Method of providing anti-corrosion coatings comprising polyamide-imides

By incorporating nanoplatelets like graphene into polyamide-imide coatings, the electrical conductivity and corrosion protection issues of PAIs are addressed, resulting in a coating that significantly enhances the lifespan of energy storage devices.

GB2608977BActive Publication Date: 2024-12-04VERSARIEN PLC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
GB2022016313
Authority / Receiving Office
GB · GB
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-04-03
Filing Date
2021-04-06
Publication Date
2024-12-04
Estimated Expiration
2041-04-06

AI Technical Summary

Technical Problem

Polyamide-imides (PAIs) lack electrical conductivity, making them unsuitable for applications requiring this property, such as energy storage devices where corrosion of metallic electrodes by corrosive electrolytes significantly affects device lifespan, and there is a need for an anti-corrosion coating that is also electrically conductive.

Method used

A method involving dispersing nanoplatelets, such as graphene, in a liquid to form an aqueous dispersion and blending with a polyamide-imide precursor, followed by coating, drying, and curing, which results in a conductive and thermally conductive coating that protects electrodes and current collectors in energy storage devices.

Benefits of technology

The resulting composite coating exhibits enhanced electrical conductivity, improved adhesion, and extended device longevity by preventing corrosion while maintaining mechanical and chemical properties of PAIs, with the best electrical conductivity being 0.2 S/m, significantly higher than previous PAI-based coatings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000001_0000
    Figure 00000001_0000
  • Figure 00000001_0001
    Figure 00000001_0001
  • Figure 00000002_0000
    Figure 00000002_0000
Patent Text Reader

Abstract

High performance polyamide-imide composites which are also electrically conductive are disclosed. The composites are made by mixing water-based dispersions of graphene with water-based polyamide-imide precursors. These composites are especially useful as anti-corrosion and anti-wear coatings, especially to protect electrodes in energy storage devices from corrosive electrolytes.
Need to check novelty before this filing date? Find Prior Art

Description

The present invention relates to high performance composites, particularly coatings, based on polyamide-imides and layered two-dimensional materials such as graphene. 5 BACKGROUND TO THE INVENTION Polyamide-imides (PAIs) are high performance engineering plastics. They have outstanding thermal, mechanical and chemical properties and are often used in demanding applications where very high mechanical strength, stiffness and low friction in combination with high temperature, corrosion and wear resistance are required. 10 An aqueous-based PAI composition is disclosed in US6479581, and a product is commercially available under the registered trade mark Torlon. PAIs can be processed into a variety of forms, such as injection or compression moulded articles, coatings, films, fibres and adhesives. In many cases, PAIs can replace metals in structural applications. However, in terms of electrical properties, 15 PAIs are essentially insulators - the maximum reported electrical conductivity is 5 x 10 GSm'1. Whilst this can be useful in some applications (for example, PAIs are used as insulating wire coatings), PAIs are not generally useful in applications where electrical conductivity is required. Energy storage devices, e.g. batteries and supercapacitors, have lifespans which are 20 greatly affected by the corrosion of metallic electrodes by the corrosive electrolytes used in these devices. There are currently no known good anti-corrosion coatings which are suitable in this application. It is an object of the invention to provide a PAI material with enhanced electrical conductivity. It is a further object to provide an electrically conductive anti-corrosion 25 coating, particularly for use in protecting electrodes and / or current collectors in energy storage devices. It is a further object of the invention to provide PAI and nanomaterial composites with enhanced properties. STATEMENT OF INVENTION According to the present invention there is provided a method of protecting an 30 electrode and / or an current collector in a energy storage device by providing an anti 16 08 24 corrosion conductive coating on the electrode or current collector, the method comprising: dispersing nanoplatelets of less than 20nm thick in a liquid including water to form an aqueous dispersion of nanoplatelets; 5          dissolving a polyamide-imide precursor in at least water to form an aqueous solution; blending the aqueous dispersion of nanoplatelets with the aqueous solution; coating the article with the blended mixture; drying and curing the coating by applying heat. Curing the coating can be also 10 performed on substrates not compatible with high temperatures (such as PET) by localised infrared or xenon flash lamp curing. Typically, the coating is cured in an oven at about 260 degrees Celsius for at least about 30 min. The oven may be a vacuum furnace. In some embodiments, there may be a distinct drying I evaporation phase where the solvent is removed, followed by a 15 higher temperature curing phase where the PAI is formed from the precursor. This is in accordance with the known procedure for drying and curing PAI - and the manufacturer’s instructions for Torlon (RTM). The addition of nanoplatelets is found not to significantly affect the curing process. If the coating is placed on substrates that are not compatible with oven curing at high 20 temperature, localised infrared or xenon flash lamp curing can be used to cure such coatings and the curing conditions vary depending on the coating thickness. The typical curing conditions using a xenon flash lamp would be as below (Figure X).Voltage: 300V, Pulse duration <2 ms, Frequency 1 Hz, Number of pulses: 10, Distance ~10 mm 25 The coating may be electrically conductive and / or thermally conductive. A “nanoplatelet” is a high aspect ratio structure (i.e. length / thickness > 10 but preferably much greater, for example up to around 1000). Typically the thickness of a nanoplatelet is < 100nm, preferably < 50nm and most preferably <20nm, for example 1 - 15nm thick. The nanoplatelets consist of small stacks of a two-dimensional 30 material, for example a stack fewer than 15 atoms thick. In some embodiments the nanoplatelets may be a single atom thick. 16 08 24 Nanoplatelets may be made according to the method disclosed in WO2017060497, which is incorporated herein by reference. The nanoplatelets may be graphene. The loading of nanoplatelets in the aqueous dispersion of nanoparticles may be around 5   100 mg / mL. The ratio of polymer / nanoplatelets by mass, in the finished dry coating, may be less than 0.3, or less than 0.5. In other words, the finished coating may be at least 50% or at least 70% nanoplatelets. Significantly less polymer than this, the coating is found to have decreased scratch resistance and anti-corrosive properties, since the polymer cannot cross-link to form a continuous surface which protects the 10 article being coated. Nevertheless such products, although not having such desirable anti-corrosion properties, may have applications in for example lubrication and antifouling. 50% or 70% or more nanoplatelets by mass provides for good electrical conductivity which is useful in many applications. The best electrical conductivity achieved so far in a coating according to the invention 15 and using graphene nanoplatelets is 0.2 Snr1. This is more than 104 times greater than the best values reported for Torlon (RTM). The coatings show very good adhesion to metal and other substrates. The coating has been tested on aluminium, stainless steel, and Kapton (registered trade mark for a polyimide film available from DuPont). 20 In another embodiment, the nanoplatelets may be boron nitride (BN) nanoplatelets, for example hexagonal boron nitride (hBN) nanoplatelets. Use of BN, especially hBN, significantly improves the heat dissipation and thermal reflection properties of PAI. PAI is already inherently flame retardant and a BN / PAI composite coating has increased flame retardant or flame resistant properties, and may be useful in fire protection. It is 25 envisaged that other nanomaterials may be added to PAI in the same way to produce other desirable properties. In one embodiment, the nanoplatelets may comprise both graphene and BN. In other embodiments the nanomaterial may consist of or include, as well as or instead of graphene and / or BN, other materials in nanoplatelet form, for example 30 semiconductors. Molybdenum Disulfide (MoS2) and Tungsten Disulfide (WS2) have particularly interesting properties as lubricants. 16 08 24 In other aspects, an organic solvent, for example N-Methyl-2-pyrrolidone (NMP), may be used as well as or instead of water, to produce non-aqueous solutions and / or non aqueous dispersions. According to another aspect of the invention there is provided a composite material 5 including: a polyamide-imide and; nanoplatelets. The nanoplatelet material may be graphene, BN, especially hBN, Molybdenum Disulfide (MoS2), Tungsten Disulfide (WS2), or other materials or combinations. 10 The composite material may be used as a coating, or in other applications. For example, films, fibres, and adhesives may be produced. Solid articles may be made by injection or compression moulding. It is also envisaged that a composite enhanced lubricant could be made from polyamide-imide and nanoplatelets. Depending on the application and the processing of the composite material, the composite material may 15 be made according to the first aspect of the invention, or in other ways. For example, dry graphene powder (i.e. dry nanoplatelets) could be added directly to the aqueous solution of the PAI precursor. Further alternatively, the PAI precursor could be provided as a powder and added to the aqueous dispersion of nanoplatelets. Solvents other than water may be used. For example, an organic solvent such as N-Methyl-2- 20 pyrrolidone (NMP). In yet further embodiments, the nanoplatelets may be mixed with already-formed PAI, rather than with a PAI precursor, and combined by melting or otherwise. Nanoplatelets of different types can be used to provide different desirable properties in the composite. For example, hBN nanoplatelets provide good thermal dispersion 25 properties, and the resulting composite may have applications in fire protection as a thermal spray I flame spray, fire retardant coating, or in fibres used to make fire retardant clothing. Thermal dispersion properties are also useful in many aerospace, automotive, and oil and gas applications. Preferable I optional features of the second aspect of the invention are set out in claims 30    11 to 15. 16 08 24 According to another aspect of the invention there is provided an energy storage device which includes an electrolyte and one or more electrodes and / or current collectors, in which at least one of the electrodes I current collectors is coated with a polyamide-imide coating containing electrically conductive nanoplatelets, the electrode 5 I current collector being in electrical contact with the polyamide-imide coating and the polyamide-imide coating being in electrical contact with the electrolyte. Energy storage devices in this aspect of the invention include batteries (i.e. galvanic cells), supercapacitors, and fuel cells. More generally electrodes or current collectors in all kinds of electrochemical cell and other devices which include electrodes and 10 electrolyte or analogous parts, may benefit from the polyamide-imide coating of the invention. The polyamide-imide coating contains nanoplatelets, preferably graphene. The nanoplatelets enhance the conductivity of the polyamide-imide material. The coating therefore protects the electrodes from corrosion due to the electrolyte, while allowing 15 the energy storage device to work properly by providing an electrical conductor between the electrode and the electrolyte. As a result, the longevity of the energy storage device is much improved. Preferable I optional features of the third aspect of the invention are set out in claims 17 to 19. 20 BRIEF DESCRIPTION OF THE DRAWINGS For a better understanding of the present invention, and to show more clearly how it may be carried into effect, reference will now be made by way of example only to the accompanying drawings, in which: Figure 1 is a photograph of aluminium foil (on the left) and Kapton (RTM) film (on the 25 right) coated with a polyamide-imide composite according to the invention; Figure 2 is a graph showing the results of an open circuit potential (OCP) corrosion test carried out on three different coatings; Figure 3a and 3b show the results of an electrochemical impedance spectroscopy (EIS) corrosion test carried out on two different coatings; 30 Figure 4 shows the results of an OCP corrosion test carried out on the two coatings of the test in figures 3a and 3b, after the EIS test was carried out; Figure 5 is a photograph of the two coatings, after the corrosion tests were carried out; 16 08 24 Figure 6 is a series of scanning electron micrographs (SEM) of one coating; Figure 7 is a series of scanning electron micrographs (SEM) of another coating; Figure 8a shows apparatus for curing coatings, the apparatus comprising a xenon 5 pulsed lamp and a thermal imaging camera; and Figure 8b shows an image from the thermal imaging camera in Figure 8a. DESCRIPTION OF PREFERRED EMBODIMENTS Coatings according to the invention have been manufactured by mixing a water-based PAI precursor with a dispersion of graphene nanoplatelets. The PAI precursor is 10 Torlon (RTM) AI-50 obtained from the manufacturer Solvay (RTM) as a water-based solution. The graphene nanoplatelets are dispersed in water - a suitable dispersion is Graphink (RTM) 2, available from Cambridge Graphene Limited. Torlon (RTM) AI-50 has a concentration of 9% solids in water. Graphink (RTM) 2 has a concentration of 10% solids in water. 15 Experiments have been carried out with different ratios of PAI solution and graphene dispersion, as shown in table 1 and table 2 below. Torlon / GNP GNP / Torlon Finger rub test Scratch test Sheet resistance (Q) / sq 2P resistance over 1cm (O) 1.06 0.94 Pass Pass 316 930 0.80 1.26 Pass Pass 129 510 0.53 1.89 Pass Pass 66 320 0.27 3.77 Pass Fail 114 200 0.13 7.55 Pass Fail 55 160 fable 1 - Initial tests Coating # PAI solution Graphlnk2 wt (g) PAI solution / PAI wt% in Substrate Coating method 2P resistance (O) Anticorrosion test 16 08 24 wt (g) Graphlnk2 wt ratio final coating 10 10 0 10:0 100 Al Drop cast N / A Pass 9 9 1 9:1 89.01 Tested both Al and Kapton Bar coat Pass 8 8 2 8:2 78.26 Kapton Bar coat Pass 7 7 3 7:3 67.74 Al Bar coat Pass 6 6 4 6:4 57.45 Kapton Bar coat Pass 5 5 5 5:5 47.37 Al Spray 700 Pass 3 3 7 3:7 27.84 Al Spray Pass 2 2 8 2:8 18.37 Al Spray 20 Pass 1 1 9 1:9 9.09 Al Spray 20 Fail after 3 hours Table 2 - further tests Figure 1 shows a coating (coating number 8 in table 2) applied to (on the left) aluminium foil and (on the right) Kapton film. The coatings adhere well to both substrates and produce a polished I shiny finish on the surface. The sheet resistance 5 was measured by a four-point probe and the results are shown in table 1. A more basic two-point test to measure the resistance was carried out and the results are shown in column 6 of table 1. The resistivity of the coating decreases as the dosing of graphene nanoplatelets is increased. The four-point result for the 2g Torlon coating is thought to be a measurement error I experimental anomaly. 10 As noted in table 2, spray coating and bar coating have been tested. Spray coating involves the deposition of the PAI I graphene mixture as a coating onto the substrate by spraying the solution onto the heated substrate. The substrate may be heated to about 100 degrees Celsius. This method works well for coatings with relatively low polymer contents. 15 With higher polymer contents, the viscosity is higher, and so bar coating is used. In bar coating, an excess of the PAI / graphene mixture is placed on the substrate and 16 08 24 spread by rolling a bar across the substrate. The bar is a spiral film applicator -essentially a cylindrical bar with wire spiralling around it. The gap between the wire and the substrate determine the thickness of the coating. For the most viscous coating tested (all polymer, no graphene), the liquid is very 5 viscous and cannot be spray or bar coated. The liquid is manually spread into a layer. It is envisaged that other printing I coating methods, for example inkjet, flexo, gravure, screen printing, dip coating, slot die coating may be used. Although coating 1 in table 2 failed the anticorrosion test, it is thought that with increased film thickness, good performance for some applications may be achieved. 10   Work is ongoing to deposit thicker coatings made from these mixtures. Poor corrosion performance is thought to result from tiny breaks (which could be on nanometre scales) in the coating. Therefore coatings with high nanoplatelet loading, and consequently high conductivity, may still provide good anticorrosion performance when applied in a sufficiently thick coat. 15 Scratch and wear resistance were assessed by basic “finger rub” and scratch tests. It was found that a coating containing less than around a third PAI by mass did not provide good wear and scratch resistance. However this may not be a problem in some applications. Further tests were carried out on different coatings as shown in Table 2. In these tests, 20 the performance of the coatings to prevent electrochemical corrosion was tested. After coating a substrate and allowing the coating to cure and dry, a 1cm diameter circular area of the coated substrate was exposed to an electrolyte, the electrolyte having a pH of around 4.4 and consisting of zinc chloride and ammonium chloride in deionised water. The open circuit potential (OCP) is measured between the working electrode 25   (i.e, the coated substate being tested) and the reference electrode. Selected results are shown in Figure 2. It is seen that coating number 5 and coating number 7 show good corrosion resistance for the duration of the experiment (120 hours). Coating number 2 degraded after around 80 hours. The results of this second set of experiments were in line with the first basic scratch and wear tests. 30 Figures 3a and 3b show the results of a standard electrochemical impedance spectroscopy (EIS) accelerated corrosion test carried out on two different coatings (in Figure 3a, coating number 7 of table 2, and in Figure 3b, coating number 5 of table 2). Each plot shows minimal degradation during the test. 16 08 24 Figure 4 shows the results of a repeat of the open circuit potential (OCP) test (see description of Figure 2 above), performed after the EIS accelerated corrosion test. These results confirm that both coatings have not undergone significant corrosion. Figure 5 shows a photograph of coated substates after the above-described corrosion 5 tests were carried out. The coatings show no visible signs of corrosion. Figure 6 shows a scanning electron micrograph (SEM) of coating number 7 in table 2. The top micrographs in the figure are from outside the tested area, i.e. outside the area exposed to the corrosive electrolyte. The bottom micrographs are from inside the area exposed to the corrosive electrolyte. The polymer appears to provide good coverage 10 over the graphene flakes; as a result it is difficult to focus the micrograph to see individual flakes. Figure 7 shows an SEM of coating number 1 in table 2. It is clear that with this lower amount of polymer, there is no good continuous coverage. The coating shows significant cracks and the aluminium surface is exposed. It is apparent that significant 15 changes to the surface have occurred as a result of exposure to the corrosive electrolyte. Figure 8a shows a xenon pulsed lamp apparatus for curing the graphene I PAI coating on a PET substrate. Figure 8b is a thermal image taken during the curing process. The composites of the invention provide a material with the desirable mechanical and 20 anti-corrosion properties of PAI, but which are electrically conductive due to the addition of graphene nanoplatelets. These composites may have particular applications as coatings for protecting electrodes in energy storage devices, for example batteries and supercapacitors. The embodiments described above are provided by way of example only, and various 25 changes and modifications will be apparent to persons skilled in the art without departing from the scope of the present invention as defined by the appended claims.

Claims

1. A method of protecting electrodes and / or current collectors in energy storage devices by providing an anti-corrosion conductive coating on a substrate, the method comprising:5                  dispersing nanoplatelets of less than 20nm thick in a liquid includingwater to form an aqueous dispersion of nanoplatelets;dissolving a polyamide-imide precursor in at least water to form an aqueous solution;blending the aqueous dispersion of nanoplatelets with the aqueous10solution;19 06 24coating the substrate with the blended mixture;drying and curing the coating by applying heat by vacuum or convection oven.

2. A method as claimed in claim 1, in which the nanoplatelets include graphene 15           nanoplatelets.

3. A method as claimed in claim 1 or claim 2, in which the loading of nanoplatelets in the aqueous dispersion of nanoplatelets is at least 50mg / mL.

4. A method as claimed in claim 3, in which the loading of nanoplatelets in the aqueous dispersion of nanoplatelets is at least 80mg / mL.20       5. A method as claimed in claim 4, in which the loading of nanoplatelets in theaqueous dispersion of nanoplatelets is at least 90mg / mL.

6. A method as claimed in any one of claims 2 to 5, in which the nanoplatelets form at least 60% by mass of the cured and dried coating.

7. A method as claimed in claim 6, in which the nanoplatelets form at least 70% 25          by mass of the cured and dried coating.

8. A method as claimed in any of claims 1 to 7, in which the nanoplatelets include boron nitride (BN) nanoplatelets.19 06 249. A method as claimed in claim 8, in which the nanoplatelets include hexagonal boron nitride (hBN) nanoplatelets.

10. An energy storage device including:an electrolyte; and5                 one or more electrodes and / or current collectors,in which at least one of the electrodes I current collectors is coated with a polyamide-imide coating containing graphene nanoplatelets, the electrode I current collector being in electrical contact with the polyamide-imide coating and the polyamide-imide coating being in electrical contact with the electrolyte.10       11. An energy storage device as claimed in claim 10, in which the nanoplateletsare less than 20nm thick.

12. An energy storage device as claimed in claim 10 or claim 11, in which the coating comprises at least 60% nanoplatelets by weight.

13. An energy storage device as claimed in claim 12, in which the coating 15          comprises at least 70% nanoplatelets by weight.

14. An energy storage device as claimed in any one of claims 10 to 13, in which the energy storage device is a galvanic cell.

15. An energy storage device as claimed in any one of claims 10 to 13, in which the energy storage device is a supercapacitor.20       16. An energy storage device as claimed in any one of claims 10 to 13, in whichthe energy storage device is a fuel cell.

Citation Information

Patent Citations

  • Nanometer protective coating special for aluminum non-stick pan, preparing method and coating technology of coating

    CN110066596A

  • Silicon-graphene nanocomposites for electrochemical applications

    EP3069398A1

  • Sliding engine component

    EP3169726A1

  • Low contact resistance PEM fuel cell

    US20040253505A1