HIGH-PRESSURE CASTING SYSTEM

The high-pressure casting system addresses cold flake issues by using heat transfer channels and insulation to maintain molten metal temperature, enhancing surface quality and mechanical properties of die-cast parts.

DE102023126176B3Active Publication Date: 2024-10-17GM GLOBAL TECHNOLOGY OPERATIONS LLC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
DE102023126176
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2023-09-01
Filing Date
2023-09-27
Publication Date
2024-10-17
Estimated Expiration
2043-09-27

AI Technical Summary

Technical Problem

High-pressure casting processes result in cold flakes that cause irregular structures and defects on the surface and interior of the finished part due to partial solidification of molten metal in the filler can, leading to surface and interior defects.

Method used

A high-pressure casting system with proximal and distal channels for heat transfer fluid circulation, insulation layers, and controlled temperature management to minimize temperature loss and solidification during the casting process.

Benefits of technology

Reduces cold flakes, improving surface quality and mechanical properties of die-cast parts by maintaining consistent molten metal temperature and preventing premature solidification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A die-cast part, such as an electric drive unit, a high-pressure casting system, and a method for forming a die-cast part. The high-pressure casting system comprises a filling sleeve including a filling hole, a pouring trough connected to the filling hole, a furnace connected to the pouring trough, a mold cavity connected to the filling sleeve via a sprue post, and a heating system comprising at least one proximal channel positioned below the filling hole under the filling sleeve. The feed material is melted in the furnace and transferred through a pouring trough into the preheated filling sleeve via a filling hole. The feed material is injected into a mold cavity, the temperature of which is above the solidus temperature of the feed material upon entering the mold cavity.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND

[0001] The present invention relates to a high-pressure casting system according to the preamble of claim 1, as it is of the type is essentially known from DE 30 41 340 A1.

[0002] Further prior art can also be found in the documents DE 26 41 116 A1 and CH 367 288 A.

[0003] High pressure casting is a process for producing near-net shapes or final shapes from metal that have little Requires post-process finishing. The process is typically used for aluminum, zinc and magnesium During the process, molten metal is forced through a piston at relatively high speeds from a filling can, and pressed into a closed mold. The molten metal cools and begins to solidify, and once it is sufficiently solid, it is removed from the mold.

[0004] However, if the molten metal partially solidifies in the filling sleeve, the solidified layer near the Filling liner surfaces can lead to cold flakes or particles that solidify before entering the mold cavity. Cold flakes create irregular structures and irregularities in the finished part. These structures and Irregularities can occur on the surface and inside the part, and can lead to surface and internal defects lead.

[0005] Although current high pressure casting processes and systems serve their purpose, there is still a lack of High pressure casting processes and systems still need to be developed to reduce cold flakes. SUMMARY

[0006] According to the invention, a high-pressure casting system is presented which is characterized by the features of claim 1 distinguishes.

[0007] In further embodiments, the at least one proximal channel comprises a range of two to six parallel channels running parallel to the filling can, and at least one circumferential channel that connects the parallel channels connects. In further embodiments, the parallel channels are arranged around the lower half of the filling box. spaced apart.

[0008] In each of the foregoing embodiments, the at least one distal channel is formed by the sprue post. at least one section of the circumference of the filling can is wrapped around it. In further embodiments, the at least one distal canal, two distal canals.

[0009] In each of the foregoing embodiments, at least one sprue channel is located below the sprue post. positioned.

[0010] In each of the foregoing embodiments, an insulating layer is provided above the casting trough, wherein the The amount of insulation and the type of insulation chosen can result in a melting temperature loss of a starting material. It provides temperatures below 20 degrees Celsius. In other embodiments, the insulating layer consists of fiberglass.

[0011] According to various additional aspects, the present invention relates to a method for forming a Die-cast part. The process involves melting a raw material in a furnace at a furnace temperature, preheating a filling can using a heating system that includes at least one proximal channel, Transfer of the starting material through a pouring trough into a filling can through a filling hole, wherein at least one proximal channel positioned below the filler hole under the filler sleeve, and injection of the starting material into a Mold cavity by advancing a piston in the filling sleeve according to an injection speed profile, wherein the Temperature of the starting material above the solidus temperature of the starting material when entering the mold cavity.

[0012] In the above embodiments, the method further comprises circulating heat transfer fluid through the at least one proximal channel.

[0013] In each of the above embodiments, the furnace temperature is 100 degrees Celsius to 150 degrees Celsius above the solidus temperature.

[0014] In each of the above embodiments, the solidus temperature is determined by phase simulation.

[0015] In each of the above embodiments, the method comprises simulating a temperature loss of the molten feedstock as it is transferred through the runner to determine if the Temperature loss is greater than a permissible temperature loss, and adjusting the amount or type of insulation, surrounding the trough when the temperature is greater than the permissible temperature loss. In other In some embodiments, the permissible temperature loss is 20 degrees Celsius or less.

[0016] In each of the above embodiments, the filling sleeve is preheated to a preheating temperature, and the Preheating temperature and injection speed profile are determined by simulating the temperature of the starting material in the filling sleeve. In other embodiments, the preheating temperature of the Filling can in the range of 150 degrees Celsius and 200 degrees Celsius and the speed of the Injection speed profile covers a variety of speeds in the range from 0.4 meters per second to 0.7 meters per second.

[0017] According to several additional aspects, the present invention relates to an electric drive unit for a Vehicle. The electric drive unit comprises a housing that has a surface. The housing is made of a Magnesium alloy formed, with the casing having less than ten cold flakes per square meter on the surface. of the casing. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The drawings described herein are for illustrative purposes only. Fig. 1 illustrates cold flake formation in a die-cast part. Fig. 2 illustrates a high-pressure casting system according to embodiments of the present invention. Fig. 3 illustrates a filling can and a mold according to embodiments of the present invention. Fig. 4A illustrates the melt temperature distribution of the leading melt in a filling can without Heating channels in the filling sleeve. The scale at the bottom of the figure correlates with the length of the filling sleeve, and the scale on the left side represents the temperature in degrees Celsius. Fig. 4B illustrates the melt temperature distribution of the leading melt in a filling can without Heating channels in the filling sleeve. The scale at the bottom of the figure correlates with the length of the filling sleeve, and the scale on the left side represents the temperature in degrees Celsius. Fig. 5A illustrates the melt temperature distribution of the leading melt in a filling can with Inclusion of heating channels in the filling sleeve according to embodiments of the present invention. The scale bottom of the figure correlates with the length of the filling can, and the scale on the left represents the temperature in degrees Celsius. Fig. 5B illustrates the melt temperature distribution of the leading melt in a filling can with Inclusion of heating channels in the filling sleeve according to embodiments of the present invention. The scale bottom of the figure correlates with the length of the filling can, and the scale on the left represents the temperature in degrees Celsius. Fig. 6 illustrates the connection between the pouring trough and the filling pipe of a dosing furnace according to Embodiments of the present invention. Fig. 7 illustrates a simulated temperature distribution of the melt when filling into a non-insulated Filling can. The scale at the bottom of the figure correlates with the size of the melt, and the scale on the left represents the temperature in degrees Celsius. Fig. 8 illustrates a simulated temperature distribution of the melt when filling into an insulated Filling can according to embodiments of the present invention. The scale at the bottom of the figure correlates with the Size of the melt, and the scale on the left represents the temperature in degrees Celsius. Fig. 9 illustrates a flowchart of a procedure for selecting the melting temperature of the starting material during the die casting process, according to embodiments of the present invention. Fig. 10 illustrates a flowchart of an embodiment of a method for forming a die-cast part, according to embodiments of the present invention. Fig. 11 illustrates a vehicle that includes a housing for an electric drive unit, which is located under The system and method described herein were used. DETAILED DESCRIPTION

[0019] The term ‘vehicle’ used herein is not limited to motor vehicles. Although the present The technology described herein primarily relates to die-cast parts used in connection with vehicles. It can be used, but it is not limited to vehicles with combustion engines or electric vehicles. The concepts can be used in a variety of applications, such as in conjunction with components for use in Motorcycles, mopeds, locomotives, airplanes, watercraft and other vehicles, as well as in other Applications with hydrogen fuel cells and in applications with electric motors. Applications include for example, components for industrial machines and engines, agricultural equipment, compressors, Defense installations, heating, ventilation and air conditioning systems, power generators for residential and Commercial buildings and pumps where lubrication of the components is desirable.

[0020] Several examples of the invention, which are shown in the accompanying drawings, will now be referred to in detail. are illustrated. Whenever possible, the same or similar images are used in the drawings and the description. Reference symbols are used to refer to identical or similar parts or steps. The drawings are located in They are presented in a simplified form and are not to scale.

[0021] The present invention relates to high-pressure casting systems and methods for forming die-cast parts which are in can be used in a vehicle. High-pressure casting is a process for producing near-final or final shapes from Metals that require little post-processing. Such parts can include, but are not limited to, those made of metal. on housings for the drive unit of electric vehicles, gearbox covers, housings for sensors, including Lidar, shadow poles, brackets for electric motors and stepper motors, shields for telematics and other electronic equipment, sensor and airbag housings, fuel supply parts, air conditioning systems, winding spools for Safety belts, locking cylinders, transmission and chassis components, connectors, brake components and Engine blocks.

[0022] High pressure casting can be understood as a process in which molten metal is injected into a The metal is kept under pressure during solidification to prevent the to compensate for shrinkage occurring during the solidification process. In embodiments, the injection pressure, the The pressure with which the molten metal is forced into the cavity is minimal, as the filling can is in the range of 40%. up to 50% filled. Intensification pressures, i.e., the pressure under which the starting material is subjected during solidification in the The pressure held in the cavity ranges from 30 megapascals (MPa) to 100 MPa, including all values ​​and ranges. in it. High-pressure casting differs, for example, from gravity systems, where gravity is used to fill the die. the mold cavity is sufficient.

[0023] Fig. 1 illustrates a section of a die-cast part 100 which has a cold flake 102 on the surface of the The die-cast part comprises 100. In the illustrated image, the cold flake 102 leads to a discontinuity of the surface 104. of the die-cast part 100. Cracks 106 and other surface deformations 108 are present in the surface 104 of the die-cast part. 100 can be seen adjacent to the cold flake 102. In addition to the interruption of surface 104 and the impairment Due to surface properties, Cold Flake 102 can also reduce local material strength. Cold Flakes 102 can caused by the solidification and formation of a skin on the melt, while the melt is molten during the Residence time, i.e., the time between introducing the melt into the filling nozzle and injecting the melt into the mold cavity, located in the filling box of the casting machine.

[0024] Fig. 2 illustrates an image of a high-pressure casting system 200 for use herein. The high-pressure casting system 200 It generally includes a furnace 202 for melting the starting material 204 for the die-casting process. Starting material 204 comprises a metal or metal alloy comprising one or more of the following metals: Magnesium, aluminum, zinc, copper, lead, and tin. The starting material 204 is then conveyed through a trough 206 via a The material is conveyed through the filling hole 209 into the die-casting machine 208, which is described in more detail herein. The die-casting machine 208 The starting material 204 is injected into a mold cavity 210 within the mold mounted in the die-casting machine 208. 212. The mold cavity 210 is a negative of the component shape and the starting material 204 takes the shape of the Mold cavity 210 to form the die-cast part.

[0025] An embodiment of a die-casting machine 208 is illustrated in Fig. 3. The die-casting machine 208 generally includes a filling canister 302 in which a "filling" of the starting material 204 is collected before it by advancing a piston 303 towards the mold cavity 210, the material is injected (or "shot"). Filling sleeve 302 can be made of tool steel such as H13. The filling sleeve 302 is equipped with a sprue post 304 (also (called a "biscuit"), which forms a sprue. The sprue post 304 is connected to the mold cavity 210 via a The sprue system 306 is connected, which connects the mold cavity 210 at one or more locations to the The mold 212 can connect sprue posts 304. The mold 212 can include one or more slides 308, each slide 308 is activated by a cam 310.

[0026] Again with reference to Fig. 2 as well as to Fig. 3, a heating system is provided to To avoid temperature losses in the die-casting system 200, the heating system includes a circulator in various embodiments. 220, which heats a heat transfer fluid 224, such as oil, and through one or more proximal channels 314, which the Filling sleeve 302, one or more distal channels 316 surrounding the filling sleeve near the biscuit 304, and one or more channels 318 below the sprue biscuit 304 as well as any additional channels, such as channels 332 in the form that may be provided. The circulator 220 and the channels 314, 316 may, for example, using insulated hoses 226. The form 212 also includes one or more Channels 332 in the mold cavity. The heat transfer fluid 224 is heated in the circulator 220 to temperatures of up to 350 degrees Celsius, including all values ​​and ranges, such as in the range from 150 degrees Celsius to 200 degrees Celsius, whereby the heat transfer fluid 224 is also circulated through the channels 314, 316, 318. In alternative or additional In various embodiments, the heating system includes a heating controller (not illustrated) which provides a power supply and It includes circuits for processing temperature control algorithms, which are equipped with a range of are coupled to resistance heating elements or induction heating elements in channels 314, 316, 318.

[0027] In the illustrated embodiment, the proximal channels 314 extend from the underside of the filling hole 209 at a first end 320 of the filling can 302 to the middle point 322 or near the middle Point 332 of the filling box 302. It should be noted that in alternative or additional embodiments the proximal channels 314 can extend to the biscuit 304. In embodiments, the proximal channels 314 comprise parallel channels 324, which run essentially parallel to the filling box 302, and a channel 326, which is around the Filling box 302 is wound near or around the center point 322, and connects the parallel channels 324. Furthermore The parallel channels 324 can extend around the lower half of the filling box 302 below the filling hole 209. be spaced apart. For example, in embodiments, between two and six parallel channels 324 can be arranged around the The lower half of the filling can 302 should be spaced apart.

[0028] The distal channels 316 are illustrated such that they extend proximally around the entire circumference of the filling sleeve 302. to the biscuit 304 at the second end 330 of the filling canister 302. Two distal channels 316 are illustrated. However, there can also be more than two channels, up to ten channels, or alternatively, only one. Only one canal may be present. Furthermore, the distal canals 316 may only extend around a portion of the circumference of the Filling sleeve 302. In addition, below the sprue post 304, a sprue channel 318 The channels 314, 316, 318 all form circuits, each comprising an inlet and an outlet, which are connected to the circulator 220 so that the heat transfer fluid 224 can flow through the channels 314, 316, 318 and stagnation of the heat transfer fluid 224 is prevented.

[0029] The proximal channels 314, distal channels 316 and sprue channels 318 are spaced apart in the range of 50 Millimeters (mm) to 2500 mm, including all values ​​and ranges, from the inner wall 312 of the filling sleeve 302 placed with which the molten starting material 204 comes into contact. In addition, the channels 314, 316, 318 may take any number of cross-sections, such as circular, elliptical, rectangular or square. Furthermore, channels 314, 316, 318 can be incorporated into a block in which the filling box 302 is formed, or contact the filling box 302 in some other way.

[0030] Figures 4A and 4B illustrate the loss of the melting temperature of the starting material 204 without the Heating system and heating channels 314, 316, 318, as described using simulation software for the casting process, as described MagmaSoft, ProCAST, Flow3D, Anycasting, was determined. The melting temperature when introduced into the filling cylinder 302 The temperature was determined to be 720 degrees Celsius. After a dwell time of 1.6 seconds in filling can 302, 13 percent of the The mold cavity 210 was filled and 0.27 percent of the total weight of the starting material 204 solidified. Furthermore, the amount of material that solidified decreased. the temperature of the starting material 204 increased by 100 degrees Celsius and approached the inner wall 312 of the filling can by 100 degrees Celsius. The temperature losses increased to 130 degrees Celsius, and 1 percent of the molten material... The starting material 204 solidified when, after a residence time of 2.4 seconds, it passed 200 millimeters through the Filling box 302 was advanced and 27 percent of the mold cavity 210 was filled.

[0031] Figures 5A and 5B illustrate the loss of the melting temperature of the starting material 204 in a System with heating channels 314, 316, 318 in the filling box 302, as implemented using a casting process- The melting temperature was determined using simulation software such as MagmaSoft, ProCAST, Flow3D, and Anycasting. The temperature at which the product was placed in the filling canister was determined to be 720 degrees Celsius. After a dwell time of 1.6 seconds in the filling canister, 302 13 percent of the mold cavity 210 was filled, zero (0) percent of the total weight of the starting material 204 solidified. Furthermore, the temperature of the starting material dropped by 50 degrees Celsius and approached the inner wall 312 of the The filling can was heated by 100 degrees Celsius. The temperature losses increased to 90 degrees Celsius and 0.03 percent of the The starting material 204 solidified when the molten starting material 204, after a residence time of 2.4 seconds, reached 200 millimeters through the filling bushing 302 and 28 percent of the mold cavity 210 was filled.

[0032] Fig. 6 illustrates a connection between the filling box 302 and the trough 206. In the illustrated In this embodiment, the trough 206 is connected to the filling box 302 via a pouring trough 610, which is located above the pouring trough 610. The illustrated filling funnel can be omitted. To minimize temperature loss in the starting material 204 during the addition of the To reduce the starting material 204, in embodiments the casting trough 610 is fitted with a layer of insulation 614. covered. Insulation 614 includes, for example, fiberglass, mineral wool, MANNIGLAS® (available from Lydall, Rochester, NH), KAOWOOL Blanket (available from THERMAL CERAMICS INC. Augusta, Georgia), or ceramic. In further In embodiments, the insulation 614 is applied over the entire length of the trough 206 back to the furnace 202. Insulation 614 can have an R-value ranging from 2 per inch to 8 per inch, including all values ​​and ranges. it. Furthermore, the insulation is described with a thickness ranging from 0.5 inches to 6 inches, including all values ​​and ranges. in it, upset.

[0033] The insulation reduces the loss of melt temperature when the starting material 204 enters the casting trough 610 through. Fig. 7 illustrates a simulation of the temperature of the starting material 204 without insulation 0.4 Seconds after the starting material 204 is introduced from the trough 206 into the filling box 302. At this point, The filling container 302 is 14 percent full, and 0.03 percent by weight of the starting material 204 has solidified. Furthermore Furthermore, the melting temperature on the inner wall 612 of the casting trough 610 dropped by 50 degrees Celsius.

[0034] Fig. 8 illustrates a simulation of the temperature of the starting material 204 with the application of insulation. 0.4 seconds after the starting material 204 is introduced from the trough 206 into the filling box 302. At this point The filling container 302 is 14 percent full, and 0.03 percent by weight of the starting material 204 has solidified. Furthermore Furthermore, the melting temperature on the inner wall 312 of the casting trough 610 only dropped by 20 degrees Celsius.

[0035] Fig. 9 illustrates a method 900 for simulating the production of a die-cast part according to Various designs are used to select process parameters and form the die-cast part. This also includes... Reference is made to Figures 2, 3, and 6. In Block 902, an assumption is made about the temperature of the The starting material 204 is encountered as it exits the furnace 202. In embodiments, the temperature for the Melting of the starting material 204 in the furnace, i.e., the furnace temperature, in block 906 using the information in block 904 The phase simulations performed were selected. In the phase simulations in block 904, the solidus temperature of the starting material 204 determined, especially if the starting material is a multi-component alloy It's about the simulation software. Software for performing such simulations can include, for example, CALPHAD code such as Thermo-Calc, Pandat, JMatPro, etc. The solidus temperature can be understood as the highest temperature at which an alloy is solid. Furthermore, the amount of starting material 204 required to fill the cavity in one shot is based on The volume is determined by the cavity volume. It should be noted that the 302 filling can should only be filled to 40 to 50 percent. is permitted. In block 906, the furnace temperature is then set based on calculations of the expected temperature loss. determined when the starting material 204 is transferred from the furnace 202 into the casting trough 610 and then from the filling box 302 is injected. However, the selected oven temperature must not exceed a temperature that damages the material or degrade its components or cause problems during processing, such as undesirable phase transformations in the source material 204.

[0036] In block 908, thermal analyses and simulations of the die casting process are carried out, whereby the Temperature of the starting material 204 upon exiting the furnace 202 is used as a boundary condition. In block 910 It is simulated how the molten starting material 204 enters the casting channel 610 insulated as described above and enters the filling hole 209 of the filling sleeve 302. In block 912 it is determined whether the Melt temperature loss of the starting material 204 passing through the casting channel 610 in the simulation is greater than or is smaller than the permissible melt temperature loss, T . This is determined by whether the melt temperature permissible when passing through the pouring channel 610 or in the filling sleeve 302 falls below the solidus temperature, and can, for example, in the range of up to 20 degrees Celsius, including all values ​​and ranges contained therein, in order to To avoid temperature losses during injection, which lower the melt temperature to a temperature below The simulation of the casting process can be carried out using simulation software such as MagmaSoft, ProCAST, Flow3D, Anycasting.

[0037] If the temperature loss in block 912 is greater than the allowable melt temperature loss, T , then permissible the simulation is repeated in block 910 by changing a parameter such as the amount or type of insulation 614 for the casting channel 610, or by using a higher melt temperature of the starting material and a higher furnace temperature is started. If the temperature loss in block 912 is less (not greater) than the permissible Melt temperature loss, T , then a simulation is performed in block 914 to determine the local permissible Preheating temperature of the filling sleeve on the inner wall 312 and the injection profile including the speeds for the feed of the starting material 204 through the filling sleeve 302 with the piston 303 using the above In block 916, a determination is made whether the temperature of the starting material 204 falls below the solidus temperature in the filling can 302 or whether the temperature of the starting material 204 in the filling sleeve 302 is too high, so that the starting material 204 cannot be properly Mold cavity 210 solidifies because it takes too long to solidify, or when solidifying due to the cooling profile, a exhibits an undesirable phase.

[0038] When the temperature of the starting material 204 falls below the solidus temperature in the filling sleeve 302, the injection profiles are set and the simulation run is repeated in block 914. Various aspects of the process can be adjusted to control the temperature of the starting material 204 in the filling sleeve 302 and during injection For example, the preheating temperature of the filling sleeve 302 can be adjusted via the heating system. In addition, the speed profile, ie the injection profile, of the piston 303 in the filling sleeve 302 can be adjusted As illustrated below, the injection profile affects the temperature of the feedstock 204 in the filling cylinder 302. However, the injection profile speeds are limited; at excessively high speeds Profile velocities introduce turbulence into the base material 204, which leads to defects in the die-cast part. This can occur, for example, in the inclusion of oxides or pores. If the temperature of the starting material 204 does not fall below the As the solidus temperature in the filling box 302 drops, die-cast parts can be produced in block 918 using the various methods. Parameters are produced that were determined in the procedure 900 described above.

[0039] During the simulations mentioned above, various known boundary conditions are introduced into the system entered, for example, the geometry of the various components of the high-pressure casting system 200, the Coefficient of thermal expansion of the various components in the high-pressure casting system: 200 and in the starting material: 204 materials used and the thermal conductivity coefficient k of the various materials used in the high pressure casting system 200 and in the Starting material 204 materials used. In addition, various variables are entered into the system, For example, the temperature of the starting material 204 leaving the furnace and entering the casting trough 610, Temperatures of the starting material 204 leaving the runner 610 and entering the filling sleeve 302, the weight of the starting material 204 being transmitted by the system 200 and the speed at which the source material 204 is transmitted by each Part of the system 200 flows.

[0040] Table 1 provides a non-binding example of the effects of the injection profile and the oil temperature on the Temperature loss of the melt in the feedstock. The base rate can be the same as in a standard or The initial profile shows the speed used, and the proposed speed 1 and the proposed Speed ​​2 are examples of changes that can be made to an initial profile. Table 1 Injection profile and oil temperature compared to melting temperature loss Piston position Base velocity Suggested velocity 1 Suggested velocity 2 (mm) (meters per second) (meters per second) (meters per second) 100 0.25 0.3 0.4 200 0.3 0.35 0.45 400 0.4 0.5 0.6 500 0.4 0.55 0.7 650 0.25 0.55 0.7 Oil temperature melting temperature loss (Degrees Celsius) (Degrees Celsius) 180 60 58 52 220 59 56 50

[0041] As can be seen above, an increase in the flow rate can be achieved via the injection profile, i.e. at the Different piston positions reduce the melting temperature loss of the starting material 204. This can for example, this could be due to a reduction in the residence time of the starting material 204 in the filling container 302. Residence time can be understood as the time that the starting material 204 remains within the filling container 302.

[0042] Fig. 10 illustrates a method 1000 for forming a die-cast part. Reference is also made hereto to Fig. 2, Fig. 3, Figures 6 and 9 are referenced. In block 1010, the starting material 204 is heated in furnace 202 at the furnace temperature. melted, which was selected in block 906 as described above. In embodiments, the Oven temperature in the range of 100 degrees Celsius to 150 degrees Celsius above the solidus temperature, including all Values ​​and ranges therein. In block 1012, the starting material 204 is fed through the trough 206 and the launder 610 into the Filling sleeve 302. The amount or type of insulation 614 surrounding the trough 206 and the pouring channel 610 can based on the simulations performed in block 910 before the starting material 204 is the trough 206 and the pouring channel 610. In embodiments, the amount of insulation and the type of selected insulation provides a melt temperature loss of the starting material of less than 20 degrees Celsius, and are selected from the insulating materials mentioned above. Furthermore, the filling sleeve 302 is heated to a certain temperature. In embodiments, the filling sleeve 302 is filled with a heat transfer fluid preheated, which is heated to a preheating temperature in the range of 150 degrees Celsius and 200 degrees Celsius. In In these embodiments, the temperature loss in the filling box 302 is not greater than 50 degrees Celsius. Regarding the filling box 302 A vacuum is applied to prevent reactive gases, including water vapor, from entering the filling canister 302. penetrate. In block 1014, the starting material 204 is injected into the mold cavity 210. In embodiments The injection profile speed ranges from 0.4 meters per second to 0.7 meters per second. Furthermore, The temperature loss of the starting material in embodiments during injection is not greater than 100 degrees. Celsius. During the injection phase, the injection profile is based on the simulations performed in Block 914. In block 1016, the starting material 204 is kept under pressure in the mold cavity 210. The pressure is generated by the forward movement of the punch 303 to further fill the mold cavity 210 with the starting material 204 while the starting material 204 shrinks during cooling in the mold cavity 210. After sufficient Solidification, the die-cast part is removed from the mold cavity 210, such as by manual removal or by Removal using an ejector system in the mold 212 and triggered by the opening of the mold 212 to expose the mold cavity 210.

[0043] In embodiments, the die-cast part is a drive unit housing for an electric motor, used in a vehicle. For example, reference is made to Fig. 11, which shows a vehicle 1100 which comprises an electric drive unit 1110 comprising a housing 1112 consisting of a Magnesium alloy AE44 (Mg-4%Al-4%Re) using the methods and systems described above The housing of the electric drive unit must contain less than 10 cold flakes per square meter surface of the housing. Alternatively or additionally, since more than one die-cast part is produced during a single Cycle can be formed, the die-cast part is a housing for the drive unit, a carrier for the drive unit, a gearbox cover, a housing for sensors including lidar, a shadow post, a Mounting bracket for electric motors and stepper motors, a shield for telematics and other electronic equipment, a housing for sensors and airbags, a part for the fuel inlet, an air conditioning system, a coil for the Seat belt retractor, a lock housing, a transmission and chassis part, a connector, a brake component and Engine blocks.

[0044] The systems and methods presented herein for reducing cold flakes in die casting offer a range of Advantages. These advantages include, for example, improved mechanical properties of metal castings. These advantages include, for example, the improvement of surface properties. These advantages include Furthermore, for example, the reduction of structural irregularities in castings by cold flakes. Further advantages include, for example, a reduced scrap rate.

Claims

1. High-pressure casting system (200), comprising: a filling sleeve (302) comprising a filling hole (209); a pouring trough (610) connected to the filling hole (209); a furnace (202) connected to the trough (610); a mold cavity (210) connected to the filler sleeve (302) via a sprue post (304); and a heating system; characterized in that the heating system comprises at least one proximal channel (314) which is located below the filling hole (209) under the filling sleeve (302) and which extends to the center point (322) of the filling sleeve (302); and wherein the heating system comprises a hot oil circulator (220) connected to the at least one proximal channel (314) is connected.

2. High pressure casting system (200) according to claim 1, wherein the at least one proximal channel (314) is in the range of two to six parallel channels (314) running parallel to the filling sleeve (302) and comprising at least one circumferential channel, which connects the parallel channels.

3. High-pressure casting system (200) according to claim 2, wherein the parallel channels are arranged around the lower half of the filling sleeve (302) are spaced around.

4. High pressure casting system (200) according to claim 2, further comprising at least one distal channel (316) passing through the Sprue post (304) is wrapped around at least a portion of the circumference of the filler sleeve (302).

5. High pressure casting system (200) according to claim 4, wherein the at least one distal channel (316) comprises two distal channels (316) includes.

6. High pressure casting system (200) according to claim 4, further comprising at least one runner (318) located below of the sprue post (304).

7. High pressure casting system (200) according to claim 1, wherein an insulating layer (614) is provided over the casting trough (610), Where the amount of insulation and the type of insulation chosen can cause a melt temperature loss of starting material of less than 20 degrees Celsius.

Citation Information

Patent Citations

  • device for feeding liquid material to the loading chamber of an injection or compression molding machine

    CH367288A

  • Die casting machine delivery line and filling chamber junction - has branch with pneumatically operated piston and connecting block below

    DE2641116A1

  • Die-casting process for the production of low-gas, low-pore and low-oxide castings using a cold-chamber die-casting machine

    DE3041340A1