical fiber.
[0031] Electroforming solution supply source 6 is disposed on the side of the transparent conductive substrate 2, and the number of electroforming solution supply sources 6 is generally 1-4. The electroforming solution supply source 6 is used to supply electroforming solution to the electroforming space on the transparent conductive substrate 2. It should be explained that when the cutout template 3 moves upward from the upper surface of the transparent conductive substrate 2, the area below the solid areas of the cutout template 3, excluding the cutout pattern 301, corresponds to the electroforming space. Each of the four sides of the transparent conductive substrate 2 is provided with a surrounding plate 8. The electroforming liquid supply source 6 is a container filled with electroforming liquid. The surrounding plate 8 is provided with through holes corresponding to the outlet of the electroforming liquid supply source 6. The outlet of the electroforming liquid supply source 6 and the corresponding through holes on the surrounding plate 8 together form an electrolyte inlet channel, so that the electroforming liquid in the electroforming liquid supply source 6 can pass through the surrounding plate 8 and enter the electroforming space. In addition, a one-way valve is provided at the outlet of the electroforming liquid supply source 6, so that the electroforming liquid in the electroforming liquid supply source 6 can only flow into the electroforming space and cannot flow backward.
[0032] An electroforming apparatus is used to deposit metal ions in the electroforming solution within the electroforming space, thereby forming electroformed metal 9. In this embodiment, the electroformed metal 9 is pure copper. However, other materials that can be used include nickel, nickel-cobalt alloys, alternating copper-nickel composite coatings, or the co-deposition of graphene microsheets or carbon nanotubes in the copper electroforming solution to form a highly thermally conductive composite coating. Additives in the electroforming solution (such as polyethylene glycol PEG, sodium polydipropane sulfonate SPS, and chlorinated polymers Cl) are also included. - The types and concentrations of (etc.) can be adjusted according to the target grain size and deposition rate.
[0033] The residual medium treatment device includes an electroforming liquid discharge channel. Electroforming liquid within the electroforming space can be discharged through this channel. The discharge channel can be a pipe structure. A through hole connected to the discharge channel is provided on the surrounding plate 8. One end of the discharge channel is connected to the corresponding through hole on the surrounding plate 8, and the other end can be connected to a waste liquid collection container for collecting residual electroforming liquid. A one-way valve is provided on the discharge channel to ensure that only electroforming liquid within the electroforming space flows out through it.
[0034] In actual use, two processes need to be performed alternately: (1) Photoresist patterning process: The hollow template 3 moves along the direction close to the transparent conductive substrate 2 until the bottom surface abuts against the transparent conductive substrate 2 or the top surface of the already formed structure, and supplies liquid photoresist into the hollow pattern 301. The photoresist curing device is started to cure the photoresist and form a masking wall 7 attached to the lower structure of the transparent conductive substrate 2; (2) Electroforming metal 9 filling process: The hollow template 3 moves along the direction away from the substrate until its bottom surface is lower than the top surface of the just cured masking wall 7, so that the upper end of the masking wall 7 is embedded in the lower end of the hollow pattern 301, and a slender annular isolation gap (structural overlap area) is formed between the two. The high flow resistance of this gap constitutes passive fluid isolation, preventing the side electroforming liquid from flowing into the upper photoresist area. At the same time, the movement of the hollow template 3 away from the substrate causes the electroforming space to generate negative pressure, and the electroforming liquid is drawn in through the liquid inlet one-way valve and the metal is deposited by electricity. After the electroformed metal 9 is deposited, the cutout template 3 moves along the direction close to the transparent conductive substrate 2, and the residual electroformed solution is discharged through the liquid outlet check valve. The above cycle is repeated, and the photoresist masking wall 7 and electroformed metal 9 are stacked layer by layer until the target microchannel height is reached. The transparent conductive substrate 2 is fixed in the same clamping position (i.e., on the support base) throughout the process.
[0035] The single reciprocating motion (moving away - approaching) of the cutout template 3 achieves four functions: defining the pattern of the photoresist (through the cutout pattern 301); enclosing a closed electroforming space after embedding the cutout lower end into the upper end of the masking wall 7; achieving passive isolation between the electroforming liquid and the photoresist by utilizing the high flow resistance of the structural overlap area; and achieving the intake and discharge of the electroforming liquid (self-pumping liquid replacement) through the volume change generated by the movement of the cutout template 3 (expanding when moving away and shrinking when approaching) in conjunction with the one-way valve.
[0036] In this embodiment, the electroforming apparatus includes an electroforming power supply (including but not limited to a DC power supply). The positive electrode of the electroforming power supply is electrically connected to the electroforming anode. The electroforming anode is fixed to the perforated template 3. Specifically, the electroforming anode can be directly fixed in the groove on the lower surface of the perforated template 3, or the electroforming anode can be indirectly fixed to the perforated template 3 through a connector (such as a connecting rod or connecting frame), so that the electroforming anode can move closer to or further away from the transparent conductive substrate 2 synchronously with the perforated template 3. The electroforming anode is an insoluble anode, specifically an iridium-plated titanium mesh. The negative electrode of the electroforming power supply is electrically connected to the transparent conductive substrate 2, i.e., the transparent conductive substrate 2 serves as the cathode. When the electroforming power supply is energized, electroformed metal 9 can be deposited on the transparent conductive substrate 2.
[0037] In this embodiment, the residual medium processing device can also discharge uncured liquid photoresist. That is, the residual medium processing device can also include a photoresist discharge channel to discharge the uncured liquid photoresist in the cutout pattern 301. Specifically, the photoresist discharge channel can also directly use the photoresist delivery tube described above. The injection and discharge of liquid photoresist are achieved by the forward and reverse rotation of the micro pump. For example, when it is necessary to inject liquid photoresist into the cutout pattern 301, the micro pump rotates forward, so that the liquid photoresist in the photoresist supply source 5 is delivered into the cutout pattern 301. If there is too much liquid photoresist in the cutout pattern 301 or there is still liquid photoresist involved after curing, the micro pump can be reversed to draw the liquid photoresist in the cutout pattern 301 back to the photoresist supply source 5.
[0038] In addition, the residual media treatment device may also include a cleaning media supply channel, through which cleaning media is supplied to the shielding wall 7 or the electroformed metal 9 for cleaning. The cleaning media can be deionized water, an aqueous cleaning solution compatible with the electroforming solution, or other liquids that will not significantly damage the shielding wall 7 and the electroformed metal 9. After cleaning, dry gas can be introduced into the cleaning media supply channel or negative pressure can be applied to reduce the residue of cleaning media on the surface of the shielding wall 7 and the electroformed metal 9. As for the specific structure of the cleaning media supply channel, it can share the same flow path with the electroforming solution. Only a cleaning media inlet pipe needs to be connected in parallel at the outlet (or corresponding through hole of the enclosure plate 8) of the electroforming solution supply source 6. Each pipe is equipped with an electrically controlled valve to prevent interconnection. The end of the cleaning media inlet pipe away from the enclosure plate 8 is used to connect to the cleaning media source. At the same time, a cleaning medium inlet pipe needs to be connected in parallel at the electroforming liquid discharge channel. Each pipe is equipped with an electric control valve to prevent them from being connected to each other. The end of the cleaning medium inlet pipe away from the enclosure 8 is used to connect to the cleaning medium collection container for separate collection from the electroforming liquid to avoid cross-contamination between the two process media.
[0039] In this embodiment, the photoresist curing device is a UV light source, and the photoresist curing device is disposed below the transparent substrate 1. Specifically, a 365nm UV-LED surface array light source with an irradiance of 20mW / cm² can be disposed below the transparent substrate 1. 2 The light emitted by the UV light source can pass upward through the transparent substrate 1 and the transparent conductive substrate 2 to UV cure the photoresist.
[0040] In this embodiment, a vibration device is also included, which is used to apply vibration to at least one of the cutout template 3, the transparent conductive substrate 2, or the liquid photoresist when the liquid photoresist is supplied to the cutout pattern 301.
[0041] When vibration needs to be applied to the cutout template 3, the vibration device simply needs to be fixed to the cutout template 3. When vibration needs to be applied to the transparent conductive substrate 2, the vibration device simply needs to be fixed to the transparent conductive substrate 2. When vibration needs to be applied to the liquid photoresist, the vibration device can be installed on the photoresist delivery tube or in the photoresist supply source 5. Any device capable of transmitting vibration to the cutout template 3, the transparent conductive substrate 2, or the liquid photoresist within the cutout pattern 301 is acceptable.
[0042] The vibration device uses an existing ultrasonic transducer to apply ultrasonic vibration to the cut-out template 3 during the photoresist supply process. The ultrasonic frequency can be selected between 20kHz and 1MHz, and the power density is 0.1W / cm². 2 Up to 5W / cm 2 This process removes air bubbles from the photoresist, thereby improving the photoresist molding quality. Of course, other vibration devices can also include electro-ceramic transducers, magnetostrictive transducers, and other equipment.
[0043] During operation, in at least one photoresist patterning process, while or after supplying liquid photoresist into the cutout pattern 301 and before UV exposure, ultrasonic vibration is applied to the cutout template 3, the transparent conductive substrate 2, or the liquid photoresist to help remove air bubbles from the cutout pattern 301.
[0044] In this embodiment, the pressure detection device, vibration device, lifting drive device 4, photoresist curing device, and flow control components (i.e., valves on each liquid pipeline) are all electrically connected to the control unit. The control unit can be a common back-end host, PLC controller, etc. The control unit determines the fluid isolation state of the isolation gap based on the pressure detection signal obtained by the pressure detection device, and controls the lifting drive device 4 to adjust the position of the cutout template 3 when the fluid isolation state does not meet the preset conditions. Specifically, when the cutout template 3 moves to the upper end of the photoresist masking wall 7 and enters the cutout pattern 301 to form a structural overlap area, the control unit can obtain the pressure value, pressure change rate, and / or pressure holding status of the electroforming space under the predetermined flow path state and the position of the cutout template 3, and indirectly determine the fluid isolation state of the structural overlap area (i.e., the isolation gap) based on this. When the detection result does not meet the preset conditions, the control unit can control the lifting drive device 4 to adjust the position or movement stroke of the cutout template 3, and re-perform the pressure detection after adjustment; when the preset conditions are still not met after adjustment, the control unit can pause the subsequent liquid supply or electroforming process and output an abnormal prompt.
[0045] In this embodiment, the inner wall of the hollow pattern 301 has a stronger wettability to the liquid photoresist than the upper surface of the hollow template 3. Specifically, a photophilic photoresist layer is provided on the inner wall of the hollow pattern 301 through selective oxygen plasma treatment, and a photophobic photoresist layer is provided on the upper surface of the hollow template 3 through FDTS vapor deposition. The photophilic photoresist layer has a stronger hydrophilicity than the photophobic photoresist layer. The purpose of this arrangement is to ensure that the liquid photoresist preferentially resides in the hollow pattern 301 during supply and does not spontaneously climb to the upper surface of the hollow template 3.
[0046] In other embodiments, differences in wettability can be achieved through the material itself, plasma treatment, surface roughness, or chemical modification.
[0047] In this embodiment, a temperature regulating device is also included to regulate the temperature of the liquid photoresist and / or electroforming solution. Specifically, the temperature regulating device includes a photoresist heating device and / or an electroforming solution heating device. The photoresist heating device is disposed in the photoresist supply source 5 and can preheat the photoresist in the photoresist supply source 5. The electroforming solution heating device is disposed in the electroforming solution supply source 6 and is used to regulate the temperature of the electroforming solution, thereby regulating the electroforming parameters of the electroforming molding apparatus. The photoresist heating device and the electroforming solution heating device can employ existing heating equipment such as electric heating tubes or electric heating rods.
[0048] Example 2 like Figures 2-7As shown, this embodiment provides a layer-by-layer fabrication method for microchannel arrays, based on the microchannel array fabrication apparatus disclosed in Embodiment 1, including the following steps: S1, Photoresist patterning process: such as Figure 2 As shown, the cutout template 3 is moved along the direction close to the transparent conductive substrate 2 until the bottom surface of the cutout template 3 abuts against the top surface of the transparent conductive substrate 2 (this is based on the absence of any structure) or an existing structure (this is based on some special cases with local structures). Liquid photoresist is supplied into the cutout pattern 301. The photoresist curing device is activated to cure the photoresist and form a masking wall 7 attached to the transparent conductive substrate 2 or the existing structure.
[0049] S2, Electroforming Metal 9 Filling Process: (e.g.) Figure 3 As shown, the cutout template 3 is moved away from the transparent conductive substrate 2 until the bottom surface of the cutout template 3 is lower than the top surface of the newly solidified masking wall 7. This causes the upper end of the masking wall 7 to embed into the interior of the cutout pattern 301 near the transparent conductive substrate 2. An isolation gap is formed between the inner wall of the cutout pattern 301 and the outer wall of the masking wall 7. This isolation gap prevents the electroforming liquid in the electroforming space from flowing into the cutout pattern 301. Furthermore, during the movement of the cutout template 3 away from the transparent conductive substrate 2, the electroforming liquid in the electroforming liquid supply source 6 can be drawn into the electroforming space. As shown, the electroforming power supply is turned on to deposit metal (i.e., electroformed metal 9) in the electroforming space. Figure 5 As shown, after the metal is deposited to a preset thickness, the hollow template 3 is moved in a direction close to the transparent conductive substrate 2, and the residual electroforming liquid in the electroforming space is discharged through the electroforming liquid discharge channel.
[0050] S3. Repeat steps S1-S2, as follows: Figures 5-6 As shown, the process involves injecting and curing photoresist, as well as injecting and depositing electroforming solution onto the already formed structure, until the resulting metal structure reaches a predetermined number of layers or a predetermined height.
[0051] S4. Remove the masking walls 7 formed by the stacking of each layer to complete the fabrication of the entire microchannel array. The final microchannel array has a channel wall height of not less than 1 mm and an aspect ratio of not less than 15:1. There are many methods for removing photoresist: chemical stripping, plasma ashing, pyrolysis, or a combination of the above methods can be used. The specific removal method depends on the type of photoresist used.
[0052] In this embodiment, in the structural overlap area, the overlap height of the upper end of the masking wall 7 embedded with the hollow pattern 301 near the substrate is 5 micrometers to 20 micrometers. In a cross-section perpendicular to the extension direction of the masking wall 7, the isolation gap between the outer surface of the masking wall 7 and the inner surface of the hollow pattern 301 is 0.5 micrometers to 5 micrometers.
[0053] In this embodiment, after step S2 (electroplated metal 9 filling process) is completed in each cycle, the top of the electroformed metal 9 formed this time is lower than the top surface of the masking wall 7 formed in step S1 (photoresist patterning process) this time, and the height difference between the two is 2 micrometers to 10 micrometers.
[0054] In this embodiment, different electroforming parameters are used in at least two (including two) steps S2. The electroforming parameters include at least one of current density and electroforming liquid temperature, such that the average grain size of the deposited electroformed metal 9 increases from the side closer to the transparent conductive substrate 2 to the side farther away from the transparent conductive substrate 2 along the height direction of the channel wall, forming a grain gradient along the height direction.
[0055] Of course, all electroforming parameters can also be kept consistent and selected according to actual needs.
[0056] The following specific examples and comparative figures illustrate the advantages of Embodiment 1 and Embodiment 2, as follows: I. Applicable Product Environment and Testing Conditions To ensure comparability of data between specific examples and comparative examples, the following descriptions are based on a uniform benchmark product environment and test conditions.
[0057] Liquid cooling plate reference parameters The liquid cooling plate is made of oxygen-free copper and has dimensions of 120mm × 80mm × 15mm. The bottom surface of the liquid cooling plate is integrally formed using electroforming, featuring a parallel array of elongated microchannels. Each microchannel array consists of multiple parallel elongated microchannels extending along the flow direction of the cooling medium and channel walls (ribs) located between adjacent microchannels. Each microchannel has a cross-sectional width of 150μm ± 5μm and a channel wall width of 150μm ± 5μm (channel center-to-center spacing 300μm). The two ends of each microchannel are connected to the inlet and outlet manifolds of the liquid cooling plate, respectively. The microchannel depth (i.e., channel wall height) H varies from 0.5mm to 5mm depending on the number of circulation layers in the specific example. The cooling medium is deionized water (conductivity not exceeding 1μS / cm), supplied by a constant-temperature circulating water bath with an inlet temperature of 25±0.5℃ and a flow rate of 1.5L / min. It should be noted that the hollow pattern 301 of the hollow template 3 of the present invention defines the planar outline of the photoresist masking wall 7. The hollow pattern 301 is a parallel array of elongated through-slots, and the corresponding elongated masking wall 7 is formed after the photoresist is cured. Electroformed metal 9 fills the gaps between adjacent masking walls 7. After removing the masking walls 7, the above-mentioned parallel array of microchannels is obtained (the space occupied by the masking walls 7 becomes the microchannel, and the space filled by the electroformed metal 9 becomes the channel wall). The size of the hollow pattern 301 determines the final size of the microchannel and the channel wall. In addition to the parallel elongated shape, the hollow pattern 301 can also take other shapes, and the corresponding microchannel structure will change accordingly.
[0058] Reference parameters of the chip to be cooled The thermal test chip (TTC) used is an analog high-performance GPU chip. The chip measures 25mm × 25mm, is 0.8mm thick, has a rated thermal design power (TDP) of 350W, and corresponds to an average heat flux density of approximately 56W / cm³. 2 When the chip is running at full load in a steady state, the average surface temperature of the chip is approximately 98±5℃, and the temperature in the central hot spot area can reach 105±5℃.
[0059] Performance testing methods (1) Channel wall verticality and interlayer alignment accuracy: The planar position of the channel wall centerline is measured every 50 μm along the channel wall height direction. The offset of each layer relative to the reference is calculated with the bottom channel wall centerline as the reference. The standard deviation of the offset of each layer is defined as the interlayer alignment accuracy. At least 5 cross-sectional positions are measured for each sample, and at least 3 channel walls are measured at each position.
[0060] (2) Depth-to-width ratio determination: Measure the total height H of the channel wall and the distance W between adjacent channel walls (i.e., the channel width), depth-to-width ratio = H / W.
[0061] (3) Grain size of electroformed copper layer: an analysis area is taken every 50 μm along the height of the channel wall, and the average grain size is calculated using the equivalent circle diameter method. At least 500 grains are counted at each location.
[0062] (4) Thermal conductivity of the channel wall: Laser flash calorimetry (LFA) was used. Samples were taken in segments along the height of the channel wall (each segment approximately 100 μm thick). The thermal diffusivity α was measured at 25 °C. The density ρ was determined by Archimedes' method and the specific heat capacity Cp was determined by differential scanning calorimetry (DSC). The thermal conductivity λ = α·ρ·Cp was calculated. Each sample was measured independently three times, and the average value was taken.
[0063] (5) Overall heat dissipation performance of the liquid cooling plate: The prepared microchannel liquid cooling plate was installed on the thermal test chip with an assembly pressure of 0.30±0.02MPa. Thermal paste (thermal conductivity not less than 5W / (m·K), coating thickness about 50μm) was applied between the top surface of the chip and the bottom surface of the liquid cooling plate. Under the conditions of cooling water inlet temperature of 25±0.5℃ and flow rate of 1.5L / min, the chip was operated at full power of 350W until thermal steady state (defined as the chip surface temperature change not exceeding 0.2℃ within 30 minutes). The temperature distribution at multiple points (not less than 9 points) on the chip surface was recorded, and the highest temperature T on the chip surface was calculated. max (°C), chip surface temperature difference ΔT (difference between the highest and lowest temperatures, °C), and overall thermal resistance R of the liquid cooling plate. total = (T max -T in ) / P, where T in Where is the cooling water inlet temperature (°C), and P is the chip power (W).
[0064] (6) Inlet and outlet pressure drop test: The microchannel liquid cooling plate was connected to the constant temperature circulating water bath. Under the conditions of inlet water temperature of 25±0.5℃ and flow rate of 1.5L / min, the steady-state pressure drop ΔP was measured by high-precision differential pressure sensors (accuracy ±10Pa) at both ends of the liquid cooling plate. Each sample was measured 3 times and the average value was taken. For the comparison test before and after flushing aging, the initial pressure drop ΔP was measured under the same flow rate and temperature conditions. initial and the voltage drop ΔP after aging aged Calculate the pressure drop increase = (ΔP) aged -ΔP initial ) / ΔP initial ×100%.
[0065] II. Specific Examples Specific Example 1: Layer-by-layer fabrication of a 50-layer copper microchannel array using an integrated device Device Composition The transparent substrate 1 is a quartz glass plate (5 mm thick, with a transmittance of not less than 90% at 365 nm wavelength), which is fixedly mounted on a support base. FTO conductive glass is placed on the transparent substrate 1 as a transparent conductive substrate 2 (sheet resistance 7 Ω / sq, transmittance of not less than 80% at 365 nm wavelength). The transparent conductive substrate 2 remains stationary throughout the entire fabrication process.
[0066] The cutout template 3 is made of a 500μm thick single-crystal silicon wafer through deep reactive ion etching (DRIE). It has an array of elongated through-slots (i.e., cutout pattern 301) running along its thickness direction (orthogonal to the surface of the transparent conductive substrate 2). Each through-slot has a cross-sectional dimension of 150μm (slot width) × 500μm (slot depth, corresponding to the thickness of the cutout template 3), a length of 25mm (corresponding to the chip coverage area), and a center-to-center distance of 300μm between adjacent through-slots. The through-slot array covers an area of approximately 25mm × 25mm, with approximately 40 parallel through-slots. The cutout template 3 is mounted on a lifting drive device 4 and is driven by a rotary motor (i.e., a stepper motor) to reciprocate along a direction orthogonal to the surface of the transparent conductive substrate 2 (i.e., the up-down direction), with a positioning resolution of 0.1μm.
[0067] The surface of the cutout template 3 undergoes a zoned wettability treatment: the upper surface of the cutout template 3 is deposited with perfluorodecyltrichlorosilane (FDTS) at 150℃ for 2 hours to form a photophobic resist layer (with a contact angle of not less than 100° as tested with SU-8); the inner wall of the channel is treated with selective oxygen plasma (power 100W, oxygen flow rate 50sccm, treatment time 90 seconds) to obtain a photophilic resist layer with a target SU-8 contact angle of not more than 35° (this target contact angle can also be obtained through ultraviolet ozone treatment, coating with a hydrophilic undercoat, etc.). The difference in wettability between the hydrophobic upper surface and the hydrophilic inner wall causes the liquid photoresist to preferentially remain in the channel during supply and not spontaneously overflow to the upper surface.
[0068] A photoresist supply source 5 (containing SU-8 2050 negative photoresist, preheated to 60℃ to reduce viscosity) is located above the cutout template 3. Photoresist is supplied to the area at the cutout pattern 301 via a micro-pump and photoresist delivery tube. Electroforming solution supply sources 6 are located on both sides of the cutout template 3 (electroforming solution formula: CuSO4·5H2O 200g / L, H2SO4 50g / L, HCl 50mg / L, polyethylene glycol PEG8000 200mg / L, sodium polydisulfide dipropane sulfonate SPS 5mg / L). An inlet check valve is installed at the outlet of the electroforming solution supply source 6 (allowing only electroforming solution to flow from the supply source 6 into the electroforming space), and an outlet check valve is installed in the discharge channel (allowing only waste liquid to be discharged from the electroforming space). A 365nm UV-LED surface array light source (irradiance 20mW / cm²) is located below the transparent substrate 1. 2The insoluble anode (iridium-plated titanium mesh) is fixed in the groove of the non-perforated area on the bottom surface of the perforated template 3.
[0069] Operating steps Photoresist patterning process (first cycle): The cutout template 3 moves along the direction close to the transparent conductive substrate 2 until its bottom surface abuts against the surface of the FTO transparent conductive substrate 2, and a normal pressure of 0.30±0.02MPa is applied to ensure tight contact. The micropump is turned on to inject liquid SU-8 photoresist into the through-hole array, and the pump is stopped after filling is complete. Backside exposure is performed from below the transparent substrate 1 using a 365nm UV-LED with an exposure dose of 300mJ / cm². 2 The photoresist within the through-slot (i.e., the perforated pattern 301) undergoes a cross-linking reaction and solidifies under UV irradiation. Due to the approximately 5% to 7% volume shrinkage of the photoresist during the cross-linking process, a very small isolation gap (approximately 0.5 μm to 3 μm) naturally forms between the outer surface of the solidified masking wall 7 and the inner surface of the perforated pattern 301. After solidification, elongated masking walls 7 are obtained attached to the surface of the FTO transparent conductive substrate 2. The height of a single layer of masking wall 7 is 50 μm (i.e., the thickness of the photoresist used in this filling). In a plane parallel to the surface of the transparent conductive substrate 2, each masking wall 7 has a cross-sectional width of 150 μm (consistent with the width of the through-slot) and a length of approximately 25 mm, with a total of approximately 40 walls. The spacing between the masking walls 7 is 150 μm.
[0070] Electroforming metal 9 filling process (first cycle): UV light source turned off. The cutout template 3 moves 30μm away from the transparent conductive substrate 2 (the bottom surface of the template moves 30μm upward from the surface of the transparent conductive substrate 2). At this time, the upper end of the masking wall 7 (height 50μm) is embedded inside the lower end of the cutout pattern 301, with an overlap height of 50-30=20μm. After curing, there is a natural isolation gap of about 0.5μm to 3μm between the outer surface of the masking wall 7 and the inner surface of the cutout pattern 301 (generated by the volume shrinkage during the photoresist crosslinking and curing process, not obtained by additional processing). The isolation gap and the 20μm overlap height together form a slender annular flow channel. The characteristic size of this annular flow channel is on the order of micrometers. Liquid entering this channel needs to overcome significant capillary inlet pressure. According to the Young-Laplace equation ΔP=2γcosθ / r (where γ is the surface tension of the liquid, θ is the contact angle, and r is the half-width of the gap), for a gap on the order of 1μm, the capillary inlet pressure is about several hundred kilopascals (water γ≈72mN / m), which is much greater than the driving pressure difference generated by the gravity of the liquid column in the device (the height of the liquid column is about 10mm, corresponding to a pressure difference of about 0.1 kilopascals). Therefore, the electroforming liquid cannot flow from the side through the isolation gap to the photoresist area above the hollow template 3. Similarly, the photoresist above (with higher viscosity and greater surface tension) cannot penetrate downward into the electroforming space. The tiny gap between the outer surface of the shielding wall 7 and the inner surface of the hollow pattern 301 not only ensures that the hollow template 3 can slide freely back and forth, but also constitutes a physical barrier for fluid isolation. The movement of the perforated template 3 away from the transparent conductive substrate 2 expands the volume of the electroforming space, and the resulting negative pressure draws fresh electroforming liquid into the electroforming space through the liquid inlet check valve. Using the FTO conductive surface as the cathode and the iridium-plated titanium mesh as the anode, the electroforming power supply is turned on, and a current density of 2 A / dm³ is applied. 2 Copper layers are deposited under conditions of 25±1℃. The Cu in the electroforming solution within the electroforming space... 2+ The storage capacity supports the deposition of a copper layer approximately 42 μm thick. After alternating between photoresist patterning and electroforming metal 9 filling processes, until the electroforming metal 9 reaches a thickness of 42 μm, the upper surface of the copper layer is approximately 8 μm below the top surface of the masking wall 7. The electroforming power supply is then disconnected, and the cutout template 3 moves at a speed of 2 mm / s along a direction approaching the transparent conductive substrate 2, squeezing out residual electroforming liquid within the electroforming space. This liquid is then discharged through the electroforming liquid discharge channel, pushing open the one-way valve for directional discharge. The cutout template 3 stops moving when its bottom surface is flush with the top surface of the masking wall 7.
[0071] Cycle: Repeat the above two processes a total of 50 times. In each cycle, the height of the masking wall 7 is approximately 50 μm (the height of the masking wall 7 is 50 μm in the first cycle, and is supplemented to 50 μm in subsequent cycles, with an actual solidification thickness of 42 μm), and the copper layer deposition thickness is approximately 42 μm. The height of the cutout template 3 increases by approximately 50 μm each time it approaches the endpoint of the transparent conductive substrate 2. The transparent conductive substrate 2 remains in the same position throughout the entire process without any movement. After 50 cycles, a channel wall formed by multiple layers of copper is obtained, with a total channel wall height of approximately 2.1 mm (50 layers × 42 μm) and a channel width of 150 μm, corresponding to an aspect ratio of approximately 14:1. When the number of cycles increases to 70, the total channel wall height can reach approximately 2.94 mm, and the aspect ratio can reach approximately 19.6:1.
[0072] Test Results Interlayer alignment accuracy: After 50 cycles, the standard deviation of the planar position offset of the center line of each channel wall is no greater than 1μm. The good alignment accuracy comes from the fact that the transparent conductive substrate 2 is fixed throughout the process, without the need for repeated transfer and reclamping.
[0073] Heat dissipation performance: The overall heat dissipation of the liquid cooling plate was tested according to the above performance test method (5). Under full power conditions of 350W, the highest surface temperature T of the 50-layer microchannel liquid cooling plate (total channel wall height 2.1mm, channel width 150μm, depth-to-width ratio approximately 14:1) was 150μm. max =68±1℃, chip surface temperature difference ΔT=7±1℃, overall thermal resistance of liquid cooling plate R total =0.123±0.003K / W.
[0074] Electroforming quality of the channel walls: The average grain size of the 50 copper layers was 2.1 ± 0.4 μm, and the overall thermal conductivity of the channel walls was 390 ± 5 W / (m·K). No microcracks or pores were observed at the interlayer interfaces, indicating good interlayer bonding during layer-by-layer electroforming.
[0075] For reference, a conventional one-step electroforming process was used with a channel width of 150 μm. Due to the high aspect ratio of the microchannel, the electric field density at the orifice is significantly higher than at the bottom during electroforming, resulting in a much higher copper deposition rate at the orifice. This leads to bridging at the orifice before the bottom is filled, creating internal voids. Conventional one-step electroforming cannot achieve defect-free channel walls exceeding approximately 800 μm in height (corresponding to an aspect ratio of approximately 5.3:1). This specific example, through layer-by-layer electroforming, controls the deposition thickness to 42 μm per deposition step (the instantaneous aspect ratio of the electroforming space is approximately 0.28:1 – 30 μm height / 150 μm width), fundamentally avoiding the orifice bridging problem inherent in high aspect ratio electroforming.
[0076] Specific Example 2: Layered Differentiated Electroforming – Grain Gradient The difference from Specific Example 1 is that the 50 electroforming metal filling processes use three different sets of electroforming parameters to form a grain size gradient along the channel wall height direction.
[0077] Electroforming stages 1 to 15 (near the two sides of the FTO transparent conductive substrate, i.e., the bottom layer of the channel wall): current density 1.5 A / dm 2 The electrolyte temperature was 20±0.5℃. The low current density and low temperature resulted in a higher nucleation rate for copper deposition than the grain growth rate, promoting fine-grained nucleation. The resulting copper layer had an average grain size of 0.8±0.2μm, a hardness of 135±5HV (Vickers hardness), and a thermal conductivity of 385±5W / (m·K). The fine grains in the bottom layer helped resist erosion and wear caused by long-term cooling water scouring.
[0078] Electroforming stages 16 to 35 (intermediate layer of the channel wall): Current density 2.5 A / dm 2 The electrolyte temperature was 25±0.5℃. The average grain size of the obtained copper layer was 1.5±0.3μm, the hardness was 118±4HV, and the thermal conductivity was 395±3W / (m·K).
[0079] Electroforming cycles 36 to 50 (top layer of channel wall, two sides away from the FTO transparent conductive substrate): Current density 4A / dm 2 The electrolyte temperature was 30±0.5℃. The high current density and relatively high temperature resulted in a higher grain growth rate than nucleation rate during copper deposition, promoting grain growth. The resulting copper layer had an average grain size of 3.2±0.5μm and a thermal conductivity of 405±2W / (m·K). The larger grains in the top layer, coupled with lower grain boundary density and reduced grain boundary area, facilitated heat conduction. Simultaneously, the larger grain surface area provided a more uniform distribution of vaporization nuclei for the liquid cooler under extreme conditions (when local hotspots reached the nucleation boiling initiation temperature), which helped suppress localized film boiling, thus resulting in higher heat dissipation efficiency.
[0080] The equivalent series thermal conductivity of the channel wall along the z-axis is approximately 395 W / (m·K), which is about 1.3% higher than the uniform electroforming scheme in Specific Example 1 (390 W / (m·K)). Under the same 350W full-power heat dissipation test conditions, the overall thermal resistance R of the liquid cooling plate is... total=0.121±0.003K / W, a slight improvement (approximately -1.6%) compared to 0.123K / W in Specific Example 1. While the improvement in heat dissipation is small, the enhanced erosion resistance resulting from the finer grains at the bottom layer is significant for the long-term stability of the liquid cooler. After accelerated erosion aging tests (deionized water, flow rate 5m / s, containing Al2O3 abrasive particles with a particle size of 1~5μm, concentration 0.1wt%, for 50 hours, equivalent to simulating approximately 5 years of cumulative erosion under normal operating conditions), the inlet and outlet pressure drop ΔP in Specific Example 2 increased from the initial 8.5kPa to 9.1kPa, while in Specific Example 1, ΔP increased from the initial 8.6kPa to 10.6kPa. The finer grains at the bottom layer in Specific Example 2 demonstrate a stronger ability to suppress the surface roughening of the channel walls and the increase in flow resistance caused by erosion. The suppression of the pressure drop increase means that the pump power consumption of the liquid cooler is more stable during long-term service, and the system energy efficiency decays more slowly.
[0081] Specific Example 3: Ultrasonic Assisted Photoresist Filling The difference from Specific Example 1 is that, in each photoresist patterning process, while supplying liquid photoresist into the cutout pattern 301, a piezoelectric ceramic transducer (resonant frequency 40kHz, power density 0.5W / cm²) fixed to the side of the cutout template 3 is used. 2 Apply ultrasonic vibration to the hollow template 3 for 30 seconds, and then perform UV exposure curing after the vibration ends.
[0082] Compared with a specific example without ultrasonic vibration, each batch consisted of 5 substrates. Each substrate had approximately 40 elongated slots (corresponding to 40 microchannels) on its perforated template 3, with each slot approximately 25 mm in length. The surface of each masking wall 7 was examined along its length using an optical microscope at 500x magnification. Group without ultrasound (specific example 1): The average number of bubble defects (defined as circular or elliptical surface depressions with a diameter of not less than 10 μm) detected per substrate was 68 ± 15. Based on 40 masking walls, each approximately 25 mm long, the bubble defect density was approximately 1.7 defects / mm². 2 .
[0083] Ultrasonic test setup (in this specific example): Bubble defect density is approximately 0.275 bubbles / mm². 2 .
[0084] The reduction of bubble defects directly improves the molding integrity and density uniformity of the masking wall 7. Improved width uniformity means higher dimensional consistency of each channel wall, which helps ensure consistent processing quality of the microchannel array and high yield in mass production.
[0085] III. Comparative Example Comparative Example 1: Independent Dual-Bath Layer-by-Layer Transfer – Without Integrated Device This comparative example represents the standard operating procedure without an integrated device. The photoresist patterning and electroforming metal 9 filling are arranged in two separate stations: the photoresist bath station (including the same cutout template 3, SU-8 photoresist bath and back UV light source as in Specific Example 1) and the independent electroforming bath station (including an independent electroforming tank, electroforming anode and electroforming power supply).
[0086] The operation process is as follows: The substrate is initially placed in the photoresist bath station for template contact – photoresist is filled – backside exposure and curing (same parameters as in Example 1) – liquid draining – rinsing three times with deionized water – drying with nitrogen. Then, the operator manually removes the substrate from the photoresist bath station and transfers it to an independent electroforming bath station, re-clamps it, completes electroforming (same parameters as in Example 1) – liquid draining – rinsing – drying – manually transfers it back to the photoresist bath station – re-clamps it, and begins the next cycle. A total of 50 cycles are performed.
[0087] Test Results: After 50 cycles, the cumulative planar position deviation between layers (the standard deviation of the centerline offset of each layer based on the centerline of the bottom channel wall) was ±8-15 μm (compared to no more than 1 μm in Specific Example 1). The main reason for the increased deviation is that the repositioning of the substrate on the fixture after each manual transfer introduces random positional errors, and these errors accumulate and increase with the number of cycles. The total preparation cycle is long, with the extra time mainly used for rinsing, drying, handling, and re-clamping alignment. Among the 5 test substrates, 2 experienced localized cracking (crack length approximately 100 to 300 μm) at the edge region of masking wall 7 during the transfer process, resulting in defects in the corresponding channel walls.
[0088] Comparative Example 2: Full-high photoresist masking wall 7+ layer-by-layer electroforming – without using layer-by-layer photoresist. This comparative example illustrates a case where the photoresist masking wall 7 is formed in a single step, with only electroforming using a layer-by-layer method. First, SU-8 2050 is used for spin coating and back-side UV exposure on the FTO transparent conductive substrate 2 (exposure dose 300 mJ / cm²). 2 A 2.1mm full-height masking wall 7 is fabricated, with a planar outline identical to that in Specific Example 1 (elongated shape, cross-sectional width designed at 150μm, spacing of 150μm). The substrate with the full-height masking wall 7 is then mounted into the same integrated device as in Example 1. The perforated template 3 is used only for layer-by-layer electroforming (photoresist filling and curing are no longer performed). Note: Under high aspect ratio electroforming conditions, if layer-by-layer electroforming is not used, the aperture will be sealed before the bottom of the aperture is filled. This is explained accordingly in Specific Example 1.
[0089] Because the full-height masking wall 7 is fabricated in one step using a separate photolithography process (rather than being formed layer by layer within this device), there is an unavoidable manufacturing deviation between its cross-sectional dimensions and the cutout pattern 301 of the cutout template 3 (the actual cross-sectional width of the masking wall 7 deviates from the design value of 150 μm by approximately ±2 to 5 μm). In the area of the smaller-sized masking wall 7 (actual width approximately 145~148 μm): after the upper end of the masking wall 7 is embedded into the lower end of the cutout pattern 301, the gap between the outer surface of the masking wall 7 and the inner surface of the cutout exceeds the tolerance of the capillary seal (>5 μm, corresponding to a capillary inlet pressure drop below approximately tens of kPa, insufficient to block system pressure differential fluctuations), the overlapping seal fails, and the electroforming liquid flows through the gap from the side to the photoresist area above the template, causing photoresist contamination and deviation of the electroforming liquid composition after contacting the residual photoresist. Abnormal deposition (local protrusions or depressions) occurs in the electroformed copper layer in this area, and the surface quality of the channel wall is significantly reduced. In the area of the larger-sized shielding wall 7 (actual width approximately 152~155μm): the shielding wall 7 cannot be embedded with the hollow pattern 301, the bottom surface of the hollow template 3 is blocked by the top surface of the shielding wall 7 and cannot move to the predetermined sealing position, and the electroforming cycle in this area cannot be performed.
[0090] This comparative example demonstrates that the layer-by-layer photoresist scheme of the present invention allows each masking wall 7 to be formed in situ within the cutout pattern 301. The cross-sectional dimensions of each cured masking wall 7 naturally match the cutout pattern 301, and the gap is uniquely determined by the curing shrinkage of the photoresist itself (approximately 5%~7%), unaffected by dimensional deviations in the external photolithography process. This natural matching is unattainable with full-height, one-step masking walls 7—no matter how optimized the independent photolithography process is, there will always be an unavoidable deviation between the dimensions of the masking wall 7 and the template cutout pattern 301, leading to unreliable sealing reliability and cycle success rate.
[0091] IV. Overall Performance Comparison Specific Example 1 (Integrated Layer-by-Layer Foundation): 50-layer channel wall with a total height of 2.1mm, an aspect ratio of approximately 14:1 (approximately 19.6:1 for 70 layers), interlayer alignment accuracy no greater than 1μm, channel wall thermal conductivity of 390W / (m·K), inlet and outlet pressure drop ΔP = 8.6kPa, and overall thermal resistance R of the liquid cooling plate. total =0.123K / W, chip surface temperature difference ΔT=7℃.
[0092] Specific Example 2 (Grain Gradient): Channel wall equivalent thermal conductivity 395 W / (m·K), R_total=0.121 K / W, ΔT=6℃, ΔP=8.5 kPa; After accelerated erosion aging, the increase in ΔP is only 7.1% (23.3% in Specific Example 1).
[0093] Specific Example 3 (Ultrasonic Assistance): Bubble defect density reduced from approximately 1.7 bubbles / mm 2Reduced to approximately 0.275 particles / mm 2 This is beneficial for consistent processing quality and high batch yield.
[0094] Comparative Example 1 (Independent Two-Bath Transfer): The cumulative alignment deviation between layers is ±8 to 15 μm, the preparation cycle is long, and there is a risk of mask wall 7 transfer failure.
[0095] Comparative Example 2 (Full-height PR + Layer-by-layer electroforming): Dimensional deviations in the shielding wall 7 lead to sealing failure or template jamming, resulting in a low cycle success rate.
[0096] In the description of this invention, it should be understood that the terms "longitudinal," "lateral," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this invention, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention. Furthermore, the terms "first," "second," "third," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance. Thus, a feature defined with "first," "second," etc., may explicitly or implicitly include one or more of that feature. In the description of this invention, unless otherwise stated, "a plurality of" means two or more.
[0097] In the description of this invention, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to fixed connections, detachable connections, or integral connections; they can refer to mechanical connections or electrical connections; they can refer to direct connections or indirect connections through an intermediate medium; and they can refer to the internal communication between two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.
[0098] If this invention discloses or relates to components or structural parts that are fixedly connected to each other, then, unless otherwise stated, a fixed connection can be understood as: a detachable fixed connection (e.g., using bolts or screws) or a non-detachable fixed connection (e.g., riveting, welding). Of course, a fixed connection can also be replaced by an integral structure (e.g., manufactured in one piece using a casting process) (except where it is obviously impossible to use an integral molding process).
[0099] In addition, unless otherwise stated, the terms used in any of the technical solutions disclosed in this invention to indicate positional relationships or shapes include states or shapes that are similar to, close to, or approximate with those states or shapes.
[0100] Any component provided by this invention can be assembled from multiple individual components or can be a single component manufactured by a one-piece molding process.
[0101] It should be noted that the structures, proportions, sizes, etc., depicted in the accompanying drawings of this specification are only used to complement the content disclosed in the specification, so as to enable those skilled in the art to understand and read them, and are not intended to limit the conditions under which the present invention can be implemented. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in the proportions, or adjustments to the size, without affecting the effects and objectives that the present invention can produce, should still fall within the scope of the technical content disclosed in the present invention.
[0102] It should also be noted that in the embodiments of this application, the same reference numerals are used to denote the same component or the same part.
[0103] Any adaptive changes made according to actual needs are within the scope of protection of this invention.
[0104] Specific examples have been used to illustrate the principles and implementation methods of this invention. The descriptions of the above embodiments are only for the purpose of helping to understand the method and core ideas of this invention. Furthermore, those skilled in the art will recognize that, based on the ideas of this invention, there will be changes in the specific implementation methods and application scope. Therefore, the content of this specification should not be construed as a limitation of this invention.
Claims
1. An apparatus for making an array of microchannels, characterized by, include: A transparent substrate (1) is provided, on which a transparent conductive substrate (2) is placed. A hollow template (3) is located above the transparent conductive substrate (2). The hollow template (3) has a hollow pattern (301). The hollow template (3) is connected to a lifting drive device (4). The lifting drive device (4) is used to move the hollow template (3) closer to or away from the transparent conductive substrate (2). A photoresist supply source (5) is provided, which is capable of introducing liquid photoresist into the hollow pattern (301); A photoresist curing apparatus is used to cure liquid photoresist on the transparent conductive substrate (2); Electroforming solution supply source (6), the electroforming solution supply source (6) is used to supply electroforming solution to the electroforming space on the transparent conductive substrate (2); An electroforming apparatus, wherein the electroforming apparatus is used to deposit and form metal ions in the electroforming liquid within the electroforming space; as well as A residual medium treatment device includes an electroforming liquid discharge channel, through which the electroforming liquid in the electroforming space can be discharged.
2. The apparatus for making an array of microchannels of claim 1 wherein: The electroforming device includes an electroforming power source, the positive electrode of which is electrically connected to the electroforming anode, the electroforming anode being fixed on the hollow template (3), the electroforming anode being able to move closer to or further away from the transparent conductive substrate (2) synchronously with the hollow template (3), and the negative electrode of the electroforming power source being electrically connected to the transparent conductive substrate (2).
3. The apparatus for making an array of microchannels of claim 1 wherein: The residual medium processing device can also discharge uncured liquid photoresist.
4. The apparatus for making an array of microchannels of claim 1 wherein: It also includes a vibration device for applying vibration to at least one of the cutout template (3), the transparent conductive substrate (2), or the liquid photoresist when liquid photoresist is supplied to the cutout pattern (301).
5. The apparatus for making an array of microchannels of claim 1 wherein: It also includes a pressure detection device and a control unit, wherein the pressure detection device is used to measure the pressure within the electroforming space; The control unit is connected to the pressure detection device and the lifting drive device (4) respectively. The control unit determines the fluid isolation state of the isolation gap according to the pressure detection signal obtained by the pressure detection device, and controls the lifting drive device (4) to adjust the position of the hollow template (3) when the fluid isolation state does not meet the preset conditions.
6. The fabrication apparatus for a microchannel array according to claim 1, characterized in that: The inner wall of the hollow pattern (301) has a stronger wettability to the liquid photoresist than the upper surface of the hollow template (3).
7. The fabrication apparatus for a microchannel array according to claim 1, characterized in that: It also includes a temperature regulating device for regulating the temperature of the liquid photoresist and / or the electroforming solution.
8. A method for layer-by-layer fabrication of a microchannel array, characterized in that, The fabrication apparatus for the microchannel array according to any one of claims 1-7 includes the following steps: S1, Photoresist patterning process: The cutout template (3) is moved in a direction close to the transparent conductive substrate (2) until the bottom surface of the cutout template (3) abuts against the transparent conductive substrate (2) or the top surface of the formed structure; liquid photoresist is supplied into the cutout pattern (301); the photoresist curing device is started to cure the photoresist to form a masking wall (7) attached to the transparent conductive substrate (2) or the formed structure. S2, Electroforming Metal Filling Process: The hollow template (3) is moved away from the transparent conductive substrate (2) until the bottom surface of the hollow template (3) is lower than the top surface of the newly solidified masking wall (7), so that the upper end of the masking wall (7) is embedded in the hollow pattern (301) on the side close to the transparent conductive substrate (2). An isolation gap is formed between the inner wall of the hollow pattern (301) and the outer wall of the masking wall (7). The isolation gap can prevent the electroforming liquid in the electroforming space from flowing into the hollow pattern (301). During the movement of the hollow template (3) away from the transparent conductive substrate (2), the electroforming liquid in the electroforming liquid supply source (6) can be sucked into the electroforming space. The electroforming power supply is turned on to deposit metal in the electroforming space. After the metal is deposited to a preset thickness, the hollow template is moved towards the transparent conductive substrate (2) to discharge the residual electroforming liquid in the electroforming space through the electroforming liquid discharge channel. S3. Repeat steps S1-S2 until the formed metal structure reaches the predetermined number of layers or the predetermined height. S4. Remove the masking wall (7) formed by the superposition of each layer to complete the fabrication of the entire microchannel array.
9. The layer-by-layer fabrication method of the microchannel array according to claim 8, characterized in that: After each step S2 is completed, the top of the electroformed metal (9) formed in this step is lower than the top surface of the shielding wall (7) formed in this step S1.
10. The layer-by-layer fabrication method of the microchannel array according to claim 8, characterized in that: Different electroforming parameters are used in at least two steps S2, the electroforming parameters including at least one of current density and electroforming solution temperature.