Display back panel and display module
By using nano-injection molding of metal substrates and plastic parts, the problems of high weight and processing cost of automotive display back panels have been solved, achieving a lightweight and thin design and efficient production, and improving connection reliability and structural strength.
Patent Information
- Application Number
- CN202522748158.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-24
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-12-24
AI Technical Summary
Existing automotive display back panels are too heavy to meet the requirements for lightweight and thin designs, and have high processing costs, short mold life, poor processing precision, and cannot form complex structures.
The process utilizes nano-injection molding of metal substrates and plastic parts. By forming a nanoscale microporous structure on the metal substrate and embedding the plastic parts within the micropores, the process is simplified and the connection reliability is improved through the integrated manufacturing of heterogeneous materials.
The design of the monitor back panel is made thinner and lighter, which reduces processing costs and weight, improves connection reliability and production efficiency, and enhances the overall structural strength.
Smart Images

Figure CN224958395U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of display technology, and more particularly to a display backplate and display module. Background Technology
[0002] The design of automotive display back panels needs to meet stringent automotive-grade requirements to ensure long-term reliability, safety, and durability in complex automotive environments such as vibration, high and low temperature shocks, and humidity changes.
[0003] In related technologies, automotive display back panels are manufactured using integrated die casting combined with subsequent CNC (Computer Numerical Control) precision machining. Die-cast automotive display back panels offer good strength and reliability; however, the minimum wall thickness is limited by the die-casting process, resulting in a heavy weight that cannot meet the demands for lightweight and thin products. Furthermore, die-casting molds have short lifespans, requiring frequent replacements and increasing mold costs. Subsequent CNC machining suffers from poor precision, making it impossible to form complex structures, and low CNC production efficiency, further increasing the manufacturing cost of automotive display back panels. Utility Model Content
[0004] This application provides a display back panel and a display module, which reduces the weight of the display back panel and simplifies the manufacturing process, thereby at least partially solving the above-mentioned technical problems.
[0005] To achieve the above objectives, according to a first aspect of this application, a display backplate is provided, comprising: Metal matrix; A plastic part is connected to the periphery of the metal substrate, and the plastic part and the metal substrate are connected to form a receiving cavity; The metal substrate has a number of nanoscale microporous structures, and the plastic part is embedded in the microporous structures.
[0006] Optionally, the metal substrate includes a base plate and a connecting portion, with the connecting portion disposed on at least one side of the base plate, and the plastic part being fitted and connected to the connecting portion.
[0007] Optionally, the connecting portion includes a bent portion that extends from one side of the base plate and is bent and connected to the base plate, and the plastic part covers the bent portion.
[0008] Optionally, the connecting portion includes a plurality of protrusions, which are spaced apart. Adjacent protrusions form a groove with the base plate, and the plastic part fills the groove and covers the protrusions.
[0009] Optionally, the protrusion extends from one side of the base plate and is bent and connected to the base plate.
[0010] Optionally, the groove portion includes a first groove portion and a second groove portion, wherein the first groove portion is closer to the bottom plate than the second groove portion, and the size of the first groove portion is larger than the size of the second groove portion.
[0011] Optionally, the metal substrate is formed into the microporous structure through nanoprocessing, wherein the pore size of the microporous structure is D, and 100nm≤D≤150nm.
[0012] Optionally, the pore walls of the microporous structure are concave and convex, and the pore size of the concave and convex surface is d, wherein 10nm≤d≤40nm.
[0013] Optionally, the plastic part includes a positioning portion disposed at at least two corners of the base plate, and the side of the positioning portion located within the receiving cavity is at least partially lower than the side of the base plate located within the receiving cavity.
[0014] According to a second aspect of this application, a display module is provided, including a display back panel as described in any of the preceding claims.
[0015] In the display back panel and display module of this application embodiment, the display back panel is made of metal substrate and plastic parts through nano-injection molding, which simplifies the processing technology, reduces processing costs, and reduces the weight of the display back panel. This is conducive to realizing the thin and light design of the display back panel and the entire display module. The plastic parts and microporous structure form a mechanical interlock, which improves the connection reliability between the metal substrate and the plastic parts.
[0016] Other features and advantages of this application will be described in detail in the following detailed description section. Attached Figure Description To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0017] To gain a more complete understanding of this application and its beneficial effects, the following description will be provided in conjunction with the accompanying drawings, wherein the same reference numerals in the following description denote the same parts.
[0018] Figure 1 This is a first axial view of the display back panel provided in an exemplary embodiment of this disclosure; Figure 2 This is a second axial view of the display backplate provided in an exemplary embodiment of this disclosure; Figure 3 yes Figure 2 Enlarged schematic diagram of part B in the middle; Figure 4 yes Figure 2 An enlarged schematic diagram of part A in the middle; Figure 5 This is a schematic diagram of the structure of the metal substrate of the display back panel provided in an exemplary embodiment of this disclosure; Figure 6 This is a schematic diagram of the structure of the plastic component of the display back panel provided in an exemplary embodiment of this disclosure; Figure 7 This is an enlarged schematic diagram of the microporous structure provided in an exemplary embodiment of this disclosure; Figure 8 This is an enlarged view of the connection between the plastic part and the microporous structure provided in the exemplary embodiments of this disclosure; Figure 9 This is a top view of the display back panel provided in an exemplary embodiment of this disclosure; Figure 10 yes Figure 9 CC section view; Figure 11 yes Figure 10 A magnified view of a section at point D.
[0019] Explanation of reference numerals in the attached figures: 100. Monitor back panel; 110. Metal substrate; 111. Base plate; 1111. First side; 1112. Second side; 1113. Third side; 1114. Fourth side; 112. Connecting part; 1121. Bending part; 1122. Protrusion; 113. Groove; 1131. First groove wall; 1132. Second groove wall; 1133. First groove; 1134. Second groove; 114. Microporous structure; 115. Concave-convex surface; 120. Plastic part; 121. Plastic frame; 1211. First side wall; 1212. Second side wall; 1213. Third side wall; 1214. Fourth side wall; 122. Filler part; 123. Clearance part; 124. Positioning part; 130. First connecting part; 140. Second connecting part; 150. Third connecting part; 160. Receiving cavity. Detailed Implementation
[0020] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the protection scope of this application.
[0021] See Figure 1 , Figure 2 , Figure 7 , Figure 8 , Figure 9 , Figure 10 and Figure 11 This application provides a display back panel 100, which can be applied to backlight modules, such as for use as an automotive back panel. The display back panel 100 includes a metal substrate 110 and a plastic component 120. The plastic component 120 is connected to the periphery of the metal substrate 110, and the plastic component 120 and the metal substrate 110 are integrally bonded through a nano-molding process. The plastic component 120 and the metal substrate 110 are connected to form a receiving cavity 160. The metal substrate 110 is processed with nanotechnology to form a nanoscale microporous structure 114, and the plastic component 120 is embedded within the microporous structure 114.
[0022] The metal substrate 110 is a stamped part, manufactured from metal materials using a stamping process. The material for the metal substrate 110 is selected from the AL1000~7000 series, such as AL5052. The plastic part 120 can be made of PPA, PPS, PAT, etc. Using a stamped metal substrate 110 instead of a traditional die-cast part simplifies the processing and reduces manufacturing costs. The combination of the metal substrate 110 and the plastic part 120 significantly reduces the weight of the display back panel 100, facilitating a thinner and lighter design for the display back panel 100.
[0023] By using nano-injection molding, the plastic part 120 is directly molded onto the metal substrate 110, achieving integrated manufacturing of heterogeneous materials. Compared to die-cast backplates, which require multiple secondary processing (such as CNC) and assembly, this solution offers faster production cycles, better consistency, and lower overall production costs.
[0024] In some examples, a microporous structure 114 is prepared on the surface of the metal substrate 110 by chemical or electrochemical means. The microporous structure 114 contains residual chemical treatment liquid. The plastic part 120 reacts chemically with the chemical treatment liquid in the microporous structure 114 and fuses with it, resulting in an anchoring effect in the plastic, which improves the reliability of the connection between the metal substrate 110 and the plastic part 120.
[0025] In this embodiment, the display back panel 100 is formed by nano-injection molding of a metal substrate 110 and a plastic part 120. Compared with the die-cast automotive back panels in related technologies, the back panel is lighter, which is beneficial for achieving a thinner and lighter design of the display back panel 100 and the entire display module. The plastic part 120 and the microporous structure 114 form a mechanical interlock, which can better buffer and adapt to the thermal stress caused by the difference in thermal expansion coefficients between the metal and the plastic, and improve the connection reliability between the metal substrate 110 and the plastic part 120.
[0026] In some examples, a metal substrate 110 is prepared using a stamping process, and a microporous structure 114 is prepared on the surface of the metal substrate 110 using chemical or electrochemical methods. Then, the metal substrate 110 is placed in an injection mold, and molten engineering plastic is injected into the mold. After cooling and solidification, the display back panel 100 is formed by demolding. The processing technology of the display back panel 100 in the embodiments of this application is simple and reduces processing costs.
[0027] In some embodiments, see Figure 2 , Figure 3 , Figure 4 and Figure 5 The metal substrate 110 includes a base plate 111 and a connecting part 112. The connecting part 112 is provided on at least one side of the base plate 111, and the plastic part 120 is fitted and connected to the connecting part 112.
[0028] For example, see Figure 2 , Figure 3 , Figure 4 and Figure 5 The base plate 111 is a rectangular flat plate, and includes a first side 1111, a second side 1112, a third side 1113, and a fourth side 1114. The first side 1111 and the third side 1113 are arranged opposite to each other, and the second side 1112 and the fourth side 1114 are arranged opposite to each other. A connecting portion 112 is provided on the first side 1111 of the base plate 111. The connecting portion 112 includes a first side located in the receiving cavity 160. A plastic part 120 is fitted and connected to the connecting portion 112, and the plastic part 120 covers the other sides of the connecting portion 112 except for the first side. The plastic part 120 is disposed with the base plate 111.
[0029] In this embodiment, compared to the plastic part 120 being directly bonded to the side of the base plate 111, the plastic part 120 is connected to the base plate 111 through the connecting part 112, and the plastic part 120 is fitted into the connecting part 112, which increases the contact connection between the plastic part 120 and the metal substrate 110. The plastic part 120 and the metal substrate 110 are firmly bonded, which improves the reliability of the display back panel 100.
[0030] See some sub-instances. Figure 2 , Figure 3 , Figure 4 and Figure 5 The connecting part 112 includes a bent part 1121, which extends from one side of the base plate 111 and is bent and connected to the base plate 111. The plastic part 120 covers at least one side and top surface of the bent part 1121 away from the receiving cavity 160.
[0031] For example, see Figure 2 , Figure 3 , Figure 4 and Figure 5The bending portion 1121 is disposed on the first side 1111 of the base plate 111, and the bending portion 1121 is formed by bending the edge of the first side 1111 of the base plate 111 upward or downward. During injection molding, the plastic part 120 covers the sidewall at least from the outer side and top of the bending portion 1121.
[0032] In this embodiment, the sidewall of the display back panel 100 is formed by connecting the bent portion 1121 to the plastic part 120, which not only increases the contact area and interlocking volume between the metal substrate 110 and the plastic, but also improves the overall rigidity and torsional strength of the display back panel 100.
[0033] In some embodiments, see Figure 2 , Figure 3 , Figure 4 and Figure 5 The connecting portion 112 includes a plurality of protrusions 1122, which are spaced apart. Adjacent protrusions 1122 form a groove 113 with the base plate 111. The plastic part 120 fills the groove 113 and covers the protrusions 1122. The plurality of protrusions 1122 are equally spaced along the direction extending from the side of the base plate 111.
[0034] In some examples, see Figure 2 , Figure 3 , Figure 4 ,and Figure 5 A protrusion 1122 is formed by a toothed structure cut from the side of the base plate 111. The protrusion 1122 and the base plate 111 are located in the same plane, and adjacent protrusions 1122 and the side of the base plate 111 form a groove 113. Correspondingly, the plastic part 120 has a filling part 122 corresponding to the groove 113 on the base plate 111, and a clearance area corresponding to the protrusion 1122, which engage with the toothed structure on the base plate 111.
[0035] In some examples, the protrusion 1122 is formed by bulging from one side of the base plate 111 to the other side, and the protrusion 1122 is disposed near the edge of the base plate 111. Adjacent protrusions 1122 and the surface of the base plate 111 form a groove 113. The plastic part 120 is perpendicularly connected to the base plate 111, and the plastic part 120 covers the protrusion 1122 and fills the groove 113.
[0036] In this embodiment, the connecting portion 112 consists of multiple spaced protrusions 1122, and the plastic part 120 and the connecting portion 112 form a multi-interlocking structure, which improves the connection reliability between the plastic part 120 and the metal substrate 110.
[0037] See in some examples Figure 2 , Figure 3 , Figure 4 , Figure 5 and Figure 6 The protrusion 1122 extends from one side of the base plate 111 and is bent and connected to the base plate 111.
[0038] See some sub-examples. Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 and Figure 11 The base plate 111 has a bent portion 1121 on its first side 1111, and protrusions 1122 on its second side 1112, third side 1113, and fourth side 1114. The bent portion 1121 is formed by bending the edge of the first side 1111 of the base plate 111 upwards. The protrusions 1122 are spaced apart along the extending direction of the side of the base plate 111 on which they are located. The protrusions 1122 on the second side 1112 are spaced apart along the extending direction of the second side 1112, the protrusions 1122 on the third side 1113 are spaced apart along the extending direction of the third side 1113, and the protrusions 1122 on the fourth side 1114 are spaced apart along the extending direction of the fourth side 1114. Adjacent protrusions 1122 form grooves 113 on the side of the base plate 111, and a toothed structure perpendicular to the base plate 111 is formed on the side of the base plate 111. The plastic part 120 is a plastic frame 121. The plastic frame 121 includes a first sidewall 1211, a second sidewall 1212, a third sidewall 1213, and four sidewalls. The first sidewall 1211 is connected to the bent portion 1121 on the first side 1111, and the first sidewall 1211 covers the outer surface and top surface of the bent portion 1121. The second sidewall 1212 corresponds to the second side 1112, the third sidewall 1213 corresponds to the third side 1113, and the fourth sidewall 1214 corresponds to the fourth side plate. The plastic part 120 has a filling portion 122 corresponding to the groove 113 on the base plate 111, and a clearance portion 123 corresponding to the protrusion 1122. The second sidewall 1212 and the corresponding second sidewall 1112 form a toothed structure that engages with each other. The third sidewall 1213 and the corresponding third sidewall 1113 form a toothed structure that engages with each other. The fourth sidewall 1214 and the corresponding fourth sidewall 1114 form a toothed structure that engages with each other. The protrusions 1122 and the plastic part 120 together form the sidewall of the display back panel 100, and the bent part 1121 and the plastic part 120 form the sidewall of the display back panel 100, which improves the structural strength of the sidewall of the display back panel 100, increases the contact area and interlocking volume between the metal substrate 110 and the plastic, and ensures reliable connection between the metal substrate and the plastic part 120.
[0039] In some embodiments, see Figure 3 , Figure 4 and Figure 5The groove portion 113 includes a first groove portion 1133 and a second groove portion 1134. The first groove portion 1133 is closer to the bottom plate 111 than the second groove portion 1134, and the size of the first groove portion 1133 is larger than the size of the second groove portion 1134.
[0040] In some embodiments, see Figure 3 , Figure 4 and Figure 5 A protrusion 1122 extends from one side of the base plate 111 and is bent and connected to the base plate 111. Adjacent protrusions 1122 and the side of the base plate 111 form a groove 113. The groove 113 includes a first groove wall 1131 and a second groove wall 1132, with the first groove wall 1131 and the second groove being disposed opposite each other. A section of the first groove wall 1131 away from the base plate 111 protrudes toward the second groove wall 1132. Thus, the groove 113 is formed with at least a first groove 1133 and a second groove 1134.
[0041] In this embodiment of the application, by setting the size of the first groove 1133 to be larger than the size of the second groove 1134, the groove 113 forms a structure that is smaller at the top and larger at the bottom. The plastic part 120 fills the groove 113 and forms an interlocking structure with the groove 113, thereby improving the connection strength between the plastic part 120 and the metal substrate 110.
[0042] In some embodiments, see Figure 7 The metal substrate 110 is nano-processed to form a microporous structure 114, the pore size of the microporous structure 114 being D, wherein 100nm≤D≤150nm. The value of D can be 100nm, 110nm, 120nm, 130nm, 140nm, 145nm, 150nm or other unlisted values.
[0043] In this embodiment, the aperture of the microporous structure 114 is set within a suitable range to ensure that the plastic can be injected deeply and smoothly into the micropores to form a strong "plastic rivet" structure, thereby achieving a high-strength macroscopic mechanical interlock between the metal and the plastic, providing the main structural load-bearing capacity for the overall connection.
[0044] In some embodiments, see Figure 7 The pore walls of the microporous structure 114 are concave-convex surfaces 115, and the pore size of the concave-convex surface 115 is d, where 10nm≤d≤40nm. The value of d can be 10nm, 20nm, 30nm, 350nm, 40nm or other unlisted values.
[0045] In this embodiment, the walls of the microporous structure 114 are irregular surfaces 115, forming a secondary micro-rough structure that maximizes the bonding area and micro-mechanical interlocking. The concave hole size d is set within a suitable range, increasing the physical surface area of the plastic-metal contact. Furthermore, when the plastic penetrates the tiny concave holes, it forms numerous additional micro-anchor points with varying orientations, significantly improving the bonding strength and durability of the interface, and enhancing the reliability and long-term stability of the connection.
[0046] In some embodiments, see Figure 3 , Figure 4 and Figure 6 For mounting the light guide plate, the plastic part 120 includes a positioning part 124, which is disposed on at least two corners of the base plate 111. The side of the positioning part 124 located in the receiving cavity 160 is at least partially lower than the side of the base plate 111 located in the receiving cavity 160.
[0047] See in some examples Figure 3 , Figure 4 and Figure 6 The plastic part 120 includes a plastic frame 121 and a positioning part 124. The plastic frame 121 and the positioning part 124 are integrally injection molded, which facilitates processing and reduces processing steps.
[0048] See some sub-examples. Figure 2 , Figure 3 , Figure 4 , Figure 5 and Figure 6The base plate 111 includes a first side 1111, a second side 1112, a third side 1113, and a fourth side 1114. The first side 1111 and the third side 1113 are arranged opposite to each other, and the second side 1112 connects the first side 1111 and the third side 1113. The first side 1111 has a bent portion 1121, and the second side 1112, the third side 1113, and the fourth side 1114 all have protrusions 1122. Positioning portions 124 are provided at the first corners of the second side 1112 and the third side 1113, and at the second corners of the second side 1112 and the fourth side 1114. The base plate 111 at the first corner and the second corner both form stepped side surfaces, and the positioning portions 124 are connected to and fitted into the stepped side surfaces. The plane on one side of the positioning part 124 located in the receiving cavity 160 is at least partially lower than the plane on one side of the base plate 111 located within the receiving cavity 160. The positioning part 124 is an "L"-shaped groove, ensuring the accuracy and firmness of its own installation and preventing displacement during injection molding or use. The positioning part 124 and the base plate 111 together form the bottom of the display back panel 100. The thickness of the positioning part 124 is at least partially less than the thickness of the base plate 111, and the positioning part 124 is recessed into one side of the base plate 111 located within the receiving cavity 160. Two positioning parts 124 are spaced apart for positioning and installing the light guide plate.
[0049] In some examples, the base plate 111 has mounting holes near the corners, and the positioning part 124 is formed in the mounting holes by injection molding.
[0050] In this embodiment, by forming a positioning part 124 on the back panel, the structural strength of the display back panel 100 is optimized, precise positioning and assembly are facilitated, and the performance and cost of the display back panel 100 are balanced.
[0051] In some embodiments, see Figure 2 , Figure 3 , Figure 4 and Figure 6 The plastic component 120 includes a plastic frame 121, on the side of the plastic frame 121 away from the base plate 111, a plurality of first snap-fit portions 130 are formed. Each first snap-fit portion 130 can be a slot. The first sidewall 1211, second sidewall 1212, third sidewall 1213, and fourth sidewall 1114 are all provided with first snap-fit portions 130, which are used for assembling and fixing the hollow frame of the display module. The display backplate 100 and the entire display module can be quickly snapped into place without the need for tools.
[0052] In some embodiments, see Figure 2 , Figure 3 , Figure 4 , Figure 5 and Figure 6The plastic component 120 includes a plastic frame 121, on the side of the plastic frame 121 away from the receiving cavity 160, a plurality of second snap-fit portions 140 are formed. The second snap-fit portions 140 can be slots. The second snap-fit portions 140 are formed in the middle and / or bottom of the outer side of the plastic frame 121. The second snap-fit portions 140 are used to precisely engage with clips or guide rails on the device housing, such as on a center console, to achieve quick snap-fit installation of the display back panel 100 and the entire display module without the need for tool locking.
[0053] In some embodiments, see Figure 2 , Figure 3 , Figure 4 , Figure 5 and Figure 6 The plastic component 120 includes a plastic frame 121, on one side of the receiving cavity 160, a plurality of third snap-fit portions 150 are formed. Each third snap-fit portion 150 can be a slot. The third snap-fit portions 150 are used to fix and position internal components. The third snap-fit portions 150 provide a precise internal assembly reference, which is crucial for ensuring display uniformity, preventing light leakage and component displacement, and is a key structure for achieving precise internal assembly of the module.
[0054] According to a second aspect of this disclosure, a display module is provided, which includes the aforementioned display back panel 100. This display module possesses all the beneficial effects of the aforementioned display back panel 100, which will not be elaborated further herein.
[0055] In the description of this application, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more features. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.
[0056] In the above embodiments, the descriptions of each embodiment have different focuses. For parts not described in detail in a certain embodiment, please refer to the relevant descriptions in other embodiments.
[0057] The embodiments, implementation methods, and related technical features of this application can be combined and substituted for each other without conflict.
[0058] The above are merely preferred embodiments of this application and are not intended to limit this application in any way. Any simple modifications, equivalent changes, and alterations made to the above embodiments based on the technical essence of this application without departing from the scope of the technical solution of this application shall still fall within the scope of the technical solution of this application.
Claims
1. A display backplane, characterized by The display backboard comprises: a metal base; a plastic part connected to the periphery of the metal base, the plastic part and the metal base connected to form a containing cavity; wherein the metal base is formed with a plurality of nano-scale micro-pore structures, and the plastic part is embedded in the micro-pore structures.
2. The display backplane of claim 1, wherein, The metal base comprises a bottom plate and a connecting part, at least one side of the bottom plate is provided with the connecting part, and the plastic part is embedded and connected with the connecting part.
3. The display backplane of claim 2, wherein, The connecting part comprises a bending part, the bending part extends from one side of the bottom plate and is bently connected with the bottom plate, and the plastic part covers the bending part.
4. The display backplane of claim 2, wherein, The connecting part comprises a plurality of protruding parts, the plurality of protruding parts are arranged at intervals, adjacent protruding parts form a groove part with the bottom plate, the plastic part fills the groove part and covers the protruding parts.
5. The display backplane of claim 4, wherein, The protruding part extends from one side of the bottom plate and is bently connected with the bottom plate.
6. The display backplane of claim 5, wherein, The groove part comprises a first groove part and a second groove part, the first groove part is closer to the bottom plate than the second groove part, and the size of the first groove part is larger than the size of the second groove part.
7. The display backplane of claim 2, wherein, The metal base is formed with the micro-pore structure through nano processing, and the pore diameter of the micro-pore structure is D, wherein 100nm≤D≤150nm.
8. The display backplane of claim 7, wherein, The pore wall of the micro-pore structure is a concave-convex surface, and the concave hole size of the concave-convex surface is d, wherein 10nm≤d≤40nm.
9. The display backplane of claim 2, wherein, The plastic part comprises a positioning part, the positioning part is arranged at at least two corners of the bottom plate, and at least part of the side of the positioning part in the containing cavity is lower than the side of the bottom plate in the containing cavity.
10. A display module, characterized by The display backboard comprises the display backboard according to any one of claims 1 to 9.