battery cells

By improving the insulating film structure and fixing method of lithium-ion battery cells, and using adhesive to fix the electrode assembly around the perimeter and bottom, combined with side plate support, the problems of low production efficiency and safety in the existing technology have been solved, and efficient and safe cell production has been achieved.

CN123121107APending Publication Date: 2026-11-17SVOLT ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611624553.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-20
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing lithium-ion battery cells, the two ends of the bare cell insulation film are fixed to the corresponding lower plastic or lower plastic and end plate by hot melting. This results in low production efficiency, easy misalignment of hot melting points, burn-out and penetration of the bare cell insulation film, which affects production yield and cell safety performance.

Method used

An insulating film is used to wrap the sides and bottom of the electrode assembly and is fixed with adhesive. Only the opening end of the insulating film is heat-fused to the lower insulating part on the first cover plate. This eliminates the need for the insulating end plate or lower plastic structure at the bottom of the electrode assembly. Combined with the support and protection of the side plate, this simplifies the assembly process and reduces the heat melting point.

Benefits of technology

This improved production efficiency, avoided misalignment during hot melting and burn-off of the insulation film, ensured the production yield and safety performance of the battery cells, and saved on parts and assembly steps.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123121107A_ABST
    Figure CN123121107A_ABST
Patent Text Reader

Abstract

This application relates to the field of battery technology, and in particular to a battery cell, comprising a casing, an electrode assembly, an insulating film, two cover plates, a lower insulating component, and side plates. The insulating film covers the perimeter and bottom of the electrode assembly, and is fixed by adhesive at the end points on the sides and bottom. The coated electrode assembly is installed inside the casing, and the two cover plates are installed at both ends of the casing. The lower insulating component is installed inside one of the cover plates, and part of its structure extends into the opening end of the insulating film, and the two are heat-fused together. The side plates mate with the small side of the electrode assembly and can be installed outside or inside the insulating film. It is evident that by directly wrapping the perimeter and bottom of the electrode assembly with the insulating film, there is no need for insulating end plates or lower plastic structures, thus saving components. Furthermore, there is no need for heat-fusion welding with end plates or lower plastic, saving assembly steps, improving production efficiency, and reducing the heat melting point and various locations affected by heat melting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of battery technology, and in particular to a battery cell. Background Technology

[0002] Currently, lithium-ion batteries are widely used in various fields such as transportation power supply, power storage, new energy storage power supply, aerospace and military industries due to their advantages such as large capacity, high operating voltage, strong charge retention capacity, and long cycle life. The core component of a lithium-ion battery is the cell, and the blade cell is a commonly used type of cell. The blade cell structure generally includes a cover plate, shell, end plate, bare cell insulating film, electrode assembly, electrolyte, etc. Among them, the main function of the bare cell insulating film is insulation and protection, protecting the electrode assembly and preventing the electrode assembly from bridging the shell, which would cause a short circuit inside the cell. Currently, the bare cell insulating film is mainly fixed by heat fusion to the lower plastic of the two cover plates, or one end of the bare cell insulating film is fixed to the lower plastic of one cover plate by heat fusion, and the other end of the bare cell insulating film is fixed to the insulating end plate on the other side by heat fusion. Regardless of the fixing method, a lot of heat fusion is required, which reduces production efficiency, and the heat fusion points are prone to misalignment, burning of the bare cell insulating film, and penetration, which affects the production yield and cell safety performance. Summary of the Invention

[0003] The purpose of this application is to provide a battery cell that, to a certain extent, solves the technical problems existing in the prior art where the two ends of the bare battery cell insulation film are fixed to the corresponding lower plastic or the lower plastic and end plate by hot melting, which reduces production efficiency and has many hot melting points, making it easy to cause misalignment, burn-through of the bare battery cell insulation film, and other problems, thus affecting production yield and battery cell safety performance.

[0004] This application provides a battery cell, comprising: a housing, an electrode assembly, an insulating film, a first cover plate, a lower insulating member, a second cover plate, and a side plate; wherein, the insulating film covers the periphery and bottom of the electrode assembly, and is fixed by adhesive at the end of the side portion and the end of the bottom portion; the side plate is installed on the small side of the electrode assembly, and the side plate is either covered inside the insulating film or installed outside the insulating film, and the side plate is fixed to the insulating film by heat fusion; The assembly formed by the electrode assembly, the side plate, and the insulating film is installed inside the housing. The first cover plate and the second cover plate are respectively installed at both ends of the housing. The insulating film makes the periphery of the electrode assembly insulated from the housing and the bottom of the electrode assembly insulated from the second cover plate. The lower insulating member is installed on the inner side of the first cover plate facing the electrode assembly. A portion of the structure of the lower insulating member extends into the opening end of the insulating film covering the electrode assembly. The insulating film and the lower insulating member are fixed by heat fusion.

[0005] In the above technical solution, further, when the insulating film is in the unfolded state, the insulating film includes a body and a first bottom assembly surface and a second bottom assembly surface connected to the body; wherein, the body forms a plurality of crease lines arranged sequentially along a first preset direction; the first bottom assembly surface and the second bottom assembly surface are disposed on the same side of the body along a second preset direction, and crease lines are formed between the first bottom assembly surface and the second bottom assembly surface and the body; When the insulating film covers the outside of the electrode assembly, the body covers the periphery of the electrode assembly; the first bottom assembly surface and the second bottom assembly surface are folded and fit with the bottom end of the electrode assembly along its length.

[0006] In any of the above technical solutions, the insulating film further includes a bottom adhesive portion, and along the second preset direction, the bottom adhesive portion is connected to the outer side of the first bottom assembly surface away from the body, and a crease line is provided between the two, and an adhesive layer is provided on the bottom adhesive portion, and when the insulating film covers the outside of the electrode assembly, the bottom adhesive portion is folded and attached to the structure of the body covering the large surface side of the electrode assembly.

[0007] In any of the above technical solutions, the number of the bottom adhesive portions is multiple, and they are arranged sequentially at intervals along the first preset direction.

[0008] In any of the above technical solutions, the width of the coated electrode assembly is W0, the width of the bottom adhesive portion along the first preset direction is W3, the number of bottom adhesive portions is n, and 0.4≤nW3 / W0≤0.6.

[0009] In any of the above technical solutions, the length of the coated electrode assembly is L0, the length of the bottom adhesive portion along the second preset direction is L2, and 0.5≤10L2 / L0≤1.0.

[0010] In any of the above technical solutions, the length of the coated electrode assembly is L0, and L0 = 450-500 mm.

[0011] In any of the above technical solutions, the width of the coated electrode assembly is W0, and W0 = 140-210 mm.

[0012] In any of the above technical solutions, the adhesive layer on the bottom adhesive portion does not extend beyond the outer periphery of the bottom adhesive portion, and there is a gap C between the entire outer periphery of the adhesive layer on the bottom adhesive portion and the entire outer periphery of the bottom adhesive portion, where C = 2-3 mm.

[0013] In any of the above technical solutions, the adhesive layer on the bottom adhesive part is further described as an insulating and corrosion-resistant double-sided adhesive.

[0014] In any of the above technical solutions, the insulating film further includes a side adhesive portion, and along the first preset direction, the side adhesive portion is connected to one side of the body and a crease line is provided between the two, and an adhesive layer is provided on the side adhesive portion, and when the insulating film covers the outside of the electrode assembly, the side adhesive portion is folded and attached to the structure of the body covering the large surface side of the electrode assembly.

[0015] In any of the above technical solutions, the number of side adhesive portions is multiple, and they are arranged sequentially at intervals along a second preset direction.

[0016] In any of the above technical solutions, the length of the coated electrode assembly is L0, the length of the side adhesive portion along the second preset direction is L3, the number of the side adhesive portions is m, and 0.45≤mL3 / L0≤0.65.

[0017] In any of the above technical solutions, the width of the coated electrode assembly is W0, and the width of the side adhesive portion along the first preset direction is W2, where 0.1≤W2 / W0≤0.2.

[0018] In any of the above technical solutions, the adhesive layer on the side adhesive portion does not extend beyond the outer periphery of the side adhesive portion, and there is a gap C between the entire outer periphery of the adhesive layer on the side adhesive portion and the entire outer periphery of the side adhesive portion, and C=2-3mm.

[0019] In any of the above technical solutions, the adhesive layer on the side adhesive portion is further described as an insulating and corrosion-resistant double-sided adhesive.

[0020] In any of the above technical solutions, further, when the insulating film is in the unfolded state, the body includes a first side assembly small surface, a first large surface, a side small surface, a second large surface, and a second side assembly small surface; wherein, the first side assembly small surface, the first large surface, the side small surface, the second large surface, and the second side assembly small surface are arranged sequentially along a first preset direction, and a crease line is provided between any two adjacent surfaces; the first bottom assembly surface is disposed on one side of the first large surface along a second preset direction, and the second bottom assembly surface is disposed on one side of the second large surface along a second preset direction; When the insulating film covers the outside of the electrode assembly, the first large surface and the second large surface respectively mate with the two sides of the electrode assembly along its thickness direction. The first side assembly small surface and the second side assembly small surface are folded and mate with one side of the electrode assembly along its width direction. The side small surface mates with the other side of the electrode assembly along its width direction. The first bottom assembly surface and the second bottom assembly surface are folded and mate with the bottom of the electrode assembly along its length direction. The side small surface and / or the second side assembly small surface are provided with the side plate and are fixed to the side plate by heat fusion.

[0021] In any of the above technical solutions, the side facet and the second side combined facet are further provided with the side plate, and are respectively fixed to the corresponding side plate by heat fusion.

[0022] In any of the above technical solutions, the side plate provided on the side facet is a first side plate, and along the thickness direction of the side facet, the projection of the first side plate falls completely within the projection of the side facet. The distance between the first side plate and the corresponding sides of the side facet along the second preset direction is D, and D = 8-10 mm. The distance between the first side plate and the adjacent fold lines along the first preset direction is E, and E = 5-6 mm. The side plate provided on the second side facet is a second side plate, and after the electrode assembly, the two side plates and the insulating film are assembled, the second side plate and the first side plate are symmetrically arranged about the electrode assembly.

[0023] In any of the above technical solutions, the thickness of the insulating film is t1, the depth of the crease line is h, and 1 / 3 < h / t1 < 1 / 2.

[0024] In any of the above technical solutions, the thickness of the insulating film is further t1, and t1 = 0.12-0.15 mm.

[0025] In any of the above technical solutions, the crease line between the side facet and the first large facet is a third crease line, the crease line between the side facet and the second large facet is a fourth crease line, and the distance between the end of the third crease line and the end of the fourth crease line and the edge of the first large facet extending along the first preset direction along the second preset direction is A, and A=1-2mm.

[0026] In any of the above technical solutions, the thickness of the electrode assembly before coating is T', and the width of the first side assembly facet and the second side assembly facet along the first preset direction is W1, and W1=T'-(3-5mm).

[0027] In any of the above technical solutions, the thickness of the electrode assembly before coating is T', and the width of the first bottom assembly surface and the second bottom assembly surface along the second preset direction is L1, and L1=T'-(3-5mm).

[0028] In any of the above technical solutions, the first large surface and the second large surface, the first side combined small surface and the second side combined small surface, the first bottom combined surface and the second bottom combined surface, and the side small surface itself are all symmetrically arranged about the center line of the side small surface along the second preset direction.

[0029] In any of the above technical solutions, the crease line between the side facet and the second large facet is the fourth crease line, and the distance between the side edge of the first bottom composite surface that is close to and parallel to the fourth crease line and the fourth crease line along the first preset direction is B1, and B1 = 4-5mm.

[0030] In any of the above technical solutions, the crease line between the second side panel and the second large panel is the fifth crease line, and the distance between the side of the first bottom panel that is close to and parallel to the fifth crease line and the fifth crease line along the first preset direction is B2, and B2 = 4-5mm.

[0031] In any of the above technical solutions, further, a plurality of hot-melt zones are formed between any of the side plates and the insulating film, and the plurality of hot-melt zones are arranged sequentially at intervals along the length direction of the side plate.

[0032] In any of the above technical solutions, the area of ​​the large side of a single side plate is S0, the area of ​​a single hot melt zone is S1, the number of hot melt zones on any side plate is k, and 0.25≤10kS1 / S0≤0.4.

[0033] In any of the above technical solutions, the thickness of the side plate is t2, and t2 = 0.5-0.8m.

[0034] In any of the above technical solutions, the side plate is further provided with a first positioning hole, and the insulating film is provided with a second positioning hole corresponding to the first positioning hole.

[0035] In any of the above technical solutions, the bottom of the coated electrode assembly abuts against the second cover plate.

[0036] In any of the above technical solutions, the second cover plate and the housing are either an integral structure or an independent structure connected by welding.

[0037] In any of the above technical solutions, the insulating film is further described as an integral structure.

[0038] In any of the above technical solutions, further, the insulating film covering the two small sides of the electrode assembly is provided with a plurality of first through holes, and the plurality of first through holes are arranged sequentially at intervals along the length direction of the electrode assembly or simultaneously at intervals along the length direction and the thickness direction of the electrode assembly; the side plate is formed with a plurality of second through holes, and the plurality of second through holes are arranged sequentially at intervals along the length direction of the side plate or simultaneously at intervals along the length direction and the width direction of the side plate, and the second through holes are staggered with the first through holes.

[0039] In any of the above technical solutions, further, the insulating film covering the bottom of the electrode assembly is provided with a plurality of third through holes, and the plurality of third through holes are arranged sequentially at intervals along the width direction of the electrode assembly.

[0040] In any of the above technical solutions, further, when the insulating film is in the unfolded state, any two of the first preset direction, the second preset direction, and the thickness direction of the insulating film are perpendicular to each other, and when the insulating film covers the electrode assembly, the second preset direction is the same as the length direction of the electrode assembly.

[0041] In any of the above technical solutions, the battery cell further includes a positive terminal, a negative terminal, and an explosion-proof valve, wherein the positive terminal and the negative terminal are installed on the first cover plate, and the explosion-proof valve is installed on the second cover plate.

[0042] In any of the above technical solutions, the electrode assembly further includes at least one electrode group, and when the number of electrode groups is multiple, the multiple electrode groups are stacked together along the thickness direction of the electrode group.

[0043] Compared with the prior art, the beneficial effects of this application are as follows: The battery cell provided in this application modifies the structure and fixing method of the bare battery cell's insulating film. It directly wraps the perimeter and bottom of the electrode assembly with the insulating film and fixes it with adhesive. Therefore, only the open end of the insulating film needs to be heat-fused to the lower insulating component on the first cover plate. Since the bottom of the electrode assembly is covered with the insulating film, there is no need for insulating end plates or lower plastic structures, saving components. Furthermore, there is no need for heat-fusion welding to end plates or lower plastic, reducing assembly steps, improving production efficiency, and reducing heat-fusion points. This effectively avoids problems such as misalignment, burning of the bare battery cell's insulating film, and penetration, thus ensuring production yield and battery cell safety performance. Moreover, by reasonably limiting the size and performance of the insulating film and adhesive tape area, it meets the bonding and strength requirements. In addition, a side plate is provided on the small side of the electrode assembly, providing support and protection for the electrode assembly and facilitating its insertion into the casing. Attached Figure Description

[0044] To more clearly illustrate the technical solutions in the specific embodiments of this application or the prior art, the drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.

[0045] Figure 1 A schematic diagram showing the insulating film in an unfolded state according to an embodiment of this application; Figure 2 Another schematic diagram showing the insulating film in an unfolded state as provided in the embodiments of this application; Figure 3 for Figure 2 A partially enlarged structural diagram; Figure 4 for Figure 2 Another enlarged schematic diagram of the structure; Figure 5 for Figure 2 Another enlarged schematic diagram of the structure; Figure 6 This is a schematic diagram of the side plate provided in an embodiment of this application; Figure 7 An assembly diagram of the insulating film in the unfolded state and its assembly with the side plate, provided in the embodiments of this application; Figure 8 Another assembly diagram of the insulating film in the unfolded state and with the side plate provided in the embodiment of this application; Figure 9 for Figure 8A magnified structural diagram at point A; Figure 10 An assembly diagram of the insulating film, electrode assembly, and side plate provided in the embodiments of this application; Figure 11 Another assembly diagram of the insulating film, electrode assembly, and side plate provided in the embodiments of this application; Figure 12 An exploded view of the battery cell provided in the embodiments of this application; Figure 13 This is a schematic diagram of the structure of the electrode assembly before coating provided in an embodiment of this application.

[0046] Figure label: 1-Shell; 2-Explosion-proof valve; 3-Insulating film; 31-First side assembly small surface; 32-First large surface; 33-Side small surface; 34-Second large surface; 35-Second side assembly small surface; 36-First bottom assembly surface; 37-Second bottom assembly surface; 38-Bottom adhesive part; 39-Side adhesive part; 310-Adhesive layer; 311-Fold line; 3111-Third fold line; 3112-Fourth fold line; 3113-Fifth fold line; 312-First through hole; 313-Third through hole; 314-Body body; 315-Second positioning hole; 4-First cover plate; 6-Second cover plate; 7-Side plate; 71-Second through hole; 72-First positioning hole; 8-Hot melting point; 9-Hot melting zone; 10-Positive electrode post; 11-Negative electrode post; 12-Electrode assembly; a-First preset direction; b-Second preset direction. Detailed Implementation

[0047] The technical solutions of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are some embodiments of this application, but not all embodiments.

[0048] The components of the embodiments of this application described and shown in the accompanying drawings can be arranged and designed in a variety of different configurations. Therefore, the following detailed description of the embodiments of this application provided in the drawings is not intended to limit the scope of the claimed application, but merely to illustrate selected embodiments of the application.

[0049] Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0050] In the description of this application, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0051] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.

[0052] The following reference Figures 1 to 13 This application describes a battery cell according to some embodiments.

[0053] See Figures 1 to 13 As shown, an embodiment of this application provides a battery cell, including: a housing 1, an electrode assembly 12, an insulating film 3, a first cover plate 4, a lower insulating member, a second cover plate 6, and a side plate 7; wherein, the insulating film 3 covers the periphery and bottom of the electrode assembly 12, and is fixed by adhesive at the end of the side portion and the end of the bottom portion; the side plate 7 is installed on the small side of the electrode assembly 12, and the side plate is either covered inside the insulating film 3 or installed outside the insulating film 3, and the side plate 7 is fixed to the insulating film 3 by heat fusion, that is, the side plate 7 is installed on the small side of the electrode assembly 12. The insulating film 3 covers the periphery and bottom of the assembly of the electrode assembly 12 and the side plate 7. It is fixed with adhesive at the end of the side and the end of the bottom. The side plate 7 and the insulating film 3 are fixed by heat fusion. Alternatively, the insulating film 3 covers the periphery and bottom of the electrode assembly 12. It is fixed with adhesive at the end of the side and the end of the bottom. The side plate 7 is installed on the small side of the electrode assembly 12 after the film is wrapped. The side plate 7 and the insulating film 3 are fixed by heat fusion. The assembly formed by the electrode assembly 12, side plate 7, and insulating film 3 is installed inside the housing 1. The first cover plate 4 and the second cover plate 6 are respectively installed at both ends of the housing 1. The insulating film 3 insulates the periphery of the electrode assembly 12 from the housing 1 and simultaneously insulates the bottom of the electrode assembly 12 from the second cover plate 6. A lower insulating member is installed on the inner side of the first cover plate 4 facing the electrode assembly 12, and a portion of the lower insulating member extends into the opening end of the insulating film 3 covering the electrode assembly 12. The insulating film 3 and the lower insulating member are fixed by heat fusion. Figure 10 The image shows the heat melting point 8 between the insulating film 3 and the lower insulating member.

[0054] As can be seen from the structure described above, the battery cell provided in this application modifies the structure and fixing method of the bare battery cell insulating film 3. The insulating film 3 directly wraps around the perimeter and bottom of the electrode assembly 12 and is fixed with adhesive. Therefore, only the open end of the insulating film 3 needs to be heat-fused to the lower insulating component on the first cover plate 4. Since the bottom of the electrode assembly 12 is covered with the insulating film 3, there is no need for insulating end plates or lower plastic structures, saving components. Furthermore, there is no need for heat-fusion welding to end plates or lower plastic, saving assembly steps, improving production efficiency, and reducing the number of heat-fusion points (8). This effectively avoids problems such as misalignment, burning of the bare battery cell insulating film 3, and penetration, thereby ensuring production yield and battery cell safety performance. In addition, a side plate 7 is provided on the small side of the electrode assembly 12, providing support and protection for the electrode assembly 12 and facilitating its insertion into the casing.

[0055] Furthermore, preferably, the bottom of the coated electrode assembly 12 abuts against the second cover plate 6. That is to say, in this application, it is not necessary to provide an end plate and a lower plastic between the second cover plate 6 and the bottom of the coated electrode assembly 12. Of course, it is not limited to this. An end plate and a lower plastic can also be provided between the second cover plate 6 and the bottom of the coated electrode assembly 12, depending on the actual needs.

[0056] Furthermore, preferably, the second cover plate 6 and the shell 1 are either an integral structure or an independent structure connected by welding, both of which meet the usage requirements.

[0057] Further, preferably, the electrode assembly 12 includes at least one electrode group, and when there are multiple electrode groups, the multiple electrode groups are stacked together along the thickness direction of the electrode group. Further, preferably, the number of electrode assembly 12 is two, and the two electrode groups are stacked together sequentially along the thickness direction of the electrode group. Of course, it is not limited to this, and the number of electrode groups can also be one or more, depending on the actual needs. It should also be noted that when there are multiple electrode groups, the small facets of multiple electrode groups located on the same side share a side plate 7, and the insulating film 3 covers the outside of the assembly of all electrode groups and side plate 7.

[0058] In addition, it should be noted that the battery cell can also be equipped with an end plate and a lower plastic on the side of the second cover plate 6. During assembly, it is only necessary to put the bottom of the coated electrode assembly 12 against the end plate and the lower plastic, without the need for heat melting or welding.

[0059] In one embodiment of this application, preferably, as shown below, Figure 2 As shown, when the insulating film 3 is in the unfolded state, the insulating film 3 includes a body 314 and a first bottom assembly surface 36 and a second bottom assembly surface 37 connected to the body 314; wherein, the body 314 has a plurality of crease lines 311 arranged sequentially along a first preset direction a; the first bottom assembly surface 36 and the second bottom assembly surface 37 are disposed on the same side of the body 314 along the second preset direction b, and crease lines 311 are formed between the first bottom assembly surface 36 and the second bottom assembly surface 37 and the body 314; When the insulating film 3 covers the outside of the electrode assembly 12, the body 314 covers the periphery of the electrode assembly 12; the first bottom assembly surface 36 and the second bottom assembly surface 37 are folded and fit with the bottom end of the electrode assembly 12 along its length direction.

[0060] As can be seen from the structure described above, the body 314 is used to cover the four sides of the electrode assembly 12. The first bottom assembly surface 36 and the second bottom assembly surface 37 are folded and overlapped together to cover the bottom of the electrode assembly 12. It can be seen that the insulating film 3 is configured as a structure with a hollow interior and an opening at the top along the length of the electrode assembly 12. This opening at the top serves to avoid obstacles and facilitates the engagement of the electrode tabs and other components of the electrode assembly 12 with the electrode post.

[0061] Furthermore, preferably, the insulating film 3 is an integral structure with high overall strength and is easy to wrap; of course, it is not limited to this.

[0062] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2As shown, the insulating film 3 also includes a bottom adhesive portion 38, and along the second preset direction b, the bottom adhesive portion 38 is connected to the outer side of the first bottom assembly surface 36 away from the body 314, and a crease line 311 is provided between the two. An adhesive layer 310 is provided on the bottom adhesive portion 38. When the insulating film 3 covers the outside of the electrode assembly 12, the bottom adhesive portion 38 is folded and attached to the structure of the body 314 covering the large surface side of the electrode assembly 12.

[0063] As can be seen from the structure described above, when the electrode assembly 12 is wrapped, the side plate 7 is installed close to the electrode assembly 12. This assembly is covered inside the insulating film 3. After the first bottom assembly surface 36 and the second bottom assembly surface 37 are folded and overlapped, the bottom adhesive part 38 is folded onto the second large surface 34 of the insulating film 3 to achieve adhesion and fixation with the second large surface 34. This improves production efficiency, eliminates the need for additional adhesive tape equipment, simplifies the production process, and avoids the problem that using ordinary tape to directly stick to the outside of the insulating film 3 will stick to some of the vent holes, affecting the venting / electrolyte wetting of the electrode assembly 12.

[0064] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, there are multiple adhesive base portions 38, which are arranged sequentially at intervals along the first preset direction a.

[0065] As can be seen from the structure described above, the multiple sequentially spaced bottom adhesive portions 38 improve the stability and firmness of the bottom after adhesive bonding, and are less prone to wrinkling or bulging.

[0066] In one embodiment of this application, preferably, as shown below, Figure 3 and Figure 11 As shown, the width of the coated electrode assembly 12 is W0 (it should be noted that this width W0 is determined according to the actual situation. When the insulating film 3 only covers the electrode assembly, W0 refers to the overall width of all coated electrode assemblies, i.e., the electrode assembly 12. When the insulating film 3 covers both the electrode assembly and the side plate 7, W0 refers to the overall width of all coated electrode assemblies, i.e., the electrode assembly 12 and the side plate 7. The specific width is selected according to the actual situation). The width of the bottom adhesive part 38 along the first preset direction a is W3, and the number of bottom adhesive parts 38 is n, and 0.4≤nW3 / W0≤0.6.

[0067] Based on the structure described above, it is evident that the width and number of the adhesive base 38, as well as the width of the coated electrode assembly 12, have a certain impact on whether the bottom of the insulating film 3 will lift after bonding, and on the stability and firmness of the bond. Therefore, the above-mentioned relationship nW3 / W0 is recommended. When the value of nW3 / W0 is too small, it indicates that the width and / or number of bonding areas are insufficient, the gap between two adjacent bonding areas is large, and there is a problem of lifting after bonding. When the value of nW3 / W0 is too large, the width of the bonding area is large and / or the number is large, increasing the cost and bonding steps. Moreover, since the adjacent adhesive base 38 are close together, interference problems are likely to occur. Therefore, nW3 / W0 should be taken within the above-mentioned optimal range of 0.4-0.6 to ensure that there is no lifting after bonding, as well as the stability and firmness of the bond, and that the bonding operation is easy, without interference, and also helps to reduce costs and assembly steps. Of course, nW3 / W0 is not limited to the above optimal range. It can also be set to nW3 / W0 < 0.4 or nW3 / W0 > 0.6, depending on the actual needs.

[0068] In one embodiment of this application, preferably, as shown below, Figure 2 and Figure 11 As shown, the length of the coated electrode assembly 12 is L0, and the length of the bottom adhesive portion 38 along the second preset direction b is L2, and 0.5≤10L2 / L0≤1.0.

[0069] Based on the structure described above, it is evident that the length of the adhesive base 38 and the width of the coated electrode assembly 12 have a certain impact on whether the bottom of the insulating film 3 will lift after bonding, as well as the stability and firmness of the bond. Therefore, the relationship 10L² / L₀ is recommended. When the value of 10L² / L₀ is too small, it indicates that the width of the bonding area is insufficient, leading to lifting after bonding. When the value of 10L² / L₀ is too large, the width of the bonding area is too large, increasing costs and potentially causing interference during bonding. Therefore, 10L² / L₀ should be within the optimal range of 0.5-1.0 to ensure no lifting after bonding, good stability and firmness, and ease of bonding without interference. Of course, 10L² / L₀ is not limited to the optimal range; it can also be set to <0.5 or >1.0, depending on the specific needs.

[0070] In one embodiment of this application, preferably, as shown below, Figure 11 As shown, the length of the coated electrode assembly 12 is L0, and L0 = 450-500mm, which meets the current usage requirements. Of course, L0 is not limited to the above optimal range; it can also be set to L0 < 450mm or L0 > 500mm, depending on the actual needs.

[0071] In one embodiment of this application, preferably, as shown below, Figure 11 As shown, the width of the coated electrode assembly 12 is W0, and W0 = 140-210mm, which meets the current usage requirements. Of course, W0 is not limited to the above optimal range; it can also be set to W0 < 140mm or W0 > 210mm, depending on the actual needs.

[0072] In one embodiment of this application, preferably, as shown below, Figure 3 As shown, the adhesive layer 310 on the bottom adhesive portion 38 does not extend beyond the outer periphery of the bottom adhesive portion 38, and there is a gap C between the entire outer periphery of the adhesive layer 310 on the bottom adhesive portion 38 and the entire outer periphery of the bottom adhesive portion 38, where C = 2-3 mm.

[0073] As described above, when the adhesive layer 310 on the bottom adhesive portion 38 extends beyond the corresponding bottom adhesive portion 38, the extended adhesive layer 310 structure will be exposed on the outer side of the insulating film 3 away from the electrode assembly 12. During installation, it may adhere to the housing 1, causing interference, affecting assembly, or even tearing the insulating film 3 from the electrode assembly 12. Therefore, C should be within the optimal range described above to ensure the area of ​​the adhesive region within a limited space, preventing peeling after adhesion, ensuring stability and firmness after adhesion, and facilitating the installation of the coated electrode assembly 12 into the housing without easily causing interference. Of course, C is not limited to the optimal range described above; C < 2mm or C > 3mm can also be selected according to actual needs.

[0074] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the adhesive layer 310 on the base adhesive part 38 is an insulating and corrosion-resistant double-sided adhesive, and preferably, the temperature resistance range is -40-120℃, the peel force at 180° is required to be N>35N (GB / T2792-2014), the peel force with PP is >20N (to ensure the bonding strength between the adhesive layer 310 and the first folded edge), the holding force meets the following requirements: >60h without falling off (ASTM D3654), the initial tack is >25N (GB / T31125-2014), to ensure the bonding effect.

[0075] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the insulating film 3 also includes a side adhesive portion 39, and along the first preset direction a, the side adhesive portion 39 is connected to one side of the body 314 and a crease line 311 is provided between the two. The side adhesive portion 39 is provided with an adhesive layer 310. When the insulating film 3 covers the outside of the electrode assembly 12, the side adhesive portion 39 is folded and attached to the structure of the body 314 covering the large surface side of the electrode assembly 12.

[0076] As can be seen from the structure described above, when the electrode assembly 12 is wrapped, the side plate 7 is installed close to the electrode assembly 12. This assembly is covered inside the insulating film 3. After the first side assembly small surface 31 and the second side assembly small surface 35 are folded and overlapped, the side adhesive part 39 is folded onto the second large surface 34 of the insulating film 3 to achieve adhesion and fixation with the second large surface 34. This improves production efficiency, eliminates the need for additional tape pasting equipment, simplifies the production process, and avoids the problem that using ordinary tape to directly paste on the outside of the insulating film 3 will stick to some of the vent holes, affecting the venting / electrolyte wetting of the electrode assembly 12.

[0077] Furthermore, preferably, the first side assembly surface 31 described below is provided with a side adhesive portion 39, and a crease line 311 is provided between the two. Of course, it is not limited to this, and the side adhesive portion 39 may also be provided on the second side assembly surface 35.

[0078] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, there are multiple side adhesive portions 39, which are arranged sequentially at intervals along the second preset direction b.

[0079] As can be seen from the structure described above, the multiple sequentially spaced side adhesive portions 39 improve the stability and firmness of the adhesive side, and are less prone to wrinkling or bulging.

[0080] In one embodiment of this application, preferably, as shown below, Figure 3 and Figure 11 As shown, the length of the coated electrode assembly 12 is L0, the length of the side adhesive portion 39 along the second preset direction b is L3, the number of side adhesive portions 39 is m, and 0.45≤mL3 / L0≤0.65.

[0081] Based on the structure described above, it is evident that the length and number of side adhesive portions 39, as well as the length of the coated electrode assembly 12, have a certain impact on whether the insulating film 3 will lift after side bonding, and on the stability and firmness of the bond. Therefore, the above-mentioned relationship mL3 / L0 is recommended. When the value of mL3 / L0 is too small, it indicates that the length and / or number of bonding areas are insufficient, the gap between two adjacent bonding areas is large, and there is a problem of lifting after bonding. When the value of mL3 / L0 is too large, the width of the bonding area is large and / or the number is large, increasing the cost and bonding steps. Moreover, since the adjacent side adhesive portions 39 are close together, interference problems are likely to occur. Therefore, mL3 / L0 is set within the above-mentioned optimal range of 0.45-0.65 to ensure that the bond does not lift, and that the bond is stable and firm. It is also easy to bond, does not cause interference, and helps to reduce costs and assembly steps. Of course, the value of mL3 / L0 is not limited to the above-mentioned optimal range. It can also be set to mL3 / L0 < 0.45 or mL3 / L0 > 0.65, depending on the actual needs.

[0082] In one embodiment of this application, preferably, as shown below, Figure 11 As shown, the width of the coated electrode assembly 12 is W0, and the width of the side adhesive portion 39 along the first preset direction a is W2, where 0.1≤W2 / W0≤0.2.

[0083] Based on the structure described above, it is clear that if the value of W2 / W0 is too small, the width of the bonding area on the side is insufficient, leading to peeling after bonding. This results in an unstable and weak bonded structure. Conversely, if the value of W2 / W0 is too large, it increases material costs and may exceed the bonding limits. Therefore, W2 / W0 should be within the optimal range of 0.1-0.2 to ensure sufficient tape width, prevent peeling after bonding, and maintain stability and strength. This also facilitates bonding operations, avoids interference, and helps reduce costs. Of course, W2 / W0 is not limited to the optimal range; it can also be set to <0.1 or >0.2, depending on the specific needs.

[0084] In one embodiment of this application, preferably, as shown below, Figure 3 As shown, the adhesive layer 310 on the side adhesive portion 39 does not extend beyond the outer periphery of the side adhesive portion 39, and there is a gap C between the entire outer periphery of the adhesive layer 310 on the side adhesive portion 39 and the entire outer periphery of the side adhesive portion 39, and C = 2-3 mm.

[0085] As described above, when the adhesive layer 310 on the side adhesive portion 39 extends beyond the corresponding side adhesive portion 39, the extended adhesive layer 310 structure will be exposed on the outer side of the insulating film 3 away from the electrode assembly 12. During installation, it may adhere to the housing 1, causing interference, affecting assembly, or even tearing the insulating film 3 from the electrode assembly 12. Therefore, C should be within the optimal range described above to ensure the area of ​​the adhesive region within a limited space, preventing warping after adhesion, ensuring stability and firmness after adhesion, and facilitating the installation of the coated electrode assembly 12 into the housing without easily causing interference. Of course, C is not limited to the optimal range described above; C < 2mm or C > 3mm can also be selected according to actual needs.

[0086] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the adhesive layer 310 on the side adhesive part 39 is an insulating and corrosion-resistant double-sided adhesive, and preferably, the temperature resistance range is -40-120℃, the peel force at 180° is required to be N>35N (GB / T2792-2014), the peel force with PP is >20N (to ensure the bonding strength between the adhesive layer 310 and the first folded edge), the holding force meets the following requirements: >60h without falling off (ASTM D3654), the initial tack is >25N (GB / T31125-2014), to ensure the bonding effect.

[0087] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 , Figure 10 As shown, when the insulating film 3 is in the unfolded state, the body 314 includes a first side assembly small surface 31, a first large surface 32, a side small surface 33, a second large surface 34, and a second side assembly small surface 35; wherein, the first side assembly small surface 31, the first large surface 32, the side small surface 33, the second large surface 34, and the second side assembly small surface 35 are arranged sequentially along a first preset direction a, and a crease line 311 is provided between any two adjacent ones; the first bottom assembly surface 36 is disposed on one side of the first large surface 32 along a second preset direction b, and the second bottom assembly surface 37 is disposed on one side of the second large surface 34 along a second preset direction b, and the first bottom assembly surface 36 and the second bottom assembly surface 37 are located on the same side of the body 314 along the second preset direction b; When the insulating film 3 covers the outside of the electrode assembly 12, the first large surface 32 and the second large surface 34 respectively mate with the two sides of the electrode assembly 12 along its thickness direction. The first side combination small surface 31 and the second side combination small surface 35 are folded and mate with one side of the electrode assembly 12 along its width direction. The side small surface 33 mates with the other side of the electrode assembly 12 along its width direction. The first bottom combination surface 36 and the second bottom combination surface 37 are folded and mate with the bottom of the electrode assembly 12 along its length direction. The side small surface 33 and / or the second side combination small surface 35 are provided with side plates 7 (it can be seen that the two side plates 7 are respectively provided on the two small surface sides of the electrode assembly 12 along its width direction), and are fixed to the side plates 7 by heat fusion.

[0088] As can be seen from the structure described above, the first side assembly facet 31 and the second side assembly facet 35 cooperate as the side end of the electrode assembly 12 after being wrapped, and cooperate with the assembly of one small side facet of the electrode assembly 12 and the side plate 7. The first large facet 32 ​​and the second large facet 34 cooperate with the two large faces of the electrode assembly 12. The side facet 33 cooperates with the assembly of the other small side facet of the electrode assembly 12 and the side plate 7. The first bottom assembly facet 36 and the second bottom assembly facet 37 serve as the bottom end of the electrode assembly 12 after being wrapped, and cooperate with the bottom of the electrode assembly 12. It can be seen that the insulating film 3 is ultimately formed into a structure that is hollow inside and has an opening at the top along the length of the electrode assembly 12. This top opening serves to avoid interference, making it easier for the electrode tabs of the electrode assembly 12 to cooperate with the poles.

[0089] In one embodiment of this application, preferably, as shown below, Figures 6 to 9 As shown, both the side facet 33 and the second side combined facet 35 are equipped with side plates 7, and are respectively fixed to the corresponding side plates 7 by heat fusion.

[0090] As can be seen from the structure described above, side plates 7 are installed on both small sides of the pole assembly 12 in this application, thereby achieving support and protection on both sides when the pole assembly 12 is installed in the housing, further accelerating the installation efficiency and supporting the pole assembly 12.

[0091] Of course, it is not limited to this. Alternatively, a side plate 7 may be provided on only one small side of the pole assembly 12, depending on the actual needs.

[0092] In one embodiment of this application, preferably, as shown below, Figure 9As shown, the side plate 7 provided on the side facet 33 is the first side plate 7, and along the thickness direction of the side facet 33, the projection of the first side plate 7 falls completely within the projection of the side facet 33. The distance between the two sides of the first side plate 7 along the second preset direction b and the two sides of the corresponding side facet 33 is D, and D = 8-10mm. The distance between the two sides of the first side plate 7 along the first preset direction a and the fold lines 311 that are close to each other on both sides is E, and E = 5-6mm. The side plate 7 provided on the second side assembly facet 35 is the second side plate 7. After the electrode assembly 12, the two side plates 7 and the insulating film 3 are assembled, the second side plate 7 and the first side plate 7 are symmetrically arranged about the electrode assembly 12.

[0093] As can be seen from the structure described above, the gaps D and E mentioned above are provided between the edges of the first side plate 7 and the side face 33 to avoid coating interference and help improve assembly efficiency. Of course, it is not limited to this. For D, D can be <8mm or D>10mm, depending on the actual needs. For E, E can be <5mm or E>6mm, depending on the actual needs.

[0094] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the thickness of the insulating film 3 is t1, the depth of the crease line 311 is h (t1 and h are not shown in the figure), and 1 / 3 < h / t1 < 1 / 2.

[0095] Based on the structure described above, if h / t1 is too small, it means that the depth of the crease line 311 is small, making folding difficult. If h / t1 is too large, it means that the depth of the crease line 311 is large, affecting the strength of this area and reducing the insulation performance. Therefore, h / t1 should be taken within the above-mentioned optimal range to ensure that it is easy to fold along the crease line 311 to cover the pole assembly 12, while meeting the strength requirements and ensuring the insulation performance. Of course, h / t1 is not limited to the above-mentioned optimal range; h / t1 can also be <1 / 3 or >1 / 2, depending on the actual needs.

[0096] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the thickness of the insulating film 3 is t1 (t1 is not shown in the figure), and t1 = 0.12-0.15 mm, which meets the requirements of strength and insulation. Of course, it is not limited to this. t1 can also be made < 0.12 mm or > 0.15 mm, depending on the actual needs.

[0097] In one embodiment of this application, preferably, as shown below, Figure 2 and Figure 5As shown, the crease line 311 between the side facet 33 and the first large facet 32 ​​is the third crease line 3111, and the crease line 311 between the side facet 33 and the second large facet 34 is the fourth crease line 3112. The distance between the end of the third crease line 3111 and the end of the fourth crease line 3112 and the edge of the first large facet 32 ​​extending along the first preset direction a along the second preset direction b is A, and A = 1-2 mm.

[0098] As described above, the third crease line 3111 and the fourth crease line 3112 do not extend the entire length, but leave a certain area at the ends. This prevents complete breakage along the crease line 311, ensuring connection strength and further improving insulation. Of course, A is not limited to the above optimal range; A can also be set < 1 mm or > 2 mm, depending on actual needs.

[0099] In one embodiment of this application, preferably, as shown below, Figure 3 and Figure 13 As shown, the thickness of the electrode assembly 12 before coating is T', and the widths of the first side assembly surface 31 and the second side assembly surface 35 along the first preset direction a are both W1, and W1 = T' - (3-5mm).

[0100] As can be seen from the structure described above, the width of the first side assembly facet 31 and the second side assembly facet 35 is less than the thickness of the pole assembly 12. In this way, when the first side assembly facet 31 and the second side assembly facet 35 are folded together, there will be no wrinkling or other problems caused by the extra structure. This not only facilitates the subsequent insertion into the shell, but also further improves the insulation performance.

[0101] In one embodiment of this application, preferably, as shown below, Figure 4 and Figure 13 As shown, the thickness of the electrode assembly 12 before coating is T', and the width of the first bottom assembly surface 36 and the second bottom assembly surface 37 along the second preset direction b is L1, and L1 = T' - (3-5mm).

[0102] As can be seen from the structure described above, the width of the first bottom assembly surface 36 and the second bottom assembly surface 37 is less than the thickness of the pole assembly 12. In this way, when the first side assembly surface 31 and the second side assembly surface 35 are folded together, there will be no wrinkling or other problems caused by the extra structure. This not only facilitates the later insertion into the shell, but also further improves the insulation performance.

[0103] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2As shown, the first large surface 32 and the second large surface 34, the first side combination small surface 31 and the second side combination small surface 35, the first bottom combination surface 36 and the second bottom combination surface 37, and the side small surface 33 are all symmetrically arranged about the center line of the side small surface 33 along the second preset direction b, which facilitates processing and manufacturing and assembly accuracy, etc., and of course, it is not limited to this.

[0104] Furthermore, preferably, the first side combination small surface 31, the first large surface 32, the side small surface 33, the second large surface 34, and the second side combination small surface 35 are all flush with each other along the two sides of the second preset direction b.

[0105] Furthermore, preferably, the first side assembly facet 31, the first large facet 32, the side facet 33, the second large facet 34, the second side assembly facet 35, the first bottom assembly facet 36, and the second bottom assembly facet 37 are all rectangular structures to meet the assembly requirements with the cuboid-shaped pole assembly 12. Of course, it is not limited to this, and can also adaptively change with the shape of the pole assembly 12.

[0106] In one embodiment of this application, preferably, as shown below, Figure 4 As shown, the crease line 311 between the side facet 33 and the second large facet 34 is the fourth crease line 3112. The distance between the side edge of the first bottom assembly surface 36 that is close to and parallel to the fourth crease line 3112 and the fourth crease line 3112 along the first preset direction a is B1, and B1 = 4-5 mm. This ensures no interference during the folding and assembly process, meets assembly requirements, and helps improve assembly efficiency. Of course, B1 is not limited to the above optimal range; it can also be set to < 4 mm or > 5 mm, depending on actual needs.

[0107] In one embodiment of this application, preferably, as shown below, Figure 4 As shown, the crease line 311 between the second side assembly small surface 35 and the second large surface 34 is the fifth crease line 3113. The distance between the side edge of the first bottom assembly surface 36 that is close to and parallel to the fifth crease line 3113 and the fifth crease line 3113 along the first preset direction a is B2, and B2 = 4-5 mm. This ensures no interference during the folding and assembly process, meets assembly requirements, and helps improve assembly efficiency. Of course, B2 is not limited to the above optimal range; it can also be set to < 4 mm or > 5 mm, depending on actual needs.

[0108] In one embodiment of this application, preferably, as shown below, Figure 7 and Figure 8 As shown, multiple hot-melt zones 9 are formed between any side plate 7 and the insulating film 3, and the multiple hot-melt zones 9 are arranged sequentially at intervals along the length direction of the side plate 7.

[0109] As can be seen from the structure described above, multiple heat-fusion zones 9 are arranged sequentially and at intervals along the length of the side plate 7, which further enhances the stability and firmness of the side plate 7 after it is heat-fused and fixed to the insulating film 3. Of course, this is not the only option; a single heat-fusion zone 9 may also be provided.

[0110] In one embodiment of this application, preferably, as shown below, Figure 7 As shown, the area of ​​the large side of a single side plate 7 is S0, the area of ​​a single hot melt zone 9 is S1, and the number of hot melt zones 9 on any side plate 7 is k, and 0.25≤10kS1 / S0≤0.4, ensuring that the surface is flat and does not warp after hot melting, the fixing strength meets the requirements, and it will not affect the coating.

[0111] In one embodiment of this application, preferably, as shown below, Figure 6 As shown, the thickness of the side plate 7 is t2 (t2 is not shown in the figure), and t2 = 0.5-0.8m, to ensure strength, thereby ensuring the support and protection of the pole assembly 12. Of course, it is not limited to this, t2 can also be made < 0.5m or > 0.8m, depending on the actual needs.

[0112] In one embodiment of this application, preferably, as shown below, Figure 6 As shown, the side plate 7 has a first positioning hole 72, and the insulating film 3 has a second positioning hole 315 corresponding to the first positioning hole 72. When the side plate 7 and the insulating film 3 are assembled, the first positioning hole 72 and the second positioning hole 315 correspond to each other, thereby playing the role of assembly positioning. In addition, the first positioning hole 72 and the second positioning hole 315 can also play the role of positioning during processing. Of course, the first positioning hole 72 and the second positioning hole 315 may not be provided, depending on the actual needs.

[0113] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the insulating film 3 is an integral structure with high overall strength and is not easily damaged, providing better insulation and protection for the electrode assembly 12.

[0114] In one embodiment of this application, preferably, as shown below, Figure 1 , Figure 2 , Figure 5 and Figure 6As shown, the insulating film 3 covers the two small side surfaces of the electrode assembly 12 and is provided with a plurality of first through holes 312. The plurality of first through holes 312 are arranged sequentially and spaced apart along the length direction of the electrode assembly 12 or simultaneously arranged sequentially and spaced apart along both the length direction and the thickness direction of the electrode assembly 12. That is, the first side assembly surface 31, the side surface 33, and the second side assembly surface 35 are all provided with a plurality of first through holes 312. The plurality of first through holes 312 on the first side assembly surface 31, the side surface 33, and the second side assembly surface 35 are arranged sequentially and spaced apart along the second preset direction b or simultaneously arranged sequentially and spaced apart along both the first preset direction a and the second preset direction b. The side plate 7 has a plurality of second through holes 71, and the plurality of second through holes 71 are arranged sequentially at intervals along the length direction of the side plate 7 or along both the length and width directions of the side plate 7. In the state where the insulating film 3 covers the assembly of the electrode assembly 12 and the side plate 7, the second through holes 71 are staggered with the first through holes 312.

[0115] As can be seen from the structure described above, multiple first through holes 312 are provided on the first side assembly surface 31, side surface 33, and second side assembly surface 35, which helps to accelerate the wetting of the side of the electrode assembly 12 and the venting during thermal runaway of the battery cell, further improving the wetting effect of the electrode assembly 12 and the venting during thermal runaway. Furthermore, a second through hole 71 is provided on the side plate 7, which helps to accelerate the wetting of the side and bottom of the electrode assembly 12 and the venting during thermal runaway of the battery cell, further improving the wetting effect of the electrode assembly 12 and the venting during thermal runaway. Moreover, the second through hole 71 is staggered with the first through hole 312, which plays a role in insulation protection.

[0116] Of course, the second through hole 71 may not be provided on the side plate 7. In addition, if the second through hole 71 is provided, the second through hole 71 and the first through hole 312 may not be staggered, that is, the two can be set opposite to each other.

[0117] In addition, it should be noted that the first through hole 312 may not be provided, depending on the actual needs.

[0118] In one embodiment of this application, preferably, as shown below, Figure 1 and Figure 2 As shown, the insulating film 3 covering the bottom of the electrode assembly 12 has a plurality of third through holes 313, and the plurality of third through holes 313 are arranged sequentially at intervals along the width direction of the electrode assembly 12. That is, the first bottom assembly surface 36 and the second bottom assembly surface 37 both have a plurality of third through holes 313, and the first through holes 312 on the first bottom assembly surface 36 and the second bottom assembly surface 37 are arranged sequentially at intervals along the first preset direction a.

[0119] As can be seen from the structure described above, multiple third through holes 313 are provided on both the first bottom assembly surface 36 and the second bottom assembly surface 37, which helps to accelerate the wetting of the bottom of the electrode assembly 12 and the venting during thermal runaway of the battery cell, further improving the wetting effect of the electrode assembly 12 and the venting during thermal runaway.

[0120] It should be noted that the third through hole 313 may not be provided, or the first through hole 312 may be provided on one or more of the first side assembly surface 31, side surface 33, second side assembly surface 35, first bottom assembly surface 36 and second bottom assembly surface 37, depending on the actual needs.

[0121] In one embodiment of this application, preferably, as shown below, Figure 2 As shown, when the insulating film 3 is in the unfolded state, any two of the first preset direction a, the second preset direction b, and the thickness direction of the insulating film 3 are perpendicular to each other. When the insulating film 3 covers the electrode assembly 12, the second preset direction b is the same as the length direction of the electrode assembly 12, which meets the requirements for use and assembly. Of course, it is not limited to this.

[0122] In one embodiment of this application, preferably, as shown below, Figure 10 and Figure 12 As shown, the battery cell also includes a positive terminal 10, a negative terminal 11, and an explosion-proof valve 2. The positive terminal 10 and the negative terminal 11 are installed on the first cover plate 4, and the explosion-proof valve 2 is installed on the second cover plate 6, thereby achieving electrothermal separation and further improving safety and reliability.

[0123] In summary, multiple sets of experiments were conducted to verify the effectiveness of this technical solution: Experimental method: Constant current charging was performed with I = rated charging power P / nominal voltage U until the thermal runaway judgment condition (fire and explosion) was triggered, or the temperature reached 300℃. Then, heating and charging were stopped and the patient was observed for 1 hour.

[0124] Test requirements: It should not ignite or explode after thermal runaway, and should not rupture at a location other than the explosion-proof valve or pressure relief point.

[0125] For details, please refer to section 6.7.4.2.1 of the national standard GB / T 36276.

[0126] Preferably, the initial thermal runaway performance test of the battery cell is carried out according to the following steps: a) The test sample that has completed the initial charging according to national standard 6.2.4.1.1 is placed in the thermal runaway test device; b) Select heating components and temperature sensors and place them on the surface of the test sample. Set the temperature sampling period to 1s. Set the condition for thermal runaway to be that three consecutive temperature rise rate values ​​are ≥3℃ / s or that fire or explosion occurs. c) Connect the test sample to the charging / discharging device and its voltage data sampling line; d) Charge with a constant current of I=P / U, start heating, and record time, voltage, current, temperature, and rate of temperature rise. Record the experimental phenomena, including expansion, leakage, smoke, fire, explosion, shell rupture and rupture location. e) When the conditions for triggering thermal runaway are met, or the temperature reaches 300°C, or the test time reaches 4 hours, stop charging and heating, observe for 1 hour, and record the time, voltage, temperature, temperature rise rate, and test phenomena, including expansion, leakage, smoke, fire, explosion, shell rupture and rupture location. f) Disconnect the test sample from the charging / discharging device, remove the heating element and data sampling line, and take out the test sample; g) Record the temperature at which thermal runaway occurs as the thermal runaway temperature; h) Repeat steps a) to g) until all test samples are tested.

[0127] The verification results are shown in Table 1 below: Table 1 Experimental Data

[0128] Based on the experimental data in the table, it can be seen that when the above design scheme is met, there are no abnormalities in the cell coating, no peeling or falling off in the adhesive area, and the strength meets the requirements.

[0129] It should be noted that, unless otherwise specified, all dimensional parameters mentioned in this manual were obtained under the following conditions: Test environment: Measurements were conducted at a temperature of 23℃±2℃ and a relative humidity of 50%±10%. Before measurement, the sample of the battery cell or casing to be measured was placed in this environment and left to stand for at least 2 hours to allow the sample temperature to match the ambient temperature, thereby reducing measurement errors caused by temperature changes. During measurement, the sample was left in a natural state, and no external force was applied to the sample.

[0130] Measurement equipment: Linear dimensions can be measured using an image measuring instrument (image measuring projector) with a measurement accuracy of not less than 0.01 mm; or using vernier calipers with an accuracy of not less than 0.02 mm; for dimensions requiring high precision, a coordinate measuring machine can be used; wall thickness and other dimensions can be measured using a micrometer with an accuracy of not less than 0.001 mm; and protrusions and other structures can be measured using a dial indicator in conjunction with a measuring platform with a measurement accuracy of not less than 0.01 mm.

[0131] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A battery cell, characterized in that, include: The assembly comprises a housing, an electrode assembly, an insulating film, a first cover plate, a lower insulating component, a second cover plate, and a side plate; wherein the insulating film covers the perimeter and bottom of the electrode assembly, and is fixed by adhesive at the end of the side portion and the end of the bottom portion; the side plate is installed on the small side of the electrode assembly, and the side plate is either covered inside the insulating film or installed outside the insulating film, and the side plate is fixed to the insulating film by heat fusion; The assembly formed by the electrode assembly, the side plate, and the insulating film is installed inside the housing. The first cover plate and the second cover plate are respectively installed at both ends of the housing. The insulating film makes the periphery of the electrode assembly insulated from the housing and the bottom of the electrode assembly insulated from the second cover plate. The lower insulating member is installed on the inner side of the first cover plate facing the electrode assembly. A portion of the structure of the lower insulating member extends into the opening end of the insulating film covering the electrode assembly. The insulating film and the lower insulating member are fixed by heat fusion.

2. The battery cell according to claim 1, characterized in that, When the insulating film is in an unfolded state, the insulating film includes a body and a first bottom assembly surface and a second bottom assembly surface connected to the body; wherein, the body has a plurality of crease lines arranged sequentially along a first preset direction; the first bottom assembly surface and the second bottom assembly surface are disposed on the same side of the body along a second preset direction, and crease lines are formed between the first bottom assembly surface and the second bottom assembly surface and the body; When the insulating film covers the outside of the electrode assembly, the body covers the periphery of the electrode assembly; the first bottom assembly surface and the second bottom assembly surface are folded and fit with the bottom end of the electrode assembly along its length.

3. The battery cell according to claim 2, characterized in that, The insulating film also includes a bottom adhesive portion, and along a second preset direction, the bottom adhesive portion is connected to the outer side of the first bottom assembly surface away from the body, and a crease line is provided between the two. An adhesive layer is provided on the bottom adhesive portion, and when the insulating film covers the outside of the electrode assembly, the bottom adhesive portion is folded and attached to the structure of the body covering the large surface side of the electrode assembly.

4. The battery cell according to claim 3, characterized in that, The number of the adhesive base portions is multiple, and they are sequentially spaced along the first preset direction; and / or The width of the coated electrode assembly is W0, the width of the bottom adhesive portion along the first preset direction is W3, the number of bottom adhesive portions is n, and 0.4≤nW3 / W0≤0.6; and / or The length of the coated electrode assembly is L0, the length of the bottom adhesive portion along the second preset direction is L2, and 0.5 ≤ 10L2 / L0 ≤ 1.0; and / or The length of the coated electrode assembly is L0, and L0 = 450-500 mm; and / or The width of the coated electrode assembly is W0, and W0 = 140-210 mm; and / or The adhesive layer on the bottom adhesive portion does not extend beyond the outer periphery of the bottom adhesive portion, and there is a gap C between the entire outer periphery of the adhesive layer on the bottom adhesive portion and the entire outer periphery of the bottom adhesive portion, where C = 2-3 mm; and / or The adhesive layer on the bottom adhesive part is an insulating and corrosion-resistant double-sided adhesive.

5. The battery cell according to claim 2, characterized in that, The insulating film also includes a side adhesive portion, and along the first preset direction, the side adhesive portion is connected to one side of the body and a crease line is provided between the two. The side adhesive portion is provided with an adhesive layer. When the insulating film covers the outside of the electrode assembly, the side adhesive portion is folded and attached to the structure of the body covering the large surface side of the electrode assembly.

6. The battery cell according to claim 5, characterized in that, The number of the side adhesive portions is multiple, and they are arranged sequentially at intervals along a second preset direction; and / or The length of the coated electrode assembly is L0, the length of the side adhesive portion along the second preset direction is L3, the number of side adhesive portions is m, and 0.45≤mL3 / L0≤0.65; and / or The width of the coated electrode assembly is W0, and the width of the side adhesive portion along the first preset direction is W2, where 0.1 ≤ W2 / W0 ≤ 0.2; and / or The adhesive layer on the side adhesive portion does not extend beyond the outer periphery of the side adhesive portion, and there is a gap C between the entire outer periphery of the adhesive layer on the side adhesive portion and the entire outer periphery of the side adhesive portion, where C = 2-3 mm; and / or The adhesive layer on the side adhesive portion is all insulating and corrosion-resistant double-sided adhesive.

7. The battery cell according to claim 2, characterized in that, When the insulating film is unfolded, the body includes a first side assembly small surface, a first large surface, a side small surface, a second large surface, and a second side assembly small surface; wherein, the first side assembly small surface, the first large surface, the side small surface, the second large surface, and the second side assembly small surface are arranged sequentially along a first preset direction, and a crease line is provided between any two adjacent surfaces; the first bottom assembly surface is disposed on one side of the first large surface along a second preset direction, and the second bottom assembly surface is disposed on one side of the second large surface along a second preset direction; When the insulating film covers the outside of the electrode assembly, the first large surface and the second large surface respectively mate with the two sides of the electrode assembly along its thickness direction. The first side assembly small surface and the second side assembly small surface are folded and mate with one side of the electrode assembly along its width direction. The side small surface mates with the other side of the electrode assembly along its width direction. The first bottom assembly surface and the second bottom assembly surface are folded and mate with the bottom of the electrode assembly along its length direction. The side small surface and / or the second side assembly small surface are provided with the side plate and are fixed to the side plate by heat fusion.

8. The battery cell according to claim 7, characterized in that, Both the side facet and the second side combined facet are equipped with the side plate, and are respectively fixed to the corresponding side plate by heat fusion; The side plate provided on the side facet is the first side plate, and along the thickness direction of the side facet, the projection of the first side plate falls completely within the projection of the side facet. The distance between the first side plate and the corresponding sides of the side facet along the second preset direction is D, where D = 8-10 mm. The distance between the first side plate and the adjacent fold lines along the first preset direction is E, where E = 5-6 mm. The side plate provided on the second side facet is the second side plate, and after the electrode assembly, the two side plates, and the insulating film are assembled, the second side plate and the first side plate are symmetrically arranged about the electrode assembly; and / or The thickness of the insulating film is t1, the depth of the crease line is h, and 1 / 3 < h / t1 < 1 / 2; and / or The thickness of the insulating film is t1, and t1 = 0.12-0.15 mm; and / or The crease line between the small side surface and the first large surface is the third crease line, and the crease line between the small side surface and the second large surface is the fourth crease line. The distance between the end of the third crease line and the end of the fourth crease line and the edge of the first large surface extending along the first preset direction along the second preset direction is A, and A = 1-2 mm. and / or The thickness of the electrode assembly before coating is T', and the width of both the first and second side assembly facets along the first preset direction is W1, where W1 = T' - (3 - 5 mm); and / or The thickness of the electrode assembly before coating is T', and the width of the first bottom assembly surface and the second bottom assembly surface along the second preset direction is L1, and L1=T'-(3-5mm).

9. The battery cell according to claim 7, characterized in that, The first large surface and the second large surface, the first side combined small surface and the second side combined small surface, the first bottom combined surface and the second bottom combined surface, and the side small surface itself are all symmetrically arranged about the center line of the side small surface along the second preset direction; The crease line between the side facet and the second large facet is the fourth crease line, and the distance between the side edge of the first bottom composite facet that is close to and parallel to the fourth crease line and the fourth crease line along the first preset direction is B1, and B1 = 4-5mm. The crease line between the second side panel and the second large panel is the fifth crease line, and the distance between the side of the first bottom panel that is close to and parallel to the fifth crease line and the fifth crease line along the first preset direction is B2, where B2 = 4-5 mm.

10. The battery cell according to any one of claims 1 to 9, characterized in that, Multiple hot-melt zones are formed between any of the side plates and the insulating film, and the multiple hot-melt zones are arranged sequentially at intervals along the length direction of the side plate; The area of ​​the large side of a single side plate is S0, the area of ​​a single hot-melt zone is S1, the number of hot-melt zones on any side plate is k, and 0.25≤10kS1 / S0≤0.4; and / or The thickness of the side plate is t2, and t2 = 0.5-0.8 m; and / or The side plate has a first positioning hole, and the insulating film has a second positioning hole corresponding to the first positioning hole; and / or The bottom of the coated electrode assembly abuts against the second cover plate; and / or The second cover plate is either an integral part of the housing or a separate structure connected by welding; and / or The insulating film is an integral structure; and / or The insulating film covering the two small sides of the electrode assembly has multiple first through holes, and the multiple first through holes are arranged sequentially and spaced apart along the length direction of the electrode assembly or simultaneously arranged sequentially and spaced apart along the length direction and the thickness direction of the electrode assembly; the side plate has multiple second through holes, and the multiple second through holes are arranged sequentially and spaced apart along the length direction of the side plate or simultaneously arranged sequentially and spaced apart along the length direction and the width direction of the side plate, and the second through holes are staggered with the first through holes; The insulating film covering the bottom of the electrode assembly has multiple third through holes, and these third through holes are sequentially spaced along the width direction of the electrode assembly; and / or When the insulating film is in its unfolded state, any two of the first preset direction, the second preset direction, and the thickness direction of the insulating film are perpendicular to each other, and when the insulating film covers the electrode assembly, the second preset direction is the same as the length direction of the electrode assembly; and / or The battery cell further includes a positive terminal, a negative terminal, and an explosion-proof valve, wherein the positive terminal and the negative terminal are mounted on the first cover plate, and the explosion-proof valve is mounted on the second cover plate; and / or The electrode assembly includes at least one electrode group, and when there are multiple electrode groups, the multiple electrode groups are stacked together along the thickness direction of the electrode group.