Capillary casting thermoelectric PN junction
By manufacturing TEG using capillary casting, the problems of high cost and material inhomogeneity in TEG manufacturing have been solved, achieving efficient and stable thermoelectric conversion, and making it suitable for power generation applications under various environmental conditions.
Patent Information
- Application Number
- CN202580028085.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-02-26
- Filing Date
- 2025-02-25
- Publication Date
- 2026-11-17
AI Technical Summary
Traditional thermoelectric generators (TEGs) are manufactured in a costly manner, with uneven material distribution and a tendency to crack, and rely on expensive infrastructure, which limits their widespread application.
TEG is manufactured using a capillary casting method. By sandwiching a conductive substrate between barrier components and immersing it in a high-temperature molten alloy, the molten alloy enters the mold cavity through capillary action, forming an interlocked PN junction. This simplifies the manufacturing process and improves material uniformity and structural stability.
It significantly reduces TEG production costs, simplifies the manufacturing process, improves the uniformity of material composition and structural integrity, and is suitable for power generation under various environmental conditions, especially in scenarios with unstable sunlight or limited space.
Smart Images

Figure CN123126071A_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a thermoelectric PN junction, and more specifically, to a plurality of interlocked junctions manufactured using capillary casting. Background Technology
[0002] The pursuit of efficient energy conversion technologies has long been a key driver of innovation, especially in the renewable energy sector. Photovoltaic (PV) cells, which directly convert sunlight into electricity, are becoming increasingly popular due to improved efficiency and scalability. However, despite these advancements, PV cells retain inherent limitations, particularly when environmental conditions or space constraints challenge their feasibility. For example, in regions with unstable sunlight, high-latitude areas with prolonged darkness, or urban environments where space is extremely scarce, the deployment of PV cells is often uneconomical or impractical. Summary of the Invention
[0003] According to a first aspect, a method for manufacturing a PN junction for a thermoelectric generator is provided, the method comprising: sandwiching a conductive substrate between a pair of inert barrier members, wherein the conductive substrate includes a cavity defined by a periphery of the substrate; immersing at least a portion of the cavity in a tellurium-based molten alloy at a temperature higher than that of the substrate while the substrate is sandwiched, wherein immersing the cavity in the molten alloy causes the molten alloy to be drawn into the cavity by capillary action; and solidifying the molten alloy by removing the substrate from the molten alloy, wherein the conductive substrate acts as one of a negative dopant or a positive dopant of the PN junction, and the solidified alloy acts as the other of a negative dopant or a positive dopant of the PN junction.
[0004] A conductive substrate can act as a positive dopant, while a solidified alloy can act as a negative dopant. Alternatively, a conductive substrate can act as a negative dopant, while a solidified alloy can act as a positive dopant.
[0005] The conductive substrate can be copper.
[0006] The pair of barrier elements can be ceramic. The ceramic can be alumina ceramic.
[0007] The barrier and the conductive substrate can be coplanar.
[0008] The conductive substrate and the barrier can be tubular, and the barrier can extend inside and outside the conductive substrate, respectively.
[0009] The molten alloy may also include antimony.
[0010] The molten alloy may also include glass powder with a size of micron or smaller.
[0011] The molten alloy may include 3 parts tellurium, 1.5 parts antimony and 0.1 parts micron-sized glass powder.
[0012] The molten alloy may also include bismuth.
[0013] The molten alloy may include 3 parts tellurium, 1.5 parts antimony, 0.5 parts bismuth and 0.1 parts micron-sized glass powder.
[0014] Before immersion, the substrate may include multiple discontinuous segments; during immersion, molten alloy may be drawn into the segments; and the mold cavity may be shaped such that after solidification, the segments are held together by the solidified alloy that interlocks the segments together.
[0015] During immersion, molten alloy can enter the mold cavity through the gate, and the width of the gate can be less than the maximum width of the mold cavity.
[0016] According to another aspect, at least one PN junction for a thermoelectric generator is provided, the at least one junction comprising: a conductive substrate including a plurality of segments spaced apart from each other; and one or more tellurium-based alloy castings located between respective pairs of one or more segments, wherein each of the one or more castings interlocks one of the pairs of segments of the respective one or more segments together, and wherein the conductive substrate acts as one of the negative doping material or the positive doping material of the PN junction, and the solidified alloy acts as the other of the negative doping material or the positive doping material of the PN junction.
[0017] The conductive substrate can be copper.
[0018] The alloy may include 3 parts tellurium, 1.5 parts antimony, 0.5 parts bismuth and 0.1 parts micron-sized glass powder.
[0019] The conductive substrate can be tubular. Alternatively, the conductive substrate can be planar.
[0020] Each of the multiple sections may include a mold cavity and a gate for accommodating a portion of one or more castings, and the width of the gate may be less than the maximum width of the mold cavity.
[0021] According to another aspect, a thermoelectric generator is provided, which includes a plurality of the aforementioned PN junctions connected in series and / or in parallel.
[0022] This invention does not necessarily describe the full scope of all aspects. Other aspects, features, and advantages will become apparent to those skilled in the art after reading the following description of specific embodiments. Attached Figure Description
[0023] In the accompanying drawings illustrating one or more exemplary embodiments: Figure 1A and Figure 1B These are a front view and a perspective view of a conductive substrate for manufacturing a series of thermoelectric PN junctions, according to an exemplary embodiment.
[0024] Figure 2A and Figure 2B The following are examples of the process for manufacturing this series of PN junctions according to exemplary embodiments. Figure 1A and Figure 1B How the conductive substrate is sandwiched between two barrier elements.
[0025] Figure 3 An exemplary embodiment is shown. Figure 2B The sandwich conductive substrate is immersed in a molten alloy and then removed so that the series of thermoelectric PN junctions can be cast using capillary casting.
[0026] Figure 4A and Figure 4B These include: Figure 3 Front view and perspective view of a thermoelectric generator with a series of thermoelectric PN junctions produced by capillary casting.
[0027] Figure 5A This is a perspective view of a conductive substrate for a capillary-cast tubular thermoelectric generator according to an exemplary embodiment.
[0028] Figure 5B This is according to an exemplary embodiment, immediately preceding capillary casting. Figure 5A A perspective view of a series of conductive substrates and tubular barrier members used to clamp the series of conductive substrates during capillary casting.
[0029] Figure 6 The following is illustrated by repeated execution according to an exemplary embodiment. Figure 3 An array of multiple thermoelectric generators manufactured by capillary casting.
[0030] Figure 7 An exemplary embodiment is shown. Figure 6 A thermoelectric generator used to generate electricity by combining a heat source and a radiator. Detailed Implementation
[0031] Thermoelectric generators (TEGs) utilize thermal gradients to produce electricity through the Seebeck effect, offering a highly attractive alternative to PV batteries and enabling the generation of power from thermal gradients that would otherwise be wasted. Unlike PV batteries, TEGs do not rely on sunlight, allowing them to operate under a variety of conditions, including indoors or at night. This makes them suitable for applications such as waste heat recovery systems in automotive or industrial environments, where they can utilize thermal gradients that would otherwise be idle and lost as waste heat.
[0032] Despite its potential, widespread adoption of TEG has been hampered by manufacturing challenges. Traditionally, TEG has been manufactured by sintering particles made from a mixture of thermoelectric materials, which often results in inhomogeneity of the mixture and a tendency for the material to crack. Furthermore, sintering requires precise assembly and uses environmentally harmful materials, leading to high production costs, which makes TEG less attractive compared to its photovoltaic counterparts.
[0033] This disclosure addresses these manufacturing obstacles by employing a "capillary casting" method to manufacture TEG. Compared to conventional sintering methods used for TEG, this technology significantly reduces costs associated with TEG production, not only in terms of raw material usage but also by simplifying the manufacturing process, resulting in a more uniform material composition and improved structural integrity. Furthermore, the capillary casting method eliminates the need for the extensive and expensive infrastructure associated with PV cell production. Therefore, the upfront investment and operating costs for establishing TEG manufacturing are only a fraction of those required for a PV cell facility.
[0034] In at least some embodiments and further described below, this disclosure describes a method for manufacturing a PN junction for TEG. Prior to casting, a conductive substrate is sandwiched between a pair of barrier members. The substrate includes a cavity defined by its outer periphery, thereby providing access to the interior of the cavity through a gate at the edge of the substrate. While the substrate is sandwiched, at least a portion of the cavity is immersed in a molten alloy at a higher temperature than the substrate. The molten alloy is tellurium-based (i.e., tellurium is the heaviest component of the alloy by weight), and the cavity is immersed by means of the temperature difference between the substrate and the molten alloy, causing the molten alloy to be drawn into the cavity by capillary action. The substrate is then removed from the molten alloy and allowed to cool, thereby solidifying the molten alloy. Depending on the material used, the conductive substrate acts as either a negative or positive dopant for the PN junction, while the solidified alloy acts as either a negative or positive dopant for the PN junction.
[0035] The immersed conductive substrate may comprise multiple segments spaced apart from each other. In this case, the cavities formed in these segments can be shaped such that one or more castings are formed between corresponding pairs of segments, wherein each of these castings interlocks a corresponding pair of segments in the one or more segments. In this way, welding for connecting these segments can be avoided, thus saving labor and making the TEG mechanically more robust.
[0036] Now refer to Figure 1A and Figure 1BThis illustration shows a front view and a perspective view of a conductive substrate 102 for manufacturing a series of thermoelectric PN junctions according to an exemplary embodiment. In the illustrated embodiment, the substrate 102 is copper, although in other embodiments, the substrate 102 may be made of another metal or alloy, as further described below. The substrate 102 includes a plurality of segments 103 spaced apart from each other. These segments 103 are longitudinally aligned with each other, and each segment 103 includes a pair of cavities 104 located on opposite sides of that segment 103. Each cavity 104 can be accessed from the outside of the segment 103 through a corresponding gate 106 in the segment 103. The periphery of the segment 103 defines the cavity 104; therefore, and as further described below, even if the front and rear sides of the segment 103 are sealed, a liquid such as molten metal can longitudinally cross the left and right ends of the segment 103 and enter the cavity 104. The substrate 102 can be manufactured by precisely cutting a copper sheet of a desired thickness into a desired shape, for example, as shown below. Figure 1A and Figure 1B As shown.
[0037] Figure 2A and Figure 2B The following are examples of the process for manufacturing this series of PN junctions according to exemplary embodiments. Figure 1A and Figure 1B The conductive substrate is sandwiched between the first barrier and the second barrier 202a, b. In the illustrated embodiment, the barrier 202a, b are pure alumina ceramic sheets, although in at least some other embodiments they may simply be ceramic sheets or sheets made of another non-conductive / insulating material. Figure 2A Specifically, barrier members 202a and 202b are lowered to cover the front and rear sides of substrate 102 respectively to clamp substrate 102, and Figure 2B An end view of the substrate 102 and the barriers 202a and b is depicted when the substrate 102 is clamped by the barriers 202a and b. The sandwich substrate 102 is fixed together, for example by using clamps, to ensure proper alignment and stability.
[0038] Figure 3 An exemplary embodiment is shown. Figure 2BThe sandwich conductive substrate 102 is immersed in and then removed from the molten alloy 304 for casting the series of thermoelectric PN junctions using capillary casting. More specifically, the sandwich substrate 102 is lowered into the molten alloy 304 at time t1 to a depth corresponding to an immersion line 302, which corresponds to at least a portion of the gate 106 being immersed in the molten alloy 304. This brings the gate 106 into direct contact with the molten alloy 304. During immersion, due to the temperature difference between the cooler sandwich substrate 102 and the hotter molten alloy 304, the molten alloy 304 is drawn into the mold cavity 104 via its corresponding gate 106 through capillary action, and is also drawn into the space between adjacent sections 103.
[0039] Fused alloy 304 is tellurium-based and may include any one or more of several additional components. For example, fused alloy 304 may also include any one or more of antimony, bismuth, and glass powder, wherein antimony provides structural stability after solidification; bismuth allows the solidified alloy to expand slightly relative to fused alloy 304 to promote a close fit between the solidified alloy and the substrate 102; and glass powder, such as micron-sized (or smaller) glass powder, promotes good adhesion between the solidified alloy and the substrate 102. "Micron-sized" or smaller refers to glass powder whose constituent particles have a diameter of one micron or smaller. Specifically, using glass powder is counterintuitive because glass is an insulator, but experiments have shown that adding appropriate amounts of glass powder promotes good mechanical properties (i.e., adhesion) without unduly impairing conductivity. Various combinations of the above components can be used to manufacture fused alloy 304. For example, bismuth may not be present in fused alloy 304; more generally, fused alloy 304 may include tellurium and any one or more of antimony, bismuth, and glass powder. The exemplary fused alloy 304 may include, for example, 3 parts tellurium, 1.5 parts antimony and 0.1 parts micron-sized glass powder, and optionally also includes 0.5 parts bismuth.
[0040] Once the cavity 104 is filled, the sandwich substrate 102 is removed from the molten alloy 304 at time t2. Typically, the difference between time t1 and t2 is less than 1 second. Once the sandwich substrate 102 is removed, the molten alloy 304 cools, and subsequently, the barrier elements 202a and 202b are removed. The barrier elements 202a and 202b are made of an inert material (i.e., a material that does not physically or chemically bond with the alloy in its molten or solidified state, nor with the substrate 102), and therefore can be removed relatively easily by simply physically pulling the barrier elements 202a and 202b from the substrate 102. If some adhesion exists (e.g., due to some bonding between the barrier elements 202a and 202b and the alloy 304), a release agent such as a boron nitride spray can be used to help release the barrier elements 202a and 202b from the composite substrate 102 and the solidified alloy. The resulting solidified alloy is a homogeneous alloy mixture, which reduces susceptibility to cracking and the environmental hazards associated with conventional powder metallurgy (e.g., sintering).
[0041] Figure 4A and Figure 4B These include: Figure 3 The front and perspective views of TEG402, which is a series of thermoelectric PN junctions 406 produced by capillary casting. Each PN junction 406 is a "thermoelectric module" that generates a voltage across its terminals in response to the thermal difference across the junction 406.
[0042] More specifically, by means of the capillary action described above, which draws molten alloy 304 into the mold cavity 104 and the spaces between the sections 103, Figure 1A and Figure 1B The discontinuous sections 103 have been secured together by a solidified alloy 404 that now interlocks the sections 103 together. In the illustrated embodiment, the width of the gate 106 is less than the maximum width of the mold cavity 104; more specifically, in the illustrated embodiment where the mold cavity 104 is circular, the width of the gate 106 is less than the diameter of the mold cavity 104. This results in the sections 103 forming a jigsaw puzzle-like interlocking connection. Although Figure 4A and Figure 4B The image shows a specific type of interlocking connection, but other interlocking shapes can also be used, as shown below. Figure 5A and Figure 5B As described, the use of solidified alloy 404 to interlock the various sections 103 not only enhances the structural stability of TEG 402 but also improves electrical continuity.
[0043] exist Figure 4A and Figure 4BIn this embodiment, substrate 102 is copper, and solidified alloy 404 comprises 3 parts tellurium, 1.5 parts antimony, 0.5 parts bismuth, and 0.1 parts micron-sized glass powder. Substrate 102 acts as a negative dopant for PN junction 406, while solidified alloy 404 acts as a positive dopant for PN junction 406. However, in at least some other embodiments, substrate 102 may act as a positive dopant, while solidified alloy 404 may act as a negative dopant. For example, in embodiments where substrate 102 is antimony telluride or bismuth telluride instead of copper, substrate 102 may act as a positive dopant.
[0044] therefore, Figure 4A and Figure 4B The TEG 402 comprises several thermoelectric modules in the form of PN junctions 406 connected in series. Each module generates a voltage in response to heat applied across the modules, and because the modules of the TEG 402 are connected in series, the voltages generated by each module are summed. For example, a TEG 402 comprising an array of approximately 100 mm × 50 mm of PN junctions 406 connected in series (each approximately 4 mm long) can generate approximately 5 W of power.
[0045] Figure 6 The following is illustrated by repeated execution according to an exemplary embodiment. Figure 3 The TEG 402 array 600 is manufactured by capillary casting. Any TEG 402 can be connected in series or in parallel (not shown) with any other TEG 402, thereby contributing to the flexibility of power generation.
[0046] As mentioned above, although Figures 1A to 4B The embodiment shown depicts a coplanar substrate 102 and barrier members 202a, b, but other shapes and configurations are also possible. For example, Figure 5A It is used for, for example Figure 5B A perspective view of another embodiment of the conductive substrate 102 with a stacked tubular configuration shown on the left. Figures 1A to 4B Like substrate 102, used for Figure 5A The tubular embodiment of the substrate 102 includes a cavity 104 defined by an outer periphery 108 of the substrate 102 and a corresponding gate 106. The substrate 102 is generally cylindrical and includes a set of two cavities 104 spaced 180 degrees apart on one edge, and another set of two cavities 104 spaced 180 degrees apart on opposite edges, the two sets of cavities being offset from each other by 90 degrees. These substrates 102 may be spaced apart from each other and arranged according to… Figure 5B The edge-to-edge stacking shown on the left has a configuration similar to... Figure 1A The configuration shown in the planar implementation is similar.
[0047] Figure 5B The right side shows a clamping device, according to an exemplary embodiment, as part of performing capillary casting. Figure 5B A series of tubular barrier elements 202a, b on the left side of the conductive substrate 102. In Figure 5B In the process of capillary casting, the first barrier element 202a is in Figure 5B The outer curved surface of the stacked body extends outward, while the second barrier 202b is in Figure 5B The stack extends within the internal curved surface of the stack, thereby clamping the substrate 102. Figure 5A and Figure 5B In this embodiment, when the substrate 102 is clamped, the barrier members 202a and b are also coaxial with the stack of substrates 102. The first barrier member 202a includes a series of holes 502 through which the molten alloy 304 can be drawn into the mold cavity 106 of the substrate 102 by capillary action when the sandwich substrate 102 is immersed in the molten alloy 304. When the substrate segments 103 are clamped by the barrier members 202a and b, the holes 502 are spaced apart between the substrate segments; this allows the molten alloy 304 to be drawn into the space between the segments 103 and into the mold cavity 106 of the corresponding adjacent segments 103 when immersed in the molten alloy 304. Although these holes 502 are in Figure 5B The hole 502 is shown in the first barrier 202a, but in at least some other embodiments (not shown), the hole 502 may be additionally or alternatively provided in the second barrier 202b. The sandwich substrate 102 may then be immersed in the molten alloy 304 and then removed, as described above for the coplanar embodiment, to form TEG.
[0048] Exemplary use cases Although less efficient than photovoltaic panels, thermoelectric panels manufactured using the capillary casting method described above are effective in scenarios with limited sunlight, partial shading, or limited installation space. These panels can operate under a variety of environmental conditions, thus providing a stable power generation solution based on thermal difference and independent of sunlight.
[0049] One exemplary application of TEG 402 is the recovery of waste heat from automotive radiator systems. Internal combustion engine (ICE) vehicles generate a significant amount of heat, much of which is not used for propulsion but is dissipated as waste heat. By integrating a thermoelectric module into the vehicle's radiator system (where coolant captures engine heat), this waste heat can be converted into electrical energy. Figure 7 An exemplary implementation is shown in the figure. Figure 6 The TEG 402 array 600 is used in conjunction with a heat source 702 and a heat sink 704 to generate electrical energy. For ease of illustration, electrical connections to the array 600 and its internal electrical connections are not shown, nor is a frame that can be used to encapsulate and protect the array 600 and ensure good thermal contact with both the heat source 702 and the heat sink 704.
[0050] exist Figure 6 In this configuration, array 600 is positioned such that one side engages with the hot coolant discharged from the engine (i.e., heat source 702), while the opposite side is exposed to ambient temperature or a secondary cooling mechanism (in... Figure 6 (The radiator is 704). The temperature difference across the thermoelectric module induces a voltage via the Seebeck effect, thereby generating electricity that can be used to power the vehicle's electronics, charge the battery, or support other onboard systems. This process effectively recaptures energy that would otherwise be lost, improving the vehicle's overall energy efficiency without requiring external energy input or increasing operational complexity.
[0051] TEG 402's modular design makes it easy to integrate into existing vehicle designs, potentially allowing for retrofitting into existing fleets or incorporating it into new vehicle manufacturing. Integration into vehicles not only reduces fuel consumption by lessening the alternator's power generation load but also aligns with the trend towards improved energy efficiency and a reduced carbon footprint for automobiles.
[0052] It should be understood that various modifications, alterations and adjustments (including but not limited to size, material, location and operating mechanism) can be made to the specific components and configurations disclosed without departing from the nature and scope of this disclosure.
[0053] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting. Therefore, unless the context clearly indicates otherwise, the singular forms “a,” “an,” and “the,” as used herein, are intended to include the plural forms as well. It should also be understood that when the terms “comprises” and “comprising” are used in this specification, they indicate the presence of one or more of the stated features, integers, steps, operations, elements, and components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and groups. Directional terms such as “top,” “bottom,” “upward,” “downward,” “vertically,” and “laterally” are used in the following description only to provide relative reference and are not intended to imply any limitation on how any article of art is positioned in use, how it is mounted in an assembly, or how it is mounted relative to the environment. Furthermore, unless otherwise indicated, the term "connect" and its variations (such as "connected," "connects," and "connecting") used in this specification are intended to include both indirect and direct connections. For example, if a first device is connected to a second device, the coupling can be achieved through a direct connection or through an indirect connection via other devices and connections. Similarly, if a first device is communicatively connected to a second device, communication can be achieved through a direct connection or through an indirect connection via other devices and connections.
[0054] Directional terms such as “top,” “bottom,” “up,” “down,” “vertically,” and “horizontally” are used in the following description only to provide relative reference and are not intended to imply any limitation on how any article is positioned in use, how it is mounted in a component, or how it is mounted relative to the environment.
[0055] The use of phrases such as “at least one of X, Y, and Z,” “at least one of X, Y, or Z,” “at least one or more of X, Y, and Z,” “at least one or more of X, Y, and / or Z,” or “at least one of X, Y, and / or Z” is intended to include single items (e.g., only X, or only Y, or only Z) and multiple items (e.g., {X and Y}, {X and Z}, {Y and Z}, or {X, Y, and Z}). The phrase “at least one” and similar phrases are not intended to convey that every possible item must be present, although every possible item may be present.
[0056] It is anticipated that any aspect or portion of any implementation discussed in this specification may be implemented or combined with any other aspect or portion of any implementation discussed in this specification, provided that such portions are not mutually exclusive.
[0057] While every effort has been made to provide a detailed and accurate description of this disclosure herein, it should be noted that the scope of this disclosure is not limited to the precise configurations and embodiments described. The description provided is intended to illustrate the principles of this disclosure and not to limit it to the specific embodiments shown. The scope of this disclosure is intended to be defined by the appended claims and their equivalents, and their potential applications in other fields.
Claims
1. A method for manufacturing a PN junction for a thermoelectric generator, the method comprising: A conductive substrate is sandwiched between a pair of inert barrier members, wherein the conductive substrate includes a cavity defined by the periphery of the substrate. While the substrate is being clamped, at least a portion of the mold cavity is immersed in a tellurium-based molten alloy at a temperature higher than that of the substrate, wherein immersion of the mold cavity in the molten alloy causes the molten alloy to be drawn into the mold cavity by capillary action; and The molten alloy is solidified by removing the substrate from the molten alloy, wherein the conductive substrate acts as either a negative or positive dopant material of the PN junction, and the solidified alloy acts as either a negative or positive dopant material of the PN junction.
2. The method according to claim 1, wherein, The conductive substrate acts as the positive doping material, while the solidified alloy acts as the negative doping material.
3. The method according to claim 1, wherein, The conductive substrate acts as the negative doping material, while the solidified alloy acts as the positive doping material.
4. The method according to claim 3, wherein, The conductive substrate is copper.
5. The method according to any one of claims 1 to 4, wherein, The pair of barrier elements are ceramic.
6. The method according to claim 5, wherein, The ceramic is alumina ceramic.
7. The method according to any one of claims 1 to 6, wherein, The barrier and the conductive substrate are coplanar.
8. The method according to any one of claims 1 to 6, wherein, The conductive substrate and the barrier are tubular, and the barrier extends inside and outside the conductive substrate, respectively.
9. The method according to any one of claims 1 to 8, wherein, The molten alloy also includes antimony.
10. The method according to any one of claims 1 to 10, wherein, The molten alloy also includes glass powder with a size of micrometer or smaller.
11. The method according to claim 10, wherein, The molten alloy comprises 3 parts of the tellurium, 1.5 parts of the antimony, and 0.1 parts of the micron-sized glass powder.
12. The method according to any one of claims 1 to 10, wherein, The molten alloy also includes bismuth.
13. The method according to claim 10, wherein, The molten alloy comprises 3 parts of the tellurium, 1.5 parts of the antimony, 0.5 parts of the bismuth, and 0.1 parts of the micron-sized glass powder.
14. The method according to any one of claims 1 to 13, wherein: Prior to the immersion, the substrate comprises multiple disconnected segments; During the immersion, the molten alloy is also drawn into the spaces between the sections; and The mold cavity is shaped such that, after solidification, the sections are fixed together by means of the solidified alloy that interlocks the sections together.
15. The method according to claim 14, wherein, During the immersion, the molten alloy enters the mold cavity through a gate, wherein the width of the gate is less than the maximum width of the mold cavity.
16. At least one PN junction for a thermoelectric generator, said at least one PN junction comprising: A conductive substrate comprising multiple segments spaced apart from each other; as well as One or more tellurium-based alloy castings located between corresponding one or more segment pairs, wherein each of the one or more castings interlocks a corresponding segment pair of the one or more segment pairs together, and wherein the conductive substrate acts as one of the negative doping material or positive doping material of the PN junction, and the solidified alloy acts as the other of the negative doping material or positive doping material of the PN junction.
17. The at least one PN junction according to claim 16, wherein, The conductive substrate is copper.
18. At least one PN junction according to claim 16 or 17, wherein, The alloy comprises 3 parts tellurium, 1.5 parts antimony, 0.5 parts bismuth, and 0.1 parts micron-sized glass powder.
19. At least one PN junction according to any one of claims 16 to 18, wherein, The conductive substrate is tubular.
20. At least one PN junction according to any one of claims 16 to 19, wherein, Each of the plurality of sections includes a mold cavity and a gate for accommodating a portion of one of the one or more castings, wherein the width of the gate is less than the maximum width of the mold cavity.