Battery cells and battery cell manufacturing methods

By designing terminal slots on the rivet terminals and forming protrusions that match the current collector during the welding process, the problem of easy separation of burrs during welding is solved, thus improving the reliability of the battery cells.

CN123125731APending Publication Date: 2026-11-17LG ENERGY SOLUTION LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202580027928.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-11-04
Filing Date
2025-10-28
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

During the battery cell manufacturing process, burrs generated when welding current collectors and rivet terminals are easily separated, leading to defects in the battery cell.

Method used

By designing terminal grooves on the rivet terminals and using ultrasonic welding during the welding process, the contact area between the welding rod and the manifold is recessed, forming a protrusion that matches the manifold, reducing the possibility of burr separation.

Benefits of technology

This reduces the likelihood of burrs separating from the current collector and lowers the occurrence of battery cell defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123125731A_ABST
    Figure CN123125731A_ABST
Patent Text Reader

Abstract

According to this disclosure, a battery cell manufacturing apparatus may be provided, the apparatus comprising: a moving unit for conveying a battery cell including a cell tab with a barcode displayed on the cell tab; and an identification device facing the movement path of the battery cell conveyed by the moving unit and identifying the barcode, wherein the identification device includes a guiding unit that sprays air toward the cell tab to prevent the cell tab from bending.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application claims the benefit of Korean Patent Application No. 10-2024-0154348, filed on November 4, 2024, the disclosure of which is incorporated herein by reference in its entirety.

[0002] This disclosure relates to battery cells and methods for manufacturing battery cells. Background Technology

[0003] Rechargeable and dischargeable battery cells (secondary batteries) are widely used in mobile devices such as digital cameras, mobile phones and laptops, and especially in recent years, secondary batteries have gained attention as an energy source for electric vehicles and energy storage systems (ESS).

[0004] Based on the shape of the casing, battery cells can be classified as cylindrical battery cells or prismatic battery cells, in which the electrode assembly is embedded in a cylindrical or prismatic metal can, or as pouch cells, in which the electrode assembly is embedded in a pouch-shaped casing formed by diaphragms.

[0005] Cylindrical battery cells include rivet terminals for transmitting current from the electrode assembly to the outside. During the manufacturing of cylindrical battery cells, a process of welding current collectors and rivet terminals is performed to electrically connect the rivet terminals and current collectors.

[0006] Furthermore, ultrasonic welding can be used in the welding of the current collector and rivet terminals. Here, burrs may form; burrs are debris generated from deformed portions of the current collector due to friction between the welding rod and the current collector in contact with the welding rod. Burrs can be small and thin in a linear shape and may be easily separated from the current collector. If burrs separate from the current collector and remain inside the battery cell, defects may occur in the battery cell. Summary of the Invention

[0007] Technical issues

[0008] This disclosure aims to address at least some of the aforementioned defects in the prior art, and in the battery cell manufacturing method, by forming the burrs generated during the welding process into a block shape, the possibility of the burrs separating from the current collector can be reduced.

[0009] Technical solution

[0010] According to one aspect, a method for manufacturing a battery cell is provided, the method comprising: an alignment step of aligning a first current collector and a rivet terminal electrically connected to an electrode assembly into contact with each other; and a welding step of welding the rivet terminal and the first current collector using ultrasonic welding, the rivet terminal including a terminal groove, wherein a region of the surface facing the first current collector is recessed inward at the terminal groove, and the welding step may be a step of welding by abutting a welding electrode against a welding point of the first current collector positioned corresponding to the terminal groove.

[0011] The first width, which is the depth of the terminal slot, can be less than or equal to the second width, which is the thickness of the first current collector.

[0012] The diameter of the terminal slot can be larger than the diameter of the tip of the welding rod.

[0013] The diameter of the terminal slot can be greater than or equal to the sum of the diameter of the tip of the welding rod and twice the second width.

[0014] The welding steps may include: a pressure step, in which pressure is applied to the first current collector using the tip of the welding electrode toward the terminal slot; and a friction step, in which friction is generated between the first current collector and the rivet terminal by rotating or vibrating the welding electrode.

[0015] The first manifold can be a flat plate before the pressurization step is performed.

[0016] The first current collector may include protrusions, at least a portion of which is bent and accommodated in a terminal slot after the soldering step.

[0017] The protrusion may include a shape corresponding to the terminal slot.

[0018] According to another aspect, a battery cell is also provided, the battery cell comprising: an electrode assembly including a positive electrode, a negative electrode, and a separator inserted between the positive and negative electrodes; a can containing the electrode assembly; a rivet terminal electrically connected to the electrode assembly, and at least a portion of the rivet terminal being contained in the can; and a first current collector electrically connected to the electrode assembly and the rivet terminal, the rivet terminal including a terminal groove, wherein a region facing the surface of the first current collector is recessed inward, a first width being the depth of the terminal groove being less than or equal to a second width being the thickness of the first current collector, and the first current collector including a protrusion, at least a portion of the protrusion being bent and contained in the terminal groove.

[0019] At least a portion of the protrusion of the first current collector can be ultrasonically welded to the rivet terminal.

[0020] The protrusion may include a shape corresponding to the terminal slot.

[0021] The protrusion can be formed by bending the first manifold during the ultrasonic welding process.

[0022] Beneficial effects

[0023] According to the exemplary embodiments of this disclosure, the likelihood of burrs separating from the current collector of the battery cell can be reduced, thereby reducing the occurrence of battery cell defects. Attached Figure Description

[0024] Figure 1 This is a cross-sectional view of a battery cell according to an exemplary embodiment of the present disclosure.

[0025] Figure 2 This is a cross-sectional view showing the welding steps during the manufacture of a battery cell according to an exemplary embodiment of the present disclosure.

[0026] Figure 3 This is a flowchart illustrating a battery cell manufacturing method according to an exemplary embodiment of the present disclosure.

[0027] Figure 4 This is a cross-sectional view showing the process of welding current collectors and rivet terminals during the manufacture of a conventional battery cell.

[0028] Figure 5 This is a cross-sectional view showing the process of welding a first current collector and rivet terminals during the manufacture of a battery cell according to an exemplary embodiment of the present disclosure.

[0029] Figure 6 yes Figure 5 A magnified view of part A.

[0030] Figure 7 This is a cross-sectional view showing the process of welding a first current collector and rivet terminals during the manufacture of a battery cell according to an exemplary embodiment of the present disclosure.

[0031] Figure 8 yes Figure 7 A magnified view of part B.

[0032] Figure 9 (a) is an image taken by magnifying the surface of the current collector plate welded to the rivet terminals of a conventional battery cell, and Figure 9 (b) is an image taken by magnifying the surface of the current collector plate welded to the rivet terminals of a battery cell according to an exemplary embodiment of the present disclosure.

[0033] Figure 10 (a) is a three-dimensional image showing the surface of a current collector plate welded to rivet terminals of a conventional battery cell, and Figure 10 (b) is a three-dimensional image of the surface of a current collector plate welded to a rivet terminal according to an exemplary embodiment of the present disclosure. Detailed Implementation

[0034] The terminology used in describing the example embodiments has been selected as much as possible from currently widely used common terms, while taking into account the functionality obtained according to this disclosure. However, these terms may be replaced by other terms based on the intent, habits, or emergence of new technologies of those skilled in the art. Furthermore, in certain cases, terms arbitrarily chosen by the applicant of this disclosure may be used, and in such cases, the meaning of these terms may be described in the corresponding descriptive section of this disclosure. Therefore, it should be noted that the terms used herein can be interpreted based on their actual meaning and the overall content of this specification, rather than simply on their names.

[0035] The suffixes such as “part,” “component,” or “section” used when referring to components as used in this specification are merely for ease of writing and are used interchangeably, and do not necessarily imply any different meaning or function. Furthermore, in describing exemplary embodiments of this disclosure, detailed descriptions of related known technologies that might obscure the subject matter of the exemplary embodiments may be omitted. Moreover, the accompanying drawings are provided only to facilitate understanding of the exemplary embodiments of this disclosure and should not be construed as limiting the technical scope of this disclosure, and are intended to cover all modifications, equivalents, and alternatives falling within the spirit and scope of this disclosure.

[0036] Ordinal terms such as “first” and “second” can be used to describe various components, but these components are not limited by these terms, which are only used to distinguish one component from another.

[0037] When a component is described as "connected to another component" or "connected to another component," it can be directly connected to or connected to another component, or there can be one or more intermediate components. Conversely, when a component is described as "directly connected to another component" or "directly connected to another component," it should be interpreted as no intermediate components exist.

[0038] In this disclosure, singular terms may include plural terms unless there is a clear contextual conflict in the description.

[0039] Terms such as “comprising” or “including” used in this specification are used to indicate the presence of features, numbers, operations, actions, components, parts or combinations thereof, and it should be understood that these terms do not preclude the possibility that one or more other features, numbers, operations, actions, components, parts or combinations thereof may be present or added.

[0040] The expression "at least one of a, b and c" as used in this specification may include "only a", "only b", "only c", "a and b", "a and c", "b and c", or "all of a, b and c".

[0041] In the following description, exemplary embodiments of the present disclosure will be described in detail with reference to the accompanying drawings, enabling those skilled in the art to readily implement the present disclosure. However, the present disclosure can be applied in many different forms and is not limited to the embodiments described herein.

[0042] In the following, exemplary embodiments of the present disclosure will be described in detail with reference to the accompanying drawings.

[0043] Figure 1 This is a cross-sectional view of battery cell 1 according to an exemplary embodiment of the present disclosure, and Figure 2 This is a cross-sectional view showing the welding step S300 during the manufacture of battery cell 1 according to an exemplary embodiment of the present disclosure.

[0044] Reference Figure 1 and Figure 2 According to an exemplary embodiment of the present disclosure, the battery cell 1 may include an electrode assembly 100. The electrode assembly 100 may include a positive electrode 110, a negative electrode 120, and a separator 130. The separator 130 may be inserted between the positive electrode 110 and the negative electrode 120. In the electrode assembly 100, a plurality of positive electrodes 110, negative electrodes 120, and separators 130 may be alternately stacked. The electrode assembly 100 may be wound and configured into a core shape. Here, a central hole 140, serving as a predetermined void space, may be formed at the center of the electrode assembly 100. The central hole 140 may be a void space formed at the center during the winding process of the electrode assembly 100, and may be formed along the length direction of the electrode assembly 100.

[0045] A battery cell 1 according to an exemplary embodiment of the present disclosure may include a can 200. The can 200 may house an electrode assembly 100. The can 200 may be formed of a conductive material through which current can flow. The can 200 may be configured to have a cylindrical shape to house the core-shaped electrode assembly 100. The can 200 may be configured to seal its internal space. The can 200 may include an upward-facing first surface 210 and a downward-facing second surface 220. After housing the electrode assembly 100 and electrolyte, the can 200 may be sealed. The first surface 210 may seal the top of the can 200 using inserted rivet terminals 500, which will be described later. The second surface 220 may be configured as a cap plate and seal the bottom of the can 200.

[0046] Although the electrode assembly 100 and the can 200 are described as a coil shape and a cylinder shape, respectively, in this specification when describing the battery cell 1 of the present disclosure, their shapes may be appropriately modified to achieve the purpose of the present disclosure. For example, the electrode assembly 100 may be stacked in one direction, and the can 200 may be formed in a rectangular prism shape.

[0047] The battery cell 1 disclosed herein may include a rivet terminal 500. The rivet terminal 500 may be electrically connected to an electrode assembly 100. A first current collector 300, described later, may be inserted between the rivet terminal 500 and the electrode assembly 100. The rivet terminal 500 may be formed of a conductive material to allow current flow. At least a portion of the rivet terminal 500 may be housed within a canister 200. In other words, at least a portion of the rivet terminal 500 may be exposed to the outside of the canister 200. The rivet terminal 500 may be configured to output electrical energy from the electrode assembly 100 to the outside.

[0048] The battery cell 1 disclosed herein may include current collectors 300 and 400. Current collectors 300 and 400 may be electrically connected to the positive electrode 110 or the negative electrode 120 of the electrode assembly 100. Current collectors 300 and 400 may include a first current collector 300 and a second current collector 400. The first current collector 300 may be electrically connected to the positive electrode 110 of the electrode assembly 100, and the second current collector 400 may be electrically connected to the negative electrode 120 of the electrode assembly 100. However, the possibility that the first current collector 300 is connected to the negative electrode 120 and the second current collector 400 is connected to the positive electrode 110 is not excluded. The first current collector 300 may be electrically connected to the electrode assembly 100 and also electrically connected to the rivet terminal 500. For example, the first current collector 300 may be soldered to multiple positive electrodes 110 of the electrode assembly 100 and may also be soldered to the rivet terminal 500. Here, the second current collector 400 may be electrically connected to a portion of the can 200.

[0049] The specific shapes of the rivet terminal 500 and the first current collector 300, as well as the welding step S300 for welding the rivet terminal 500 and the first current collector 300, will be described in detail below.

[0050] Figure 3 This is a flowchart illustrating a battery cell manufacturing method 1 according to an exemplary embodiment of the present disclosure. Figure 4 This is a cross-sectional view showing the process of welding the current collector 300' and the rivet terminal 500' during the manufacture of a conventional battery cell 1. Figure 5 This is a cross-sectional view showing the process of welding the first current collector 300 and the rivet terminal 500 during the manufacture of battery cell 1 according to an exemplary embodiment of the present disclosure. Figure 6 yes Figure 5 A magnified view of part A. Figure 7This is a cross-sectional view showing the process of welding the first current collector 300 and the rivet terminal 500 during the manufacture of battery cell 1 according to an exemplary embodiment of the present disclosure. Figure 8 yes Figure 7 A magnified view of part B. Figure 9 (a) is an image taken by magnifying the surface of the current collector plate of a conventional battery cell 1 welded to the rivet terminal 500. Figure 9 (b) is an image taken by magnifying the surface of the current collector plate welded to the rivet terminal 500 of the battery cell 1 according to an exemplary embodiment of the present disclosure. Figure 10 (a) is a three-dimensional image showing the surface of a current collector plate of a conventional battery cell 1 welded to a rivet terminal 500, and Figure 10 (b) is a three-dimensional image of the surface of the current collector plate of the battery cell 1 welded to the rivet terminal 500 according to an exemplary embodiment of the present disclosure.

[0051] Figure 5 and Figure 7 This diagram illustrates welding step S300, which can be performed sequentially. Figure 5 and Figure 7 The operation.

[0052] Reference Figures 3 to 10 as well as Figure 1 and Figure 2 The present disclosure will describe in detail the battery cell 1 and the battery cell manufacturing method 1 according to exemplary embodiments.

[0053] A battery cell manufacturing method 1 according to an exemplary embodiment of the present disclosure may include an alignment step S200. A preliminary step S100 may be performed before the alignment step S200. For example, the preliminary step S100 may be the process of inserting the electrode assembly 100 into the can 200 or inserting the rivet terminal 500 into the can 200. The alignment step S200 may be the step of aligning the first current collector 300 electrically connected to the electrode assembly 100 and the rivet terminal 500 into contact with each other. Figure 5 This could be a diagram showing the state after performing alignment step S200. The first current collector 300 may include solder points 310 contacted by solder rods 600, and the rivet terminal 500 may include terminal slots 550, which will be described later. Alignment step S200 may be a step of precisely aligning the solder points 310 and the terminal slots 550 of the rivet terminal 500, and bringing the rivet terminal 500 and the first current collector 300 into contact with each other.

[0054] A battery cell manufacturing method 1 according to an exemplary embodiment of this disclosure may include a welding step S300. Welding step S300 may be a step of welding a rivet terminal 500 and a first current collector 300. Here, welding may be ultrasonic welding. Ultrasonic welding may be a method of joining two materials by generating friction between the two materials using a welding electrode 600. In ultrasonic welding, friction may be generated by vibrating or rotating the welding electrode 600 when it comes into contact with at least one material to be welded. The tip 610 of the welding electrode in contact with the material to be welded may include various shapes to prevent slippage. (See reference...) Figure 9 and Figure 10 Due to welding, a grid pattern corresponding to the tip 610 of the welding electrode can be formed on one surface of the first current collector 300 being welded. However, such a shape is merely an example and is not limited to a grid pattern.

[0055] Reference Figure 1 and Figure 5 According to an exemplary embodiment of this disclosure, the rivet terminal 500 may include a terminal head 510, a terminal shaft 520, a terminal bottom 530, and a terminal wing 540. The terminal head 510 may be a portion protruding from and exposed above the can 200. The terminal shaft 520 may be a shaft extending below the terminal head 510 and passing through a first surface 210, which is the upper surface of the can 200. The terminal bottom 530, as a downwardly protruding region, may be a portion that contacts the first manifold 300. The terminal wing 540 may be a portion that protrudes laterally from the terminal shaft 520 and engages with a surface of the can 200 to prevent the rivet terminal 500 inserted into the can 200 from separating from the can 200.

[0056] Reference Figure 5 and Figure 6 The rivet terminal 500 according to an exemplary embodiment of the present disclosure may include a terminal groove 550. The terminal groove 550 may be formed in a region facing the first current collector 300. The terminal groove 550 may be formed by inward recessing from the aforementioned region. The term "inward" as used herein may mean the interior of the rivet terminal 500.

[0057] According to an exemplary embodiment of this disclosure, welding step S300 may be performed by abutting a welding electrode 600 against a welding point 310 of the first current collector 300, which is positioned to correspond to the terminal slot 550. The welding point 310 may be positioned to correspond to the terminal slot 550 and may be the area where the welding electrode 600 is placed. The area of ​​the first current collector 300 including the welding point 310 may deform and melt due to friction and / or pressure from the welding electrode 600, thereby fusing with the rivet terminal 500.

[0058] For example, welding step S300 according to an exemplary embodiment of this disclosure may include a pressure step S310 and a friction step S320. (See also...) Figure 5 and Figure 6 The pressurization step S310 can be a step of applying pressure to the first current collector 300 using the tip 610 of a welding electrode toward the terminal slot 550. The first current collector 300 may be a flat plate before performing the pressurization step S310. (See reference...) Figure 7 and Figure 8 The friction step S320 can be a step of generating friction between the first current collector 300 and the rivet terminal 500 by rotating or vibrating the welding rod 600.

[0059] According to an exemplary embodiment of this disclosure, the protrusion 320 can be formed in the first current collector 300 via a pressing step S310 and / or a friction step S320. At least a portion of the first current collector 300, which corresponds to the terminal slot and was previously a flat plate, can be bent to form the protrusion 320 accommodated in the terminal slot 550. That is, the protrusion 320 can be a portion formed by bending the first current collector 300 during an ultrasonic welding process. At least a portion of the protrusion 320 can be ultrasonically welded to the first current collector 300.

[0060] The first current collector 300 according to an exemplary embodiment of this disclosure may include a protrusion 320 after welding step S300. The protrusion 320 may be received within a terminal slot 550 and may include a shape corresponding to the terminal slot 550. The protrusion 320 may be deformed by the pressure and / or friction of the welding electrode 600 to fit into the terminal slot 550. However, minor gaps between the protrusion 320 and the terminal slot 550 that may occur during the manufacturing process are permissible.

[0061] In the battery cell manufacturing method 1 according to an exemplary embodiment of the present disclosure, a subsequent process S400 may be performed after the welding step S300. For example, the subsequent process S400 may be the process of injecting electrolyte into the tank 200 or sealing the second surface 220 at the bottom of the tank 200.

[0062] Reference Figure 6 The first width t1 can be less than or equal to the second width t2 of the first current collector 300, where the first width t1 is the depth of the terminal slot 550 according to an exemplary embodiment of this disclosure. If the first width t1 is greater than the second width t2, the first current collector 300 may undergo plastic deformation during the welding process and be cut off before welding. That is, a portion of the area of ​​the first current collector 300 corresponding to the terminal slot 550 may be cut off by the welding rod 600 due to its excessive recess into the terminal slot 550. Therefore, the first width t1 can be formed to be less than or equal to the second width t2 to prevent this from happening.

[0063] Reference Figure 8 According to an exemplary embodiment of this disclosure, the diameter d1 of the terminal groove 550 can be larger than the diameter d2 of the tip 610 of the welding rod. For example, if the cross-section of the tip 610 of the welding rod is circular, the cross-section of the terminal groove 550 can also be formed as circular. Here, the diameter d1 of the terminal groove 550 can be formed to be larger than the diameter d2 of the tip 610 of the welding rod, such that the tip 610 of the welding rod is properly accommodated within the terminal groove 550 during the welding process. More specifically, the diameter d1 of the terminal groove 550 can be greater than or equal to the sum of the diameter d2 of the tip 610 of the welding rod and twice the second width t2. The diameter d1 of the terminal groove 550 is sufficient to accommodate the tip of the welded portion and the protrusion 320 within the terminal groove 550.

[0064] Reference Figure 4 Because conventional rivet terminals 500' do not include terminal slots 550, ultrasonic welding is performed by abutting a flat current collector 300' against one surface of the flat rivet terminal 500'. As a result, small, fine, linear burrs B' are observed to form. Figure 9 (a) and Figure 10 As shown in (a), the burrs B' formed as thin burrs and protruding upward from the current collector can be easily separated from the current collector 300' and can cause internal defects in the battery cell 1.

[0065] According to the exemplary embodiments of the battery cell 1 and battery cell manufacturing method 1 of this disclosure, the burrs B formed during the welding process can be formed in block form. That is, the burrs B formed in the battery cell 1 of this disclosure and by the battery cell manufacturing method 1 can have sufficient thickness and mass to prevent easy separation from the first current collector 300. (Refer to...) Figure 9 (b) and Figure 10 (b) According to the exemplary embodiment of this disclosure, the burr B can be formed to have a greater thickness and mass than a conventional burr B', and therefore can be less easily separated from the first current collector 300. Thus, defects in the battery cell 1 that may be caused by the burr B can be reduced.

[0066] While this disclosure has been shown and described with reference to preferred exemplary embodiments for the purpose of illustrating the principles of this disclosure, this disclosure is not limited to the configurations and operations shown and described. Rather, those skilled in the art will readily understand that many changes and modifications can be made to this disclosure without departing from the spirit and scope of the appended claims.

Claims

1. A method for manufacturing a battery cell, the method comprising: In the alignment step, the first current collector and the rivet terminals, which are electrically connected to the electrode assembly, are aligned to make contact with each other. as well as In the welding step, ultrasonic welding is used to weld the rivet terminal to the first current collector. The rivet terminal includes a terminal groove, wherein the area of ​​the terminal groove facing the surface of the first current collector is recessed inward, and The welding step is a step of welding by bringing the welding rod against the welding point of the first manifold, which is positioned to correspond to the terminal slot.

2. The battery cell manufacturing method according to claim 1, wherein, The first width, which is the depth of the terminal slot, is less than or equal to the second width, which is the thickness of the first current collector.

3. The battery cell manufacturing method according to claim 2, wherein, The diameter of the terminal slot is larger than the diameter of the tip of the welding rod.

4. The battery cell manufacturing method according to claim 3, wherein, The diameter of the terminal slot is greater than or equal to the sum of the diameter of the tip of the welding electrode and twice the second width.

5. The battery cell manufacturing method according to claim 1, wherein, The welding steps include: The pressurization step involves applying pressure to the first current collector using the tip of the welding electrode towards the terminal slot; and The friction step generates friction between the first manifold and the rivet terminal by rotating or vibrating the welding electrode.

6. The battery cell manufacturing method according to claim 5, wherein, The first manifold is a flat plate before the pressurization step is performed.

7. The battery cell manufacturing method according to claim 1, wherein, The first manifold includes a protrusion, at least a portion of which is bent after the welding step and accommodated in the terminal slot.

8. The battery cell manufacturing method according to claim 7, wherein, The protrusion has a shape corresponding to the terminal slot.

9. A battery cell, the battery cell comprising: An electrode assembly, the electrode assembly including a positive electrode, a negative electrode, and a diaphragm inserted between the positive electrode and the negative electrode; A container that houses the electrode assembly; A rivet terminal, the rivet terminal being electrically connected to the electrode assembly, and at least a portion of the rivet terminal being housed in the can; as well as A first current collector, electrically connected to the electrode assembly and the rivet terminal. The rivet terminal includes a terminal groove, wherein the area of ​​the terminal groove facing the surface of the first collector plate is recessed inward. Wherein, the first width, which is the depth of the terminal slot, is less than or equal to the second width, which is the thickness of the first current collector, and The first current collector includes a protrusion, at least a portion of which is bent and accommodated in the terminal slot.

10. The battery cell according to claim 9, wherein, At least a portion of the protrusion of the first manifold is ultrasonically welded to the rivet terminal.

11. The battery cell according to claim 9, wherein, The protrusion has a shape corresponding to the terminal slot.

12. The battery cell according to claim 9, wherein, The protrusion is formed by bending the first manifold during the ultrasonic welding step.

Citation Information

Patent Citations

  • Method for bug repair of multi-chunk program and apparatus thereof

    KR1020240154348A