Laser welding protective cover plate

By designing the protective gas passage and dust removal channel through the inclination angle, the dust removal and protective gas injection process are isolated, and the problem of poor welding in the prior art is solved, and the stability and quality improvement of the welding process is achieved.

CN221935671UActive Publication Date: 2024-11-01广东瑞浦兰钧能源有限公司
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420507604.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-15
Publication Date
2024-11-01
Estimated Expiration
2034-03-15

AI Technical Summary

Technical Problem

In the existing laser welding protective cover plate, the dust removal process and the protective air jet process affect each other, resulting in poor welding of the adapter sheet.

Method used

A laser welding protective cover plate is designed, including a protective gas channel, a dust removal channel and a laser channel. The channels penetrate to the laser channel at a certain inclination angle respectively to prevent the outlets of the protective gas and the dust removal channel from overlapping in the laser channel, thereby isolating the dust removal and Protect the air jet process.

Benefits of technology

It effectively solves the problem of mutual interference between the dust removal process and the protective air jet process, ensures the stability and quality of the welding process, and avoids poor welding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221935671U_ABST
    Figure CN221935671U_ABST
Patent Text Reader

Abstract

The utility model discloses a laser welding protective cover plate which comprises a first pressing plate, a protective gas channel, a dust removal channel and a laser channel are arranged in the first pressing plate, and the protective gas channel, the dust removal channel and the laser channel all penetrate through the first pressing plate. A first inclined angle is formed between the dust removal channel and the horizontal direction; the second pressing plate is connected with the first pressing plate, the laser channel penetrates through the second pressing plate, and the dust removal channel and the shielding gas channel penetrate to the laser channel from the side, close to the first pressing plate, of the second pressing plate. And a second inclined angle is formed between the shielding gas channel and the horizontal direction in the second pressing plate. By means of the laser welding protection cover plate, the problem that in the prior art, when an adapter piece is welded, the dust removal process and the shielding gas spraying process influence each other, and consequently the adapter piece is poor in welding can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of batteries and relates to a laser welding protective cover plate. Background Art

[0002] When laser welding the adapter, the high-energy heat source of the laser will quickly melt the material of the adapter to form a molten pool keyhole. The metal in the molten state is very active and can easily undergo a violent oxidation reaction with oxygen in the atmosphere. Intuitively, a large amount of welding slag splashes and slag is everywhere. For this reason, shielding gas is added during the welding process to isolate the molten pool from oxygen. The shielding gas spraying around the molten pool will form a flowing inert gas environment, so that the molten metal will not come into direct contact with oxygen.

[0003] However, in the existing protective cover, since the protective gas port for spraying protective gas and the dust removal port for dust removal during the welding process are not separated, the protective gas will be sucked away during dust removal, and the protective gas will make the dust removal unstable when spraying protective gas, resulting in poor welding of the adapter. Utility Model Content

[0004] The utility model provides a laser welding protective cover plate, which is used to solve the problem in the prior art that when welding an adapter, a dust removal process and a protective gas injection process affect each other, resulting in poor welding of the adapter.

[0005] In order to solve the above technical problems, the utility model provides a laser welding protective cover plate, which includes:

[0006] A first pressing plate, wherein a protective gas channel, a dust removal channel and a laser channel are provided in the first pressing plate, and the protective gas channel, the dust removal channel and the laser channel all pass through the first pressing plate, and the dust removal channel is inclined at a first angle to the horizontal direction;

[0007] The second pressing plate is connected to the first pressing plate, the laser channel passes through the second pressing plate, the dust removal channel and the protective gas channel both pass through the laser channel from the side of the second pressing plate close to the first pressing plate, and the protective gas channel is inclined at a second angle to the horizontal direction in the second pressing plate.

[0008] Optionally, the first inclination angle is 45 degrees.

[0009] Optionally, the second inclination angle is 45 degrees.

[0010] Optionally, an entrance aperture of the laser channel in the first pressing plate is larger than an entrance aperture of the laser channel in the second pressing plate.

[0011] Optionally, a cross-sectional area of ​​the laser channel gradually decreases in a direction from an entrance to an exit of the laser channel on the first pressure plate.

[0012] Optionally, the second pressing plate is in the shape of a quadrangular pyramid, a first bottom surface of the second pressing plate close to the first pressing plate and a second bottom surface of the second pressing plate away from the first pressing plate are respectively two bottom surfaces of the quadrangular pyramid, and an area of ​​the first bottom surface is greater than an area of ​​the second bottom surface.

[0013] Optionally, the slope of the side slope of the second pressing plate close to the protective gas channel is 150 degrees.

[0014] Optionally, when welding the welding workpiece, two surfaces of the welding workpiece in contact with the second pressing plate are perpendicular.

[0015] Optionally, a positioning boss is provided on a side of the second pressing plate away from the first pressing plate.

[0016] Optionally, the laser welding protection cover plate further includes a buffer spring, and the buffer spring is detachably connected between the first pressing plate and the second pressing plate.

[0017] Compared with the prior art, the laser welding protective cover provided by the utility model has the following beneficial effects:

[0018] The laser welding protection cover plate in the utility model separates the protection gas channel from the dust removal channel, and allows the protection gas channel and the dust removal channel to pass through the laser channel. Firstly, the laser and the protection gas can be merged in the laser channel, and then welding can be performed at the bottom of the second pressure plate, and since the dust removal channel also passes through the laser channel, the welding slag generated during welding can be sucked away through the dust removal channel; secondly, since the protection gas channel and the dust removal channel respectively pass through the laser channel at a certain inclination angle, the protection gas outlet of the protection gas channel in the laser channel and the dust removal outlet of the dust removal channel in the laser channel will not overlap, and then it can be understood that when the workpiece is welded, the dust removal process and the protection gas injection process will not interfere with each other, thereby solving the problem in the prior art that when the adapter is welded, the dust removal process and the protection gas injection process affect each other, resulting in poor welding of the adapter. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only part of the embodiments of the utility model, rather than all of the embodiments. For ordinary technicians in this field, without paying creative work, other drawings obtained based on these drawings all fall within the scope of protection of the utility model.

[0020] Figure 1 It is a three-dimensional diagram of a laser welding protective cover plate provided by an embodiment of the utility model in a certain direction;

[0021] Figure 2 It is a three-dimensional view of a laser welding protection cover plate provided by an embodiment of the utility model in another direction;

[0022] Figure 3 It is a cross-sectional view of a laser welding protective cover plate provided by an embodiment of the utility model in a certain direction;

[0023] Figure 4 It is a three-dimensional diagram of a laser welding protection cover plate provided by an embodiment of the utility model in another direction.

[0024] Description of the figure number:

[0025] 100 - first pressing plate, 110 - protective gas channel, 120 - dust removal channel, 130 - laser channel, 200 - second pressing plate, 210 - boss, 300 - buffer spring. DETAILED DESCRIPTION

[0026] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.

[0027] In order to make the description of the disclosed content more detailed and complete, the following is an illustrative description of the implementation methods and specific embodiments of the utility model. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0028] It should be noted that the terms "first", "second", etc. in the specification and claims of the present utility model and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the utility model described herein can be implemented in an order other than those illustrated or described herein.

[0029] In the description of the embodiments of the present invention, unless otherwise specified, “ / ” means or, for example, A / B can mean A or B; “and / or” in the text is merely a description of the association relationship of associated objects, indicating that three relationships may exist, for example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. In addition, in the description of the embodiments of the present invention, “multiple” means two or more than two, and other quantifiers are similar. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention, and the embodiments of the present invention and the features in the embodiments may be combined with each other without conflict.

[0030] like Figure 1 and Figure 2 The figure shows a three-dimensional view of a laser welding protective cover plate provided by an embodiment of the utility model in two directions, and the laser welding protective cover plate includes:

[0031] A first pressing plate 100, wherein a protective gas channel 110, a dust removal channel 120 and a laser channel 130 are provided in the first pressing plate 100, and the protective gas channel 110, the dust removal channel 120 and the laser channel 130 all pass through the first pressing plate 100, and the dust removal channel 120 is inclined at a first angle to the horizontal direction;

[0032] The second pressing plate 200 is connected to the first pressing plate 100, the laser channel 130 passes through the second pressing plate 200, the dust removal channel 120 and the protective gas channel 110 both pass through the laser channel 130 from the side of the second pressing plate 200 close to the first pressing plate 100, and the protective gas channel 110 is in a second inclination angle with the horizontal direction in the second pressing plate 200.

[0033] It can be understood that the shielding gas channel 110 is a channel for transmitting shielding gas to the place where the welding reaction occurs during the welding process. The shielding gas here can be any shielding gas, for example, helium; the dust removal channel 120 is a channel for dust removal during the welding process, which is used to remove the welding slag generated during the welding process of the workpiece; and the laser channel 130 is a channel for emitting laser to the welding point for welding.

[0034] It should be noted that the second pressing plate 200 and the first pressing plate 100 may be connected in any manner. For example, the second pressing plate 200 and the first pressing plate 100 may be connected in a detachable manner or a fixed manner.

[0035] It should be noted that the specific values ​​of the first inclination angle and the second inclination angle can be set according to specific needs of the application and are not limited in detail here.

[0036] It can be understood that the protective gas channel 110, the dust removal channel 120 and the laser channel 130 are independent channels; on this basis, it can be understood that since the laser channel 130 passes through the second pressure plate 200, the dust removal channel 120 and the protective gas channel 110 both pass through from the side of the second pressure plate 200 close to the first pressure plate 100 to the laser channel 130, so the positions of the outlets of the protective gas channel 110 and the dust removal channel 120 in the laser channel 130 are different, thereby avoiding the mutual interference between the protective gas injection process and the dust removal process.

[0037] It should be noted that the protective gas channel 110 is a continuous channel in the first pressing plate 100 and the second pressing plate 200, so that the protective gas ejected from the protective gas channel 110 in the first pressing plate 100 can be ejected to the entrance of the protective gas channel 110 in the second pressing plate 200. Similarly, the dust removal channel 120 is a continuous channel in the first pressing plate 100 and the second pressing plate 200.

[0038] It can be understood that by isolating the shielding gas channel 110 from the dust removal channel 120 and allowing the shielding gas channel 110 and the dust removal channel 120 to pass through the laser channel 130, firstly, the laser and the shielding gas can be merged in the laser channel 130, and then welding can be performed at the bottom of the second pressure plate 200, and since the dust removal channel 120 also passes through the laser channel 130, the welding slag generated during welding can be sucked away through the dust removal channel 120; secondly, since the shielding gas channel 110 and the dust removal channel 120 respectively pass through the laser channel 130 at a certain inclination angle, the shielding gas outlet of the shielding gas channel 110 in the laser channel 130 and the dust removal outlet of the dust removal channel 120 in the laser channel 130 will not overlap, and then it can be understood that when welding the workpiece, the dust removal process and the shielding gas injection process will not interfere with each other, thereby solving the problem in the prior art that when welding the adapter, the dust removal process and the shielding gas injection process affect each other, resulting in poor welding of the adapter.

[0039] Optionally, the entrances of the protective gas channel 110 and the dust removal channel 120 of the first pressure plate 100 can be respectively arranged on opposite sides of the laser channel 130, so that the outlets of the protective gas channel 110 and the dust removal channel 120 at the laser channel 130 can be farther away, thereby minimizing the interference between the two channels.

[0040] Optionally, the laser channel 130 may penetrate the first pressing plate 100 and the second pressing plate 200 in a direction perpendicular to the plate surfaces of the first pressing plate 100 and the second pressing plate 200 respectively, so that the laser in the laser channel 130 can reach the welding point more quickly.

[0041] In an optional implementation, Figure 3 The figure shows a cross-sectional view of a laser welding protection cover plate provided by an embodiment of the present utility model when viewed in the direction from the first pressing plate 100 to the second pressing plate 200, and the first inclination angle is 45 degrees.

[0042] It can be understood that when the angle between the dust removal channel 120 and the horizontal direction is too large, the component force of the welding slag in the dust removal channel 120 in the vertical direction will increase, thereby increasing the difficulty of sucking the welding slag out of the dust removal channel 120; and when the angle between the dust removal channel 120 and the horizontal direction is too small, when the dust removal channel 120 penetrates into the laser channel 130, the outlet of the dust removal channel 120 in the laser channel 130 will be too high from the bottom of the laser channel 130, and the welding point of the welding workpiece is located at the bottom of the laser channel 130, so the height of the dust removal channel 120 from the bottom of the laser channel 130 is too high, which will make it difficult to suck the welding slag into the dust removal channel 120. Therefore, in this implementation, it is chosen to set the first inclination angle to 45 degrees.

[0043] In an optional implementation, Figure 3 As shown, the second inclination angle is 45 degrees.

[0044] It can be understood that, when the angle between the shielding gas channel 110 and the horizontal direction is too small, when the shielding gas channel 110 penetrates into the laser channel 130, the outlet of the shielding gas channel 110 in the laser channel 130 will be too high from the bottom of the laser channel 130, and the welding point of the welding workpiece is located at the bottom of the laser channel 130, so the height of the shielding gas channel 110 from the bottom of the laser channel 130 is too high, which will cause the shielding gas sprayed in the shielding gas channel 110 to be difficult to reach the welding point. When the angle between the shielding gas channel 110 and the horizontal direction is too large, when the shielding gas channel 110 penetrates into the laser channel 130, the outlet of the shielding gas channel 110 in the laser channel 130 may penetrate to the bottom of the second pressure plate 200, resulting in the outlet of the shielding gas channel 110 not being in the laser channel 130, and unable to provide shielding gas for the welding process. Therefore, in this implementation, the second inclination angle is set to 45 degrees.

[0045] In an optional implementation, Figure 3 As shown, the entrance diameter of the laser channel 130 in the first pressing plate 100 is larger than the entrance diameter of the laser channel 130 in the second pressing plate 200 .

[0046] It should be noted that the specific values ​​of the entrance diameter of the laser channel 130 at the first pressing plate 100 and the entrance diameter of the second pressing plate 200 can be set according to the specific needs of the application.

[0047] It can be understood that the laser in the laser channel 130 is transmitted from the first pressure plate 100 to the second pressure plate 200, so the entrance of the laser channel 130 in the first pressure plate 100 is the initial entrance of the laser. Setting the initial entrance of the laser to have a larger aperture can prevent the laser from splashing onto the surface of the first pressure plate 100 and allow more laser to enter.

[0048] In an optional implementation, Figure 3 As shown, the cross-sectional area of ​​the laser channel 130 gradually decreases from the entrance to the exit of the laser channel 130 on the first pressing plate 100 .

[0049] It can be understood that the cross-sectional area of ​​the laser channel 130 gradually decreases from the entrance to the exit of the first pressure plate 100, so that when the laser is injected into the laser channel 130, as much laser as possible can enter the laser channel 130, thereby avoiding laser splashing and waste.

[0050] In an optional implementation, Figure 4 FIG. 1 is a three-dimensional view of a laser welding protective cover provided by an embodiment of the utility model in another direction, as shown in FIG. Figure 3 and Figure 4 As shown, the second pressing plate 200 is in the shape of a quadrangular pyramid, and the first bottom surface of the second pressing plate 200 close to the first pressing plate 100 and the second bottom surface of the second pressing plate 200 away from the first pressing plate 100 are respectively the two bottom surfaces of the quadrangular pyramid, and the area of ​​the first bottom surface is greater than the area of ​​the second bottom surface.

[0051] It should be noted that the areas of the first bottom surface and the second bottom surface can be set according to specific needs during application and are not limited in detail here.

[0052] It can be understood that since the second pressure plate 200 is in the shape of a quadrangular pyramid and the area of ​​the first bottom surface is larger than the area of ​​the second bottom surface, the second pressure plate 200 has a certain slope along the direction from the first bottom surface to the second bottom surface. On this basis, the second pressure plate 200 can have a certain load-bearing capacity for the first pressure plate 100, and since the laser enters the second pressure plate 200 from the first pressure plate 100, the shielding gas also enters the second pressure plate 200 from the first pressure plate 100, and then the welding process occurs at the bottom of the second pressure plate 200 through the laser and the shielding gas, so the second pressure plate 200 needs strong firmness and stability, and the design of the second pressure plate 200 in this implementation method can make the second pressure plate 200 have strong firmness and stability.

[0053] In an optional implementation, Figure 3 and Figure 4As shown, the slope of the side slope of the second pressing plate 200 close to the protective gas channel 110 is 150 degrees.

[0054] It can be understood that when the slope of the side slope of the second pressure plate 200 close to the shielding gas channel 110 is less than 90 degrees, the area of ​​the first bottom surface of the second pressure plate 200 close to the first pressure plate 100 will be smaller than the area of ​​the second bottom surface of the second pressure plate 200 away from the first pressure plate 100. It can be understood that the load-bearing capacity of this structure is poor; when the slope of the side slope of the second pressure plate 200 close to the shielding gas channel 110 is a smaller obtuse angle, the load-bearing capacity cannot reach the optimal level; and when the slope of the side slope of the second pressure plate 200 close to the shielding gas channel 110 is a larger obtuse angle, the height of the laser channel 130 will be lower, which may cause the welding slag generated by welding to fly out directly from the laser channel 130. Therefore, in this implementation, the slope of the side slope of the second pressure plate 200 close to the shielding gas channel 110 is 150 degrees to achieve better results.

[0055] In an optional implementation, Figure 3 and Figure 4 As shown, when welding the welding workpiece, the two surfaces of the welding workpiece in contact with the second pressing plate 200 are perpendicular.

[0056] It can be understood that the two surfaces of the welding workpiece in contact with the second pressing plate 200 during welding are perpendicular, so that the welding slag generated during welding of the welding workpiece is not easy to fall off.

[0057] In an optional implementation, Figure 3 and Figure 4 As shown, a positioning boss 210 is provided on a side of the second pressing plate 200 away from the first pressing plate 100 .

[0058] Specifically, the volume and position of the positioning boss 210 can be set according to the specific needs of the application. For example, in order to prevent the positioning boss 210 from interfering with the welding of the workpiece, the positioning boss 210 can be set at the edge of the bottom surface of the second pressure plate 200. In order to make the volume of the second pressure plate 200 smaller, the volume of the positioning boss 210 can be made smaller than a preset threshold.

[0059] It can be understood that, by designing the positioning boss 210 on the second pressing plate 200, the entire laser welding protective cover plate can be positioned to prevent the protective cover plate from deviating when welding the workpiece.

[0060] In an optional implementation, Figure 1 and Figure 4As shown, the laser welding protection cover plate further includes a buffer spring 300 , and the buffer spring 300 is detachably connected between the first pressing plate 100 and the second pressing plate 200 .

[0061] It should be noted that the installation direction of the buffer spring 300 may be the direction of laser jetting, so that the pressure generated by the laser jetting may be buffered by the buffer spring 300 .

[0062] It should be noted that the number of buffer springs 300 can be set according to the specific needs of the application. For example, in order to minimize the number of buffer springs 300 so that the support of the buffer springs 300 to the first pressure plate 100 is sufficiently stable, when the first pressure plate 100 is square, four buffer springs 300 can be arranged under the first pressure plate 100 at the four corners of the first pressure plate 100.

[0063] It is also understandable that the buffer spring 300 is detachable to facilitate replacement and maintenance of the buffer spring 300 , the first pressing plate 100 , and the second pressing plate 200 .

[0064] The technical solution provided by the present invention is introduced in detail above. The present invention uses specific examples to illustrate the principle and implementation mode of the present invention. The description of the above embodiments is only used to help understand the method and core idea of ​​the present invention. At the same time, for those skilled in the art, according to the idea of ​​the present invention, there will be changes in the specific implementation mode and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.

[0065] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A laser welding protective cover plate, characterized in that: include: A first pressing plate, wherein a protective gas channel, a dust removal channel and a laser channel are provided in the first pressing plate, and the protective gas channel, the dust removal channel and the laser channel all pass through the first pressing plate, and the dust removal channel is inclined at a first angle to the horizontal direction; The second pressing plate is connected to the first pressing plate, the laser channel passes through the second pressing plate, the dust removal channel and the protective gas channel both pass through the laser channel from the side of the second pressing plate close to the first pressing plate, and the protective gas channel is inclined at a second angle to the horizontal direction in the second pressing plate.

2. The laser welding protective cover plate according to claim 1, characterized in that: The first inclination angle is 45 degrees.

3. The laser welding protective cover plate according to claim 1, characterized in that: The second inclination angle is 45 degrees.

4. The laser welding protective cover plate according to claim 1, characterized in that: The entrance aperture of the laser channel in the first pressing plate is larger than the entrance aperture of the laser channel in the second pressing plate.

5. The laser welding protective cover plate according to claim 1, characterized in that: The cross-sectional area of ​​the laser channel gradually decreases in a direction from the entrance to the exit of the laser channel on the first pressure plate.

6. The laser welding protective cover plate according to claim 1, characterized in that: The second pressing plate is in the shape of a quadrangular pyramid, a first bottom surface of the second pressing plate close to the first pressing plate and a second bottom surface of the second pressing plate away from the first pressing plate are two bottom surfaces of the quadrangular pyramid respectively, and an area of ​​the first bottom surface is larger than an area of ​​the second bottom surface.

7. The laser welding protective cover plate according to claim 6, characterized in that: The slope of the side slope of the second pressing plate close to the protective gas channel is 150 degrees.

8. The laser welding protective cover plate according to claim 1, characterized in that: When welding the welding workpiece, the two surfaces of the welding workpiece in contact with the second pressing plate are perpendicular.

9. The laser welding protective cover plate according to claim 1, characterized in that: A positioning boss is arranged on a side of the second pressing plate away from the first pressing plate.

10. The laser welding protective cover plate according to claim 1, characterized in that: Also includes: A buffer spring is detachably connected between the first pressing plate and the second pressing plate.

Citation Information

Cited By

  • Iron frame assembly welding equipment

    CN119159237A