Laminated product with adjustable thickness by thinning, made from stone paper
The laminated product using stone paper sheets and a thermosetting adhesive addresses environmental concerns of traditional metal shims by offering a sustainable, peelable solution with reduced energy consumption and recyclability.
Patent Information
- Application Number
- FR2023002644
- Authority / Receiving Office
- FR · FR
- Patent Type
- Utility models
- Current Assignee / Owner
- Filing Date
- 2023-03-21
- Publication Date
- 2024-09-27
- Estimated Expiration
- 2033-03-21
AI Technical Summary
Existing adjustment shims made from metals like aluminum, stainless steel, carbon steel, brass, or titanium have significant environmental impact due to energy consumption, CO2 emissions, and recycling difficulties.
A laminated product using an alternating stack of stone paper sheets bonded with a thermosetting adhesive material, where each sheet can be detached without tearing, made from calcium carbonate and high-density polyethylene, with a bonding force lower than the sheet's tearing resistance.
Reduces environmental impact and provides peelable adjustment shims with reduced energy consumption and recyclability, utilizing stone paper as a sustainable alternative to traditional metals.
Abstract
Description
Title of the invention: Laminated product with adjustable thickness by thinning, made from stone paper. Technical field
[0001] The invention falls within the field of laminated products and more particularly within the field of peelable wedges.
[0002] PRIOR ART AND DISADVANTAGES OF PRIOR ART
[0003] More specifically, the invention relates to a laminated product having a thickness adjustable by delamination, this product comprising an alternating stack of sheets and layers of an adhesive material, each sheet having an intrinsic resistance to tearing, and each layer of adhesive material connecting two adjacent sheets of the stack to each other by a bonding force weaker than the resistance of the sheets to tearing, resulting in each sheet being able to be detached from the stack without tearing.
[0004] Products of this type are known from the prior art and are notably used as shims for mechanical assemblies. These assemblies generally exhibit significant clearances at certain points, resulting from the combination of manufacturing tolerances. These clearances are compensated for by inserting shims. The thickness of these shims is adjusted by removing the upper or lower sheets one by one until the desired thickness is achieved.
[0005] The sheets are generally metallic sheets, for example based on aluminium, stainless steel, carbon steel, brass or titanium, thermoplastic organic polymer sheets.
[0006] Nevertheless, the use of such materials has a significant environmental impact, particularly with regard to the amount of energy deployed, CO2 emissions generated, water consumption and recycling difficulties.
[0007] OBJECTIVE OF THE INVENTION
[0008] The invention thus aims to offer a laminated product that is more environmentally friendly. Description of the invention
[0009] To this end, the laminated product of the invention has a thickness adjustable by thinning, this product comprising an alternating stack of sheets and layers of an adhesive material, each sheet having an intrinsic tear resistance, and each layer of adhesive material connecting two adjacent sheets of the stack to each other by a bonding force weaker than the tear resistance of the sheets, with the result that each sheet can be detached from the stack without tear. The laminated product of the invention is characterized in that each sheet of the stack is a paper substitute based on natural mineral powder and polymer.
[0010] The laminated product of the invention may also include the following optional features considered individually or in all possible technical combinations: - Natural mineral powder is calcium carbonate. - the polymer is high-density polyethylene. - the paper substitute contains between 60 and 80% by mass of calcium carbonate. - the adhesive material is a thermosetting polymer. - The adhesive material is a water-based epoxy resin. - The adhesive material is an acrylic resin. DETAILED DESCRIPTION OF THE INVENTION
[0011] Other features and advantages of the invention will become clear from the description given below.
[0012] The present invention relates to a laminated product having a thickness adjustable by delamination, this product comprising an alternating stack of sheets and layers of an adhesive material, each sheet having an intrinsic resistance to tearing, and each layer of adhesive material connecting two adjacent sheets of the stack to each other by a bonding force weaker than the resistance of the sheets to tearing, resulting in each sheet being able to be detached from the stack without tearing.
[0013] It was discovered, within the framework of the invention, that a paper substitute could be used to constitute the sheets of the laminated product while exhibiting the peelability necessary for the required applications.
[0014] The paper substitute is known as stone paper. It is a sheet that is bleached by a mineral filler of calcium carbonate.
[0015] More specifically, stone paper is substantially obtained by mixing a natural mineral powder filler with a polymer.
[0016] By way of example, the natural mineral powder, which is the main constituent of clay paper, is preferably calcium carbonate but can also be alone or in mixture, for example, powdered coal, calcium sulfate, silica powder or chalk powder.
[0017] Calcium carbonate is preferred as it is available in virtually inexhaustible natural quantities and is presented as a quarry waste that does not require an extraction process.
[0018] The polymer is preferably high-density polyethylene, but can also be polypropylene, polylactic acid or polypropylene alone or in mixture.
[0019] High-density polyethylene (HD-PE) is preferred, which can, for example, be produced from sugarcane waste.
[0020] Stone paper made from calcium carbonate powder and high-density polyethylene is known to be used as a substitute for paper and paper-derived products such as packaging materials or advertising media.
[0021] Surprisingly, the inventor discovered that stone paper made it possible to manufacture a setting wedge that met the peelability requirements.
[0022] A shim made from stone paper advantageously reduces the environmental impact compared to the materials usually used to make such shims.
[0023] Moreover, since stone paper falls back into dust after several years under the influence of the sun, wind and weather, no particular recycling is to be expected.
[0024] The laminated product of the invention forming a peelable adjustment wedge is manufactured in the following way.
[0025] The sheets of stone paper are cut to the desired dimensions.
[0026] The sheets are bonded on one side with a thermosetting polymer. The thermosetting polymer can be an acrylic resin, a non-aqueous epoxy resin, or an aqueous epoxy resin. The latter is preferred to avoid the use of solvents and various pollutants.
[0027] The gluing operation is carried out by any type of gluing machine, spraying by means of a nozzle or a gun, by application with a manual roller, by printing on an offset type machine, or by soaking the sheet in a bath of adhesive material.
[0028] The thermosetting polymer, after its monomer crosslinking treatment into a polymer, constitutes an adhesive material, its quantity and treatment being chosen and adapted so that the bonding force linking two adjacent sheets is weaker than the resistance of these sheets to tearing, with the result that each sheet can be detached from the stack without tearing.
[0029] In some cases, additives are added to the resin. These additives may include hardeners to impart specific characteristics to the laminated product.
[0030] The glued sheets finally undergo a final polymerization operation under pressure. This operation consists of stacking the sheets between two parallel flat supports, these supports being pressed against each other at room temperature or heated in a heated press for a predetermined time so that the resin polymerizes.
[0031] This operation must give the rolled product the desired mechanical qualities of parallelism, flatness, cohesion and peelability.
[0032] The flat supports consist of two calibrated steel plates of significant thickness, for example 50 mm. The plates are traversed around their periphery by threaded rods or screws, on which a clamping force is applied.
[0033] Polymerization is carried out with temperature cycles between 60 and 120°C. Advantageously, the polymerization temperature can be raised to 60°C because the changes in the properties of the stone paper at this temperature give the laminated product obtained the required characteristics.
[0034] Finally, the laminated product is machined or cut if necessary to the appropriate dimensions, so that it has the correct shapes and dimensions in the plane of the sheets.
[0035] Peelability tests are carried out on a laminated product of the invention comprising sheets of stone paper made from calcium carbonate and high-density polyethylene marketed, in particular, under the trade name Armen Paper® and for two different adhesive materials.
[0036] Example 1: Water-based epoxy resin as an adhesive material
[0037] The aqueous epoxy resin used is marketed, in particular, under the trade name Sikafloor®-2540 W.
[0038] The manufacturing process of the laminated product involving the use of this aqueous epoxy resin is as previously described.
[0039] Peelability tests are performed according to ASTM D 903.
[0040] The results are presented in the Table below. Pelatability ++ - Insufficient
[0041] + Correct
[0042] ++ Very good
[0043] Table 1
[0044] Example 2: Acrylic resin as an adhesive material
[0045] The acrylic resin used is commercially available, notably from the company MétalTop.
[0046] The manufacturing process of the laminated product involving the use of this acrylic resin is as previously described.
[0047] Peelability tests are carried out in the same way as for example 1.
[0048] The results are presented in the Table below. Pelatability ++ - Insufficient
[0049] + Correct
[0050] ++ Very good
[0051] Table 2
Claims
Claims
1. A laminated product having an adjustable thickness by disintegration, said product comprising an alternating stack of sheets () and layers () of an adhesive material, each sheet () having an intrinsic tear resistance, and each layer () of adhesive material connecting two adjacent sheets () of the stack to each other by a bonding force lower than the tear resistance of the sheets (), with the result that each sheet () can be detached from the stack () without tearing, characterized in that each sheet () of the stack is a paper substitute based on natural mineral powder and polymer.
2. Rolled product according to the preceding claim, characterized in that the natural mineral powder is calcium carbonate.
3. Laminated product according to any one of the preceding claims, characterized in that the polymer is high density polyethylene.
4. Laminated product according to any one of the preceding claims, characterized in that the paper substitute comprises between 60 and 80% by mass of calcium carbonate.
5. Laminated product according to any one of the preceding claims, characterized in that the adhesive material is a thermosetting polymer.
6. Laminated product according to any one of the preceding claims, characterized in that the adhesive material is an epoxy resin in aqueous phase.
7. Laminated product according to any one of the preceding claims, characterized in that the adhesive material is an acrylic resin.