A light-emitting chip and its fabrication method
By employing a composite structure and a roughened structure of transparent conductive layer and metal layer stacked in the light-emitting chip, the problem of balancing the conductivity and light extraction performance of electrodes and transmission lines is solved, achieving efficient light extraction and stable ohmic contact, and improving the electrical performance and mechanical reliability of the device.
Patent Information
- Application Number
- CN202611568995.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-10
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, it is difficult to balance the conductivity of the electrodes and transmission lines of light-emitting chips with the light emission performance of the light-emitting region. Ohmic contacts cannot be formed between the N-type gallium nitride layer and the ITO layer, resulting in poor performance of the N-type electrodes.
A composite structure of transparent conductive layer and metal layer is used as electrode and transmission line. The roughened structure improves the crystal surface of semiconductor layer, increases ohmic contact area, and optimizes interface contact through metal interlayer to form stable ohmic contact.
It improves light extraction efficiency and light emission uniformity, reduces transmission resistance and voltage drop, enhances mechanical strength and reliability, and extends the lifespan of the device.
Smart Images

Figure CN123124535A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor display chip technology, and more specifically to a light-emitting chip and its fabrication method. Background Technology
[0002] A micro-LED (Light Emitting Diode) display is a pixel array display consisting of light-emitting diode (LED) chips with a size of less than 50 micrometers and an active driver array. When the LED chip operates, driving current needs to be injected through electrodes and transmission lines; the performance of the electrodes and transmission lines directly affects the chip's photoelectric characteristics.
[0003] In related technologies, if pure metals such as gold (Au), silver (Ag), copper (Cu), and aluminum (Al) are used as electrodes and transmission lines, although these metal materials have extremely low bulk resistivity and good mechanical strength, they also have high light absorption and reflectivity in the visible light band. Electrodes located in the light-emitting area will create a significant light-blocking effect, leading to a decrease in the effective light-emitting area of the chip and a reduction in light extraction efficiency. If transparent conductive oxides such as indium tin oxide (ITO) are used as electrodes and transmission lines, although they have high optical transmittance in the visible light band and can improve light emission, their resistivity is typically several orders of magnitude higher than that of metals. This limits their lateral current expansion capability, causing a rapid increase in line resistance when used as long-distance transmission lines, resulting in a significant voltage drop. Under high-current driving conditions, this leads to a significant increase in chip operating voltage, power consumption, and heat generation. Furthermore, transparent conductive oxides are brittle materials, prone to cracking or even fracture under bending, stretching, or thermal stress, resulting in low mechanical reliability.
[0004] In gallium nitride (GaN)-based micro-LEDs, there are P-type GaN layers, an active layer, and an N-type GaN layer. For the N-type GaN layer, while using pure ITO as the transparent electrode can achieve good light transmittance, it is often difficult to form an ideal ohmic contact between ITO and the N-type GaN surface. This leads to problems such as high contact resistivity, nonlinear IV characteristics, increased forward operating voltage, and reduced current injection efficiency. Furthermore, high contact resistance causes more significant Joule heating during operation, reducing the power efficiency of the Micro-LED chip, exacerbating heat generation, and potentially causing current congestion, uneven light emission, and decreased device reliability. Therefore, while directly placing pure ITO as the electrode on the N-type GaN surface improves light transmittance, achieving low contact resistance is difficult.
[0005] Therefore, a solution is needed to address the problems in related technologies, such as the difficulty in simultaneously achieving both the conductivity of electrodes and transmission lines and the light emission performance of the light-emitting region, as well as the inability to form ohmic contacts between the N-type gallium nitride layer and the ITO layer, resulting in poor performance of the N-type electrodes. Summary of the Invention
[0006] This invention provides a light-emitting chip and its fabrication method to solve the problems in related technologies, such as the difficulty in simultaneously achieving the conductivity of electrodes and transmission lines and the light emission performance of the light-emitting region, as well as the inability to form ohmic contacts between the N-type gallium nitride layer and the ITO layer, resulting in poor performance of the N-type electrode.
[0007] In a first aspect, the present invention provides a light-emitting chip, comprising: The base layer includes the luminescent region and the edge region located on the side of the luminescent region; An epitaxial structure is located on the surface of a substrate layer and includes a second semiconductor layer, an active layer, and a first semiconductor layer stacked sequentially, wherein the second semiconductor layer is relatively close to the substrate layer; the epitaxial structure is located in the light-emitting region; a roughened structure is provided on the side surface of the first semiconductor layer facing away from the active layer; A first ohmic contact layer is located on the roughened structure surface; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer; The first electrode is located on the side surface of the first ohmic contact layer that is opposite to the first semiconductor layer; the first electrode is located in the light-emitting region; the first electrode includes a first transparent conductive layer. A first transmission line structure is located in the edge region of the side of the first electrode. The first transmission line structure includes a first transparent conductive layer and a first metal layer stacked together, wherein the first metal layer is located on the side of the first transparent conductive layer facing away from the substrate layer; the first transparent conductive layer in the first electrode is connected to the first transparent conductive layer in the first transmission line structure.
[0008] The light-emitting chip provided by this invention has the following characteristics: First, the first electrode located in the light-emitting region is composed of a first transparent conductive layer, which can reduce the shading and absorption of light emitted from the light-emitting region by the electrode, reduce light loss caused by light absorption and reflection, thereby improving the light extraction efficiency and light emission uniformity of the chip. Second, the first transmission line structure located in the edge region is a composite structure of the first transparent conductive layer and the first metal layer. The first metal layer in the composite structure can reduce the transmission resistance and voltage drop effect of the first transmission line structure, improve the lateral current expansion capability, reduce the chip driving voltage and power consumption, and also enhance the mechanical strength and ductility of the first transmission line structure, reducing the risk of cracks, fractures and conductive failures caused by the brittleness of the first transparent conductive layer, thereby improving the stability and reliability of the device during processing, packaging and long-term operation. Furthermore, since the first transparent conductive layer has excellent chemical inertness, it can withstand the high temperature environment and acid and alkali etching processes in subsequent processes, preventing thermal migration or detachment of the electrodes and transmission lines, thereby significantly enhancing the long-term reliability and service life of the device. On the other hand, by roughening the surface of the first semiconductor layer in the light-emitting region on the side facing away from the active layer, the crystal plane of the first semiconductor layer can be altered, the surface work function of the first semiconductor layer can be reduced, the Fermi level pinning effect can be alleviated, and the contact area between the first ohmic contact layer and the first semiconductor layer can be increased, thereby reducing the interfacial barrier between the first ohmic contact layer and the first semiconductor layer. This allows the first ohmic contact layer and the first semiconductor layer to form an ohmic contact, promoting carrier tunneling transport and thus improving the performance of the first electrode. Furthermore, the roughened structure can also improve the light extraction path, further enhancing the light extraction efficiency.
[0009] In one alternative implementation, the first semiconductor layer is an N-type semiconductor layer and the second semiconductor layer is a P-type semiconductor layer.
[0010] The light-emitting chip provided by the present invention can change the crystal plane of the N-type semiconductor layer by setting the surface of the N-type semiconductor layer on the side away from the active layer to a roughened structure, thereby reducing the work function of the N-type semiconductor layer, alleviating the Fermi level pinning effect, and increasing the contact area between the first ohmic contact layer and the N-type semiconductor layer. This allows the first ohmic contact layer and the N-type semiconductor layer to form an ohmic contact, promoting carrier tunneling transport.
[0011] In one optional embodiment, the light-emitting chip further includes: a metal interlayer located between the roughened structure and the first ohmic contact layer; the work function of the metal interlayer is less than the electron affinity of the first semiconductor layer; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer through the metal interlayer; and the light transmittance of the metal interlayer is greater than 80%.
[0012] The light-emitting chip provided by this invention, by setting a metal interlayer on the roughened structural surface, can reduce the surface potential of the N-type semiconductor layer and alleviate the Fermi level pinning effect. The work function of the metal interlayer is lower than the electron affinity of the first semiconductor layer, which helps to lower the electron injection barrier at the metal-N-type semiconductor interface. This allows the first ohmic contact layer to form an ohmic contact with the first semiconductor layer through the metal interlayer with low contact resistance, further reducing contact resistivity and improving the current transmission efficiency of the first electrode. The transmittance of the metal interlayer is greater than 80%, which does not increase light absorption loss in the light-emitting area. It can improve the interface electrical contact characteristics and reduce contact resistivity while ensuring low light absorption loss, achieving a stable ohmic contact between the N-type semiconductor interface and the first ohmic contact layer. Therefore, this invention effectively enhances the chip's light extraction efficiency, external quantum efficiency, and wall-plugging efficiency while improving the device's current injection efficiency and reducing the operating voltage.
[0013] In one alternative embodiment, the material of the first semiconductor layer includes N-type gallium nitride, and the material of the second semiconductor layer includes P-type gallium nitride; The materials of the metal interlayer include titanium or indium; the thickness of the metal interlayer is 3~10nm; the metal interlayer has a coarsened structure with a homomorphic coating.
[0014] The light-emitting chip provided by this invention has a metal interlayer thickness of 3~10nm, which can improve the electrical contact at the interface without increasing the light absorption loss, thus ensuring the light extraction efficiency and light emission uniformity of the light-emitting area. The metal interlayer covers the roughened structure in a similar shape, which can ensure the uniformity of contact performance at various positions on the roughened surface and improve the reliability and stability of the first electrode.
[0015] In one optional embodiment, the roughening structure includes a plurality of arrayed protrusions, the protrusions being pyramidal in shape. The width of the protrusion is 50~300nm; the height of the protrusion is 40~300nm.
[0016] The light-emitting chip provided by this invention has a roughened structure comprising multiple arrayed protrusions. The protrusions are pyramidal in shape, which can alter the crystal plane of the first semiconductor layer, reduce the surface work function of the first semiconductor layer, alleviate the Fermi level pinning effect, increase the interfacial contact area between the first semiconductor layer and the first ohmic contact layer, reduce the contact resistance of the ohmic contact formed between the first semiconductor layer and the first ohmic contact layer, and further improve the performance of the first electrode. Furthermore, it can disrupt the total internal reflection conditions at the flat interface, improve the light emission path of the light-emitting region, and help improve the light extraction efficiency of the light-emitting chip.
[0017] In one alternative implementation, the light-emitting chip further includes: The second ohmic contact layer is located between the second semiconductor layer and the substrate layer; the second ohmic contact layer covers the substrate layer and is located in both the light-emitting region and the edge region; the second ohmic contact layer forms an ohmic contact with the second semiconductor layer; the epitaxial structure forms a stepped structure with the second ohmic contact layer; the surface of the second ohmic contact layer exposed on the side of the epitaxial structure is a mesa; the mesa is located in the edge region. The second electrode is located on the platform of the epitaxial structure. The second electrode includes a second transparent conductive layer and a second metal layer stacked together. The second metal layer is located on the side of the second transparent conductive layer that is opposite to the second ohmic contact layer. The second transmission line structure is located on the side of the second electrode away from the epitaxial structure. The second transmission line structure includes a second transparent conductive layer and a second metal layer stacked together. The second transparent conductive layer in the second electrode is connected to the second transparent conductive layer in the second transmission line structure, and the second metal layer in the second electrode is connected to the second metal layer in the second transmission line structure.
[0018] The light-emitting chip provided by this invention achieves electrical connection and electrical lead-out to one side of the second semiconductor layer by constructing a second electrode and a second transmission line structure on the mesa of the epitaxial structure. The second electrode and the first electrode cooperate to form a complete current path. The second transmission line structure includes a second transparent conductive layer and a second metal layer stacked together, which can reduce the transmission resistance and voltage drop effect of the second transmission line structure, improve the lateral current expansion capability, enhance the mechanical strength and ductility of the second transmission line structure, and also enhance the long-term reliability and service life of the device.
[0019] In one optional embodiment, the light-emitting chip further includes: a passivation layer covering a portion of the surface of the epitaxial structure facing away from the substrate layer and the sidewalls of the epitaxial structure, and covering the surface of the second ohmic contact layer exposed on the side of the epitaxial structure; The first electrode penetrates the passivation layer and is connected to the first ohmic contact layer; The second transparent conductive layer in the second electrode penetrates the passivation layer and is connected to the second ohmic contact layer.
[0020] The light-emitting chip provided by the present invention can form a protective layer and electrical isolation on the surface and sidewalls of the epitaxial structure by setting a passivation layer, and define the contact windows of the first electrode and the second electrode to avoid direct contact between the electrodes and the sidewalls of the epitaxial structure, which would cause short circuits or leakage.
[0021] In one optional embodiment, the first transparent conductive layer in the first electrode and the first transparent conductive layer in the first transmission line structure are the same layer that extends continuously. The second transparent conductive layer in the second electrode and the second transparent conductive layer in the second transmission line structure are the same layer that extends continuously. The second metal layer in the second electrode and the second metal layer in the second transmission line structure are the same layer that extends continuously. The materials of both the first and second ohmic contact layers include indium tin oxide; Both the first and second transparent conductive layers are made of indium tin oxide. Both the first and second metal layers are made of gold.
[0022] The light-emitting chip provided by this invention has a first transparent conductive layer in the first electrode and a first transparent conductive layer in the first transmission line structure that are continuously extending from the same layer. These layers can be formed in a single process, simplifying the manufacturing process and reducing the interface resistance between the first electrode and the first transmission line structure. Similarly, the second transparent conductive layer in the second electrode and a second transparent conductive layer in the second transmission line structure are continuously extending from the same layer. These layers can also be formed in a single process, simplifying the manufacturing process and reducing the interface resistance between the second electrode and the second transmission line structure. Both the first and second ohmic contact layers are made of indium tin oxide, which improves the ohmic contact performance between the first ohmic contact layer and the first semiconductor layer, reduces contact resistance, and ensures the light transmittance of the light-emitting area. Both the first and second metal layers are made of gold, which improves the conductivity and transmission performance of the second electrode, the first transmission line structure, and the second transmission line structure.
[0023] In a second aspect, the present invention also provides a method for preparing a light-emitting chip, for preparing the light-emitting chip of the first aspect and any embodiment thereof, comprising: An intermediate wafer is provided; the intermediate wafer includes a substrate layer and an epitaxial layer located on the surface of the substrate layer, which are stacked sequentially; the epitaxial layer includes a second semiconductor layer, an active layer and a first semiconductor layer stacked sequentially, wherein the second semiconductor layer is relatively close to the substrate layer; the intermediate wafer includes a light-emitting region and an edge region; the epitaxial layer is located in the light-emitting region and the edge region; The surface of the first semiconductor layer facing away from the active layer is roughened to form a roughened structure. Plasma treatment is applied to the roughened surface structure. A first ohmic contact layer is formed on the roughened structure surface; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer; The first ohmic contact layer and the epitaxial layer are patterned, and the first ohmic contact layer and the epitaxial layer in the edge region are removed, while the first ohmic contact layer and the epitaxial layer in the light-emitting region are retained; the epitaxial layer in the remaining light-emitting region is used as the epitaxial structure. A first electrode is formed on the surface of a first ohmic contact layer, and a first transmission line structure is formed in the edge region of the side of the first electrode; the first electrode includes a first transparent conductive layer; the first transmission line structure includes a first transparent conductive layer and a first metal layer stacked together, wherein the first metal layer is located on the side of the first transparent conductive layer facing away from the substrate layer; the first transparent conductive layer in the first electrode is connected to the first transparent conductive layer in the first transmission line structure.
[0024] The method for fabricating a light-emitting chip provided by this invention involves roughening the surface of the first semiconductor layer on the side facing away from the active layer to form a roughened structure. This alters the crystal plane of the first semiconductor layer, reduces its surface work function, alleviates the Fermi level pinning effect, and increases the contact area of the first semiconductor layer. Plasma treatment of the roughened structure allows for the modulation of the surface states, defect structures, and interface bands of the first semiconductor layer, helping to lower the interface barrier between the first semiconductor layer and the subsequently formed metal interlayer, thus promoting carrier tunneling transport. The formation of the metal interlayer improves the electrical contact characteristics of the ohmic contact interface while maintaining low light absorption loss, reducing contact resistivity and facilitating stable ohmic contact between the first semiconductor layer and the first ohmic contact layer. Following the first ohmic contact layer, an ohmic contact is formed between the first ohmic contact layer and the first semiconductor layer. Subsequently, patterning defines the epitaxial structure within the light-emitting region, and a first electrode composed of a first transparent conductive layer is formed in the light-emitting region. A first transmission line structure, consisting of a first transparent conductive layer and a first metal layer stacked in the edge region, is formed. This approach balances the light emission performance, conductivity, and mechanical reliability of the light-emitting chip. The method for fabricating a light-emitting chip provided by this invention effectively enhances the chip's light extraction efficiency, external quantum efficiency, and wall-insertion efficiency while improving the device's current injection efficiency and reducing the operating voltage. The fabrication process is simple and efficient, with good process compatibility and feasibility, providing a technical solution for the fabrication of high-performance vertical structure Micro-LED devices that combines electrical advantages, optical advantages, and process feasibility.
[0025] In one alternative embodiment, plasma treatment of the roughened structural surface includes: oxygen plasma treatment of the roughened structural surface. After plasma treatment of the roughened structure surface, the process further includes: forming a metal interlayer on the roughened structure surface; the metal interlayer conformally covering the roughened structure; and the work function of the metal interlayer being less than the electron affinity of the first semiconductor layer. A first ohmic contact layer is formed on the roughened structure surface, including: A first ohmic contact layer is formed on the surface of the metal interlayer; The first ohmic contact layer is annealed to form an ohmic contact with the first semiconductor layer; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer through a metal interlayer.
[0026] The method for fabricating a light-emitting chip provided by this invention regulates the surface states, defect structures, and interface defects of the roughened surface through oxygen plasma treatment. The work function of the metal interlayer is less than the electron affinity of the first semiconductor layer, which helps to reduce the interface barrier between the first semiconductor layer and the subsequently formed metal interlayer and promotes carrier tunneling transport. After forming a first ohmic contact layer on the surface of the metal interlayer, the first ohmic contact layer is annealed, which can promote the formation of a stable ohmic contact between the first ohmic contact layer and the first semiconductor layer through the metal interlayer and reduce the contact resistivity.
[0027] In one alternative embodiment, the intermediate wafer further includes a second ohmic contact layer located between the second semiconductor layer and the substrate layer; Provide intermediate wafers, including: An epitaxial layer is provided on a growth substrate, the epitaxial layer comprising a first semiconductor layer, an active layer and a second semiconductor layer stacked sequentially, wherein the first semiconductor layer is relatively close to the growth substrate. A second ohmic contact layer is formed on the side surface of the epitaxial layer opposite to the growth substrate, and a first metal bonding layer is formed on the side surface of the second ohmic contact layer opposite to the epitaxial layer. A base layer having a second metal bonding layer formed on its surface is provided; The first metal bonding layer is bonded to the second metal bonding layer to bond the epitaxial layer to the base layer; The grown substrate layer is removed by laser lift-off. The surface of the first semiconductor layer exposed after the growth substrate is removed is thinned.
[0028] The method for fabricating a light-emitting chip provided by the present invention involves transferring an epitaxial layer to a substrate layer via metal bonding and removing the growth substrate layer by laser lift-off to obtain an intermediate wafer with the first semiconductor layer facing the light-emitting side. Thinning treatment exposes the surface of the first semiconductor layer and achieves the target thickness, providing a basis for subsequent roughening treatment and the formation of electrodes and transmission lines.
[0029] In one alternative embodiment, after patterning the first ohmic contact layer and the epitaxial layer, the epitaxial structure and the second ohmic contact layer exposed on its side form a stepped structure; the surface of the second ohmic contact layer exposed on the side of the epitaxial structure is a mesa; the mesa is located in the edge region. Before the first electrode is formed on the surface of the first ohmic contact layer, the following is also included: A passivation layer is formed, which covers a portion of the surface of the epitaxial structure facing away from the substrate and the sidewalls of the epitaxial structure, and also covers the surface of the second ohmic contact layer exposed on the side of the epitaxial structure. A first via and a second via are formed within the passivation layer, the first via exposing a first ohmic contact layer and the second via exposing a second ohmic contact layer.
[0030] The method for fabricating a light-emitting chip provided by the present invention forms a stepped structure with the epitaxial structure after patterning and the second ohmic contact layer. A passivation layer covers the surface of the stepped structure to form protection and isolation. The first via and the second via respectively define contact windows leading to the first ohmic contact layer and the second ohmic contact layer, providing accurate contact positions for the formation of the first electrode and the second electrode.
[0031] In one alternative embodiment, in the step of forming a first electrode on the surface of the first ohmic contact layer and forming a first transmission line structure in the edge region of the side of the first electrode, the first transparent conductive layer in the first electrode fills the first via and connects to the first ohmic contact layer. The step of forming a first electrode on the surface of the first ohmic contact layer and forming a first transmission line structure in the edge region on the side of the first electrode further includes: A second electrode is formed on the surface of the second ohmic contact layer, and a second transmission line structure is formed in the edge region of the side of the second electrode; the second electrode includes a second transparent conductive layer and a second metal layer stacked together; the second transparent conductive layer in the second electrode fills a second via and connects to the second ohmic contact layer.
[0032] The method for fabricating a light-emitting chip provided by the present invention forms a first electrode, a first transmission line structure, and a second electrode and a second transmission line structure in the same process system. The first transparent conductive layer in the first electrode fills a first via and is connected to a first ohmic contact layer. The second transparent conductive layer in the second electrode fills a second via and is connected to a second ohmic contact layer. The process is simple, efficient, and has good process compatibility and feasibility. Attached Figure Description
[0033] To more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.
[0034] Figure 1 This is a schematic diagram of the structure of a light-emitting chip according to an embodiment of the present invention; Figure 2 This is a top view schematic diagram of the structure of a light-emitting chip according to an embodiment of the present invention; Figure 2 for Figure 1 A top-down view; Figure 3 This is a schematic flowchart of a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 4 This is a schematic flowchart illustrating a method for fabricating a light-emitting chip according to an embodiment of the present invention. Figure 5 This is a schematic diagram of the structure for forming an epitaxial layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 6 This is a schematic diagram of the structure of forming a first ohmic contact layer and a second metal bonding layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention. Figure 7 This is a schematic diagram of the structure of forming a first metal bonding layer on a substrate layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 8 This is a schematic diagram of the structure for forming an intermediate wafer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 9 This is a schematic diagram of the structure forming a protrusion structure in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 10 This is a schematic diagram of the structure for forming a metal interlayer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 11 This is a schematic diagram of the structure for forming the first ohmic contact layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 12A This is a schematic diagram of the structure forming an epitaxial structure in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 12B This is a top view schematic diagram of the structure forming an epitaxial structure in a method for fabricating a light-emitting chip according to an embodiment of the present invention. Figure 12B for Figure 12A A top-down view; Figure 13 This is a schematic diagram of the structure for forming a passivation layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 14 This is a schematic diagram of the structure for forming a first via and a second via in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 15A This is a schematic diagram of the structure of forming a first transparent conductive layer and a second transparent conductive layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 15BThis is a top view schematic diagram of the structure forming the first transparent conductive layer and the second transparent conductive layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention. Figure 15B for Figure 15A A top-down view; Figure 16A This is a schematic diagram of the structure for forming a first metal layer and a second metal layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention; Figure 16B This is a top view schematic diagram of the structure forming the first metal layer and the second metal layer in a method for fabricating a light-emitting chip according to an embodiment of the present invention. Figure 16B for Figure 16A A top-down view.
[0035] Figure label: 10. Base layer; 20. Epitaxial structure; 21. First semiconductor layer; 22. Second semiconductor layer; 23. Active layer; 211. Protrusion structure; 31. First ohmic contact layer; 32. Second ohmic contact layer; 40. Passivation layer; 41. First via; 42. Second via; 51. First transparent conductive layer; 52. Second transparent conductive layer; 61. First metal layer; 62. Second metal layer; 70. Metal sandwich layer; 80. Bonding layer; 81. First metal bonding layer; 82. Second metal bonding layer; 90. Growth substrate layer; 91. Buffer epitaxial layer; 101, Light-emitting region; 102, Edge region; 201, First electrode; 202, Second electrode; 301, First transmission line structure; 302, Second transmission line structure. Detailed Implementation
[0036] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. It is understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, the accompanying drawings show only the parts relevant to the invention and not all structures. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without inventive effort are within the scope of protection of the present invention.
[0037] In the following description, descriptions of well-known structures and techniques are omitted to avoid unnecessarily obscuring the concepts of the present invention. Various structural schematic diagrams according to embodiments of the present invention are shown in the accompanying drawings. These drawings are not to scale, and some details are enlarged for clarity, and some details may be omitted. The shapes of the various regions and layers shown in the drawings, as well as their relative sizes and positional relationships, are merely exemplary and may deviate in practice due to manufacturing tolerances or technical limitations. Furthermore, those skilled in the art can design regions / layers with different shapes, sizes, and relative positions as needed. In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element, or there may be an intermediate layer / element between them. Additionally, if a layer / element is "on" another layer / element in one orientation, then when the orientation is reversed, the layer / element may be "below" the other layer / element.
[0038] As described in the background section, if pure metal is used as the electrode and transmission line in the light-emitting chip of the related technology, the light-blocking effect of the metal will reduce the light extraction efficiency of the chip; if transparent conductive oxide is used as the electrode and transmission line, there are problems such as high transmission line resistance, significant voltage drop, and poor mechanical brittleness.
[0039] In a gallium nitride (GaN)-based micro light-emitting diode (Micro-LED), there are P-type gallium nitride layers, an active layer, and an N-type gallium nitride layer. As a typical wurtzite-structured group III nitride semiconductor, GaN exhibits a significant spontaneous polarization effect along the C-axis. Different polar faces (i.e., the N-polar face and the Ga-polar face) lead to significant differences in surface charge properties and interface band structure.
[0040] When an ITO layer is formed on the surface of a Ga polar facet p-type gallium nitride (GaN) layer, the relatively high work function of ITO helps to reduce the interface barrier that holes need to overcome to be injected into the valence band of the GaN layer from the ITO. Simultaneously, the Ga polar facet has a negative polarization-bound charge, which tends to attract positively charged holes, reducing hole depletion on the surface of the p-type GaN layer and bringing the valence band edge closer to the Fermi level. After appropriate annealing, oxygen in the ITO may also form Ga-O bonds with Ga atoms at the interface, promoting Ga atom diffusion and Ga vacancy formation. Ga vacancies are acceptor defects, which can increase the effective hole concentration near the interface, thereby compressing the width of the space charge region. This allows holes to cross the interface barrier through thermal emission or tunneling, ultimately exhibiting an approximately linear current-voltage characteristic.
[0041] However, when an ITO layer is formed on the surface of an N-type gallium nitride (GaN) layer with an N-polarity, the high work function of ITO is not conducive to electron transport, easily leading to a high electronic Schottky barrier at the ITO / N-type GaN interface. Although the positive polarization charge of an ideal N-polarity surface may theoretically attract electrons, the actual N-polarity surface is chemically highly reactive, easily generating Ga vacancies, oxide layers, dangling bonds, and complex surface states during laser lift-off, mechanical polishing, wet processing, and sputtering deposition. Among these, Ga vacancies and some interface states have acceptor properties, which can trap free electrons, reduce the effective electron concentration near the interface, and cause Fermi level pinning and conduction band bending. Therefore, although ITO has high visible light transmittance and good conductivity, when it directly contacts an N-type GaN layer with an N-polarity, it often exhibits high contact resistivity and non-ideal current transport characteristics, leading to increased forward operating voltage, increased Joule heating, and reduced power efficiency in Micro-LED chips, ultimately affecting the optoelectronic performance and long-term reliability of the device.
[0042] like Figure 1 and Figure 2 As shown, this embodiment provides a light-emitting chip, including: a substrate layer 10, an epitaxial structure 20, a first ohmic contact layer 31, a first electrode 201, and a first transmission line structure 301. The substrate layer 10 includes a light-emitting region 101 and an edge region 102 located on the side of the light-emitting region 101. The epitaxial structure 20 is located on the surface of the substrate layer 10 and includes a second semiconductor layer 22, an active layer 23, and a first semiconductor layer 21 stacked sequentially, wherein the second semiconductor layer 22 is relatively close to the substrate layer 10; the epitaxial structure 20 is located in the light-emitting region 101. A roughened structure is provided on the surface of the first semiconductor layer 21 facing away from the active layer 23. The first ohmic contact layer 31 is located on the surface of the roughened structure; the first ohmic contact layer 31 forms an ohmic contact with the first semiconductor layer 21. The first electrode 201 is located on the surface of the first ohmic contact layer 31 facing away from the first semiconductor layer 21; the first electrode 201 is located in the light-emitting region 101; the first electrode 201 includes a first transparent conductive layer 51. The first transmission line structure 301 is located in the edge region 102 on the side of the first electrode 201. The first transmission line structure 301 includes a first transparent conductive layer 51 and a first metal layer 61 stacked together, wherein the first metal layer 61 is located on the side of the first transparent conductive layer 51 facing away from the substrate layer 10; the first transparent conductive layer 51 in the first electrode 201 is connected to the first transparent conductive layer 51 in the first transmission line structure 301.
[0043] In specific implementation, the substrate 10 can be a silicon substrate, or other conductive or semiconductor substrates that can provide mechanical support for the epitaxial structure 20. This embodiment does not limit the specific material of the substrate 10. The light-emitting region 101 is the light-emitting chip region in the light-emitting chip, and the edge region 102 is the region on the side of the light-emitting region 101 used for arranging structures such as transmission lines. The material of the first ohmic contact layer 31 includes a transparent oxide (e.g., indium tin oxide). The roughened structure can change the crystal plane of the first semiconductor layer 21, reduce the work function of the first semiconductor layer surface, alleviate the Fermi level pinning effect, and effectively increase the interface contact area, which is beneficial for achieving ohmic contact between the first ohmic contact layer 31 and the first semiconductor layer 21, thereby improving the performance of the first electrode 201. Simultaneously, the roughened structure can also improve the light emission path, reduce total internal reflection loss, and thus improve the light extraction efficiency of the device.
[0044] Because the first electrode 201 is made of a transparent conductive material, the light emitted from the chip's light-emitting region 101 can pass through the first electrode 201, reducing the electrode's blocking and absorption of the emitted light. The first transmission line structure 301 is used to transmit driving current to the light-emitting region 101. The first metal layer 61 covers the first transparent conductive layer 51 to form a composite transmission line, which significantly reduces the resistance and voltage drop of the transmission line, improves the lateral current expansion capability, and enhances the mechanical strength and ductility of the transmission line, reducing the risk of cracks, fractures, and conductive failures in the transparent conductive layer due to brittleness.
[0045] The light-emitting chip provided in this embodiment has the following characteristics: First, the first electrode located in the light-emitting area is composed of a first transparent conductive layer, which can reduce the shading and absorption of light emitted from the light-emitting area by the electrode, reduce light loss caused by light absorption and reflection, thereby improving the light extraction efficiency and light emission uniformity of the chip. Second, the first transmission line structure located in the edge area is a composite structure of the first transparent conductive layer and the first metal layer. The first metal layer in the composite structure can reduce the transmission resistance and voltage drop effect of the first transmission line structure, improve the lateral current expansion capability, reduce the chip driving voltage and power consumption, and also enhance the mechanical strength and ductility of the first transmission line structure, reducing the risk of cracks, fractures and conductive failures caused by the brittleness of the first transparent conductive layer, thereby improving the stability and reliability of the device during processing, packaging and long-term operation. Furthermore, since the first transparent conductive layer has excellent chemical inertness, it can withstand the high temperature environment and acid and alkali etching processes in subsequent processes, preventing thermal migration or detachment of the electrodes and transmission lines, thereby significantly enhancing the long-term reliability and service life of the device. On the other hand, by roughening the surface of the first semiconductor layer in the light-emitting region on the side facing away from the active layer, the crystal plane of the first semiconductor layer can be changed, the surface work function of the first semiconductor layer can be reduced, the Fermi level pinning effect can be alleviated, and the contact area between the first ohmic contact layer and the first semiconductor layer can be increased, thus reducing the interfacial barrier between the first ohmic contact layer and the first semiconductor layer. This allows the first ohmic contact layer and the first semiconductor layer to form an ohmic contact, promoting carrier tunneling transport and improving the performance of the first electrode. Furthermore, the roughened structure can also improve the light emission path, further enhancing the light extraction efficiency. Therefore, this embodiment can improve the ohmic contact performance of the first electrode while increasing the transmittance of the light-emitting region, and can also reduce the transmission resistance and voltage drop effect of the first transmission line structure, improve the lateral current spread capability, and reduce the chip driving voltage and power consumption.
[0046] In some alternative implementations, the light-emitting chip is a vertically structured Micro-LED chip.
[0047] In related technologies, metal electrodes in vertical structure Micro-LED devices exhibit significant reflection and absorption of emitted light.
[0048] Therefore, this embodiment improves the light transmittance of the light-emitting region 101 by setting the first electrode 201 of the light-emitting region 101 as a light-transmitting first transparent conductive layer 51, effectively reducing the optical loss in the light extraction process of traditional metal electrodes, and improving the light extraction efficiency and wall-insertion efficiency of the device. By setting the first transmission line structure 301 as a composite structure of the first transparent conductive layer 51 and the first metal layer 61, the advantages of the high conductivity of the metal material and the high light transmittance of the first transparent conductive layer 51 are fully combined, reducing the transmission resistance and voltage drop effect of the first transmission line structure 301, improving the lateral current expansion capability, reducing the chip driving voltage and power consumption, and also improving the mechanical properties of the device. This reduces the risk of cracking, peeling and failure of the first transparent conductive layer under stress, improves the ductility, mechanical strength and long-term working stability of the device, thereby enhancing the reliability and service life of the Micro-LED device in complex working environments.
[0049] In some alternative implementations, the first semiconductor layer 21 is an N-type semiconductor layer and the second semiconductor layer 22 is a P-type semiconductor layer.
[0050] An ohmic contact refers to an electrical contact with approximately linear and symmetrical current-voltage characteristics and low contact resistivity. In related technologies, an effective ohmic contact cannot be formed between an N-type semiconductor layer (e.g., an N-type gallium nitride layer) and a transparent conductive oxide (e.g., ITO). In this embodiment, by forming a roughened structure on the surface of the N-type semiconductor layer to change the crystal plane, an ohmic contact layer 31 can be formed between the first ohmic contact layer 31 and the N-type semiconductor layer. The material of the first ohmic contact layer 31 includes transparent conductive oxides such as ITO.
[0051] The light-emitting chip provided in this embodiment can change the crystal plane of the N-type semiconductor layer by setting the surface of the N-type semiconductor layer facing away from the active layer to a roughened structure, thereby reducing the work function of the surface of the first semiconductor layer, alleviating the Fermi level pinning effect, and increasing the contact area between the first ohmic contact layer and the N-type semiconductor layer. This allows the first ohmic contact layer and the N-type semiconductor layer to form an ohmic contact, promoting carrier tunneling transport and further improving the performance of the first electrode.
[0052] In one possible implementation, the first semiconductor layer 21 is made of N-type gallium nitride, the second semiconductor layer 22 is made of P-type gallium nitride, and the active layer 23 is a multiple quantum well (MQW) layer. It should be noted that the material system of the epitaxial structure 20 can also be other semiconductor material systems capable of achieving electroluminescence; this embodiment does not limit this.
[0053] In some alternative implementations, such as Figure 1As shown, the light-emitting chip also includes: a metal interlayer 70 located between the roughened structure and the first ohmic contact layer 31; the work function of the metal interlayer 70 is less than the electron affinity of the first semiconductor layer 21; the first ohmic contact layer 31 forms an ohmic contact with the first semiconductor layer 21 through the metal interlayer 70; the light transmittance of the metal interlayer 70 is greater than 80%.
[0054] In practical implementation, the work function refers to the minimum energy required for an electron to escape from the interior of the material to the vacuum level; the electron affinity refers to the energy difference between the conduction band bottom of the semiconductor and the vacuum level. When the work function of the metal interlayer 70 is less than the electron affinity of the semiconductor, it is beneficial to reduce the electron injection barrier at the interface between the metal and the N-type semiconductor. The light transmittance of the metal interlayer 70 is greater than 80%. The metal interlayer 70, with a thickness on the nanometer scale, reduces the interface barrier and improves ohmic contact while almost not increasing light absorption loss.
[0055] The light-emitting chip provided in this embodiment reduces the surface potential of the N-type semiconductor layer and alleviates the Fermi level pinning effect by setting a metal interlayer on the roughened structural surface. The work function of the metal interlayer is lower than the electron affinity of the first semiconductor layer, which helps to lower the electron injection barrier at the metal-N-type semiconductor interface. This allows the first ohmic contact layer to form an ohmic contact with the first semiconductor layer through the metal interlayer with low contact resistance, further reducing contact resistivity and improving the current transmission efficiency of the first electrode. The transmittance of the metal interlayer is greater than 80%, which does not increase light absorption loss in the light-emitting area. It improves the interface electrical contact characteristics and reduces contact resistivity while ensuring low light absorption loss, achieving a stable ohmic contact between the N-type semiconductor interface and the first ohmic contact layer. Therefore, this invention effectively enhances the chip's light extraction efficiency, external quantum efficiency, and wall-plugging efficiency while improving the device's current injection efficiency and reducing the operating voltage.
[0056] In some alternative embodiments, the metal interlayer 70 is made of titanium or indium. The metal interlayer 70 can also be made of other metal materials with low work function; this embodiment does not limit the specific material of the metal interlayer 70.
[0057] In some alternative embodiments, the thickness of the metal interlayer 70 is 3~10 nm. Optionally, the thickness of the metal interlayer 70 is 3 nm.
[0058] In some alternative implementations, the metal interlayer 70 is conformally covered with a roughened structure.
[0059] In practice, the metal interlayer 70 is shaped to cover the roughened structure, that is, the metal interlayer 70 extends continuously along the surface contour of the pyramidal protrusion structure 211.
[0060] The light-emitting chip provided in this embodiment has a metal interlayer thickness of 3~10nm, which can improve the electrical contact at the interface without increasing the light absorption loss, thus ensuring the light extraction efficiency and light emission uniformity of the light-emitting area. The metal interlayer covers the roughened structure in a similar shape, which can ensure the uniformity of contact performance at various positions on the roughened surface and improve the reliability and stability of the first electrode.
[0061] In some alternative implementations, such as Figure 1 As shown, the roughened structure includes multiple arrayed protrusions 211, each in the shape of a pyramid. The arrayed pyramidal protrusions 211 can increase the interface contact area, which is beneficial for the subsequent formation of ohmic contacts. They can also disrupt the total internal reflection conditions at the flat interface, which is beneficial for improving light extraction efficiency.
[0062] In some alternative implementations, the protrusion structure 211 is in the shape of a pyramid.
[0063] In some alternative embodiments, the protrusion structure 211 is shaped as a hexagonal pyramid. By forming a dense hexagonal pyramid structure, the crystal plane at the surface position of the first semiconductor layer 21 can be transformed from (000-1) to (10-1-1).
[0064] In some optional embodiments, the width of the protrusion structure 211 is 50~300nm; the height of the protrusion structure 211 is 40~300nm. It should be noted that the width and height of the protrusion structure 211 can be adjusted according to the roughening process conditions, and this embodiment does not limit this.
[0065] The light-emitting chip provided in this embodiment has a roughened structure including multiple arrayed protrusions. The protrusions are pyramidal in shape, which can change the crystal plane of the first semiconductor layer, reduce the surface work function of the first semiconductor layer, alleviate the Fermi level pinning effect, increase the interface contact area between the first semiconductor layer and the first ohmic contact layer, reduce the contact resistance of the ohmic contact formed between the first semiconductor layer and the first ohmic contact layer, and disrupt the total internal reflection condition at the flat interface, improve the light emission path of the light-emitting region, and help improve the light extraction efficiency of the light-emitting chip.
[0066] In some alternative embodiments, the roughened structure of the surface of the first semiconductor layer 21 is adapted to be formed by roughening and plasma surface treatment processes. The first semiconductor layer 21 is an N-type semiconductor layer.
[0067] In specific implementation, a roughened structure is formed on the surface of the N-type semiconductor layer through roughening treatment. This alters the crystal planes of the N-type semiconductor layer, reduces its surface work function, and alleviates the Fermi level pinning effect, facilitating ohmic contact between the first ohmic contact layer 31 and the first semiconductor layer 21. Combining plasma surface treatment with the modulation of the surface states, defect structure, and interface bands of the N-type semiconductor layer helps lower the interface barrier between the first ohmic contact layer 31 and the N-type semiconductor layer, promoting carrier tunneling transport. Furthermore, by introducing a metal interlayer 70, the interfacial electrical contact characteristics can be improved while maintaining low light absorption loss, reducing contact resistivity and achieving stable ohmic contact between the N-type semiconductor layer and the first ohmic contact layer 31. Therefore, this embodiment effectively enhances the chip's light extraction efficiency, external quantum efficiency, and wall-plugging efficiency while improving device current injection efficiency and reducing operating voltage.
[0068] In some alternative implementations, such as Figure 1 As shown, the light-emitting chip also includes: a second ohmic contact layer 32, a second electrode 202, and a second transmission line structure 302.
[0069] The second ohmic contact layer 32 is located between the second semiconductor layer 22 and the substrate layer 10; the second ohmic contact layer 32 covers the substrate layer 10 and is located in both the light-emitting region 101 and the edge region 102; the second ohmic contact layer 32 and the second semiconductor layer 22 form an ohmic contact; the epitaxial structure 20 and the second ohmic contact layer 32 form a stepped structure; the surface of the second ohmic contact layer 32 exposed on the side of the epitaxial structure 20 is a mesa; the mesa is located in the edge region 102.
[0070] The second electrode 202 is located on the platform of the side of the epitaxial structure 20. The second electrode 202 includes a second transparent conductive layer 52 and a second metal layer 62 stacked together. The second metal layer 62 is located on the side of the second transparent conductive layer 52 that is opposite to the second ohmic contact layer 32.
[0071] The second transmission line structure 302 is located on the side of the second electrode 202 away from the epitaxial structure 20. The second transmission line structure 302 includes a second transparent conductive layer 52 and a second metal layer 62 stacked together. The second transparent conductive layer 52 in the second electrode 202 is connected to the second transparent conductive layer 52 in the second transmission line structure 302, and the second metal layer 62 in the second electrode 202 is connected to the second metal layer 62 in the second transmission line structure 302.
[0072] The light-emitting chip provided in this embodiment achieves electrical connection and electrical lead-out to one side of the second semiconductor layer by constructing a second electrode and a second transmission line structure on the mesa of the epitaxial structure. The second electrode and the first electrode cooperate to form a complete current path. The second transmission line structure includes a second transparent conductive layer and a second metal layer stacked together, which can reduce the transmission resistance and voltage drop effect of the second transmission line structure, improve the lateral current expansion capability, enhance the mechanical strength and ductility of the second transmission line structure, and also enhance the long-term reliability and service life of the device.
[0073] In some alternative implementations, such as Figure 1 As shown, the light-emitting chip also includes a passivation layer 40, which covers a portion of the surface of the epitaxial structure 20 facing away from the substrate layer 10 and the sidewalls of the epitaxial structure 20, and covers the surface of the second ohmic contact layer 32 exposed on the side of the epitaxial structure 20.
[0074] In some alternative embodiments, the first electrode 201 penetrates the passivation layer 40 and is connected to the first ohmic contact layer 31; the second transparent conductive layer 52 in the second electrode 202 penetrates the passivation layer 40 and is connected to the second ohmic contact layer 32.
[0075] The light-emitting chip provided in this embodiment can form a protective layer and electrical isolation on the surface and sidewalls of the epitaxial structure by setting a passivation layer, and defines the contact windows of the first electrode and the second electrode to avoid direct contact between the electrodes and the sidewalls of the epitaxial structure, which could cause short circuits or leakage.
[0076] In some alternative embodiments, the material of the passivation layer 40 includes silicon dioxide, and the thickness of the passivation layer 40 is 2000~3000 Å.
[0077] In some alternative implementations, the passivation layer 40 has a thickness of 2700 Å.
[0078] In specific implementation, the material and thickness of the passivation layer 40 can be selected according to the isolation and protection requirements. For example, other insulating dielectric materials can also be used, but this embodiment does not limit this. The passivation layer 40 forms a protective cover and electrical isolation for the epitaxial structure 20, preventing the electrodes from directly contacting the sidewalls of the epitaxial structure 20 and causing short circuits or leakage.
[0079] In some alternative embodiments, the first ohmic contact layer 31 is made of a transparent conductive oxide. The first transparent conductive layer 51 is also made of a transparent conductive oxide.
[0080] In specific implementation, the material of the first ohmic contact layer 31 includes a transparent conductive oxide, which, after annealing, can form a stable ohmic contact with the first semiconductor layer 21. The first electrode 201 is located in the light-emitting region 101 and includes a first transparent conductive layer 51 made of a transparent conductive oxide. Because the first electrode 201 is made of a transparent conductive material, the light emitted from the chip's light-emitting region 101 can pass through the first electrode 201, reducing the electrode's blocking and absorption of the emitted light. In addition, the transparent conductive oxide has excellent chemical inertness and can withstand the high-temperature environment and acid-base etching processes in the manufacturing process, preventing the first electrode 201 from thermally migrating or detaching, thereby significantly enhancing the long-term reliability and lifespan of the device and improving the reliability of the first electrode 201.
[0081] In some alternative embodiments, the material of the first metal layer 61 includes a conductive metal.
[0082] In a specific implementation, the first transmission line structure 301 includes a first transparent conductive layer 51 and a first metal layer 61 stacked together. The transparent conductive oxide possesses excellent chemical inertness, allowing it to withstand the high-temperature environment and acid / alkali etching processes during manufacturing, preventing thermal migration or detachment of the first transmission line structure 301. This significantly enhances the long-term reliability and lifespan of the device, improving the overall reliability of the first transmission line structure 301. The first metal layer 61 covers the first transparent conductive layer 51 to form a composite transmission line, which significantly reduces the resistance and voltage drop of the transmission line, improves the lateral current spread capability, and enhances the mechanical strength and ductility of the first transmission line structure 301, reducing the risk of cracks, fractures, and conductive failures in the transparent conductive layer due to brittleness.
[0083] In some alternative embodiments, the material of the second ohmic contact layer 32 comprises a transparent conductive oxide. The material of the second transparent conductive layer 52 comprises a transparent conductive oxide.
[0084] In some alternative embodiments, the material of the first metal layer 61 includes a conductive metal.
[0085] In specific implementation, the material of the second ohmic contact layer 32 includes a transparent conductive oxide, which, after annealing, can form a stable ohmic contact with the second semiconductor layer 22. The second transmission line structure 302 includes a second transparent conductive layer 52 and a second metal layer 62 stacked together. The transparent conductive oxide possesses excellent chemical inertness, can withstand the high-temperature environment and acid-base etching processes during manufacturing, and prevents thermal migration or detachment of the second transmission line structure 302, thereby significantly enhancing the long-term reliability and lifespan of the device and improving the reliability of the second transmission line structure 302. The second metal layer 62 covers the second transparent conductive layer 52 to form a composite transmission line, which can significantly reduce the resistance and voltage drop of the transmission line, improve the lateral current spreading capability, and enhance the mechanical strength and ductility of the second transmission line structure 302, reducing the risk of cracks, fractures, and conductive failures in the transparent conductive layer due to brittleness.
[0086] In some alternative embodiments, the first transparent conductive layer 51 in the first electrode 201 and the first transparent conductive layer 51 in the first transmission line structure 301 are the same layer that extends continuously.
[0087] In some optional embodiments, the second transparent conductive layer 52 in the second electrode 202 and the second transparent conductive layer 52 in the second transmission line structure 302 are the same layer that extends continuously, and the second metal layer 62 in the second electrode 202 and the second metal layer 62 in the second transmission line structure 302 are the same layer that extends continuously.
[0088] In some alternative embodiments, the first ohmic contact layer 31 is made of indium tin oxide and, after annealing, can form a stable ohmic contact with the first semiconductor layer 21. The second ohmic contact layer 32 is also made of indium tin oxide and, after annealing, can form a stable ohmic contact with the second semiconductor layer 22.
[0089] In some alternative implementations, such as Figure 1 As shown, the light-emitting chip also includes a bonding layer 80 located between the substrate layer 10 and the first ohmic contact layer 31. The bonding layer 80 includes a first metal bonding layer 81 and a second metal bonding layer 82, wherein the first metal bonding layer 81 is in contact with the substrate layer 10, and the second metal bonding layer 82 is located on the side of the first metal bonding layer 81 facing away from the substrate layer 10.
[0090] In some alternative embodiments, the materials of the first transparent conductive layer 51 and the second transparent conductive layer 52 both include indium tin oxide.
[0091] In some alternative embodiments, the first metal layer 61 and the second metal layer 62 are both made of gold.
[0092] The light-emitting chip provided in this embodiment has a first transparent conductive layer in the first electrode and a first transparent conductive layer in the first transmission line structure that are continuously extending from the same layer. These layers can be formed in a single process, simplifying the manufacturing process and reducing the interface resistance between the first electrode and the first transmission line structure. Similarly, the second transparent conductive layer in the second electrode and the second transparent conductive layer in the second transmission line structure are continuously extending from the same layer. These layers can also be formed in a single process, simplifying the manufacturing process and reducing the interface resistance between the second electrode and the second transmission line structure. Both the first and second ohmic contact layers are made of indium tin oxide, which improves the ohmic contact performance between the first ohmic contact layer and the first semiconductor layer, reduces contact resistance, and ensures the light transmittance of the light-emitting area. Both the first and second metal layers are made of gold, which improves the conductivity and transmission performance of the second electrode, the first transmission line structure, and the second transmission line structure.
[0093] In some alternative embodiments, the thickness of the first ohmic contact layer 31 is 50-200 nm; the thickness of the second ohmic contact layer 32 is 100-200 nm.
[0094] In some alternative embodiments, the thickness of the first transparent conductive layer 51 located above the passivation layer 40 is 100~200nm, and the thickness of the first metal layer 61 is 600~800nm.
[0095] In some alternative embodiments, the thickness of the second transparent conductive layer 52 located above the passivation layer 40 is 100~200nm, and the thickness of the second metal layer 62 is 600~800nm.
[0096] In some alternative embodiments, the thickness of the first ohmic contact layer 31 is 150 nm; the thickness of the second ohmic contact layer 32 is 150 nm.
[0097] In some alternative embodiments, the thickness of the first transparent conductive layer 51 located above the passivation layer 40 is 150 nm, and the thickness of the first metal layer 61 is 750 nm.
[0098] In some alternative embodiments, the thickness of the second transparent conductive layer 52 located above the passivation layer 40 is 150 nm, and the thickness of the second metal layer 62 is 750 nm.
[0099] It should be noted that the thickness of each film layer can be adjusted according to the requirements of light transmission and conductivity, but this embodiment does not limit this.
[0100] like Figure 3 As shown, this embodiment provides a method for preparing a light-emitting chip, which is used to prepare a light-emitting chip corresponding to any of the above embodiments. The preparation method includes, but is not limited to, steps S101 to S106.
[0101] Step S101: Provide an intermediate wafer; the intermediate wafer includes a substrate layer 10 and an epitaxial layer located on the surface of the substrate layer 10, which are stacked sequentially. The epitaxial layer includes a second semiconductor layer 22, an active layer 23, and a first semiconductor layer 21, which are stacked sequentially, wherein the second semiconductor layer 22 is relatively close to the substrate layer 10; the intermediate wafer includes a light-emitting region 101 and an edge region 102; the epitaxial layer is located in the light-emitting region 101 and the edge region 102, such as... Figure 8 As shown.
[0102] Step S102: Roughen the surface of the first semiconductor layer 21 on the side facing away from the active layer 23 to form a roughened structure, such as... Figure 9 As shown.
[0103] Step S103: Perform plasma treatment on the roughened surface structure.
[0104] Step S104: Form a first ohmic contact layer 31 on the roughened structure surface; the first ohmic contact layer 31 forms an ohmic contact with the first semiconductor layer 21, such as... Figure 11 As shown.
[0105] Step S105: The first ohmic contact layer 31 and the epitaxial layer are patterned. The first ohmic contact layer 31 and the epitaxial layer in the edge region 102 are removed, while the first ohmic contact layer 31 and the epitaxial layer in the light-emitting region 101 are retained. The remaining epitaxial layer in the light-emitting region 101 serves as the epitaxial structure 20, such as... Figure 12A and Figure 12B As shown.
[0106] Step S106: A first electrode 201 is formed on the surface of the first ohmic contact layer 31, and a first transmission line structure 301 is formed in the edge region 102 on the side of the first electrode 201; the first electrode 201 includes a first transparent conductive layer 51; the first transmission line structure 301 includes a first transparent conductive layer 51 and a first metal layer 61 stacked together, wherein the first metal layer 61 is located on the side of the first transparent conductive layer 51 facing away from the substrate layer 10; the first transparent conductive layer 51 in the first electrode 201 is connected to the first transparent conductive layer 51 in the first transmission line structure 301, such as... Figure 16A and Figure 16B As shown.
[0107] The method for fabricating a light-emitting chip provided in this embodiment roughens the surface of the first semiconductor layer on the side facing away from the active layer to form a roughened structure. This alters the crystal plane of the first semiconductor layer, reduces its surface work function, alleviates the Fermi level pinning effect, and increases the contact area of the first semiconductor layer. Plasma treatment of the roughened structure allows for the modulation of the surface states, defect structures, and interface bands of the first semiconductor layer, helping to lower the interface barrier between the first semiconductor layer and the subsequently formed metal interlayer, promoting carrier tunneling transport. Forming the metal interlayer improves the electrical contact characteristics of the ohmic contact interface while maintaining low light absorption loss, reducing contact resistivity and facilitating stable ohmic contact between the first semiconductor layer and the first ohmic contact layer. Following the first ohmic contact layer, an ohmic contact is formed between the first ohmic contact layer and the first semiconductor layer. Subsequently, patterning defines the epitaxial structure within the light-emitting region, and a first electrode composed of a first transparent conductive layer is formed in the light-emitting region. A first transmission line structure, consisting of a first transparent conductive layer and a first metal layer stacked in the edge region, is formed. This approach balances the light emission performance, conductivity, and mechanical reliability of the light-emitting chip. The method for fabricating the light-emitting chip provided in this embodiment effectively enhances the chip's light extraction efficiency, external quantum efficiency, and wall-insertion efficiency while improving the device's current injection efficiency and reducing the operating voltage. The fabrication process is simple and efficient, with good process compatibility and feasibility, providing a technical solution that combines electrical advantages, optical advantages, and process feasibility for the fabrication of high-performance vertical structure Micro-LED devices.
[0108] In some alternative implementations, the first semiconductor layer 21 is an N-type semiconductor layer and the second semiconductor layer 22 is a P-type semiconductor layer.
[0109] In specific implementation, by roughening and surface treating the surface of the N-type semiconductor layer and forming a metal interlayer 70, the interfacial contact area can be effectively increased and the light extraction path improved, reducing total internal reflection loss and thus improving the light extraction efficiency of the Micro-LED device. Simultaneously, the crystal plane changes caused by surface roughening facilitate ohmic contact. Combined with plasma surface treatment processes to modulate the surface states, defect structures, and interfacial bands of the N-type semiconductor layer, this helps lower the interfacial barrier between the first ohmic contact layer 31 and the N-type semiconductor layer, promoting carrier tunneling transport. Furthermore, by introducing the metal interlayer 70, the interfacial electrical contact characteristics can be improved while maintaining low light absorption loss, reducing contact resistivity and achieving stable ohmic contact between the N-type semiconductor layer and the first ohmic contact layer 31. Therefore, this embodiment effectively enhances the chip's light extraction efficiency, external quantum efficiency, and wall-insertion efficiency while improving the device's current injection efficiency and reducing the operating voltage, providing a technical solution for the fabrication of high-performance vertical structure Micro-LED devices that combines electrical advantages, optical advantages, and process feasibility.
[0110] In some alternative implementations, the material of the first semiconductor layer 21 includes N-type gallium nitride, and the material of the second semiconductor layer 22 includes P-type gallium nitride.
[0111] In some alternative embodiments, the roughened structural surface is subjected to plasma treatment, including: oxygen plasma treatment of the roughened structural surface.
[0112] In some alternative implementations, such as Figure 10 As shown, after plasma treatment of the roughened structure surface, the process further includes: forming a metal interlayer 70 on the roughened structure surface; the metal interlayer 70 isomorphically covering the roughened structure; and the work function of the metal interlayer 70 is less than the electron affinity of the first semiconductor layer 21.
[0113] In some alternative implementations, such as Figure 11 As shown, forming a first ohmic contact layer 31 on the roughened structure surface includes: forming a first ohmic contact layer 31 on the surface of the metal interlayer 70; annealing the first ohmic contact layer 31 to form an ohmic contact between the first ohmic contact layer 31 and the first semiconductor layer 21; and the first ohmic contact layer 31 forming an ohmic contact with the first semiconductor layer 21 through the metal interlayer 70.
[0114] In practice, the first ohmic contact layer 31 fills the gaps in the roughened structure, and the surface of the first ohmic contact layer 31 is planar.
[0115] The method for fabricating a light-emitting chip provided in this embodiment regulates the surface states, defect structures, and interface defects of the roughened surface through oxygen plasma treatment. The work function of the metal interlayer is less than the electron affinity of the first semiconductor layer, which helps to reduce the interface barrier between the first semiconductor layer and the subsequently formed metal interlayer and promotes carrier tunneling transport. After forming a first ohmic contact layer on the surface of the metal interlayer, the first ohmic contact layer is annealed, which can promote the formation of a stable ohmic contact between the first ohmic contact layer and the first semiconductor layer through the metal interlayer and reduce the contact resistivity.
[0116] In some alternative embodiments, the intermediate wafer also includes a second ohmic contact layer 32 located between the second semiconductor layer 22 and the substrate layer 10.
[0117] In some alternative embodiments, during the annealing process of the first ohmic contact layer 31, the annealing process can also enable the second ohmic contact layer 32 to form an ohmic contact with the second semiconductor layer 22.
[0118] In some alternative implementations, the annealing temperature is 150~300°C.
[0119] In some alternative embodiments, an intermediate wafer is provided, including: providing an epitaxial layer formed on a growth substrate 90, the epitaxial layer comprising a first semiconductor layer 21, an active layer 23, and a second semiconductor layer 22 sequentially stacked, wherein the first semiconductor layer 21 is relatively close to the growth substrate 90, such as... Figure 5 As shown; a second ohmic contact layer 32 is formed on the surface of the epitaxial layer facing away from the growth substrate layer 90, and a second metal bonding layer 82 is formed on the surface of the second ohmic contact layer 32 facing away from the epitaxial layer, as shown. Figure 6 As shown; a base layer 10 with a first metal bonding layer 81 formed on its surface is provided, such as Figure 7 As shown; the first metal bonding layer 81 and the second metal bonding layer 82 are bonded to bond the epitaxial layer to the substrate layer 10; the growth substrate layer 90 is removed by laser lift-off; the surface of the first semiconductor layer 21 exposed after the removal of the growth substrate layer 90 is thinned, as shown. Figure 8 As shown.
[0120] The method for fabricating a light-emitting chip provided in this embodiment involves transferring an epitaxial layer to a substrate layer via metal bonding and removing the growth substrate layer 90 by laser lift-off to obtain an intermediate wafer with the first semiconductor layer facing the light-emitting side. Thinning treatment exposes the surface of the first semiconductor layer and achieves the target thickness, providing a basis for subsequent roughening treatment and the formation of electrodes and transmission lines.
[0121] In some alternative embodiments, an epitaxial layer formed on the growth substrate 90 is provided, including: forming an epitaxial layer on the growth substrate 90 by epitaxial growth, the epitaxial layer including a buffer epitaxial layer 91, a first semiconductor layer 21, an active layer 23 and a second semiconductor layer 22 stacked sequentially.
[0122] In practice, the growth substrate 90 is made of aluminum oxide (i.e., sapphire). The buffer epitaxial layer 91 is an unintentionally doped gallium nitride buffer layer, the first semiconductor layer 21 is made of N-type gallium nitride, the active layer 23 is a multi-quantum well layer, and the second semiconductor layer 22 is made of P-type gallium nitride.
[0123] In some alternative embodiments, after removing the growth substrate layer 90 by laser lift-off, the method further includes removing the buffer epitaxial layer 91.
[0124] In some alternative implementations, such as Figure 12A and Figure 12B As shown, after the first ohmic contact layer 31 and the epitaxial layer are patterned, the epitaxial structure 20 and the second ohmic contact layer 32 exposed on its side form a stepped structure; the surface of the second ohmic contact layer 32 exposed on the side of the epitaxial structure 20 is a mesa; the mesa is located in the edge region 102.
[0125] In practice, the etching of the patterned processing stops on the surface of the second ohmic contact layer 32, the epitaxial layer retained in the light-emitting region 101 forms a protruding epitaxial structure 20, the surface of the second ohmic contact layer 32 in the edge region 102 is exposed to form a mesa, and the epitaxial structure 20 and the mesa together form a stepped structure.
[0126] In some alternative implementations, a wafer may include multiple light-emitting structures, and from a top view, the epitaxial structures 20 of the multiple light-emitting chips are arranged in a multi-array configuration.
[0127] In some optional embodiments, before forming the first electrode 201 on the surface of the first ohmic contact layer 31, the method further includes: forming a passivation layer 40, which covers a portion of the surface of the epitaxial structure 20 facing away from the substrate layer 10 and the sidewalls of the epitaxial structure 20, and covers the surface of the second ohmic contact layer 32 exposed on the side of the epitaxial structure 20, such as... Figure 13 As shown; a first via 41 and a second via 42 are formed within the passivation layer 40. The first via 41 exposes the first ohmic contact layer 31, and the second via 42 exposes the second ohmic contact layer 32, as shown. Figure 14 As shown.
[0128] In specific implementation, the first via 41 defines a contact window leading to the first ohmic contact layer 31, facilitating the electrical connection between the first electrode 201 and one side of the light-emitting area 101; the second via 42 defines a contact window leading to the second ohmic contact layer 32. Since the second ohmic contact layer 32 is electrically connected to the second conductive layer, an electrical connection with the second conductive layer on the bottom of the chip can be achieved through the second via 42. The position and number of the first via 41 and the second via 42 can be set according to the electrode layout, and this embodiment does not limit this.
[0129] The method for fabricating a light-emitting chip provided in this embodiment involves an epitaxial structure formed after patterning and a second ohmic contact layer forming a stepped structure. A passivation layer covers the surface of the stepped structure to provide protection and isolation. The first via and the second via respectively define contact windows leading to the first ohmic contact layer and the second ohmic contact layer, providing accurate contact positions for the formation of the first electrode and the second electrode.
[0130] In some alternative embodiments, in the steps of forming a first electrode 201 on the surface of the first ohmic contact layer 31 and forming a first transmission line structure 301 in the edge region 102 on the side of the first electrode 201, the first transparent conductive layer 51 in the first electrode 201 fills the first via 41 and connects to the first ohmic contact layer 31.
[0131] In some optional embodiments, the step of forming a first electrode 201 on the surface of the first ohmic contact layer 31 and forming a first transmission line structure 301 in the edge region 102 on the side of the first electrode 201 further includes: forming a second electrode 202 on the surface of the second ohmic contact layer 32 and forming a second transmission line structure 302 in the edge region 102 on the side of the second electrode 202; the second electrode 202 includes a second transparent conductive layer 52 and a second metal layer 62 stacked together; the second transparent conductive layer 52 in the second electrode 202 fills the second via 42 and connects to the second ohmic contact layer 32.
[0132] The method for fabricating a light-emitting chip provided in this embodiment involves forming the first electrode, the first transmission line structure, and the second electrode and the second transmission line structure in the same process system. The first transparent conductive layer in the first electrode fills the first via and is connected to the first ohmic contact layer, and the second transparent conductive layer in the second electrode fills the second via and is connected to the second ohmic contact layer. The process is simple, efficient, and has good process compatibility and feasibility.
[0133] In some optional embodiments, the process of forming the first electrode 201, the first transmission line structure 301, the second electrode 202, and the second transmission line structure 302 includes the following steps: S1. Delineating a predetermined region for the first electrode 201, a predetermined region for the first transmission line, a predetermined region for the second electrode 202, and a predetermined region for the second transmission line on the surface of the passivation layer 40; the predetermined region for the first electrode 201 is located in the light-emitting region 101, and the predetermined regions for the first transmission line, the second electrode 202, and the second transmission line are located in the edge region 102. S2. Forming a first transparent conductive layer 51 in the predetermined regions for the first electrode 201 and the first transmission line, and forming a second transparent conductive layer 52 in the predetermined regions for the second electrode 202 and the second transmission line; wherein, the first transparent conductive layer 51 located within the light-emitting region 101 and in the predetermined region for the first electrode 201 serves as the first electrode 201, such as... Figure 15A and Figure 15B As shown. S3, a first metal layer 61 is formed on the surface of the first transparent conductive layer 51 in the preset region of the first transmission line, and a second metal layer 62 is formed on the surface of the second transparent conductive layer 52; the first transparent conductive layer 51 and the first metal layer 61 in the preset region of the first transmission line constitute the first transmission line structure 301; the second transparent conductive layer 52 and the second metal layer 62 in the preset region of the second transmission line constitute the second transmission line structure 302; the second transparent conductive layer 52 and the second metal layer 62 in the preset region of the second electrode 202 constitute the second electrode 202, as shown. Figure 16A and Figure 16B As shown.
[0134] like Figure 4 As shown, the present invention also provides a specific flowchart of a method for preparing a light-emitting chip, including but not limited to steps S201 to S213.
[0135] Step S201: Provide an epitaxial layer formed on the growth substrate 90. The epitaxial layer includes a first semiconductor layer 21, an active layer 23, and a second semiconductor layer 22 stacked sequentially, wherein the first semiconductor layer 21 is relatively close to the growth substrate 90, such as... Figure 5 As shown.
[0136] In practice, an epitaxial layer is formed by epitaxial growth on the growth substrate layer 90. In some examples, such as Figure 5As shown, a complete epitaxial layer can be formed on a sapphire substrate 90 by sequentially growing a buffer epitaxial layer 91, a first semiconductor layer 21, an active layer 23, and a second semiconductor layer 22 using a metal-organic chemical vapor deposition (MOCVD) process. The buffer epitaxial layer 91 is an unintentionally doped gallium nitride buffer layer (u-GaN), the first semiconductor layer 21 is made of N-type gallium nitride (N-GaN), the active layer 23 is a multiple quantum well layer, and the second semiconductor layer 22 is made of P-type gallium nitride (P-GaN). The thickness of the buffer epitaxial layer 91 is 3.7 μm, and the thickness of the first semiconductor layer 21 is 1.6 μm.
[0137] Step S202: A second ohmic contact layer 32 is formed on the side of the epitaxial layer facing away from the growth substrate layer 90, and a first metal bonding layer 81 is formed on the side of the second ohmic contact layer 32 facing away from the epitaxial layer, such as... Figure 6 As shown.
[0138] In specific implementations, the material of the second ohmic contact layer 32 includes indium tin oxide, and the thickness of the second ohmic contact layer 32 is 100~200 nm. In some examples, 150 nm of indium tin oxide is deposited on the surface of the first semiconductor layer 21 by magnetron sputtering as the second ohmic contact layer 32. The material of the first metal bonding layer 81 includes gold; optionally, metallic gold is deposited on the surface of the second ohmic contact layer 32 by electron beam evaporation as the first metal bonding layer 81.
[0139] Step S203, providing a base layer 10 with a second metal bonding layer 82 formed on its surface, such as Figure 7 As shown.
[0140] In a specific implementation, the material of the substrate 10 includes silicon, and the material of the second metal bonding layer 82 includes tin; optionally, metallic tin is deposited on the surface of the silicon substrate 10 by an electron beam evaporation process as the second metal bonding layer 82.
[0141] Step S204: The first metal bonding layer 81 and the second metal bonding layer 82 are bonded to bond the epitaxial layer to the substrate layer 10; the growth substrate layer 90 is removed by laser lift-off; the surface of the first semiconductor layer 21 exposed after the removal of the growth substrate layer 90 is thinned to obtain an intermediate wafer, such as... Figure 8 As shown.
[0142] In specific implementation, firstly, the first metal bonding layer 81 and the second metal bonding layer 82 are brought into contact and bonded using a bonding machine, so that the epitaxial layer is bonded to the substrate layer 10. The first metal bonding layer 81 and the second metal bonding layer 82 form a bonding layer 80, which is located between the second ohmic contact layer 32 and the substrate layer 10. Then, the growth substrate layer 90 is removed using an Nd:YAG laser through a laser lift-off process. Finally, the surface of the first semiconductor layer 21 is polished using a chemical mechanical polishing (CMP) process, and the polished surface of the first semiconductor layer 21 is thinned to 1.2 μm using inductively coupled plasma (ICP) etching, resulting in the desired layer. Figure 8 The intermediate wafer shown is formed by sequentially stacking a base layer 10, a second ohmic contact layer 32, and an epitaxial layer. The epitaxial layer includes a second semiconductor layer 22, an active layer 23, and a first semiconductor layer 21, which are sequentially stacked, wherein the second semiconductor layer 22 is in contact with the second ohmic contact layer 32. The intermediate wafer includes a light-emitting region 101 and an edge region 102; the epitaxial layer is located in the light-emitting region 101 and the edge region 102. It should be noted that the thickness after thinning can be adjusted according to the device design. This embodiment does not limit this, and 1.2 μm is used as an example for illustration.
[0143] Step S205: Roughen the surface of the first semiconductor layer 21 on the side facing away from the active layer 23 to form a roughened structure, such as... Figure 9 As shown.
[0144] In specific implementation, a potassium hydroxide (KOH) solution is used to wet-etch the surface of the first semiconductor layer 21. After etching, a dense, roughened structure is formed on the surface of the first semiconductor layer 21. The roughened structure includes multiple hexagonal pyramidal protrusions 211, and the crystal plane changes from (000-1) to (10-1-1). Figure 9 As shown. In some examples, the width of the protrusion structure 211 is 50~300nm; the height of the protrusion structure 211 is 50~300nm. It should be noted that the roughening treatment can also be achieved by other surface treatment methods that can form the protrusion structure 211 on the surface. This embodiment does not limit the specific method of roughening treatment. The roughened structure increases the interface contact area and improves the light emission path. At the same time, the transformation of the crystal plane is beneficial to the subsequent formation of ohmic contacts.
[0145] Step S206: Perform oxygen plasma treatment on the roughened surface structure.
[0146] In practice, the roughened surface is treated with oxygen plasma (O2Plasma) to modulate the surface states, defect structures, and interfacial bands, thereby reducing the interfacial barrier and promoting carrier tunneling transport. In some examples, the oxygen plasma treatment process conditions are: time 2–10 min, power 30–300 W. It should be noted that the process parameters for plasma treatment can be adjusted according to the surface condition; this embodiment does not limit this.
[0147] Step S207: A metal interlayer 70 is formed on the surface of the roughened structure. The metal interlayer 70 conformally covers the roughened structure, such as... Figure 10 As shown, the work function of the metal interlayer 70 is less than the electron affinity of the first semiconductor layer 21.
[0148] In specific implementations, the material of the metal interlayer 70 includes titanium or indium, and the thickness of the metal interlayer 70 is 3~10nm. In some examples, the material of the metal interlayer 70 includes titanium, and the thickness of the metal interlayer 70 is 3nm; a 3nm thick titanium metal is formed on the roughened structure surface as the metal interlayer 70 through a thermal evaporation process.
[0149] Step S208: Form a first ohmic contact layer 31 on the surface of the metal interlayer 70, such as... Figure 11 As shown, the first ohmic contact layer 31 is annealed to form an ohmic contact with the first semiconductor layer 21; the first ohmic contact layer 31 forms an ohmic contact with the first semiconductor layer 21 through the metal interlayer 70.
[0150] In specific implementations, annealing can also enable the second ohmic contact layer 32 to form an ohmic contact with the second semiconductor layer 22. The material of the first ohmic contact layer 31 includes indium tin oxide, and the thickness of the first ohmic contact layer 31 includes 50~200 nm. The annealing temperature is 150~300℃. In some examples, firstly, indium tin oxide with a thickness of 150 nm is deposited on the surface of the metal interlayer 70 by magnetron sputtering as the first ohmic contact layer 31; then, annealing is performed at 150~300℃ to enable the first ohmic contact layer 31 to form an ohmic contact with the first semiconductor layer 21, and the second ohmic contact layer 32 can also form an ohmic contact with the second semiconductor layer 22, resulting in... Figure 11 The structure is shown. The annealing temperature can be adjusted according to the material system. In this embodiment, the annealing temperature is not limited. Here, annealing at 200℃ is used as an example for explanation.
[0151] Step S209: The first ohmic contact layer 31, the metal interlayer 70, and the epitaxial layer are patterned. The first ohmic contact layer 31 and the epitaxial layer in the edge region 102 are removed, while the first ohmic contact layer 31 and the epitaxial layer in the light-emitting region 101 are retained. The remaining epitaxial layer in the light-emitting region 101 serves as the epitaxial structure 20. The epitaxial structure 20 and the second ohmic contact layer 32 exposed on its side form a stepped structure. The surface of the second ohmic contact layer 32 exposed on the side of the epitaxial structure 20 is a mesa. The mesa is located in the edge region 102, such as... Figure 12A and Figure 12B As shown.
[0152] In practice, firstly, a first photoresist pattern corresponding to the epitaxial structure is obtained through photolithography. The photoresist in the second photoresist pattern covers the first ohmic contact layer of the light-emitting region, exposing the first ohmic contact layer in the edge region. Then, the first ohmic contact layer 31, the metal interlayer 70, and the epitaxial layer in the areas not covered by the photoresist pattern are removed by inductively coupled plasma (ICP) etching, obtaining the mesa structure located in the light-emitting region 101. Afterward, the wafer is immersed in a resist remover solution and subjected to ultrasonic treatment for 10 minutes to remove the photoresist pattern on the wafer, resulting in the structure shown below. Figure 12A and Figure 12B The structure is shown. It should be noted that the ultrasonic time can be adjusted according to the adhesive removal effect, but this embodiment does not limit this.
[0153] Step S210: Form a passivation layer 40. The passivation layer 40 covers a portion of the surface of the epitaxial structure 20 facing away from the substrate layer 10 and the sidewalls of the epitaxial structure 20, and covers the surface of the second ohmic contact layer 32 exposed on the side of the epitaxial structure 20. A first via 41 and a second via 42 are formed within the passivation layer 40. The first via 41 exposes the first ohmic contact layer 31, and the second via 42 exposes the second ohmic contact layer 32, as shown below. Figure 13 and Figure 14 As shown.
[0154] In specific implementation, firstly, a 2700 Å silicon dioxide layer 40 is deposited as a passivation layer 40 using plasma-enhanced chemical vapor deposition (PECVD). The passivation layer 40 covers the surface of the stepped structure. Subsequently, a second photoresist pattern is formed on the surface of the passivation layer 40 by photolithography. Then, a first via 41 and a second via 42 penetrating the passivation layer 40 are etched within the passivation layer 40 by inductively coupled plasma (ICP) etching. The first via 41 is located above the epitaxial structure 20 and exposes the first ohmic contact layer 31, while the second via 42 is located on the mesa on the side of the epitaxial structure 20 and exposes the second ohmic contact layer 32. Finally, the wafer is immersed in a resist remover and ultrasonically removed for 10 minutes to obtain the desired result. Figure 14 The structure shown.
[0155] Step S211: Divide the surface of the passivation layer 40 into a first electrode preset region, a first transmission line preset region, a second electrode preset region, and a second transmission line preset region; the first electrode preset region is located in the light-emitting region 101, and the first transmission line preset region, the second electrode preset region, and the second transmission line preset region are located in the edge region 102.
[0156] In specific implementation, a third photoresist pattern corresponding to the first electrode 201, the second electrode 202, the first transmission line structure 301, and the second transmission line structure 302 is obtained through photolithography. The third photoresist pattern exposes the preset regions of the first electrode, the first transmission line, the second electrode, and the second transmission line. The preset regions of the first electrode and the first transmission line are continuous regions, and the preset regions of the second electrode 202 and the second transmission line are also continuous regions.
[0157] Step S212: A first transparent conductive layer 51 is formed in the first electrode preset region and the first transmission line preset region; a second transparent conductive layer 52 is formed in the second electrode preset region and the second transmission line preset region. The first transparent conductive layer 51 in the first electrode preset region fills the first via 41 and connects to the first ohmic contact layer 31; the second transparent conductive layer 52 in the second electrode preset region fills the second via 42 and connects to the second ohmic contact layer 32. The first transparent conductive layer 51 located in the light-emitting region 101 serves as the first electrode 201. Figure 15A and Figure 15B As shown.
[0158] In specific implementation, both the first transparent conductive layer 51 and the second transparent conductive layer 52 are made of indium tin oxide (ITO). ITO of 150 nm is deposited on the surface of the passivation layer 40 by magnetron sputtering, simultaneously forming the first transparent conductive layer 51 and the second transparent conductive layer 52. The first transparent conductive layer 51, within a predetermined region of the first electrode 201, covers the first ohmic contact layer 31, serving as the first electrode 201 and reducing the electrode's obstruction of light emission from the chip. Simultaneously, the first transparent conductive layer 51 extends to cover a predetermined region of the first transmission line, serving as the first transparent conductive layer 51 within the first transmission line structure 301. A continuous second transparent conductive layer 52 is simultaneously formed in the predetermined regions of the second electrode 202 and the second transmission line. Finally, the wafer is immersed in a resist remover and ultrasonically treated for 10 minutes to remove the third photoresist pattern, resulting in the desired image. Figure 15A and Figure 15B The structure shown.
[0159] Step S213: A first metal layer 61 is formed on the surface of the first transparent conductive layer 51 in the preset region of the first transmission line, and a second metal layer 62 is formed on the surface of the second transparent conductive layer 52; the first transparent conductive layer 51 and the first metal layer 61 in the preset region of the first transmission line constitute the first transmission line structure 301; the second transparent conductive layer 52 and the second metal layer 62 in the preset region of the second transmission line constitute the second transmission line structure 302; the second transparent conductive layer 52 and the second metal layer 62 in the preset region of the second electrode constitute the second electrode 202, as shown below. Figure 16A and Figure 16B As shown.
[0160] In specific implementation, both the first metal layer 61 and the second metal layer 62 are made of gold. First, a fourth photoresist pattern corresponding to the second electrode 202, the first transmission line structure 301, and the second transmission line structure 302 is obtained through laser direct writing exposure. The fourth photoresist pattern exposes the preset areas of the first transmission line, the second electrode, and the second transmission line; that is, the light-emitting area 101 retains the photoresist pattern, while the electrode and transmission line preset areas within the edge area 102 are without photoresist. Subsequently, 750nm of metallic gold is deposited by electron beam evaporation as the first metal layer 61 and the second metal layer 62. The first metal layer 61 covers the first transparent conductive layer 51 located in the edge area 102, and the second metal layer 62 covers the second transparent conductive layer 52. This avoids voltage drop when the transparent conductive layer acts as a transmission line alone and enhances the mechanical strength and ductility of the transmission line. Finally, most of the photoresist and its metal are removed by applying and removing high-temperature adhesive tape. The wafer is then immersed in a resist remover solution and ultrasonically treated for 10 minutes to remove residual photoresist, resulting in the desired image. Figure 16A and Figure 16B The light-emitting chip shown is an example. It should be noted that laser direct writing exposure can also be replaced by electron beam exposure for pattern exposure and development; the deposition of metallic gold can also be achieved using magnetron sputtering or thermal evaporation deposition systems. This embodiment does not limit the exposure method or the metal deposition method.
[0161] like Figure 16A and Figure 16BAs shown, in the formed light-emitting structure, the first electrode 201 is located within the light-emitting region 101, and the first transmission line structure 301 is located within the edge region 102 on the side of the first electrode 201. The first electrode 201 includes a first transparent conductive layer 51. The first transmission line structure 301 includes a first transparent conductive layer 51 and a first metal layer 61 stacked together, wherein the first metal layer 61 is located on the side of the first transparent conductive layer 51 facing away from the substrate layer 10. The first transparent conductive layer 51 in the first electrode 201 is connected to the first transparent conductive layer 51 in the first transmission line structure 301. Therefore, the first transparent conductive layer 51 in the first electrode 201 and the first transparent conductive layer 51 in the first transmission line structure 301 are the same layer that is continuously extended and formed in a single film deposition. The second transparent conductive layer 52 in the second electrode 202 and the second transparent conductive layer 52 in the second transmission line structure 302 are the same layer that is continuously extended and formed in a single film deposition. The second metal layer 62 in the second electrode 202 and the second metal layer 62 in the second transmission line structure 302 are the same layer that is continuously extended and formed in a single film deposition.
[0162] The process method provided in this embodiment is simple, efficient, and has good process compatibility and feasibility. Compared with the traditional complex multilayer transparent electrode fabrication process, this embodiment only requires adding a laser direct writing process to the existing technology process to realize the construction of the composite electrode structure, thus simultaneously possessing the low resistance characteristics of metal electrodes and the high light transmittance characteristics of ITO transparent electrodes.
[0163] It should be noted that the light-emitting chip and its fabrication method provided in this embodiment can be applied to various vertically structured light-emitting diode devices, such as high-resolution Micro-LED and Mini-LED display devices.
[0164] In the description of this specification, the references to terms such as "this embodiment," "an embodiment," "some embodiments," "example," "specific example," or "some examples," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example, which are included in at least one embodiment or example of the present invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples. Furthermore, those skilled in the art can combine and integrate the different embodiments or examples described in this specification and the features of different embodiments or examples without contradiction. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of the present invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0165] The above description does not provide detailed explanations of the technical aspects of each layer's patterning, etching, etc. However, those skilled in the art should understand that various technical means can be used to form layers and regions of the desired shape. Furthermore, to form the same structure, those skilled in the art can also design methods that are not entirely identical to those described above. Additionally, although various embodiments have been described above, this does not mean that the measures in the various embodiments cannot be used advantageously in combination.
[0166] The above description is merely a preferred embodiment of the present invention and the technical principles employed. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described above, and various obvious changes, readjustments, combinations, and substitutions can be made without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in detail through the above embodiments, the present invention is not limited to the above embodiments, and may include many other equivalent embodiments without departing from the concept of the present invention. The scope of protection of the present invention is determined by the scope of the appended claims.
Claims
1. A light-emitting chip, characterized in that, include: The base layer includes a light-emitting region and an edge region located on the side of the light-emitting region; An epitaxial structure, located on the surface of the substrate layer, includes a second semiconductor layer, an active layer, and a first semiconductor layer stacked sequentially, wherein the second semiconductor layer is relatively close to the substrate layer; the epitaxial structure is located in the light-emitting region; a roughened structure is provided on the side surface of the first semiconductor layer facing away from the active layer; A first ohmic contact layer is located on the surface of the roughened structure; The first ohmic contact layer forms an ohmic contact with the first semiconductor layer; A first electrode is located on the side surface of the first ohmic contact layer opposite to the first semiconductor layer; the first electrode is located in the light-emitting region; the first electrode includes a first transparent conductive layer. A first transmission line structure is located in the edge region on the side of the first electrode. The first transmission line structure includes a first transparent conductive layer and a first metal layer stacked together, wherein the first metal layer is located on the side of the first transparent conductive layer facing away from the substrate layer; the first transparent conductive layer in the first electrode is connected to the first transparent conductive layer in the first transmission line structure.
2. The light-emitting chip according to claim 1, characterized in that, The first semiconductor layer is an N-type semiconductor layer, and the second semiconductor layer is a P-type semiconductor layer.
3. The light-emitting chip according to claim 2, characterized in that, The light-emitting chip further includes: a metal interlayer located between the roughened structure and the first ohmic contact layer; the work function of the metal interlayer is less than the electron affinity of the first semiconductor layer; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer through the metal interlayer.
4. The light-emitting chip according to claim 3, characterized in that, The material of the first semiconductor layer includes N-type gallium nitride, and the material of the second semiconductor layer includes P-type gallium nitride; The metal interlayer is made of titanium or indium; the thickness of the metal interlayer is 3~10nm; the metal interlayer conformally covers the roughened structure. The light transmittance of the metal interlayer is greater than 80%.
5. The light-emitting chip according to claim 1, characterized in that, The coarsening structure includes multiple arrayed protrusions, and the protrusions are pyramidal in shape. The width of the protrusion structure is 50~300nm; the height of the protrusion structure is 40~300nm.
6. The light-emitting chip according to claim 2, characterized in that, The light-emitting chip also includes: A second ohmic contact layer is located between the second semiconductor layer and the substrate layer; the second ohmic contact layer covers the substrate layer and is located in both the light-emitting region and the edge region; the second ohmic contact layer forms an ohmic contact with the second semiconductor layer; the epitaxial structure forms a stepped structure with the second ohmic contact layer; the surface of the second ohmic contact layer exposed on the side of the epitaxial structure is a mesa; the mesa is located in the edge region; The second electrode is located on the mesa of the epitaxial structure. The second electrode includes a second transparent conductive layer and a second metal layer stacked together. The second metal layer is located on the side of the second transparent conductive layer that is opposite to the second ohmic contact layer. The second transmission line structure is located on the side of the second electrode away from the epitaxial structure. The second transmission line structure includes a second transparent conductive layer and a second metal layer stacked together. The second transparent conductive layer in the second electrode is connected to the second transparent conductive layer in the second transmission line structure, and the second metal layer in the second electrode is connected to the second metal layer in the second transmission line structure.
7. The light-emitting chip according to claim 6, characterized in that, The light-emitting chip further includes: a passivation layer covering a portion of the surface of the epitaxial structure facing away from the substrate layer and the sidewall of the epitaxial structure, and covering the surface of the second ohmic contact layer exposed on the side of the epitaxial structure; The first electrode penetrates the passivation layer and is connected to the first ohmic contact layer; The second transparent conductive layer in the second electrode penetrates the passivation layer and is connected to the second ohmic contact layer.
8. The light-emitting chip according to claim 6, characterized in that, The first transparent conductive layer in the first electrode and the first transparent conductive layer in the first transmission line structure are the same layer that extends continuously. The second transparent conductive layer in the second electrode and the second transparent conductive layer in the second transmission line structure are the same layer that extends continuously; the second metal layer in the second electrode and the second metal layer in the second transmission line structure are the same layer that extends continuously. Both the first ohmic contact layer and the second ohmic contact layer are made of indium tin oxide. Both the first transparent conductive layer and the second transparent conductive layer are made of indium tin oxide. Both the first metal layer and the second metal layer are made of gold.
9. A method for fabricating a light-emitting chip, characterized in that, The preparation method includes: An intermediate wafer is provided; the intermediate wafer includes a base layer and an epitaxial layer located on the surface of the base layer, which are stacked sequentially; the epitaxial layer includes a second semiconductor layer, an active layer and a first semiconductor layer stacked sequentially, wherein the second semiconductor layer is relatively close to the base layer; the intermediate wafer includes a light-emitting region and an edge region; the epitaxial layer is located in the light-emitting region and the edge region; The surface of the first semiconductor layer facing away from the active layer is roughened to form a roughened structure; The roughened surface is subjected to plasma treatment; A first ohmic contact layer is formed on the surface of the roughened structure; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer; The first ohmic contact layer and the epitaxial layer are patterned, and the first ohmic contact layer and the epitaxial layer in the edge region are removed, while the first ohmic contact layer and the epitaxial layer in the light-emitting region are retained; the remaining epitaxial layer in the light-emitting region is used as an epitaxial structure. A first electrode is formed on the surface of the first ohmic contact layer, and a first transmission line structure is formed in the edge region of the side of the first electrode; the first electrode includes a first transparent conductive layer; the first transmission line structure includes a first transparent conductive layer and a first metal layer stacked together, wherein the first metal layer is located on the side of the first transparent conductive layer facing away from the substrate layer; the first transparent conductive layer in the first electrode is connected to the first transparent conductive layer in the first transmission line structure.
10. The method for preparing a light-emitting chip according to claim 9, characterized in that, The plasma treatment of the roughened structural surface includes: oxygen plasma treatment of the roughened structural surface; After plasma treatment of the roughened structure surface, the method further includes: forming a metal interlayer on the roughened structure surface; the metal interlayer conformally covering the roughened structure; the work function of the metal interlayer being less than the electron affinity of the first semiconductor layer. The formation of the first ohmic contact layer on the roughened structure surface includes: The first ohmic contact layer is formed on the surface of the metal interlayer; The first ohmic contact layer is annealed to form an ohmic contact with the first semiconductor layer; the first ohmic contact layer forms an ohmic contact with the first semiconductor layer through the metal interlayer.
11. The method for preparing a light-emitting chip according to claim 9, characterized in that, The intermediate wafer also includes a second ohmic contact layer located between the second semiconductor layer and the substrate layer; The provision of the intermediate wafer includes: An epitaxial layer is provided formed on a growth substrate, the epitaxial layer comprising a first semiconductor layer, an active layer and a second semiconductor layer stacked sequentially, wherein the first semiconductor layer is relatively close to the growth substrate. A second ohmic contact layer is formed on the side surface of the epitaxial layer opposite to the growth substrate, and a first metal bonding layer is formed on the side surface of the second ohmic contact layer opposite to the epitaxial layer. A base layer having a second metal bonding layer formed on its surface is provided; The first metal bonding layer is bonded to the second metal bonding layer to bond the epitaxial layer to the substrate layer; The grown substrate layer is removed by laser ablation; The surface of the first semiconductor layer exposed after the growth substrate is removed is thinned.
12. The method for preparing a light-emitting chip according to claim 11, characterized in that, After patterning the first ohmic contact layer and the epitaxial layer, the epitaxial structure and the second ohmic contact layer exposed on its side form a stepped structure; the surface of the second ohmic contact layer exposed on the side of the epitaxial structure is a mesa. The platform is located in the edge region; Before forming the first electrode on the surface of the first ohmic contact layer, the method further includes: A passivation layer is formed, which covers a portion of the surface of the epitaxial structure facing away from the substrate layer and the sidewalls of the epitaxial structure, and covers the surface of the second ohmic contact layer exposed on the side of the epitaxial structure; A first via and a second via are formed within the passivation layer, wherein the first via exposes the first ohmic contact layer and the second via exposes the second ohmic contact layer.
13. The method for preparing a light-emitting chip according to claim 12, characterized in that, In the step of forming a first electrode on the surface of the first ohmic contact layer and forming a first transmission line structure in the edge region of the side of the first electrode, the first transparent conductive layer in the first electrode fills the first via and connects with the first ohmic contact layer. The step of forming a first electrode on the surface of the first ohmic contact layer and forming a first transmission line structure in the edge region of the side of the first electrode further includes: A second electrode is formed on the surface of the second ohmic contact layer, and a second transmission line structure is formed in the edge region of the side of the second electrode; The second electrode includes a second transparent conductive layer and a second metal layer stacked together; the second transparent conductive layer in the second electrode fills the second via and connects to the second ohmic contact layer.