Back-contact solar cells and their fabrication methods, cell modules and photovoltaic systems
By using a tunneling oxide layer, an in-situ boron-doped amorphous silicon layer, and a barrier silicon oxide layer in the fabrication of back-contact solar cells, combined with laser annealing and phosphorus diffusion, the process steps are simplified, solving the problems of complex processes and high costs in existing technologies, and achieving more efficient production.
Patent Information
- Application Number
- CN202611170067.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-03
- Publication Date
- 2026-11-17
AI Technical Summary
Existing methods for fabricating back-contact solar cells are complex and costly, mainly due to the need for high-precision mask fabrication and patterning processes.
The process involves sequentially forming a tunneling oxide layer, an in-situ boron-doped amorphous silicon layer, and a barrier silicon oxide layer on the back side of a silicon substrate. P-type and N-type polycrystalline silicon layers are then formed through laser annealing and phosphorus diffusion. Combined with laser grooving, trenches are formed, simplifying the process steps and avoiding localized removal of the mask.
It reduces the difficulty of production processes and the requirements for processing precision, simplifies the process flow, reduces costs, and improves production efficiency.
Smart Images

Figure CN123124484A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of solar cell technology, and in particular to a back-contact solar cell, its preparation method, cell module, and photovoltaic system. Background Technology
[0002] In related technologies, back-contact solar cells typically involve depositing a P-type doped layer across the entire back surface of a silicon substrate, followed by forming a mask layer on the same back surface. Using patterning processes such as photolithography, the mask layer for the desired P-type regions is retained, exposing the patterned mask layer for the N-type regions. The P-type doped layer in the exposed areas is then removed, and residual mask and byproducts are cleaned away. An N-type doped layer is then deposited in the N-type regions. Finally, the mask layer and N-type doped layer in the P-type regions are removed, resulting in alternating P-type and N-type doped layers on the back surface of the silicon substrate. Because the mask layer needs to be etched according to a pattern to form a patterned mask, high precision is required in mask fabrication, leading to a complex manufacturing process and high costs. Summary of the Invention
[0003] This invention provides a method for preparing a back-contact solar cell, aiming to solve the problems of complex manufacturing processes and high costs associated with existing back-contact solar cell preparation methods.
[0004] This invention is achieved by providing a method for fabricating a back-contact solar cell, comprising the following steps: A silicon substrate is provided, the back side of which includes a first region and a second region; A tunneling oxide layer, an in-situ boron-doped first amorphous silicon layer, a barrier silicon oxide layer, and a second amorphous silicon layer are sequentially formed on the back side of the silicon substrate. The first region is subjected to laser annealing to crystallize the second amorphous silicon layer in the first region into a first barrier polycrystalline silicon layer, while activating the boron dopant in the first amorphous silicon layer in the first region to form a P-type polycrystalline silicon layer. Phosphorus diffusion is performed on the back side of the silicon substrate to dope the first amorphous silicon layer in the second region with phosphorus to form an N-type polycrystalline silicon layer, and the first barrier polycrystalline silicon layer and the barrier silicon oxide layer in the first region, and the second amorphous silicon layer and the barrier silicon oxide layer in the second region are transformed into phosphosilicate glass. Laser grooving is performed between the first region and the second region to form a trench between the P-type polysilicon layer and the N-type polysilicon layer; Remove the phosphosilicate glass from the first region and the second region.
[0005] Preferably, after the laser grooving step between the first region and the second region, and before the step of removing the phosphosilicate glass from the first region and the second region, the method further includes: A textured surface is formed on the front side of the silicon substrate and on the surface of the trench.
[0006] Preferably, the thickness of the barrier silicon oxide layer is 1~2 nm.
[0007] Preferably, the thickness of the second amorphous silicon layer is 20~50nm.
[0008] Preferably, the thickness of the barrier silicon oxide layer is greater than the thickness of the tunneling oxide layer.
[0009] Preferably, the laser energy density of the laser annealing treatment is 350~600mJ / cm².
[0010] The present invention also provides a method for fabricating a back-contact solar cell, comprising the following steps: A silicon substrate is provided, the back side of which includes a first region, a second region, and an isolation region disposed between the first region and the second region; A tunneling oxide layer, an in-situ boron-doped first amorphous silicon layer, a barrier silicon oxide layer, and a second amorphous silicon layer are sequentially formed on the back side of the silicon substrate. The first region is subjected to laser annealing to crystallize the second amorphous silicon layer in the first region into a first barrier polycrystalline silicon layer, while activating the boron dopant in the first amorphous silicon layer in the first region to form a P-type polycrystalline silicon layer. The isolation region is subjected to laser crystallization treatment, so that the second amorphous silicon layer of the isolation region is crystallized into a second barrier polycrystalline silicon layer, and the boron dopant in the first amorphous silicon layer of the isolation region is not activated. Phosphorus diffusion is performed on the back side of the silicon substrate, the first amorphous silicon layer in the second region is doped with phosphorus to form an N-type polycrystalline silicon layer, and the first barrier polycrystalline silicon layer and the barrier silicon oxide layer in the first region, the second barrier polycrystalline silicon layer and the barrier silicon oxide layer in the isolation region, the second amorphous silicon layer and the barrier silicon oxide layer in the second region are transformed into phosphosilicate glass, and the first amorphous silicon layer in the isolation region is transformed into an isolation polycrystalline silicon layer. Remove the phosphosilicate glass from the first region, the second region, and the isolation zone.
[0011] Preferably, the laser energy density of the laser crystallization process is less than the activation threshold of the boron dopant in the first amorphous silicon layer, and the laser energy density of the laser crystallization process is greater than the crystallization threshold of the second amorphous silicon layer.
[0012] Preferably, the laser energy density of the laser annealing treatment is higher than that of the laser crystallization treatment.
[0013] Preferably, the laser energy density of the laser annealing treatment is 350~600mJ / cm²; the laser energy density of the laser crystallization treatment is 150~300mJ / cm².
[0014] The present invention also provides a back-contact solar cell, which is prepared by the above-described method for preparing a back-contact solar cell.
[0015] The present invention also provides a battery assembly including the aforementioned back-contact solar cell.
[0016] The present invention also provides a photovoltaic system including the above-described battery module.
[0017] The present invention provides a method for fabricating a back-contact solar cell by sequentially forming a tunneling oxide layer, an in-situ boron-doped first amorphous silicon layer, a barrier silicon oxide layer, and a second amorphous silicon layer on the back side of a silicon substrate. Then, a first region is subjected to laser annealing, causing the second amorphous silicon layer in the first region to crystallize into a first barrier polycrystalline silicon layer. Simultaneously, the boron dopant in the first amorphous silicon layer in the first region is activated, causing the first amorphous silicon layer in the first region to form a P-type polycrystalline silicon layer. Phosphorus diffusion is then performed to dope the first amorphous silicon layer in the second region with phosphorus to form an N-type polycrystalline silicon layer. The first barrier polycrystalline silicon layer and barrier silicon oxide layer in the first region, and the second amorphous silicon layer and barrier silicon oxide layer in the second region, are transformed into phosphosilicate glass. Finally, laser grooving is performed between the first and second regions, and the phosphosilicate glass is removed. The back-contact solar cell fabrication method of the present invention does not require the stepwise deposition of P-type polycrystalline silicon layers and N-type polycrystalline silicon layers. Instead, it can deposit an in-situ boron-doped first amorphous silicon layer over the entire surface, then form a P-type polycrystalline silicon layer through local laser activation, and form an N-type polycrystalline silicon layer through local phosphorus diffusion. Finally, the entire surface of the phosphorus-silicon glass is removed. This eliminates the need for local mask removal to form a patterned mask, which reduces the difficulty of the process, lowers the requirements for processing precision, simplifies the production process, reduces process costs, and is more conducive to the production of back-contact solar cells.
[0018] Alternatively, the method for fabricating a back-contact solar cell provided by the present invention involves sequentially forming a tunneling oxide layer, an in-situ boron-doped first amorphous silicon layer, a barrier silicon oxide layer, and a second amorphous silicon layer on the back side of a silicon substrate. Then, a first region is subjected to laser annealing, causing the second amorphous silicon layer in the first region to crystallize into a first barrier polycrystalline silicon layer. Simultaneously, boron in the first amorphous silicon layer in the first region is activated, causing the first amorphous silicon layer in the first region to form a P-type polycrystalline silicon layer. Next, a laser crystallization process is performed on the isolation region, causing the second amorphous silicon layer in the isolation region to crystallize into a second barrier polycrystalline silicon layer, without activating the boron dopant in the first amorphous silicon layer in the isolation region. Then, phosphorus diffusion is performed on the back side of the silicon substrate, causing phosphorus doping in the first amorphous silicon layer in the second region to form an N-type polycrystalline silicon layer. The first barrier polycrystalline silicon layer and barrier silicon oxide layer in the first region, the second barrier polycrystalline silicon layer and barrier silicon oxide layer in the isolation region, and the second amorphous silicon layer and barrier silicon oxide layer in the second region are transformed into phosphosilicate glass. Finally, the phosphosilicate glass is removed. Another method for fabricating a back-contact solar cell according to the present invention also does not require the stepwise deposition of P-type polycrystalline silicon layers and N-type polycrystalline silicon layers. Instead, an in-situ boron-doped first amorphous silicon layer can be deposited across the entire surface, followed by local laser activation to form a P-type polycrystalline silicon layer, and local phosphorus diffusion to form an N-type polycrystalline silicon layer. This method reduces the complexity of the process and eliminates the need for local mask removal to form a patterned mask, thus reducing the requirements for processing precision. The manufacturing process is relatively simple, which helps to reduce process costs and is more conducive to the production of back-contact solar cells. Attached Figure Description
[0019] Figure 1 This is a process flow diagram of a method for fabricating a back-contact solar cell according to Embodiment 1 of the present invention; Figure 2 The diagram shows the structural changes corresponding to the fabrication method of a back-contact solar cell provided in Embodiment 1 of the present invention. Figure 3 This is a process flow diagram of a method for fabricating a back-contact solar cell according to Embodiment 2 of the present invention; Figure 4 This diagram illustrates the structural changes corresponding to a method for fabricating a back-contact solar cell according to Embodiment 2 of the present invention. Detailed Implementation
[0020] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. Examples of embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the invention, and should not be construed as limiting the invention. Furthermore, it should be understood that the specific embodiments described herein are merely illustrative of the invention and are not intended to limit the invention.
[0021] In the description of this invention, it should be understood that the terms "upper", "lower", "back", "front", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention.
[0022] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0023] The following disclosure provides numerous different embodiments or examples for implementing various structures of the invention. To simplify the disclosure, specific examples of components and arrangements are described below. These are merely examples and are not intended to limit the invention. Furthermore, reference numerals and / or letters may be repeated in different examples; such repetition is for simplification and clarity and does not in itself indicate a relationship between the various embodiments and / or arrangements discussed. In addition, examples of various specific processes and materials are provided in this invention, but those skilled in the art will recognize the application of other processes and / or the use of other materials.
[0024] Example 1 Please refer to Figure 1 and Figure 2 This invention provides a method for fabricating a back-contact solar cell, comprising the following steps: S11, a silicon substrate 1 is provided, the back side 11 of the silicon substrate 1 includes a first region 111 and a second region 112; In this step, the silicon substrate 1 includes a back side 11 and a front side 12 disposed opposite to each other. The front side 12 of the silicon substrate 1 is the side of the silicon substrate 1 that faces sunlight when the back contact solar cell is working normally. That is, the front side 12 of the silicon substrate 1 is the side that mainly receives sunlight when the back contact solar cell is working normally. Of course, the back side 11 of the silicon substrate 1 can also receive some sunlight when the back contact solar cell is working normally.
[0025] In this step, an N-type silicon wafer can be selected as the silicon substrate 1, and it can be thoroughly cleaned to remove surface contaminants. Specifically, the back side 11 of the silicon wafer can be polished to make its surface flatter, which is beneficial for subsequent film deposition.
[0026] S12, a tunneling oxide layer 2, an in-situ boron-doped first amorphous silicon layer 3, a barrier silicon oxide layer 4, and a second amorphous silicon layer 5 are sequentially formed on the back side 11 of the silicon substrate 1. In this step, PECVD (plasma-enhanced chemical vapor deposition) or LPCVD (low-pressure chemical vapor deposition) can be used to sequentially form a tunneling oxide layer 2, an in-situ boron-doped first amorphous silicon layer 3, a barrier silicon oxide layer 4, and a second amorphous silicon layer 5 on the entire back side 11 of the silicon substrate 1. That is, both the first region 111 and the second region 112 of the silicon substrate 1 form a stacked structure of the tunneling oxide layer 2, the in-situ boron-doped first amorphous silicon layer 3, the barrier silicon oxide layer 4, and the second amorphous silicon layer 5. Of course, the tunneling oxide layer 2, the in-situ boron-doped first amorphous silicon layer 3, the barrier silicon oxide layer 4, and the second amorphous silicon layer 5 can also be formed by other methods.
[0027] In this step, the tunneling oxide layer 2 can specifically be one or a stack of at least two of the following: silicon oxide layer, aluminum oxide layer, silicon nitride layer, and silicon oxynitride layer. The thickness of the tunneling oxide layer 2 is 0.5~1.5 nanometers, allowing majority carriers to tunnel through while blocking minority carrier recombination, thereby significantly reducing interfacial recombination losses.
[0028] In this step, the first amorphous silicon layer 3 with boron doping in situ is specifically a first amorphous silicon layer 3 containing boron dopant, and the boron dopant in the first amorphous silicon layer 3 is in an inactive state.
[0029] In one embodiment of the present invention, the thickness of the blocking silicon oxide layer 4 is greater than the thickness of the tunneling oxide layer 2.
[0030] In this embodiment, the thickness of the barrier silicon oxide layer 4 is greater than the thickness of the tunneling oxide layer 2. Thus, the barrier silicon oxide layer 4, together with the first barrier polycrystalline silicon layer 6, is more conducive to reducing the diffusion of phosphorus atoms into the P-type polycrystalline silicon layer 7 in the subsequent phosphorus diffusion process, thereby reducing the phosphorus atom content in the P-type polycrystalline silicon layer 7.
[0031] In some embodiments, the ratio of the thickness of the barrier silicon oxide layer 4 to the thickness of the tunneling oxide layer 2 can be 1.2 to 3. In this way, the barrier silicon oxide layer 4 can be paired with the first barrier polycrystalline silicon layer 6 to provide good barrier effect against phosphorus atoms in the subsequent phosphorus diffusion process, preventing phosphorus from diffusing to the P-type polycrystalline silicon layer 7, and facilitating the processing and preparation of the barrier silicon oxide layer 4.
[0032] In one embodiment of the present invention, the thickness of the barrier silicon oxide layer 4 is 1~2 nm. Controlling the thickness of the barrier silicon oxide layer 4 to 1~2 nm facilitates the preparation of the silicon oxide layer and allows the barrier silicon oxide layer 4 to be paired with the first barrier polycrystalline silicon layer 6. In the phosphorus diffusion process, it has a good barrier effect on phosphorus atoms, preventing phosphorus from diffusing to the P-type polycrystalline silicon layer 7. In the phosphorus diffusion process, phosphorus atoms can diffuse through the barrier silicon oxide layer 4 into the first amorphous silicon layer 3 of the second region 112, so that the first amorphous silicon layer 3 of the second region 112 is transformed into the N-type polycrystalline silicon layer 8.
[0033] As an embodiment of the present invention, the thickness of the second amorphous silicon layer 5 is 20~50nm.
[0034] In this embodiment, the thickness of the second amorphous silicon layer 5 is controlled to be 20~50nm. This avoids the second amorphous silicon layer 5 being too thin, which would result in the first barrier polycrystalline silicon layer 6 being too thin. This ensures that the first barrier polycrystalline silicon layer 6 has a good blocking effect on phosphorus atoms during phosphorus diffusion, and also avoids the first barrier polycrystalline silicon layer 6 being too thick, which would prevent it from being completely converted into phosphorus silicon glass 9. At the same time, it prevents the barrier silicon oxide layer 4 from being unable to be completely converted into phosphorus silicon glass 9 during the phosphorus diffusion process, thus avoiding residual barrier silicon oxide layer 4 that would affect battery performance.
[0035] In some embodiments, the thickness of the second amorphous silicon layer 5 is greater than the thickness of the first amorphous silicon layer 3, which is more conducive to increasing the thickness of the first barrier polycrystalline silicon layer 6 formed by the second amorphous silicon layer 5, ensuring that the first barrier polycrystalline silicon layer 6 has a good blocking effect on phosphorus atoms during phosphorus diffusion. For example, the ratio of the thickness of the second amorphous silicon layer 5 to the thickness of the first amorphous silicon layer 3 can be 1.1 to 2.
[0036] S13, laser annealing is performed on the first region 111 to crystallize the second amorphous silicon layer 5 of the first region 111 into the first barrier polycrystalline silicon layer 6, and at the same time, the boron dopant in the first amorphous silicon layer 3 of the first region 111 is activated to transform the first amorphous silicon layer 3 of the first region 111 into the P-type polycrystalline silicon layer 7. In this step, an excimer laser can be used for laser annealing. When the laser emits a high-energy laser pulse that irradiates the first region 111, the second amorphous silicon layer 5 and the first amorphous silicon layer 3 of the first region 111 absorb the laser energy, causing the second amorphous silicon layer 5 of the first region 111 to change from an amorphous state to a polycrystalline state, thereby transforming the second amorphous silicon layer 5 of the first region 111 into a first barrier polycrystalline silicon layer 6; at the same time, the boron atoms in the first amorphous silicon layer 3 of the first region 111 are activated with sufficient energy, the boron dopant in the first amorphous silicon layer 3 is activated, the activated boron atoms occupy lattice positions, and the first amorphous silicon layer 3 of the first region 111 also changes from an amorphous state to a polycrystalline state, thereby transforming the first amorphous silicon layer 3 of the first region 111 into a boron-doped P-type polycrystalline silicon layer 7.
[0037] In this step, a laser is used to crystallize the second amorphous silicon layer 5 of the first region 111 into a first barrier polycrystalline silicon layer 6, and the first amorphous silicon layer 3 of the first region 111 is transformed into a P-type polycrystalline silicon layer 7. The first barrier polycrystalline silicon layer 6 can act as a barrier, preventing phosphorus from diffusing into the P-type polycrystalline silicon layer 7 in the subsequent phosphorus diffusion process, so that the first amorphous silicon layer 3 of the first region 111 can be reliably transformed into a P-type polycrystalline silicon layer 7. Since the first barrier polycrystalline silicon layer 6 is not formed above the first amorphous silicon layer 3 of the second region 112, phosphorus atoms can diffuse into the first amorphous silicon layer 3 of the second region 112 in the subsequent phosphorus diffusion process, so that the first amorphous silicon layer 3 of the second region 112 is transformed into an N-type polycrystalline silicon layer 8, thereby forming a P-type polycrystalline silicon layer 7 and an N-type polycrystalline silicon layer 8 on the back side 11 of the silicon substrate 1. Therefore, in this embodiment of the invention, an amorphous silicon layer is deposited on the back side 11 of the silicon substrate 1. A P-type polycrystalline silicon layer 7 can be formed by local laser, and an N-type polycrystalline silicon layer 8 can be formed by local phosphorus diffusion, which simplifies the fabrication process of the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8.
[0038] As an embodiment of the present invention, the laser energy density of the laser annealing process is 350~600mJ / cm². By controlling the laser energy density of the laser annealing process within this range, the second amorphous silicon layer 5 of the first region 111 can be well transformed into the first barrier polycrystalline silicon layer 6, and the first amorphous silicon layer 3 of the first region 111 can be well transformed into the boron-doped P-type polycrystalline silicon layer 7.
[0039] S14, phosphorus diffusion is performed on the back side 11 of the silicon substrate 1, so that the first amorphous silicon layer 3 of the second region 112 is doped with phosphorus to form an N-type polycrystalline silicon layer 8, and the first barrier polycrystalline silicon layer 6 and barrier silicon oxide layer 4 of the first region 111, and the second amorphous silicon layer 5 and barrier silicon oxide layer 4 of the second region 112 are transformed into phosphorosilicate glass 9. In this step, the laser-annealed silicon substrate 1 can be placed in a diffusion furnace for phosphorus diffusion. Specifically, the laser-annealed silicon substrate 1 can be placed in a high-temperature (800℃~900℃) diffusion furnace, and phosphorus oxychloride (POCl3) and oxygen are introduced. Phosphorus atoms migrate into the interior of the silicon substrate 1, so that the first barrier polycrystalline silicon layer 6 and barrier silicon oxide layer 4 in the first region 111, and the second amorphous silicon layer 5 and barrier silicon oxide layer 4 in the second region 112 are completely converted into phosphosilicate glass 9 (PSG). At the same time, phosphorus atoms diffuse into the first amorphous silicon layer 3 in the second region 112, so that the first amorphous silicon layer 3 in the second region 112 is doped with phosphorus and crystallized into an N-type polycrystalline silicon layer 8. Since the first region 111 has a first barrier polysilicon layer 6, the first barrier polysilicon layer 6 can prevent phosphorus from diffusing into the P-type polysilicon layer 7. Since the second region 112 does not have a first barrier polysilicon layer 6, phosphorus atoms can diffuse into the first amorphous silicon layer 3 of the second region 112, causing the first amorphous silicon layer 3 to be doped with phosphorus to form an N-type polysilicon layer 8.
[0040] S15, laser grooving is performed between the first region 111 and the second region 112 to form a trench 10 between the P-type polysilicon layer 7 and the N-type polysilicon layer 8; In this step, after forming the P-type polysilicon layer 7 and the N-type polysilicon layer 8, a trench 10 is formed between the P-type polysilicon layer 7 and the N-type polysilicon layer 8 by laser, thereby forming an isolation region 113 between the first region 111 and the second region 112. The trench 10 is formed at the location of the isolation region 113, so that the P-type polysilicon layer 7 and the N-type polysilicon layer 8 are physically isolated by the trench 10, preventing short circuits between the P-type polysilicon layer 7 and the N-type polysilicon layer 8.
[0041] S17, remove the phosphorus glass 9 from the first region 111 and the second region 112.
[0042] In this step, acid washing can be used to remove the phosphosilicate glass 9. Specifically, the silicon substrate 1 on which the phosphosilicate glass 9 was formed in the previous steps can be immersed in a hydrofluoric acid (HF) solution. The HF reacts with the phosphosilicate glass 9, dissolving and removing it. Then, it is rinsed with deionized water to remove residual acid and reaction byproducts. Finally, it is dried using compressed air or nitrogen.
[0043] As an embodiment of the present invention, after the laser grooving step between the first region 111 and the second region 112, and before the step of removing the phosphosilicate glass 9 from the first region 111 and the second region 112, the method further includes: S16, a textured surface 16 is formed on the surface of the front side 12 and the trench 10 of the silicon substrate 1.
[0044] Specifically, a wet chemical etching process is used to texturize the surface of the front side 12 and trench 10 of the silicon substrate 1 using an alkaline solution (such as a dilute solution of sodium hydroxide or potassium hydroxide). This creates a pyramid-shaped textured surface 16 on the surface of the front side 12 and trench 10 of the silicon substrate 1, reducing the reflection of sunlight from the surface of the front side 12 and trench 10 of the silicon substrate 1 and improving the solar energy utilization efficiency of the battery. Simultaneously, during the texturing process, the phosphosilicate glass 9 protects the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8, preventing them from being damaged.
[0045] As an embodiment of the present invention, after the step of removing the phosphosilicate glass 9 from the first region 111 and the second region 112, the method further includes: Metal electrodes are formed on the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8, respectively.
[0046] Specifically, metal electrodes can be formed on the P-type polysilicon layer 7 and the N-type polysilicon layer 8 by screen printing or electroplating. Furthermore, prior to the metal electrode formation step, passivation films can be formed on the P-type polysilicon layer 7 and the N-type polysilicon layer 8, with the metal electrodes contacting the P-type polysilicon layer 7 or the N-type polysilicon layer 8 through the passivation films. The passivation films can be one or a stack of at least two of the following: silicon nitride, silicon oxynitride, and aluminum oxide.
[0047] Specifically, when forming the metal electrode, a burn-through paste can be printed on the passivation film layer, allowing the paste to burn through the passivation film layer and contact the P-type polycrystalline silicon layer 7 or the N-type polycrystalline silicon layer 8, and then sintered to form the metal electrode. Alternatively, an opening can be made in the passivation film layer, and a non-burn-through paste can be printed at the opening location, followed by sintering to form the metal electrode; or, an opening can be made in the passivation film layer, and the metal electrode can be electroplated at the opening location.
[0048] The present invention provides a method for fabricating a back-contact solar cell by sequentially forming a tunneling oxide layer 2, an in-situ boron-doped first amorphous silicon layer 3, a barrier silicon oxide layer 4, and a second amorphous silicon layer 5 on the back side 11 of a silicon substrate 1. Then, a laser annealing process is performed on a first region 111 to crystallize the second amorphous silicon layer 5 into a first barrier polycrystalline silicon layer 6. Simultaneously, boron in the first amorphous silicon layer 3 of the first region 111 is activated, causing the first amorphous silicon layer 3 of the first region 111 to form a P-type polycrystalline silicon layer 7. Phosphorus diffusion is then performed to dope the first amorphous silicon layer 3 of the second region 112 with phosphorus to form an N-type polycrystalline silicon layer 8. The first barrier polycrystalline silicon layer 6 and the barrier silicon oxide layer 4 of the first region 111, and the second amorphous silicon layer 5 and the barrier silicon oxide layer 4 of the second region 112 are transformed into phosphosilicate glass 9. Finally, laser grooving is performed between the first region 111 and the second region 112, and the phosphosilicate glass 9 is removed. The back-contact solar cell fabrication method of this invention does not require the stepwise deposition of P-type polycrystalline silicon layer 7 and N-type polycrystalline silicon layer 8. Instead, it can deposit an in-situ boron-doped first amorphous silicon layer 3 over the entire surface, then form the P-type polycrystalline silicon layer 7 through local laser activation, and form the N-type polycrystalline silicon layer 8 through local phosphorus diffusion. This reduces the difficulty of the process and eliminates the need for local mask removal to form a patterned mask, thus reducing the requirements for processing precision. The production process is relatively simple, which can reduce the process cost and is more conducive to the production of back-contact solar cells.
[0049] Example 2 Please refer to Figure 3 and Figure 4 This invention provides a method for fabricating a back-contact solar cell, comprising the following steps: Step 21, a silicon substrate 1 is provided. The back side 11 of the silicon substrate 1 includes a first region 111, a second region 112, and an isolation region 113 disposed between the first region 111 and the second region 112. In this step, the silicon substrate 1 includes a back side 11 and a front side 12 disposed opposite to each other. The front side 12 of the silicon substrate 1 is the side of the silicon substrate 1 that faces sunlight when the back contact solar cell is working normally. That is, the front side 12 of the silicon substrate 1 is the side that mainly receives sunlight when the back contact solar cell is working normally. Of course, the back side 11 of the silicon substrate 1 can also receive some sunlight when the back contact solar cell is working normally.
[0050] In this step, an N-type silicon wafer can be selected as the silicon substrate 1, and it can be thoroughly cleaned to remove surface contaminants. Specifically, the back side 11 of the silicon wafer can be polished to make its surface flatter, which is beneficial for subsequent film deposition.
[0051] Step 22: A tunneling oxide layer 2, an in-situ boron-doped first amorphous silicon layer 3, a barrier silicon oxide layer 4, and a second amorphous silicon layer 5 are sequentially formed on the back side 11 of the silicon substrate 1. In this step, PECVD (plasma-enhanced chemical vapor deposition) or LPCVD (low-pressure chemical vapor deposition) can be used to sequentially form a tunneling oxide layer 2, an in-situ boron-doped first amorphous silicon layer 3, a barrier silicon oxide layer 4, and a second amorphous silicon layer 5 on the entire back side 11 of the silicon substrate 1. That is, the first region 111, the second region 112, and the isolation region 113 of the silicon substrate 1 all form a stacked structure of tunneling oxide layer 2, in-situ boron-doped first amorphous silicon layer 3, barrier silicon oxide layer 4, and second amorphous silicon layer 5. Of course, the tunneling oxide layer 2, the in-situ boron-doped first amorphous silicon layer 3, the barrier silicon oxide layer 4, and the second amorphous silicon layer 5 can also be formed by other methods.
[0052] The tunneling oxide layer 2 can be a stack of one or more of the following: silicon oxide layer, aluminum oxide layer, silicon nitride layer, and silicon oxynitride layer. The thickness of the tunneling oxide layer 2 is 0.5~1.5 nanometers, allowing majority carriers to tunnel through while blocking minority carrier recombination, thus significantly reducing interfacial recombination losses.
[0053] In this step, the first amorphous silicon layer 3 with boron doping in situ is specifically a first amorphous silicon layer 3 containing boron dopant, and the boron dopant in the first amorphous silicon layer 3 is in an inactive state.
[0054] In one embodiment of the present invention, the thickness of the blocking silicon oxide layer 4 is greater than the thickness of the tunneling oxide layer 2.
[0055] In this embodiment, the thickness of the barrier silicon oxide layer 4 is greater than the thickness of the tunneling oxide layer 2. This increases the thickness of the barrier silicon oxide layer 4, which is more conducive to preventing phosphorus atoms from diffusing into the P-type polycrystalline silicon layer 7 during the subsequent phosphorus diffusion process, thereby reducing the phosphorus atom content in the P-type polycrystalline silicon layer 7.
[0056] In some embodiments, the ratio of the thickness of the barrier silicon oxide layer 4 to the thickness of the tunneling oxide layer 2 can be 1.2 to 3. This is more conducive to preventing phosphorus atoms from diffusing into the P-type polycrystalline silicon layer 7 during subsequent phosphorus diffusion processes, and also facilitates the processing and fabrication of the barrier silicon oxide layer 4.
[0057] In one embodiment of the present invention, the thickness of the barrier silicon oxide layer 4 is 1~2 nm. Controlling the thickness of the barrier silicon oxide layer 4 to 1~2 nm facilitates the preparation of the silicon oxide layer and allows the barrier silicon oxide layer 4 to have a good barrier effect on phosphorus atoms in the phosphorus diffusion process, preventing phosphorus from diffusing to the P-type polycrystalline silicon layer 7.
[0058] As an embodiment of the present invention, the thickness of the second amorphous silicon layer 5 is 20~50nm.
[0059] In this embodiment, the thickness of the second amorphous silicon layer 5 is controlled to be 20~50nm. This avoids the second amorphous silicon layer 5 being too thin, which would result in the first barrier polycrystalline silicon layer 6 being too thin. This ensures that the first barrier polycrystalline silicon layer 6 has a good barrier effect on phosphorus during phosphorus diffusion, and also avoids the first barrier polycrystalline silicon layer 6 being too thick, which would prevent it from being completely converted into phosphorus silicon glass 9. At the same time, it prevents the barrier silicon oxide layer 4 from being unable to be completely converted into phosphorus silicon glass 9 during the phosphorus diffusion process, thus avoiding the barrier silicon oxide layer 4 residue from affecting battery performance.
[0060] In some embodiments, the thickness of the second amorphous silicon layer 5 is greater than the thickness of the first amorphous silicon layer 3, which is more conducive to increasing the thickness of the first barrier polycrystalline silicon layer 6 formed by the second amorphous silicon layer 5, ensuring that the first barrier polycrystalline silicon layer 6 has a good blocking effect on phosphorus during phosphorus diffusion. For example, the ratio of the thickness of the second amorphous silicon layer 5 to the thickness of the first amorphous silicon layer 3 can be 1.1 to 2.
[0061] Step 23: Perform laser annealing on the first region 111 to crystallize the second amorphous silicon layer 5 of the first region 111 into the first barrier polycrystalline silicon layer 6, and at the same time activate the boron dopant in the first amorphous silicon layer 3 of the first region 111 to transform the first amorphous silicon layer 3 of the first region 111 into the P-type polycrystalline silicon layer 7. In this step, lasers are used to simultaneously crystallize the second amorphous silicon layer 5 of the first region 111 into a first barrier polycrystalline silicon layer 6 and convert the first amorphous silicon layer 3 of the first region 111 into a P-type polycrystalline silicon layer 7. On the one hand, a P-type polycrystalline silicon layer 7 is formed in the first region 111, and the first barrier polycrystalline silicon layer 6 is formed at the same time. The first barrier polycrystalline silicon layer 6 can act as a mask, which can prevent phosphorus from diffusing into the P-type polycrystalline silicon layer 7 in the subsequent phosphorus diffusion process, so that the first amorphous silicon layer 3 of the first region 111 can be reliably converted into a P-type polycrystalline silicon layer 7. Since no polycrystalline silicon layer is formed above the first amorphous silicon layer 3 of the second region 112 to block phosphorus atoms, phosphorus atoms can diffuse into the first amorphous silicon layer 3 of the second region 112 in the subsequent phosphorus diffusion process, so that the first amorphous silicon layer 3 of the second region 112 is converted into an N-type polycrystalline silicon layer 8, thereby forming a P-type polycrystalline silicon layer 7 and an N-type polycrystalline silicon layer 8.
[0062] In one embodiment of the present invention, the laser energy density of the laser annealing process is 350~600 mJ / cm². By controlling the laser energy density within this range, the second amorphous silicon layer 5 in the first region 111 can be well transformed into the first barrier polycrystalline silicon layer 6, and the first amorphous silicon layer 3 in the first region 111 can be well transformed into the boron-doped P-type polycrystalline silicon layer 7.
[0063] Step 24: Laser crystallization treatment is performed on the isolation region 113 to crystallize the second amorphous silicon layer 5 of the isolation region 113 into the second barrier polycrystalline silicon layer 17, and the boron dopant in the first amorphous silicon layer 3 of the isolation region 113 is not activated. In this step, the isolation region 113 is subjected to laser crystallization treatment using a laser, so that the second amorphous silicon layer 5 of the isolation region 113 is crystallized into the second barrier polycrystalline silicon layer 17. During this process, the laser does not activate the boron dopant in the first amorphous silicon layer 3 of the isolation region 113, so that the first amorphous silicon layer 3 of the isolation region 113 has a good isolation effect on the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8 in the subsequently formed isolation polycrystalline silicon layer 18.
[0064] In one embodiment of the present invention, the laser energy density of the laser crystallization process is less than the activation threshold of the boron dopant in the first amorphous silicon layer 3, and the laser energy density of the laser crystallization process is greater than the crystallization threshold of the second amorphous silicon layer 5. In this way, during the laser crystallization process of the isolation region 113, the second amorphous silicon layer 5 of the isolation region 113 is crystallized into the second barrier polycrystalline silicon layer 17, and the boron dopant in the first amorphous silicon layer 3 of the isolation region 113 is not activated, so as to avoid affecting the isolation effect of the isolation region 113.
[0065] As an embodiment of the present invention, the laser energy density of laser annealing is higher than that of laser crystallization.
[0066] In this embodiment, the laser energy density of the laser annealing treatment is higher than that of the laser crystallization treatment. This is beneficial because the laser annealing treatment allows the second amorphous silicon layer 5 in the first region 111 to be effectively transformed into the first barrier polycrystalline silicon layer 6, and also allows the first amorphous silicon layer 3 in the first region 111 to be effectively transformed into a boron-doped P-type polycrystalline silicon layer 7. Simultaneously, the laser crystallization treatment allows the second amorphous silicon layer 5 in the isolation region 113 to crystallize into the second barrier polycrystalline silicon layer 17, while ensuring that the boron dopant in the first amorphous silicon layer 3 of the isolation region 113 is not activated, thus avoiding affecting the isolation effect of the isolation region 113. In some embodiments, the laser energy density of the laser annealing treatment and the laser energy density of the laser crystallization treatment can be 1.3~3.
[0067] As an embodiment of the present invention, the laser energy density of the laser crystallization treatment is 150~300mJ / cm².
[0068] In this embodiment, by controlling the laser energy density of the laser crystallization process within the above-mentioned range, the second amorphous silicon layer 5 of the isolation region 113 can be crystallized into the second barrier polycrystalline silicon layer 17, and the activation of the boron dopant in the first amorphous silicon layer 3 of the isolation region 113 can be avoided. This helps to ensure the isolation effect of the isolation polycrystalline silicon layer 18 formed by the first amorphous silicon layer 3 of the isolation region 113, and can achieve good isolation between the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8.
[0069] Step 25: Phosphorus diffusion is performed on the back side 11 of the silicon substrate 1. The first amorphous silicon layer 3 of the second region 112 is doped with phosphorus to form an N-type polycrystalline silicon layer 8. The first barrier polycrystalline silicon layer 6 and barrier silicon oxide layer 4 of the first region 111, the second barrier polycrystalline silicon layer 17 and barrier silicon oxide layer 4 of the isolation region 113, and the second amorphous silicon layer 5 and barrier silicon oxide layer 4 of the second region 112 are transformed into phosphosilicate glass 9. The first amorphous silicon layer 3 of the isolation region 113 is transformed into an isolation polycrystalline silicon layer 18. In this step, the laser-crystallized silicon substrate 1 can be placed in a diffusion furnace for phosphorus diffusion. Specifically, the laser-annealed silicon substrate 1 can be placed in a high-temperature (800℃~900℃) diffusion furnace, and phosphorus oxychloride (POCl3) and oxygen are introduced. Phosphorus atoms migrate into the interior of the silicon substrate 1, causing the first barrier polycrystalline silicon layer 6 and barrier silicon oxide layer 4 in the first region 111, the second barrier polycrystalline silicon layer 17 and barrier silicon oxide layer 4 in the isolation region 113, and the second amorphous silicon layer 5 and barrier silicon oxide layer 4 in the second region 112 to be completely transformed into phosphosilicate glass 9 (PSG). At the same time, phosphorus atoms diffuse into the first amorphous silicon layer 3 in the second region 112, causing the first amorphous silicon layer 3 in the second region 112 to be doped with phosphorus and crystallized into an N-type polycrystalline silicon layer 8. Because the first region 111 has a first barrier polysilicon layer 6, which can prevent phosphorus from diffusing into the P-type polysilicon layer 7, and because the isolation region 113 has a second barrier polysilicon layer 17, which can prevent phosphorus from diffusing into the first amorphous silicon layer 3 of the isolation region 113, in the phosphorus diffusion process, the first amorphous silicon layer 3 of the isolation region 113 crystallizes only into an isolation polysilicon layer 18. The boron content of the isolation polysilicon layer 18 is much lower than that of the P-type polysilicon layer 7, and the boron content of the isolation polysilicon layer 18 is much lower than that of the phosphorus content of the N-type polysilicon layer 8. Therefore, the isolation polysilicon layer 18 can achieve good electrical isolation between the P-type polysilicon layer 7 and the N-type polysilicon layer 8.
[0070] Step 27: Remove the phosphosilicate glass 9 from the first region 111, the second region 112, and the isolation region 113.
[0071] In this step, acid washing can be used to remove the phosphosilicate glass 9. Specifically, the silicon substrate 1 on which the phosphosilicate glass 9 was formed in the previous steps can be immersed in a hydrofluoric acid (HF) solution. The HF reacts with the phosphosilicate glass 9, dissolving and removing it. Then, it is rinsed with deionized water to remove residual acid and reaction byproducts. Finally, it is dried using compressed air or nitrogen.
[0072] As an embodiment of the present invention, after the phosphorus diffusion step on the back side 11 of the silicon substrate 1 and before the step of removing the phosphorus-silicon glass 9 of the first region 111, the second region 112, and the isolation region 113, the method further includes: S26, a textured surface 16 is formed on the front side 12 of the silicon substrate 1.
[0073] Specifically, a wet chemical etching process is used to texturize the front side 12 of the silicon substrate 1 using an alkaline solution (such as a dilute solution of sodium hydroxide or potassium hydroxide), forming a pyramid-shaped textured surface 16 on the front side 12 of the silicon substrate 1. This reduces the reflection of sunlight by the front side 12 of the silicon substrate 1, improving the solar energy utilization efficiency of the battery. Simultaneously, during the texturing process, the phosphosilicate glass 9 protects the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8, preventing them from being damaged.
[0074] As an embodiment of the present invention, after the step of removing the phosphosilicate glass 9 from the first region 111, the second region 112, and the isolation region 113, the method further includes: Metal electrodes are formed on the P-type polycrystalline silicon layer 7 and the N-type polycrystalline silicon layer 8, respectively.
[0075] Specifically, metal electrodes can be formed on the P-type polysilicon layer 7 and the N-type polysilicon layer 8 by screen printing or electroplating. Furthermore, prior to the metal electrode formation step, passivation films can be formed on the P-type polysilicon layer 7 and the N-type polysilicon layer 8, with the metal electrodes contacting the P-type polysilicon layer 7 or the N-type polysilicon layer 8 through the passivation films. The passivation films can be one or a stack of at least two of the following: silicon nitride, silicon oxynitride, and aluminum oxide.
[0076] Specifically, when forming the metal electrode, a burn-through paste can be printed on the passivation film layer, allowing the paste to burn through the passivation film layer and contact the P-type polycrystalline silicon layer 7 or the N-type polycrystalline silicon layer 8, and then sintered to form the metal electrode. Alternatively, an opening can be made in the passivation film layer, and a non-burn-through paste can be printed at the opening location, followed by sintering to form the metal electrode; or, an opening can be made in the passivation film layer, and the metal electrode can be electroplated at the opening location.
[0077] The method for fabricating a back-contact solar cell provided in this embodiment of the invention involves sequentially forming a tunneling oxide layer 2, an in-situ boron-doped first amorphous silicon layer 3, a barrier silicon oxide layer 4, and a second amorphous silicon layer 5 on the back side 11 of a silicon substrate 1. Then, a laser annealing process is performed on a first region 111, causing the second amorphous silicon layer 5 in the first region 111 to crystallize into a first barrier polycrystalline silicon layer 6. Simultaneously, boron in the first amorphous silicon layer 3 in the first region 111 is activated, causing the first amorphous silicon layer 3 in the first region 111 to form a P-type polycrystalline silicon layer 7. Finally, a laser crystallization process is performed on the isolation region 113. The second amorphous silicon layer 5 of the isolation region 113 is crystallized into a second barrier polycrystalline silicon layer, and the boron dopant in the first amorphous silicon layer 3 of the isolation region 113 is not activated. Then, phosphorus diffusion is performed on the back side 11 of the silicon substrate 1. The first amorphous silicon layer 3 of the second region 112 is doped with phosphorus to form an N-type polycrystalline silicon layer 8. The first barrier polycrystalline silicon layer 6 and barrier silicon oxide layer 4 of the first region 111, the second barrier polycrystalline silicon layer and barrier silicon oxide layer 4 of the isolation region 113, and the second amorphous silicon layer 5 and barrier silicon oxide layer 4 of the second region 112 are all converted into phosphosilicate glass 9. Then, the phosphosilicate glass 9 is removed. The back-contact solar cell fabrication method of this invention does not require the stepwise deposition of P-type polycrystalline silicon layer 7 and N-type polycrystalline silicon layer 8. Instead, it can deposit an in-situ boron-doped first amorphous silicon layer 3 over the entire surface, then form the P-type polycrystalline silicon layer 7 through local laser activation, and form the N-type polycrystalline silicon layer 8 through local phosphorus diffusion. This reduces the difficulty of the process and eliminates the need for local mask removal to form a patterned mask, thus reducing the requirements for processing precision. The production process is relatively simple, which can reduce the process cost and is more conducive to the production of back-contact solar cells.
[0078] Example 3 This invention also provides a back-contact solar cell, prepared by the preparation method of the back-contact solar cell in any of the above embodiments. It should be noted that this battery module has the same or similar beneficial effects as the preparation method of the back-contact solar cell described above, and the related aspects between the two can be referred to each other. To avoid repetition, further details are omitted here.
[0079] Example 4 This invention also provides a battery assembly including the back-contact solar cell described in the above embodiments. It should be noted that this battery assembly has the same or similar beneficial effects as the back-contact solar cell, and the related aspects between the two can be referred to each other; to avoid repetition, they will not be repeated here.
[0080] In this embodiment, multiple back-contact solar cells in the battery module are connected in series by solder ribbons to form a battery string, thereby achieving series current collection and output.
[0081] It is understood that in such embodiments, the battery assembly may also include a metal frame, a backsheet, photovoltaic glass, and an encapsulating film. The encapsulating film may be filled between the back side 11 and front side 12 of the back-contact solar cell, the photovoltaic glass, adjacent cells, etc. As a filler, it may be a transparent colloid with good light transmittance and aging resistance. For example, the encapsulating film may be an EVA film or a POE film, and the specific choice can be made according to the actual situation, without limitation.
[0082] Photovoltaic glass can be applied to the encapsulant film on the front side 12 of the back-contact solar cell. The photovoltaic glass can be ultra-clear glass, which has high light transmittance, high transparency, and superior physical, mechanical, and optical properties. For example, ultra-clear glass can achieve a light transmittance of over 92%. It can protect the back-contact solar cell while minimizing impact on its efficiency. Simultaneously, the encapsulant film bonds the photovoltaic glass and the back-contact solar cell together, providing sealing, insulation, and waterproofing / moisture protection for the back-contact solar cell.
[0083] The backsheet can be attached to the adhesive film on the back side 11 of the back-contact solar cell. The backsheet provides protection and support for the back-contact solar cell, offering reliable insulation, water resistance, and aging resistance. Multiple options are available for the backsheet, typically tempered glass, acrylic glass, or aluminum alloy TPT composite adhesive film, etc. The specific choice depends on the specific circumstances and is not limited here. The backsheet, back-contact solar cell, adhesive film, and photovoltaic glass can be mounted on a metal frame. The metal frame serves as the main external support structure for the entire battery module, providing stable support and installation. For example, the battery module can be installed at the desired location using the metal frame.
[0084] Example 5 This invention also provides a photovoltaic system, which includes the battery module described in the above embodiments. It should be noted that this photovoltaic system has the same or similar beneficial effects as the back-contact solar cell described above, and the related aspects between the two can be referred to each other; to avoid repetition, they will not be repeated here.
[0085] In this embodiment, the photovoltaic system can be applied in photovoltaic power plants, such as ground-mounted power plants, rooftop power plants, and floating power plants. It can also be applied to equipment or devices that utilize solar energy to generate electricity, such as user solar power supplies, solar streetlights, solar cars, and solar buildings. Of course, it is understood that the application scenarios of the photovoltaic system are not limited to these; that is, the photovoltaic system can be applied in all fields that require solar energy to generate electricity. Taking a photovoltaic power generation system network as an example, the photovoltaic system may include a photovoltaic array, a combiner box, and an inverter. The photovoltaic array may be an array combination of multiple battery modules; for example, multiple battery modules can form multiple photovoltaic arrays. The photovoltaic array is connected to the combiner box, which can collect the current generated by the photovoltaic array. The collected current flows through the inverter and is converted into AC power required by the mains power grid before being connected to the mains power grid to achieve solar power supply.
[0086] In the description of this specification, references to terms such as "some embodiments," "illustrative embodiments," "examples," "specific examples," or "some examples," etc., indicate that a specific feature, structure, material, or characteristic described in connection with an embodiment or example is included in at least one embodiment or example of the invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.
[0087] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A method for fabricating a back-contact solar cell, characterized in that, Includes the following steps: A silicon substrate is provided, the back side of which includes a first region and a second region; A tunneling oxide layer, an in-situ boron-doped first amorphous silicon layer, a barrier silicon oxide layer, and a second amorphous silicon layer are sequentially formed on the back side of the silicon substrate. The first region is subjected to laser annealing to crystallize the second amorphous silicon layer in the first region into a first barrier polycrystalline silicon layer, while activating the boron dopant in the first amorphous silicon layer in the first region to form a P-type polycrystalline silicon layer. Phosphorus diffusion is performed on the back side of the silicon substrate to dope the first amorphous silicon layer in the second region with phosphorus to form an N-type polycrystalline silicon layer, and the first barrier polycrystalline silicon layer and the barrier silicon oxide layer in the first region, and the second amorphous silicon layer and the barrier silicon oxide layer in the second region are transformed into phosphosilicate glass. Laser grooving is performed between the first region and the second region to form a trench between the P-type polysilicon layer and the N-type polysilicon layer; Remove the phosphosilicate glass from the first region and the second region.
2. The method for preparing a back-contact solar cell according to claim 1, characterized in that, After the laser grooving step between the first region and the second region, and before the step of removing the phosphosilicate glass from the first region and the second region, the method further includes: A textured surface is formed on the front side of the silicon substrate and on the surface of the trench.
3. The method for preparing a back-contact solar cell according to claim 1, characterized in that, The thickness of the barrier silicon oxide layer is 1~2nm.
4. The method for preparing a back-contact solar cell according to claim 1, characterized in that, The thickness of the second amorphous silicon layer is 20~50nm.
5. The method for preparing a back-contact solar cell according to claim 1, characterized in that, The thickness of the barrier silicon oxide layer is greater than the thickness of the tunneling oxide layer.
6. The method for fabricating a back-contact solar cell according to claim 1, characterized in that, The laser energy density of the laser annealing process is 350~600mJ / cm².
7. A method for fabricating a back-contact solar cell, characterized in that, Includes the following steps: A silicon substrate is provided, the back side of which includes a first region, a second region, and an isolation region disposed between the first region and the second region; A tunneling oxide layer, an in-situ boron-doped first amorphous silicon layer, a barrier silicon oxide layer, and a second amorphous silicon layer are sequentially formed on the back side of the silicon substrate. The first region is subjected to laser annealing to crystallize the second amorphous silicon layer in the first region into a first barrier polycrystalline silicon layer, while activating the boron dopant in the first amorphous silicon layer in the first region to form a P-type polycrystalline silicon layer. The isolation region is subjected to laser crystallization treatment, so that the second amorphous silicon layer of the isolation region is crystallized into a second barrier polycrystalline silicon layer, and the boron dopant in the first amorphous silicon layer of the isolation region is not activated. Phosphorus diffusion is performed on the back side of the silicon substrate, the first amorphous silicon layer in the second region is doped with phosphorus to form an N-type polycrystalline silicon layer, and the first barrier polycrystalline silicon layer and the barrier silicon oxide layer in the first region, the second barrier polycrystalline silicon layer and the barrier silicon oxide layer in the isolation region, the second amorphous silicon layer and the barrier silicon oxide layer in the second region are transformed into phosphosilicate glass, and the first amorphous silicon layer in the isolation region is transformed into an isolation polycrystalline silicon layer. Remove the phosphosilicate glass from the first region, the second region, and the isolation region.
8. The method for preparing a back-contact solar cell according to claim 7, characterized in that, The laser energy density of the laser crystallization process is less than the activation threshold of the boron dopant in the first amorphous silicon layer, and the laser energy density of the laser crystallization process is greater than the crystallization threshold of the second amorphous silicon layer.
9. The method for preparing a back-contact solar cell according to claim 7, characterized in that, The laser energy density of the laser annealing treatment is higher than that of the laser crystallization treatment.
10. The method for preparing a back-contact solar cell according to claim 7, characterized in that, The laser energy density of the laser annealing treatment is 350~600mJ / cm²; the laser energy density of the laser crystallization treatment is 150~300mJ / cm².
11. A back-contact solar cell, characterized in that, It is prepared by the method for preparing a back-contact solar cell according to any one of claims 1 to 10.
12. A battery assembly, characterized in that, Including the back-contact solar cell as described in any one of claims 1 to 11.
13. A photovoltaic system, characterized in that, Includes the battery assembly as described in claim 12.