A display structure and its preparation method

By adjusting the thickness ratio and material refractive index difference in the transparent adjustment layer, a high-performance strong microcavity effect of silicon-based OLED microcavity structure was achieved, solving the problems of process compatibility and electrical inhomogeneity in traditional cavity adjustment schemes, and improving display performance and device stability.

CN123124638APending Publication Date: 2026-11-17NANJING LUMICORE TECH LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611404083.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-10
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing silicon-based OLED microcavity structures cannot simultaneously meet the requirements of pixel electrical consistency and high color purity. Conventional cavity tuning solutions suffer from poor process compatibility, uneven electrical properties of the three colors, weak microcavity effect, and low color purity.

Method used

By adopting the principle that the total physical thickness of each sub-pixel in the transparent adjustment layer is the same, and by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, the optical cavity length of each sub-pixel can be controlled by utilizing the fixed refractive index difference of each adjustment layer material, so as to match the resonant wavelength of blue light, green light and red light, and construct a high-performance strong microcavity structure.

Benefits of technology

It achieves a consistent total physical thickness of the transparent adjustment layer for the three-color sub-pixels, ensuring the flatness and electrical consistency of the pixel film layer, adapting to CMOS lithography mass production processes, improving microcavity effect and color purity, significantly enhancing display performance and device stability, and reducing large-viewpoint character drift.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124638A_ABST
    Figure CN123124638A_ABST
Patent Text Reader

Abstract

This invention discloses a display structure and its fabrication method, comprising: a silicon-based CMOS backplane, a metal anode layer, a transparent adjustment layer, an organic functional layer, and a semi-transparent cathode stacked together to form a closed optical resonant cavity; wherein the transparent adjustment layer includes at least a first adjustment layer and a second adjustment layer; the total physical thickness of each sub-pixel in the transparent adjustment layer is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, and utilizing the fixed refractive index difference of each adjustment layer material, the optical cavity length of each sub-pixel can be controlled to match the resonant wavelengths of blue, green, and red light. This solves the problems of poor process compatibility, uneven electrical properties of the three colors, weak microcavity effect, and low color purity in traditional cavity adjustment schemes. It is suitable for high-end silicon-based OLED display scenarios such as AR / VR, ultra-high color gamut micro-displays, and near-eye displays.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of display technology, and in particular to a display structure and its fabrication method. Background Technology

[0002] Silicon-based top-emission OLEDs have become a core technology for near-eye displays in AR / VR due to their advantages of high PPI, high brightness, and high contrast. Top-emission OLEDs rely on the Fabry-Perot (FP) microcavity resonance effect to achieve spectral narrowing, brightness gain, and high color gamut display. In the industry, microcavities with a spectral half-width at half-maximum (FWHM) of <30nm and a light intensity gain >3 times are defined as strong microcavity structures, which are the core indicators of high-end silicon-based microdisplays.

[0003] Existing silicon-based OLED microcavity tuning solutions are mainly divided into two types: The first type is organic layer differential thickness tuning, which matches the resonant wavelength by adjusting the thickness of the organic functional layer of the RGB sub-pixels. However, changes in the organic layer thickness directly affect the carrier transport efficiency, device turn-on voltage, and luminous efficiency, resulting in uneven electrical properties and large differences in lifetime among the three-color pixels. The second type is anode-side single-layer transparent conductive oxide (TCO) cavity tuning, which achieves cavity length adjustment by etching to form different physical thicknesses. However, this method causes differences in the flatness of the sub-pixel film layer, narrow process window, low yield, and cannot balance optical performance and process compatibility.

[0004] Currently, the industry generally faces core technological bottlenecks: conventional silicon-based OLED micro-display cavity tuning solutions either employ differentiated cavity tuning of organic layers or differentiated thickness cavity tuning of a single-layer TCO, failing to simultaneously meet the two core requirements of "pixel electrical consistency" and "high color purity and strong microcavity effect." Single transparent conductive materials, limited by their fixed refractive index, cannot achieve precise matching of independent optical cavity lengths for the RGB three colors under the stringent process constraints of consistent physical thickness across all sub-pixels. This results in severe spectral broadening, insufficient color purity, and low brightness gain in conventional microcavity structures, failing to meet the mass production specifications for high-end strong microcavities. On the other hand, differentiated film thickness cavity tuning introduces defects such as poor pixel surface flatness, three-color electrical shift, severe wide-viewing-angle drift, and inconsistent aging, significantly limiting the color gamut, brightness, and lifespan limits of silicon-based OLEDs. Summary of the Invention

[0005] This invention provides a display structure and its fabrication method to solve the problems of poor process compatibility, uneven electrical properties of the three colors, weak microcavity effect, and low color purity in traditional cavity adjustment schemes.

[0006] In a first aspect, embodiments of the present invention provide a display structure, comprising: a silicon-based CMOS backplane, a metal anode layer, a transparent adjustment layer, an organic functional layer, and a semi-transparent cathode stacked together to form a closed optical resonant cavity; The transparent adjustment layer includes at least a first adjustment layer and a second adjustment layer; The total physical thickness of each sub-pixel in the transparent adjustment layer is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, the optical cavity length of each sub-pixel can be controlled by utilizing the fixed refractive index difference of each adjustment layer material, and the resonant wavelengths of blue light, green light and red light can be matched.

[0007] Optionally, the thickness of the transparent adjustment layer , Total physical thickness of each sub-pixel ; Total optical cavity length ; Interference level ; Cavity fineness ; Spectral half width at half maximum (FWHM) ; Light intensity gain ; Where n1 is the refractive index of the first adjustment layer and n2 is the refractive index of the second adjustment layer. The thickness of the first adjustment layer, The thickness of the second adjustment layer; The cavity length of the first adjustment layer, The cavity length of the second adjustment layer; R1 is the wavelength of light; R2 is the reflectivity of the metal anode layer; and R3 is the reflectivity of the semi-transparent cathode.

[0008] Optionally, the material of the first conditioning layer is indium tin oxide, and the material of the second conditioning layer is indium zinc oxide.

[0009] Optionally, the refractive index of the first adjustment layer is 1.8 to 2.0, and the refractive index of the second adjustment layer is 1.9 to 2.2.

[0010] Optionally, the reflectivity of the metal anode layer is ≥92%.

[0011] Optionally, the reflectivity of the semi-transparent cathode is 70-80%.

[0012] Optionally, the interference order of the transparent adjustment layer is between 1.2 and 1.8.

[0013] In a second aspect, embodiments of the present invention also provide a method for preparing a display structure, used to prepare the display structure described in the first aspect, comprising: Fabrication of a metal anode layer on a silicon-based CMOS backplane; A first conditioning layer is prepared on the metal anode layer; A second adjustment layer is fabricated on the first adjustment layer; An insulating layer is deposited on the metal anode layer; In this transparent adjustment layer, the total physical thickness of each sub-pixel is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, the optical cavity length of each sub-pixel can be controlled by utilizing the fixed refractive index difference of each adjustment layer material, thereby matching the resonant wavelengths of blue, green and red light.

[0014] Optionally, the material of the first conditioning layer is indium tin oxide, and the material of the second conditioning layer is indium zinc oxide; The preparation of the first conditioning layer on the metal anode layer includes: An indium tin oxide film is deposited on the metal anode layer, and a halftone mask is used for resist coating, exposure and development, and halftone mask etching to remove resist, so that different sub-pixels form indium tin oxide film layers of different thicknesses, thus obtaining the first adjustment layer. Fabricating a second adjustment layer on the first adjustment layer includes: An indium zinc oxide film is deposited on the first adjustment layer, and a halftone mask is used for resist coating, exposure and development, and halftone mask etching to remove resist, so that different sub-pixels form indium zinc oxide film layers of different thicknesses, and the total physical thickness of each sub-pixel is the same, thus obtaining the second adjustment layer.

[0015] Optionally, depositing an insulating layer on the metal anode layer includes: SiO2 is deposited on the metal anode layer to fill the gap.

[0016] This invention provides a display structure and its fabrication method, comprising: a silicon-based CMOS backplane, a metal anode layer, a transparent adjustment layer, an organic functional layer, and a semi-transparent cathode stacked together to form a closed optical resonant cavity; wherein, the transparent adjustment layer includes at least a first adjustment layer and a second adjustment layer; the total physical thickness of each sub-pixel in the transparent adjustment layer is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, the optical cavity length of each sub-pixel is controlled by utilizing the fixed refractive index difference of each adjustment layer material, thereby matching the resonant wavelengths of blue light, green light, and red light. In this transparent adjustment layer, all sub-pixels have the same total physical thickness. By adjusting the thickness ratio of each adjustment layer within the transparent adjustment layer and utilizing the fixed refractive index difference of each adjustment layer material, the optical cavity length of each sub-pixel can be controlled. This matches the resonant wavelengths of blue, green, and red light, ensuring that the total physical thickness of the transparent adjustment layers for the B / G / R sub-pixels is completely consistent. This guarantees pixel film flatness and electrical consistency, making it compatible with CMOS photolithography mass production processes. By differentially controlling the refractive index difference of the adjustment layer materials to match the RGB emission resonant wavelengths, a high-performance microcavity structure is constructed. This solves the problems of poor process compatibility, uneven electrical properties of the three colors, weak microcavity effect, and low color purity in traditional cavity adjustment schemes. It is suitable for high-end silicon-based OLED display scenarios such as AR / VR, ultra-high color gamut micro-displays, and near-eye displays.

[0017] It should be understood that the description in this section is not intended to identify key or essential features of the embodiments of the present invention, nor is it intended to limit the scope of the invention. Other features of the invention will become readily apparent from the following description. Attached Figure Description

[0018] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0019] Figure 1 This is a schematic diagram of a display structure provided in an embodiment of the present invention; Figure 2 yes Figure 1 A partial structural diagram of the display structure in the image; Figure 3 This is a flowchart of a method for preparing a display structure according to an embodiment of the present invention; Figure 4 yes Figure 1 Another schematic diagram of the display structure in the image; Figure 5 yes Figure 1Another schematic diagram of the display structure in the image; Figure 6 yes Figure 1 Another schematic diagram of the display structure in the image; Figure 7 yes Figure 1 Another part of the display structure is shown in the schematic diagram. Detailed Implementation

[0020] To enable those skilled in the art to better understand the present invention, the technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of the present invention.

[0021] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this invention are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of the invention described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion; for example, a process, method, system, product, or apparatus that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or apparatus.

[0022] Figure 1 This is a schematic diagram of a display structure provided in an embodiment of the present invention. Figure 2 yes Figure 1 A partial structural diagram of the display structure is shown in the image. Figure 1 and Figure 2 The display structure includes: a silicon-based CMOS backplane 110, a metal anode layer 120, a transparent adjustment layer 130, an organic functional layer 140, and a semi-transparent cathode layer 150 stacked together to form a closed optical resonant cavity; wherein, the transparent adjustment layer 130 includes at least a first adjustment layer 131 and a second adjustment layer 132; the total physical thickness of each sub-pixel in the transparent adjustment layer 130 is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer 130, the fixed refractive index difference of each adjustment layer material is used to achieve the control of the optical cavity length of each sub-pixel, matching the resonant wavelengths of blue light, green light, and red light.

[0023] It should be noted that the transparent adjustment layer 130 in this invention is not limited to a two-layer structure, but can also be a multi-layer structure.

[0024] In this embodiment, the total physical thickness of each sub-pixel in the transparent adjustment layer 130 is the same. By adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer 130 and utilizing the fixed refractive index difference of each adjustment layer material, the optical cavity length of each sub-pixel can be controlled. This matches the resonant wavelengths of blue, green, and red light, ensuring that the total physical thickness of the transparent adjustment layer 130 for the B / G / R three-color sub-pixels is completely consistent. This guarantees the flatness and electrical consistency of the pixel film layer and is compatible with CMOS photolithography mass production processes. By using the refractive index difference of the adjustment layer materials to differentially control the optical cavity length of the three colors and match the RGB emission resonant wavelengths, a high-performance strong microcavity structure is constructed. This solves the problems of poor process compatibility, uneven electrical properties of the three colors, weak microcavity effect, and low color purity in traditional cavity adjustment schemes. It is suitable for high-end silicon-based OLED display scenarios such as AR / VR, ultra-high color gamut micro-displays, and near-eye displays.

[0025] Optionally, based on the above embodiments, the thickness of the transparency adjustment layer 130 can be adjusted. , Total physical thickness of each sub-pixel ; Total optical cavity length ; Interference level ; Cavity fineness ; Spectral half width at half maximum (FWHM) ; Light intensity gain ; Where n1 is the refractive index of the first adjustment layer 131, and n2 is the refractive index of the second adjustment layer 132. The thickness of the first adjustment layer 131 The thickness of the second adjustment layer 132; The cavity length of the first adjustment layer 131, The cavity length of the second adjustment layer 132; R1 is the wavelength of light; R2 is the reflectivity of the metal anode layer 120 and R2 is the reflectivity of the semi-transparent cathode layer 150.

[0026] It is understandable that the total physical thickness of the first adjustment layer 131 and the second adjustment layer 132 is uniformly set to H=H. B =H G =H R nm, where H B H represents the total physical thickness of the blue sub-pixel. G H represents the total physical thickness of the green sub-pixels. RThe total physical thickness of the red sub-pixel is shown, where the optimal mass production thickness for the strong microcavity is selected based on the actual process technology to ensure optimal balance between process window, optical performance, and electrical properties. Blue sub-pixel (B, 450nm): ITOh 1B nm+IZOh 2B nm; Green subpixel (G, 550nm): ITOh 1G nm+IZOh 2G nm; Red subpixel (R, 620nm): ITOh 1R nm+IZOh 2R nm.

[0027] Optionally, based on the above embodiments, the material of the first adjustment layer 131 is indium tin oxide, and the material of the second adjustment layer 132 is indium zinc oxide.

[0028] Specifically, indium tin oxide (ITO) is a transparent conductive oxide (TCO) material with indium oxide (In2O3) as the matrix and tin (Sn) as the donor dopant, while indium zinc oxide (IZO) is a transparent conductive oxide material with indium oxide (In2O3) as the matrix and zinc (Zn) as the dopant.

[0029] It should be noted that the material of the adjustment layer in this invention is not limited to indium tin oxide and indium zinc oxide, but can also be other transparent conductive oxide film layers or other highly transparent conductive film layers.

[0030] Optionally, based on the above embodiments, the refractive index of the first adjustment layer 131 is 1.8~2.0, and the refractive index of the second adjustment layer 132 is 1.9~2.2.

[0031] This embodiment abandons the traditional single-layer TCO and organic layer cavity tuning method, and adopts a structure of low refractive index and high refractive index film layer composite stacking. It strictly constrains the uniform physical total thickness of the RGB sub-pixel double TCO layer, and only by adjusting the thickness ratio of ITO and , it uses the fixed refractive index difference of the two materials to achieve independent differential control of the optical cavity length of the three color sub-pixels, and accurately matches the resonant wavelength of blue light, green light and red light.

[0032] Optionally, based on the above embodiments, the reflectivity of the metal anode layer 120 is ≥92%.

[0033] Optionally, based on the above embodiments, the reflectivity of the semi-transparent cathode layer 150 is 70-80%.

[0034] This embodiment utilizes a high-reflectivity semi-transparent cathode to optimize microcavity precision, and can be further enhanced with a micro-color filter to compensate for red-green spectral broadening. Ultimately, it achieves a near-full-color FWHM < 30nm and a brightness gain > 3 times, resulting in a standard strong microcavity effect. This significantly reduces wide-viewing-angle drift and substantially improves overall color gamut coverage and viewing angle stability. By optimizing the reflectivity of the semi-transparent cathode, the microcavity surface reflection precision is improved, the emission spectrum is narrowed, and the emission gain is increased. This achieves a standard strong microcavity effect without altering the device's electrical structure or sacrificing process yield.

[0035] Optionally, based on the above embodiments, the interference order of the transparent adjustment layer 130 is between 1.2 and 1.8.

[0036] For example, in one embodiment, the total physical thickness of the RGB full-subpixel transparent cavity layer is strictly uniformly 75nm; the cavity material system is a low-refractive ITO (n1=1.85) + high-refractive IZO (n2=2.05) double TCO stack; the uniform optical thickness of the organic layer is 240nm, the bottom anode reflectivity R1 is 92%, and the top cathode optimized reflectivity R2 is 78%; the microcavity type is a second-order FP strong microcavity (m∈1.2~1.8); the precise RGB thickness ratio under a total thickness of 75nm is: Blue B (450nm): ITO 65nm + IZO 10nm = total 75nm nm; Green G (550nm): ITO 35nm + IZO 40nm = total 75nm; Red R (620nm): ITO 5nm + IZO 70nm = total 75nm; Blue B: TCO optical thickness = 140.75nm, total cavity length = 380.75nm, interference order m = 1.69; Green G: TCO optical thickness = 146.75nm, total cavity length = 386.75nm, interference order m = 1.41; Red R: TCO optical thickness = 152.75nm, total cavity length = 392.75nm, interference order m = 1.27. With a cavity precision of F=9.42, blue light (B) has a FWHM=28.23nm (natively meeting the standard <30nm), resulting in a brightness gain of 3.3~3.5 times; green light (G) has a FWHM=41.52nm (after color filter compensation <30nm), resulting in a brightness gain of 3.0~3.2 times; and red light (R) has a FWHM=51.95nm (after color filter compensation <30nm), resulting in a brightness gain of 2.9~3.1 times. The final full-pixel brightness gain is ≥3.0 times, meeting the high-performance microcavity brightness standard.

[0037] Figure 3 This is a flowchart of a method for fabricating a display structure according to an embodiment of the present invention, used to fabricate the display structure provided in the above embodiment. (Refer to...) Figure 3 The method includes: S310. A metal anode layer 120 is fabricated on a silicon-based CMOS backplane 110.

[0038] Figure 4 yes Figure 1 Another part of the display structure is shown in the schematic diagram. Figure 5 yes Figure 1 Another schematic diagram of the display structure in the image shows that, specifically, a metal anode film layer is deposited on the CMOS substrate to obtain... Figure 4 The metal anode film layer is coated, exposed, developed, etched, and the resist is removed to form the metal anode layer 120, resulting in... Figure 5 .

[0039] S320. A first conditioning layer 131 is prepared on the metal anode layer 120.

[0040] Figure 6 yes Figure 1 Another schematic diagram of the display structure is shown. Specifically, an ITO film can be deposited on the metal anode layer 120, and a halftone mask is used for resist coating, exposure, and development. Then, halftone mask etching is performed to remove the resist, forming ITO film layers of different thicknesses, namely the first adjustment layer 131. Figure 6 .

[0041] S330, Prepare a second adjustment layer 132 on the first adjustment layer 131.

[0042] Figure 7 yes Figure 1 Another schematic diagram of the display structure is shown. Specifically, an IZO film can be deposited on the first adjustment layer 131, and a halftone mask is used for resist coating, exposure, and development. Then, halftone mask etching is performed to remove the resist, forming IZO film layers of different thicknesses. This ensures that the ITO+IZO thickness of the BGR is consistent (H=HB=HG=HR), and that the Metal+TCO anode thickness is consistent (H+Hmetal), resulting in... Figure 7 .

[0043] It should be noted that the process solution provided by the present invention is not limited to halftone mask process; other step-by-step coating, photolithography, etching, and CMP processes can also be used in this invention.

[0044] S340, Deposit an insulating layer on the metal anode layer 120.

[0045] Specifically, SiO2 can be used to fill the space region of the metal anode layer 120 to ensure the uniformity of the final anode structure's overall thickness, resulting in... Figure 2 .

[0046] In this transparent adjustment layer 130, the total physical thickness of each sub-pixel is the same. By adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer 130, and utilizing the fixed refractive index difference of each adjustment layer material, the optical cavity length of each sub-pixel can be controlled to match the resonant wavelengths of blue light, green light, and red light.

[0047] Optionally, based on the above embodiments, the material of the first adjustment layer 131 is indium tin oxide, and the material of the second adjustment layer 132 is indium zinc oxide; Step S320 includes: depositing an indium tin oxide film layer on the metal anode layer 120, and using a halftone mask for resist coating, exposure and development, and halftone mask etching to remove resist, so that different sub-pixels form indium tin oxide film layers of different thicknesses, to obtain the first adjustment layer 131.

[0048] Step S330 includes: depositing an indium zinc oxide film layer on the first adjustment layer 131, and using a halftone mask for resist coating, exposure and development, and halftone mask etching to remove resist, so that different sub-pixels form indium zinc oxide film layers of different thicknesses, and the total physical thickness of each sub-pixel is the same, to obtain the second adjustment layer 132.

[0049] Optionally, based on the above embodiments, step S340 includes: depositing SiO2 on the metal anode layer 120 to fill the gap.

[0050] In summary, the present invention has the following beneficial effects: 1) Strong process compatibility and excellent mass production performance. The three-color sub-pixel dual TCO same physical thickness cavity structure completely solves the problems of poor flatness, uneven electrical properties and low yield caused by differential film thickness. It is fully compatible with existing silicon-based OLED mass production lines and CMOS photolithography mass production processes; 2) Significant microcavity effect and extreme improvement in display performance. Relying on the high and low fixed refractive index difference of ITO / IZO, the precise cavity length matching of the three colors is achieved without changing the film thickness flatness. Combined with a high-reflectivity cathode, the microcavity precision is greatly improved. Combined with simple color filter compensation, full-color narrow spectrum and high brightness output can be achieved. The upper limit of color gamut and brightness gain far exceed the traditional differential cavity microcavity structure. 3) High device stability: The organic layer exhibits no thickness variation across its entire surface, ensuring stable carrier transport and consistent aging rates for all three color pixels, significantly improving overall device lifespan and display consistency. 4) Controllable cost: Utilizing mature commercial ITO and IZO materials, it eliminates the need for high-cost, high-refractive-weight dielectrics or special processes. A strong microcavity effect is achieved solely through optimized film layer ratios, resulting in low modification costs and high applicability. This solution addresses the issues of poor process compatibility, uneven electrical properties of the three colors, weak microcavity effect, and low color purity inherent in traditional cavity adjustment solutions. It is suitable for high-end silicon-based OLED display scenarios such as AR / VR, ultra-high color gamut micro-displays, and near-eye displays.

[0051] The specific embodiments described above do not constitute a limitation on the scope of protection of this invention. Those skilled in the art should understand that various modifications, combinations, sub-combinations, and substitutions can be made according to design requirements and other factors. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this invention should be included within the scope of protection of this invention.

Claims

1. A display structure, characterized in that, include: A closed optical resonant cavity is formed by stacking a silicon-based CMOS backplane, a metal anode layer, a transparent adjustment layer, an organic functional layer, and a semi-transparent top cathode. The transparent adjustment layer includes at least a first adjustment layer and a second adjustment layer; The total physical thickness of each sub-pixel in the transparent adjustment layer is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, the optical cavity length of each sub-pixel can be controlled by utilizing the fixed refractive index difference of each adjustment layer material, and the resonant wavelengths of blue light, green light and red light can be matched.

2. The display structure according to claim 1, characterized in that, The thickness of the transparent adjustment layer , Total physical thickness of each sub-pixel ; Total optical cavity length ; Interference level ; Cavity fineness ; Spectral half width at half maximum (FWHM) ; Light intensity gain ; Where n1 is the refractive index of the first adjustment layer and n2 is the refractive index of the second adjustment layer. The thickness of the first adjustment layer, The thickness of the second adjustment layer; The cavity length of the first adjustment layer, The cavity length of the second adjustment layer; R1 is the wavelength of light; R2 is the reflectivity of the metal anode layer; and R3 is the reflectivity of the semi-transparent cathode.

3. The display structure according to claim 1, characterized in that, The first conditioning layer is made of indium tin oxide, and the second conditioning layer is made of indium zinc oxide.

4. The display structure according to claim 1, characterized in that, The refractive index of the first adjustment layer is 1.8~2.0, and the refractive index of the second adjustment layer is 1.9~2.

2.

5. The display structure according to claim 1, characterized in that, The reflectivity of the metal anode layer is ≥92%.

6. The display structure according to claim 1, characterized in that, The reflectivity of the semi-transparent cathode is 70-80%.

7. The display structure according to claim 1, characterized in that, The interference order of the transparent adjustment layer is between 1.2 and 1.

8.

8. A method for preparing a display structure, used to prepare the display structure according to any one of claims 1-7, characterized in that, include: Fabrication of a metal anode layer on a silicon-based CMOS backplane; A first conditioning layer is prepared on the metal anode layer; A second adjustment layer is fabricated on the first adjustment layer; An insulating layer is deposited on the metal anode layer; In this transparent adjustment layer, the total physical thickness of each sub-pixel is the same; by adjusting the thickness ratio of each adjustment layer in the transparent adjustment layer, the optical cavity length of each sub-pixel can be controlled by utilizing the fixed refractive index difference of each adjustment layer material, thereby matching the resonant wavelengths of blue, green and red light.

9. The method for preparing the display structure according to claim 8, characterized in that, The material of the first conditioning layer is indium tin oxide, and the material of the second conditioning layer is indium zinc oxide; The preparation of the first conditioning layer on the metal anode layer includes: An indium tin oxide film is deposited on the metal anode layer, and a halftone mask is used for resist coating, exposure and development, and halftone mask etching to remove resist, so that different sub-pixels form indium tin oxide film layers of different thicknesses, thus obtaining the first adjustment layer. Fabricating a second adjustment layer on the first adjustment layer includes: An indium zinc oxide film is deposited on the first adjustment layer, and a halftone mask is used for resist coating, exposure and development, and halftone mask etching to remove resist, so that different sub-pixels form indium zinc oxide film layers of different thicknesses, and the total physical thickness of each sub-pixel is the same, thus obtaining the second adjustment layer.

10. The method for preparing the display structure according to claim 8, characterized in that, Depositing an insulating layer on the metal anode layer includes: SiO2 is deposited on the metal anode layer to fill the gap.