Perovskite solar cell
By incorporating multiple protective structures into perovskite solar cells, including an edge sealing layer, an encapsulating film, and an encapsulation layer, the problem of chemical reactions caused by moisture penetration is solved, thus extending the lifespan of the cells.
Patent Information
- Application Number
- CN202522253636.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-24
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-10-24
AI Technical Summary
Existing perovskite solar cell encapsulation processes cannot effectively prevent moisture penetration, leading to chemical reactions in the perovskite layer and affecting cell performance and lifespan.
It adopts a multi-protection structure, including the coordinated operation of an edge sealing layer, an encapsulating film, a first encapsulation layer, a desiccant layer, and a second encapsulation layer, to prevent moisture from corroding the battery body, absorb water vapor, and block harmful components.
It enhances the battery's resistance to water oxidation, extends the battery's working life in extreme outdoor environments, and improves the battery's lifespan.
Smart Images

Figure CN224959982U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of solar cell technology, specifically a perovskite solar cell. Background Technology
[0002] In the fabrication of thin-film solar cells, interconnection between cell units is achieved through laser or mechanical scribing, enabling high-voltage / low-current output. It is well known that the perovskite layer in perovskite solar cells is sensitive to water and oxygen. Under the influence of water and oxygen, the perovskite material, the main component of the cell, undergoes a chemical reaction, directly leading to a deterioration in solar cell performance. Therefore, to prevent water and oxygen from entering the perovskite layer, companies in the industry have conducted extensive research on cell encapsulation structures. The mainstream encapsulation process involves coating a film on a glass substrate, then bonding the front and rear glass plates together using a heat-applied encapsulating film. Simultaneously, sealant is applied to the edges of the glass plates, thus achieving a complete seal for the entire cell module.
[0003] However, current solar cell encapsulation technology has the following problems: perovskite solar cells are more susceptible to water vapor penetration than ordinary silicon cells, and their sealant layer still cannot completely isolate water vapor. With the intrusion and accumulation of water vapor or in extreme environments, the water vapor inside the cell will cause increasingly severe erosion of the perovskite. It is still impossible to guarantee that perovskite cells can continue to work outdoors for a certain number of years under this encapsulation method.
[0004] Therefore, the waterproofing issue in perovskite solar cell encapsulation urgently needs improvement. Utility Model Content
[0005] The purpose of this invention is to provide a perovskite solar cell that, through the arrangement of multiple protective structures, works synergistically to prevent moisture from corroding the cell body, thereby enhancing the cell body's resistance to water oxidation, extending the cell's lifespan, and making it work for a longer period in extreme outdoor environments; thus solving the problems of poor waterproofing effect and reduced working life of existing perovskite solar cells mentioned in the background art.
[0006] To achieve the above objectives, this utility model provides the following technical solution:
[0007] A perovskite solar cell includes a backplate, a frontplate, and a cell body disposed between the frontplate and the backplate, arranged vertically. The frontplate and the backplate are encapsulated with edge sealing layers at their peripheral edges. The cell body, the backplate, and the edge sealing layers enclose a sealed space. An encapsulating film is laid inside the sealed space to fill its internal space. The cell body includes a back electrode, a photoelectric conversion layer, and a front electrode arranged sequentially from top to bottom. The front electrode is laid on the frontplate. A first encapsulation layer, a desiccant layer, and a second encapsulation layer are disposed between the encapsulating film and the back electrode.
[0008] Preferably, the front electrode has several first grooves that penetrate its upper and lower surfaces at equal intervals along its width direction, and the bottom of the photoelectric conversion layer extends downward to the bottom of the first grooves and abuts against the top surface of the front plate.
[0009] Preferably, the photoelectric conversion layer has several second etched grooves that penetrate its upper and lower surfaces at equal intervals along its width direction, and the bottom of the back electrode extends downward to the bottom of the second etched grooves and abuts against the top surface of the front electrode.
[0010] Preferably, the back electrode has several third grooves that extend downward to the top surface of the front electrode at equal intervals along its width direction.
[0011] Preferably, the first encapsulation layer is laid on the top surface of the back electrode and the inner wall of the third scribe groove, the desiccant layer is filled in the third scribe groove and is wrapped by the first encapsulation layer, and the second encapsulation layer is laid on the top surface of the first encapsulation layer to cooperate with the first encapsulation layer to cover the desiccant layer.
[0012] Preferably, the first encapsulation layer is laid on the top surface of the back electrode and the inner wall of the third scribe groove, the desiccant layer is laid on the top surface of the first encapsulation layer, and the second encapsulation layer is laid on the top surface of the desiccant layer, which in turn covers the desiccant layer with the first encapsulation layer; the bottom of the encapsulation film is filled into the third scribe groove and adheres to the surface of the second encapsulation layer.
[0013] Preferably, the photoelectric conversion layer is one of an HTL hole transport layer, a perovskite layer, or an ETL electron transport layer; the front electrode material is fluorine-doped tin oxide (FTO), and the back electrode material is aluminum-doped zinc oxide (AZO).
[0014] Preferably, the photoelectric conversion layer is one of an HTL hole transport layer, a perovskite layer, or an ETL electron transport layer; the front electrode material is fluorine-doped tin oxide (FTO), and the back electrode material is metallic Al or metallic Ag.
[0015] Preferably, the materials of the first encapsulation layer and the second encapsulation layer are one or more of SiN, SiO2, AlN, and Al2O3.
[0016] Preferably, the desiccant layer material is one or more of MgO and CaO.
[0017] Compared with the prior art, the beneficial effects of this utility model are as follows: It features a multi-layered protective structure. First, the front and back panels are sealed by an edge sealing layer to prevent moisture from entering the enclosed space and corroding the battery body. Next, an encapsulating film covers the battery body, preventing moisture from entering and corroding the battery body due to a loose or failed edge sealing layer. Finally, the first encapsulation layer, desiccant layer, and second encapsulation layer work together to encapsulate the desiccant layer, preventing chemical reactions between the desiccant layer and the chemicals in the battery body. The desiccant layer absorbs moisture in the enclosed space, thereby enhancing the battery body's resistance to water oxidation, extending battery life, and making it work longer in extreme outdoor environments. Attached Figure Description
[0018] Figure 1 This is a schematic diagram of the structure of a perovskite solar cell according to Embodiment 1 of this utility model;
[0019] Figure 2 This is a schematic diagram of the structure of a perovskite solar cell according to Embodiment 2 of this utility model.
[0020] In the diagram: 1. Front panel; 2. Back panel; 3. Battery body; 31. Back electrode; 311. Third groove; 32. Photoelectric conversion layer; 321. Second groove; 33. Front electrode; 333. First groove; 4. Sealed space; 5. Encapsulating film; 6. First encapsulation layer; 7. Desiccant layer; 8. Second encapsulation layer; 9. Edge sealing layer. Detailed Implementation
[0021] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0022] In the description of this utility model, it should be understood that the terms "center," "longitudinal," "transverse," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," and "counterclockwise," etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the accompanying drawings and are only for the convenience of describing this utility model and simplifying the description. They do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this utility model. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined with "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this utility model, "several" or "more than" means two or more, unless otherwise explicitly specified. In this utility model, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model according to the specific circumstances.
[0023] Example 1
[0024] Please see Figure 1 A perovskite solar cell includes a backplate 2 and a frontplate 1 arranged vertically, and a cell body 3 disposed between the frontplate 1 and the backplate 2. Edge sealing layers 9 are encapsulated at the peripheral edges of the frontplate 1 and the backplate 2. The cell body 3, the backplate 2, and the edge sealing layers 9 enclose a sealed space 4, and an encapsulating film 5 fills the sealed space 4. The cell body 3 includes a back electrode 31, a photoelectric conversion layer 32, and a front electrode 33 arranged sequentially from top to bottom. The front electrode 33 is laid on the frontplate 1. A first encapsulation layer 6, a desiccant layer 7, and a second encapsulation layer 8 are disposed between the encapsulating film 5 and the back electrode 31. In this embodiment, the edge sealing layer 9 is a rubber that serves a sealing function, such as butyl rubber, which can be in the form of colloidal butyl rubber. After encapsulation, the colloidal butyl rubber is cured into a solid edge sealing layer 9. The encapsulation film 5 is made of EVA resin, POE plastic, or PVB (polyvinyl butyral). Both the front panel 1 and the rear panel are made of transparent glass.
[0025] This novel perovskite solar cell features a multi-layered protective structure. First, the front panel 1 and back panel 2 are sealed by an edge sealing layer 9 to prevent moisture from entering the sealed space 4 and corroding the cell body 3. Next, an encapsulating film 5 covers the cell body 3, preventing moisture from entering and corroding the cell body 3 if the edge sealing layer 9 is not tight or fails. Finally, the first encapsulation layer 6, the desiccant layer 7, and the second encapsulation layer 8 work together to encapsulate the desiccant layer 7, preventing chemical reactions between the desiccant layer 7 and the chemicals in the cell body 3. The desiccant layer 7 absorbs moisture in the sealed space 4, thereby enhancing the water oxidation resistance of the cell body 3, extending its lifespan, and making it work longer in extreme outdoor environments. Furthermore, the first encapsulation layer 6 and the second encapsulation layer 8 can also prevent some harmful components in the encapsulating film 5 from entering the cell body 3, further extending the cell lifespan.
[0026] The front electrode 33 has several first etched grooves 333 evenly spaced along its width direction, penetrating its upper and lower surfaces. The bottom of the photoelectric conversion layer 32 extends downward to the bottom of the first etched grooves 333 and abuts against the top surface of the front plate 1. The photoelectric conversion layer 32 has several second etched grooves 321 evenly spaced along its width direction, penetrating its upper and lower surfaces. The bottom of the back electrode 31 extends downward to the bottom of the second etched grooves 321 and abuts against the top surface of the front electrode 33. The back electrode 31 has several third etched grooves 311 evenly spaced along its width direction, penetrating downward to the top surface of the front electrode 33. Through the arrangement of the first etched grooves 333, the second etched grooves 321, and the second etched grooves 321, the battery body 3 is divided into a series-connected battery power generation unit. The positive and negative electrodes of the battery power generation units are connected through the second etched grooves 321.
[0027] The first encapsulation layer 6 is laid on the top surface of the back electrode 31 and the inner wall of the third etched groove 311. The desiccant layer 7 fills the third etched groove 311 and is wrapped by the first encapsulation layer 6. The second encapsulation layer 8 is laid on the top surface of the first encapsulation layer 6, and works with the first encapsulation layer 6 to cover the desiccant layer 7, preventing the desiccant layer 7 from reacting chemically with the chemical substances in the battery body 3 and the encapsulating film 5. In this embodiment, the materials of the first encapsulation layer 6 and the second encapsulation layer 8 are one or more of SiN, SiO2, AlN, and Al2O3; the materials of the desiccant layer 7 are one or more of MgO and CaO.
[0028] During fabrication, after the third groove 311 of the battery body 3 is etched, a first encapsulation layer 6 is deposited on the top surface of the back electrode 31 and the inner wall of the third groove 311 by vacuum deposition. Then, a desiccant layer 7 is deposited in the third groove 311 by evaporation deposition in a PVD physical vapor deposition apparatus. Subsequently, a second encapsulation layer 8, identical to the first encapsulation layer 6, is deposited on the top surface of the back electrode 31 and the desiccant layer 7 by the same vacuum deposition method, so that the desiccant layer 7 is completely covered by the first encapsulation layer 6 and the second encapsulation layer 8. The vacuum deposition method can be plasma chemical vapor deposition (PECVD), atomic layer deposition (ALD), or physical vapor deposition (PVD), with plasma chemical vapor deposition (PECVD) being preferred.
[0029] The photoelectric conversion layer 32 is one of the following: HTL hole transport layer, perovskite layer, or ETL electron transport layer. As the power generation layer of the solar cell, the photoelectric conversion layer 32 can realize the conversion of light energy and electrical energy. The front electrode 33 and the back electrode 31 are both transparent conductive oxides, which can allow light to pass through and enter the photoelectric conversion layer 32 of the battery body 3, thus realizing bi-sided power generation. The front electrode 33 is made of fluorine-doped tin oxide (FTO), and the back electrode 31 is made of aluminum-doped zinc oxide (AZO).
[0030] In this embodiment, since the desiccant layer 7 is light-absorbing, the desiccant layer 7 is only placed in the third scribe groove 311 to avoid the desiccant layer 7 affecting the light entering the battery body 3 from the back plate 2.
[0031] Example 2
[0032] Example 2 relates to a perovskite solar cell. The difference between Example 2 and Example 1 is that:
[0033] The front electrode 33 is still made of tin oxide-doped fluorine-containing FTO, but the back electrode 31 is made of metal Al or metal Ag. In this embodiment, the perovskite solar cell can only generate electricity from one side, with the front electrode 33 facing the light. Since metal Al or metal Ag is reflective, the desiccant layer 7 can be coated over a large area without considering the light incident on the back plate 2, resulting in a wider waterproof coverage area.
[0034] The first encapsulation layer 6 is laid on the top surface of the back electrode 31 and the inner wall of the third scribe groove 311. The desiccant layer 7 is laid on the top surface of the first encapsulation layer 6, and the second encapsulation layer 8 is laid on the top surface of the desiccant layer 7, which is covered by the first encapsulation layer 6. The bottom of the encapsulation film 5 is filled into the third scribe groove 311 and adheres to the surface of the second encapsulation layer 8.
[0035] In this embodiment, the coating area of the desiccant layer 7 is smaller than that of the first encapsulation layer 6 and the second encapsulation layer 8. The first encapsulation layer 6 and the second encapsulation layer 8 completely wrap the outer periphery of the desiccant layer 7 to prevent the material of the desiccant layer 7 from leaking and reacting chemically with the metal material of the back electrode 31, which would cause the back electrode 31 to be corroded.
[0036] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the present invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A perovskite solar cell comprising a backsheet (2), a frontsheet (1) and a cell body (3) housed between the frontsheet (1) and the backsheet (2) in a top-bottom arrangement, characterized in that: The front plate (1) and the back plate (2) are sealed by an edge sealing layer (9) at the peripheral edge, the battery body (3), the back plate (2) and the edge sealing layer (9) form a closed space (4), the closed space (4) is filled with an encapsulation adhesive film (5), the battery body (3) comprises a back electrode (31), a photoelectric conversion layer (32) and a front electrode (33) arranged in sequence from top to bottom, the front electrode (33) is arranged on the front plate (1), and the encapsulation adhesive film (5) is arranged between the back electrode (31) and the first encapsulation layer (6), the desiccant layer (7) and the second encapsulation layer (8).
2. The perovskite solar cell according to claim 1, characterized in that: The front electrode (33) is provided with a plurality of first notch grooves (333) penetrating the upper and lower surfaces of the front electrode (33) at equal intervals along the width direction of the front electrode (33), and the photoelectric conversion layer (32) extends downward to the bottom of the first notch groove (333) and abuts against the top surface of the front plate (1).
3. The perovskite solar cell according to claim 2, characterized in that: The photoelectric conversion layer (32) is provided with a plurality of second notch grooves (321) penetrating the upper and lower surfaces of the photoelectric conversion layer (32) at equal intervals along the width direction of the photoelectric conversion layer (32), and the back electrode (31) extends downward to the bottom of the second notch groove (321) and abuts against the top surface of the front electrode (33).
4. The perovskite solar cell according to claim 2, characterized in that: The back electrode (31) is provided with a plurality of third notch grooves (311) penetrating the top surface of the front electrode (33) at equal intervals along the width direction of the back electrode (31).
5. The perovskite solar cell according to claim 4, characterized in that: The first encapsulation layer (6) is arranged on the top surface of the back electrode (31) and the inner wall of the third notch groove (311), the desiccant layer (7) is filled in the third notch groove (311) and is wrapped by the first encapsulation layer (6), and the second encapsulation layer (8) is arranged on the top surface of the first encapsulation layer (6) and cooperates with the first encapsulation layer (6) to wrap the desiccant layer (7).
6. The perovskite solar cell according to claim 4, characterized in that: The first encapsulation layer (6) is arranged on the top surface of the back electrode (31) and the inner wall of the third notch groove (311), the desiccant layer (7) is arranged on the top surface of the first encapsulation layer (6), the second encapsulation layer (8) is arranged on the top surface of the desiccant layer (7), and the first encapsulation layer (6) cooperates to wrap the desiccant layer (7); and the bottom of the encapsulation adhesive film (5) is filled into the third notch groove (311) and is attached to the surface of the second encapsulation layer (8).
7. The perovskite solar cell according to claim 1, characterized in that: The photoelectric conversion layer (32) is one of an HTL hole transport layer, a perovskite layer or an ETL electron transport layer; the material of the front electrode (33) is FTO fluorine-doped tin oxide, and the material of the back electrode (31) is AZO aluminum-doped zinc oxide. 8.The perovskite solar cell of claim 1, characterized in that: The photoelectric conversion layer (32) is one of an HTL hole transport layer, a calcium titanate layer or an ETL electron transport layer; the material of the front electrode (33) is an FTO fluorine-doped tin oxide, and the material of the back electrode (31) adopts a metal Al or a metal Ag.