A dry powder direct coating device

By designing a powder metering extrusion assembly and a composite assembly, uniform distribution and stable conveying of powder were achieved, solving the problems of uneven feeding and fluctuations in dry coating, and improving the quality of electrode production and battery performance.

CN224976729UActive Publication Date: 2026-11-17SHENZHEN XINYUREN TECH
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522662562.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-16
Publication Date
2026-11-17
Estimated Expiration
2035-12-16

AI Technical Summary

Technical Problem

In existing dry coating technologies, manual feeding methods result in uneven powder distribution in the lateral direction and inconsistent thickness in the longitudinal direction, which cannot meet the requirements of high-speed and wide-width mass production and affects coating quality and battery performance.

Method used

A powder metering extrusion assembly is used to meter and extrude powder into a film. Combined with a composite assembly, the powder is directly coated onto the surface of the foil. This assembly includes a screw, a metering die, and a dispersing assembly to ensure uniform distribution and stable delivery of the powder.

Benefits of technology

It improves the yield rate of electrode production and battery life, solves the problems of uneven feeding and feeding fluctuation, and adapts to the needs of high-speed and wide-range mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224976729U_ABST
    Figure CN224976729U_ABST
Patent Text Reader

Abstract

This utility model relates to the field of battery electrode coating technology, and discloses a dry powder direct coating device, including a powder metering extrusion component and a composite component. The powder metering extrusion component is disposed above or to the side of the composite component. The powder metering extrusion component is used for metering powder and extruding the metered powder into a film, which is then transferred to the composite component. The composite component then laminates the film-formed powder onto the surface of a foil. This solution uses a powder metering extrusion component to meter the powder before extruding it into a film. This way, after the powder is transferred to the composite component, it can be directly laminated onto the foil surface without additional thinning treatment, solving the problems of uneven feeding and feeding fluctuations, improving the yield of electrode production and the service life of the battery.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of battery electrode coating technology, and in particular to a multi-layer die coating mechanism. Background Technology

[0002] In the mass production process of dry coating, the uniformity of the coating (both transverse and longitudinal) directly determines the quality stability of the foil coating, thus affecting the performance of downstream products such as batteries. Currently, the dry coating feeding methods on the market have significant technical defects: 1. Outdated feeding method: Most of the time, the powder is added between the two rollers manually. Manual operation makes it difficult to ensure that the powder is evenly distributed in the lateral direction, which can easily lead to local powder accumulation or gaps, resulting in deviations in the lateral thickness of the coating. At the same time, the manual feeding speed cannot be kept constant, which will cause frequent fluctuations in the longitudinal material pressure between the two rollers, ultimately resulting in inconsistent longitudinal thickness of the coating. 2. Poor mass production adaptability: The instability of the above-mentioned manual feeding method is further amplified, which cannot meet the needs of high-speed and wide-width mass production. When running at high speed, unevenness in the lateral direction and changes in the longitudinal material pressure will cause the film quality of the roller to drop sharply, resulting in large-area thickness deviation problems, which seriously restricts the mass production efficiency and product yield of the dry coating process. Existing coating mechanisms lack integrated quantitative metering and uniform feeding design, which cannot solve the problem of lateral and longitudinal thickness fluctuations caused by manual feeding, and are difficult to adapt to high-speed and wide-width mass production scenarios.

[0003] Chinese patent CN202411820155.X discloses a method for preparing dry electrode sheets by spray coating, including the following steps: Step S1: Dry powder is poured into two feeding mechanisms; Step S2: Current collector is released vertically by an unwinding mechanism; Step S3: The first ends of two dry self-supporting films symmetrically arranged along the longitudinal direction of the current collector are cut by a preliminary composite mechanism; Step S4: The two laminated dry self-supporting films and current collector are rolled together at a rolling mechanism to form an electrode sheet; Step S5: The electrode sheet is guided into a single-section drying oven by a guide roller for drying. By cutting off the first end of the dry self-supporting film with a first-end cutter, the first end of the dry self-supporting film is flush when it is rolled together with the current collector. This ensures that the first end of the rolled electrode sheet is also flush, eliminating the need to cut the first end of the electrode sheet when it is put into use later, thus avoiding waste of the current collector. However, this method lacks quantitative processing during material feeding and needs improvement.

[0004] This invention overcomes the shortcomings of the prior art and provides a dry powder direct coating device that can quantitatively process powder before extruding it into a film, thus solving the problems of uneven lateral feeding and longitudinal material pressure fluctuation. Utility Model Content

[0005] The main purpose of this utility model is to provide a dry powder direct coating device, including a powder metering extrusion component and a composite component. The powder metering extrusion component is located above or to the side of the composite component. The powder metering extrusion component is used for metering powder and extruding the metered powder into a film and transferring it to the composite component. The composite component then laminates the film-formed powder onto the surface of a foil.

[0006] Optionally, the powder metering extrusion assembly includes a metering die, a screw, and a screw motor. The screw motor is connected to the screw via a drive, and the metering die is connected to the screw. The screw motor drives the screw to push the powder out of the metering die.

[0007] Optionally, the powder metering extrusion assembly includes a feed trough, a metering die, and a dispersing assembly. The outlet of the feed trough is connected to the metering die via a conveying pipe. The dispersing assembly is located in the conveying pipe and is used to disperse flocculent powder into granular powder.

[0008] Optionally, the metering die head includes an upper die and a lower die. The upper die is provided with a funnel-shaped material trough, and a first metering roller is provided at the bottom outlet of the material trough. The first metering roller is connected to a metering roller motor through a coupling.

[0009] Optionally, the metering die head includes an upper die and a lower die, with a gap between the upper die and the lower die. The lower die is provided with a semi-circular flow channel, the middle of which is concave downwards. The semi-circular flow channel communicates with the gap. A first metering roller is provided on the outlet side of the semi-circular flow channel. The first metering roller is connected to a metering roller motor via a coupling. A shim is provided between the upper die and the lower die, and the distance between the first metering roller and the upper die or the lower die is adjusted by the shim.

[0010] Optionally, the upper mold is provided with a plurality of evenly distributed flow limiting blocks in the transverse direction. The plurality of flow limiting blocks are individually controlled by a flow regulator, and the gap between the flow limiting blocks and the lower mold is adjusted by the flow regulator.

[0011] Optionally, the first metering roller can be located on the upper or lower side of the flow limiting block, the first metering roller can be located on the upper or lower mold, or between the upper and lower molds, and the number of the first metering rollers can be multiple.

[0012] Optionally, the first metering roller can be a smooth roller, a metering roller with grooves on its surface, or a uniform roller with forward and reverse spirals on its surface.

[0013] Optionally, the composite component includes a composite roller, and two composite rollers form a composite roller group; The powder metering extrusion assembly conveys powder to the composite roller, and the powder film is directly transferred to the front and back of the foil through the composite roller; Alternatively, the powder metering extrusion assembly delivers powder to a composite roller group, which transfers the powder film onto the front side of the foil, and then another composite roller group transfers the powder film to the back side of the foil.

[0014] Optionally, the composite component further includes a transfer roller located between the powder metering extrusion component and the composite roller. The powder metering extrusion component delivers powder to the transfer roller, and the powder film is transferred to the composite roller or composite roller group via the transfer roller. The number of transfer rollers between the powder metering extrusion component and the composite roller is one or more.

[0015] Compared with the prior art, the present invention has the following beneficial effects: The dry powder direct coating device provided by this utility model quantitatively processes the powder through a powder quantitative extrusion component and then extrudes it into a film. In this way, after the powder is transferred to the composite component, it can be directly laminated to the foil surface without additional thinning treatment, which solves the problems of uneven feeding and feeding fluctuation, and improves the yield of electrode production and the service life of the battery. Attached Figure Description

[0016] One or more embodiments are illustrated by way of example with reference to the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements having the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.

[0017] Figure 1 This is a schematic diagram of the first embodiment of the dry powder direct coating device of this utility model.

[0018] Figure 2 This is a schematic diagram of a second embodiment of the dry powder direct coating device of this utility model.

[0019] Figure 3 This is a schematic diagram of the first metering die head in an embodiment of the dry powder direct coating device of this utility model.

[0020] Figure 4 This is a schematic diagram of the second type of metering die in an embodiment of the dry powder direct coating device of this utility model.

[0021] Figure 5 This is an exploded view of the second metering die head in an embodiment of the dry powder direct coating device of this utility model.

[0022] Figure 6 This is a top view of the second metering die head in an embodiment of the dry powder direct coating device of this utility model.

[0023] Figure 7 This is a cross-sectional view of the second metering die in an embodiment of the dry powder direct coating device of this utility model. Figure 1 .

[0024] Figure 8 This is a cross-sectional view of the second metering die in an embodiment of the dry powder direct coating device of this utility model. Figure 2 .

[0025] Figure 9 This is a schematic diagram showing the various uniform metering rollers of the metering die head in an embodiment of the dry powder direct coating device of this utility model.

[0026] Figure 10 This is a schematic diagram of various uniform metering rollers of the metering die head in an embodiment of the dry powder direct coating device of this utility model.

[0027] Figure 11 This is a schematic diagram of the second type of powder metering extrusion component in the embodiment of the dry powder direct coating device of this utility model.

[0028] Figure 12 This is a top view of the second type of powder metering extrusion component in the embodiment of the dry powder direct coating device of this utility model.

[0029] Figure 13 This is a schematic diagram of the third type of powder quantitative extrusion component in the embodiment of the dry powder direct coating device of this utility model.

[0030] Figure 14 This is a schematic diagram of the feeding of the powder quantitative extrusion component in the third embodiment of the dry powder direct coating device of this utility model.

[0031] Figure 15 This is a schematic diagram of the fourth type of powder quantitative extrusion component in the embodiment of the dry powder direct coating device of this utility model.

[0032] Figure 16 This is a schematic diagram of the scraper assembly in an embodiment of the dry powder direct coating device of this utility model.

[0033] Figure 17 This is a side view of the scraper assembly in an embodiment of the dry powder direct coating device of this utility model.

[0034] Figure 18 This is a schematic diagram of the pressure roller assembly in an embodiment of the dry powder direct coating device of this utility model.

[0035] Figure 19 The diagram shows two composite components of the dry powder direct coating device of this utility model.

[0036] Figure 20 This is an embodiment of the composite roller configuration of the dry powder direct coating device of this utility model.

[0037] Figure 21 This invention relates to an embodiment of a dry powder direct coating device, which describes a configuration of a composite roller and a transfer roller.

[0038] Figure 22 This is another embodiment of the dry powder direct coating device of this utility model, which shows the arrangement of the composite roller and the transfer roller.

[0039] Figure label: 1-Powder metering extrusion assembly; 10-Metering die head; 101-Upper die; 102-Lower die; 103-Material trough; 104-Metering roller; 105-Coupling; 106-Metering roller motor; 107-Semi-arc flow channel; 108-Gasket; 109-Flow limiting block; 110-Flow regulator; 11-Screw; 12-Screw motor; 13-Feed trough; 14-Dispersion assembly; 15-Material conveying pipe; 20-Metering roller; 201-Boss; 202-Fixed seat; 203-Lifting motor; 204-Lifting coupling; 2 05-Screw; 206-Guide rail; 207-Rotating motor; 208-Conveying structure; 2081-Metering tank; 209-Rotating roller; 210-Linear motor; 2-Composite component; 21-Composite roller; 22-Transfer roller; 23-Drive motor; 24-Reducer; 25-Rotary joint; 26-Bearing seat; 3-Foil material; 4-Scraper assembly; 41-Clamping plate; 42-Scraper; 43-First slide table; 44-Support frame; 45-Push cylinder; 46-Baffle; 5-Pressure roller assembly; 51-Pressure roller; 52-Second slide table. Detailed Implementation

[0040] To facilitate understanding of this utility model, a more detailed description is provided below with reference to the accompanying drawings and specific embodiments. It should be noted that when an element is described as being "fixed to" another element, it can be directly on the other element, or one or more intermediate elements may exist between them. When an element is described as being "connected to" another element, it can be directly connected to the other element, or one or more intermediate elements may exist between them. The terms "vertical," "horizontal," "left," "right," "inner," "outer," and similar expressions used in this specification are for illustrative purposes only. In the description of this utility model, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating relative importance or implying the number of indicated technical features. Thus, unless otherwise stated, features defined as "first" or "second" may explicitly or implicitly include one or more of that feature; "multiple" means two or more. The term "comprising" and any variations thereof mean non-exclusive inclusion, where one or more other features, integers, steps, operations, units, components, and / or combinations thereof may be present or added.

[0041] Furthermore, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly, for example, as a fixed connection, a detachable connection, or an integral connection; as a mechanical connection or an electrical connection; as a direct connection or an indirect connection through an intermediate medium, or as a connection within two components. All technical and scientific terms used in this specification have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used in this specification is for the purpose of describing particular embodiments only and is not intended to limit the scope of the invention. The term "and / or" as used in this specification includes any and all combinations of one or more of the associated listed items.

[0042] Furthermore, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0043] This utility model embodiment is applicable to the production and manufacturing of battery electrode sheets in the field of new energy battery production, and is used to achieve electrode sheets obtained by direct dry powder coating on the surface of foil. Specifically, it includes the following steps: S100, Quantitative processing of powder materials.

[0044] S200: The quantitatively processed powder is extruded into a film and transferred to the composite component.

[0045] S300: Powder film is laminated onto the surface of foil through composite components.

[0046] Steps S100 and S200 are processed by the same powder metering extrusion assembly. Specifically, the powder metering extrusion assembly can achieve quantitative metering through structures such as a screw, metering die, and metering groove. The powder after metering extrusion does not require additional thinning treatment, resulting in more uniform transfer and solving the technical problems of uneven feeding and feeding fluctuations.

[0047] In addition, before step S100, there is a dispersion step S101: dispersing the flocculent powder into granular powder. The dispersion step can ensure that the powder is granular when it is quantified in the powder metering extrusion component, improve metering accuracy, make the subsequent powder film formation more uniform, and improve the electrical performance of the electrode.

[0048] like Figure 1-21 The diagram shown is a schematic representation of an embodiment of the dry powder direct coating device provided by this utility model.

[0049] Please refer to Figure 1-21This embodiment is used to implement the above method embodiment, including a powder metering extrusion component 1 and a composite component 2. The powder metering extrusion component 1 is disposed above or on the side of the composite component 2. The powder metering extrusion component 1 is used for powder metering and extruding the metered powder into a film and transferring it to the composite component 2. The composite component 2 composites the film-formed powder onto the surface of the foil 3.

[0050] In one embodiment, such as Figure 1 As shown, the powder metering extrusion assembly 1 includes a metering die 10, a screw 11 and a screw motor 12. The screw motor 12 is connected to the screw 11 in a transmission connection, and the metering die 10 is connected to the screw 11. The screw motor 12 drives the screw 11 to push the powder out of the metering die 10.

[0051] The screw 11 is a multi-stage variable pitch screw, integrating mixing, fiberization, and metering functions. It can pre-treat the powder (mixing homogenization and fiberization) while simultaneously achieving quantitative conveying. By adjusting the screw 11 speed through the screw motor 12, the powder conveying speed can be precisely controlled, thereby adjusting the longitudinal forming speed of the powder coating. The metering die 10 is connected to the discharge end of the screw 11, employing a structure that combines screw 11 pressurization with metering die 10. After being pressurized by the screw 11, the powder is uniformly extruded through the metering die 10, ensuring that the powder is evenly distributed laterally on the surface of the transfer roller 22 or composite roller 21 of the subsequent composite component 2.

[0052] In another embodiment, such as Figure 2 As shown, the powder metering extrusion assembly includes a feed trough 13, a metering die 10, and a dispersing assembly 14. The outlet of the feed trough 13 is connected to the metering die 10 via a conveying pipe 15. The dispersing assembly 14 is located in the conveying pipe 15 and is used to disperse flocculent powder into granular powder. The dispersing assembly 14 ensures that the powder is granular during metering in the powder metering extrusion assembly, improving metering accuracy, making subsequent powder film formation more uniform, and enhancing the electrical performance of the electrode.

[0053] like Figure 2 As shown, the dispersion component 14 can specifically be a silo wall vibrator, with multiple silo wall vibrators evenly distributed on the outside of the conveying pipe 15 and in contact with it. The vibration generated by the silo wall vibrator disperses the flocculent powder into granular powder. Alternatively, the dispersion component 40 can be an ultrasonic vibrator, also with multiple ultrasonic vibrators evenly distributed on the outside of the conveying pipe 15 and in contact with it. The high-frequency vibration generated by the ultrasonic waves impacts the flocculent powder, dispersing it into granular powder.

[0054] The feed trough 13 has a funnel-shaped structure, with the upper part being the inlet and the lower part being the outlet. The diameter of the inlet is larger than that of the outlet, and the outlet is connected to the conveying pipe 15, facilitating the entry of powder into the feed trough 13 from above. Under the action of gravity, the powder gathers at the lower end of the feed trough 13 and is then output downwards through the conveying pipe 15. During the conveying process in the conveying pipe 15, the powder is dispersed by vibration through the dispersing component 14.

[0055] The dispersion component 14 transforms flocculent powder into granular powder, avoiding metering errors caused by powder agglomeration and ensuring accurate feeding by the metering component, thus improving the consistency of electrode thickness. After the granular powder forms a film, a richer and more uniform pore structure is created inside the electrode, significantly increasing the electrode porosity and providing a smoother path for ion migration, effectively improving the electrical performance of the electrode (such as charge-discharge efficiency and cycle stability). The dispersion component 14 can be implemented using ultrasonic dispersion, airflow dispersion, or stirring dispersion, and its simple structure and easy installation make it compatible with existing dry coating production lines, resulting in low modification costs and high practicality.

[0056] The metering die 10 has two structural forms, the first form being as follows: Figure 3 As shown, the metering die 10 includes an upper die 101 and a lower die 102. The upper die 101 is provided with a funnel-shaped material trough 103, and a uniform metering roller 104 is provided at the bottom outlet of the material trough 103. The uniform metering roller 104 is connected to the metering roller motor 106 via a coupling 105. This metering die 10 has a relatively simple structure. The lateral uniformity of the powder is adjusted by adjusting the metering die 10, and the discharge speed is adjusted by adjusting the rotation speed of the uniform metering roller 104. The distance between the metering die 10 and the composite component 2 can be adjusted by raising and lowering the motor.

[0057] The second form is as follows Figure 4-8 As shown, the metering die 10 includes an upper die 101 and a lower die 102, with a gap between them. The lower die 102 has a semi-circular flow channel 107, which is concave in the middle and communicates with the gap. Specifically, the semi-circular flow channel 107 has a coat hanger-like structure. In other embodiments, the semi-circular flow channel 107 can be replaced with a direct current channel. Figure 7 As shown, since the middle part of the metering die head 10 is connected to the powder quantitative extrusion component 1, the powder diffuses from the middle of the semi-arc flow channel 107 to both sides. The pressure in the middle is greater. Designing the flow channel as semi-arc can balance the pressure of the powder in the lateral direction, so that the pressure of the powder in the lateral direction is equal and the output is more uniform.

[0058] A uniform metering roller 104 is provided on the outlet side of the semi-arc flow channel 107. The uniform metering roller 104 is connected to the metering roller motor 106 through a coupling 105. The uniform metering roller 104 is located at the outlet of the metering die head 10 and forms an adjustable gap with the metering die head 10. The film thickness is precisely controlled by adjusting this gap.

[0059] A shim 108 is provided between the upper die 101 and the lower die 102. The shim 108 is used to adjust the gap between the uniform metering roller 104 and the upper die 101 or the lower die 102. Replaceable shims 108 are provided on both sides of the metering die head 10. By adjusting the thickness of the shim 108, the output thickness of the metering die head 10 can be initially adjusted to adapt to different coating thickness requirements.

[0060] In addition, the upper die 101 is provided with multiple evenly distributed flow-limiting blocks 109 along the transverse direction. These flow-limiting blocks 109 are individually controlled by a flow regulator 110. The flow regulator 110 adjusts the gap between the flow-limiting blocks 109 and the lower die 102, thereby adjusting the thickness of the extruded material. The multiple flow-limiting blocks 109 are positioned in front of the uniform metering roller 104, allowing for fine-tuning of the transverse thickness of the powder extruded from the metering die 10, further ensuring the transverse uniformity of the coating. The flow regulator 110 can be a flow adjustment handle or a motor.

[0061] Specifically, such as Figure 9 As shown, the uniform metering roller 104 can be located on the upper or lower side of the flow limiting block 109, that is, on the rear or front side of the feeding direction. The uniform metering roller 104 can also be located on the upper mold 101 or the lower mold 102, or between the upper mold 101 and the lower mold 102. In addition, the number of uniform metering rollers 104 can also be multiple.

[0062] The leveling and metering roller 104 can be a smooth roller (such as...) Figure 10 a) of the metering rollers, and a metering roller with grooves on its surface (such as the a roller in the middle). Figure 10 (b roller in the middle) or a uniform roller with positive and negative spirals on its surface (such as...) Figure 10 The C-roller is designed to accommodate different powder properties. The uniform roller with forward and reverse spirals on its surface can evenly disperse the powder, thus solving the problem of uneven dispersion of the powder film.

[0063] In another embodiment, the powder metering extrusion assembly 1 can also be as follows: Figure 11-18 The metering extrusion structure shown includes a metering roller 20, a conveying structure 208, and a composite component 2. The conveying structure 208 is provided with a metering groove 2081. The metering roller 20 is located above the conveying structure 208. The metering roller 20 and the metering groove 2081 form a metering opening. The conveying structure 208 is a strip structure or a roller structure with a predetermined inclined angle. The powder is formed into a powder film through the metering opening. The inclined end of the conveying structure 208 is provided with a composite component 2, which is used to laminate the powder film onto the surface of the foil.

[0064] The powder is formed by the metering roller 20 and the metering groove 2081 into a metering orifice and extruded into a powder film of a predetermined width and thickness. When the conveying structure 208 is a strip structure with a predetermined angle of inclination, the powder can move downward along the inclined conveying structure 208 under its own gravity. After being formed into a film through the metering orifice, it continues to move downward to the composite component 2. The composite component 2 is then used to bond the powder to the surface of the foil to obtain an electrode sheet.

[0065] The metering roller 20 has a boss 201 on its surface that matches the width of the metering groove 2081. The boss 201 fits into the metering groove 2081, ensuring that the two sides of the powder film are neat. The thickness of the powder film can be adjusted by changing the height of the metering roller 20 to adjust the distance between it and the bottom of the metering groove 2081. The thickness of the powder film can also be adjusted by changing the outer diameter of the metering roller 20 or the height of the boss 201 to adjust the distance between it and the bottom of the metering groove 2081.

[0066] The metering roller 20 is connected to a lifting motor 203 at both ends via a fixed base 202. The lifting motor 203 is connected to the fixed base 202 via a lifting coupling 204 and a lead screw 205. The fixed base 202 is matched and connected to the guide rail 206. The lifting motor 203 drives the metering roller 20 to move up and down. The height of the metering roller 20 is adjusted by the lifting motor 203, thereby adjusting the distance between the metering roller 20 and the metering groove 2081. The metering roller 20 is connected to a rotary motor 207, which drives the metering roller 20 to rotate. The rotary motor 207 drives the metering roller 20 to rotate to accommodate the movement of powder through the metering port, preventing powder from accumulating and clogging at the metering port.

[0067] like Figure 13 As shown, the conveying structure 208 is a roller structure, that is, the metering trough 2081 is located on the surface of the rotating roller 209. The rotating roller 209 is connected to the linear motor 210 through a reducer. The two ends of the rotating roller 209 are supported and connected by bearing seats. The linear motor 210 drives the rotating roller 209 to rotate, and the rotation of the rotating roller 209 drives the powder to move. Figure 14 As shown, at this time, the powder is conveyed to the surface of the rotating roller 209 through the powder metering extrusion assembly 1, and then metered and extruded into a film through the metering groove 2081 on the surface of the rotating roller 209.

[0068] Composite component 2 includes a composite roller 21, a transfer roller 22, a drive motor 23, a rotary joint 25, and a reducer 24. The two ends of the transfer roller 22 are fixed by bearing seats 26, and the drive motor 23 and the transfer roller 22 are connected sequentially via the rotary joint 25 and the reducer 24. Figure 18 As shown, a transitional composite roller 21 is also provided between the transfer roller 22 and the foil 3. The composite roller 21 and the transfer roller 22 can have the same structure, and the different names are only used for differentiation.

[0069] like Figure 15 As shown, there are multiple transfer rollers 22, with a doctor blade assembly 4 and a pressure roller assembly 5 between adjacent transfer rollers 22. The doctor blade assembly 4 is used to change the transfer direction of the powder film, ensuring that the powder film is transferred and moved in a predetermined direction. The pressure roller assembly 5 is used to press the powder film onto the surface of the transfer roller 22. Here, the transfer roller 22 can be replaced by a composite roller 21.

[0070] Specifically, such as Figure 16-17 As shown, the scraper assembly 4 includes a clamping plate 41, a scraper 42, and a first slide 43. The clamping plate 41 clamps both sides of the scraper 42, and both ends of the clamping plate 41 are hinged to the first slide 43. The first slide 43 is provided with a support frame 44, which is connected to a push cylinder 45. The extension end of the push cylinder 45 is hinged to the clamping plate 41, and a baffle 46 is provided in the middle of the clamping plate 41. The clamping plate 41 clamps both sides of the scraper 42 to fix the scraper 42. The height of the scraper 42 is adjusted by the first slide 43, and the angle of the scraper 42 is adjusted by pushing the clamping plate 41 to rotate by the push cylinder 45.

[0071] Specifically, such as Figure 18 As shown, the pressure roller assembly 5 includes a pressure roller 51 and a second slide table 52. The two ends of the pressure roller 51 are hinged to the second slide table 52 via bearings. The distance between the pressure roller 51 and the transfer roller 22 is adjusted by the second slide table 52.

[0072] In addition, the surface materials of adjacent transfer rollers 22 are different, or the coatings on the surfaces of adjacent transfer rollers 22 are different, or the surface roughness of adjacent transfer rollers 22 is different. The direction of powder film movement during transfer can be changed by changing the surface material, coating, or roughness of the transfer rollers 22.

[0073] In one embodiment, the composite component 2 includes a composite roller 21, and two composite rollers 21 form a composite roller group. For example... Figure 1 As shown, the powder metering extrusion assembly 1 conveys powder to the composite roller 21, and the composite roller 21 directly laminates the powder film to the front and back of the foil 3.

[0074] Or such as Figure 20 As shown, the powder metering extrusion assembly 1 conveys powder to the composite roller group, which transfers the powder film to the front side of the foil through the composite roller group, and then transfers the powder film to the back side of the foil through another composite roller group.

[0075] In another embodiment, such as Figure 21 As shown, the composite assembly 2 also includes a transfer roller 22, which is located between the powder metering extrusion assembly 1 and the composite roller 21. The powder metering extrusion assembly conveys powder to the transfer roller, which then transfers the powder film to the composite roller 21 or the composite roller assembly. The composite roller 21 and the transfer roller 22 can have the same structure; the different names are only for differentiation. Figure 22As shown, the number of transfer rollers 22 between the powder metering extrusion assembly 1 and the composite roller 21 can be one or more. This design of the composite roller 21 and transfer roller 22 is suitable for scenarios requiring precise control of coating thickness reduction.

[0076] This embodiment solves the problem of uniform feeding by replacing manual feeding with screw pressurization and metering die extrusion structure, achieving uniform lateral distribution of powder; the stable conveying and adjustable speed design of the multi-stage variable pitch screw avoids longitudinal material pressure fluctuations, fundamentally solving the problem of lateral and longitudinal thickness variation of coating. This embodiment is suitable for high-speed, wide-width mass production. Its integrated mixing, fiberization, and metering design, combined with precise thickness adjustment structures (such as gaskets, metering roller gaps, and flow-limiting blocks), maintains stable coating thickness even at high speeds, meeting the efficiency and quality requirements of wide-width mass production. This embodiment offers flexible functionality, allowing for the selection of multiple transfer schemes based on coating thickness requirements (whether thinning is necessary). Furthermore, the metering rollers are replaceable, adapting to powders with different properties, making it widely applicable.

[0077] In summary, the embodiments provided by this utility model quantitatively process the powder using the same powder quantitative extrusion component before extruding it into a film. This allows the powder to be directly transferred to the foil surface without additional thinning treatment after being transferred to the composite component, shortening the process path, reducing equipment complexity and production energy consumption, and improving mass production efficiency. Quantitatively processing the powder before extruding it into a film solves the problems of uneven feeding and feeding fluctuations, improving the yield rate of electrode production and the lifespan of the battery.

[0078] The above embodiments are only used to illustrate the technical solutions of this utility model, and are not intended to limit it. Under the concept of this utility model, the technical features of the above embodiments or different embodiments can also be combined, the steps can be implemented in any order, and there are many other variations of different aspects of this utility model as described above. For the sake of brevity, they are not provided in detail. Although this utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. These modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this utility model.

Claims

1. A dry powder direct coating apparatus, characterized by, The device includes a powder metering extrusion assembly and a composite assembly. The powder metering extrusion assembly is located above or to the side of the composite assembly. The powder metering extrusion assembly is used for metering powder and extruding the metered powder into a film, which is then transferred to the composite assembly. The composite assembly laminates the film-formed powder onto the surface of a foil. The powder metering extrusion assembly includes a metering die, a screw, and a screw motor. The screw motor is driven by the screw, and the metering die is connected to the screw. The screw motor drives the screw to push the powder out of the metering die.

2. The dry powder direct coating apparatus of claim 1, wherein, The powder metering extrusion assembly includes a feed trough, a metering die, and a dispersing assembly. The outlet of the feed trough is connected to the metering die via a conveying pipe. The dispersing assembly is located in the conveying pipe and is used to disperse flocculent powder into granular powder.

3. The dry powder direct coating apparatus according to claim 2, characterized in that, The metering die head includes an upper die and a lower die. The upper die is provided with a funnel-shaped material trough. A first metering roller is provided at the bottom outlet of the material trough. The first metering roller is connected to a metering roller motor through a coupling.

4. The dry powder direct coating apparatus according to claim 2, characterized in that, The metering die head includes an upper die and a lower die, with a gap between the upper die and the lower die. The lower die is provided with a semi-circular flow channel, the middle of which is concave downwards. The semi-circular flow channel communicates with the gap. A first metering roller is provided on the outlet side of the semi-circular flow channel. The first metering roller is connected to a metering roller motor via a coupling. A shim is provided between the upper die and the lower die, and the gap between the first metering roller and the upper die or the lower die is adjusted by the shim.

5. The dry powder direct coating apparatus according to claim 4, characterized in that, The upper mold is provided with multiple evenly distributed flow limiting blocks along the lateral direction. The multiple flow limiting blocks are individually controlled by a flow regulator, which adjusts the gap between the flow limiting blocks and the lower mold.

6. The dry powder direct coating apparatus according to claim 5, characterized in that, The first metering roller can be located on the upper or lower side of the flow limiting block. The first metering roller can be located on the upper or lower mold, or between the upper and lower molds. The number of the first metering rollers can be multiple.

7. The dry powder direct coating apparatus according to claim 4, characterized in that, The first metering roller can be a smooth roller, a metering roller with grooves on its surface, or a uniform roller with positive and negative spirals on its surface.

8. The dry powder direct coating apparatus according to claim 1, characterized in that, The composite component includes a composite roller, and two composite rollers form a composite roller group; The powder metering extrusion assembly conveys powder to the composite roller, and the composite roller directly laminates the powder film to the front and back of the foil. Alternatively, the powder metering extrusion assembly conveys the powder to a composite roller group, which transfers the powder film to the front side of the foil, and then another composite roller group transfers the powder film to the back side of the foil.

9. The dry powder direct coating apparatus according to claim 8, characterized in that, The composite component also includes a transfer roller, which is located between the powder metering extrusion component and the composite roller. The powder metering extrusion component conveys powder to the transfer roller, and the powder film is transferred to the composite roller or composite roller group through the transfer roller. The number of transfer rollers between the powder metering extrusion assembly and the composite roller is one or more.

Citation Information

Patent Citations

  • Method for preparing dry-method electrode plate through glue spraying and coating

    CN119517929A