Foaming pillow filled with multi-density materials

Through the integrated foaming process, multi-density materials are preset in the mold to form a multi-density pillow core, which solves the problem that the existing technology cannot meet the different hardness needs of sleep, achieves precise control of pillow core hardness and simplifies production, and improves pillow quality. comfort and longevity.

CN221888020UActive Publication Date: 2024-10-25TENGFEI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420494253.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Priority Date
2023-04-07
Filing Date
2024-03-14
Publication Date
2024-10-25
Estimated Expiration
2034-03-14

AI Technical Summary

Technical Problem

Existing filled foam pillows cannot meet the different softness and hardness needs of the human head during sleep. The traditional process is complicated and difficult to accurately control the hardness of the pillow core, and the splicing joints are easily deformed and reduce the lifespan.

Method used

A foam pillow preparation method filled with multi-density materials is used. Materials of different hardnesses are preset in the mold through an integrated foaming process, and foaming technology is used to form a multi-density pillow core, including a side sleeping area, a brain fossa support area and a neck support area. , avoiding the defects of traditional splicing and jacket foaming.

Benefits of technology

It achieves precise control of the pillow core hardness, simplifies the production process, avoids instability at the splicing joints and foaming of the outer cover, and improves the comfort and service life of the pillow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221888020U_ABST
    Figure CN221888020U_ABST
Patent Text Reader

Abstract

The utility model relates to a foaming pillow filled with multi-density materials, and belongs to the technical field of sleep pillows in the household industry. The foaming pillow comprises a pillow inner which is integrally formed in a foaming mode, the pillow inner comprises a plurality of filling areas, and filling blocks are arranged in the filling areas. The filling area comprises a left sleeping area, a right sleeping area, a brain nest area, a front neck supporting area and a rear neck supporting area; the filling blocks comprise a left sleeping filling block, a right sleeping filling block, a brain nest filling block, a front neck supporting filling block and a rear neck supporting filling block which are respectively arranged in the left sleeping area, the right sleeping area, the brain nest area, the front neck supporting area and the rear neck supporting area. According to the spliced pillow, the technical problems that a traditional spliced pillow is unstable due to the fact that gluing is not firm and tenon-and-mortise splicing gaps are too large are solved; the side sleeping area, the brain nest supporting area and the neck supporting area are arranged on the wrapping part in the pillow inner, and the brain supporting filling modules with different hardness are arranged in the corresponding areas, so that the requirements of different people for different sleeping comfort degrees are met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of sleeping pillows in the home furnishing industry, and particularly relates to a foam pillow filled with multi-density materials. Background Art

[0002] At present, most pillows are filled with a uniform density, which cannot meet the different softness and hardness requirements of the head during sleep. Users want the pillow to be soft, but too soft will lead to a lack of support for the neck, and the neck will feel strained and sore after sleeping for a long time; if the pillow core is too hard as a whole, the brain cavity will not be covered, and the sleeping experience will be poor and uncomfortable. The general solution on the market is to use a softer sponge as the main body of the pillow core, and reserve two grooves in the neck support area at the bottom of the pillow core during molding and foaming, so as to facilitate the later filling of materials of different hardness to meet the requirements of different groups of people for neck comfort, which increases the complexity of the process; another method is to splice materials such as sponges of different hardness by gluing, mortise and tenon joints, etc. in the later stage. The Chinese invention patent application document with publication number: CN115489137A discloses a spliced ​​pillow core formed by splicing a plurality of splicing blocks, the spliced ​​pillow core is molded as a whole, and the base materials of at least two splicing blocks are different, but this method of pillow will cause the splicing of different materials to be unstable due to long-term extrusion, thereby deforming and reducing the lifespan.

[0003] Existing foaming pillows (such as the Chinese invention patent with publication number CN108215047 A) generally use a sewn outer shell, and multiple TPU film bags are attached inside the outer shell. After the headrest shape is sewn, an injection port is left in a hidden place, and the foaming raw materials are injected into the TPU film bag. There will be a film barrier between each density sponge. Our pillow foaming does not require a TPU film bag. It only needs to add multiple raw material nozzles with soft and hard formulas. After injecting a foaming raw material of one softness into the mold, another foaming raw material of another softness is injected immediately. Multiple soft and hard raw materials will merge with each other during the foaming process and be naturally spliced. This method has a complicated production process, and cannot accurately control the hardness of each part of the pillow core. In addition, the formed pillow is generally covered with a coat, which is difficult to be used as a daily home sleep pillow. Utility Model Content

[0004] The main technical problem solved by the utility model is to provide a preparation method of a foam pillow filled with multi-density materials. Through an integrated foaming process: materials of different hardness (sponge, air bag, hose, gel, silica gel, fiber cotton) are pre-placed at designated positions, and the pillow core is wrapped as a whole through foaming technology. The main body of the pillow core is softer memory foam (hardness 0-10 degrees), and other parts, such as the neck groove at the bottom, are polyurethane sponges with a density of 20-35 and a hardness of 25-45, or various hard flower bags and medicine bags. The production process is simplified, and the hardness of specific areas of the pillow can be accurately controlled to meet the hardness requirements of various parts of the human body during sleep.

[0005] In order to solve the above technical problems, a technical solution adopted by the utility model is:

[0006] A method for preparing a foam pillow filled with multi-density materials, comprising the following steps:

[0007] Step 1: Prepare the foaming raw material A and the foaming raw material B according to their specific gravity and store them in a raw material tank;

[0008] Step 2: Mold pretreatment: apply a release agent on the inner wall of the mold cavity and place the filling block at the designated position;

[0009] Step 3: Mixing and pouring: Mix the foaming raw material A and the foaming raw material B evenly, and pour them into the lower mold of the mold after pressurization;

[0010] Step 4: Heating and forming: heating the mold to allow the foaming material in the mold to foam and form, and heat-preserving the mold;

[0011] Step 5. Let it stand and mature: Take out the pillow core and put it on the shelf and let it stand for 24-48 hours to mature.

[0012] Preferably, the foaming raw material A comprises, by mass, 100-120 parts of polyether polyol (molecular weight 3000), 0.1-0.5 parts of catalyst, 2-4 parts of foaming agent, 0.5-2 parts of foam stabilizer, 0-0.1 parts of color paste, and 0.5-2 parts of antioxidant;

[0013] The foaming raw material B includes at least one of toluene diisocyanate and diphenylmethane diisocyanate in an amount of 27-50 parts by mass.

[0014] Preferably, the foaming agent is water or dichloromethane;

[0015] The catalyst includes tertiary amine catalyst and organic metal catalyst;

[0016] The foam stabilizer is silicone oil;

[0017] The antioxidant is an anti-yellowing agent containing phosphorus functional groups and polyhydroxyl groups;

[0018] The release agent is polysiloxane with a melting point of 30°C-60°C.

[0019] Preferably, the step three, mixing and pouring comprises pouring along the inner wall of the lower mold in a clockwise direction for 2-8 seconds with a nozzle flow rate of 100-200 g / s.

[0020] Preferably, the step 2 of placing the filling block at the designated position further comprises pasting or hanging a plurality of filling blocks in the upper mold cavity of the mold according to the human body support position of the pillow core.

[0021] Preferably, in step 4, the temperature of the mold for heating and molding is 30-60° C., and the temperature holding time is 3-8 min.

[0022] A multi-density material filled foam pillow prepared by the above-mentioned multi-density material filled foam pillow preparation method comprises an integrally foamed pillow core, wherein the pillow core comprises a plurality of filling areas, each of which is provided with a filling block.

[0023] Preferably, the filling area includes a left sleeping area, a right sleeping area, a brain fossa area, a front neck support area and a back neck support area, and the filling blocks include a left sleeping filling block, a right sleeping filling block, a brain fossa filling block, a front neck support filling block and a back neck support filling block which are respectively arranged in the left sleeping area, the right sleeping area, the brain fossa area, the front neck support area and the back neck support area.

[0024] Preferably, the hardness of the left sleeping filling block is 10-100°; the hardness of the right sleeping filling block is 10-100°; the hardness of the brain fossa filling block is 0-100°; the hardness of the front neck support filling block is 10-100°; the hardness of the back neck support block is 10-100°.

[0025] It is further preferred that the hardness of the left sleeping filling block is 10-20°; the hardness of the right sleeping filling block is 10-20°; the hardness of the brain fossa filling block is 0-5°; the hardness of the front neck support filling block is 25-45°; and the hardness of the back neck support block is 15-20°.

[0026] Preferably, the filling block comprises any one of sponge, air bag, hose, gel, silica gel, fiber cotton, traditional Chinese medicine and herbal medicine, or any combination of any two or more thereof.

[0027] The beneficial technical effects of the utility model are:

[0028] 1. The utility model arranges a side sleeping area, a brain support area, and a neck support area in the pillow core, and arranges filling modules at corresponding positions to meet the different needs of sleeping people for brain support. The pillow core is foamed in one piece, avoiding the problems of adhesive strength and instability caused by large gaps in mortise and tenon joints in traditional spliced ​​pillows.

[0029] 2. The utility model uses an integrated foaming process for the pillow core, places materials of different hardness in designated positions in advance, and covers the pillow core as a whole through foaming technology, thereby avoiding the problem that traditional foam pillows need to be foamed inside a cover. At the same time, the preparation process of the present application ensures that the foam pillow will not produce odor or surface damage, improves the foaming quality, and allows the foaming material to be better combined with the filling material. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 This is a structural schematic diagram of a foam pillow filled with multi-density materials of the utility model;

[0031] The parts in the accompanying drawings are marked as follows:

[0032] 1. Pillow core, 2. Filling block for sleeping on the left side, 3. Filling block for sleeping on the right side, 4. Filling block for the head cavity, 5. Filling block for front neck support, 6. Filling block for back neck support. DETAILED DESCRIPTION

[0033] In order to more clearly understand the technical means of the utility model and implement it according to the contents of the specification, the specific implementation methods of the utility model are further described in detail below in conjunction with the drawings and embodiments. The following embodiments are used to illustrate the utility model but are not used to limit the scope of the utility model.

[0034] In the description of the present invention, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "front", "back", etc. indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.

[0035] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "set" should be understood in a broad sense, for example, they can be fixedly connected or set, or detachably connected or set, or integrally connected or set. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0036] Embodiment 1:

[0037] This specific embodiment discloses in detail a method for preparing a foam pillow filled with multi-density materials, including the following steps:

[0038] Step 1: Prepare the foaming raw material A and the foaming raw material B according to their specific gravity and store them in a raw material tank;

[0039] Step 2: Mold pretreatment: apply a release agent on the inner wall of the mold cavity and place the filling block at the designated position;

[0040] Step 3: Mixing and pouring: Mix the foaming raw material A and the foaming raw material B evenly, and pour them into the lower mold of the mold after pressurization;

[0041] Step 4: Heating and forming: heating the mold to allow the foaming material in the mold to foam and form, and heat-preserving the mold;

[0042] Step 5. Let it stand and mature: Take out the pillow core and put it on the shelf and let it stand for 24 hours to mature.

[0043] Foaming raw materials A and B are stored in separate raw material tanks. When the machine is started, the raw material components will be extracted according to the set formula dosage, and the actual dosage and flow rate will be recorded through a metering pump. The inside of the mold will be wiped with a release agent in advance (to facilitate removing the sample after foaming is completed), and the hard material will be fixed to the mold punch (upper mold) with double-sided tape. After the raw materials are mixed evenly, they will be injected into the lower mold through a pressure nozzle, heated and formed, taken out after insulation, and placed on a shelf for 24 hours to complete the maturation process.

[0044] Preferably, the foaming raw material A comprises, by mass, 100 parts of polyether polyol (molecular weight 3000), 0.1 parts of catalyst, 2 parts of foaming agent, 0.5 parts of foam stabilizer, 0 parts of color paste, and 0.5 parts of antioxidant;

[0045] The foaming raw material B includes 27 parts by mass of toluene diisocyanate (TDI) or 27 parts by mass of diphenylmethane diisocyanate or 27 parts by mass of a mixture of toluene diisocyanate and diphenylmethane diisocyanate.

[0046] The production of carbamate by polyether polyol and isocyanate (TDI, MDI) is the backbone reaction of the foam reaction.

[0047] Preferably, the foaming agent is dichloromethane; the heat of vaporization of dichloromethane is 29KJ / mol, so dichloromethane as a foaming agent will significantly increase the elongation of the foam and reduce the internal temperature rise during the foam reaction, which is not conducive to the formation of hard segments. Therefore, adding dichloromethane can easily make the foam soften and feel elastic to the touch.

[0048] The catalyst includes a tertiary amine catalyst and an organic metal catalyst; the tertiary amine catalyst in this embodiment is triethylenediamine, which can promote the reaction between the foaming raw material B and the foaming agent; the organic metal catalyst in this embodiment is stannous octoate, which can promote the gel reaction.

[0049] The foam stabilizer is silicone oil; the foam stabilizer can make the pores fine and uniform. When the system is in the low viscosity stage, it stabilizes the pore wall / the pores can grow to a thickness suitable for opening the pores, creating conditions for the final opening of the pores. Bubble opening and pore bursting are necessary stages in the foaming of soft foams, otherwise closed pores will occur, resulting in a decrease in foam performance. However, pore opening and pore bursting must occur when the foaming reaction and gel reaction are basically completed and balanced. That is, when the foam rises to the highest point and the strength of the bubble can support its own weight, otherwise it will also cause the foam to collapse. Therefore, another important function of the foam stabilizer is to dissolve the polyurea generated by the reaction in the early stage of foaming, which can help with pore opening and pore bursting in the later stage of foaming.

[0050] The antioxidant is an anti-yellowing agent containing phosphorus functional groups and polyhydroxyl groups; the macromolecular groups are linked by phosphorus atoms and have good antioxidant effects; the hydroxyl groups can react with excess TDI. The chemical formula of the oxidant is as follows:

[0051]

[0052] Among them: R1 and R2 are connected by C and P (phosphorus atom) to form a phosphorus-containing functional group. It has an antioxidant effect; R3 is a polyhydroxy macromolecule that can combine with multiple phosphorus functional groups and retain some hydroxyl groups. The remaining hydroxyl groups can react with isocyanate (TDI).

[0053] When the pillow is foaming, in order to keep the foam stable, an excessive amount of foaming raw material B is often added to stabilize the foam. However, after the foaming raw material B reacts with the polyether polyol of the foaming raw material A, the excess TDI will react with water in the air to produce aniline and aniline urea. At the same time, aniline and aniline urea have odor and color, which causes the foam pillow core to have odor and deterioration. This problem is solved by adding an antioxidant. The reaction rate of the antioxidant with TDI is lower than that of the polyether polyol and higher than that of the water in the air. The antioxidant reacts with TDI and consumes TDI, thereby avoiding the problem of odor and deterioration of the foam pillow core.

[0054] The release agent has a melting point of 30°C polysiloxane. Oily wax dispersions are commonly used. Frequent wiping will form a white wax layer inside the mold, which will affect the size and appearance of the product. Low-melting-point water-based polysiloxane has the characteristics of a low melting point and will evaporate and dry quickly after wiping. It can polymerize into a solid film on the mold surface. One application can be used for many consecutive production cycles, thereby improving production efficiency.

[0055] Preferably, the step three, mixing and pouring includes pouring the mixture along the inner wall of the lower mold clockwise for 2-8 seconds, and the nozzle flow rate is 100g / s. Too high a nozzle flow rate during pouring will cause a large amount of air to be mixed into the raw materials, and there will be more bubbles in the pillow core, resulting in poor foaming effect.

[0056] Preferably, the step 2 of placing the filling block at the designated position further comprises pasting or hanging a plurality of filling blocks in the upper mold cavity of the mold according to the human body support position of the pillow core.

[0057] Preferably, in the step 4, the mold temperature for heating and molding is 30° C., and the insulation time is 3 minutes.

[0058] A multi-density material filled foam pillow prepared by the above-mentioned multi-density material filled foam pillow preparation method comprises an integrally foamed pillow core 1, wherein the pillow core comprises a plurality of filling areas, each of which is provided with a filling block.

[0059] Preferably, the filling area includes a left sleeping area, a right sleeping area, a brain fossa area, a front neck support area and a back neck support area, and the filling blocks include a left sleeping filling block 2, a right sleeping filling block 3, a brain fossa filling block 4, a front neck support filling block 5 and a back neck support filling block 6 which are respectively arranged in the left sleeping area, the right sleeping area, the brain fossa area, the front neck support area and the back neck support area.

[0060] Preferably, the hardness of the left sleeping filling block is 10-20°, the hardness of the right sleeping filling block is 10-20°, the hardness of the brain fossa filling block is 0-5°, the hardness of the front neck support filling block is 25-45°, and the hardness of the back neck support block is 15-20°.

[0061] Preferably, the filling block comprises any one of sponge, air bag, hose, gel, silica gel, fiber cotton, traditional Chinese medicine and herbal medicine, or any combination of any two or more thereof.

[0062] The present application sets a side sleeping area, a brain support area, and a neck support area through the covering part inside the pillow core, and sets filling modules at the corresponding positions to solve the different needs of brain support for sleeping people. The pillow core is foamed in one piece, avoiding the problems of adhesive strength of traditional spliced ​​pillows and instability caused by excessive gaps in mortise and tenon joints.

[0063] Embodiment 2:

[0064] This specific embodiment discloses in detail a method for preparing a foam pillow filled with multi-density materials, including the following steps:

[0065] Step 1: Prepare the foaming raw material A and the foaming raw material B according to their specific gravity and store them in a raw material tank;

[0066] Step 2: Mold pretreatment: apply a release agent on the inner wall of the mold cavity and place the filling block at the designated position;

[0067] Step 3: Mixing and pouring: Mix the foaming raw material A and the foaming raw material B evenly, and pour them into the lower mold of the mold after pressurization;

[0068] Step 4: Heating and forming: heating the mold to allow the foaming material in the mold to foam and form, and heat-preserving the mold;

[0069] Step 5. Let it stand and mature: Take out the pillow core and put it on the shelf and let it stand for 48 hours to mature.

[0070] Foaming raw materials A and B are stored in separate raw material tanks. When the machine is started, the raw material components will be extracted according to the set formula dosage, and the actual dosage and flow rate will be recorded through a metering pump. The inside of the mold will be wiped with a release agent in advance (to facilitate removing the sample after foaming is completed), and the hard material will be fixed to the mold punch (upper mold) with double-sided tape. After the raw materials are mixed evenly, they are injected into the lower mold through a pressure nozzle, heated and formed, taken out after insulation, and placed on a shelf for 48 hours to complete the maturation process.

[0071] Preferably, the foaming raw material A comprises, by mass, 120 parts of polyether polyol (molecular weight 3000), 0.5 parts of catalyst, 4 parts of foaming agent, 2 parts of foam stabilizer, 0.1 parts of color paste, and 2 parts of antioxidant;

[0072] The foaming raw material B includes 50 parts by mass of toluene diisocyanate (TDI) or 50 parts by mass of diphenylmethane diisocyanate or 50 parts by mass of a mixture of toluene diisocyanate and diphenylmethane diisocyanate.

[0073] The production of carbamate by polyether polyol and isocyanate (TDI, MDI) is the backbone reaction of the foam reaction.

[0074] Preferably, the foaming agent is dichloromethane; the heat of vaporization of dichloromethane is 29KJ / mol, so dichloromethane as a foaming agent will significantly increase the elongation of the foam and reduce the internal temperature rise during the foam reaction, which is not conducive to the formation of hard segments. Therefore, adding dichloromethane can easily make the foam soften and feel elastic to the touch.

[0075] The catalyst includes a tertiary amine catalyst and an organic metal catalyst; the tertiary amine catalyst in this embodiment is triethylenediamine, which can promote the reaction between the foaming raw material B and the foaming agent; the organic metal catalyst in this embodiment is stannous octoate, which can promote the gel reaction.

[0076] The foam stabilizer is silicone oil; the foam stabilizer can make the pores fine and uniform. When the system is in the low viscosity stage, it stabilizes the pore wall / the pores can grow to a thickness suitable for opening the pores, creating conditions for the final opening of the pores. Bubble opening and pore bursting are necessary stages in the foaming of soft foams, otherwise closed pores will occur, resulting in a decrease in foam performance. However, pore opening and pore bursting must occur when the foaming reaction and gel reaction are basically completed and balanced. That is, when the foam rises to the highest point and the strength of the bubble can support its own weight, otherwise it will also cause the foam to collapse. Therefore, another important function of the foam stabilizer is to dissolve the polyurea generated by the reaction in the early stage of foaming, which can help with pore opening and pore bursting in the later stage of foaming.

[0077] The antioxidant is an anti-yellowing agent containing phosphorus functional groups and polyhydroxyl groups; the macromolecular groups are linked by phosphorus atoms and have good antioxidant effects; the hydroxyl groups can react with excess TDI. The hydroxyl groups can react with excess TDI. The chemical formula of the oxidant is as follows:

[0078]

[0079] Among them: R1 and R2 are connected by C and P (phosphorus atom) to form a phosphorus-containing functional group. It has an antioxidant effect; R3 is a polyhydroxy macromolecule that can combine with multiple phosphorus functional groups and retain some hydroxyl groups. The remaining hydroxyl groups can react with isocyanate (TDI).

[0080] When the pillow is foaming, in order to keep the foam stable, an excessive amount of foaming raw material B is often added to stabilize the foam. However, after the foaming raw material B reacts with the polyether polyol of the foaming raw material A, the excess TDI will react with water in the air to produce aniline and aniline urea. At the same time, aniline and aniline urea have odor and color, which causes the foam pillow core to have odor and deterioration. This problem is solved by adding an antioxidant. The reaction rate of the antioxidant with TDI is lower than that of the polyether polyol and higher than that of the water in the air. The antioxidant reacts with TDI and consumes TDI, thereby avoiding the problem of odor and deterioration of the foam pillow core.

[0081] The release agent has a melting point of 60°C polysiloxane. Oily wax dispersions are commonly used. Frequent wiping will form a white wax layer inside the mold, which will affect the size and appearance of the product. Low-melting-point water-based polysiloxane has the characteristics of a low melting point and will evaporate and dry quickly after wiping. It can polymerize into a solid film on the mold surface. One application can be used for many consecutive production cycles, thereby improving production efficiency.

[0082] Preferably, the step three, mixing and pouring includes pouring along the inner wall of the lower mold clockwise for 8 seconds with a nozzle flow rate of 200g / s. Too high a nozzle flow rate during pouring will cause a large amount of air to be mixed into the raw materials, and there will be more bubbles in the pillow core, resulting in poor foaming effect.

[0083] Preferably, the step 2 of placing the filling block at the designated position further comprises pasting or hanging a plurality of filling blocks in the upper mold cavity of the mold according to the human body support position of the pillow core.

[0084] Preferably, in step 4, the mold temperature for heating and molding is 60° C., and the temperature holding time is 8 minutes.

[0085] A multi-density material filled foam pillow prepared by the above-mentioned multi-density material filled foam pillow preparation method comprises an integrally foamed pillow core, wherein the pillow core comprises a plurality of filling areas, each of which is provided with a filling block.

[0086] Preferably, the filling area includes a left sleeping area, a right sleeping area, a brain fossa area, a front neck support area and a back neck support area, and the filling blocks include a left sleeping filling block, a right sleeping filling block, a brain fossa filling block, a front neck support filling block and a back neck support filling block which are respectively arranged in the left sleeping area, the right sleeping area, the brain fossa area, the front neck support area and the back neck support area.

[0087] Preferably, the left sleeping filling block is a right-angle trapezoidal sponge with a hardness of 10-20°, a shape of 5 cm upper bottom, 10 cm lower bottom, and 10 cm high, and a density of 20 g / cm 3 The right sleeping filling block is a right-angle trapezoidal sponge with a hardness of 10-20°, a shape of 5cm upper bottom, 10cm lower bottom, and 10cm high, and a density of 20g / cm 3 The brain fossa filling block is a square sponge with a hardness of 0-5°, a side length of 10 cm, and a density of 10g / cm 3 The front neck support filling block is a rectangular sponge with a hardness of 25-45°, a length of 10 cm and a width of 5 cm, and a density of 25 g / cm 3 The back neck support block is a rectangular sponge with a hardness of 15-20° and a length of 8cm and a width of 3cm and a density of 25g / cm 3 .

[0088] Preferably, the filling block comprises any one of sponge, air bag, hose, gel, silica gel, fiber cotton, traditional Chinese medicine and herbal medicine, or any combination of any two or more thereof.

[0089] The present application sets a side sleeping area, a brain support area, and a neck support area through the covering part inside the pillow core, and sets filling modules at the corresponding positions to solve the different needs of brain support for sleeping people. The pillow core is foamed in one piece, avoiding the problems of adhesive strength of traditional spliced ​​pillows and instability caused by excessive gaps in mortise and tenon joints.

[0090] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. It should be pointed out that a person skilled in the art can make several improvements and modifications without departing from the technical principle of the present invention, and these improvements and modifications should also be regarded as within the protection scope of the present invention.

Claims

1. A foam pillow filled with multi-density materials, characterized by: The invention comprises an integrally foamed pillow core, the pillow core comprises a plurality of filling areas, each of the filling areas is provided with a filling block; the filling area comprises a left sleeping area, a right sleeping area, a brain fossa area, a front neck support area and a back neck support area, and the filling blocks comprise a left sleeping filling block, a right sleeping filling block, a brain fossa filling block, a front neck support filling block and a back neck support filling block which are respectively arranged in the left sleeping area, the right sleeping area, the brain fossa area, the front neck support area and the back neck support area.

2. A foam pillow filled with multi-density materials according to claim 1, characterized in that: The hardness of the left side sleeping filling block is 10-100°.

3. The foam pillow filled with multi-density materials according to claim 1, characterized in that: The hardness of the right side sleeping filling block is 10-100°.

4. The foam pillow filled with multi-density materials according to claim 1, characterized in that: The hardness of the brain fossa filling block is 0-100°.

5. The foam pillow filled with multi-density materials according to claim 1, characterized in that: The hardness of the front neck support filling block is 10-100°.

6. The foam pillow filled with multi-density materials according to claim 1, characterized in that: The hardness of the back neck supporting filling block is 10-100°.

7. The foam pillow filled with multi-density materials according to claim 1, characterized in that: The filling block includes any one of sponge, air bag, hose, gel, silica gel, fiber cotton and traditional Chinese medicine or any combination of any two or more thereof.

8. The foam pillow filled with multi-density materials according to claim 1, characterized in that: The hardness of the left-side sleeping filling block is 10-20°, the hardness of the right-side sleeping filling block is 10-20°, the hardness of the brain fossa filling block is 0-5°, the hardness of the front neck support filling block is 25-45°, and the hardness of the back neck support filling block is 15-20°.