Step golden finger plate pressing module
By designing a reasonable component stacking structure and covering protective layer in the step gold finger board lamination module, the problems of glue flow and plate damage in the production of step gold finger boards are solved, improving product quality and reducing costs.
Patent Information
- Application Number
- CN202420473581.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-11
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-03-11
AI Technical Summary
During the production process of step gold finger boards, glue flow, board damage and defective parts often occur, which affects product quality.
A step gold finger board lamination module is designed, which includes an upper buffer component, an upper core board, an upper adhesive layer, a sub-board, a covering protective layer, a lower adhesive layer, a lower core board and a lower Buffer components, through reasonable setting and stacking structure, use a covering protective layer (polyimide film) to cover the pads to enhance adhesion to avoid glue flow and board damage, and remove the protective layer during subsequent depth-controlled slot milling to ensure Avoid glue residue.
It effectively avoids glue flow and plate damage, improves product quality, reduces costs, and simplifies the operating process.
Smart Images

Figure CN221930268U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a step gold finger plate pressing module. Background Art
[0002] With the development of multifunctional electronic product technology, in order to improve product performance, product assembly density, and reduce product volume and weight, the design of PCB is also changing with each passing day. At the same time, in order to increase the heat dissipation area and enhance the safety of surface components, and meet the high-speed and high-information requirements of communication products, it is necessary to design groove area to fix components, and the step board design came into being. At the same time, with the rapid development of the electronics and communications industries, high-frequency and RF designs are becoming more and more extensive, and step boards are increasingly using high-frequency materials to meet the requirements of signal transmission. The step gold finger board can meet higher signal transmission speed and sensitivity requirements, and can achieve high-density and high-reliability component connection and layout, while improving space utilization and performance stability. However, in the production process of the step gold finger board, it is often necessary to press the step gold finger board pressing module, which is prone to glue flow and board damage, and it is easy to have poor loading. Utility Model Content
[0003] In order to overcome the deficiencies of the prior art, the utility model aims to provide a step gold finger plate pressing module, which can avoid glue flow and plate damage, thereby avoiding the situation of poor component loading.
[0004] The purpose of the utility model is achieved by the following technical solutions:
[0005] A step gold finger board pressing module comprises an upper buffer assembly, an upper core board, an upper adhesive layer, a sub-board, a covering protective layer, a lower adhesive layer, a lower core board and a lower buffer assembly; the lower adhesive layer and the lower core board are combined to form a lower combined layer, and a slotted area for milling grooves is provided on the lower combined layer; the lower end of the slotted area extends to the lower core board, and the upper end of the slotted area extends to the lower adhesive layer; the covering protective layer is adhered to the lower adhesive layer and is opposite to the slotted area; the upper buffer assembly, the upper core board, the upper adhesive layer, the sub-board, the lower adhesive layer, the lower core board and the lower buffer assembly are stacked in sequence from top to bottom; a soldering pad is provided on the sub-board, and the covering protective layer covers and adheres to the soldering pad of the sub-board, and the adhesive force between the covering protective layer and the lower adhesive layer is greater than the adhesive force between the covering protective layer and the soldering pad.
[0006] The covering protection layer is a polyimide film used for covering and adhering to the pad.
[0007] The lower core board includes a first core board dielectric layer, a first upper copper foil layer and a first lower copper foil layer; the first upper copper foil layer is located above the first lower copper foil layer; the first core board dielectric layer is arranged between the first upper copper foil layer and the first lower copper foil layer; the lower adhesive layer is stacked above the first upper copper foil layer.
[0008] The slotted area extends from the first lower copper foil layer of the lower core board to the lower adhesive layer.
[0009] The slotted area is rectangular.
[0010] The sub-board includes a middle dielectric layer, a second upper copper foil layer and a second lower copper foil layer; the second upper copper foil layer is located above the second lower copper foil layer; the middle dielectric layer is arranged between the second upper copper foil layer and the second lower copper foil layer, and the pad is located on the second lower copper foil layer.
[0011] The upper adhesive layer includes an upper prepreg.
[0012] The underlying adhesive layer includes an underlying prepreg.
[0013] The upper buffer component comprises an upper buffer paper cushion layer and an upper release film layer; the upper buffer paper cushion layer and the upper release film layer are arranged in sequence from top to bottom.
[0014] The lower buffer component comprises a lower buffer paper cushion layer and a lower release film layer; the lower release film layer and the lower buffer paper cushion layer are arranged in sequence from top to bottom.
[0015] Compared with the prior art, the beneficial effects of the present invention are:
[0016] The utility model provides a step gold finger board pressing module, which can avoid glue flow and board damage by reasonably arranging an upper buffer component, an upper core board, an upper adhesive layer, a sub-board, a covering protective layer, a lower adhesive layer, a lower core board and a lower buffer component. The covering protective layer can be removed together when the depth of the grooved area is controlled and milled subsequently to avoid residual glue on the pad, so as to avoid the problem of poor assembly and improve the quality of the product. Moreover, the product quality can be improved at a low cost, which is conducive to promotion. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a structural schematic diagram of the utility model;
[0018] Figure 2 It is an exploded schematic diagram of the utility model;
[0019] Among them, 10, upper buffer assembly; 11, upper buffer paper pad layer; 12, upper release film layer; 20, upper core board; 21, second core board dielectric layer; 22, third upper copper foil layer; 23, third lower copper foil layer; 30, upper adhesive layer; 40, sub-board; 41, solder pad; 42, middle dielectric layer; 43, second upper copper foil layer; 44, second lower copper foil layer; 50, covering protective layer; 60, lower adhesive layer; 70, lower core board; 71, first core board dielectric layer; 72, first upper copper foil layer; 73, first lower copper foil layer; 80, lower buffer assembly; 81, lower buffer paper pad layer; 82, lower release film layer; 91, slotting area. DETAILED DESCRIPTION
[0020] The present invention is further described below in conjunction with the accompanying drawings and specific implementation methods. It should be noted that, under the premise of no conflict, the various embodiments or technical features described below can be arbitrarily combined to form a new embodiment.
[0021] like Figure 1-2 As shown, a step gold finger board pressing module comprises an upper buffer assembly 10, an upper core board 20, an upper adhesive layer 30, a sub-board 40, a covering protective layer 50, a lower adhesive layer 60, a lower core board 70 and a lower buffer assembly 80; the lower adhesive layer 60 and the lower core board 70 are combined to form a lower assembly layer, and a slotted area 91 for milling a groove is provided on the lower assembly layer; the lower end of the slotted area 91 extends to the lower core board 70, and the upper end of the slotted area 91 extends to the lower adhesive layer 60; The covering protective layer 50 is adhered to the lower adhesive layer 60 and is opposite to the groove area 91; the upper buffer component 10, the upper core board 20, the upper adhesive layer 30, the sub-board 40, the lower adhesive layer 60, the lower core board 70, and the lower buffer component 80 are stacked in sequence from top to bottom; the sub-board 40 is provided with a soldering pad 41, and the covering protective layer 50 covers and adheres to the soldering pad 41 of the sub-board 40, and the adhesion between the covering protective layer 50 and the lower adhesive layer 60 is greater than the adhesion between the covering protective layer 50 and the soldering pad 41.
[0022] The utility model provides a step gold finger board pressing module, which reasonably arranges an upper buffer component 10, an upper core board 20, an upper adhesive layer 30, a sub-board 40, a covering protective layer 50, a lower adhesive layer 60, a lower core board 70 and a lower buffer component 80. In the process of pressing using a vacuum fast press, the upper buffer component 10 and the upper buffer component 10 can be used to balance pressure and block glue, effectively control the uniformity of board thickness, and cover the pad 41 of the sub-board 40 with the covering protective layer 50 to avoid glue flow and board damage. At the same time, because the adhesion between the covering protective layer 50 and the lower adhesive layer 60 is greater than the adhesion between the covering protective layer 50 and the pad 41, the covering protective layer 50 can be removed together with the grooved area 91 when the groove is subsequently milled to control the depth of the groove 91, so as to avoid residual glue on the pad 41, so as to avoid the situation of poor assembly, improve the quality of the product, and at the same time, improve the product quality, and the cost is low, which is conducive to promotion.
[0023] The covering protective layer 50 is a polyimide film used to cover and adhere to the pad 41. During the high temperature and high pressure lamination process, the polyimide film can be closely attached to the pad 41, and the holding force performance is good, so as to improve the protection of the pad 41. At the same time, the adhesion between the polyimide film and the underlying adhesive layer 60 is greater than the adhesion between the polyimide film and the smooth and flush pad 41. When the groove area 91 is subsequently milled to control the depth, the polyimide film can be removed together to avoid residual glue on the pad 41, which is convenient for operation.
[0024] Specifically, the polyimide film is a covering film cut by laser, so that it is convenient to process.
[0025] The lower core board 70 includes a first core board dielectric layer 71, a first upper copper foil layer 72 and a first lower copper foil layer 73; the first upper copper foil layer 72 is located above the first lower copper foil layer 73; the first core board dielectric layer 71 is arranged between the first upper copper foil layer 72 and the first lower copper foil layer 73; the lower adhesive layer 60 is stacked on the first upper copper foil layer 72. The slotted area 91 extends from the first lower copper foil layer 73 of the lower core board 70 to the lower adhesive layer 60. The slotted area 91 is rectangular. By adopting the above-mentioned arrangement, it is convenient to control the depth of the slotted area 91 and reduce the manufacturing cost.
[0026] The sub-board 40 includes a middle dielectric layer 42, a second upper copper foil layer 43 and a second lower copper foil layer 44; the second upper copper foil layer 43 is located above the second lower copper foil layer 44; the middle dielectric layer 42 is arranged between the second upper copper foil layer 43 and the second lower copper foil layer 44, and the pad 41 is located in the second lower copper foil layer 44 to reduce the manufacturing cost.
[0027] The upper core board 20 includes a second core board dielectric layer 21, a third upper copper foil layer 22 and a third lower copper foil layer 23; the third upper copper foil layer 22 is located above the third lower copper foil layer 23; the second core board dielectric layer 21 is arranged between the third upper copper foil layer 22 and the third lower copper foil layer 23; the upper adhesive layer 30 is stacked below the third lower copper foil layer 23. By adopting the above arrangement, the manufacturing cost can be reduced.
[0028] The upper adhesive layer 30 includes an upper prepreg. The number of the upper prepregs included in the upper adhesive layer 30 can be set according to actual needs, for example, one or two.
[0029] The lower adhesive layer 60 includes a lower prepreg. On the basis of using the polyimide film for the cover protection layer 50, the lower adhesive layer 60 is further made of a lower prepreg, which can improve the adhesion between the cover protection layer 50 and the lower adhesive layer 60.
[0030] The number of the lower prepreg sheets included in the lower adhesive layer 60 can be set according to actual needs, for example, one or two.
[0031] The upper buffer assembly 10 includes an upper buffer paper cushion layer 11 and an upper release film layer 12; the upper buffer paper cushion layer 11 and the upper release film layer 12 are arranged in sequence from top to bottom. By adopting the above arrangement of the upper buffer assembly 10, the upper core plate 20 does not directly contact the upper buffer paper cushion layer 11, further improving the pressure equalization and glue resistance.
[0032] The lower buffer assembly 80 includes a lower buffer paper cushion layer 81 and a lower release film layer 82; the lower release film layer 82 and the lower buffer paper cushion layer 81 are arranged in sequence from top to bottom. By adopting the above arrangement of the lower buffer assembly 80, the lower core plate 70 does not directly contact the lower buffer paper cushion layer 81, further improving the pressure equalization and glue resistance.
[0033] The above-mentioned implementation modes are only preferred implementation modes of the present invention, and cannot be used to limit the protection scope of the present invention. Any non-substantial changes and substitutions made by technicians in this field on the basis of the present invention shall fall within the scope of protection required by the present invention.
Claims
1. A step gold finger plate pressing module, characterized in that: It includes an upper buffer component, an upper core plate, an upper adhesive layer, a sub-plate, a covering protective layer, a lower adhesive layer, a lower core plate and a lower buffer component; the lower adhesive layer and the lower core plate are combined to form a lower combined layer, and a slotted area for milling grooves is provided on the lower combined layer; the lower end of the slotted area extends to the lower core plate, and the upper end of the slotted area extends to the lower adhesive layer; the covering protective layer is adhered to the lower adhesive layer and is opposite to the slotted area; the upper buffer component, the upper core plate, the upper adhesive layer, the sub-plate, the lower adhesive layer, the lower core plate and the lower buffer component are stacked in sequence from top to bottom; a soldering pad is provided on the sub-plate, and the covering protective layer covers and adheres to the soldering pad of the sub-plate, and the adhesion between the covering protective layer and the lower adhesive layer is greater than the adhesion between the covering protective layer and the soldering pad.
2. The step gold finger plate pressing module according to claim 1, characterized in that: The covering protection layer is a polyimide film used for covering and adhering to the pad.
3. The step gold finger plate pressing module according to claim 1, characterized in that: The lower core board includes a first core board dielectric layer, a first upper copper foil layer and a first lower copper foil layer; the first upper copper foil layer is located above the first lower copper foil layer; the first core board dielectric layer is arranged between the first upper copper foil layer and the first lower copper foil layer; the lower adhesive layer is stacked above the first upper copper foil layer.
4. The step gold finger plate pressing module according to claim 3, characterized in that: The slotted area extends from the first lower copper foil layer of the lower core board to the lower adhesive layer.
5. The step gold finger plate pressing module according to claim 3, characterized in that: The slotted area is rectangular.
6. The step gold finger plate pressing module according to claim 1, characterized in that: The sub-board includes a middle dielectric layer, a second upper copper foil layer and a second lower copper foil layer; the second upper copper foil layer is located above the second lower copper foil layer; the middle dielectric layer is arranged between the second upper copper foil layer and the second lower copper foil layer, and the pad is located on the second lower copper foil layer.
7. The step gold finger plate pressing module according to claim 1, characterized in that: The upper adhesive layer includes an upper prepreg.
8. The step gold finger plate pressing module according to claim 1, characterized in that: The underlying adhesive layer includes an underlying prepreg.
9. The step gold finger plate pressing module according to claim 1, characterized in that: The upper buffer component comprises an upper buffer paper cushion layer and an upper release film layer; the upper buffer paper cushion layer and the upper release film layer are arranged in sequence from top to bottom.
10. The step gold finger plate pressing module according to claim 1, characterized in that: The lower buffer component comprises a lower buffer paper cushion layer and a lower release film layer; the lower release film layer and the lower buffer paper cushion layer are arranged in sequence from top to bottom.