Thin film capacitor structure of new energy automobile
By arranging a hollow groove at the bottom of the plastic packaging base of the new energy vehicle film capacitor, the problem of the insulating paper being rolled up during the injection molding process is solved, ensuring the stability of the insulation performance and capacitor quality, and achieving good contact between the insulating paper and the copper bar. insulation.
Patent Information
- Application Number
- CN202420322857.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-21
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-02-21
AI Technical Summary
In new energy vehicles, the insulating paper of film capacitors is prone to rolling problems during the injection molding process, affecting the insulation performance.
A hollow groove is provided at the bottom edge of the plastic package base of the capacitor body so that the injection mold can press the edge of the insulating paper to prevent it from rolling over. At the same time, the thickness and flatness of the copper bar, as well as the thickness of the insulating paper and glue layer, are controlled to ensure the stability and stability of the capacitor. quality.
It effectively avoids the curling problem of insulating paper during the injection molding process, ensures the insulation performance and the stability of the capacitor, and avoids deformation during the capacitor processing process.
Smart Images

Figure CN221884913U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of electronic equipment, and in particular to a film capacitor structure of a new energy vehicle. Background Art
[0002] A thin film capacitor is needed in new energy vehicles. It consists of two stacked copper bars. The two copper bars are separated by insulating paper to avoid short circuit between the two copper bars and ensure the insulation requirements between the two copper bars. At the same time, in order to fix the edges of the two copper bars and the insulating paper, they are encapsulated and fixed by injection molding plastic. Therefore, the insulating paper needs to have high temperature resistance. At the same time, in order to ensure that the insulating paper can play a good insulating role between the two copper bars, the insulating paper needs to extend beyond the edge of the lower copper bar. The edge of the insulating paper that extends beyond the edge of the lower copper bar is prone to curling when it is impacted by injection pressure during injection molding, affecting the insulation performance. Utility Model Content
[0003] The utility model aims to provide a thin film capacitor structure for new energy vehicles, and specifically to provide a thin film capacitor structure with good insulation performance for new energy vehicles.
[0004] To achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a thin-film capacitor structure for new energy vehicles, comprising an upper copper busbar, a lower copper busbar, insulating paper and a plastic packaging base, wherein the insulating paper is tightly arranged between the upper copper busbar and the lower copper busbar to form a capacitor body, the edge of the insulating paper exceeds the edge of the lower copper sheet, and the edge of the upper copper busbar exceeds the edge of the insulating paper; the plastic packaging base is encapsulated and fixed to the edge of the capacitor body, and a plurality of hollow grooves are arranged on the bottom edge of the plastic packaging base corresponding to the edge of the insulating paper.
[0005] Preferably, the thickness of the upper copper busbar and the lower copper busbar are both 1±0.03 mm.
[0006] Preferably, the planarity of the upper copper busbar and the lower copper busbar is no greater than 0.1.
[0007] Specifically, the insulating paper is fixedly connected to the upper copper busbar through the first glue layer, and the insulating paper is fixedly connected to the lower copper busbar through the second glue layer.
[0008] Preferably, the overall thickness of the insulating paper, the first glue layer and the second glue layer is 0.35-0.4 mm.
[0009] Preferably, the thickness of the insulating paper is 0.18 mm, and the thickness of the first glue layer and the second glue layer is 0.1 mm.
[0010] The beneficial effect of the utility model is that: by setting a hollow groove at the bottom edge of the plastic packaging base encapsulated on the capacitor body composed of two layers of copper bars and insulating paper, the hollow groove corresponds to the edge portion of the insulating paper that exceeds the edge of the lower copper bar, so that during injection molding, the injection mold at the hollow groove can be used to press the edge of the insulating paper, thereby effectively avoiding the problem of curling of the insulating paper during the injection molding process to affect the insulation performance. At the same time, the thickness and flatness of the copper bar and the overall thickness of the insulating paper are controlled to avoid the problem of deformation affecting the quality during the capacitor processing. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Attached Figure 1 The bottom structure diagram of the film capacitor in the embodiment;
[0012] Attached Figure 2 A diagram showing the split state of a thin film capacitor in an embodiment;
[0013] Attached Figure 3 is an overall structural diagram of the capacitor body in the embodiment;
[0014] Attached Figure 4 A bottom view of a thin film capacitor in an embodiment;
[0015] Attached Figure 5 For attachment Figure 4 Cross-section of the middle AA;
[0016] Attached Figure 6 For attachment Figure 5 Enlarged schematic diagram of part A in the middle. DETAILED DESCRIPTION
[0017] Example 1, reference Figure 1-5 A thin-film capacitor structure for new energy vehicles includes an upper copper busbar 1, a lower copper busbar 2, an insulating paper 3 and a plastic packaging base 4. The insulating paper 3 is tightly arranged between the upper copper busbar 1 and the lower copper busbar 2 to form a capacitor body. The edge of the insulating paper 3 exceeds the edge of the lower copper sheet 2, and the edge of the upper copper busbar 1 exceeds the edge of the insulating paper 3; the plastic packaging base 4 is packaged and fixed to the edge of the capacitor body, and a plurality of hollow grooves 41 are arranged on the bottom edge of the plastic packaging base 4 corresponding to the edge of the insulating paper.
[0018] In this embodiment, the upper copper busbar 1 and the lower copper busbar 2 are separated by the insulating paper 3 to form a capacitor body. After the capacitor body is formed, a plastic packaging base 4 is arranged at the edge of the capacitor body by injection molding, wherein the hollow groove 41 arranged at the bottom edge of the plastic packaging base 4 corresponds to the edge portion of the insulating paper 3 extending beyond the edge of the lower copper busbar 2. Due to the presence of the hollow groove 41, the corresponding injection mold will be provided with a corresponding core at the position of the hollow groove 41. This part of the core can press the edge of the insulating paper 3 to prevent the edge of the insulating paper 3 from curling up during the injection molding process, thereby ensuring the insulation performance of the insulating paper 3 between the upper copper busbar 1 and the lower copper busbar 2, and improving the stability of the capacitor quality.
[0019] Specifically, the insulating paper 3 is fixedly connected to the upper copper busbar 1 through a first glue layer 31 , and the insulating paper 3 is fixedly connected to the lower copper busbar 2 through a second glue layer 32 .
[0020] In order to ensure that the capacitor body can maintain a certain flatness during injection molding and is not prone to deformation, preferably, the thickness of the upper copper bar 1 and the lower copper bar 2 are both 1±0.03mm; the flatness of the upper copper bar 1 and the lower copper bar 2 is not greater than 0.1; the overall thickness of the insulating paper 3, the first glue layer 31 and the second glue layer 32 is 0.35~0.4mm, specifically, the thickness of the insulating paper 3 is 0.18mm, and the thickness of the first glue layer 31 and the second glue layer 32 is 0.1mm.
[0021] Of course, the above are only preferred implementation modes of the present utility model, and are not intended to limit the scope of use of the present utility model. Therefore, any equivalent changes made to the principle of the present utility model should be included in the protection scope of the present utility model.
Claims
1. A thin film capacitor structure for a new energy vehicle, characterized in that: It includes an upper copper bar, a lower copper bar, insulating paper and a plastic packaging base. The insulating paper is tightly arranged between the upper copper bar and the lower copper bar to form a capacitor body. The edge of the insulating paper exceeds the edge of the lower copper sheet, and the edge of the upper copper bar exceeds the edge of the insulating paper. The plastic packaging base is encapsulated and fixed to the edge of the capacitor body, and a plurality of hollow grooves are arranged on the bottom edge of the plastic packaging base corresponding to the edge of the insulating paper.
2. The thin film capacitor structure of a new energy vehicle according to claim 1, characterized in that: The thickness of the upper copper busbar and the lower copper busbar is 1±0.03 mm.
3. The thin film capacitor structure of a new energy vehicle according to claim 2, characterized in that: The planarity of the upper copper busbar and the lower copper busbar is no greater than 0.
1.
4. The thin film capacitor structure of a new energy vehicle according to claim 1, characterized in that: The insulating paper is fixedly connected to the upper copper busbar through a first glue layer, and the insulating paper is fixedly connected to the lower copper busbar through a second glue layer.
5. The thin film capacitor structure of a new energy vehicle according to claim 4, characterized in that: The overall thickness of the insulating paper, the first glue layer and the second glue layer is 0.35-0.4 mm.
6. The thin film capacitor structure of a new energy vehicle according to claim 5, characterized in that: The thickness of the insulating paper is 0.18 mm, and the thickness of the first glue layer and the second glue layer is 0.1 mm.
Citation Information
Cited By
Capacitor copper bar insulation cold pasting connection process method
CN121812390A
Capacitor double-layer copper bar creepage distance fixing process for new energy automobile
CN122000215A