Phenol-free multi-purpose thermal direct recording media

DE202020006063U1Active Publication Date: 2024-10-02APPVION LLC
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
DE202020006063
Authority / Receiving Office
DE · DE
Patent Type
Utility models
Current Assignee / Owner
Filing Date
2020-12-10
Publication Date
2024-10-02
Estimated Expiration
2030-12-31

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Recording medium (104), comprising: a substrate; and a thermally responsive layer (114) supported by the substrate, wherein the thermally responsive layer (114) comprises a leuco dye and several developers; wherein the recording medium (104) is essentially phenol-free; and wherein the several developers comprise 1,3-diphenylurea (DPU) and urea urethane (UU).
Need to check novelty before this filing date? Find Prior Art

Description

Field of the invention The present invention relates to sheet-like recording media designed for recording or printing using conventional thermal recording technologies. The invention also relates to direct thermal recording media, with particular application to such media that incorporate a leuco dye and an acidic developer to provide a heat-activated printing mechanism. The invention also relates to related systems and articles. State of the art In direct thermal recording, an image is created by selectively heating the recording material (sometimes referred to as thermochromic-coated paper, thermal paper, thermal recording material or media, or thermally responsive recording material) at selected locations by passing the material under, or otherwise over, a thermal printhead. The recording material includes a coating of a thermally responsive layer, and the image is provided by a heat-induced color change of the thermally responsive layer. Some common uses of direct thermal recording may include, but are not limited to, sales receipts, labels for food or other merchandise, or event tickets. Numerous types of direct thermal recording media are known. See, for example, U.S. Patent Nos. 3,539,375 (Baum); 3,674,535 (Blose et al.); 3,746,675 (Blose et al.); 4,151,748 (Baum); 4,181,771 (Hanson et al.); 4,246,318 (Baum); and 4,470,057 (Glanz). In these cases, basic colorless or lightly colored chromogenic materials, such as a leuco dye, and an acidic color developer material are contained in a coating or substrate that, when heated to a suitable temperature, melts or softens, allowing the materials to react, forming a colored mark or image at the location where heat is applied. Thermally responsive recording materials exhibit characteristic thermal responses that produce an image with sufficient intensity or contrast upon thermal exposure. Depending on the application, such materials may be exposed to certain contaminants or environmental influences. For example, direct thermal media used as labels for pharmaceutical applications may be exposed to hand sanitizer. Direct thermal media used in other applications may be exposed to environmental agents or conditions typical of such applications, such as perspiration (water), heat and / or humidity, sunlight, or meat-wrapping film, to name a few. Ideally, a barcode or other image thermally printed on a direct thermal recording medium should remain visible and functional when exposed to such agents. However, developing such capabilities for a direct thermal product can be difficult and not always possible or practical. Unrelated to this topic, concerns were raised many years ago about the presence of phenol-based chemicals in direct thermal recording media. Phenol material was originally present in the thermally responsive layer of thermal recording materials, and specifically in the developer chemical that reacts with the leuco dye in the layer intended to produce a heat-induced color change. Alternatively, phenol-free developer chemicals were developed to address these concerns. A group of such chemicals was introduced about 20 years ago by Ciba Specialty Chemical Corp. under the Pergafast™ brand, including Pergafast 201 (3-(3-Tosylureido)phenyl p-toluenesulfonate). This developer is still widely used today in the manufacture of phenol-free direct thermal recording materials. Some other well-known phenol-free developers include NKK 1304. (N-[2-(3-phenylureido)phenyl]benzenesulfonamide), distributed by Nippon Soda Co. Ltd., tolbutamide (1-butyl-3-(4-methylphenyl)sulfonylurea) and dapsone (4,4'-diaminodiphenylsulfone). Brief description of the invention We have discovered a unique developer chemistry for use in the thermally responsive layer of direct thermal recording media. Besides being non-phenolic, this unique chemistry can be used to create direct thermal recording materials capable of withstanding multiple types of environmental conditions or agents, and in this sense, these can be described as multipurpose recording materials. This unique chemistry utilizes a combination of two non-phenolic developers, neither of which, on its own (when used with a suitable leuco dye), can produce a direct thermal recording material with such properties, but when combined, provide surprising and unexpected results. The two developers are 1,3-diphenyl urea (“DPU”) and urea urethane (“UU”).We have further found that the unique chemistry allows the product's thermally responsive layer to have an extremely low basis weight, meaning it is extremely thin. This allows for reduced product mass and a number of related benefits, including a reduction in the post-use waste stream associated with direct thermal recording materials, for improved environmental impact. We have thus developed a new family of phenol-free direct thermal recording materials or media. These materials are designed for direct thermal imaging, and the resulting images can be robust enough to withstand several different environmental influences or agents. The materials use a combination of two non-phenolic developers, neither of which alone can produce a direct thermal recording material with the desired multipurpose functionality. We therefore disclose herein, among other things, recording media comprising a substrate and a thermally responsive layer supported by the substrate. The recording media are substantially phenol-free, and the thermally responsive layer includes a leuco dye and a plurality of developers including 1,3-diphenylurea (DPU) and ureaurethane (UU). The recording media may further include a basecoat between the thermally responsive layer and the substrate, and a topcoat supported by the substrate such that the thermally responsive layer is disposed between the topcoat and the substrate. The thermally responsive layer may have a basis weight of less than 1.48 g / m² (1 lb / 3300 ft²), or in a range of 0.9 to less than 1.48 g / m². The DPU and the UU may be distributed throughout the thermally responsive layer. Substantially no developers other than DPU and UU need be present in the thermally responsive layer. The DPU and the UU may be present in the thermally responsive layer in a weight fraction falling within the range of 1 / 3 to 3, or 1 / 2 to 2, or it may be substantially 1. The print quality of the recording medium, when printed with a thermal printer energy setting of 11.7 mJ / mm2 at a print speed of 6 inches per second (ips), i.e., substantially 15 cm / s, can be characterized by an ANSI value (at a wavelength of 650 nm, or at 670 nm, or at both 65 nm and 670 nm) of at least 1.5. The print quality of the recording medium can still be characterized by an ANSI value of at least 1.5 after one or all of the following has occurred: the printed recording medium is soaked with water for 24 hours and then removed and dried; the printed recording medium is immersed in water and then placed in contact with a polyvinyl chloride meat wrap under a weight of 7 pounds (substantially 3.2 kg) for 24 hours, and then removed and dried;The printed recording medium is immersed in boiling water for 20 minutes, then removed and dried; the printed recording medium is heated to 60°C for 24 hours, then removed and cooled; the printed recording medium is exposed to air at 40°C and 90% relative humidity for 24 hours, then removed and cooled; the printed recording medium is subjected to an accelerated sunlight test at 0.67 W / m2 for 7 hours and then removed; or a drop of a 70% ethyl alcohol-based hand cleaner is placed on the printed recording medium and allowed to dry. We also disclose substantially phenol-free recording media comprising a flexible substrate and a thermally responsive layer supported by the substrate, wherein the thermally responsive layer includes a leuco dye and a plurality of developers including DPU and UU. The DPU and UU may both be distributed throughout the thermally responsive layer and may be present in the thermally responsive layer in a relative weight fraction that is within a range of 1 / 3 to 3, or 1 / 2 to 2, or that is substantially 1. A print quality of the recording medium printed at a thermal printer energy setting of 11.7 mJ / mm2 at a print speed of 15 cm / s (6 inches per second, inches per second (ips)) may be characterized by an ANSI value (at 650 nm, 670 nm, or both 650 nm and 670 nm) of at least 1.5. The print quality of the printed recording medium may still be characterized by an ANSI value of at least 1.5 after any, or all, of the following: the printed recording medium is immersed in water and then placed in contact with a polyvinyl chloride meat wrap under a weight of 3.2 kg (7 lbs) for 24 hours, and then removed and dried; the printed recording medium is heated to 60°C for 24 hours, then removed and cooled; or the printed recording medium is exposed to air at 40°C and 90% relative humidity for 24 hours, then removed and cooled. We disclose numerous related methods, systems and items. These and other aspects of the present disclosure will become apparent from the further detailed description. However, the above summaries should not be construed as limitations on the claimed subject matter, which subject matter is defined solely by the appended claims. Short description of the drawings The inventive objects and systems will now be described in more detail with reference to the drawings, wherein: Fig. 1 is a schematic perspective view of a roll of direct thermal recording material or medium, and Fig. 2 is an enlarged schematic front view of a direct thermal recording material, also serving as a schematic sectional view. In the drawings, like reference numerals indicate like elements. Detailed description of illustrative embodiments As described above, we have discovered a unique developer chemistry for use in the thermally responsive layer of direct thermal recording materials. The new chemistry involves a combination of two developers that, when used together with a suitable leuco dye, can form a multipurpose direct thermal recording material capable of passing multiple environmental exposure tests, but when used individually in an otherwise identical thermal recording material, fails the same tests. Indeed, one of the developers, when used alone with a suitable leuco dye, produces a direct thermal recording material that, after imaging by a direct thermal printer and prior to any environmental exposure tests, produces an image that fails even the minimum standard for machine-readable barcodes.The two phenol-free developers of this unique combination are 1,3-diphenylurea (“DPU”) and urea urethane (“UU”). The unique chemistry also allows the product's thermally responsive layer to have an extremely low basis weight, meaning it is ultra-thin. This low coating weight, in turn, provides lower material costs, lower manufacturing costs, and an overall lower product weight and mass. The reduced product mass also reduces the post-consumer waste stream associated with direct thermal recording materials, resulting in a reduced environmental impact. Direct thermal recording materials are often manufactured in large rolls on industrial coating machines from a continuous web of paper or other flexible substrate material. Such a roll 100 of direct thermal recording material 104 is shown schematically in Fig. 1. After manufacturing, the roll 100 can be converted into individual sheets, labels, or smaller rolls by slitting, cutting, or other standard means. An enlarged side or cross-sectional view of the recording material 104 is shown schematically in Fig. 2 to illustrate the typical substructure consisting of component layers or coatings. The recording material 104 can be made by applying several different coatings to at least one side or major surface 110a of a substrate 110. We can refer to the major surface 110a as the front surface of the substrate, and the exposed major surface 104a can be the front surface of the recording material 104. The opposite major surface 104b can be the back surface of the recording material. Briefly, the substrate 110 is coated with a base layer 112, a thermally responsive layer 114, and a top layer 116. The coatings are preferably applied in the order shown, with layer 114 between layers 112, 116, and with layer 112 between layer 114 and the substrate 110. In some cases, the base layer 112 can be omitted, or both the base layer and the top layer can be omitted.The coatings can be formed in any suitable manner, including roll coating, knife coating, rod coating, gravure coating, curtain coating, spot coating, and so on. Furthermore, additional layers and coatings can be added to or incorporated into the recording material on its front and / or back sides. For example, one or more coatings can be applied to the opposite side of the substrate, i.e., to the main surface 110b, as described below. First, however, the other elements of the direct thermal recording material 104 will now be described in more detail. The substrate 110 can be made of any material that can be coated or applied with the other layers and then supports them. The type of substrate material is not critical. Generally, the substrate 110 is in sheet or roll form and can be or include a support element such as a web, tape, strip, film, cardboard, or the like. In this regard, a sheet refers to an object with two large (main) surface dimensions and a comparatively small thickness dimension, and in some cases, the sheet can be wound into a roll. In this regard, the substrate 110 is typically thin and flexible, but strong enough to withstand the forces and stresses acting on it in a coating machine without unwanted tearing. The substrate 110 can be opaque, transparent, or translucent, and can be colored or achromatic.The substrate material may be fibrous, including, for example, paper and filamentous synthetic materials. It may be a film, including, for example, cellophane and synthetic polymer sheets that are cast, extruded, or otherwise formed. Suitable plastic films include films made of polypropylene (including oriented polypropylene (OPP) and biaxially oriented polypropylene (BOPP)), polyethylene (PE), and polyethylene terephthalate (PET). The substrate material may thus be non-cellulosic. An exemplary substrate 110 may be or include a neutral-gauge base paper. The thickness of the substrate 110 may depend on its composition, but a typical thickness (caliper) range is from 1.9 to 12 mils (e.g., 50 to 300 µm), or other suitable thicknesses. The paper may have a basis weight of 35 to 200 g / m3, but other suitable basis weights may also be used. The paper may also be treated with one or more agents, such as a surface primer. Uncoated papers, including unprimed, conventionally primed, or lightly treated base papers, may be used. The substrate 110 may be of simple construction and free of gloss coatings or other substantially functional coatings.For example, the substrate 110 may be of substantially uniform composition throughout its thickness, rather than a multilayer construction or a material to which one or more separate functional coatings have already been applied. However, in some cases, it may be desirable to treat, prepare, or otherwise process the substrate 110 in preparation for coating with one or more of the other layers shown in the drawing. The base layer 112 may be applied directly to the surface 110a of the substrate 110 before other coatings are applied. The base layer 112 may, in some cases, be referred to or characterized as a thermally insulating layer, separator layer, heat-reflective layer, insulating layer, or primer layer. By adapting the layer 112 to have a thermal conductivity that is less than both the thermal conductivity of the thermally responsive layer and the thermal conductivity of the substrate 110, the base layer 112 may provide some thermal isolation between these other layers. Such thermal isolation enhances image quality, imaging speed, or both by ensuring that heat delivered from the thermal printhead (not shown) to the front surface 104a is not lost by conduction through the thermally responsive layer 114 into the more massive substrate 110. The base layer 112 may include hollow sphere pigments (HSP) such as product name Ropaque™ TH-2000 or TH-500EF, available from The Dow Chemical Company, or other suitable materials. The HSP is useful for reducing the thermal conductivity of the base layer. The base layer 112 may be made by a process in which a dispersion is applied to the surface 110a of the substrate and then dried. In some cases, the base layer 112 may be eliminated and omitted from the product design. When included as part of the recording material, the thermally insulating layer may have a thickness in the range of 2 to 12 µm, or another suitable thickness. The thermally responsive layer 114 can be applied to the base layer 112, or to the substrate 110 if the base layer is omitted. The 114 can alternatively be referred to as a thermally sensitive colorant layer. This layer 114 comprises a colorant composition that is thermally sensitive, meaning it changes color upon sufficient heating. The colorant composition includes two main components: a colorant dye (electron donor dye precursor), also referred to as a leuco dye or chromogenic material, and an acidic developer. The leuco dye and the acidic developer are typically ground to individual particle sizes of between 1 and 10 micrometers, dispersed in a binder, and distributed homogeneously and in continuous proportion to one another throughout the layer 114.Sufficient heating at any location allows the acid developer particles to react with the leuco dye particles, resulting in a color change at the heating site, usually from light to dark. Known systems and materials are described in U.S. Patents 3,539,375 (Baum), 3,674,535 (Blose et al.), 3,746,675 (Blose et al.), 4,151,748 (Baum), 4,181,771 (Hanson et al.), 4,246,318 (Baum), 4,470,057 (Glanz), and 5,955,398 (Fischer et al.). The acidic developer is preferably non-phenolic and advantageously comprises, as already described above, a combination of two different non-phenolic developer materials, in particular 1,3-diphenylurea ("DPU") and ureaurethane ("UU"). DPU may alternatively be referred to by names such as 1-3-diphenylurea; N,N'-diphenylurea; diphenylurea; urea, -diphenyl; CARBANILIDE; diphenylcarbamide; or C13H12N2O. UU may alternatively be referred to by names such as urethaneurea; urethane-urea copolymer; polyurethaneurea, or poly(urethaneurea); polyurethaneurea elastomer, or poly(urethaneurea) elastomer; polyureaurethane; poly(urea)urethane; poly(urea-urethane)polymer; poly(urea-urethane), heat-cured; poly(ether-urethaneurea); Poly(ester-urethane-urea); poly(ester-urethane)-urea elastomer; or C4H11N3O3. One motivation for using non-phenolic developers in the thermally responsive layer 114 is to satisfy market demand for phenol-free receipts, labels, and the like. As such, it is often desirable, but not always required, that not only the thermally responsive layer 114 be phenol-free or substantially phenol-free, but that the entire direct thermal recording material 104 be phenol-free or substantially phenol-free. We use the term "substantially phenol-free" to encompass both articles that are completely and entirely phenol-free and articles that contain only traces of phenolic material below threshold levels. Neither DPU nor UU are particularly noteworthy when used as such with a suitable leuco dye. Indeed, when UU is used with no other developer materials, but only with a suitable leuco dye in a thermally responsive layer, the resulting direct thermal recording material, when imaged with a direct thermal printer, produces an initial image that does not meet even the minimum requirements for barcode machine readability. On the other hand, when the UU in such a product is completely replaced by DPU—i.e., when the DPU itself is used as the sole developer in layer 114—the image initially produced by the direct thermal printer meets the minimum requirements for barcode machine readability, but no longer does so once the printed sample has been subjected to any of the environmental exposure tests described below.Surprisingly, when DPU and UU are used in combination, and of course with a suitable leuco dye, the resulting direct thermal recording material not only produces a thermally generated image that meets the minimum requirements for barcode machine readability, but also maintains this image quality after the printed sample has been subjected to environmental exposure tests that are failed by otherwise identical recording materials containing only DPU or only UU as developer. In embodiments employing the combination of DPU with UU, the DPU, the UU, and the selected leuco dye are each preferably homogeneously and evenly distributed throughout the thermally responsive layer 114. This does not necessarily mean that these various materials have equal proportions in this layer. In most cases, however, we have found it desirable to have approximately the same amount of DPU as UU, i.e., a relative DPU / UU weight ratio of approximately 1. However, other DPU / UU weight ratios may also be employed, as demonstrated in the examples below. For example, the DPU / UU ratio may range from 1 / 3 to 3, or from 1 / 2 to 2, or it may be approximately 1. When DPU and UU are used in combination, they are preferably the only developers used in layer 114. However, if desired, one or more other chemical developers may be added in addition to DPU and UU. If so done, such developers are preferably included individually and collectively in layer 114 in a weight percentage less than that of DPU and UU. In addition to the DPU and UU, the thermally responsive layer 114 naturally includes at least one leuco dye designed to react with the multiple developers at elevated temperatures to produce a mark or color change. The leuco dye(s) may be any known dye(s) capable of such a reaction. Examples include, without limitation:- ODB-2 (CAS No. 89331-94-2, chemical name spiro(isobenzofuran-1(3H),9'-(9H)xanthen)-3-one, 6'-(dibutyl)amino)-3'-methyl-2'-(phenylamino)-);- BK305 (CAS No. 129473-78-5, chemical name spiro(isobenzofuran-1(3H),9'-(9H)xanthen)-3-one, 6'-(diphenylamino)-3'-methyl-2'-(phenylamino)-); and- ETAC (CAS No. 59129-79-2, chemical name Spiro(isobenzofuran-1(3H),9'-(9H)xanthen)-3-one, 6'-(ethyl(4-methylphenyl)amino)-3'-methyl-2'-(phenylamino)-). The thermally responsive layer 114 also includes one or more suitable binders to help hold the particles in the layer together. Such binders may include poly(vinyl alcohol), hydroxyethylcellulose, methylcellulose, isopropylcellulose, starch, modified starches, gelatin, and the like. Latex materials including polyacrylates, polyvinyl acetates, polystyrene, and the like may also be employed. The binders help maintain the mechanical integrity of layer 114 during brushing or handling forces resulting from use or storage of the recording material. There should be enough binder to impart such protection, but not so much as to impair reactive contact between the color-forming reactive materials. The binder may be present at 5 to 30% by weight of the dried coating. In addition to the leuco dye, developers, and binder, the coloring composition of layer 114 may also include one or more materials called modifiers that aid in coloring. The modifiers may function as one or both of (a) lowering the melting point of the dye / developer, and (b) acting as a type of solvent in which the dye and developer dissolve or melt. The modifier may thus facilitate the reaction between the leuco dye and the developer to produce a more intense or faster image, or both. See, for example, U.S. Patents 4,531,140 (Suzuki et al.), 4,794,102 (Petersen et al.), 5,098,882 (Teraji et al.), 6,835,691 (Mathiaparanam et al.), and 6,921,740 (Hizatate et al.). Typically, the thermally responsive layer of a conventional direct thermal recording material would be applied at a thickness corresponding to a basis weight of 1.5 to 6 lb / 3300 ft² (2.2 to 8.9 g / m²), or more typically 2-4 lb / 3300 ft² (3.0 to 5.9 g / m²), for a finished dry thickness in the range of 1.2 to 4.8 µm, or 1 to 5 µm. A practical lower limit is a coating weight of approximately 1 lb / 3300 ft² (~1.48 g / m²). The thermally responsive layer 114 of the inventive recording material can, if desired, also be applied in the same coating weights and thicknesses, but we have found that another advantage of the disclosed combination of DPU / UU developers is that the layer 114 can be made much thinner while still providing acceptable thermal image quality.In particular, layer 114 can be made with a coating weight of less than 1 lb / 3300 ft² (1.48 g / m²). We have demonstrated acceptable product properties down to a coating weight of layer 114 (containing DPU and UU developer) of 0.9 g / m². Thus, the coating weight of layer 114 can range from 0.9 to 8.9 g / m², or 0.9 to 5.9 g / m², or 0.9 to 2.2 g / m², or 0.9 to 1.48 g / m², or 0.9 to, but less than, 1.48 g / m². The ability to form the thermally responsive layer 114 ultra-thin has a number of advantages, such as lower product weight / mass, lower product costs, and reduced environmental impact with regard to the post-use waste stream. Returning to Fig. 2, a topsheet 116 is shown on, and in contact with, the thermally responsive layer 114. In the illustrated embodiment, the outer major surface of the topsheet 116 is exposed to air and corresponds to the outer major surface 104a of the direct thermal recording material 104. The topsheet 116 is optional and may be omitted if desired. When present, it can protect the underlying layers of the recording material 104 from unwanted contaminants or substances. For example, some topsheets can serve as barriers or seals against moisture penetration by oils or other unwanted liquids. The topsheet 116 can be any topsheet of conventional design. The topsheet 116 can include, for example, binders such as modified or unmodified polyvinyl alcohols, acrylic binders, crosslinkers, lubricants, and fillers such as aluminum trihydrate (aluminum hydroxide) and / or silicas. The topsheet 116 can have a thickness in the range of 0.5 to 2 µm, or another suitable thickness. The disclosed recording materials may also include additional layers and coatings other than those described above. Such other layers or coatings include coatings that may be applied to the back surface 110b of the substrate 110. One such layer is illustrated in Fig. 2, designated 118. This layer 118 may be an adhesive layer comprising a pressure-sensitive adhesive (PSA), a hot-melt adhesive, or another suitable adhesive. By providing it on the back surface of the recording material 104, the recording material may serve as a label and may be attached to containers, films, or other bodies such that its front, thermally printed side is visible to users. A release liner (not shown) for covering a PSA layer until use may also be included.Release coatings may also be applied to the surface for applications that do not require films. Direct thermal recording materials can potentially be used in a variety of configurations and, as such, can be exposed to a wide variety of environmental influences, contaminants, and conditions. Images formed on such materials by direct thermal printing are known to degrade when exposed to at least one of these conditions. A given recording material may experience degradation under fewer or more of these conditions, depending on its precise construction, including the chemicals used to manufacture the thermally responsive layer. Of course, the more environmental conditions the recording material can withstand without significant image degradation, the more environments and applications the recording material can be used in. Dry heat: One environmental condition of interest is the exposure of the imaged material to heat, i.e., heat resistance. Of course, if an imaged recording material is heated to a sufficiently high temperature, e.g., a printhead temperature of at least about 200°C, the leuco dye will react with the developer throughout the thermally responsive layer, causing the entire front surface of the recording material to change color and obscure any image previously formed on it. This refers to an environment heated substantially above ordinary room temperature, but in the neighborhood of 60°C, which an imaged recording material might experience when affixed as a label to a cup or coffee container or other hot beverage, or when affixed to a package of food to be heated or cooked in a microwave oven. Plasticizers: Another environmental condition of interest is contact with a plasticized film, particularly polyvinyl chloride (PVC) film used in grocery stores to wrap meat products. Direct thermal recording materials can be used on the front of labels that come into contact with PVC films from other packages. Water: Another environmental condition of interest is immersion in water. This can occur when a printed label or ticket is left in a garment and inadvertently put through a wash cycle. The most favorable environmental condition is when the water is at room temperature, or possibly lukewarm. Boiling water: This interesting environmental condition is like the immersion in water condition, but the water is at boiling temperature. Humidity: Another humid environmental condition of interest is exposure to hot, humid conditions such as those found in tropical regions. This can include temperatures around 450°C and a relative humidity of 90%. Sunlight: Another environmental condition of interest is exposure to sunlight. Disinfectants: Another environmental condition of interest is exposure to alcohol-based hand sanitizers. Examples and counterexamples In accordance with the above teachings, a number of direct thermal media examples and comparative examples were prepared and tested. In preparing the samples, a number of dispersion formulations were prepared. These were of two types: dispersion formulations of leuco dyes and dispersion formulations of acid developers. The formulations for the leuco dyes followed a first recipe, "A," and the formulations for the developers followed a second recipe, "B," as follows, where all parts or percentages are by weight: Table 1 Dispersion A Formulation Table 1 Dispersion A Formulation chromogenic material (leuco dye)30.0 Binder, 20% solution of polyvinyl alcohol in water25.0 Defoaming and dispersing agents0.4 Water44.6 Table 2: Dispersion B formulation Table 2: Dispersion B formulation Developer material 38.0 Binder, 20% solution of polyvinyl alcohol in water18.0 Defoaming and dispersing agents0.4 Water43.6 A formulation designated Dispersion A1 followed recipe “A” and employed ODB-2, i.e., 2-anilino-3-methyl-6-dibutylaminofluoran, as the chromogenic material. A formulation designated Dispersion A2 followed recipe “A” and employed BK-305, i.e., 2-anilino-3-methyl-6-dipentylaminofluoran, as the chromogenic material. A formulation designated Dispersion B1 followed recipe “B” and used DPU, i.e. 1,3-diphenylurea, as the developer material. A formulation designated Dispersion B2 followed Recipe "B" and employed UU, i.e., urea urethane (specifically, the Urea Urethane Compound sold by Chemipro Kasei Kaisha Ltd., CAS No. 321860-75-7) as the developer material. A formulation designated Dispersion B3 followed Recipe "B" and employed D-8, i.e., 4-hydroxyphenyl-4-isopropoxyphenyl sulfone, as the developer material. A formulation designated Dispersion B4 followed Recipe "B" and employed BPS, i.e., 4-hydroxyphenyl sulfone, as the developer material. A formulation designated Dispersion B5 followed recipe “B” and used BPS-MBE, i.e. 4-benzyloxyphenyl-4'-hydroxyphenylsulfone, as the developer material. A formulation designated Dispersion B6 followed formulation “B” and used tolbutamide, i.e. 1-butyl-3-(4-methylphenyl)sulfonylurea, as the developer material. A formulation designated Dispersion B7 followed recipe “B” and used dapsone, i.e. 4,4'-diaminodiphenyl sulfone, as the developer material. A formulation designated Dispersion B8 followed Recipe "B" and employed Pergafast™ 201, i.e., N-(p-toluenesulfonyl)-N'-(3-p-toluenesulfonyloxyphenyl)urea, sold by Solenis LLC, as the developer material. A formulation designated Dispersion B9 followed Recipe “B” and employed NKK-1304, i.e., N-[2-(3-phenylureido)phenyl]benzenesulfonamide, sold by Nippon Soda Co., Ltd, as the developer material. Various of these dispersion formulations were mixed with each other and other ingredients to produce a coating formulation for use in forming the thermally responsive layer of a given sample. The coating composition, unless otherwise stated, was as follows: Table 3: Coating formulation for thermally responsive layer Table 3: Coating formulation for thermally responsive layer Dispersion A (chromogenic material / leuco dye)22.0 Dispersion B (Developer) 38.0 Binder, 10% solution of polyvinyl alcohol in water25.0 Filler paste, 30% in water15.0 Each sample (Example or Comparative Example) was prepared in the following manner, unless otherwise stated: The first step was to coat a base layer (see, for example, layer 112 in Fig. 2 ) onto one side or major surface of a substrate (see, for example, substrate 100 in Fig. 2 ). The substrate used was a 63 g / m2 (gsm) superfine paper sheet. The base layer was thermally insulating and included a mixture of calcined clay such as Ansilex 93 from BASF Corporation, and Ropaque™ TH-2000 hollow sphere pigment (HSP) from The Dow Chemical Company, together with an SBR binder, and was applied at a coating weight of 4.5 g / m2. After drying, a thermally responsive layer (see, for example, layer 114 in Fig. 2 ) was applied over the base layer. The coating weight of the thermally responsive layer was 1.3 g / m2, unless otherwise stated. After this layer was dry, a top layer (see e.g.Layer 116 in Fig. 2 ) was coated onto the thermally responsive layer. The topcoat consisted of delaminated clay, PVOH, crosslinker, and lubricant such as zinc stearate, and was applied at a coating weight of 1.5 g / m². After the topcoat was dry, no further coatings were applied to the substrate, and the sample was ready for thermal printing and testing. The following table shows the names given to the various samples prepared and tested (Examples 1 to 6 and Comparative Examples 1 to 12) and the details of their respective thermally responsive layers: Table 4: Sample names and details of the thermally responsive layer Table 4: Sample names and details of the thermally responsive layer Example: 1A1B1 and B21:1 ratio, B1 and B2 each 19 parts1,3 Example: 2A2B1 and B21:1 ratio, B1 and B2 each 19 parts1,3 Example: 3A2B1 and B21:3 ratio, B1 to 9.5, B2 to 28.5 parts1.3 Example: 4A2B1 and B23:1 ratio, B1 to 28.5, B2 to 9.5 parts1,3 Example: 5A1B1 and B21:1 ratio, B1 and B2 each 19 parts1,1 Example: 6A1B1 and B21:1 ratio, B1 and B2 each 19 parts0.9 VB1A1B11.3 VB2A1B21.3 VB3A2B11.3 VB4A2B21.3 VB5A1B31,3 VB6A1B41.3 VB7A1B51,3 VB8A1B81,3 VB9A1B91,3 VB10A1B6 and B71:1 ratio, B6 and B7 each 19 parts1.3 VB11A1B1 and B81:1 ratio, B1 and B8 each 19 parts1.3 VB12A1B1 and B91:1 ratio, B1 and B9 each 19 parts1.3 All of these samples were thin and flexible, phenol-free, and their front surfaces were uniformly white or pale in color. Each sample was then tested for its ability to produce an image using direct thermal printing, the print quality of that image, and the print quality of the image after subjecting the printed sample to a number of different environmental tests. Thermal printing of each sample was performed using a Zebra™ thermal printer, model 140-401, at a speed of 6 inches per second (ips) and using the standard printhead energy setting of 11.7 mJ / mm². The printed image in each case was a barcode sample. The print quality or image quality of the barcode sample was assessed using a Trucheck™ barcode verifier (model TC-843) operating at a wavelength of 650 nm, with a "pass" criterion corresponding to an ANSI value of 1.5 or greater and a "fail" criterion corresponding to an ANSI value of less than 1.5. In some cases, print quality was also assessed at 670 nm using a Trucheck™ barcode verifier (model TC-854), with a "pass" criterion corresponding to an ANSI value of 1.5 or more and a "fail" criterion corresponding to an ANSI value of less than 1.5. After the initial print quality of the printed label media was measured, one sample of each sample was subjected to one of the seven environmental tests mentioned above, namely: dry heat; plasticizer; water; boiling water; humidity; sunlight; and disinfectant. For the dry heat test, the printed sample was exposed to 60°C (dry) heat for 24 hours and then removed from the heat. After this test, the quality of the printed image was tested at both 650 nm and 670 nm. For the plasticizer test, the printed sample was immersed in room-temperature water, then removed and placed under a 7-pound weight in contact with PVC meat wrap for 24 hours, then removed and dried. After this test, the image quality was tested at 650 nm. For the water test, the printed sample was soaked in water at room temperature for 24 hours, then removed and allowed to dry. After this test, the image quality was tested at 650 nm. For the boiling water test, the printed sample was glued to a plastic swatch, immersed in boiling water for 20 minutes, and then removed and allowed to dry. After this test, the image quality was tested at 650 nm. For the humidity test, the printed sample was exposed to a temperature of 40°C at 90% relative humidity for 24 hours. After this test, the image quality was tested at both 650 nm and 670 nm. For the sunlight test, the printed sample was placed in an accelerated sunlight test chamber (Q-Sun™ Xenon Test Chamber, sold by Q-Lab Corporation, Westlake, OH) at an irradiance of 0.67 W / m2 for 7 hours and then removed. Following this test, the image quality was tested at both 650 nm and 670 nm. For the sanitizer test, a drop of Purell™ hand sanitizer, sold by Gojo Industries, was placed on the printed sample and allowed to dry. After this test, the image quality was tested at both 650 nm and 670 nm. The results of some of these test runs, the initial print quality test and the print quality test after each of the environmental tests described above are reported in Table 5: Table 5 Table 5 CE1ODB2DPU1,3best.best.nbnbnbnbbest.nb CE2ODB2UU1,3n.bnbnbnbnbnbnbnb CE3BK305DPU1,3best.best.n.b.n.b.n.b.n.b.best.n.b. CE4BK305UU1,3n.b.n.b.n.b.n.b.n.b.n.b.n.b.n.b. Bsp. 1ODB21:1 DPU / UU1,3best.best.best.best.best.best.best.best. Bsp. 2BK3051:1 DPU / UU1,3best.best.best.best.best.best.best.best. Bsp. 3BK3051:3 DPU / UU1,3best.best.best.n.b.best.best.*best.*best.* Bsp. 4BK3053:1 DPU / UU1,3best.best.n.b.n.b.best.best.*best.n.b. Bsp. 5ODB21:1 DPU / UU1,1best.best.best.best.best.best.best.best. Bsp. 6ODB21:1 DPU / UU0,9best.best.best.n.b.best.best.best.n.b. In this table, a "pass" result refers to an ANSI value at 650 nm (and, where applicable, 670 nm) of at least 1.5; a "pass*" result refers to an ANSI value at 650 nm of at least 1.5 but an ANSI value at 670 nm of less than 1.5; and a "fail" result refers to an ANSI value at 650 nm (and, where applicable, 670 nm) of less than 1.5. A comparison of Comparative Examples 1-4 with Examples 1-6 in the table demonstrates that the new developer chemistry combination of DPU and UU produces a multipurpose direct thermal recording material capable of passing several environmental impact tests, but when used in an otherwise identical thermal recording material, it fails some of the environmental impact tests. The Comparative Examples using UU as such result in direct thermal recording materials that produce an image that does not even meet the minimum requirements for machine readability of barcodes. The results of Table 5 show that the relative weight ratio of DPU to UU in the thermally responsive layer need not be 1, but may vary at least from 1 / 3 to 3, as well as within narrower ranges such as 1 / 2 to 2. The results of Table 5 further show that the coating weight of the thermally responsive layer, when DPU and UU are used in combination, can be as low as 0.9 g / m2 and still produce direct thermal images with acceptable print quality. The results of the remaining comparative examples are shown in Table 6, where "Best.", "Best*" and "nb" have the same meaning as in Table 5: Table 6 Table 6 CE5ODB2D-81,3best.best.nbnbbest.best.best.nb CE6ODB2BPS1,3best.best.nbnbbest.best.best.nb CE7ODB2BPS-MBE1,3best.best.nbnbbest.best.best.*nb CE8ODB2Perg1,3best.best.nbnbbest.best.best.*nb CE9ODB2NKK1,3best.best.n.b.n.b.best.best.best.n.b. CE10ODB21:1 Tol / Dap s1,3n.b.n.b.n.b.n.b.n.b.n.b.n.b.n.b. CE11ODB21:1 DPU / Pe rg1,3best.best.n.b.n.b.best.n.b.best.n.b. CE12ODB21:1 DPU:NK K1,3best.best.n.b.n.b.best.best.best.n.b. Unless otherwise indicated, all numerical terms expressing quantities, measured properties, and so forth in the specification and claims are to be understood as modified with the term "about." Accordingly, unless otherwise indicated, the numerical parameters as recited in the specification and claims are approximations that may vary depending on the desired properties sought by those skilled in the art employing the teachings of the present application. In order not to limit the application of the doctrine of equivalents to the claims, each numerical parameter should be interpreted at least in light of the number of significant decimal places recited and by applying standard rounding techniques.Although the numerical ranges and parameters indicating the broad scope of the invention are approximate, all numerical values given in the specific examples described herein are as accurate as reasonably possible. However, each numerical value could contain errors related to testing or measurement limits. The use of relational terms such as "top," "bottom," "upper," "lower," "above," "below," and the like to describe various embodiments is used merely for convenience in describing some of the embodiments. Despite the use of these terms, the present disclosure should not be construed as being limited to any particular orientation or relative position, but should be understood to include embodiments having any orientation and relative position in addition to those noted above. Various modifications and alterations will be apparent to those skilled in the art without departing from the spirit and scope of the present invention, which is not limited to the illustrative embodiments described herein. The reader should assume that features of one disclosed embodiment may be applied to all other disclosed embodiments unless otherwise indicated. In summary, non-phenolic direct thermal recording media feature a thermally responsive layer containing a leuco dye and several non-phenolic developers, including 1,3-diphenylurea (DPU) and ureaurethane (UU). This chemistry enables multipurpose recording materials capable of withstanding several different types of environmental exposures or agents—such as immersion in water, contact with polyvinyl chloride meat wrap, boiling water, dry and moist heat, and contact with hand sanitizer. The unique non-phenolic chemistry allows the product's thermally responsive layer to have an ultra-low coating weight of less than 1.48 g / m². QUOTES CONTAINED IN THE DESCRIPTION This list of documents submitted by the applicant was generated automatically and is included solely for the convenience of the reader. This list is not part of the German patent or utility model application. The DPMA assumes no liability for any errors or omissions. Cited patent literature US 3539375 [0003, 0026]US 3674535 [0003, 0026]US 3746675 [0003, 0026]US 4151748 [0003, 0026]US 4181771 [0003, 0026]US 4246318 [0003, 0026]US 4470057 [0003, 0026]US 5955398

[0026] US 4531140

[0034] US 4794102

[0034] US 5098882

[0034] US 6835691

[0034] US 6921740

[0034]

Claims

A recording medium (104), comprising: a substrate; and a thermally responsive layer (114) carried by the substrate, wherein the thermally responsive layer (114) includes a leuco dye and a plurality of developers; wherein the recording medium (104) is substantially phenol-free; and wherein the plurality of developers includes 1,3-diphenylurea (DPU) and ureaurethane (UU). The recording medium (104) of claim 1, further comprising:a base coating (112) between the thermally responsive layer (114) and the substrate (110). Recording medium (104) according to claim 1 or 2, further comprising:a top layer (116) carried by the substrate (110) such that the thermally responsive layer (114) is disposed between the top layer (116) and the substrate (110). Recording medium (104) according to one of claims 1 to 3, wherein the thermally responsive layer (114) has a coating weight of less than 1.48 g / m2. Recording medium (104) according to one of claims 1 to 4, wherein the coating weight of the thermally responsive layer (114) is at least 0.9 g / m2. Recording medium (104) according to one of claims 1 to 5, wherein the DPU and the UU are distributed throughout the thermally responsive layer (114). Recording medium (104) according to one of the claims 1 to 6, wherein substantially no developers other than DPU and UU are present in the thermally responsive layer (114). Recording medium (104) according to one of claims 1 to 7, wherein the DPU and the UU are present in the thermally responsive layer (114) in a relative weight proportion falling within a range of 1 / 3 to 3. Recording medium (104) according to claim 8, wherein the relative weight proportion falls within a range of 1 / 2 to 2. Recording medium (104) according to claim 9, wherein the relative weight fraction is 1. The recording medium (104) according to any one of claims 1 to 10, wherein a print quality of the recording medium (104) when printed with a thermal printer energy setting of 11.7 mJ / mm2 at a print speed of 15 cm (6 inches) per second is characterized by an ANSI value of at least 1.

5. Recording medium (104) according to claim 11, wherein the print quality of the recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been soaked with water for 24 hours and then removed and dried. The recording medium (104) according to claim 11, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium has been immersed in water and then brought into contact with a polyvinyl chloride meat wrapping film under a weight of 3.2 kg (7 pounds) for 24 hours, and then removed and dried. Recording medium (104) according to claim 11, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been immersed in boiling water for 20 minutes, then removed and dried. Recording medium (104) according to claim 11, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been heated to 60°C for 24 hours, then removed and cooled. Recording medium (104) according to claim 11, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been exposed to air at 40°C and 90% relative humidity for 24 hours, then removed and cooled. The recording medium (104) according to claim 11, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been subjected to an accelerated sunlight test at 0.67 W / m2 for 7 hours. The recording medium (104) according to claim 11, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after a drop of a 70% ethyl alcohol-based hand cleaner has been applied to the printed recording medium (104) and then allowed to dry. The recording medium according to claim 1, wherein the recording medium is substantially phenol-free; wherein the substrate is flexible; wherein the DPU and the UU are both distributed throughout the thermally responsive layer (114); wherein the DPU and the UU are present in a relative weight fraction in the thermally responsive layer (114) that falls within a range of 1 / 3 to 3; and wherein a print quality of the recording medium (104), when printed with a thermal printer energy setting of 11.7 mJ / mm2 at a print speed of 15 cm (6 inches) per second, is characterized by an ANSI value of at least 1.

5. A recording medium according to claim 19, wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been immersed in water and then brought into contact with a polyvinyl chloride meat wrapping film under a weight of 3.2 kg (7 pounds) for 24 hours, and then removed and dried; wherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been heated to 60°C for 24 hours, and then removed and cooled; andwherein the print quality of the printed recording medium (104) is still characterized by an ANSI value of at least 1.5 after the printed recording medium (104) has been exposed to air at 40°C and 90% relative humidity for 24 hours, then removed and cooled.

Citation Information

Patent Citations

  • Thermo-responsive record sheet

    US3539375A

  • Heat-sensitive record material

    US3674535A

  • Heat sensitive record material

    US3746675A

  • Two color thermally sensitive record material system

    US4151748A

  • Thermally responsive record material

    US4181771A