A silicon carbide epitaxial growth apparatus and method
By designing a silicon carbide epitaxial growth device in a horizontal epitaxial furnace, multiple substrates are arranged vertically side by side and equipped with a rotation drive device, solving the problems of reactant concentration decay and particulate contamination during multi-substrate growth. This achieves high-quality uniform epitaxial growth and low particulate contamination, thereby increasing production capacity.
Patent Information
- Application Number
- CN202611573408.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-12
- Publication Date
- 2026-11-17
AI Technical Summary
Existing horizontal epitaxial furnaces struggle to achieve high-quality uniformity and low particulate contamination in multi-substrate growth. Existing improvement schemes suffer from issues such as reactant concentration decay, high equipment modification costs, or differences in airflow patterns.
A silicon carbide epitaxial growth apparatus is designed in a horizontal epitaxial furnace. By arranging multiple silicon carbide substrates vertically side by side with their main surfaces parallel to the horizontal airflow direction and equipping them with a rotary drive device, the reactive gas flows through the surface of each substrate in a parallel manner, eliminating the directional edge effect of the airflow.
It achieves high-quality and uniform epitaxial growth of multiple substrates, improves the consistency of thickness and doping concentration between wafers, reduces the risk of particle contamination, and improves intra-wafer uniformity and productivity.
Smart Images

Figure CN123108741A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of silicon carbide semiconductor material preparation technology, and in particular to a silicon carbide epitaxial growth apparatus and method. Background Technology
[0002] Silicon carbide (SiC) possesses excellent properties such as a wide bandgap, high breakdown electric field, and high thermal conductivity, making it a crucial fundamental material for high-voltage, high-frequency, and high-temperature power devices. Chemical vapor deposition (CVD) is the mainstream method for SiC homoepitaxy. In horizontal epitaxial furnaces, reactive gases flow parallel across the substrate surface, offering advantages such as good surface morphology, low particle contamination, and high yield. However, traditional horizontal furnaces are mostly used for single-wafer growth, resulting in low single-furnace capacity, which is insufficient to meet the demands of large-scale mass production.
[0003] To improve production capacity, various multi-wafer solutions have been explored in existing technologies. One approach involves setting up a vertical rotating rod in a horizontal furnace, with multiple graphite trays connected horizontally on it, and the substrate placed horizontally on the trays. While this solution achieves multi-wafer loading, the reactant concentration decreases with each substrate as the airflow passes through, resulting in significant differences in thickness and doping concentration between wafers, making it difficult to guarantee uniformity. Another approach uses a vertical or barrel furnace, placing the substrate vertically on the surface of a carrier tray or graphite barrel, and achieving multi-wafer growth through vertical airflow or radial jetting. Some of these solutions utilize close-range radial jetting from nozzles, while others use a motor-driven rotating shaft to rotate the carrier tray. Although this approach can reduce wafer warpage and particle fallout, its airflow pattern, gas path interface, and thermal field structure differ significantly from those of a horizontal furnace, making it difficult to directly adapt and resulting in high equipment modification costs. In addition, some solutions optimize the tray structure or airflow distribution in a horizontal furnace, but it is still difficult to simultaneously achieve inter-wafer uniformity, intra-wafer uniformity, and low particle contamination during multi-wafer growth.
[0004] Therefore, how to achieve high-quality and uniform epitaxial growth of multiple substrates in a horizontal epitaxial furnace has become a problem that urgently needs to be solved by those skilled in the art. Summary of the Invention
[0005] This application proposes a silicon carbide epitaxial growth apparatus and method, which realizes high-quality and uniform epitaxial growth of multiple substrates in a horizontal epitaxial furnace.
[0006] To achieve the above objectives, this application discloses the following technical solutions: In a first aspect, this application provides a silicon carbide epitaxial growth apparatus, comprising: a reaction chamber arranged in a horizontal direction; a wafer carrier mechanism disposed in the reaction chamber for fixing multiple silicon carbide substrates such that the main surface of each silicon carbide substrate is vertical and arranged side by side in a direction perpendicular to the horizontal airflow direction in the horizontal plane, with the main surface of each silicon carbide substrate parallel to the horizontal airflow direction; and a rotation drive device connected to the wafer carrier mechanism for driving the wafer carrier mechanism to rotate around the axis of the wafer carrier mechanism.
[0007] In some embodiments, the wafer carrier mechanism includes a first chassis, a second chassis, multiple trays, multiple pressure columns, and clamping columns; The first chassis and each tray are provided with multiple mounting holes along the circumference; each pressure post includes a pin section and a boss section located at one end thereto. The pin section passes through the mounting holes of the first chassis and the tray and is pinned to fit. The first chassis and the tray cooperate with the boss section to form a clamping space for clamping the silicon carbide substrate. The second chassis abuts against the outermost boss section; The hoop is attached to the outside of the first and second chassis.
[0008] In some embodiments, the reaction chamber is further provided with a growth chamber, which includes a left crescent, a right crescent, an upper baffle and a lower baffle, and the left crescent, the right crescent, the upper baffle and the lower baffle enclose a cuboid space. The wafer carrier mechanism is located within a cuboid space.
[0009] In some embodiments, the left and right halves of the moon are respectively provided with mounting grooves, and the first and second bases are respectively provided with rotating shafts. The rotating shafts cooperate with the mounting grooves to make the wafer carrier mechanism rotate around the rotating shafts.
[0010] In some embodiments, the reaction chamber is a horizontal cylindrical chamber, and the inner wall of the reaction chamber is made of graphite. The silicon carbide epitaxial growth apparatus also includes an induction heating system, which comprises multiple induction heating coils arranged around the reaction chamber.
[0011] In some embodiments, multiple induction heating coils are configured to be grouped and controlled along the axial direction of the reaction chamber.
[0012] In some embodiments, the wafer carrier mechanism includes 2-10 trays, each tray carrying a silicon carbide substrate.
[0013] Because the wafer carrier mechanism vertically positions multiple silicon carbide substrates side-by-side in a direction perpendicular to the horizontal airflow direction within a horizontal plane, and the main surface of each substrate is parallel to the horizontal airflow direction, the reactant gas can flow across the surfaces of each substrate simultaneously in a substantially parallel manner when flowing horizontally. The substrates do not obstruct each other, avoiding the problem of reactant concentration decreasing along the wafer path in horizontal series connection schemes, thus improving the consistency of inter-wafer thickness and doping concentration. Simultaneously, the rotary drive device drives the wafer carrier mechanism to rotate around its axis, making the distribution of reactant gas on the vertical substrate surface axially symmetrical, eliminating the edge effect caused by airflow directionality, and improving intra-wafer uniformity. Therefore, high-quality, uniform epitaxial growth of multiple substrates is achieved in a horizontal epitaxial furnace. Furthermore, the vertical placement of the substrates ensures that the direction of gravity is parallel to the main surface, which helps reduce warpage and lowers the risk of particles falling onto the growth surface.
[0014] Secondly, this application provides a method for silicon carbide epitaxial growth, comprising the following steps: S1: Fix multiple silicon carbide substrates vertically side by side on the wafer support mechanism, so that the main surface of each silicon carbide substrate is parallel to the horizontal airflow direction, and place the wafer support mechanism into the reaction chamber. S2: After evacuating the reaction chamber, introducing carrier gas and heating it to the epitaxial temperature, introduce the reaction gas source and doping gas source, start the rotation drive device to rotate the wafer support mechanism, and carry out epitaxial growth. S3: After growth is complete, stop ventilation, cool down in a protective atmosphere, and remove the epitaxial wafer.
[0015] In some embodiments, the epitaxial temperature in step S2 is 1500-1700℃, the pressure in the reaction chamber is 50-200mbar, the carrier gas is high-purity H2, the reaction gas source includes silicon source trichlorosilane and carbon source ethylene, and the doping gas source is nitrogen or ammonia.
[0016] In some embodiments, the rotational speed of the rotary drive device in step S2 is 30-100 rpm; the wafer carrier mechanism carries 2-10 silicon carbide substrates, and the reaction gas source flows parallel to the surface of each silicon carbide substrate at the same time.
[0017] Since step S1 fixes multiple silicon carbide substrates vertically side-by-side, with the main surface of each substrate parallel to the horizontal airflow direction, the reactant gas flowing horizontally in step S2 can simultaneously flow over the surfaces of each substrate in a substantially parallel manner, without obstructing each other. This avoids the problem of reactant concentration decreasing along the process of each substrate in the horizontal series connection scheme, which is beneficial to improving the consistency of thickness and doping concentration between wafers. At the same time, the rotation drive device activated in step S2 rotates the wafer support mechanism, making the distribution of reactant gas on the vertical substrate surface axially symmetrical, eliminating the edge effect caused by airflow directionality, which is beneficial to improving intra-wafer uniformity. Thus, this method achieves high-quality and uniform epitaxial growth of multiple substrates in a horizontal epitaxial furnace. Attached Figure Description
[0018] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are merely some examples or embodiments of this application. For those skilled in the art, other drawings can be obtained based on the provided drawings without creative effort, and this application can be applied to other similar scenarios based on the provided drawings, all of which fall within the scope of protection of this application. Unless obvious from the linguistic context or otherwise specified, the same reference numerals in the drawings represent the same structure or operation.
[0019] Figure 1 A schematic diagram of a silicon carbide epitaxial growth apparatus provided in an embodiment of this application; Figure 2 A front view of the growth chamber provided in an embodiment of this application; Figure 3 A front view of the wafer carrier mechanism provided in an embodiment of this application; Figure 4 A disassembly diagram showing the fit between the first chassis and the pressure column, provided for an embodiment of this application; Figure 5 This is a side view of the tray and pressure post mating as provided in an embodiment of this application; The annotations in the attached figures are explained as follows: 10. Silicon carbide epitaxial growth apparatus; 100 Reaction chamber; 110 Growth chamber; 111 Left crescent; 1111 Mounting slot; 112 Right crescent; 113 Upper baffle; 114 Lower baffle; 200 Wafer support mechanism; 210 First chassis; 211 Mounting hole; 212 Rotating shaft; 220 Second chassis; 230 Pallet; 240 Pressure column; 241 Pin section; 242 Boss section; 250 Hoop column; 300 silicon carbide substrate; 400 Induction heating system; 410 Induction heating coil. Detailed Implementation
[0020] The present application will now be described in further detail with reference to the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are merely illustrative of the application and not intended to limit it. The described embodiments are only a part of the embodiments of the present application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of the present application without inventive effort are within the scope of protection of the present application.
[0021] Among related technologies, horizontal epitaxial furnaces offer advantages such as better epitaxial wafer surface morphology, lower particulate contamination, and higher yield due to the parallel flow of reactant gases across the substrate surface. However, they are mostly used for single-wafer growth, resulting in low single-furnace capacity. Existing multi-wafer loading solutions, such as the horizontal series tray 230 scheme, suffer from reactant concentration decay along the process and poor inter-wafer uniformity. Vertical multi-wafer schemes using vertical or barrel furnaces are difficult to directly adapt due to significant differences in airflow patterns, gas path interfaces, and thermal field structures compared to horizontal furnaces.
[0022] The inventors discovered that if multiple substrates are placed vertically in a horizontal epitaxial furnace, with the main surface of each substrate parallel to the horizontal airflow direction, the reactant gas can flow simultaneously across the surfaces of each substrate in a substantially parallel manner. This avoids the concentration of reactants decreasing along the process, while also taking advantage of the low particle contamination and high yield of the horizontal furnace. Based on this, this application provides a silicon carbide epitaxial growth apparatus 10 and method. The overall concept is as follows: a wafer carrier mechanism 200 is provided in a reaction chamber 100 arranged in a horizontal direction, and multiple silicon carbide substrates 300 are placed vertically, with the main surface of each substrate in a vertical state, arranged side by side in a direction perpendicular to the horizontal airflow direction, and the main surface of each substrate parallel to the horizontal airflow direction; at the same time, a rotation drive device is provided to drive the wafer carrier mechanism 200 to rotate around its axis, so that the reactant gas is uniformly distributed on the vertical substrate surface. The basic embodiment of this application will be described below with reference to the accompanying drawings.
[0023] See Figure 1 and Figure 2 This application provides a silicon carbide epitaxial growth apparatus 10, including a reaction chamber 100, a wafer support mechanism 200, and a rotation drive device.
[0024] The reaction chamber 100 is arranged horizontally, providing a closed reaction space for epitaxial growth. A gas inlet is located at one end of the reaction chamber 100, and a gas outlet is located at the other end. The reaction gas enters through the gas inlet and flows horizontally to the gas outlet. In a preferred embodiment, the gas inlet can be connected to a square quartz tube and a graphite transition piece to ensure compatibility with existing horizontal furnace gas interfaces. The gas outlet can be connected to a tail gas treatment system to discharge the reacted gas. The internal pressure of the reaction chamber 100 can be regulated by a vacuum pump and a pressure control valve to maintain the low-pressure environment required for epitaxial growth.
[0025] A wafer support mechanism 200 is disposed within the reaction chamber 100 for fixing multiple silicon carbide substrates 300. The wafer support mechanism 200 vertically positions each silicon carbide substrate 300, meaning the main surface of each substrate 300 is vertical, and the substrates are arranged side-by-side in a direction perpendicular to the horizontal airflow direction, with their main surfaces parallel to the horizontal airflow direction. Thus, when the reactant gas flows horizontally, it can flow across the surfaces of each silicon carbide substrate 300 simultaneously in a substantially parallel manner, without obstructing each other, and the airflow state and reactant concentration on each substrate surface are substantially consistent. In a preferred embodiment, the silicon carbide substrate 300 can be a 4H-SiC substrate with a diameter of 6 inches. The wafer support mechanism 200 can support 2-10 silicon carbide substrates 300, and the spacing between the substrates can be optimized according to the airflow state and thermal field distribution.
[0026] A rotary drive device is connected to the wafer carrier mechanism 200 and is used to drive the wafer carrier mechanism 200 to rotate about its axis. When the wafer carrier mechanism 200 rotates, the distribution of the reactive gas on the vertical substrate surface is axisymmetric, thereby eliminating the edge effect caused by airflow asymmetry. In a preferred embodiment, the rotary drive device can be an air-floating rotary mechanism, which drives the wafer carrier mechanism 200 to rotate via gas. The air-floating rotary mechanism enables the wafer carrier mechanism 200 to remain stable during rotation, avoiding vibration and particulate contamination caused by mechanical contact.
[0027] Because the wafer carrier mechanism 200 arranges multiple silicon carbide substrates 300 vertically and side by side in a direction perpendicular to the horizontal airflow direction in the horizontal plane, and the main surface of each substrate is parallel to the horizontal airflow direction, the reactant gas can flow through the surface of each substrate simultaneously in a basically parallel manner when it flows in the horizontal direction, and the substrates do not block each other, thus avoiding the problem of reactant concentration decaying along the way in the horizontal series connection scheme, thereby improving the consistency of inter-wafer thickness and doping concentration.
[0028] Simultaneously, the rotary drive mechanism drives the wafer carrier 200 to rotate around its axis, making the distribution of reactive gas on the vertical substrate surface axially symmetrical. This eliminates the edge effect caused by the directionality of gas flow and improves intra-wafer uniformity. Thus, high-quality, uniform epitaxial growth of multiple substrates is achieved in a horizontal epitaxial furnace. Furthermore, the vertical placement of the substrate ensures that the direction of gravity is parallel to the main surface, which helps reduce warpage and lowers the risk of particles falling onto the growth surface.
[0029] See also Figure 1 and Figure 2 The chip carrier mechanism 200 includes a first chassis 210, a second chassis 220, multiple trays 230, pressure columns 240, and clamp columns 250.
[0030] The first base 210 and the second base 220 are located at opposite ends of the wafer carrier mechanism 200 along a parallel direction. The first base 210 has multiple mounting holes 211, and each tray 230 has multiple mounting holes 211 circumferentially. The pressure post 240 includes a pin section 241 and a boss section 242 at one end. The pin section 241 passes through the mounting holes 211 of the first base 210 and the mounting holes 211 of the tray 230, and engages with the mounting holes 211. The pin engagement can be achieved by providing a radial through hole in the pin section 241 and inserting a pin outside the mounting hole 211. The boss section 242 is located on the side of the tray 230 facing the second base 220. Both the first base 210 and the tray 230 engage with the boss section 242 to form a clamping space for holding the silicon carbide substrate 300.
[0031] Specifically, the first base plate 210 is located on the far left. The pin section 241 of the pressure post 240 passes through the mounting hole 211 of the first base plate 210, and the boss section 242 of the pressure post 240 cooperates with the first base plate 210 to clamp the leftmost silicon carbide substrate 300. The silicon carbide substrate 300 located in the middle is clamped between the boss section 242 and the corresponding tray 230. The boss section 242 can be disc-shaped, with a diameter larger than that of the pin section 241, to increase the contact area with the substrate and avoid local stress concentration. In a preferred embodiment, both the first base plate 210 and the second base plate 220 can be made of graphite, and the tray 230 can also be made of graphite. The pressure post 240 and the clamp post 250 can also be made of graphite to withstand the high-temperature environment required for epitaxial growth. The thickness of the first chassis 210, the second chassis 220, and the pallet 230 can be selected according to the requirements of mechanical strength and heat capacity. For example, the thickness of the first chassis 210 and the second chassis 220 can be greater than the thickness of the pallet 230.
[0032] The second chassis 220 abuts against the outer side of the outermost boss section 242. The clamping post 250 is engaged with the outer side of the first chassis 210 and the second chassis 220, fixing the first chassis 210, the second chassis 220, the multiple trays 230, the pressure post 240, and the silicon carbide substrate 300 into a single unit. The clamping post 250 can be made of graphite, and its cross-section can be rectangular or circular. It is connected to the first chassis 210 and the second chassis 220 via slots or bolts.
[0033] In a preferred embodiment, each tray 230 has four mounting holes 211 along its circumference, corresponding to four pressure posts 240. The four pressure posts 240 press a silicon carbide substrate 300 onto the tray 230 from four directions, thereby making the substrate more stable. Multiple trays 230 are arranged side by side in a horizontal direction, each tray 230 carrying a silicon carbide substrate 300, thus forming multiple vertically arranged wafer carrier positions. The four pressure posts 240 can be evenly distributed along the circumference of the tray 230, for example, at 90° intervals. A clamping space is formed between the boss section 242 of each pressure post 240 and the tray 230, and the silicon carbide substrate 300 is clamped in the clamping space. Since the four pressure posts 240 apply clamping force simultaneously from four directions, the stress on the silicon carbide substrate 300 is more uniform, which helps to avoid substrate cracking or deformation caused by local stress concentration.
[0034] In some embodiments, the reaction chamber 100 also includes a growth chamber 110. See also Figure 1 The growth chamber 110 includes a left crescent 111, a right crescent 112, an upper baffle 113, and a lower baffle 114. The left crescent 111, right crescent 112, upper baffle 113, and lower baffle 114 enclose a cuboid space. The wafer carrier mechanism 200 is disposed within this cuboid space.
[0035] The left crescent 111 and right crescent 112 are located on opposite sides of the cuboid space along the parallel direction, and their shapes are roughly semi-circular or crescent-shaped, fitting the cylindrical inner wall of the reaction chamber 100. The left crescent 111 and right crescent 112 can be made of graphite and are fixed to the inner wall of the reaction chamber 100 by bolts or slots. The upper baffle 113 and lower baffle 114 are located above and below the cuboid space, respectively, and can also be graphite plates, forming a rectangular growth channel with the left and right crescents 112. The shapes of the left crescent 111 and right crescent 112 can match the shape of the inner wall of the reaction chamber 100 to ensure a tight fit between the growth chamber 110 and the reaction chamber 100. The upper baffle 113 and lower baffle 114 can be connected to the left crescent 111 and right crescent 112 by bolts or slots, thereby forming a closed or semi-closed cuboid space.
[0036] The cuboid space formed by the left crescent 111, right crescent 112, upper baffle 113, and lower baffle 114 serves as the main growth space, regulating the airflow field and ensuring a stable laminar flow of the reactive gas as it passes through the wafer support mechanism 200. Simultaneously, the enclosed structure prevents particles from other areas of the reaction chamber 100 from entering the growth space, further reducing the risk of particulate contamination. Furthermore, the left crescent 111 and right crescent 112 also support wafer placement; that is, both ends of the wafer support mechanism 200 can be supported by the left crescent 111 and right crescent 112, respectively. In a preferred embodiment, support steps or grooves can be provided on the left crescent 111 and right crescent 112 to accommodate the first chassis 210 and the second chassis 220. The rotating shaft 212 can be inserted into the mounting grooves 1111 on the left crescent 111 and right crescent 112, thereby achieving radial support and axial positioning.
[0037] Furthermore, the left crescent 111 and the right crescent 112 are each provided with a mounting groove 1111. The first base 210 and the second base 220 are each provided with a rotating shaft 212. The rotating shaft 212 cooperates with the mounting groove 1111, allowing the wafer carrier mechanism 200 to rotate around the rotating shaft 212. In this embodiment, the rotating shaft 212 is inserted into the mounting groove 1111, which provides radial support and axial positioning for the rotating shaft 212, while allowing the rotating shaft 212 to rotate within the mounting groove 1111. The mounting groove 1111 can be a semi-circular groove, and the end of the rotating shaft 212 can be cylindrical or hemispherical. A graphite bearing or a ceramic bearing can be provided between them to reduce friction. When the rotating drive device drives the wafer carrier mechanism 200 to rotate, the rotating shaft 212 rotates within the mounting groove 1111, thereby driving the entire wafer carrier mechanism 200 to rotate around its axis. The rotating shaft 212 can be integrally formed with the first chassis 210 and the second chassis 220, or it can be fixed to the first chassis 210 and the second chassis 220 by means of threaded connection or pin connection.
[0038] Optionally, the reaction chamber 100 is a horizontal cylindrical cavity with an inner wall made of graphite. The graphite inner wall can be formed by chemical vapor deposition or by embedding a graphite tube inside a cylindrical quartz tube. The silicon carbide epitaxial growth apparatus 10 also includes an induction heating system 400. The induction heating system 400 includes multiple induction heating coils 410 arranged around the reaction chamber 100. The multiple induction heating coils 410 are spaced apart along the axial direction of the reaction chamber 100. The induction heating coils 410 can be copper tubes, through which alternating current and cooling water are passed to generate eddy currents in the graphite inner wall and heat it. The number of turns and spacing of the induction heating coils 410 can be selected according to the cavity size and heating requirements.
[0039] When an alternating current is applied to the induction heating coil 410, an alternating magnetic field is generated, which induces eddy currents on the graphite inner wall of the reaction chamber 100 and generates heat, thereby heating the interior of the reaction chamber 100 to the temperature required for epitaxy. The frequency of the induction heating coil 410 can be 10-100kHz, and the power can be selected according to the size of the chamber and the heating requirements.
[0040] Based on the induction heating system 400, multiple induction heating coils 410 are configured to be controlled in groups along the axial direction of the reaction chamber 100. Through group control, the power of the induction heating coils 410 at different axial positions can be independently adjusted, thereby regulating the axial temperature distribution within the reaction chamber 100. Since the multiple substrates of the wafer carrier mechanism 200 are arranged side-by-side along a direction perpendicular to the airflow direction, and each substrate is located at the same or similar positions axially, the regulation of the axial temperature distribution can make the thermal field of each substrate more uniform, which is beneficial for improving the thickness uniformity between and within wafers.
[0041] For example, the coils can be divided into three groups, corresponding to the inlet, middle, and outlet of the cavity, respectively, and the axial temperature difference can be compensated by independently adjusting the power of each group. In other embodiments, the coils can also be divided into two, four, or more groups, and the number of groups can be selected according to the cavity length and temperature uniformity requirements. Through group control, the required temperature gradient can also be formed within the cavity to adapt to the needs of different epitaxial processes.
[0042] As an alternative, the wafer carrier mechanism 200 includes 2-10 trays 230, each tray 230 carrying a silicon carbide substrate 300. The number of trays 230 can be adjusted according to production capacity requirements and cavity size. When production capacity needs to be increased, the number of trays 230 can be increased; when uniformity needs to be maintained, the number of trays 230 can be appropriately reduced.
[0043] In a preferred embodiment, there are four trays 230, each supporting four 6-inch silicon carbide substrates 300. In other embodiments, there may be six or eight trays 230, supporting six or eight substrates respectively. As the number of trays 230 increases, the axial length of the wafer carrier mechanism 200 increases accordingly. Thermal uniformity can be maintained by adjusting the grouping control of the induction heating coils 410. For example, when the number of trays 230 increases to six or eight, the number of groups of the induction heating coils 410 can be increased accordingly to compensate for temperature non-uniformity caused by the increased axial length.
[0044] The second aspect of this application also describes a silicon carbide epitaxial growth method, using any of the aforementioned silicon carbide epitaxial growth apparatus 10, comprising the following steps.
[0045] S1: Fix multiple silicon carbide substrates 300 vertically side by side on the wafer carrier mechanism 200, so that the main surface of each silicon carbide substrate 300 is parallel to the horizontal airflow direction, and place the wafer carrier mechanism 200 into the reaction chamber 100.
[0046] Specifically, each silicon carbide substrate 300 is placed on its corresponding tray 230 and first base 210, with the main surface of the silicon carbide substrate 300 in a vertical position. The pin segments 241 of the pressure pillars 240 are respectively inserted into the mounting holes 211 of the first base 210 and the tray 230, and the boss segments 242 of the pressure pillars 240 cooperate with the tray 230 or the first base 210 to clamp the silicon carbide substrate 300. Each tray 230 is fixed by four circumferentially distributed pressure pillars 240, stably clamping the silicon carbide substrate 300 between the boss segments 242 and the tray 230; the same applies to the first base 210. Then, the second base 220 is abutted against the outer side of the outermost boss segment 242 and secured to the outer side of the first base 210 and the second base 220 by clamping posts 250, thus fixing the entire wafer carrier mechanism 200 into a single unit. The wafer carrier mechanism 200 with the substrate fixed is placed into the reaction chamber 100, so that the wafer carrier mechanism 200 is located in the cuboid space formed by the left half-moon 111, the right half-moon 112, the upper baffle 113 and the lower baffle 114.
[0047] S2: After evacuating the reaction chamber 100, introducing carrier gas, and heating it to the epitaxial temperature, a reaction gas source and a dopant gas source are introduced. The rotation drive device is then activated to rotate the wafer support mechanism 200 for epitaxial growth. Evacuating the chamber removes air and moisture from the reaction chamber 100, preventing adverse effects on epitaxial growth. Introducing carrier gas establishes a protective atmosphere within the reaction chamber 100 and carries the reaction gas source and dopant gas source into the growth region. After heating to the epitaxial temperature, the reaction gas source and dopant gas source undergo a chemical vapor deposition reaction on the substrate surface, generating a silicon carbide epitaxial layer.
[0048] S3: After growth is complete, stop ventilation, cool down in a protective atmosphere, and remove the epitaxial wafer.
[0049] Since step S1 fixes multiple silicon carbide substrates 300 vertically side-by-side, with the main surface of each substrate parallel to the horizontal airflow direction, the reactant gas flowing horizontally in step S2 can simultaneously flow over the surfaces of each substrate in a substantially parallel manner, without obstructing each other. This avoids the problem of reactant concentration decreasing along the process of each substrate in the horizontal series connection scheme, which is beneficial to improving the consistency of thickness and doping concentration between wafers. At the same time, the rotation drive device activated in step S2 rotates the wafer support mechanism 200, making the distribution of reactant gas on the vertical substrate surface axially symmetrical, eliminating the edge effect caused by airflow directionality, which is beneficial to improving intra-wafer uniformity. Thus, this method achieves high-quality uniform epitaxial growth of multiple substrates in a horizontal epitaxial furnace.
[0050] To further improve the crystal quality and surface morphology of the epitaxial layer, this application embodiment further defines the process parameters and gas types in step S2. Specifically, in step S2, the epitaxial temperature is 1500-1700℃, the pressure in the reaction chamber 100 is 50-200 mbar, the carrier gas is high-purity H2, the reaction gas source includes silicon source trichlorosilane and carbon source ethylene, and the doping gas source is nitrogen or ammonia.
[0051] The epitaxial temperature is set to 1500-1700℃, ensuring sufficient decomposition and reactivity of the silicon and carbon sources on the substrate surface. This avoids insufficient growth rate or decreased crystal quality due to excessively low temperatures, as well as intensified gas-phase nucleation and increased surface roughness due to excessively high temperatures. The pressure in the reaction chamber 100 is set to 50-200 mbar, falling within the low-pressure epitaxial growth range. This helps suppress homogeneous reactions in the gas phase, reduces reactant consumption before reaching the substrate, and improves the thickness uniformity and surface morphology of the epitaxial layer. High-purity H2 is used as the carrier gas, effectively carrying the reaction gas source and dopant gas source into the reaction chamber 100 and providing a protective atmosphere during heating, growth, and cooling. Trichlorosilane is used as the silicon source, and ethylene as the carbon source; both have moderate reactivity, facilitating controllable chemical vapor deposition on the substrate surface. Nitrogen or ammonia is used as the dopant gas source, introducing n-type doping during growth to meet the doping concentration requirements of power devices for the drift layer.
[0052] In one specific embodiment, the epitaxial temperature can be 1600℃, the pressure of the reaction chamber 100 can be 100mbar, the carrier gas flow rate can be 100sccm, the trichlorosilane flow rate can be 50sccm, the ethylene flow rate can be 30sccm, and the doping gas source flow rate can be adjusted according to the target doping concentration.
[0053] Based on the above process parameters, the embodiments of this application can further limit the rotation speed of the rotary drive device and the number of wafers carried by the wafer carrier mechanism 200, so as to balance the uniformity within the wafer and the single-furnace capacity. Specifically, in step S2, the rotation speed of the rotary drive device is 30-100 rpm; the wafer carrier mechanism 200 carries 2-10 silicon carbide substrates 300, and the reaction gas source flows parallel to the surface of each silicon carbide substrate 300 at the same time.
[0054] A rotation speed of 30-100 rpm enables the wafer carrier mechanism 200 to drive multiple silicon carbide substrates 300 to rotate stably, resulting in an axisymmetric distribution of the reactive gas on the vertical substrate surface. This reduces the impact of airflow directionality on the wafer thickness and doping uniformity. If the rotation speed is too low, the axisymmetry of the airflow on the substrate surface will be insufficient; if the rotation speed is too high, it may cause airflow turbulence or additional disturbance to the substrate fixing structure. The wafer carrier mechanism 200 carries 2-10 silicon carbide substrates 300, which can effectively increase the single-furnace capacity and reduce the single-wafer production cost while ensuring inter-wafer and intra-wafer uniformity.
[0055] Since the silicon carbide substrates 300 are arranged vertically side by side and their main surfaces are parallel to the horizontal airflow direction, the airflows formed by the reaction gas source and the doping gas source can flow parallel to each substrate surface simultaneously, making the airflow state and reactant concentration on each substrate surface basically consistent. In one specific embodiment, the rotation speed of the rotary drive device can be 80 rpm, and the wafer carrier mechanism 200 can carry four 6-inch silicon carbide substrates 300. After 60 minutes of growth, the epitaxial layer thickness obtained is approximately 12 μm, with an inter-wafer thickness difference of less than 2% and an inter-wafer doping concentration difference of less than 3%. In other embodiments, when the number of wafers carried is increased to 6 or 8, the uniformity between and within wafers can be maintained by appropriately increasing the rotation speed or adjusting the grouping control of the induction heating coils 410.
[0056] In the above context, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature.
[0057] In the description of the embodiments of this application, unless otherwise stated, " / " means "or". For example, A / B can mean A or B. "And / or" in this article is merely a description of the relationship between related objects, indicating that there can be three relationships. For example, A and / or B can mean: A exists alone, A and B exist simultaneously, and B exists alone.
[0058] It should be noted that, for ease of description, only the parts relevant to the application are shown in the accompanying drawings. Unless otherwise specified, the embodiments and features described in this application can be combined with each other.
[0059] The above description is merely a preferred embodiment of this application and an explanation of the technical principles employed, and is not intended to limit this application. Various modifications and variations can be made to this application by those skilled in the art. The scope of this application is not limited to technical solutions formed by specific combinations of the above-described technical features, but should also cover other technical solutions formed by arbitrary combinations of the above-described technical features or their equivalents without departing from the above-described application concept. For example, technical solutions formed by substituting the above features with (but not limited to) technical features with similar functions disclosed in this application.
Claims
1. A silicon carbide epitaxial growth apparatus, characterized in that, include: A reaction chamber (100) is arranged in a horizontal direction; A wafer carrier mechanism (200) is disposed in the reaction chamber (100) for fixing multiple silicon carbide substrates (300), such that the main surface of each silicon carbide substrate (300) is vertically arranged and arranged side by side in a direction perpendicular to the horizontal airflow direction in the horizontal plane, and the main surface of each silicon carbide substrate (300) is parallel to the horizontal airflow direction. A rotation drive device, connected to the wafer carrier mechanism (200), is used to drive the wafer carrier mechanism (200) to rotate around the axis of the wafer carrier mechanism (200).
2. The silicon carbide epitaxial growth apparatus as described in claim 1, characterized in that, The wafer carrier mechanism (200) includes a first chassis (210), a second chassis (220), multiple trays (230), multiple pressure columns (240), and hoop columns (250). The first chassis (210) and each of the trays (230) are provided with a plurality of mounting holes (211) along the circumferential direction; each of the pressure posts (240) includes a pin section (241) and a boss section (242) located at one end thereof. The pin section (241) passes through the mounting holes (211) of the first chassis (210) and the tray (230) and is engaged with them. The first chassis (210) and the tray (230) are engaged with the boss section (242) to form a clamping space for clamping the silicon carbide substrate (300). The second chassis (220) abuts against the outer side of the outermost boss section (242); The hoop (250) is engaged with the outside of the first chassis (210) and the second chassis (220).
3. The silicon carbide epitaxial growth apparatus as described in claim 2, characterized in that, The reaction chamber (100) is further provided with a growth chamber (110), which includes a left crescent (111), a right crescent (112), an upper baffle (113), and a lower baffle (114). The left crescent (111), the right crescent (112), the upper baffle (113), and the lower baffle (114) enclose a cuboid space. The wafer carrier (200) is disposed within the cuboid space.
4. The silicon carbide epitaxial growth apparatus as described in claim 3, characterized in that, The left half-moon (111) and the right half-moon (112) are respectively provided with mounting grooves (1111), and the first chassis (210) and the second chassis (220) are respectively provided with rotating shafts (212). The rotating shafts (212) cooperate with the mounting grooves (1111) so that the wafer carrier mechanism (200) rotates around the rotating shafts (212).
5. The silicon carbide epitaxial growth apparatus as described in claim 1, characterized in that, The reaction chamber (100) is a horizontal cylindrical chamber, and the inner wall of the reaction chamber (100) is made of graphite. The silicon carbide epitaxial growth apparatus further includes an induction heating system (400), which includes a plurality of induction heating coils (410) arranged around the reaction chamber (100).
6. The silicon carbide epitaxial growth apparatus as described in claim 5, characterized in that, The plurality of said induction heating coils (410) are configured to be grouped and controlled along the axial direction of said reaction chamber (100).
7. The silicon carbide epitaxial growth apparatus as described in claim 2, characterized in that, The wafer carrier (200) includes 2-10 trays (230), each tray (230) carrying one silicon carbide substrate (300).
8. A method for silicon carbide epitaxial growth, characterized in that, Includes the following steps: S1: Fix multiple silicon carbide substrates (300) vertically side by side on the wafer support mechanism (200), so that the main surface of each silicon carbide substrate (300) is parallel to the horizontal airflow direction, and place the wafer support mechanism (200) into the reaction chamber (100); S2: After evacuating the reaction chamber (100), introducing carrier gas and heating it to the epitaxial temperature, introduce the reaction gas source and doping gas source, start the rotation drive device to make the wafer support mechanism (200) rotate, and carry out epitaxial growth. S3: After growth is complete, stop ventilation, cool down in a protective atmosphere, and remove the epitaxial wafer.
9. The silicon carbide epitaxial growth method as described in claim 8, characterized in that, The epitaxial temperature in step S2 is 1500-1700℃, the pressure in the reaction chamber (100) is 50-200mbar, the carrier gas is high-purity H2, the reaction gas source includes silicon source trichlorosilane and carbon source ethylene, and the doping gas source is nitrogen or ammonia.
10. The silicon carbide epitaxial growth method as described in claim 8, characterized in that, The rotational speed of the rotary drive device in step S2 is 30-100 rpm; the wafer carrier mechanism (200) carries 2-10 silicon carbide substrates (300), and the reaction gas source flows parallel to the surface of each silicon carbide substrate (300).