A wafer drying mechanism

By designing flow equalization plates and jet nozzles in the wafer drying mechanism, the problem of uneven airflow during wafer drying was solved, achieving uniform drying of the wafer surface and improving product yield.

CN224957063UActive Publication Date: 2026-11-10吉姆西半导体科技(无锡)股份有限公司
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522612264.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-09
Publication Date
2026-11-10
Estimated Expiration
2035-12-09

AI Technical Summary

Technical Problem

In existing technologies, uneven airflow of drying gas during wafer drying can lead to over-drying or under-drying of some wafers, affecting product yield.

Method used

A wafer drying mechanism is designed. By setting a flow equalization plate on the inner side wall of the drying chamber, the flow area of ​​the flow equalization hole increases with the distance from the air inlet. Combined with the design of the jet pipe, the airflow is ensured to be evenly distributed on the wafer surface.

Benefits of technology

This achieves uniform drying of the wafer surface, avoiding problems of over-drying or insufficient drying, and improving the yield of wafer products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224957063U_ABST
    Figure CN224957063U_ABST
Patent Text Reader

Abstract

This application relates to the field of semiconductor processing equipment technology, and more particularly to a wafer drying mechanism, comprising: a drying chamber with an inlet hole on its side wall for introducing drying gas; a flow equalization plate disposed on the inner side wall of the drying chamber, defining a flow channel for the drying gas to flow between the flow equalization plate and the side wall of the drying chamber; and a plurality of flow equalization holes on the flow equalization plate, the flow area of ​​which increases with the distance between the flow equalization hole and the inlet hole. In this design, a smaller flow area is provided in the high-pressure region near the inlet hole to increase the local flow resistance of the drying gas, thereby limiting excessive gas flow from this area. In the low-pressure region far from the inlet hole, a larger flow area is provided to reduce the local flow resistance of the drying gas, ensuring sufficient gas can flow out. This balances the original uneven gas flow caused by pressure difference, making the gas flow of the flow equalization holes at different positions on the entire flow equalization plate tend to be consistent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of semiconductor processing equipment technology, and in particular to a wafer drying mechanism. Background Technology

[0002] A wafer drying chamber is a device used to thoroughly remove moisture from the surface of a wafer after cleaning. Chinese invention patent CN115206846A discloses a semiconductor process equipment and its drying device. In the drying device, a support plate is used to support the wafer, and the support plate has a uniform flow hole structure for drying gas to pass through, so that the drying gas can flow evenly over the wafer to achieve the drying of the wafer.

[0003] Because the above-mentioned scheme places the flow equalization holes on the support plate, when a basket full of wafers is placed on the support plate, the bottom of the basket will block or completely cover the flow equalization holes, making it difficult for the drying gas to pass through, resulting in poor gas flow and affecting the drying effect of the wafers. To overcome the shortcomings of the bottom ventilation scheme, the existing technology has proposed an improved scheme of setting flow equalization plates on both sides of the drying chamber, so that the drying gas acts on the wafers from the side. However, this scheme introduces a new problem: since the diameter and spacing of the flow equalization holes in the flow equalization plates are the same, and the pressure of the drying gas gradually decreases along the flow direction in the flow channel, the flow rate of the flow equalization holes closer to the air inlet is large, and the flow rate of the flow equalization holes farther from the air inlet is small. The drying gas preferentially flows out from the flow equalization holes closer to the air inlet, thus forming an uneven airflow distribution in the chamber. The consequence of this is that a small number of wafers will have defects due to over-drying, while most wafers will still have residual moisture due to insufficient drying, ultimately affecting the wafer product yield.

[0004] Therefore, how to provide a drying mechanism that can make the airflow act uniformly on the wafer from both sides is a technical problem that needs to be solved by those skilled in the art. Utility Model Content

[0005] This application provides a wafer drying mechanism that enables the drying airflow to act uniformly on the wafer, avoiding the problems of insufficient or excessive drying of the wafer, thereby improving the yield of wafer products.

[0006] The technical solution adopted in this application is as follows: A wafer drying mechanism, comprising: The drying chamber has an air inlet on its side wall for introducing drying gas; A flow equalization plate is disposed on the inner wall of the drying chamber, and the flow equalization plate and the side wall of the drying chamber define a flow channel for the drying gas to flow. The flow equalization plate has a plurality of flow equalization holes, and the flow area of ​​the flow equalization holes increases as the distance between the flow equalization holes and the air inlet increases.

[0007] Preferably, the flow equalization holes include at least a first group of holes, a second group of holes, and a third group of holes arranged sequentially from the center to the periphery on the flow equalization plate. The flow area of ​​the flow equalization holes in the second group of holes is greater than the flow area of ​​the first group of holes, and the flow area of ​​the flow equalization holes in the third group of holes is greater than the flow area of ​​the second group of holes.

[0008] Preferably, the diameters of the flow equalization holes in the first orifice group, the second orifice group, and the third orifice group increase sequentially.

[0009] Preferably, the drying chamber is provided with at least two placement stations for accommodating wafer baskets.

[0010] Preferably, the flow equalization plate is provided with at least two flow equalization areas corresponding to the placement station, and each flow equalization area is provided with the flow equalization hole.

[0011] Preferably, the mechanism further includes a movable jet pipe disposed above the drying chamber for jet purging into the drying chamber.

[0012] Preferably, the jet pipe has a plurality of elongated vent holes, the extension direction of which is parallel to the axis of the jet pipe. Along the axial direction of the jet pipe, any two adjacent vent holes are spaced at a predetermined distance.

[0013] Preferably, the vent holes are arranged in two rows, and the channels of the two rows of vent holes are inclined towards each other.

[0014] Preferably, the mechanism further includes a cover disposed on the top of the drying chamber for covering the drying chamber to maintain the internal temperature.

[0015] Preferably, the cover is a folding structure, comprising two plate groups. One plate group includes a first plate and a second plate rotatably connected by a first hinge, and the other plate group includes a third plate and a fourth plate rotatably connected by a second hinge. The first plate and the third plate abut against each other, causing the second plate and the fourth plate to abut against the top of the opposite side walls of the drying chamber, respectively. The first plate, the second plate, the third plate, and the fourth plate form a continuous plane.

[0016] According to the specific embodiments provided in this application, the following technical effects are disclosed: This application relates to the field of semiconductor processing equipment technology, and more particularly to a wafer drying mechanism, comprising: a drying chamber with an air inlet on its side wall for introducing drying gas; a flow equalization plate disposed on the inner side wall of the drying chamber, defining a flow channel for the drying gas to flow between the flow equalization plate and the side wall of the drying chamber; and a plurality of flow equalization holes on the flow equalization plate, the flow area of ​​which increases with the distance between the flow equalization hole and the air inlet. In this design, a smaller flow area is provided in the high-pressure region near the air inlet to increase the local flow resistance of the drying gas, thereby limiting excessive gas flow. In the low-pressure region far from the air inlet, a larger flow area is provided to reduce the local flow resistance of the drying gas, ensuring sufficient gas flow. This balances the uneven gas flow caused by the pressure difference, making the gas flow of the flow equalization holes at different positions on the entire flow equalization plate more uniform, avoiding the problem of insufficient or excessive wafer drying, and thus improving the yield of wafer products. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0018] Figure 1 This is a schematic diagram showing the jet pipe provided in an embodiment of this application located above the drying chamber; Figure 2 This is a schematic diagram showing the distribution of flow equalization holes on the flow equalization plate provided in the embodiments of this application; Figure 3 This is a schematic diagram of the jet pipe provided in an embodiment of this application; Figure 4 This is a side view schematic diagram of the jet pipe provided in the embodiment of this application operating above the drying chamber; Figure 5 This is a schematic diagram of the cover provided in an embodiment of this application; Figure 6 This is a schematic diagram of the cover provided in the embodiment of this application covering the top of the drying chamber.

[0019] Figure label: 1. Drying chamber; 10. Air inlet; 2. Flow equalization plate; 20. First orifice group; 21. Second orifice group; 22. Third orifice group; 200. Flow equalization hole; 3. Wafer flower basket; 4. Jet nozzle fittings; 40. Vent hole; 5. Cover; 50. First plate; 51. Second plate; 52. Third plate; 53. Fourth plate; 6. Crossbar; 7. Sliding groove; 8. Pulleys. Detailed Implementation

[0020] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0021] As described in the background section, Chinese invention patent CN115206846A places the flow equalization holes on a carrier plate. When a basket full of wafers is placed on the carrier plate, the bottom of the basket may block or completely cover the flow equalization holes, making it difficult for the drying gas to pass through and resulting in poor gas flow, which affects the drying effect of the wafers. To overcome the shortcomings of the bottom ventilation scheme, the prior art has proposed an improved scheme of setting flow equalization plates on both sides of the drying chamber, so that the drying gas acts on the wafers from the side. However, this scheme introduces a new problem: since the diameter and spacing of the flow equalization holes in the flow equalization plates are the same, and the pressure of the drying gas gradually decreases along the flow direction in the flow channel, the gas flow rate of the flow equalization holes closer to the air inlet is large, and the gas flow rate of the flow equalization holes farther from the air inlet is small. The drying gas preferentially flows out from the flow equalization holes closer to the air inlet, thus forming an uneven airflow distribution in the chamber. The consequence of this is that a small number of wafers will have defects due to over-drying, while most wafers will still have residual moisture due to insufficient drying, ultimately affecting the wafer product yield.

[0022] Based on this, this application provides a wafer drying mechanism, which aims to solve the problem of insufficient or excessive wafer drying caused by uneven airflow of drying gas in the prior art.

[0023] The embodiments of this application will be analyzed in detail below with reference to the accompanying drawings.

[0024] A wafer drying mechanism, reference Figure 1 and Figure 2 It includes: a drying chamber 1, the side wall of which is provided with an air inlet 10 for introducing drying gas; a flow equalization plate 2 provided on the inner side wall of the drying chamber 1, the flow equalization plate 2 and the side wall of the drying chamber 1 defining a flow channel for the drying gas to flow; the flow equalization plate 2 is provided with a plurality of flow equalization holes 200, the flow area of ​​the flow equalization holes 200 increases with the increase of the distance between the flow equalization holes 200 and the air inlet 10.

[0025] The air inlet 10 is connected to a drying gas supply device outside the wafer drying mechanism via a pipe. After the drying gas enters the flow channel through the air inlet 10, it disperses and flows towards the far end of the flow channel. During this process, pressure loss occurs due to friction with the flow channel wall (i.e., the surface of the flow equalization plate 2 and the inner wall of the drying chamber 1), causing the pressure of the drying gas to gradually decrease from the air inlet 10 to the ends of the flow channel. In this embodiment, the flow equalization hole 200 on the flow equalization plate 2 satisfies the characteristic that "the flow area of ​​the flow equalization hole 200 increases with the distance between the flow equalization hole 200 and the air inlet 10." The flow area refers to the effective cross-sectional area that the drying gas can actually pass through in the flow path. A larger flow area makes it easier for the gas to pass through, and vice versa. Specifically, in the high-pressure zone near the air inlet 10, a smaller flow area is used to create high flow resistance, limiting the outflow of excessive drying gas. In the low-pressure zone away from the air inlet 10, a larger flow area is used to create low flow resistance, ensuring sufficient drying gas outflow. This balances the pressure difference caused by pressure loss along the flow path and overcomes the problem of uneven airflow distribution in the original equal-diameter, equal-spacing flow equalizer, making the gas flow rate of the equalizing holes 200 at different positions on the entire flow equalizer 2 more consistent. Furthermore, uniform airflow means that all wafers in the wafer basket 3, and the moisture on the surface of each wafer, can be removed under the same conditions, avoiding the problems of insufficient or excessive wafer drying, thereby improving the yield of wafer products.

[0026] Based on the first example where "the flow area of ​​the uniform flow orifice 200 increases with the distance between the uniform flow orifice 200 and the air inlet 10", the spacing of the uniform flow orifices 200 remains constant, i.e., the density remains constant, and the diameter of the uniform flow orifice 200 gradually increases as it moves away from the air inlet 10. For example, on the orthographic projection surface of the air inlet 10 and the uniform flow plate 2, the diameter of the uniform flow orifice 200 in the region closer to the air inlet 10 is R1, the diameter of the uniform flow orifice 200 in the middle region slightly further away is R2, and the diameter of the uniform flow orifice 200 in the farthest region is R3, and R1 < R2 < R3.

[0027] Based on the second example where "the flow area of ​​the uniform flow orifice 200 increases with the distance between the uniform flow orifice 200 and the air inlet 10", the orifice diameter of the uniform flow orifice 200 is kept consistent, but the distribution density of the uniform flow orifice 200 is changed. For example, on the orthographic projection surface of the air inlet 10 and the uniform flow plate 2, the spacing of the uniform flow orifices 200 in the area close to the air inlet 10 is D1, the spacing of the uniform flow orifices 200 in the middle area slightly further away is D2, and the spacing of the uniform flow orifices 200 at the farthest end is D3, and D1 > D2 > D3 is satisfied.

[0028] Based on the third example that "the flow area of ​​the uniform flow hole 200 increases with the increase of the distance between the uniform flow hole 200 and the air inlet 10", and combining the above two examples, on the orthographic projection surface of the air inlet 10 and the uniform flow plate 2, in the direction close to the air inlet 10, the diameter of the uniform flow hole 200 and the density of the uniform flow hole 200 can be appropriately reduced, and in the direction away from the air inlet 10, the diameter of the uniform flow hole 200 and the density of the uniform flow hole 200 can be appropriately increased.

[0029] In summary, the gas flow rate of the flow equalization holes 200 at different positions on the entire flow equalization plate 2 is made to be consistent.

[0030] As a preferred embodiment, refer to Figure 2 The flow equalization hole 200 includes at least a first orifice group 20, a second orifice group 21 and a third orifice group 22 arranged sequentially from the center to the periphery on the flow equalization plate 2. The flow area of ​​the flow equalization hole 200 in the second orifice group 21 is greater than the flow area of ​​the first orifice group 20, and the flow area of ​​the flow equalization hole 200 in the third orifice group 22 is greater than the flow area of ​​the second orifice group 21.

[0031] The three orifice groups are arranged in a stepped manner, with the flow area increasing from the center outwards. This balances the pressure distribution of the drying gas within the flow channel, providing high flow resistance near the inlet 10 and low flow resistance at the distal end, ensuring a uniform gas flow rate from the three orifice groups. Furthermore, on the orthographic projection surface of the inlet 10 and the flow equalization plate 2, the center of the three orifice groups is the orthographic projection point of the inlet 10.

[0032] As an example, refer to Figure 1 and Figure 2 The flow equalization holes 200 in the first orifice group 20 are arranged in a rectangular array, the flow equalization holes 200 in the second orifice group 21 are arranged in a rectangular frame array around the outer periphery of the first orifice group 20, and the flow equalization holes 200 in the third orifice group 22 are arranged in a rectangular frame array around the outer periphery of the second orifice group 21.

[0033] Since most of the drying chambers 1 and wafer baskets 3 are rectangular, the three orifice groups are arranged in a rectangular shape to evenly cover the work area of ​​the wafer baskets 3, ensuring that all wafers in the work area receive a consistent drying effect. In the central first orifice group 20 area, a smaller orifice diameter provides greater flow resistance to limit the drying airflow; in the middle second orifice group 21 area, a medium orifice diameter provides medium flow resistance to moderately guide the drying airflow; and in the outermost third orifice group 22 area, a larger orifice diameter provides minimum flow resistance to enhance the output of the drying airflow.

[0034] As a preferred embodiment, refer to Figure 2The diameter of the flow equalization holes 200 in the first orifice group 20, the second orifice group 21 and the third orifice group 22 increases sequentially.

[0035] Among them, the diameter of the flow equalization holes 200 in the three orifice groups gradually increases, so that the flow area gradually increases, matching the pressure distribution from high pressure to low pressure in the flow channel from the air inlet 10 to the surrounding area, ensuring that the gas flow rate of each orifice group is uniform.

[0036] As a preferred embodiment, refer to Figure 1 The drying chamber 1 is equipped with at least two placement stations for accommodating the wafer baskets 3.

[0037] The multiple placement stations allow a single drying chamber 1 to dry a larger number of wafers, thus increasing the capacity of the drying chamber 1.

[0038] As an example, refer to Figure 1 The drying chamber 1 has two placement stations, which are arranged along the length of the drying chamber 1. Two flow equalization plates 2 are located on both sides of the placement stations.

[0039] As a preferred embodiment, refer to Figure 1 and Figure 2 The flow equalization plate 2 is provided with at least two flow equalization areas corresponding to the placement positions, and each flow equalization area is provided with flow equalization holes 200.

[0040] As an example, Figure 1 The flow equalization plate 2 has two flow equalization regions A. Each flow equalization region A has a first orifice group 20, a second orifice group 21 and a third orifice group 22. The diameter of the flow equalization holes 200 in the three orifice groups increases sequentially.

[0041] As a preferred embodiment, refer to Figure 1 , Figure 3 and Figure 4 The mechanism also includes a movable jet pipe 4 located above the drying chamber 1 for jet purging into the drying chamber 1.

[0042] The jet nozzle 4 can be connected to a drying gas supply device outside the wafer drying mechanism. The jet nozzle 4 moves horizontally above the drying chamber 1 and continuously sprays drying gas. Combined with the drying gas sprayed from both sides of the wafer basket 3, it achieves all-round drying of the wafer.

[0043] As a preferred embodiment, refer to Figure 3 The jet pipe 4 has several elongated vent holes 40, the extension direction of which is parallel to the axis of the jet pipe 4; in the axial direction of the jet pipe 4, any two adjacent vent holes 40 are spaced apart by a preset distance.

[0044] The vents 40 are spaced apart rather than being a single, elongated slit. This avoids excessive length of the vents 40, which could lead to deformation under prolonged high-temperature operation and affect the service life of the jet nozzle 4. It should be noted that the spacing between the two vents 40 is set according to actual operating conditions. The extension direction of the vents 40 is parallel to the axis of the jet nozzle 4, creating an airflow surface with the dry gas ejected from the jet nozzle 4. This increases the contact area between the dry gas and the wafer, thus better removing moisture from the wafer surface.

[0045] As a preferred embodiment, refer to Figure 3 and Figure 4 The vent holes 40 are arranged in two rows, and the channels of the two rows of vent holes 40 are inclined towards each other.

[0046] As an example, refer to Figure 4 When the jet nozzle 4 is located directly above the drying chamber 1, the normal direction of the orifice of one row of vents 40 is defined as the first direction, and the vents 40 in this row blow dry gas in the first direction. The normal direction of the orifice of the other row of vents 40 is defined as the second direction, and the vents 40 in this row blow dry gas in the second direction. The first direction and the second direction form an angle of 45° to 90°. Figure 4 The dashed line on the left indicates the first direction, and the dashed line on the right indicates the second direction, to balance the coverage area and purging intensity of the airflow. When the jet nozzle 4 is located at the upper left of the drying chamber 1, the jet nozzle 4 rotates counterclockwise by a certain angle, ensuring that all the drying gas ejected from the two rows of vents 40 acts on the surface of the wafer, preventing it from spraying outside the drying chamber 1 and improving the utilization rate of the drying gas. When the jet nozzle 4 is located at the upper right of the drying chamber 1, the jet nozzle 4 rotates clockwise by a certain angle, ensuring that all the drying gas ejected from the two rows of vents 40 acts on the surface of the wafer, preventing it from spraying outside the drying chamber 1 and improving the utilization rate of the drying gas.

[0047] As an alternative to the above example, the jet nozzle 4 can move only horizontally without rotation. The jet nozzle 4 moves back and forth in a straight line above the drying chamber 1. When the jet nozzle 4 moves to the side of the drying chamber 1, the drying gas ejected from the two rows of vents 40 can still cover the surface of the wafer, achieving the drying process. In a preferred embodiment, there are multiple jet nozzles 4, evenly arranged at the top of the drying chamber 1.

[0048] Among them, the parallel operation of multiple jet nozzles 4 can shorten the drying time and achieve faster purging of the wafer.

[0049] As a preferred embodiment, refer to Figure 5 and Figure 6The mechanism also includes a cover 5 located on top of the drying chamber 1 to cover the drying chamber 1 and maintain the internal temperature.

[0050] The cover 5 is open when the jet nozzle 4 is spraying air, and closed when the jet nozzle 4 stops working but there are still wafer baskets 3 drying in the drying chamber 1, and when there are no wafer baskets 3 in the drying chamber 1. On the one hand, it maintains the thermal environment and ensures the stability of the drying process, and on the other hand, it prevents external dust from falling into the drying chamber 1 and maintains the internal cleanliness.

[0051] In a preferred embodiment, the cover 5 is a folding structure, comprising two plate groups. One plate group includes a first plate 50 and a second plate 51 rotatably connected by a first hinge, and the other plate group includes a third plate 52 and a fourth plate 53 rotatably connected by a second hinge. The first plate 50 and the third plate 52 abut against each other, causing the second plate 51 and the fourth plate 53 to abut against the top of the opposite side walls of the drying chamber 1, respectively. The first plate 50, the second plate 51, the third plate 52 and the fourth plate 53 form a continuous plane.

[0052] The cover 5 adopts a folding structure, which reduces the space occupied by the cover 5 itself, and also facilitates the quick opening of the cover 5 when picking up and putting down the wafer basket 3, thus shortening the picking and putting down and transporting time of the wafer basket 3.

[0053] As an example, further reference Figure 5 and Figure 6 The drying chamber 1 has crossbars 6 at the top of its two long side walls and sliding grooves 7 at the top of its two short side walls. Both ends of the first plate 50 and both ends of the third plate 52 are equipped with pulleys 8, which slide within the corresponding sliding grooves 7. When the first plate 50 and the third plate 52 slide towards each other and abut, the second plate 51 and the fourth plate 53 are secured to the crossbars 6 by their respective outer recesses, forming a continuous plane. At this time, the cover 5 is in a closed state. When the cover 5 needs to be opened, the staff or robot needs to lift the second plate 51 and the fourth plate 53 respectively, so that the recessed structure of the two separates from the crossbar 6, and then drag the second plate 51 and the fourth plate 53 outward, so that the first plate 50 and the third plate 52 move apart and break the contact. When the pulleys 8 on the first plate 50 and the third plate 52 reach the ends of the sliding groove 7 respectively, the cover 5 is in a fully open state. At this time, the second plate 51 is suspended from the first plate 50 through the first hinge, and the fourth plate 53 is suspended from the third plate 52 through the second hinge. The second plate 51 and the first plate 50 and the fourth plate 53 and the third plate 52 are all set at 90° perpendicularly.

[0054] In the description of this specification, the references to terms such as "one embodiment," "some embodiments," "example," "specific example," or "some examples," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of this application. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0055] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified.

[0056] Although embodiments of this application have been shown and described above, it is understood that the above embodiments are exemplary and should not be construed as limiting this application. Those skilled in the art can make changes, modifications, substitutions and variations to the above embodiments within the scope of this application.

Claims

1. A wafer drying mechanism, characterized in that, The institutions include: The drying chamber (1) has an air inlet (10) on its side wall for introducing drying gas. A flow equalization plate (2) is provided on the inner wall of the drying chamber (1), and the flow equalization plate (2) and the side wall of the drying chamber (1) define a flow channel for the drying gas to flow. The flow equalization plate (2) is provided with a plurality of flow equalization holes (200), and the flow area of ​​the flow equalization holes (200) increases as the distance between the flow equalization holes (200) and the air inlet (10) increases.

2. The wafer drying mechanism according to claim 1, characterized in that, The flow equalization hole (200) includes at least a first orifice group (20), a second orifice group (21) and a third orifice group (22) arranged sequentially from the center to the periphery on the flow equalization plate (2). The flow area of ​​the flow equalization hole (200) in the second orifice group (21) is greater than the flow area of ​​the first orifice group (20), and the flow area of ​​the flow equalization hole (200) in the third orifice group (22) is greater than the flow area of ​​the second orifice group (21).

3. The wafer drying mechanism according to claim 2, characterized in that, The diameters of the flow equalization holes (200) in the first orifice group (20), the second orifice group (21), and the third orifice group (22) increase sequentially.

4. The wafer drying mechanism according to any one of claims 1 to 3, characterized in that, The drying chamber (1) is provided with at least two placement stations for accommodating the wafer baskets (3).

5. The wafer drying mechanism according to claim 4, characterized in that, The flow equalization plate (2) is provided with at least two flow equalization areas corresponding to the placement station, and each flow equalization area is provided with the flow equalization hole (200).

6. The wafer drying mechanism according to claim 1, characterized in that, The mechanism also includes a movable jet pipe (4) located above the drying chamber (1) for jet purging into the drying chamber (1).

7. The wafer drying mechanism according to claim 6, characterized in that, The jet pipe (4) has several elongated vent holes (40), and the extension direction of the vent holes (40) is parallel to the axis of the jet pipe (4). In the axial direction of the jet pipe (4), any two adjacent vent holes (40) are spaced by a predetermined distance.

8. The wafer drying mechanism according to claim 7, characterized in that, The ventilation holes (40) are arranged in two rows, and the channels of the two rows of ventilation holes (40) are inclined towards each other.

9. The wafer drying mechanism according to claim 1, characterized in that, The mechanism also includes a cover (5) located on top of the drying chamber (1) for covering the drying chamber (1) to maintain the internal temperature.

10. The wafer drying mechanism according to claim 9, characterized in that, The cover (5) is a folding structure, comprising two plate groups. One plate group includes a first plate (50) and a second plate (51) rotatably connected by a first hinge. The other plate group includes a third plate (52) and a fourth plate (53) rotatably connected by a second hinge. The first plate (50) and the third plate (52) abut against each other, causing the second plate (51) and the fourth plate (53) to abut against the top of the opposite side walls of the drying chamber (1). The first plate (50), the second plate (51), the third plate (52) and the fourth plate (53) form a continuous plane.

Citation Information

Patent Citations

  • Semiconductor process equipment and drying device thereof

    CN115206846A