Coated tempered glass

By setting grooves and convex strips on both sides of the coated tempered glass and setting bumps in the grooves, the lifting and stacking sliding problems caused by flat surface of the glass are solved, and the stable stacking and firm glueing of the glass is achieved.

CN222975084UActive Publication Date: 2025-06-13ZHEJIANG LANXIN GLASS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421625321.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2025-06-13
Estimated Expiration
2034-07-10

AI Technical Summary

Technical Problem

The surface of the coated tempered glass is flat, easy to slide when carrying and stacking, and easy to slip during transportation, which is dangerous.

Method used

A first groove and a second groove are provided on both sides of the glass, and a semicircular convex strip is provided in the position therebetween. The glass is located at both ends of the convex strip, and a convex point is provided in the groove to increase the glued contact surface and fixing effect.

Benefits of technology

Through structural improvement, the glass does not slip and fall when stacked up and down, and has good placement stability. The side staggered is easy to hold and place, which increases the glued adhesion and fixation effect and reduces the risk of handling and installation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222975084U_ABST
    Figure CN222975084U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of glass, in particular to coated toughened glass, which comprises a first groove and a second groove which are arranged on two sides of coated glass after the coated glass is basically toughened, a raised line is arranged between the first groove and the second groove, and planes are reserved on the glass at two ends of the raised line. The structure of the glass is improved, the first grooves, the second grooves and the raised lines are arranged at the gluing positions of the side edges, the glass can be stacked up and down without slipping and falling off by utilizing the first grooves, the second grooves and the raised lines, the placing stability is good, the side edges of the glass are staggered, the glass is convenient to take and place, and the service life of the glass is prolonged. And through the design of the first groove, the second groove, the convex strip and the convex point, the gluing attachment fixing effect is improved by increasing the gluing contact surface, gluing is firmer, and the using effect is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of glass, in particular to a coated tempered glass. Background Technique

[0002] The surface of the coated tempered glass is flat, making it easy to slip when lifting, and because the surface is flat, it is prone to displacement and slipping during stacking and transportation, posing a danger. Content of the Utility Model

[0003] The purpose of the utility model is to provide a coated tempered glass to solve the problems of easy slipping when lifting due to the flat surface, easy displacement and slipping during stacking and transportation, and the existing danger as mentioned in the above background technique.

[0004] To achieve the above purpose, the utility model provides the following technical solutions:

[0005] A coated tempered glass, including glass, with a first groove and a second groove provided on both sides of the glass, a convex strip provided at the position between the first groove and the second groove, and planes left at both ends of the convex strip on the glass.

[0006] As a further description of the above technical solution:

[0007] The first groove and the second groove are semi-circular arcs.

[0008] As a further description of the above technical solution:

[0009] The distance from the first groove to the side of the glass is the same as the length of the plane.

[0010] As a further description of the above technical solution:

[0011] The convex strip is semi-circular.

[0012] As a further description of the above technical solution:

[0013] The first groove and the second groove are fitted with the convex strip.

[0014] As a further description of the above technical solution:

[0015] Convex points are provided in the first groove and the second groove.

[0016] Compared with the prior art, the utility model provides a coated tempered glass, which has the following beneficial effects:

[0017] 1. In the present utility model, through structural improvement of the glass, a first groove, a second groove and a rib are provided at the position where sealant is applied on the side. By means of the first groove, the second groove and the rib, the stacked glass will not slip and fall, and the placement stability is good. Moreover, the sides of the glass are staggered, which is convenient for taking and placing.

[0018] 2. In the present utility model, the design of the first groove, the second groove, the rib and the bump increases the bonding contact surface and the bonding and fixing effect, making the sealant more firm. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 is a schematic diagram of the overall structure of the present utility model;

[0020] Figure 2 for the present utility model Figure 1 is an enlarged schematic diagram of the structure of A in the present utility model.

[0021] Legend:

[0022] 1. Glass; 2. First groove; 3. Second groove; 4. Rib; 5. Plane; 6. Bump. DETAILED DESCRIPTION OF THE EMBODIMENTS

[0023] The technical solutions in the embodiments of the present utility model will be clearly and completely described below with reference to the accompanying drawings in the embodiments of the present utility model. Obviously, the described embodiments are only a part of the embodiments of the present utility model, rather than all the embodiments. All other embodiments obtained by those of ordinary skill in the art based on the embodiments of the present utility model without creative efforts shall fall within the protection scope of the present utility model.

[0024] Embodiment:

[0025] Please refer to Figure 1 - Figure 2 , the present utility model provides a coated tempered glass, including glass 1. First grooves 2 and second grooves 3 are provided on both sides of the glass 1, a rib 4 is provided at the position between the first groove 2 and the second groove 3, and planes 5 are left at both ends of the rib 4 on the glass 1.

[0026] Specifically, as Figure 2 shown, the first groove 2 and the second groove 3 are semi-circular arcs, the distance from the first groove 2 to the side of the glass 1 is the same as the length of the plane 5, the rib 4 is semi-circular, the first groove 2 and the second groove 3 are fitted with the rib 4, and the stacked glass 1 does not slip, and the reserved plane 5 does not affect the installation of the glass 1 in the frame, which is convenient for applying sealant.

[0027] Specifically, as Figure 2 shown, bumps 6 are provided in the first groove 2 and the second groove 3 to increase the firmness of the glue fixation.

[0028] Working principle:

[0029] When stacking, the convex strip 4 of the upper glass 1 can be placed aligned with the first groove 2 or the second groove 3 of the lower glass 1. In this way, the upper and lower glasses 1 are placed stably, and the sides are staggered from each other, which is convenient for handling. When lifting by hand, the first groove 2, the second groove 3 and the convex strip 4 have an anti-slip effect of increasing friction. When installing and caulking, the first groove 2, the second groove 3 and the convex strip 4 are the positions for caulking, with a large caulking contact surface. Coupled with the convex points 6, the firmness of the glue fixation is increased.

[0030] Although the embodiments of the present invention have been shown and described, it will be understood by those of ordinary skill in the art that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principle and spirit of the present invention. The scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A coated tempered glass, comprising glass (1), characterized in that: The glass (1) is provided with a first groove (2) and a second groove (3) on both sides, a convex strip (4) is provided between the first groove (2) and the second groove (3), and the glass (1) has flat surfaces (5) at both ends of the convex strip (4).

2. The coated tempered glass according to claim 1, characterized in that: The first groove (2) and the second groove (3) are semicircular arc-shaped.

3. The coated tempered glass according to claim 1, characterized in that: The distance between the first groove (2) and the side of the glass (1) is the same as the length of the plane (5).

4. The coated tempered glass according to claim 2, characterized in that: The convex strip (4) is semicircular.

5. The coated tempered glass according to claim 1, characterized in that: The first groove (2) and the second groove (3) are arranged in a matching manner with the convex strip (4).

6. The coated tempered glass according to claim 1, characterized in that: The first groove (2) and the second groove (3) are provided with convex points (6).