Methods for the surface treatment of glass spheres

The surface treatment of glass spheres addresses the weak bonding issue by roughening their surfaces, improving adhesion to resin and mechanical performance in low-density molding compounds for vehicle body parts, enabling lighter, more fuel-efficient vehicles.

DE102016107027B4Active Publication Date: 2024-11-07FORD GLOBAL TECH LLC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE102016107027
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-04-27
Filing Date
2016-04-15
Publication Date
2024-11-07
Estimated Expiration
2036-04-15

AI Technical Summary

Technical Problem

The low interfacial property between glass beads and resin in low-density molding compounds results in weak bonding, reducing the mechanical performance of vehicle body parts.

Method used

A surface treatment process for glass spheres that roughens their surfaces to enhance adhesion to resin, involving methods such as centrifugal and turning processing vessels or air plasma treatment, achieving a surface roughness of 0.01% to 0.1% of the sphere's diameter.

Benefits of technology

The treated glass spheres exhibit improved chemical bonding with resin, enhancing the mechanical properties of low-density molding layers, suitable for use in automobile body parts, contributing to lighter vehicles with better fuel efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Method for treating the outer surfaces of several glass spheres, comprising: Pouring several glass spheres into a processing vessel with a roughened lining; and Moving the processing vessel so that the multiple glass beads move against the roughened lining, thereby roughening the outer surfaces.
Need to check novelty before this filing date? Find Prior Art

Description

Technical area

[0001] This document generally relates to a surface treatment process for glass bubbles, glass bubbles produced by this process, and a low-density sheet molding compound formed using glass bubbles produced by this process. background

[0002] The government's Corporate Average Fuel Economy (CAFE) target of 4.32 l / 100 km (liters per 100 kilometers, 54.5 mpg) by 2025 has forced automakers to accelerate the use of lightweight materials in vehicles. As a result, it has been proposed to use low-density molding compound layers in the construction of vehicle body parts such as the hood instead of standard-density molding compound layers. Specifically, low-density molding compound layers have a density of 1.2 g / cm 3, while standard density molding compound layers have a density of 1.9 g / cm 3 The significant weight reduction in the formulation of low-density molding compound layers compared to standard-density molding compound layers is achieved by replacing the CaCO3 component of the standard molding compound layers with low-density glass spheres.

[0003] One of the technical challenges to be overcome in this endeavor is the poor interfacial properties between glass beads and resin. In particular, the smooth / hard surface of the glass beads results in weak bonding of the beads to the resin matrix, which tends to significantly reduce the overall mechanical performance of a low-density molding compound layer.

[0004] This document concerns a new and improved surface treatment process for glass beads which roughens the surface of the glass beads to enable better adhesion to the resin. Brief description

[0005] In accordance with the purposes and advantages described herein, a method for treating the outer surfaces of a plurality of glass spheres is provided. This method can be generally described as comprising the steps of: (a) filling a plurality of glass spheres into a processing vessel having a roughened lining, and (b) displacing the processing vessel such that the plurality of glass spheres move against the roughened lining, thereby roughening the outer surfaces.

[0006] In one possible embodiment, the method includes spinning and rotating the processing vessel. In particular, the method may include spinning the processing vessel at a speed between 60 rpm and 600 rpm and rotating the processing vessel at a speed between 60 rpm and 600 rpm, wherein the spinning and rotating are provided along two different axes. The method also includes reversing the spinning and rotating directions of the processing vessel. In one possible embodiment, the processing vessel has a spherical shape. In another possible embodiment, the processing vessel has a cylindrical shape.

[0007] The method may further include providing the plurality of glass spheres with an outer surface roughness of 0.01% to 0.1% of the diameter of the plurality of glass spheres. In one possible embodiment, the method may further include subjecting the plurality of glass spheres to an air plasma treatment. This may be accomplished by moving the plurality of glass spheres through an air plasma stream using a vibrating conveyor belt, moving the plurality of glass spheres through an air plasma stream on a chute, or dropping the plurality of glass spheres through an air plasma stream. In each of these embodiments, the method includes exposing the plurality of glass spheres to an air plasma temperature between 23°C and 500°C.

[0008] In one possible embodiment, the air plasma treatment is added after the treatment of the multiple glass spheres in the processing vessel. In one possible embodiment, the glass spheres are only mechanically processed in the processing vessel. In another possible embodiment, the glass spheres receive only an air plasma treatment.

[0009] According to an additional aspect, a method for treating the outer surfaces of a plurality of glass spheres is provided, comprising the step of subjecting the plurality of glass spheres to an air plasma treatment such that an outer surface roughness of 0.01% to 0.1% of the diameter of the plurality of glass spheres is provided.

[0010] According to another aspect, a glass sphere is provided, said glass sphere comprising a hollow glass body with an outer surface having a diameter between 16 µm and 25 µm and a surface roughness of 0.01% to 0.1% of said diameter. Further, a low-density molding compound layer is provided, comprising a resin and a plurality of glass spheres as set forth and just described.

[0011] In the following description, several preferred embodiments of the process and the glass sphere product of the process are illustrated and described. It should be understood that the process and product may have other, different embodiments and their numerous details may be modified in various, obvious aspects without departing from the process and product as set forth and described in the following claims. Therefore, the drawings and descriptions should be considered only as illustrative and not restrictive. Short description of the drawing figures

[0012] The accompanying drawings, which form part of the description, illustrate several aspects of the process and product of the process and, together with the description, serve to explain certain of its principles. In the drawings: is Fig. 1 is a schematic diagram showing a glass sphere with an original smooth surface and the same glass sphere with a roughened surface after it has been subjected to a surface treatment according to the process described here. is Fig. Figure 2 is a schematic illustration of a possible embodiment of a device for subjecting glass beads in a spherical container with a roughened inner surface to rotation and spinning along two different axes A1, A2. is Fig. 2b a view similar Fig. 2a, which shows an alternative embodiment, wherein the processing vessel has a cylindrical shape. is Fig. Figure 3a is a schematic illustration of a possible way of subjecting several glass spheres to air plasma treatment using a vibrating conveyor belt. is Fig. Figure 3b is a schematic view showing an alternative embodiment wherein the glass beads are subjected to an air plasma treatment while rolling down a ramp or chute. is Fig. 3c is a schematic illustration of another embodiment wherein a plurality of glass spheres are subjected to air plasma treatment by being dropped and passing through a tube.

[0013] Reference will now be made in detail to the present preferred embodiments of the method, examples of which are illustrated in the accompanying drawing figures. Detailed description

[0014] It will now Fig. 1, which shows a single glass sphere 10 having a hollow body 12 and a smooth outer surface 14. After being subjected to the process for treating this outer surface, the glass sphere 10 contains a hollow outer body 12 with a roughened outer surface 20. In a useful embodiment, the treated glass sphere 10 has a diameter between 16 µm and 25 µm and a surface roughness of 0.01% to 0.1% of this diameter: that is, a surface roughness between 160 nm and 2500 nm. Several surface-treated glass spheres 10, as disclosed, have a density of 1.2 g / cm 3 . Furthermore, the roughened outer surface 20 has the desired interfacial interaction with a resin to provide a low-density molding compound layer with desired mechanical properties and performance when used as a component of an automotive body part.

[0015] To achieve the desired roughness of the glass ball surface 20, the glass balls can be roughened in a spinning and turning vessel, as in Fig. 2a and Fig. 2b, or an air plasma treatment, as in Fig. 3a - 3c, or be exposed to both.

[0016] Fig. Figure 2a shows a possible embodiment of a device 30 for processing the glass spheres 10. The device 30 contains a spherical processing vessel 32 having a roughened inner lining 34. The processing vessel 32 is held at two opposite points by a bracket 36. A drive motor 38 rotates (see action arrow B) the bracket 36 and thus the processing vessel 32 about a first axis A1. A second drive motor 40 is held on the bracket 36 and serves to spin the processing vessel 32 about a second axis A2 (see action arrow C). In the illustrated embodiment, the first axis A1 and the second axis A2 are substantially perpendicular to each other.

[0017] A controller 42, connected to the two drive motors 38, 40, allows the speed of the drive motors to be adjusted and changed as desired during the processing of the glass spheres 10. The goal is to ensure that the entire outer surface of the plurality of glass spheres 10 is consistently roughened, resulting in an outer surface roughness of 0.01% to 0.1% of the diameter of the plurality of glass spheres. For this purpose, the processing vessel 32 can be spun around axis A1 at a speed between 60 rpm and 600 rpm while being rotated around axis A2 at a speed between 60 rpm and 600 rpm. The controller 42 also allows the spinning direction and the rotation direction of the processing vessel 32 to be reversed as desired.Thus, for example, the processing vessel 32 may be rotated by the drive motor 38 in a first direction at a speed between 60 and 600 rpm for a first time period of, for example, five to sixty seconds, and then in a second direction at a speed between 60 and 600 rpm for a second time period of, for example, five to sixty seconds. Likewise, the processing vessel 32 may be spun by the drive motor 40 in a third direction at a speed between 60 and 600 rpm for a third time period of, for example, five to sixty seconds, and then in a fourth direction at a speed between 60 and 600 rpm for a fourth time period of, for example, five to sixty seconds. The rotating and spinning, and the time periods, may be sequential or overlapping. The reversal of direction helps ensure that the outer surface 20 of the glass spheres 10 undergoes consistent, comprehensive roughening.

[0018] Fig. Figure 2b shows a device 46 similar to the device 30 shown in Fig. 2a. The device 46 includes a processing vessel 48 with a roughened lining 50, a bracket 52, a first drive motor 54, a second drive motor 56, and a controller 58. The two devices 30, 46 operate identically, the only difference being that the processing vessel 48 in the second device 46 has a cylindrical shape instead of a spherical shape.

[0019] It will now Fig. 3a - 3c, which show three different devices for providing an air plasma treatment to the glass spheres 10. In the Fig. In the embodiment shown in Figure 3a, the glass spheres 10 are arranged on a surface 60 of a vibrating conveyor belt 62. Therefore, the glass spheres 10 bounce up and down as they move along the vibrating conveyor belt 62 through an air plasma stream 64 coming from the overlying plasma probe 66.

[0020] How Fig. As shown in Figure 3b, the glass balls 10 roll down an incline, slide or ramp 68 through a plasma stream 70 coming from the plasma probe 72 above.

[0021] In the Fig. 3c, the glass beads 10 fall through the tube 74, falling through the air plasma stream 76 coming from the opposing plasma probes 78. In each of the embodiments for air plasma treatment shown in Fig. As shown in Figures 3a-3c, the glass spheres 10 are exposed to air plasma temperatures between 23°C and 500°C and experience an increase in surface energy, which strengthens their chemical bonding to a resin, such as that used in the production of a molding compound layer. This increases the overall mechanical performance of a part made from this low-density molding compound layer, making the parts useful as body parts, such as hoods or the like, in a motor vehicle.

[0022] Given the unique size and shape of glass spheres, the three treatment processes mentioned above are specially designed to achieve complete surface treatment. The bouncing, sliding, and falling motions ensure that the glass spheres are fully exposed to the plasma flow. Complete surface treatment gives the glass spheres better mechanical properties and performance than partial treatment.

[0023] In summary, numerous advantages arise from the surface treatment process disclosed in this document, regardless of whether this process only involves processing the glass balls 10 in the spinning and turning vessels 32, 48, which are in Fig. 2a and Fig. 2b, only a processing of the glass spheres with the help of the air plasma treatments, which in Fig.3a - 3c, or subjecting the glass balls to both rotation and spinning in the processing vessel and air plasma treatment.

[0024] By increasing the roughness and / or surface energy of the surface 20 of the treated glass spheres 10, a chemical bond between the glass spheres and a resin used to produce low-density molding compound layers is strengthened, thereby providing those molding compound layers with improved mechanical properties that enable their use as various components of automotive body panels. This advantageously enables the production of lighter-weight automotive vehicles characterized by more fuel-efficient consumption. Therefore, the process disclosed herein and the resulting low-density glass spheres and molding compound layer products produced using the glass spheres 10 with the roughened surfaces 20 represent a significant advance in the art.

[0025] The foregoing has been presented for purposes of illustration and description. It is not intended to be exhaustive, nor is it intended to limit the embodiments to the precise form disclosed. Obvious modifications and variations are possible in light of the above teachings. All such modifications and variations are within the scope of the appended claims when interpreted to the extent to which they are fairly, legally, and equitably entitled.

[0026] It is further described: A method for treating outer surfaces of a plurality of glass spheres, comprising: Filling several glass beads into a processing vessel with a roughened lining; and Moving the processing vessel so that the multiple glass balls move against the roughened lining, thereby roughening the outer surfaces. B. Method according to A, comprising spinning and rotating the processing vessel. C. Method according to A, comprising reversing the direction of spin and rotation of the processing vessel. D. The method according to C, comprising spinning the processing vessel at a speed between 60 rpm and 600 rpm about a first axis A1 and rotating the processing vessel at a speed between 60 rpm and 600 rpm about a second axis A2. E. The method of D, comprising using a spherical processing vessel. F. Method according to D, comprising using a processing vessel in cylindrical shape. G. The method of A, comprising providing the plurality of glass spheres with an outer surface roughness of 0.01% to 0.1% of a diameter of the plurality of glass spheres. H. The method of A, including subjecting the plurality of glass spheres to an air plasma treatment. I. The method of H, comprising moving the plurality of glass spheres through an air plasma stream using a vibrating conveyor belt. J. The method of H, comprising moving the plurality of glass spheres through an air plasma stream on a chute. K. The method of H, comprising dropping the plurality of glass spheres through an air plasma stream. L. Process according to H, comprising exposing a plurality of glass spheres to air plasma temperatures between 23°C and 500°C. M. The method of H, comprising supplementing the air plasma treatment after treating the plurality of glass spheres in the processing vessel. N. A method for treating outer surfaces of a plurality of glass spheres, comprising: subjecting the plurality of glass spheres to an air plasma treatment to provide an outer surface roughness of 0.01% to 0.1% of a diameter of the plurality of glass spheres. O. The method of N, comprising moving the plurality of glass spheres through an air plasma stream using a vibrating conveyor belt. P. The method of N, comprising moving the plurality of glass spheres through an air plasma stream on a chute. Q. The method of N, including dropping the plurality of glass spheres through an air plasma stream. R. The method of N comprising exposing the plurality of glass spheres to air plasma temperatures between 23°C and 500°C. S. Glass ball, comprising: a hollow glass body with an outer surface with a diameter between 16 micrometers and 25 micrometers and a surface roughness of 0.01% to 0.1% of the diameter. T. Low density molding compound layer comprising a resin and a plurality of glass beads as set forth in S.

Claims

[1] A method for treating outer surfaces of a plurality of glass spheres, comprising: Filling several glass beads into a processing vessel with a roughened lining; and Moving the processing vessel so that the multiple glass balls move against the roughened lining, thereby roughening the outer surfaces. [2] A method according to claim 1, comprising spinning and rotating the processing vessel. [3] A method according to claim 2, comprising reversing the direction of spin and rotation of the processing vessel. [4] A method according to claim 3, comprising spinning the processing vessel at a speed between 60 rpm and 600 rpm about a first axis A1 and rotating the processing vessel at a speed between 60 rpm and 600 rpm about a second axis A2. [5] A method according to claim 4, comprising using a processing vessel in spherical shape. [6] A method according to claim 4, comprising using a processing vessel in cylindrical shape. [7] The method of claim 1, comprising providing the plurality of glass spheres with an outer surface roughness of 0.01% to 0.1% of a diameter of the plurality of glass spheres. [8] The method of claim 1, including subjecting the plurality of glass spheres to an air plasma treatment. [9] The method of claim 8, including moving the plurality of glass spheres through an air plasma stream using a vibrating conveyor belt. [10] A method for treating outer surfaces of a plurality of glass spheres, comprising: Exposing the several glass spheres to an air plasma treatment to to provide the plurality of glass spheres with an outer surface roughness of 0.01% to 0.1% of the diameter of the plurality of glass spheres. [11] The method of claim 10, including moving the plurality of glass spheres through an air plasma stream using a vibrating conveyor belt. [12] The method of claim 10, including moving the plurality of glass spheres through an air plasma stream on a chute. [13] The method of claim 10, including dropping the plurality of glass spheres through an air plasma stream. [14] The method of claim 10, including exposing the plurality of glass spheres to an air plasma temperature between 23°C and 500°C.