Anti-aging color master batch
Patent Information
- Application Number
- CN202422845695.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-21
- Publication Date
- 2026-01-27
- Estimated Expiration
- 2034-11-21
Smart Images

Figure CN223834847U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of color masterbatch technology, specifically relating to an anti-aging color masterbatch. Background Technology
[0002] Color masterbatch is a plastic colorant made by dispersing a high proportion of pigments or additives with thermoplastic resin. The resin used has good wetting and dispersing properties for the colorant and good compatibility with the material being colored. However, during storage, color masterbatch may become damp or abraded, which can easily lead to pigment damage and aging, thus affecting the performance of the color masterbatch. Summary of the Invention
[0003] To address the shortcomings of existing technologies, this utility model provides an anti-aging masterbatch.
[0004] To achieve the above objectives, the present invention provides the following technical solution:
[0005] An anti-aging masterbatch, comprising:
[0006] First carrier;
[0007] A first main body is disposed at the upper end of the first carrier. The first main body includes a first outer layer and a first pigment layer. The first outer layer is disposed around the upper end of the first carrier, and the first pigment layer is disposed between the first outer layer and the first carrier.
[0008] The second body is disposed at the lower end of the first carrier. The second body includes a second outer layer and a second pigment layer. The second outer layer is disposed around the lower end of the first carrier, and the second pigment layer is disposed between the second outer layer and the first carrier.
[0009] The outer surfaces of the first carrier, the first main body, and the second main body are provided with protective layers.
[0010] Furthermore, the upper end of the first carrier is provided with a plurality of first support strips, the inner side of the first outer layer is provided with a plurality of first reinforcing grooves, and the end of the first support strip away from the first carrier is provided with a first reinforcing block, the first reinforcing block matching the first reinforcing groove, and the first reinforcing block being in the shape of an inverted triangle.
[0011] Furthermore, the lower end of the first carrier is provided with a plurality of second support strips, the inner side of the second outer layer is provided with a plurality of second reinforcing grooves, and the end of the second support strip away from the first carrier is provided with a second reinforcing block, the second reinforcing block is matched with the second reinforcing groove, and the second reinforcing block is in the shape of an inverted triangle.
[0012] Furthermore, the protective layer includes a waterproof layer, a flame-retardant layer, and a wear-resistant layer. The flame-retardant layer is disposed on the outer surface of the first carrier, the first main body, and the second main body. The waterproof layer is disposed on the outer surface of the flame-retardant layer, and the wear-resistant layer is disposed on the outer surface of the waterproof layer.
[0013] Furthermore, a first dispersion layer is provided between the first outer coating layer and the first pigment layer, and a second dispersion layer is provided between the second outer coating layer and the second pigment layer.
[0014] The anti-aging masterbatch disclosed in this utility model has the following advantages compared with the prior art: its structure is stable and reliable, which can ensure the stability of the first pigment layer and the second pigment layer in the first body and the second body. Furthermore, the protective layer can effectively reduce the risk of the first pigment layer and the second pigment layer being affected by moisture or wear, reduce the risk of aging, and make it more reliable. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the structure from one perspective of a preferred embodiment of the present invention.
[0016] Figure 2 This is a structural schematic diagram from another perspective of a preferred embodiment provided by this utility model.
[0017] Figure 3 This is a schematic diagram of the protective layer structure of a preferred embodiment of the present invention.
[0018] The reference numerals in the accompanying drawings include: 100, first main body; 110, first reinforcing groove; 120, first pigment layer; 130, first dispersion layer; 200, second main body; 210, second reinforcing groove; 220, second pigment layer; 230, second dispersion layer; 300, first carrier; 310, first support strip; 311, first reinforcing block; 320, second support strip; 321, second reinforcing block; 400, protective layer; 410, flame-retardant layer; 420, waterproof layer; 430, wear-resistant layer. Detailed Implementation
[0019] This utility model discloses an anti-aging masterbatch. The specific implementation of this utility model will be further described below with reference to preferred embodiments.
[0020] See attached diagram. Figure 1-3 , Figure 1 This is a schematic diagram of the structure from one perspective of a preferred embodiment provided by this utility model. Figure 2 This is a structural schematic diagram from another perspective of a preferred embodiment provided by this utility model. Figure 3 This is a schematic diagram of the structure of the protective layer 400 in a preferred embodiment of the present invention.
[0021] Preferred embodiment.
[0022] This embodiment provides an anti-aging masterbatch, comprising:
[0023] First carrier 300;
[0024] A first main body 100 is disposed on the upper end of the first carrier 300. The first main body 100 includes a first outer layer and a first pigment layer 120. The first outer layer is disposed on the upper end of the first carrier 300, and the first pigment layer 120 is disposed between the first outer layer and the first carrier 300.
[0025] The second body 200 is disposed at the lower end of the first carrier 300. The second body 200 includes a second outer layer and a second pigment layer 220. The second outer layer is disposed around the lower end of the first carrier 300, and the second pigment layer 220 is disposed between the second outer layer and the first carrier 300.
[0026] The outer surfaces of the first carrier 300, the first main body 100 and the second main body 200 are provided with a protective layer 400.
[0027] Furthermore, the upper end of the first carrier 300 is provided with a plurality of first support bars 310, the inner side of the first outer layer is provided with a plurality of first reinforcing grooves 110, and the end of the first support bar 310 away from the first carrier 300 is provided with a first reinforcing block 311, the first reinforcing block 311 matches the first reinforcing groove 110, and the first reinforcing block 311 is in the shape of an inverted triangle.
[0028] Furthermore, the lower end of the first carrier 300 is provided with a plurality of second support bars 320, the inner side of the second outer layer is provided with a plurality of second reinforcing grooves 210, and the end of the second support bar 320 away from the first carrier 300 is provided with a second reinforcing block 321, the second reinforcing block 321 matches the second reinforcing groove 210, and the second reinforcing block 321 is in the shape of an inverted triangle.
[0029] Furthermore, the protective layer 400 includes a waterproof layer 420, a flame-retardant layer 410, and a wear-resistant layer 430. The flame-retardant layer 410 is disposed on the outer surface of the first carrier 300, the first main body 100, and the second main body 200. The waterproof layer 420 is disposed on the outer surface of the flame-retardant layer 410, and the wear-resistant layer 430 is disposed on the outer surface of the waterproof layer 420.
[0030] Furthermore, a first dispersion layer 130 is provided between the first outer coating layer and the first pigment layer 120, and a second dispersion layer 230 is provided between the second outer coating layer and the second pigment layer 220.
[0031] Working principle: The first carrier 300 is supported and disposed between the first main body 100 and the second main body 200. The upper end of the first carrier 300 is connected and reinforced to the first outer coating layer through the first support strip 310, and the lower end of the first carrier 300 is connected and reinforced to the second outer coating layer through the second support strip 320, ensuring the structural stability of the masterbatch. The cooperation between the first reinforcing block 311 and the first reinforcing groove 110, and the cooperation between the second reinforcing block 321 and the second reinforcing groove 210, further ensure the structural stability of the masterbatch, and can well support the first pigment layer 120 and the second pigment layer 220. The first dispersion layer 130 can support the first pigment layer 120 well and can improve the pigment dispersion between adjacent first carriers 300.
[0032] The protective layer 400 ensures the wear resistance of the masterbatch through the wear-resistant layer 430, and ensures the stability of the flame-retardant layer 410 and the waterproof layer 420. The waterproof layer 420 can effectively reduce the risk of damage to the masterbatch due to moisture, and the flame-retardant layer 410 can prevent the masterbatch from being easily damaged by temperature, thereby reducing the risk of damage to the masterbatch, i.e., aging.
[0033] It is worth mentioning that the technical features such as the dispersion layer involved in this utility model patent application should be regarded as prior art. The specific structure, working principle and possible control methods and spatial arrangement methods of these technical features can be adopted by conventional choices in the field, and should not be regarded as the utility model point of this utility model patent. This utility model patent will not be further elaborated in detail.
[0034] For those skilled in the art, modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.
Claims
1. An anti-aging masterbatch, characterized in that, include: First carrier (300); A first body (100) is disposed on the upper end of the first carrier (300). The first body (100) includes a first outer layer and a first pigment layer (120). The first outer layer is disposed on the upper end of the first carrier (300), and the first pigment layer (120) is disposed between the first outer layer and the first carrier (300). The second body (200) is disposed at the lower end of the first carrier (300). The second body (200) includes a second outer layer and a second pigment layer (220). The second outer layer is disposed around the lower end of the first carrier (300), and the second pigment layer (220) is disposed between the second outer layer and the first carrier (300). The outer surfaces of the first carrier (300), the first main body (100) and the second main body (200) are provided with a protective layer (400).
2. The anti-aging masterbatch according to claim 1, characterized in that, The upper end of the first carrier (300) is provided with a plurality of first support strips (310), the inner side of the first outer layer is provided with a plurality of first reinforcing grooves (110), and the end of the first support strip (310) away from the first carrier (300) is provided with a first reinforcing block (311). The first reinforcing block (311) matches the first reinforcing groove (110), and the first reinforcing block (311) is in the shape of an inverted triangle.
3. The anti-aging masterbatch according to claim 2, characterized in that, The lower end of the first carrier (300) is provided with a plurality of second support strips (320), the inner side of the second outer layer is provided with a plurality of second reinforcing grooves (210), and the end of the second support strip (320) away from the first carrier (300) is provided with a second reinforcing block (321). The second reinforcing block (321) matches the second reinforcing groove (210), and the second reinforcing block (321) is in the shape of an inverted triangle.
4. The anti-aging masterbatch according to claim 3, characterized in that, The protective layer (400) includes a waterproof layer (420), a flame-retardant layer (410), and a wear-resistant layer (430). The flame-retardant layer (410) is disposed on the outer surface of the first carrier (300), the first body (100), and the second body (200). The waterproof layer (420) is disposed on the outer surface of the flame-retardant layer (410), and the wear-resistant layer (430) is disposed on the outer surface of the waterproof layer (420).
5. The anti-aging masterbatch according to claim 4, characterized in that, A first dispersion layer (130) is provided between the first outer coating layer and the first pigment layer (120), and a second dispersion layer (230) is provided between the second outer coating layer and the second pigment layer (220).