Tray for laminated solar cell coating process
By designing the tray for the laminated solar cell coating process, including the chassis, pressure frame and buffer parts, the problem of high fragmentation rate and plating around the cells when placed on the tray has been solved, and the effective positioning of the cells and reduction of chipped corners have been achieved. Improves the stability of the coating process.
Patent Information
- Application Number
- CN202323354892.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-11
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-11
AI Technical Summary
In the existing technology, placing single-piece finished cells directly on the pallet leads to high fragmentation rate and serious problems around plating.
A tray for the laminated solar cell coating process is designed, which includes a chassis, a pressure frame and a buffer. The chassis is provided with a placement slot for placing the finished cells. The pressure frame is pressed on the chassis to compress the edges of the finished cells. The buffer member is arranged between the pressure frame and the chassis. Through the clearance fit between the boss and the groove and the buffering effect of the spring, it ensures the effective positioning of the battery piece and reduces chipping.
It effectively reduces the phenomenon of plating around, reduces the possibility of chipping at the edge of the cell, improves the closeness of the cell, and reduces the chip rate.
Smart Images

Figure CN221861602U_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of battery technology, and specifically relates to a tray for a laminated solar cell coating process. Background Art
[0002] Crystalline silicon solar cells have the advantages of high stability, low cost, and long life, while perovskite solar cells have the advantages of high photoelectric conversion efficiency, low preparation cost, and flexibility. Crystalline silicon-perovskite tandem cells are a new type of solar cell structure that combines crystalline silicon solar cells with perovskite solar cells, giving full play to the advantages of the two materials. Crystalline silicon-perovskite tandem cells are mainly based on silicon heterojunction bottom cells. Through pyramid velvet modulation technology and efficient interface passivation technology, high-efficiency crystalline silicon-perovskite tandem cells are studied, and key problems such as perovskite velvet film formation and tandem cell opening voltage loss are solved. The efficiency of the tandem cells has been significantly improved. Crystalline silicon-perovskite tandem solar cells can significantly improve cell efficiency without much increase in material costs, and have strong market competitiveness.
[0003] The crystalline silicon heterojunction bottom cell used in the crystalline silicon-perovskite stacked cell is mainly a finished cell prepared by ultra-thin velvet silicon wafers through multiple process steps. After the ultra-thin velvet silicon wafers undergo multiple deposition and coating processes, the finished bottom cell becomes thicker, and due to the presence of structures such as metal gates, the flexibility becomes worse and the bottom cell becomes more brittle. In the prior art, a single finished cell is generally placed directly on a tray, resulting in a high fragmentation rate and serious plating wrap-around. Utility Model Content
[0004] In order to solve the technical problems in the prior art of directly placing a single finished solar cell on a tray, resulting in a high fragmentation rate and serious plating bypass, the present application provides a tray for a laminated solar cell coating process.
[0005] The present application provides a tray for a laminated solar cell coating process, comprising a bottom plate, a pressing frame and a buffer member, wherein:
[0006] The chassis is provided with a placement groove for placing the finished battery cell, and the non-coated surface of the finished battery cell faces the placement groove;
[0007] The pressing frame is pressed onto the chassis to press the edge of the finished battery cell tightly;
[0008] The buffer member is arranged between the pressing frame and the bottom plate.
[0009] In some optional embodiments, the chassis includes a chassis body and a boss, the boss is arranged above the chassis body, and the placement groove is arranged in the boss; the pressing frame includes a pressing frame body and a groove, the groove is arranged at the bottom of the pressing frame body, and when the pressing frame is pressed onto the chassis, the boss matches the groove.
[0010] In some optional embodiments, the pressing frame body includes four frame rods, the top surface of the frame rods includes a first inclined surface, a plane, and a second inclined surface arranged in sequence from the outside to the inside, and the width of the first inclined surface is greater than the width of the second inclined surface.
[0011] In some optional embodiments, the boss and the groove are clearance-fitted.
[0012] In some optional embodiments, a pressing edge is correspondingly provided on the groove, and the pressing edge is the portion where the groove overlaps with the placement slot.
[0013] In some optional embodiments, the width of the pressed edge is 3-10 mm.
[0014] In some optional embodiments, the boss is disposed in the middle of the chassis body, and the chassis body is provided with a bearing portion around the boss, and the buffer component is mounted on the bearing portion.
[0015] In some optional embodiments, the buffer member is a spring, the bottom of the spring is connected to the bearing portion, and the top of the spring contacts the bottom surface of the pressing frame body.
[0016] In some optional embodiments, the elastic force of the spring enables the bottom surface of the groove to maintain zero-pressure contact with the top surface of the finished battery cell.
[0017] In some optional embodiments, the chassis and the pressure frame are made of aluminum or aluminum-magnesium alloy.
[0018] A tray for a laminated solar cell coating process provided according to one or more embodiments of the present application has the following beneficial effects compared to the prior art:
[0019] The chassis is provided with a placement groove for placing finished battery cells; the pressing frame is pressed onto the chassis under the action of its own weight, and presses the edge of the finished battery cell tightly, so that the finished battery cell and the bottom of the placement groove fit closely, thereby ensuring effective positioning of the finished battery cell, and the non-coated surface of the finished battery cell faces the placement groove, and the non-coated surface fits closely with the bottom of the placement groove, thereby greatly reducing the phenomenon of plating bypass; the buffer component is arranged between the pressing frame and the chassis, and when the finished battery cell encounters a slight disturbance, relying on the buffering effect of the buffer component, the possibility of edge chipping of the finished battery cell can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 A schematic diagram of the structure of a tray for a laminated solar cell coating process in one or more embodiments of the present application is shown;
[0021] Figure 2 An exploded view of a tray for a stacked solar cell coating process in one or more embodiments of the present application is shown;
[0022] Figure 3 A cross-sectional view of a tray for a stacked solar cell coating process in one or more embodiments of the present application is shown;
[0023] Figure 4 A schematic structural diagram of a bottom plate of a tray for a stacked solar cell coating process in one or more embodiments of the present application is shown;
[0024] Figure 5 A three-dimensional view of a pressing frame of a tray for a stacked solar cell coating process in one or more embodiments of the present application is shown;
[0025] Figure 6 A cross-sectional view of a pressing frame of a tray for a stacked solar cell coating process in one or more embodiments of the present application is shown;
[0026] Figure 7 This application shows Figure 6 , a partial enlarged view of part A.
[0027] Explanation of the reference numerals: 100 - chassis, 101 - placement groove, 110 - chassis body, 111 - bearing portion, 120 - boss; 200 - press frame, 201 - frame rod, 202 - first inclined surface, 203 - plane, 204 - second inclined surface, 210 - press frame body, 220 - groove, 221 - press edge; 300 - buffer; 400 - finished battery cell. DETAILED DESCRIPTION
[0028] In order to make the technical personnel in the technical field to which the present application belongs to understand the present application more clearly, the technical scheme in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.
[0029] See also Figure 1-Figure 7 The present application embodiment provides a tray for a laminated solar cell coating process, comprising a bottom plate 100, a pressing frame 200 and a buffer member 300, wherein:
[0030] The chassis 100 is provided with a placement groove 101 for placing the finished battery cell 400, the non-coated surface of the finished battery cell 400 faces the placement groove 101, and the top surface of the finished battery cell 400 is the coated surface;
[0031] The pressing frame 200 is pressed on the chassis 100 to press the edge of the finished battery cell 400. The pressing frame 200 is pressed on the chassis 100 under its own weight, and there is no relative sliding between the pressing frame 200 and the chassis 100.
[0032] The buffer member 300 is disposed between the pressing frame 200 and the bottom plate 100 .
[0033] The tray for the laminated solar cell coating process provided in the embodiment of the present application is provided with a placement groove 101 for placing the finished battery cell 400 through the chassis 100; the pressing frame 200 is pressed onto the chassis 100 under the action of its own weight, and presses the edge of the finished battery cell 400 tightly, so that the finished battery cell 400 and the bottom of the placement groove 101 fit closely, ensuring the effective limitation of the finished battery cell 400, and the non-coated surface of the finished battery cell 400 faces the placement groove 101, and the non-coated surface fits closely with the bottom of the placement groove 101, which greatly reduces the plating wrap phenomenon; the buffer 300 is arranged between the pressing frame 200 and the chassis 100, and when the finished battery cell 400 encounters a slight disturbance, relying on the buffering effect of the buffer 300, the possibility of edge chipping of the finished battery cell 400 can be reduced.
[0034] In some optional embodiments, the chassis 100 includes a chassis body 110 and a boss 120, wherein the boss 120 is disposed above the chassis body 110, and the placement groove 101 is disposed in the boss 120; the pressing frame 200 includes a pressing frame body 210 and a groove 220, wherein the groove 220 is disposed at the bottom of the pressing frame body 210, and when the pressing frame 200 is pressed onto the chassis 100, the boss 120 matches the groove 220. By matching the boss 120 with the groove 220, when the pressing frame 200 is pressed onto the chassis 100, there is no relative sliding between the pressing frame 200 and the chassis 100, so that the finished battery cell 400 cannot slide, thereby ensuring effective positioning of the finished battery cell 400.
[0035] In some optional embodiments, the boss 120 and the groove 220 are clearance-matched. The boss 120 and the groove 220 are clearance-matched, so that the pressing frame 200 can be smoothly covered on the chassis 100. After covering, the side wall of the boss 120 can be limited by the side wall of the groove 220 to limit the horizontal sliding of the groove 220, so that the finished battery cell 400 cannot slide, thereby ensuring the effective positioning of the finished battery cell 400.
[0036] In some optional embodiments, the pressing frame body 210 includes four frame rods 201, and the top surface of the frame rod 201 includes a first inclined surface 202, a plane 203, and a second inclined surface 204 arranged in sequence from the outside to the inside, and the width of the first inclined surface 202 is greater than the width of the second inclined surface 204. By sequentially arranging the first inclined surface 202, the plane 203, and the second inclined surface 204 from the outside to the inside, the width of the first inclined surface 202 is greater than the width of the second inclined surface 204, forming a flow field of long upslope + horizontal flow transition zone + short downslope, which is convenient for the effective flow diffusion of the coating growth source and is not easy to form a coating non-growth area.
[0037] In some optional embodiments, the groove 220 is provided with a pressing edge 221, which is the portion where the groove 220 overlaps with the placement groove 101. By providing the pressing edge 221 on the groove 220, the four sides of the finished battery cell 400 are pressed, so that the bottom surface of the finished battery cell 400 is closely attached to the bottom surface of the placement groove 101 without shaking, and even in the atomic layer deposition process, there is basically no wrap-around plating phenomenon on the bottom surface of the finished battery cell 400.
[0038] In some optional embodiments, the width of the edge 221 is 3-10 mm. The width of the edge 221 can be adjusted according to the size of the silicon wafer, preferably set to 3-10 mm, to avoid being too narrow and not being pressed in place, making the finished cell 400 easy to shake, and to avoid being too wide and causing the edge coating to not grow.
[0039] In some optional embodiments, the boss 120 is arranged in the middle of the chassis body 110, and the chassis body 110 is provided with a bearing part 111 around the boss 120, and the buffer 300 is installed on the bearing part 111. The chassis body 110 is provided with a bearing part 111 around the boss 120, and the bearing part 111 is in a shape of four sides. The buffer 300 can be arranged on at least two sides of the bearing part 111 to form a buffer between the chassis body 110 and the cover frame body. When the finished battery cell 400 encounters a slight disturbance, the possibility of the edge of the finished battery cell 400 being broken can be reduced by relying on the buffering effect of the buffer 300. Of course, the buffer 300 can be arranged on two symmetrical sides of the bearing part 111, so that the force of the cover frame body is more uniform, so as to avoid the finished battery cell 400 from being damaged and broken due to excessive local force, and improve the reliability of the device. In this embodiment, buffer members 300 are disposed on the four sides of the bearing portion 111 , which provides a better buffering effect and improves the stability of the device.
[0040] In some optional embodiments, the buffer member 300 is a spring, the bottom of the spring is connected to the bearing part 111, and the top of the spring contacts the bottom surface of the press frame body 210. Specifically, the bearing part 111 is surrounded by a lightweight spring with a certain expansion ratio, so that when the chassis 100 and the press frame 200 are covered, the reverse tensile stress of the spring makes the finished product battery cell 400 not too tightly attached to the bottom surface of the groove 220, and when the pump is started or stopped, the finished battery cell 400 encounters a slight disturbance, and it is not easy to cause the finished product battery cell 400 to break due to the shear stress of its own weight; at the same time, the groove 220 on the upper surface of the finished battery cell 400 and the front surface of the finished product battery cell 400 can easily form a tightly fitting surface, resulting in a non-growth area of the coating on the fitting surface, and the dynamic extension of the bottom spring at different temperatures makes the finished product battery cell 400 not tightly attached to the bottom surface of the groove 220, avoiding the appearance of an edge coating non-growth area on the front perovskite surface caused by being too tight.
[0041] In some optional embodiments, the elastic force of the spring enables the bottom surface of the groove 220 to maintain zero pressure contact with the top surface of the finished battery cell 400. The elastic force of the spring enables the bottom surface of the groove 220 to maintain zero pressure contact with the top surface of the finished battery cell 400, so that the pressing frame body 210 can limit the finished battery cell 400 in the vertical direction without causing the finished battery cell 400 to be broken due to the shear stress of its own weight.
[0042] In some optional embodiments, the chassis 100 and the press frame 200 are made of aluminum or aluminum-magnesium alloy. By using lightweight aluminum or aluminum-magnesium alloy to make the chassis 100 and the press frame 200, the weight of the chassis 100 and the press frame 200 can be reduced, the fragmentation rate can be reduced, and the convenience of overall operation can be improved.
[0043] The working principle of the tray for the stacked solar cell coating process proposed in the embodiment of the present application is: the chassis 100 is placed horizontally in the vacuum coating chamber; the finished product battery cell 400 is placed in the placement groove 101 on the boss 120 of the chassis 100, the bottom surface of the finished product battery cell 400 is a non-coated surface, and the top surface is a uniformly coated surface; the pressing frame 200 is vertically pressed onto the chassis 100, so that the groove 220 falls into the edge of the boss 120, ensuring that the horizontal pressing edge 221 has no obvious shaking; the spring located on the bearing portion 111 is compressed, and the elastic force of the spring makes the bottom surface of the groove 220 maintain zero-pressure contact with the top surface of the finished battery cell 400.
[0044] The tray for the laminated solar cell coating process proposed in the embodiment of the present application has the following advantages:
[0045] (1) The boss 120 and the groove 220 are matched with each other in a clearance, so that the pressing frame 200 can be smoothly covered when covering the chassis 100. After covering, the side wall of the boss 120 can be limited by the side wall of the groove 220 to limit the horizontal sliding of the groove 220, so that the finished battery cell 400 cannot slide, thereby ensuring the effective positioning of the finished battery cell 400. Under the weight of the pressing frame 200 and the limitation of the side wall of the groove 220, the non-coated surface is closely attached to the bottom of the placement groove 101, greatly reducing the phenomenon of plating around;
[0046] (2) The reverse tensile stress of the spring prevents the finished battery cell 400 from being too tightly attached to the bottom surface of the groove 220. When the pump is started or stopped and the finished battery cell 400 encounters a slight disturbance, it is not easy to cause the finished battery cell 400 to be broken due to the shear stress of its own weight. At the same time, the groove 220 on the upper surface of the finished battery cell 400 and the front surface of the finished battery cell 400 can easily form a tightly fitting surface, resulting in a non-growth area of the coating on the fitting surface. The dynamic stretching of the spring at the bottom at different temperatures makes the finished battery cell 400 not tightly attached to the bottom surface of the groove 220, avoiding the appearance of an edge coating non-growth area on the front perovskite surface caused by being too tight.
[0047] (3) The four sides of the finished battery cell 400 are pressed by the corresponding pressing edge 221 provided on the groove 220, so that the bottom surface of the finished battery cell 400 is tightly attached to the bottom surface of the placement groove 101 without shaking. Even in the atomic layer deposition process, there is basically no wrap-around plating phenomenon on the bottom surface of the finished battery cell 400.
[0048] In the present application, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0049] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise" and "counterclockwise" indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0050] In this application, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0051] In addition, the descriptions of "first", "second", etc. in this application are only for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include one or more features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0052] Although the embodiments of the present application have been shown and described, those skilled in the art will appreciate that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present application, and that the scope of the present application is defined by the claims and their equivalents.
Claims
1. A tray for a laminated solar cell coating process, characterized in that: It includes a chassis, a pressure frame and a buffer, wherein: The chassis is provided with a placement groove for placing the finished battery cell, and the non-coated surface of the finished battery cell faces the placement groove; The pressing frame is pressed onto the chassis to press the edge of the finished battery cell tightly; The buffer member is arranged between the pressing frame and the bottom plate.
2. The tray for laminated solar cell coating process according to claim 1, characterized in that: The chassis includes a chassis body and a boss, wherein the boss is arranged above the chassis body, and the placement groove is arranged in the boss; the pressing frame includes a pressing frame body and a groove, wherein the groove is arranged at the bottom of the pressing frame body, and when the pressing frame is pressed onto the chassis, the boss matches the groove.
3. The tray for laminated solar cell coating process according to claim 2, characterized in that: The pressing frame body includes four frame rods, and the top surface of the frame rods includes a first inclined surface, a plane, and a second inclined surface arranged in sequence from the outside to the inside, and the width of the first inclined surface is greater than the width of the second inclined surface.
4. The tray for laminated solar cell coating process according to claim 2, characterized in that: The boss and the groove are clearance-fitted.
5. The tray for laminated solar cell coating process according to claim 2, characterized in that: A pressing edge is correspondingly arranged on the groove, and the pressing edge is the overlapping portion of the groove and the placement slot.
6. The tray for laminated solar cell coating process according to claim 5, characterized in that: The width of the pressed edge is 3-10 mm.
7. The tray for laminated solar cell coating process according to claim 2, characterized in that: The boss is arranged in the middle of the chassis body, and the chassis body is provided with a bearing part around the boss, and the buffer is installed on the bearing part.
8. The tray for laminated solar cell coating process according to claim 7, characterized in that: The buffer member is a spring, the bottom of the spring is connected to the bearing portion, and the top of the spring contacts the bottom surface of the pressing frame body.
9. The tray for laminated solar cell coating process according to claim 8, characterized in that: The elastic force of the spring enables the bottom surface of the groove to maintain zero-pressure contact with the top surface of the finished battery cell.
10. The tray for laminated solar cell coating process according to any one of claims 1 to 9, characterized in that: The chassis and the pressure frame are made of aluminum or aluminum-magnesium alloy.