ACTIVE MATRIX ELECTROLUMINESCENT DEVICE WITH IMPROVED RESOLUTION
The described electroluminescent display device addresses the challenges of high spatial resolution and brightness in OLED displays by isolating sub-pixels with trenches and encapsulation, enabling efficient production of microdisplays with sub-pixel sizes below 5 pm and reduced parasitic currents.
Patent Information
- Application Number
- FR2023003581
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-11
- Publication Date
- 2024-10-18
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing OLED display technologies face challenges in achieving high spatial resolution and brightness while minimizing parasitic currents and crosstalk, particularly for sub-pixels smaller than 5 pm, and current manufacturing processes are complex and costly.
An electroluminescent display device with a matrix of pixels, each composed of at least three elementary emitting zones, separated by trenches with insulating surfaces and filled with insulating elements, and encapsulated to prevent parasitic currents, using photolithography and conformal deposition techniques to ensure electrical isolation and protection of OLED stacks.
The solution enables the production of OLED microdisplays with high spatial resolution and brightness, achieving sub-pixel sizes below 5 pm, with reduced crosstalk and improved reliability by isolating OLED stacks, using known semiconductor manufacturing techniques.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: DEVICE ACTIVE MATRIX ELECTROLUMINESCENT LIGHT WITH IMPROVED RESOLUTION Technical field of the invention
[0001] The invention relates to the field of optoelectronic devices and components, and more specifically to electroluminescent devices of the OLED (Organic Light Emitting Device) type. It relates more particularly to improving the efficiency and luminance of the display color range as well as the resolution of an OLED display screen. It makes it possible to manufacture micro-screens with very high spatial resolution, i.e. with a particularly high density of pixels and sub-pixels. State of the art
[0002] Organic Light Emitting Diode (OLED) devices are well-established products for manufacturing thin lighting systems and display screens. OLED-based display screens generally comprise a matrix structure of individual pixels, which is controlled by a grid of vertical and horizontal conductive tracks; this structure can allow individual addressing of the pixels. This is illustrated schematically in [Fig.l] which will be explained below. In color displays each pixel is subdivided into sub-pixels of different colors (typically three or four, including the primary colors red, green and blue, and possibly a white sub-pixel) which cooperate to emit a luminous point (pixel) of the desired color. [Fig.2] shows three known examples of arranging sub-pixels of different colors to form a pixel capable of displaying the desired color.
[0003] The color of a pixel or sub-pixel can be generated in two different ways. In a first embodiment, an OLED diode is used which emits white light and the emitted white light is passed through a color filter. [Fig. 3] shows a cross-section of such a screen. Above the electrodes of the sub-pixels is deposited an OLED stack which covers the entire surface of the matrix and which (in this example) emits white light. The primary colors RGB (Red-Green-Blue) or RGBW (Red-Green-Blue-White) of the sub-pixels are in this case generated by color filters located above the OLED stack.
[0004] This embodiment has two advantages. First, one can use the same common OLED layer, not structured at the matrix level, for all the sub-pixels, the color being generated by the filters. Another advantage is that it It is possible to realize very small actively addressed subpixels, which improves the spatial resolution of the display. However, this approach has two drawbacks: First, the filter absorbs a significant fraction of the light intensity emitted by the pixel. For a targeted light intensity, it is therefore necessary to increase the light emission of the OLED diode. Knowing that the operational lifetime of OLED devices decreases with increasing current density or luminance, because the large number of holes and electrons passing through the organic layer causes electrochemical side reactions of organic compounds that eventually degrade these organic compounds, it would be desirable not to increase the light intensity emitted by the OLED diode beyond a certain value. Second, the display sharpness of such a device is limited by the phenomenon of crosstalk, which will be explained below.
[0005] Another way of producing the primary colors is to structure the OLED layers into sub-pixels with different emission colors. This is a second well-known embodiment, which does not use filters and thus avoids the first problem of loss of light intensity. As the process of structuring the OLED layers is quite complex and the achievable spatial resolution quite limited, it is preferred even in this case to keep a maximum of common layers (i.e. layers covering the entire surface of the matrix), generally the charge carrier transport layers, and to structure only the emitting layers. However, as in the first embodiment, it is observed that neighboring pixels or sub-pixels can interact, by capacitive coupling or by parasitic currents passing in particular through common conductive layers of the OLED stack, in the plane of the conductive layers.
[0006] An example for this parasitic current in the plane of the conductive layers is illustrated in [Fig. 4] which will be explained below. This unwanted interaction between neighboring pixels is known to those skilled in the art as "crosstalk"; it leads especially to the unwanted modification of colors in the case of color displays. The theoretical aspects of the crosstalk phenomenon in OLED devices have been studied for a long time (see for example the publication by D. Braun "Crosstalk in passive matrix polymer LED displays" published in 1998 in the journal Synthetic Metals 92, pp. 107-113).
[0007] This problem becomes more noticeable when the subpixel size decreases. Apart from digitally correcting the consequences of crosstalk (which amounts to accepting the crosstalk phenomenon and reducing its impact on the image), there are different approaches to combating crosstalk at the source, i.e. to reduce the physical phenomenon at the pixel or subpixel level.
[0008] To reduce crosstalk, WO 2019 / 193290 (MicroOled) proposes a method for delimiting two neighboring pixels by a filling element with an insulating surface which separates their base electrodes as well as their OLED layers.
[0009] It is also known to separate each pixel to isolate it from the other pixels surrounding it, to avoid short-circuit problems linked to humidity in the encapsulation layers. Document EP 2 927 985 (Universal Display Corp.) describes a structure in which each pixel is hermetically sealed and isolated from its neighboring pixels. The manufacture of such a structure requires numerous and complex process steps. It is also known to delimit the pixel areas by additional separating elements, such as walls, as described in document US 9 419 245 (Japan Display Inc.). The methods described in these two documents are complex and generate a significant additional cost.
[0010] The structure of a prior art device, which makes it possible to obtain a high light intensity, is shown schematically in [Fig. 5], which will be discussed below in greater detail. It has three elementary emitting areas (sub-pixels) of different color and does not need color filters, which ensures excellent efficiency and brightness of the device. Since the sub-pixels are also separated at their OLED layers, there is practically no crosstalk, and the image sharpness is good. This device has many functional advantages. However, since the OLED layers of said sub-pixels are different, they must be deposited separately, and unfortunately, no industrial process is known with which this device could be miniaturized with a size of the elementary emitting area (sub-pixel) less than about 20 μm.
[0011] In view of the above, an objective of the present invention is to remedy, at least partially, the drawbacks of the prior art mentioned above, and to propose an architecture for an OLED display device of the color micro-display type, which has excellent brightness, preferably by using elementary color emitting zones, and which makes it possible to significantly reduce, and preferably eliminate, lateral parasitic currents, even for pixels of very small size (typically less than 5 μm) or for structures with very small inter-pixel space. Another objective is to propose a method for manufacturing such a device, which is reliable and simple.
[0012] Objects of the invention
[0013] According to the invention, the problem is solved by an electroluminescent display device comprising a matrix of electroluminescent pixels formed from a plurality of pixels deposited on a substrate, in a matrix arrangement in rows and columns,
[0014] each pixel being formed of at least three elementary emitting zones, each of said at least three elementary emitting zones belonging to a different group of elementary emitting zones which is distinguished from the elementary emitting zones belonging to other groups by its emission color,
[0015] each elementary emission zone comprising an electroluminescent stack of organic layers, called “OLED stack”, which comprises at least one light-emitting organic layer,
[0016] said OLED stack being arranged between a control electrode and a transparent upper electrode, said transparent upper electrode being crossed by the light emitted by the OLED stack,
[0017] said electroluminescent display device being characterized in that:
[0018] two neighboring control electrodes belonging to two neighboring elementary emitting zones which each belong to a different group of elementary emitting zones are separated by a space forming a trench and having an insulating surface which covers at least the vertical sides of said neighboring electrodes and electrically insulates them from each other, and
[0019] two neighboring control electrodes belonging to two neighboring elementary emitting zones which each belong to the same group of elementary emitting zones are separated by a space forming a trench, said space being filled with a filling element which insulates said neighboring electrodes electrically from each other and fills the natural space between said two electrodes,
[0020] in each group of elementary emitting zones, the entire OLED stack with its corresponding upper electrode is separated from the neighboring sets belonging to another group of elementary emitting zones by an encapsulation layer which protects said OLED stack on its upper face and its lateral sides against the ambient air, thus forming protected islands, each island comprising sets of OLED stacks of the same group, with their upper electrode. and is understood in the vertical direction from top to bottom of the pixel matrix.
[0021] According to one aspect of the invention, said trench-forming space between two neighboring emitting zones belonging to the same group is filled with a filling element with an insulating surface. This filling element fills the natural space between two neighboring control electrodes so that said upper electrode is substantially planar.
[0022] According to another aspect, the width of said trench-forming space between two neighboring emitting zones belonging to different groups is between 0.3 μm and 1.0 pm. According to yet another aspect, the depth of said trench space is between 150 nm and 800 nm, and preferably between 150 nm and 450 nm.
[0023] This electroluminescent display device represents a first object of the present invention.
[0024] The thickness of said control electrodes is between approximately 150 nm and approximately 800 nm, and preferably between approximately 150 nm and approximately 450 nm. Advantageously, the thickness of said control electrodes is greater than that of the OLED stacks.
[0025] According to the invention, the geometry of the trench is chosen so as to produce, on the one hand, a good spatial and electrical separation between control electrodes of neighboring elementary emitting zones, in particular for the critical step of etching, and so as to have, on the other hand, an opening of the elementary emitting zones (sub-pixels) as wide as possible, even for very small sub-pixel pitches. Here, the opening of an elementary emitting zone is understood to mean the ratio between its active surface (i.e. the horizontal surface of the control electrode, possibly reduced by the overflow of the insulation layer) and the pitch of the elementary emitting zones in x multiplied by the pitch of the elementary emitting zones in y-
[0026] In an advantageous device according to the invention, the pitch of the elementary emitting zones is less than approximately 20 pm, preferably less than approximately 15 pm, more preferably less than approximately 10 pm, and even more preferably between approximately 1 pm and approximately 5 pm.
[0027] The width of the gap between control electrodes is advantageously less than about 1 μm, and preferably between about 0.3 μm and about 1.0 μm.
[0028] In advantageous embodiments of the present invention, the pitch of a sub-pixel is typically between about 1 pm and about 5 pm, and the width of the space between control electrodes is typically between about 0.3 pm and about 1.0 pm). For example, for a sub-pixel pitch in x of 3 pm, and a pitch in y of 9 pm, and a space between electrodes of 1 pm, the area of a control electrode is 2 pm x 8 pm = 16 pm2, and the aperture is therefore 16 pm / (3 pm x 9 pm) = 0.59, if there is no overflow of the insulation layer on the electrode.
[0029] The method according to the invention uses known techniques for manufacturing integrated circuits, in particular photolithography and etching techniques. In order to be able to implement these techniques, it is necessary to ensure that the etching methods used only attack the materials that must be removed, and leave intact those that must remain.
[0030] This geometry is advantageously accomplished by one or more of the following features which form particular aspects of the invention:
[0031] - The thickness of the control electrodes of the elementary emission zones is between about 150 nm and about 800 nm.
[0032] - The thickness of the control electrodes of the elementary emitting zones is greater than the thickness of the OLED stack in said elementary emitting zones.
[0033] - The insulating layer must be very thin and free from defects. Its thickness is preferably between about 10 nm and about 30 nm. It is preferably deposited by a conformal deposition technique, preferably by ALD (Atomic Layer Deposition), in order to also protect the sidewall of the OLED stack.
[0034] - The filling element is present only in horizontal spaces between sub-pixels, but the trench remains empty in the vertical spaces. In order to guarantee the continuity of the upper electrode, said filling element must be present also between the first row of pixels and the connection bar at the top as well as between the last row of pixels at the bottom and the connection bar at the bottom.
[0035] - The square space between four neighboring elementary emitting zones does not include preferably no filler element, in order to obtain continuous trenches from top to bottom of the pixel matrix, separating groups of different elementary emitting zones.
[0036] - The surface of the control electrode resists the etching of the layer well OLED, this etching being typically accomplished using an oxygen plasma. Advantageously, this electrode comprises a metal layer covered with a thin layer of a transparent conductive oxide (TCO - Transparent Conductive Oxide) which resists this type of etching well. This TCO layer is advantageously made of SnO2, possibly doped; this will be explained below.
[0037] - The encapsulation layer is selected from a material which is highly resistant to various wet and dry stages of photolithography (deposition and development of photoresists) and the etching of OLED stacks (in particular by oxygen plasma). Advantageously, it can be made of A12O3.
[0038] A second object of the present invention is a method of manufacturing an electroluminescent display device comprising a matrix of electroluminescent pixels formed of a plurality of pixels deposited on a substrate, in a matrix arrangement in rows and columns,
[0039] each pixel being formed of at least three elementary emitting zones, each of said at least three elementary emitting zones belonging to a different group of elementary emitting zones which is distinguished from the elementary emitting zones belonging to other groups by its emission color,
[0040] each elementary emission zone comprising an electroluminescent stack of organic layers, called “OLED stack”, which comprises at least one light-emitting organic layer,
[0041] in which method:
[0042] a substrate is provided provided with a control electrode for each elementary emitting zone and with an insulating layer between two neighboring electrodes, and provided with filling elements between two neighboring elementary emitting zones belonging to the same group of elementary emitting zones,
[0043] in a first group of steps, a first group of elementary emitting zones is produced, by first depositing a first OLED stack, an upper electrode and, using a conformal deposition technique, a first encapsulation layer, then a photoresist is arranged at the location of the elementary emission zones of the first group (according to the well-established photolithography methods known in microelectronics) which protects the horizontal surface and the flank of said encapsulation layer at the location of said elementary emission zones of the first group, and the zones not protected by the photoresist are etched up to the upper surface of the control electrode, and finally said photoresist is removed,
[0044] in a second group of steps, a second group of elementary emitting zones is produced, by first depositing a second OLED stack, an upper electrode and, using a conformal deposition technique,a second encapsulation layer, then a photoresist is arranged at the location of the emission zones of the second group (according to the well-established and known photolithography methods in microelectronics) which protects the horizontal surface and the flank of said encapsulation layer at the location of said elementary emission zones of the second group, and the zones not protected by the photoresist are etched up to the upper surface of the control electrode for the elementary emission zones of the third group and up to the surface of the first encapsulation layer for the elementary emission zones of the first group, and finally said photoresist is removed, ,
[0045] in a third group of steps, a third group of elementary emitting zones is produced, by first depositing a third OLED stack, an upper electrode and, using a conformal deposition technique, a third encapsulation layer, then a photoresist is arranged at the location of the emission zones of the third group (according to the well-established and known photolithography methods in microelectronics) which protects the horizontal surface and the flank of said encapsulation layer at the location of said elementary emission zones of the third group, and the zones not protected by the photoresist are etched down to the surface of the first encapsulation layer for the elementary emission zones of the first and second groups, and finally said photoresist is removed. Description of figures
[0046] Figures 1 to 6 schematically represent a perpendicular cross-section through an optoelectronic device of the OLED display type, and illustrate general, known aspects of OLED devices and displays.
[0047] Figures 7 to 34 illustrate aspects and embodiments of the invention; they are not intended to limit the scope of the invention.
[0048] More particularly, Figures 7 to 14 illustrate the structure of an OLED display device according to the invention, and certain key steps in its manufacture.
[0049] Figures 15 to 26 illustrate in greater detail steps of a method of manufacturing an OLED display device according to the invention.
[0050] Figures 27 to 34 illustrate other particular aspects of the invention.
[0051] [Fig. 1] shows the electrical diagram of a known type OLED matrix screen.
[0052] [Fig.2] shows three known examples of arranging sub-pixels of different colors to form a pixel capable of displaying the desired color.
[0053] [Fig.3] schematically shows a perpendicular cross-section of a state-of-the-art OLED display with a white-emitting OLED and color filters. This figure shows several pixels.
[0054] [Fig.4] schematically shows a perpendicular cross-section of an OLED display similar to that of [Fig.3], in which each pixel is formed of three sub-pixels. The figure shows a single pixel with its three sub-pixels.
[0055] [Fig.5] schematically shows a perpendicular cross-section of an OLED display similar to that of [Fig.4], in an embodiment with sub-pixels each emitting in a different color, and which does not use color filters.
[0056] [Fig.6] reproduces [Fig.5] of document WO 2019 / 193290.
[0057] [Fig.7] shows a top-view of an intermediate product according to the invention, manufactured using steps of the process according to the invention.
[0058] [Fig.8] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zx plane along line AA indicated in [Fig.7], on a substrate which represents the intermediate product of [Fig.7].
[0059] [Fig.9] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along line BB indicated in [Fig.7], on a substrate which represents the same intermediate product of [Fig.7].
[0060] [Fig. 10] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zx plane along line AA indicated in [Fig.7], on a substrate which represents a stage subsequent to that of the intermediate product of [Fig.8].
[0061] [Fig. 11] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in Fig. 7, on a substrate which represents a stage subsequent to that of the intermediate product of [Fig.9].
[0062] [Fig. 12] shows a top-view of an intermediate product according to the invention, manufactured using steps of the method according to the invention, at a manufacturing stage which corresponds to that of Figures 10 and 11.
[0063] [Fig. 13] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zx plane along line AA indicated in [Fig.7], on a substrate which represents the intermediate product of [Fig. 12] after a sequence of additional manufacturing steps.
[0064] [Fig. 14] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate which represents the same intermediate product of [Fig. 13],
[0065] [Fig. 15] illustrates a first sequence of steps of an embodiment of the method according to the invention for manufacturing an OLED microdisplay type device according to the invention, having three groups of pixels.
[0066] [Fig. 16] illustrates a second sequence of process steps which follows those of [Fig. 15],
[0067] [Fig. 17] illustrates a third sequence of process steps which follows those of [Fig. 16],
[0068] [Fig. 18] illustrates a fourth sequence of process steps which follows those of [Fig. 17]; it results in a sub-pixel of a first group.
[0069] [Fig. 19] illustrates a fifth sequence of process steps which follows those of [Fig. 18],
[0070] [Fig.20] illustrates a sixth sequence of process steps which follows those of the [Fig.19],
[0071] [Fig.21] illustrates an eighth sequence of process steps which follows those of [Fig.20].
[0072] [Fig.22] illustrates a ninth sequence of process steps which follows those of [Fig.21],
[0073] [Fig.23] illustrates a tenth sequence of process steps which follows those of the [Fig.22]; it results in a sub-pixel of a second group.
[0074] [Fig.24] illustrates an eleventh sequence of process steps which follows those of [Fig.23],
[0075] [Fig.25] illustrates a twelfth sequence of process steps which follows those of [Fig.24].
[0076] [Fig.26] illustrates a thirteenth sequence of process steps which follows those of [Fig.25]; it results in a sub-pixel of a third group. This intermediate product corresponds to that of figures 13 and 14.
[0077] [Fig.27] refers to [Fig.7] and illustrates the opening of the stencil through which one deposits, in the process according to the invention, the OLED stacks.
[0078] [Fig.28] refers to [Fig.7] and illustrates the opening of the stencil through which one deposits, in the method according to the invention, the upper electrode.
[0079] [Fig.29] refers to [Fig.7] of which it shows a variant.
[0080] [Fig.30] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate which represents a variant of the intermediate product of [Fig.7]; this section is analogous to that of [Fig.9].
[0081] [Fig.31] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate which represents a stage subsequent to that of the intermediate product of [Fig.30]; this section is analogous to that of [Fig.1 1].
[0082] [Fig.32] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate one step later than that of the intermediate product of [Fig. 14].
[0083] [Fig.33] schematically shows a perpendicular cross-section of a device according to the invention, according to one of its variants.
[0084] [Fig.34] shows a drawing from an image obtained by electron microscopy at scan on a cross-section of a device which illustrates the variant shown in [Fig.33].
[0085] Table 1 lists the reference numerals that are used in the figures and in this description.
[0086] Table 1: List of numerical references used in the figures 10 OLED display (known type) 12 Pixel matrix 14 OLED diode 16 Driver circuit 12 18 Field effect transistor 20 Field effect transistor22 Capacitor 30 Line driver circuit 32 Video driver circuit 36 Control unit 34 Column power supply circuit 38 Line conductor track 40 Conductor track (video signal) 42 Column conductor track 50 Pixel 51 Red subpixel 52 Blue subpixel 53 Green subpixel 54 White subpixel 70 OLED display (known type) 71 Substrate 75 Gap-fill element 76 OLED layers 72, 73, 74 Subpixel driver electrode 77 Encapsulation layer 78 Glass wafer 80 Electroluminescent layer 76 81, 82 Charge injection and transport layer 83 Charge injection and transport layer 84 Charge injection and transport layer 85 Electrode 90 Pixel 91 Blue filter for subpixel 92 Red filter for subpixel 93 Green filter for subpixel 98 Electrode for pixel 95,96,97 Electroluminescent layers Red, Green,Blue 99 Common electrode 100 OLED display device 101 Subpixel 102 Base electrode 104 Separator 105 OLED stack 106 Top injection layer 107 Common conformal electrode 108 Planarization layer 109 Color filter 110 Substrate 111 Natural space (“gap”) 112 Edge of 123 on 102 113 Pixel 123 Insulating surface fill element 200 Device according to the invention 201 Subpixels 202 Subpixel control electrode 203 Insulating surface fill element (gap fill), 205 OLED stack 207 Top electrode 210 Substrate 212 Edge of 223 or 203 on 202 211 Gap between electrodes 202 217 Bus bar for top electrode 207 218 Tooth of 217 223 Insulator layer 225 island 270 Row of non-functional subpixels 280 Photoresist 290 Encapsulation layer 300 Stencil for deposition of 205 310 Aperture of 300 400 Stencil for deposition of 207 410 Aperture of 400
[0087] Detailed description of the invention
[0088] In the present description, the expression "elementary emission zone" designates the smallest emission zone which is individually addressable. In the case of color screens in which several elementary emission zones form a pixel, the person skilled in the art usually uses the term "sub-pixel" to designate such an elementary emission zone.
[0089] [Fig-1] schematically shows the circuit of a 10-type OLED display known which comprises a pixel matrix unit 12 capable of producing an image, and a control unit 36. The OLED diodes 14 and their control circuits 16 are arranged so as to form pixels in the pixel matrix unit 12, said pixel matrix comprising rows (horizontal) and columns (vertical). Each control circuit 16 of a pixel 12 comprises a plurality of transistors 18, 20 typically made in CMOS (Complementary Metal Oxide Semiconductor) technology in the case of micro-screens, or thin-film transistors (known as TFT (Thin Film Transistor)), and a capacitor 22. The control unit 36 controls a control circuit for the rows 30 and a video addressing circuit 32, as well as a power supply circuit 34 for addressing the pixel columns; It provides addressing of the pixel circuits and controls the light emission of the 14 OLED diodes.The line driver circuit is connected to the conductive tracks 38 addressing the scanning lines of the pixel matrix. It selects the scanning lines 38 according to a signal from the control unit 36, and applies a voltage to turn on the transistors 18 located on the selected scanning line 38.
[0090] The video addressing circuit 32 is connected to conductive tracks 40 addressing the columns of the video signal. The video addressing circuit 32 receives a video signal from the control unit 36 and sends a voltage to the video conductive tracks 40 of the columns according to the conductive tracks of the rows selected by the corresponding control circuit 30. This voltage signal is written into the capacitor 32 through the transistor 18 of the OLED diode 14 of the selected pixel row. The control transistor 20 sends a current corresponding to the recorded voltage to the OLED diode 14, and thereby the OLED diode 14 of the selected row 38 emits light.
[0091] The electrical power supply circuit 34 is connected to the conductive power supply tracks 42 of the pixel columns; it supplies the OLED diodes 14 via the conductive tracks 32 and the transistors 20 of the selected pixel row.
[0092] This principle of addressing an OLED diode forming a pixel in a pixel matrix, known from WO 2019 / 193 290 A1, (Microoled), can be applied, in a manner also known as such, to the addressing of an OLED diode forming a sub-pixel in a pixel matrix of a color display device, in which each pixel comprises a plurality of sub-pixels (most often three or four) of different colors; this will be explained here in relation to [Fig. 2] which show three examples for the geometric arrangement of these sub-pixels 51, 52, 53, 54 to form a pixel 50 capable of displaying the desired color. In these figures the sub-pixels are red 51, blue 52 and green 53, and may include, as in the figure on the right, in addition a white sub-pixel 54 to increase the brightness of the pixel 50. The arrangement in the figure on the left is known by the acronym "RGB Stripe", it is the most widespread.The arrangement in the middle figure is known as "RGB quad," and the one on the right is known as "RGBW quad."
[0093] The addressing principle just described in relation to [Fig.l] and [Fig.2] is one of the addressing principles that can be implemented in relation to the present invention. The color can be obtained by controlling the color emitted by the OLED layers forming the sub-pixels or by color filters that modify the white color of the light emitted by the sub-pixels, as will be explained below in relation to [Fig.3], [Fig.4] and [Fig.5] which schematically show OLED microdisplays according to the state of the art; they illustrate the problem that the present invention seeks to solve.
[0094] In [Fig.3] is shown an overall schematic view of the structure of the device 70: we can distinguish the substrate 71 (typically of CMOS type, the addressing circuits and components are not shown), the control electrodes 72, 73, 74 of the sub-pixels separated by a gap-fill element 75, the stack of organic OLED layers 76 capable of emitting white light, the encapsulation layer 77, the colored filters of blue 91, red 92 and green 93 forming a pixel 90, the glass slice 78 as a protective cover. The size of the sub- pixels is typically of the order of 3.5 pm to 5 pm. It is noted that in this device according to the state of the art the OLED layer 76 extends over all the pixels of the device.
[0095] [Fig.4] shows an enlarged view of a device similar to that shown in [Fig.3]; this view is limited to a single pixel 90. The sub-pixels are defined, on the one hand, by the electrodes 72,73,74 which allow their individual addressing, and by the corresponding colored filters 91,92,93 which modify the light emitted by the white emission OLED stack 76 which extends over the entire surface of the device. The space between two neighboring sub-pixel control electrodes 72, 73 may be filled by a filling element 75. Said OLED stack 76 here comprises the light-emitting layer 80 itself, which is sandwiched between two charge transport layers 81, 82. More precisely, in a typical device, layer 81 comprises a hole injection and transport layer, and layer 82 an electron injection and transport layer.But it is also possible to use a so-called "inverse" stack, in this case the layer 82 comprises a hole injection and transport layer, and the layer 81 an electron injection and transport layer. The layers 81 and 82 can respectively comprise a single layer which fulfills both the functions of injection and transport of the respective charges, or several layers, for example a layer for injection and another for transport of the respective charges. A common electrode 85 evacuates the charges.
[0096] This device according to the state of the art has parasitic currents; this is illustrated in [Fig.4]. Indeed, if when a sub-pixel (for example 73) is switched on, the main current passes (marked by a thick arrow) directly through the OLED layer in the shortest direction (i.e. vertical relative to the substrate 71), part of the current propagates along other conduction paths, insofar as these conduction paths have a sufficiently low resistivity. Thus, a parasitic current is observed which propagates in the charge transport layer 81, namely in the plane of the substrate, and which then passes through the OLED layer in the neighboring sub-pixel 72 or 73. This parasitic current is marked by two dotted arrows. It leads to a parasitic light emission in the neighboring sub-pixels, which modifies the image resolution of the display and reduces the fidelity of its color.The present invention seeks to provide a means for reducing this parasitic current.
[0097] [Fig. 5] shows another device of known type in which the color of a pixel 90 is not generated, as in the devices of [Fig. 4] and [Fig. 5], by a white emitting OLED element matched with color filters for each of the three sub-pixels, but by three sub-pixels provided with electroluminescent layers 95, 96, 97 which emit directly in red, blue and green. In this embodiment, each sub-pixel 95,96,97 has its own addressing electrode 98a,b,c, but the first charge injection and transport layer 83 (for example holes), and / or the second charge injection and transport layer (for example electrons) 84 and the common electrode 99 are common to simplify device manufacturing. The problem of parasitic currents is the same as that described in relation to [Fig.4]; the contribution of the hole injection and transport layer 83 is preponderant in these parasitic currents.
[0098] In terms of luminous efficiency, the device of [Fig. 5] is significantly better than that of [Fig. 3]. On the other hand, its industrial manufacture can be quite difficult, since the organic materials that constitute an OLED device are generally deposited by a vacuum thermal evaporation process. To generate sub-pixels of different color, as in the device of [Fig. 5], a stencil (called a "shadow mask" in English) is used which is placed close to the substrate on which the OLED device is to be produced and which has openings that correspond to the position of a first type of sub-pixel during the deposition of a first type of stack of layers, for example for a red OLED. Then the operation is repeated for a second type of stack, for example for a green OLED, using a second stencil having openings that correspond to the position of the second type of sub-pixel.Then we can perform a third operation of this type in order to create a third type of sub-pixel, for example with a blue OLED.
[0099] This method does not allow the production of sub-pixels smaller than about 20 pm with a sufficiently reliable process, knowing that for micro-screens a sub-pixel size of the order of 2 pm to 5 pm would be required. In the semiconductor field, structures of this size are produced by photolithography and etching methods, but since the organic materials used in OLED devices are extremely sensitive to water and oxygen, among other things, photolithography processes cannot be used as such to structure these materials. It is observed that when an attempt is made to transpose the photolithography and etching methods known from the semiconductor field to the manufacture of OLED micro-displays, the OLED stack is attacked laterally, i.e. in its edge which is not protected, during the etching operations.This attack leads to localized degradation of the OLED stack, which risks propagating laterally. In a favorable case, this will simply reduce the emissive surface of the sub-pixel (which is already not desirable, especially since this propagation is an evolutionary process, and any reduction in the emissive surface will lead to an increase in the current density of the device which will reduce its operational lifetime); in an unfavorable case, this ends. by completely destroying the sub-pixel. According to an essential characteristic of the present invention, the edges and edges of the elementary emitting zones (sub-pixels) are protected on all sides.
[0100] The starting point of the invention is the device of [Fig.5] of document WO 2019 / 193290, which is reproduced here in [Fig.6], with adjusted numerical references. This figure shows a pixel 113 of an OLED display device 100 deposited on a substrate 110 (typically of CMOS type) with three sub-pixels 101a, 101b, 101c each of which is controlled by an individual control electrode 102a, 102b, 102c. The white OLED stack 105 which is common to all the pixels of the screen in question is separated between two neighboring sub-pixels (101a, 101b; 101b, 101c; 101c, 101a) by a separator 104 which occupies the natural space 111 (also called the “gap”) between the electrodes 102a, 102b; 102b, 102c; 102c, 102a of two neighboring sub-pixels 101a, 101b; 101b, 101c; 101c, 101a. This separator 104 which is in the form of a trench, comprises a filling element 123 with an insulating surface.The filler element 123 has a rim 112 which extends over a small portion of the control electrode 102, forming the border of the latter. The conformal electrode 107 is common to all the sub-pixels, as is the upper injection layer 106, the latter being optional.
[0101] This prior art structure very satisfactorily solves the crosstalk problem, but since it uses elementary emitting areas (sub-pixels) 101a, 101b, 101c with the same white emitting OLED stack to form a pixel 113, whose light passes through color filters 109 (arranged in the form of a plate which is placed on a smoothing layer 108) in order to generate elementary colors R, G and B at the output of the device 100, it does not solve the problem of providing a very efficient and very bright device. It would be desirable to be able to manufacture a device of similar structure, but without color filters and with OLED stacks emitting a different color for each group of sub-pixels, for example the three elementary colors red, blue and green.It would be desirable to be able to manufacture this device in the form of a microdisplay with a size of the elementary emitting zones less than 20 pm, preferably less than 5 pm, and even more preferably between approximately 1 pm and approximately 5 pm. To achieve this objective, it was necessary to invent a new method for manufacturing a microdisplay; the inventors of the present application have succeeded in doing so.
[0102] We will now explain the device according to the invention, which will be described by its structure, by its manufacturing method, and at different stages of its manufacturing. This device, as represented here, comprises three groups of elementary emitting zones (sub-pixels).
[0103] [Fig.7] shows a top-view of an intermediate product according to the invention, manufactured using steps of the method according to the invention. The structure of the substrate with its different deposited structured layers is shown schematically in two figures which represent the same intermediate product of [Fig.7], and which schematically show a perpendicular cross-section of a structured stack of layers, namely [Fig.8] which represents a section in a zx plane along the line AA indicated in [Fig.7], and [Fig.9] which represents a section in a zy plane along the line BB indicated in [Fig.7],
[0104] This intermediate product comprises a substrate 210 (which typically comprises active matrix type addressing circuits, produced using TFT or CMOS technology, well known to those skilled in the art), and electrodes 202a, 202b, 202c of sub-pixels separated by a natural space 211 ("gap") which has the shape of a trench. In this trench, an insulating layer 223 is deposited by a conformal deposition method, that is to say a method which covers the entire surface, whether horizontal, vertical or overhanging. For this purpose, the atomic deposition technique (ALD) or the plasma-enhanced chemical vapor deposition technique (PECVD) can be used. The material of this insulating layer is advantageously selected from the group formed by Si3N4, SiO2 and Al2O3. Among these three materials, A12O3 is preferred.
[0105] Said insulating layer 223 covers at least the vertical surfaces of the electrodes 202 and typically the surfaces of the entire natural space 211 between the electrodes 202. In an advantageous embodiment it also slightly covers the edge of the pixel (i.e. the upper horizontal surface) of the electrodes 202, thus forming a rim 212 on the control electrode 202.
[0106] As can be seen in [Fig.7] and in [Fig.9], the natural space (trench) 211 between the electrodes 202 is filled by a filling element 203 with an insulating surface, but only the horizontal space (i.e. along an x axis) between two sub-pixels. The vertical space (i.e. along a y axis) between two sub-pixels does not contain a filling element and forms a trench which goes from the top to the bottom of the matrix formed by all the (sub-)pixels. The surface of said filling element 203 typically consists of a photoresist or a dielectric material such as SiO2, Si3N4 or other; alternatively, said entire filling element 203 consists of such a dielectric material. Like the insulating layer 223, the filling element 203 may have a rim 212 on the control electrode 202, for the same reasons.
[0107] A variant of this embodiment will be described below in relation to figures 30 to 32. In this variant, the filling element 203 is first deposited in the natural space 211 and then the insulating layer 223.
[0108] As can be seen in [Fig.7], the substrate also comprises connection bars 217 at the top and bottom of the matrix, in the form of horizontal metal lines (bus bars), for the connection of the upper electrode of the OLED display device, as will be explained below in relation to [Fig. 12].
[0109] This substrate structure makes it possible to subsequently create islands 225 of elementary OLED emitting zones which are completely isolated and encapsulated; such an island 225 is represented in [Fig. 10] by the box with dotted contours. In [Fig. 7] these islands have a vertical column shape which crosses the active zone from top to bottom, as also emerges from the comparison between [Fig. 10] and [Fig. 11]; these two figures will be explained below. The function of the filling element 203 is here to ensure the continuity of the upper electrode 207 along the vertical column (y).
[0110] Reference is now made to [Fig. 10] and [Fig. 11], which both show the same device at the same intermediate stage of manufacture. Like [Fig.8] and [Fig.9], [Fig. 10] represents a section in a zx plane along the line AA indicated in [Fig.7], and [Fig.11] represents a section in a zy plane along the line BB indicated in [Fig.7]. On the other hand, [Fig.10] and [Fig.11] represent a more advanced stage of manufacture than that shown in [Fig.7], namely a stage of manufacture which follows that of [Fig.8] and [Fig.9].
[0111] As shown in [Fig. 10], a stack of organic layers 205a is first deposited which forms the OLED stack (i.e. an OLED diode capable of emitting light), typically by the thermal evaporation method; this technique for depositing the layers of an OLED stack currently forms the standard in the OLED device industry. It is a directional deposition, i.e. the layers will form mainly on horizontal surfaces, but not on vertical surfaces, as shown in [Fig.10]. The OLED stack 205a is completed by a top electrode 207a. It must be transparent. As can be seen from the comparison between [Fig. 10] and [Fig. 11], the top electrode 207a is common for each group of sub-pixels in a column.
[0112] The organic layers that form the OLED stack 205a are very sensitive, in particular to water and oxygen, and they must be protected against these molecules. To this end, an encapsulation layer 290a is deposited which covers the entire topography of the device, in particular both the horizontal and vertical surfaces. It typically consists of a thin layer of a transparent insulating material. Its thickness is advantageously between approximately 10 nm and approximately 30 nm. Its material is preferably selected from the group formed by Si3N4, SiO2 and A12O3. These materials have the advantage of being highly resistant to the etching step intended to remove the OLED stack; this etching can be carried out by an oxygen plasma. This encapsulation layer 290a is advantageously deposited by a conformal deposition method such as PECVD or ALD.
[0113] A hermetically isolated space is thus obtained around the OLED device from all the sub-pixels in a column 225a (also called an “island” here); these sub-pixels belong to the same group of sub-pixels (for example to the group of red sub-pixels or to the group of blue sub-pixels).
[0114] In order to connect the upper electrode 207a to the connection bar 217, the deposition of the organic materials of the OLED stack 205 should not protrude too much on the connection bars 217, and the deposition of the electrode layer 207 must at least partially cover the bus bars. [Fig. 12] shows a top view of the substrate after the deposition of the layer 207.
[0115] This intermediate device has several advantages and improvements over the state of the art.
[0116] Firstly, it allows excellent electrical isolation of the OLED layers between neighboring sub-pixels, and therefore leads to a reduction in crosstalk which is of the same quality as that described in WO 2019 / 193290.
[0117] Second, the structure of the organic layers of the OLED stack in the form of hermetically isolated islands improves the reliability of the device. In particular, a point defect (for example, water entering through a pinhole in the encapsulation layer) cannot propagate further than the dimension of a sub-pixel in the horizontal direction because it will be stopped by the natural space 211 between neighboring sub-pixels which has been arranged in the form of a trench.
[0118] Thirdly, the isolated islands 225 allow structuring of the OLED layer with photolithography methods, which makes it possible to produce, for example, the device according to [Fig. 13] and [Fig. 14], which is a device according to the invention, with three groups of different OLED stacks (red 205a, green 205b and blue 205c) and an improved spatial resolution capable of reaching an elementary emitting zone size of less than 5 pm, with optimal efficiency, and without risk of damaging the edges of the OLED stacks during an etching step. This technique also makes it possible to produce the device according to the invention, with a matrix with three groups of RGB sub-pixels, without a color filter, with such a resolution.
[0119] We will now describe, in relation to [Fig. 15] to [Fig.25], how the three groups of elementary emitting zones (sub-pixels) are deposited. These figures show one of these zones for each of these three groups of elementary emitting zones. To produce a device with three groups of elementary emitting zones (sub-pixels) each emitting light of a different color (these groups being designated here, by way of example, which represents an advantageous embodiment, by the letters R, G and B (Red, Green, Blue)), three groups of manufacturing steps are required. Each group of steps includes steps of depositing and structuring a photoresist layer, followed by at least one step of etching the entire encapsulation layer, the cathode and the OLED stack, and finally the removal ("stripping") of the photoresist.
[0120] In the context of the present description, with regard to the photoresist, techniques which are usual in the field of microelectronics can be used. They typically comprise the deposition of a layer of photoresist, its exposure to structure it on the surface, then its development. These techniques are known to those skilled in the art and will not be described here; these steps related to the localized deposition of photoresist are summarized here by the expression "arrangement" of a photoresist.
[0121] A device of the OLED micro-display type is thus obtained, shown in [Fig.12], [Fig.13] and [Fig.14], with the three sub-pixels electrically and hermetically isolated, said sub-pixels having OLED stacks emitting in a different color, namely R (205(a)), G (205(b)) and B (205(c)).
[0122] In a first group of steps, shown schematically in [Fig. 15] to [Fig. 18], a first group of elementary emitting zones (sub-pixels) is deposited, emitting light of a first color, for example red.
[0123] First, a substrate 210 is provided, provided with a control electrode 202a, 202b, 202c for each elementary emitting zone (this control electrode 202 typically being the anode), an insulating layer 223 between two neighboring electrodes 202a, 202b, 202c, and a filling element 203 in the natural space 211 between two neighboring control electrodes 202 belonging to the same group of elementary emitting zones. This insulating layer advantageously has a rim 224 on the surface of the electrode 202.
[0124] The substrate 210 is typically a silicon wafer with circuits structured according to CMOS technology which are configured to address the elementary emitting zones; this technology is known as such and will not be explained here. This substrate 210 typically comprises an insulating layer (not shown in the figures) which may in particular be an oxide, a nitride or an oxynitride; Si3N4 is typically used. The electrical contacts between the pixels are made via vertical channels arranged through this insulating layer by etching; this is also known and is not shown in the figures. On this insulating layer is deposited the pixel control electrode 202, which is typically chosen to be highly reflective.
[0125] In a very advantageous embodiment, the control electrode 202 has a thickness of between approximately 150 nm and approximately 800 nm. Too large a value impairs the resolution of the micro-display because it requires increasing the space between two elementary emitting zones. It is also very advantageous for the thickness of the control electrode 202 to be greater than the thickness of the OLED stack 205 which will be deposited on this electrode.
[0126] Said lower electrode 202 may comprise one or more layers. It may for example be made of silver, aluminum, copper, chromium or another metal with high reflectivity. If aluminum is used, it is very advantageous to protect it with a thin layer of a transparent conductive oxide (abbreviated TCO, Transparent Conductive Oxide) having a high resistance to wet etching and oxygen plasma. Such a TCO is called here “hard TCO”. It is advantageously selected from the group formed by SnO2 and doped SnO2, this doping preferably being arsenic and / or fluorine and / or nitrogen and / or niobium and / or phosphorus and / or antimony and / or aluminum and / or titanium.
[0127] In a first subgroup of steps, the result of which is illustrated in [Fig. 15], the following are successively deposited on this substrate 210: (a) a first OLED stack 205a, deposited with a directional deposition technique, i.e. a deposition technique, such as evaporation, which deposits substantially only on a horizontal surface; (b) an upper electrode 207a, and (c) a first encapsulation layer 290a. Said upper electrode 207a has a polarity opposite to that of the control electrode 202; it is typically a cathode. Said upper electrode is typically deposited with a directional deposition technique; it may be deposited by a conformal technique.
[0128] According to an essential characteristic of the invention, said encapsulation layer 290a is deposited using a conformal deposition technique, such as ALD; this ensures that it also covers and protects the wafer of the OLED stack. This protection is essential during the subsequent etching steps. Said first encapsulation layer 290 must be transparent; it is advantageously made of alumina. In a variant, several transparent encapsulation layers are deposited at this stage (such a stack is included here in the expression “first encapsulation layer”), using the same material or not; at least the first of these layers must have been deposited by a conformal deposition technique, while the other layers are preferably.
[0129] It is noted that at the end of the first subgroup of steps, the OLED stack deposited on the electrode 202b of the second group of elementary emitting zones and on the electrode 202c of the third group of elementary emitting zones is an OLED stack 205a of the first OLED stack type. As will be explained below, in subsequent groups of steps, it will subsequently be replaced by an OLED stack of type second OLED stack 205b, and finally, for the locations of third elementary emitting zones, by an OLED stack of type third OLED stack type 205c.
[0130] In a second subgroup of steps, the result of which is illustrated in [Fig. 16], a photoresist 280a is arranged on the first of these groups of elementary emitting zones. This photoresist 280a must protect the horizontal surface of the elementary emitting zone, but also its side (i.e. its lateral surface, which may be vertical).
[0131] In a third subgroup of steps, the result of which is illustrated in [Fig. 17], the stack formed by (listed from top to bottom) the encapsulation layer 290a, the upper electrode 207a, and the OLED stack 205a is etched on the areas not protected by the photoresist 280a. The etching method must be chosen so that the etching stops at the upper horizontal surface of the electrodes 202b and 202c. For etching the encapsulation layer and the electrode, a wet etching is typically used, for example a wet etching usually used in microelectronics, namely stripping with an aqueous solution of tetramethylammonium hydroxide (CAS No.: 75-59-2) at 2.38% by mass; such a product is commercially available, for example from ThermoFischer Scientific™ (electronic grade, catalog no. 44940).Alternatively, a dry etching method can also be used, for example by RIE (Reactive-Ion Etching) or IBE (Ion Beam Etching). The etching of the OLED stack is typically carried out by an oxygen plasma.
[0132] In a fourth subgroup of steps, the result of which is illustrated in [Fig. 18], the photoresist 280a is removed. This can be done by a suitable technique, known to those skilled in the art.
[0133] If an oxygen plasma is used to etch a layer deposited directly on the upper electrode for this purpose, it is preferable to avoid the upper surface of the upper electrode being made of aluminum, because the oxygen plasma will create an insulating alumina layer. Aluminum can be used provided that its upper surface is protected by a transparent conductive layer which is not attacked by the oxygen plasma; for this purpose, a tin dioxide (SnO2) layer is advantageously used.
[0134] In a second group of steps, shown schematically in [Fig. 19] to [Fig. 22], a second group of elementary emitting zones (sub-pixels) is deposited, emitting light of a second color, which is different from said first color, for example green.
[0135] In a first subgroup of steps, the result of which is illustrated in [Fig. 19], the following are successively deposited on this substrate 210: (a) a second OLED stack 205b, deposited with a directional deposition technique; (b) an upper electrode 207b, preferably with the same material as that used for the upper electrode 290a of the first group of elementary emitting zones, and (c) a second encapsulation layer 290b', preferably with the same material as that used for the first encapsulation layer 290a of the first group of elementary emitting zones. It is noted that at the end of the first subgroup of steps, the OLED stack deposited on the electrode 202c of the third group of elementary emitting zones is an OLED stack of the second OLED stack type. As will be explained below, in later stage groups it will subsequently be replaced by a third-type OLED stack 205c OLED stack.It is also noted that the elementary emitting zones of the first group comprise a stack called here “transient stack” consisting of an OLED stack 207b of the second OLED stack type, an upper electrode 207b and an encapsulation layer 290b; this transient stack will be removed subsequently. The encapsulation layer 290b covers in particular the sides of the OLED stack 205b. It is designated here, according to its position relative to the final device, by the numerical references 290a, 290b, 290c, while it is the same material. It can be continuous and then extends over the three elementary emitting zones.
[0136] In a second subgroup of steps, the result of which is illustrated in [Fig.20], a photoresist 280b is arranged on a second of these groups of elementary emitting zones, as described in relation to the first group of steps.
[0137] In a third subgroup of steps, the result of which is illustrated in [Fig. 21], the stack formed by (listed from top to bottom) the second encapsulation layer 290b, the upper electrode 207b, and the OLED stack 205b is etched on the areas not protected by the photoresist 280b. The etching method and the materials of the different layers must be chosen so that the etching stops at the upper horizontal surface of the electrode 202c and at the insulating layer 223 and the encapsulation layer 290a. Said insulating layer 223 may be made of Al2O3, which has the advantage of resisting etching with oxygen plasma which is used to remove the OLED stack. The same material is used for the encapsulation layer 290.
[0138] In a fourth subgroup of steps, the result of which is illustrated in [Fig.22], the photoresist 280b is removed, as described in relation to the first group of steps, and with the same remarks concerning the choice of techniques and protection of the upper aluminum electrode against possible oxygen plasma.
[0139] In a third group of steps, shown schematically in [Fig.23] to [Fig.26], a third group of elementary emitting zones (sub-pixels) is deposited, emitting light of a third color, which is different from said first color and said second color, for example blue.
[0140] In a first subgroup of steps, the result of which is illustrated in [Fig.23], the following are successively deposited on this substrate 210: (a) a third OLED stack 205c, deposited with a directional deposition technique; (b) an upper electrode 207c, preferably with the same material as that used for the upper electrode 207a and / or 207b of the first and second group of elementary emitting zones, and (c) a third encapsulation layer 290c, preferably with the same material as that used for the first and / or second encapsulation layer 290a, 290b of the first and second group of elementary emitting zones.
[0141] We note the presence of a transient stacking on the elementary emitting zones of the first and second groups.
[0142] In a second subgroup of steps, the result of which is illustrated in [Fig.24], a photoresist 280c is arranged on the third of these groups of elementary emitting zones, as described in relation to the first group of steps.
[0143] In a third subgroup of steps, the result of which is illustrated in [Fig. 25], the stack formed by (listed from top to bottom) the third encapsulation layer 290c, the upper electrode 207c, and the OLED stack 205c is etched on the areas not protected by the photoresist 280c. The etching method must be chosen so that the etching stops at the encapsulation layer 290a and 290b; an oxygen plasma is advantageously used to etch the OLED layer.
[0144] In a fourth subgroup of steps, the result of which is illustrated in [Fig.26], the photoresist 280c is removed, as described in relation to the first group of steps, and with the same remarks concerning the choice of techniques and protection of the upper aluminum electrode against a possible oxygen plasma.
[0145] The invention has many advantages. It makes it possible to produce OLED microdisplays with three elementary subpixels (typically RGB), having a very fine resolution with sizes of elementary emission zones (subpixels) below 20 pm, preferably below 10 pm, and even more preferably below 5 pm thanks to the high resolution of the photolithography methods used. These microdisplays have excellent efficiency and brightness thanks to the use of different OLED stacks per group of subpixels. pixel, which are optimized with respect to an emission of the primary color of the respective sub-pixel, thanks to the high surface density of elementary emitting zones, and thanks to the absence of color filters. They have excellent reliability, thanks to the total protection, including lateral, of the OLED stacks during the etching steps and throughout the lifetime of the device. Each elementary emission zone being separated and isolated from the neighboring elementary emission zones, the device avoids diatony.
[0146] These microdisplays use the subpixel arrangement shown schematically in the left representation of [Fig.2]. This arrangement is compatible with the positioning of the connection bars 217 for the upper electrode.
[0147] The manufacturing method uses known techniques and methods for manufacturing semiconductor and microelectronic devices, as well as current methods for manufacturing OLEDs. A particular advantage of the method according to the invention lies in the fact that it does not require the OLED stacks to be deposited through stencils having small openings, i.e. the size of the elementary emitting zone. This is illustrated here by [Fig. 27] which shows the opening 310 of a stencil 300 (“shadow mask” in English) placed on the surface of the substrate shown in [Fig. 7]. In the method according to the invention, the deposition of the OLED stack is common to all the elementary emitting zones.It is by etching a surface partially masked by photoresist pads, the latter using techniques allowing a lateral resolution significantly better than the stencil, that elementary emitting zones of very small dimensions are obtained; these dimensions can be approximately 5 pm or preferably less than 5 pm, or even less than 4 pm, or even less than 3 pm. In an advantageous embodiment these dimensions are between approximately 2 pm and approximately 5 pm.
[0148] The upper electrode 207 (generally the cathode) is also deposited in a common manner to all the elementary emitting zones, through the opening 410 of a stencil 400 which is shown schematically in [Fig.28]. As can be seen by comparing [Fig.28] with [Fig.7], the opening covers the connection bar 217 to which the upper electrode 207 is therefore electrically connected.
[0149] The invention can be implemented with many variants. A first variant is shown in [Fig.29], it is compatible with all the other variants of the invention. Usually, around the active area of a substrate 210 as shown in [Fig.7], at least one row of non-functional sub-pixels 270 (“dummy zone” in English) is placed. In other words, on such a substrate 210, the first and last rows of elementary emitting zones (sub-pixels) can be non-functional. This is very useful (or even necessary) in order to absorb the low masking precision during the deposition of the OLED stack: the dummy zone is used to limit the depositing the OLED layers on this area, and ensuring good contact between the upper electrode 207 and the connection bar 217.
[0150] In the variant shown in [Fig.29], the rows of non-functional sub-pixels 217 can be replaced by a connecting bar 217 which takes the form of a comb, the teeth of the comb 218 representing the dummy zone. The latter limits the deposition of the OLED layers on this zone while guaranteeing good electrical contact between the upper electrode 207 and the connecting bar 217, at least on the outer part of the connecting bar 217.
[0151] A second variant is shown in [Fig.30], [Fig.31] and [Fig.32]. It is compatible with all the other variants of the invention. This variant concerns the positioning of the insulating layer 223 relative to the filling element 203: the filling element 203 is first deposited in the natural space 211 between two neighboring electrodes 202, and then the insulating layer 223. This variant has the advantage of avoiding the attack of the filling element 203 during the etching of the OLED stacks.
[0152] [Fig.30] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate which represents a variant of the intermediate product of [Fig.7]; this section is analogous to that of [Fig.9]. In this variant, section AA corresponds to [Fig.8].
[0153] [Fig.31] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate which represents a step subsequent to that of the intermediate product of [Fig.30]. In this variant, the section AA corresponds to [Fig.10],
[0154] [Fig.32] schematically shows a perpendicular cross-section of a structured stack of layers, represented in a zy plane along the line BB indicated in [Fig.7], on a substrate one step later than that of the intermediate product of [Fig. 14]. In this variant, the section AA corresponds to [Fig. 13]
[0155] A third variant is illustrated in [Fig.33] and [Fig.34]: it is compatible with all the other variants of the invention. This variant concerns the filling element with insulating surface 203 (also called "gap fill") which fills the natural space 211 between two neighboring electrodes 202a, 202b; 202b, 202c; 202c, 202a. As stated above, the filler element 203 advantageously has a rim on the control electrode 202, and the thickness of the control electrodes 202 is advantageously greater than that of the OLED stacks 205.These thicknesses, as well as that of said filling element 203, are advantageously chosen so as to avoid that on the filling element. with insulating surface 203, the angle alpha with respect to the horizontal upper surface of the electrode 202 does not exceed at any point a value X which is approximately 40°, preferably approximately 30°, more preferably approximately 25°, and even more preferably approximately 20°, knowing that it can be a positive or negative angle. This definition of the angle alpha is clarified in [Fig.33] on which, for two different geometries, the largest angle alpha has been indicated.
[0156] Thus, the filler element 203 acts as a smoothing element for the deposition of the common electrode layer 207. This common electrode 207 is deposited by a directional deposition technique, and this creates a risk of electrical discontinuity in the case where at any point on the surface of the control electrode, the angle alpha exceeds a value of approximately 30° (positive or negative) relative to the horizontal upper surface of the control electrode. This is explained by the fact that a directional deposition technique does not deposit the same thickness of material on a horizontal surface as on a sloping surface (and does not deposit anything at all on a vertical surface).
[0157] [Fig.33] illustrates this situation schematically, while [Fig.34] shows a schematic drawing from a scanning electron microscopy image of a corresponding cross-section.
Claims
1. Claims Electroluminescent display device comprising a matrix of electroluminescent pixels formed of a plurality of pixels deposited on a substrate (210), in a matrix arrangement in rows and columns, each pixel being formed of at least three elementary emitting zones, each of said at least three elementary emitting zones belonging to a different group of elementary emitting zones which is distinguished from the elementary emitting zones belonging to other groups by its emission color, each elementary emission zone comprising an electroluminescent stack of organic layers (205), called "OLED stack", which comprises at least one light-emitting organic layer, said OLED stack (205) being arranged between a control electrode (202) and a transparent upper electrode (207), said transparent upper electrode (207) being traversed by the light emitted by the OLED stack (205),said electroluminescent display device being characterized in that: two neighboring control electrodes (202a, 202b; 202b, 202c; 202c, 202a) belonging to two neighboring elementary emitting zones which each belong to a different group of elementary emitting zones are separated by a space (211) forming a trench and having an insulating surface (223) which covers at least the vertical sides of said neighboring electrodes and electrically insulates them from each other, and two neighboring control electrodes (202a, 202a; 202b, 202b, 202c, 202c) belonging to two neighboring elementary emitting zones which each belong to the same group of elementary emitting zones are separated by a space (211) forming a trench, said space being filled with a filling element (203) which insulates said electrodes electrically adjacent to each other and fills the natural space between said two electrodes,in each group of elementary emitting zones, the entire OLED stack with its corresponding upper electrode, (205a with 207a, 205b with 207b, 205c with 207c) is separated from neighboring sets belonging to another group by an encapsulation layer (290) which protects said OLED stack on its upper face and its lateral sides against the ambient air, thus forming protected islands (225), each island comprising sets of OLED stacks of the same group, with their upper electrode.
2. Device according to claim, characterized in that said emission colors are red, blue and green.
3. Device according to claim 1 or 2, characterized in that the width of said trench-forming space is between 0.3 pm and 1.0 pm.
4. Device according to any one of claims 1 to 3, characterized in that the depth of said trench-forming space is between approximately 150 nm and approximately 850 nm, and preferably between 150 nm and 450 nm.
5. Device according to any one of claims 1 to 4, characterized in that the thickness of said control electrodes (202) is between approximately 150 nm and approximately 800 nm, and preferably between 150 nm and 450 nm.
6. Device according to any one of claims 1 to 5, characterized in that the thickness of said control electrodes (202) is greater than that of the OLED stacks (205).
7. Device according to any one of claims 1 to 6, characterized in that said filling element (203) fills the natural space between two neighboring control electrodes (202) so that said upper electrode (207) is substantially planar.
8. Device according to any one of claims 1 to 7, characterized in that the pitch of the elementary emitting zones is less than approximately 20 pm, preferably less than approximately 15 pm, more preferably less than approximately 10 pm, and even more preferably between approximately 1 pm and approximately 5 pm, and in that the width of the space between control electrodes is less than approximately 1 pm, and preferably between approximately 0.3 pm and approximately 1.0 pm.
9. Device according to any one of claims 1 to 8, characterized in that on the filling element with insulating surface
10. 203, the angle alpha relative to the horizontal upper surface of the electrode 202 does not exceed at any point a value which is approximately 40°, preferably approximately 30°, more preferably approximately 25°, and even more preferably approximately 20°, knowing that it can be a positive or negative angle. A method of manufacturing an electroluminescent display device comprising a matrix of electroluminescent pixels formed of a plurality of pixels deposited on a substrate (210), in a matrix arrangement in rows and columns, each pixel being formed of at least three elementary emitting zones, each of said at least three elementary emitting zones belonging to a different group of elementary emitting zones which is distinguished from the elementary emitting zones belonging to other groups by its emission color, each elementary emission zone comprising an electroluminescent stack of organic layers (205), called "OLED stack", which comprises at least one light-emitting organic layer, in which method: a substrate (210) is provided with a control electrode (202a, 202b, 202c) for each elementary emitting zone and an insulating layer (223) between two neighboring electrodes (202a, 202b, 202c), and provided with filling elements between two neighboring elementary emitting zones belonging to the same group of elementary emitting zones, in a first group of steps a first OLED stack (205a), an upper electrode (207a) and, using a conformal deposition technique, a first encapsulation layer (290a) are first deposited, then a photoresist is arranged at the location of the elementary emission zones of the first group which protects the horizontal surface and the flank of said encapsulation layer (290a) at the location of said elementary emission zones of the first group, and the areas not protected by the photoresist to the upper surface of the control electrode (202b and 202c), and finally said photoresist is removed,in a second group of steps, a second OLED stack (205b) is first deposited, an upper electrode (207b) and, using a conformal deposition technique, a second encapsulation layer (290b), then a photoresist is arranged at the location of the emission zones of the second group which protects the horizontal surface and the flank of said encapsulation layer (290b) at the location of said elementary emission zones of the second group, and the zones not protected by the photoresist are etched up to the upper surface of the control electrode (202c) for the elementary emission zones of the third group and up to the surface of the first encapsulation layer for the elementary emission zones of the first group, and finally said photoresist is removed, in a third group of steps, a third OLED stack (205c), an upper electrode (207c) and, using a conformal deposition technique, a third encapsulation layer (290c) are first deposited, then a photoresist is arranged at the location of the emission zones of the third group, which protects the horizontal surface and the flank of said encapsulation layer (290c) at the location of said elementary emission zones of the third group, and the zones not protected by the photoresist are etched up to the surface of the first encapsulation layer for the elementary emission zones of the first and second groups, and finally said photoresist is removed.