Strengthening structure of AMOLED screen

By using steel plates to strengthen the components on the glass plate of the AMOLED screen, the problem of easy breakage at the steps of the glass plate is solved, which significantly improves the ability to resist falling and ensures the normal display of the screen.

CN222826047UActive Publication Date: 2025-05-02TRULY SEMICON
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421605600.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2025-05-02
Estimated Expiration
2034-07-08

AI Technical Summary

Technical Problem

The glass plate steps of existing AMOLED screens are prone to break due to falling, which affects the display effect.

Method used

Instead of traditional foam, the steel plate is used to replace the steel plate, which is arranged on the colloid and bonded to the second glass plate to form a reinforcement component to enhance the anti-falling ability of the glass plate.

Benefits of technology

It significantly improves the protection ability of the glass plate, reduces the risk of rupture at the steps of the glass plate when falling, thereby ensuring the normal display of the screen.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222826047U_ABST
    Figure CN222826047U_ABST
Patent Text Reader

Abstract

The utility model relates to a strengthening structure of an AMOLED screen. The strengthening structure of the AMOLED screen comprises a first glass plate, a second glass plate and a strengthening assembly, wherein the second glass plate is arranged on the first glass plate; the reinforcing assembly comprises a steel plate and colloid, the steel plate is arranged on the colloid, and the colloid is arranged on the second glass plate. According to the scheme, the protection strength of the glass plate can be improved, and normal display of the screen is guaranteed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of display screens, in particular to a reinforcement structure of an AMOLED screen. Background Art

[0002] At present, AMOLED screens have a wide range of applications, such as smart watches, smart fixtures, e-cigarette products, etc.

[0003] In the related technology, the AMOLED screen is composed of two glass plates of different lengths. After assembly, a step is formed between the two glass plates, and finally foam is added to the back of one of the glass plates to cushion and protect the glass plate. However, the texture of the foam is relatively soft, and when the screen falls, the support strength of the foam is limited, which can still easily cause the glass plate to break at the step, thereby affecting the display. Utility Model Content

[0004] The purpose of the utility model is to overcome the deficiencies in the prior art and provide a strengthening structure of an AMOLED screen, which can enhance the protection strength of the glass plate and ensure the normal display of the screen.

[0005] The purpose of this utility model is achieved through the following technical solutions:

[0006] In a first aspect, the present application provides a reinforcement structure for an AMOLED screen, comprising: a first glass plate; a second glass plate, wherein the second glass plate is arranged on the first glass plate; a reinforcement component, wherein the reinforcement component comprises a steel plate and a colloid, wherein the steel plate is arranged on the colloid, and the colloid is arranged on the second glass plate.

[0007] The length of the steel plate is the same as that of the second glass plate.

[0008] The second glass sheet has a length greater than that of the first glass sheet.

[0009] It also includes a chip, which is arranged on the second glass plate.

[0010] It also includes an FPC board, which is arranged on the second glass plate.

[0011] It also includes optical glue, which is arranged on the first glass plate.

[0012] It also includes a cover plate, which is arranged on the optical adhesive.

[0013] The cover plate has a rectangular cross-sectional structure.

[0014] The first glass plate has a rectangular cross-sectional structure.

[0015] The steel plate has a rectangular cross-sectional structure.

[0016] Compared with the prior art, the utility model has at least the following advantages:

[0017] By using a steel plate instead of the original foam, the mechanical strength of the entire module is improved, and the drop resistance of the back of the second glass plate is also greatly improved, making it less likely for the step between the second glass plate and the first glass plate to break. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions of the embodiments of the present utility model, the drawings required for use in the embodiments are briefly introduced below.

[0019] Figure 1 It is a schematic structural diagram of the strengthening structure of the AMOLED screen in one embodiment of the utility model. DETAILED DESCRIPTION

[0020] The embodiments of the present application will be described in more detail below with reference to the accompanying drawings. Although the embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided to make the present application more thorough and complete, and to fully convey the scope of the present application to those skilled in the art.

[0021] It should be understood that although the terms "first", "second", "third", etc. may be used in this application to describe various information, this information should not be limited to these terms. These terms are only used to distinguish the same type of information from each other. For example, without departing from the scope of this application, the first information may also be referred to as the second information, and similarly, the second information may also be referred to as the first information. Thus, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.

[0022] Unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, or a detachable connection or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0023] The AMOLED screen is composed of two glass plates of different lengths. After assembly, a step is formed between the two glass plates. Finally, foam is added to the back of one of the glass plates to cushion and protect the glass plate. However, the texture of the foam is relatively soft. When the screen falls, the support strength of the foam is limited, and it is still easy to cause the glass plate to break at the step, thereby affecting the display.

[0024] In view of the above problems, the embodiments of the present application provide a reinforcement structure of an AMOLED screen, which can enhance the protection strength of the glass plate and ensure the normal display of the screen.

[0025] The technical solution of the embodiments of the present application is described in detail below with reference to the accompanying drawings.

[0026] See also Figure 1 A strengthening structure of an AMOLED screen includes: a first glass plate 100, a second glass plate 200 and a strengthening component 300, wherein the second glass plate 200 is arranged on the first glass plate 100; the strengthening component 300 includes a steel plate 310 and a colloid 320, wherein the steel plate 310 is arranged on the colloid 320, and the colloid 320 is arranged on the second glass plate 200.

[0027] It should be noted that the first glass plate 100 has a rectangular cross-sectional structure; the steel plate 310 has a rectangular cross-sectional structure. The steel plate 310 is harder than the traditional foam. Therefore, by providing the steel plate 310, the protective capability of the glass plate can be improved, making it more resistant to falling and not easy to break. Furthermore, the colloid 320 is double-sided adhesive, which can bond the steel plate 310.

[0028] See also Figure 1 In one embodiment, the length of the steel plate 310 is the same as the length of the second glass plate 200 .

[0029] It should be noted that the length of the second glass plate 200 is greater than that of the first glass plate 100 . To ensure comprehensive protection, the length of the steel plate 310 is the same as that of the second glass plate 200 .

[0030] See also Figure 1 In one embodiment, a strengthening structure of an AMOLED screen further includes a chip 400 , and the chip 400 is disposed on the second glass plate 200 .

[0031] It should be noted that the chip 400 is used to control the screen to display images.

[0032] See also Figure 1 In one embodiment, a reinforcement structure of an AMOLED screen further includes an FPC board 500 , and the FPC board 500 is disposed on the second glass plate 200 .

[0033] It should be noted that the FPC board 500 is used to be plugged into the host end.

[0034] See also Figure 1 In one embodiment, a strengthening structure of an AMOLED screen further includes an optical adhesive 600, and the optical adhesive 600 is disposed on the first glass plate 100. Specifically, a strengthening structure of an AMOLED screen further includes a cover plate 700, and the cover plate 700 is disposed on the optical adhesive 600. Specifically, the cover plate 700 has a rectangular cross-sectional structure.

[0035] It should be noted that the cover plate 700 is adhered to the first glass plate by means of an optical adhesive 600. The optical adhesive 600 is an OCA optical adhesive.

[0036] The scheme of the present application has been described in detail above with reference to the accompanying drawings. In the above embodiments, the descriptions of the various embodiments have their own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments. Those skilled in the art should also be aware that the actions and modules involved in the specification are not necessarily required for the present application. In addition, it can be understood that the steps in the method of the embodiment of the present application can be adjusted in order, merged and deleted according to actual needs, and the modules in the device of the embodiment of the present application can be merged, divided and deleted according to actual needs.

[0037] The embodiments of the present application have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The selection of terms used herein is intended to best explain the principles of the embodiments, practical applications, or improvements to the technology in the market, or to enable other persons of ordinary skill in the art to understand the embodiments disclosed herein.

Claims

1. A strengthening structure of an AMOLED screen, characterized in that: include: First glass plate; a second glass plate, the second glass plate being disposed on the first glass plate; The reinforcing component includes a steel plate and a colloid, wherein the steel plate is arranged on the colloid, and the colloid is arranged on the second glass plate.

2. The AMOLED screen reinforcement structure according to claim 1, characterized in that: The length of the steel plate is the same as that of the second glass plate.

3. The AMOLED screen reinforcement structure according to claim 1, characterized in that: The second glass sheet has a length greater than that of the first glass sheet.

4. The AMOLED screen reinforcement structure according to claim 1, characterized in that: It also includes a chip, which is arranged on the second glass plate.

5. The AMOLED screen reinforcement structure according to claim 1, characterized in that: It also includes an FPC board, which is arranged on the second glass plate.

6. The AMOLED screen reinforcement structure according to claim 1, characterized in that: It also includes optical glue, which is arranged on the first glass plate.

7. The AMOLED screen reinforcement structure according to claim 6, characterized in that: It also includes a cover plate, which is arranged on the optical adhesive.

8. The AMOLED screen reinforcement structure according to claim 7, characterized in that: The cover plate has a rectangular cross-sectional structure.

9. The AMOLED screen reinforcement structure according to claim 1, characterized in that: The first glass plate has a rectangular cross-sectional structure.

10. The AMOLED screen reinforcement structure according to claim 1, characterized in that: The steel plate has a rectangular cross-sectional structure.