METHOD FOR REPAIRING A PART DURING ADDITIVE MANUFACTURING

DE602020040800T2Inactive Publication Date: 2024-11-06INST DE RECH TECHQUE JULES VERNE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602020040800
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-05-23
Filing Date
2020-05-19
Publication Date
2024-11-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Additive manufacturing processes often result in defective parts due to material shortages, leading to scrapage and wasted time and expensive materials, as existing methods do not effectively monitor and repair defects in real-time during the manufacturing process.

Method used

A method for repairing parts additively manufactured layer by layer, involving the detection and repair of material defects by adding material during the process, using a scanning tool to identify and geolocate defects and a secondary nozzle to fill in missing material, allowing for continuous monitoring and correction as each layer is formed.

Benefits of technology

This approach enables the real-time detection and repair of material defects, reducing the number of scrapped parts and saving time and material by allowing for the identification and correction of defects during the manufacturing process, thereby improving the efficiency and quality of additive manufacturing.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a method for repairing a part during additive manufacturing layer by layer. Domaine technique

[0002] In the field of additive manufacturing, particularly but not exclusively fused filament extrusion, also known as FDM for Fused Deposition Modeling, parts produced layer by layer can present defects generated for example during the process.

[0003] Additive manufacturing processes are generally lengthy, and the finished part may prove defective during final inspection and therefore be discarded. The material used is then wasted, although it is generally expensive. In addition, the process time used to produce the part is lost. It may therefore be advantageous to carry out inspections of the part as it is manufactured.

[0004] US 2019 / 0009472 discloses a method for controlling a 3D printed part using a 3D printer.

[0005] US 2016 / 129633 relates to a 3D printing apparatus and method stacking a plurality of layers. A printing module sprays a material in liquid form onto a platform. A curing module hardens the liquid material present on the platform to form a layer. A detection module is configured to detect the profile of the surface of the formed layer. A control module receives the profile signal and controls the printing module and the curing module according to the detected profile to correct the surface of the formed layer.

[0006] US2017298580 provides mobile and automated processing using additive manufacturing. EP3459716 describes a method and system for online monitoring of three-dimensional printing.

[0007] There is a need to improve existing additive manufacturing processes. Exposé de l'invention

[0008] The present invention thus relates, according to a first of its aspects, to a method for repairing a part during additive manufacturing layer by layer with an additive manufacturing machine, comprising the following steps: a) depositing at least one layer of material on a support for the manufacture of the part, b) detecting at least one lack of material defect, if one or more defects of this type are present on said at least one layer, c) repairing said at least one lack of material defect by adding material, d) repeating steps a), b) and possibly c) until the part is produced.

[0009] Thanks to the invention, an additive manufacturing process is available which makes it possible to repair, during additive manufacturing, any detected material shortage defects. It is possible to monitor the material shortage defects of the part and repair the material shortage defect(s) by adding material, during manufacturing of the part, at the appropriate location.

[0010] Preferably, a single layer of material is deposited in step a) and step b) is carried out for this layer after its deposition. Thus, material deficiency defects can be monitored layer by layer as the part is built.

[0011] Alternatively, several layers of material are deposited in step a) before carrying out step b).

[0012] In another variant, steps a) and b) are nested, with detection being carried out as material is deposited to form a layer.

[0013] Similarly, repair step c) can be carried out after each layer has been completed. Alternatively, it is carried out after several layers have been completed.

[0014] Step a) of depositing said at least one layer of material is for example carried out using a nozzle fixed to a carriage, in particular of the additive manufacturing machine, said carriage being movable along at least two axes, preferably three orthogonal axes, relative to the support.

[0015] The material added in step c) may be different from the material deposited for each layer in step a), preferably being more fluid. It is preferably compatible. It may be of the same nature. Alternatively, the material added in repair step c) is identical to the material deposited for each layer in step a).

[0016] Step c) of repairing said at least one lack of material defect can be carried out by the nozzle. Alternatively, step c) of repairing said at least one lack of material defect is carried out by a second nozzle. Such a second nozzle is preferably present on the additive manufacturing machine, preferably close to the nozzle, which then becomes the main nozzle.

[0017] In this case, the second nozzle preferably has a diameter smaller than that of the main nozzle, in particular to fill small areas corresponding to material shortage defects.

[0018] The repair of one or more material shortage defects may consist of depositing material in the area(s) where said defect(s) have been detected, in a quantity which is determined to fill said defect(s). In this case, in addition to the detection of said defect(s) and a possible acquisition of relative topographical data, the method may comprise the step of calculating the quantity of material to be deposited in each given area, identified, with a material shortage defect.

[0019] Repairing missing material defects by adding material, particularly using a second nozzle, can be particularly advantageous for large parts. To manufacture large parts, the dimensions of the deposit are generally increased, both in width and height. Increasing the width can cause the trajectory to not fill all areas correctly. Adding material to the missing areas, particularly by using a second nozzle, can fill these unwanted holes.

[0020] Step b) of detecting at least one lack of material defect comprises the step of scanning said at least one layer, deposited in step a), to acquire topographical data on said at least one layer, and the step of processing the acquired data to detect and geolocate at least one lack of material defect, if one or more defects of this type are present on said at least one layer.

[0021] The scanning step is implemented using a profilometer, in particular a laser profilometer.

[0022] The additive manufacturing machine comprises an enclosure, in particular a closed and possibly heated enclosure, with the part support present in the enclosure. The nozzle advantageously opens into the enclosure. If present, the second nozzle also advantageously opens into the enclosure.

[0023] The additive manufacturing machine comprises an enclosure, the profilometer, is arranged outside the enclosure and the scanning step b) can be implemented by the profilometer through a portion of wall transparent to the wavelength of the profilometer, in the visible range, between 380 nm and 800 nm. The transparent wall portion forms at least part of a wall defining the enclosure. The transparent wall portion can constitute a glazed wall.

[0024] The scanning tool is preferably non-intrusive, being outside the room.

[0025] The scanning tool, in particular the profilometer, is preferably fixed relative to the carriage, in particular being fixed near the nozzle. The carriage may form part of a wall defining the enclosure and / or be mounted on such a wall.

[0026] The carriage that connects the nozzle and the scanning tool, particularly the profilometer, can be mobile or fixed. In the latter case, the support for manufacturing the part is advantageously mobile along at least two axes (X, Y), or even three orthogonal axes (X, Y, Z). This relative mobility of the carriage and / or the support makes it possible to deposit the material at the location intended for the construction of each layer of the part.

[0027] The additive manufacturing process, also called additive manufacturing, can be a material extrusion printing process, also called "material extrusion" in English, which includes in particular Fused Deposition Modeling (FDM) or Fused Filament Fabrication (FFF) technologies, 3D printing by binder jetting, also called "binder jetting" in English, which includes in particular Drop-On-Demand (DOD) technology, 3D printing by powder bed fusion, also called "powder bed fusion" in English, which includes in particular Selective Laser Sintering (SLS) and Selective Fusion (SLM) technologies, 3D printing by material jetting, 3D printing by Directed Energy Deposition, 3D printing by vat photopolymerization, also called "Vat Photopolymerization" in English, which includes in particular stereolithography (SLA) technology.The process can also be a mixture of these different technologies such as Multi Jet Fusion (MJF) technology which combines binder jetting and powder bed fusion. The additive manufacturing method of the part is preferably FDM or FFF.

[0028] The material used for additive manufacturing and / or the material added in step c) of repair is preferably a polymer, in particular a thermoplastic chosen for example from the group consisting of PAEK (Polyaryletherketone) which includes PEEK (polyetheretherketone) and PEKK (polyetherketoneketone), PEI (Polyetherimide also known as ULTEM), PPS (Polyphenylene sulfide), ABS (acrylonitrile butadiene styrene), PA (polyamide), PP (polypropylene), PLA (polylactic acid), TPU (thermoplastic polyurethane) and PET (polyethylene).

[0029] The polymer can be amorphous and / or semi-crystalline, charged or not.

[0030] The polymer may be filled with fibers, including carbon / glass fibers, mineral, metallic or vegetable filler, including glass beads, wood, or be unfilled.

[0031] Pairs of materials, in particular compatible ones, which can be used can be established, one of the materials being able to be deposited in step a) and the other of the materials being able to be deposited in step c) of repairing one or more material shortage defects.

[0032] Thus, in the case of materials of the PEKK family, in one example, the nozzle extrudes and deposits a polymer thread of type PEKK 6003, while, for the repair in step c), the second nozzle extrudes and deposits a more fluid polymer of type PEKK 6004. In another example, the nozzle extrudes and deposits a polymer thread filled with carbon fibers of type PEKK 6004 CF, while, for the repair in step c), the second nozzle extrudes and deposits an unfilled polymer of type PEKK 6004. Alternatively, the same material, for example PEKK 6004 CF, can be deposited by both nozzles or by the nozzle.

[0033] Step a) is preferably carried out by deposition of extruded polymer wire. Step c) is preferably carried out by deposition of extruded polymer wire.

[0034] The method may include a step prior to the first implementation of step a), consisting of scanning the support intended to receive the part during its manufacture, before depositing the first layer of the part. This makes it possible to take a reference for the subsequent manufacture of the part.

[0035] Step b) of detecting at least one lack of material defect can make it possible, in particular by scanning, to acquire data which can include the three-dimensional coordinates of the deposited and scanned layer.

[0036] The processing of acquired data, in particular by scanning, may include, from the acquired data, the analysis of at least one global quantity in order to monitor the additive manufacturing, layer by layer. The global quantity is preferably chosen from a thickness of the deposited layer, a standard deviation of the thickness of the deposited layer, a quantity of material deposited for the layer, a movement of the carriage at each deposited layer, the average width of the deposited wire beads and its standard deviation when the additive manufacturing is carried out by deposition of extruded polymer wire, the average roughness, in particular with the parameter Ra (arithmetic mean height of a line) or Sa (arithmetic mean height of a surface) and the geometric dimensions of the deposited layer.

[0037] The data acquired, particularly by scanning, can be used to identify areas of material deficiency, to control the geometry of the material deposit in each layer, to control roughness between layers, to know the void rate within a layer, several layers or the part.

[0038] The method may include a prior step of parameterizing the additive manufacturing machine for carrying out step a) with setpoint parameters and on the basis of reference geometric data of the part and / or of each layer of the part, stored in a memory.

[0039] In this case, the processing of the acquired data, in particular by scanning, advantageously includes a comparison of the acquired data with the set parameters and a detection of possible deviations between the acquired data and the set parameters.

[0040] Still in this case, the data processing may include a comparison of the acquired data, in particular by scanning, with the stored reference geometric data, in order to detect an average deviation of the contour of the part compared to the reference geometric data, and / or an average deviation compared to the deposition trajectories of the material constituting the part.

[0041] Indeed, the acquired data can make it possible to recognize the contours of the layer, layers or the manufactured part and thus to reconstruct the part actually manufactured, layer by layer, and compare it to the initial reference data. This can make it possible to carry out quality control and to accept or not the part from a dimensional point of view or to allow the implementation of step c) of repair.

[0042] The deposition trajectories of the material constituting the part can correspond, when the additive manufacturing is a deposition of extruded polymer wire, to the trajectories of the nozzle, which is for example controlled by numerical control programming.

[0043] The processing of the acquired data, in particular by scanning, may include the determination of the surface dimension and depth of each material defect. When the surface dimension and depth of a material defect are respectively greater than predetermined threshold values ​​of surface dimension and depth, data on this defect may be recorded, this data including in particular the coordinates, the surface dimension and the depth of the defect.

[0044] The predetermined threshold value for surface dimension is for example 5µm * 5µm, or even greater than 5µm * 5µm, for example equal to 50µm * 50µm. The predetermined threshold value for depth may be 10µm, or even greater than 10µm, for example equal to 100µm.

[0045] If it is determined, by data processing, that repair is undesirable or impossible, for example due to the presence of a number of defects greater than a predetermined threshold value and / or due to the presence of at least one defect of dimensions greater than a predetermined threshold value, the method may include scrapping the part, even if unfinished, the threshold values ​​being predetermined for a given part.

[0046] This saves process time and material that would otherwise be used to finish the part. This is because the process takes a relatively long time to implement, lasting several hours, and the material, particularly polymer, used is relatively expensive. The savings made, when a part has a major defect or a set of defects that make it non-compliant with the expected quality level, can be substantial if it can be scrapped as soon as its non-compliance is determined during manufacturing.

[0047] After a repair has been made, the method may include the step of performing a scan of the repaired layer. This makes it possible to verify that the material defect(s) are repaired satisfactorily. If this is not the case, a new repair step c) may be carried out based on the acquired and analyzed data. If the repair is deemed satisfactory, a new layer may be deposited in a new step a). Machine de fabrication additive

[0048] The invention also relates, according to another of its aspects, in combination with the above, to an additive manufacturing machine for implementing the method as defined above, the additive manufacturing preferably being printing by extrusion of material (FDM, FFF), the machine comprising: a support for the part to be manufactured, at least one coil of polymer wire, at least one nozzle for extruding and depositing the wire in order to form the part, a carriage on which the nozzle is fixed and possibly a second nozzle, at least one of the carriage and the support being movable along at least two axes, in particular three axes, relative to the other, said at least one nozzle being used for repairing material shortage defects or the machine comprising a second nozzle for repairing material shortage defects, the second nozzle preferably having a diameter smaller than that of the nozzle.

[0049] The additive manufacturing machine preferably comprises a scanning tool chosen from the group consisting of a profilometer, in particular an optical, camera or laser profilometer, preferably a laser profilometer, a distance sensor, a camera, a mechanical profilometer and a 3D scanner, preferably by structured light projection, preferably a profilometer, capable of scanning the part.

[0050] The additive manufacturing machine comprises an enclosure, in particular a closed one. In this case, the support is in the enclosure, and the profilometer is outside the enclosure, the nozzle, and the possible second nozzle, opening into the enclosure. The carriage may form all or part of a wall of the enclosure, and / or be integral with such a wall.

[0051] The enclosure may or may not be heated, and its heating temperature, if any, may vary depending on the materials used for additive manufacturing (or materials). For some materials, it is preferable to have it heated. However, some materials do not require a heated enclosure.

[0052] The heating temperature of the enclosure is, for example, defined according to the Tg (glass transition temperature) of the material used for additive manufacturing. For example, for ABS, the enclosure can be heated to a temperature between 50°C and 100°C. For PEKK, the enclosure temperature will be approximately 150°C.

[0053] The heating temperature of the enclosure can reach up to 250°C.

[0054] The enclosure can in particular be heated to avoid deformations caused by excessively large temperature gradients in the part during its manufacture.

[0055] The additive manufacturing machine comprises a wall, forming part of a wall of the enclosure, transparent to the wavelength of the profilometer, arranged so as to allow scanning by the profilometer of at least part of the part through this wall. Brève description des dessins

[0056] The invention may be better understood by reading the detailed description which follows, non-limiting examples of its implementation, and by examining the attached drawing, in which: [ Fig 1 ] there figure 1 schematically represents an example of an additive manufacturing machine according to the invention, [ Fig 2 ] there figure 2 represents in block diagram the steps of a particular implementation of the additive manufacturing process, [ Fig 3 ] there figure 3 is a schematic view of an example of a part produced using the additive manufacturing process described with respect to the figure 2 , [ Fig 4 ] there figure 4 is a graph of data from the scanning step in the implementation of the process for several parts according to the figure 3 , [ Fig 5 ] there figure 5 is a graph of data from the scanning step in the implementation of the process for several parts according to the figure 3 , [ Fig 6 ] there figure 6 is a graph of data from the scanning step in the implementation of the process for several parts according to the figure 3 , [ Fig 7 ] there figure 7 is a graph of data from the scanning step in the implementation of the process for several parts according to the figure 3 , [ Fig 8 ] there figure 8 includes several schematic images resulting from the processing of data from the scanning step, for different layers of the part of the figure 3 , during the implementation of the method according to the invention, [ Fig 9 ] there figure 9 is an enlarged photograph illustrating a portion of the room of the figure 3 , [ Fig 10 ] there figure 10 represents in block diagram the steps of an example of implementation of the method for repairing a part during additive manufacturing according to the invention, and [ Fig 11 ] there figure 11 schematically represents an example of an additive manufacturing machine according to the invention for implementing the method illustrated in the figure 10 , And [ Fig 12 ] there figure 12 schematically represents the result of the scan of an example of a part to be repaired using the method according to the invention. Description détaillée

[0057] It has been illustrated at the figure 1 an additive manufacturing machine 1 to produce a part P layer by layer and allow the repair of any defects due to lack of material. In the example illustrated, the additive manufacturing technique is a fused filament deposition process, a technology called FDM, or FFF.

[0058] The machine 1 comprises a cabinet 10 shown in dotted lines in this figure. The machine 1 comprises, housed in the cabinet 10, a support 2 for the part P to be manufactured, at least one spool 3 of wire 4 made of polymer material, a nozzle 5 for the extrusion and deposition of the wire 4 in order to form the part P, a carriage 6 on which the nozzle 5 is fixed.

[0059] At least one of the carriage 6 and the support 2 is movable along at least two axes X, Y, in this example along three axes X, Y and Z, relative to the other. In the example illustrated, the carriage 6 is movable relative to the support 2, but it does not go beyond the scope of the invention if it is the support 2 which is movable and the carriage 6 which is fixed, or if both, carriage 6 and support 2, are movable relative to each other.

[0060] Machine 1 also includes a scanning tool consisting, according to the invention, of a profilometer 7, in this example a laser, in particular of class 2, fixed relative to carriage 6. Profilometer 7 makes it possible to scan part P and to acquire topographic data of part P, layer by layer for example. The profilometer chosen in this example has an observation zone 39 mm wide, to obtain a resolution of 0.05 mm. The measuring head of the profilometer can be changed to enlarge the scanned width, which goes in the direction of a reduction in resolution, or to reduce it, in order to increase the resolution. To scan a part whose dimensions are larger than the measured width, several passes are made.

[0061] Machine 1 comprises, in cabinet 10, a closed enclosure 11. In this example, enclosure 11 is heated to a temperature of approximately 150°C for a material used for additive manufacturing consisting of PEKK. Enclosure 11 contains support 2 which carries part P, here shown with several layers C deposited. Profilometer 7 is located outside enclosure 11, in a space 13 of machine 1 which is temperature-regulated. The machine 1 comprises a wall portion 12 transparent to the wavelength of the profilometer 7, arranged so as to allow scanning by the profilometer 7 of at least a part of the part P through this wall portion 12. The wall portion 12 can be secured to the carriage 6 on which the nozzle 5 and the profilometer 7 are fixed. The nozzle 5 opens into the enclosure 11 for the deposition of material in order to manufacture the part layer by layer.

[0062] The machine 1 also comprises a computer system 15 connected at least to the profilometer 7 in order to collect data from it, to the coil 3 to control the deposition of material and to the carriage 6 so as to control the movement in X, Y and Z thereof. Alternatively, the computer system 15 connected to the profilometer 7 is not the same as that which controls the machine 1, but these two computer systems can communicate with each other when necessary, for example in the event of a machine stoppage.

[0063] The additive manufacturing machine 1 can be used to implement the additive manufacturing process which will be described with reference to the figure 2 which illustrates the stages.

[0064] The additive manufacturing method of the part P comprises a first step 20 comprising the scanning, using the profilometer 7, of the support 2, before deposition of the first layer C of the part P. This measurement is carried out to obtain a reference distance between the profilometer and the support; this is a calibration step. This acquisition of data relating to the support 2 may be omitted in an alternative implementation of the invention.

[0065] A first layer of the part P is then produced by depositing an extruded wire of polymer material using the nozzle 5, in a step 21. The carriage 6 is moved relative to the support 2 to deposit the material at the desired location.

[0066] In a step 22, the first layer C of the part P which was deposited in step 21 is scanned, using the profilometer 7, through the transparent wall 12. The beam F is visible on the figure 1 The carriage 6 can be moved relative to the support 2 to perform the scan.

[0067] In a step 23, the acquired data is processed to detect and geolocate at least one material defect, if one or more defects of this type are present, in particular on the first layer C deposited in step 21.

[0068] As illustrated, steps 21 and 22 can be carried out several times before implementing step 23. Steps 21 and 22 can, additionally or alternatively, as illustrated, be repeated after implementing step 23 until all the layers of part P have been produced.

[0069] In one variant, step 21 consists of depositing not one but several C layers before performing the scanning step 22. In another variant, the scanning of step 22 is performed as soon as the material is deposited, before producing the entire C layer, as it is deposited.

[0070] The scan performed in step 22 allows topographic data of the deposited C layer to be acquired. The X, Y and Z coordinates of the upper C layer of the part being manufactured, the layer that has just been deposited, for example, can be obtained.

[0071] The data processing step 23 includes, in particular, from the acquired data, the analysis of one or more global quantities in order to monitor the additive manufacturing process, layer by layer. Among the global quantities analyzed, mention may be made of a thickness of the deposited layer C, a standard deviation of the thickness of the deposited layer C, a quantity of material deposited for the layer C and a movement of the carriage 6 and / or of the support at each deposited layer C, an average roughness, an average width of the deposited wire beads.

[0072] During step 20, in the example illustrated, the parameterization of the additive manufacturing machine 1 is also carried out for carrying out step 21 with setpoint parameters and on the basis of reference geometric data of the part P and / or of each layer C of the part P, stored in a memory of the computer system 15.

[0073] Processing step 23 includes a comparison of the data acquired in step 22 with the setpoint parameters and a detection of possible deviations between the acquired data and the setpoint parameters.

[0074] The processing step 23 further comprises a comparison of the data acquired in step 22 with the stored reference geometric data, in order to detect an average deviation of the contour of the part P with respect to the reference geometric data and / or an average deviation with respect to the material deposition trajectories constituting the part P, programmed upstream of the manufacturing. Step 23 also comprises the determination of the surface dimension and the depth of each detected lack of material defect and, when the surface dimension and the depth of a lack of material defect are respectively greater than predetermined threshold values ​​of surface dimension and depth, the recording of the data on this defect, this data comprising in particular the coordinates, the surface dimension and the depth of the defect.

[0075] The predetermined threshold value of surface dimension is in the illustrated example 50µm * 50µm and the predetermined threshold value of depth is 100µm.

[0076] After implementing a data processing step 23, a question Q1 is answered on the presence of a number of defects greater than a predetermined threshold value and / or the presence of at least one defect with dimensions greater than a predetermined threshold value, the threshold values ​​being predetermined for a given part P. If the answer to question Q1 is that there is a number of defects greater than the predetermined threshold value and / or the presence of at least one defect with dimensions greater than the predetermined threshold value, NOK on the diagram of the figure 2 , then the process leads to step 24 of scrapping the unfinished part P. Otherwise, OK on the diagram of the figure 2 , part P is finished, by repeating steps 21 and 22.

[0077] At the end of the production of part P, a question Q2 similar to question Q1 is asked. If the answer to question Q2 is that there is a number of defects greater than the predetermined threshold value and / or the presence of at least one defect with dimensions greater than the predetermined threshold value, NOK on the diagram of the figure 2 , then the process leads to step 24 of scrapping the unfinished part P. Otherwise, OK on the diagram of the figure 2 , the completed part P is validated in a step 25.

[0078] The control carried out during manufacturing according to this process is a form of non-destructive testing, also called NDT, but which takes place throughout manufacturing unlike the usual non-destructive testing which is carried out on the finished part. This step of the usual non-destructive testing on the finished part is thus not necessary, thanks to the invention, which makes it possible on the one hand to save this usual final step and on the other hand not to have to invest in the NDT system allowing it to be implemented, a system which is generally expensive.

[0079] It has been represented on the figure 3 a part P, consisting of a tensile test piece, produced using the process described with respect to the figure 2 , implemented by additive manufacturing machine 1.

[0080] Three parts P consisting of tensile test pieces respectively named Ep_A, Ep_B and Ep_C on the model of part P illustrated on the figure 3 were carried out with machine 1 and the implementation of the additive manufacturing process described above, with the same parameters and setpoint values.

[0081] There figure 8 illustrates several of the scanned C layers of specimen Ep_C. Image 8A illustrates the second layer deposited and scanned, image 8B represents the third layer, image 8C the fourth layer, image 8D the fifth layer, image 8E the sixth layer, image 8F the seventh layer, image 8G the twelfth layer and image 8H the thirteenth layer. Images 8B to 8H show a circled area with at least one visible defect of lack of material.

[0082] THE figures 4 à 7 illustrate graphs representing at least part of the result of processing data acquired on part P during its manufacture, after deposition of each layer C, by scan, for each of the test pieces Ep_A, Ep_B and Ep_C.

[0083] The graph of the figure 4 represents the volume V expressed in mm 3< as a function of the rank n of each layer C. The graph of the figure 5 illustrates the average height H per layer, expressed in mm, as a function of the rank n of each layer C. The graph of the figure 6 illustrates the displacement of the carriage, Dp, expressed in mm, as a function of the rank n of each layer C. The graph of the figure 7 represents the standard deviation of the layer height, Dev, expressed in mm, as a function of the rank n of each layer C. Rank n corresponds to the number of the layer C deposited. The first layer deposited has rank 1, the second layer, deposited on the first layer, has rank 2, etc., up to the highest rank which corresponds to the last layer deposited for the production of the part P. On the graphs of the figures 4 à 7 , the values ​​illustrated for specimen Ep_A are small squares, those for specimen Ep_B are small circles, and those for specimen Ep_C are small triangles.

[0084] We visualize on the figures 5 And 7 outliers for specimen Ep_C, circled on the graphs, which shows a layer height defect and a very large standard deviation, also visible on the figure 8 , as indicated above.

[0085] A portion of part P has been illustrated on the figure 9 to represent the detection of defects D, identified by small crosses in this figure, of lack of material. When defects of the lack of material type are located by scanning and processing of the scan data, they are compared to threshold values, for example dimensions greater than 5µm * 5µm and depth greater than 10µm. When a defect has a size greater than at least one of the threshold values, its coordinates are recorded as well as its size (on the surface) and its depth. This can allow decisions to be made regarding the retention and further manufacture of the part P or its scrapping.

[0086] It has been represented on the figure 10 an example of implementation of the method for repairing a part during additive manufacturing according to the invention. In this example, the method may comprise the same steps as those illustrated in the method illustrated in the figure 2 , but also includes, according to the invention, a step of repairing defect(s) of lack of material as will be explained below.

[0087] Indeed, as illustrated in this figure, when the answer to question Q1 or question Q2 is NOK, a question Q3 on the possibility of repairing the lack of material defect(s) is asked. If the answer to this question Q3 is yes, then OK on the diagram, the layer C concerned by the defect and / or the part P is repaired by adding material in a step 26. On the other hand, if the answer to this question Q3 is no, then NOK on the diagram, the part, finished or not, is scrapped.

[0088] It should be noted that in the present invention the data acquired by scanning can be classified into two categories allowing two types of analysis. On the one hand, the overall quantities per layer, mentioned above, can be acquired and analyzed, in particular compared to the reference values ​​and setpoint values, to monitor the additive manufacturing process. On the other hand, material shortage defects, in particular those that can be corrected, can be detected and geolocated to be treated and repaired by adding material.

[0089] For the implementation of the method according to the invention illustrated in the figure 10 , we can use the additive manufacturing machine 1 illustrated on the figure 11 which comprises a second nozzle 16 supplied with a second wire 17 of polymer material by a second coil 18. The second wire 17 is made, in the example illustrated, of a more fluid polymer material than the wire 4. The second nozzle 16 has a smaller diameter than the nozzle 5. The second nozzle 16 and the wire 17 are used for repairing defects due to lack of material.

[0090] For the implementation of the method according to the invention illustrated in the figure 10 , one can also use the additive manufacturing machine 1 illustrated on the figure 2 , nozzle 5 and wire 4 can then be used to repair material shortage defects.

[0091] If necessary, the defect(s) due to lack of material can be repaired after the creation of a layer, or several layers, or even during the creation of a layer not entirely deposited on the previous one or on the support 2. When the repair is carried out after the creation of a layer, a new layer can then be deposited on top, then the scan carried out, then the data processing and a possible new repair, and so on until the part is created.

[0092] Furthermore, when one or more material defect(s) is / are repaired, a scan can be performed to verify the repair. If it is satisfactory, the next layer can be deposited. If the repair is not satisfactory, the defect(s) can be repaired again, before verifying by scanning and / or depositing a new layer.

[0093] It has been represented on the figure 12, schematically, a layer of a part viewed after its deposition, scanning and data processing. The contour R of the part is visible. We also visualize the filling I of the layer which is inside the contour R and we detect areas with defects D of lack of material between the contour R and the filling I, at their junction. It should be noted that a certain overlap between the two areas R and I can make it possible to fill some of these defects, but, as visible in this figure, certain defects D of lack of material remain and are to be repaired thanks to the invention. We cannot carry out too much overlap, during the deposition of material, because this can cause degradation of the surface.

[0094] An advantage of the invention is that it allows for the repair of a defective area due to a lack of material during the manufacture of the part. Another advantage is that the porosity can be reduced in the overlapping areas between the contour and the filling. Another advantage is that it allows for the limitation of the number of parts discarded because they have too many lack of material defects or one or more lack of material defects that are too large.

[0095] The invention is not limited to the examples just described, but is defined by the subject matter of the claims.

[0096] In particular, the additive manufacturing process may be other than FDM technology.

[0097] In particular, the additive manufacturing process may consist of 3D printing by binder jetting, which includes Drop-On-Demand (DOD) technology, 3D printing by powder bed fusion, which includes selective laser sintering (SLS) and selective melting (SLM) technologies, 3D printing by material jetting, 3D printing by directed energy deposition, and 3D printing by vat photopolymerization, which includes stereolithography (SLA) technology. The process may also be a mixture of these different technologies, such as Multi Jet Fusion (MJF) technology, which combines binder jetting and powder bed fusion.

Claims

1. Method for repairing a part (P) during layer-by-layer additive manufacturing using an additive manufacturing machine (1), the additive manufacturing being material extrusion printing, the additive manufacturing machine (1) including an enclosure (11), the method including the following steps: a) depositing at least one layer of material on a support (2) for manufacturing the part (P), the support (2) for the part being present in the enclosure (11), b) detecting at least one missing material defect, if one or more defects of this type are present on said at least one layer, c) repairing said at least one missing material defect by adding material, d) repeating steps a), b) and optionally c) until the part (P) is produced, wherein step b) of detecting at least one missing material defect includes the step consisting in scanning said at least one layer, deposited in step a), in order to acquire topographical data about said at least one layer, and the step consisting in processing the data acquired in order to detect and geolocate at least one missing material defect, if one or more defects of this type are present on said at least one layer, the scanning step being implemented by a profilometer, in particular a laser profilometer, the profilometer being positioned outside the enclosure, scanning step b) being implemented by the profilometer through a wall portion transparent to the wavelength of the profilometer, in the visible range, between 380 nm and 800 nm, the transparent wall portion forming at least part of a wall defining the enclosure.

2. Method according to Claim 1, wherein step a) of depositing said at least one layer of material is performed using a nozzle (5) fastened to a carriage (6), said carriage (6) being movable along at least two axes (X, Y), preferably three orthogonal axes (X, Y, Z), relative to the support (2).

3. Method according to one of the two immediately preceding claims, wherein the material added in step c) is different from the material deposited for each layer in step a), preferably being more fluid.

4. Method according to Claim 2, wherein step c) of repairing said at least one missing material defect is carried out by the nozzle (5).

5. Method according to Claim 2, wherein step c) of repairing said at least one missing material defect is carried out by a second nozzle (16).

6. Method according to the preceding claim, wherein the second nozzle (16) has a smaller diameter than that of the nozzle (5).

7. Method according to any one of the preceding claims, wherein the material used for additive manufacturing and / or the material added in the repair step c) is a thermoplastic polymer selected from the group consisting of PAEKs (polyaryletherketone), including PEEK (polyetheretherketone) and PEKK (polyetherketoneketone), PEIs (polyetherimide, also known as ULTEM), PPS (polyphenylene sulfide), ABS (acrylonitrile butadiene styrene), PA (polyamide), PP (polypropylene), PLA (polylactic acid), TPU (thermoplastic polyurethane) and PET (polyethylene).

8. Method according to any one of the preceding claims, wherein step a) is carried out by depositing extruded polymer filament.

9. Additive manufacturing machine (1) for implementing the method according to any one of the preceding claims, the additive manufacturing being material extrusion printing, the machine including: - a support (2) for the part (P) to be manufactured, - at least one spool (3) of polymer material filament (4), - at least one nozzle (5) for extruding and depositing the filament (4) in order to form the part (P), - a carriage (6) to which the nozzle (5) and optionally a second nozzle (16) is / are fastened, - at least one of the carriage (6) and the support (2) being movable along at least two axes (X, Y), in particular three axes (X, Y, Z), relative to the other, said at least one nozzle (5) being used for repairing missing material defects or the machine (1) including a second nozzle (16) for repairing missing material defects, the second nozzle (16) preferably having a smaller diameter than that of the nozzle (5), - a scanning tool, the scanning tool being a profilometer, in particular an optical profilometer, - an enclosure (11), the support being in the enclosure (11), the scanning tool being outside the enclosure (11), the nozzle (5), and the optional second nozzle (16), emerging into the enclosure (11), a part of a wall of the enclosure being transparent to the wavelength of the profilometer and being positioned so as to allow the profilometer to scan at least a part of the part through this wall.