Protective materials using expandable polyolefin composites

JP2023548308A5Pending Publication Date: 2024-11-07PREGIS INNOVATIVE PACKAGING INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023526138
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2020-10-29
Filing Date
2021-10-29
Publication Date
2024-11-07

AI Technical Summary

Technical Problem

Conventional low-density protective packaging materials are bulky and inefficient for transportation, increasing costs and reducing storage capacity due to their bulky, low-density configurations.

Method used

A protective material comprising first and second walls with an expandable composite of emulsion polyolefin dispersion and microspheres, allowing for low-volume, high-density packaging that can be expanded on-site to provide cushioning and insulation.

Benefits of technology

Enables efficient transportation and storage of packaging materials in a compact form while providing effective cushioning and insulation upon expansion, reducing transportation costs and increasing storage capacity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The present invention relates to a protective material comprising first and second walls. Each of the walls comprises superposed layers enclosing an expansion space therebetween, and an expandable composite disposed in the expansion space. The expandable composite comprises an emulsion polyolefin dispersion and a plurality of expandable microspheres. The expandable microspheres are configured to expand the emulsion polyolefin dispersion upon activation of the expandable microspheres. The present invention further relates to an intumescent web comprising a first layer, a second layer, and an expandable composite disposed between the first and second layers. The present invention also relates to a method for manufacturing the intumescent protective material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure generally relates to expandable polyolefin composites that, once expanded, provide, for example, cushioning, thermal insulation, and / or sound insulation. Further, the present disclosure relates to processes and apparatuses for manufacturing expandable polyolefin composites, as well as methods of using expandable polyolefin composites.

Summary of the Invention

Problems to be Solved by the Invention

[0002] Conventional low-density protective packaging materials, thermal insulation materials, and other low-density products are typically manufactured in a low-density configuration that is bulky. These bulky low-density configurations can include, for example, pre-formed and expanded fluid chambers (e.g., bubbles), pre-expanded foams, stuffing insertions, etc. These bulky low-density configurations are for supporting the packaging during shipping. However, before using them for packaging, they need to be shipped to the packaging and shipping locations.

[0003] Since the packaging material is already manufactured in a bulky, low-density configuration, it has to be transported as such. This increases the overall volume of the packaging material even before it is used for packaging, increases the transportation cost of the packaging material to the packaging and shipping locations, and reduces the amount of product that can be stored at those locations until use.

[0004] For at least such reasons, there is a need for systems and methods for manufacturing packaging materials in a low-volume, high-density configuration that can then be expanded later.

[0005] According to various embodiments of this disclosure, a protective material is provided. The protective material comprises first and second walls. Each wall comprises an overlapping layer (ply) enclosing an expansion space between them and an expandable composite material disposed within the expansion space. The expandable composite material comprises an emulsion polyolefin dispersion and a plurality of expandable microspheres. In some embodiments, the microspheres are encapsulated within the emulsion polyolefin dispersion. The emulsion polyolefin dispersion comprises one or more polyolefins, a polymer stabilizer comprising at least one polar polymer, and water. The expandable microspheres are configured such that the emulsion polyolefin dispersion expands upon activation of the expandable microspheres. The first and second walls are configured to house a product to be shipped and are overlapped with respect to a dimensionally defined container cavity between them, with the expansion spaces of the walls overlapping with respect to the container cavity. The first and second walls are connected to each other on multiple sides of the container cavity.

[0006] According to various embodiments, the walls can be made so as not to seal each other at the opening side of the container cavity, and this opening side is sized so that a product can be inserted into the container cavity through it. The protective material may further include a closure on the first wall configured to seal the first wall to the second wall in order to seal the opening side in order to hold the product inside the cavity.

[0007] According to various embodiments, the protective material may include a web defining a plurality of interconnected protective packaging units configured such that first and second walls are connected to and separated from one another at a series of positions. Each packaging unit may include a set of expansion spaces that surround a container cavity.

[0008] According to various embodiments, one or more polyolefins may be thermoplastic. One or more polyolefins may include ethylene-based thermoplastic polymers, propylene-based thermoplastic polymers, or combinations thereof. Ethylene-based thermoplastic polymers may include high-density polyethylene (HDPE), linear low-density polyethylene (LLDPE), low-density polyethylene (LDPE), or combinations thereof. Propylene-based thermoplastic polymers may be oriented polypropylene (OPP).

[0009] According to various embodiments, the expandable microspheres may include a blowing agent. In other embodiments, the microspheres may include a reactive component, a chemical catalyst, or a combination thereof. The expandable microspheres may include a blowing agent consisting of air, carbon dioxide, nitrogen, argon, helium, methane, ethane, propane, isobutane, n-butane, neopentane, an inert gas such as argon or helium, or a combination thereof. Multiple expandable microspheres may include an outer shell and an inner core. The outer shell of the expandable microsphere may contain one or more types of polyolefins.

[0010] According to various embodiments, multiple core materials can be separated from each other by an outer shell. The expandable microspheres may contain hydrocarbons, water, or a combination thereof. The expandable microspheres may be configured to be thermally activated. Activation causes the expandable microspheres to expand, thereby causing the emulsion polyolefin dispersion to expand. The emulsion polyolefin dispersion is configured to solidify after expansion.

[0011] According to various embodiments, a protective material is provided. The protective material includes a first wall. The first wall includes a first layer defining an expansion region and an expandable composite within the expansion region. The expandable composite comprises an emulsion polyolefin dispersion and a plurality of expandable microspheres. The emulsion polyolefin dispersion comprises one or more types of polyolefins, a polymer stabilizer comprising at least one polar polymer, and water. The expandable microspheres are configured such that the emulsion polyolefin dispersion expands upon activation of the expandable microspheres.

[0012] According to various embodiments, the first wall may include a second layer superimposed on and connected to the first layer, and the first and second layers shall define a first expansion space between them that encloses the expansion region. Additional expandable composite material may be housed in the first expansion space.

[0013] According to various embodiments, the protective material may further include a second wall. The second wall may include opposing substrate layers that are overlapped and connected to define a second expansion space between them, and additional expandable composite material contained within the second expansion space. The second and second walls are overlapped to define a dimensionally defined container cavity between them, where a product to be shipped is housed, and the expansion spaces of the walls overlap each other with respect to the container cavity. The first and second walls are connected to each other on multiple sides of the container cavity.

[0014] According to various embodiments, the expandable web comprises a first layer, a second layer, and an expandable composite deposited between the first and second layers. The expandable composite comprises an emulsion polyolefin dispersion and a plurality of expandable microspheres. The emulsion polyolefin dispersion comprises one or more polyolefins, a polymer stabilizer comprising at least one polar polymer, and water.

[0015] According to various embodiments, a method for producing an expandable protective material is provided. The method includes the step of coating an expandable composite onto the surface of a first layer. The expandable composite includes an emulsion polyolefin dispersion comprising one or more polyolefins, a polymer stabilizer comprising at least one polar polymer, and water, and a plurality of expandable microspheres configured to expand the emulsion polyolefin dispersion upon activation of the expandable microspheres. The method further includes the step of applying a second layer on top of the first layer such that the expandable composite is sandwiched between the first and second layers. [Brief explanation of the drawing]

[0016] The features of this disclosure described above and other features will become more fully apparent from the following description and the attached claims, which are to be interpreted in conjunction with the attached drawings. Understanding that these drawings are merely examples illustrating some aspects of this disclosure and should not be considered limiting its scope, this disclosure is described more specifically and in detail with reference to the attached drawings, which include the following:

[0017] [Figure 1] Figure 1 is a perspective view of the web of a fan-fold packaging unit according to one embodiment of the present disclosure. [Figure 2] Figure 2 is a schematic top and side view of one embodiment of a system for converting stock material into the separable protective packaging unit shown in Figure 1. [Figure 3] Figure 3 is a schematic top and side view of one embodiment of a system for converting stock material into the separable protective packaging unit shown in Figure 1. [Figure 4] Figure 4 is a top-view perspective of each of the web layers used in the systems of Figures 2 and 3 for making protective material. [Figure 5] Figure 5 is a top-view perspective of the web layer used in the systems of Figures 2 and 3 for creating protective material. [Figure 6]Figure 6 is a perspective and cross-sectional view of the web of the protective packaging unit formed by the systems of Figures 2 and 3 after folding the web of Figure 5 onto itself. [Figure 7] Figure 7 is a top and cross-sectional view of one embodiment of the web used to manufacture the protective material. [Figure 8] Figure 8 is a perspective and cross-sectional view of the web of Figure 7 folded onto itself. [Figure 9] Figure 9 is a cross-sectional view taken along the cutting plane X-X of Figure 3 of the folded web of Figures 5 - 6 in the systems of Figures 2 and 3. [Figure 10] Figure 10 is a cross-sectional view of the folded web of Figures 5 - 6 in the systems of Figures 2 and 3 taken along the cutting plane XI-XI of Figure 2. [Figure 11] Figure 11 is a perspective view of the web of the packaging unit in a fan-fold structure according to another embodiment of the present disclosure. [Figure 12] Figure 12 is a perspective and cross-sectional view of one embodiment of the supply roll of the web of the protective packaging unit using the web of Figure 1. [Figure 13] Figure 13 is a perspective view of another embodiment of the protective packaging unit having a closure flap. [Figure 14] Figure 14 is a perspective and cross-sectional view of a bagging machine including an inflation device according to one embodiment of the present disclosure. [Figure 15] Figure 15 is a front view of a bagging machine according to another embodiment of the present disclosure, respectively. [Figure 16] Figure 16 is a rear view of a bagging machine according to another embodiment of the present disclosure, respectively.

Mode for Carrying Out the Invention

[0018] In the following detailed description, reference will be made to the accompanying drawings that form a part hereof. In the drawings, like symbols generally identify like components unless the context indicates otherwise. The illustrative embodiments described in the detailed description, drawings, and claims are not intended to be limiting. Other embodiments may be utilized and other changes may be made without departing from the spirit or scope of the subject matter presented herein. Aspects of the present disclosure, as generally described and illustrated in the figures herein, can be arranged, substituted, combined, separated, and designed in a variety of different configurations, all of which are readily understood to be implicitly contemplated herein.

[0019] FIG. 1 shows an embodiment of a web 100 of protective material as a series of connected and separable protective packaging units 110 in a supply structure 150. The protective material can be selected to provide a stuffing and / or insulation material. For example, in one embodiment, the protective material is provided as a stuffing material inserted into a structure to provide structural stability to the structure such that the structure can withstand mechanical forces by the stuffing material. In another embodiment, the protective material is provided as a barrier material inserted into a structure to provide at least one of heat and / or sound insulation to the structure, and the barrier material can minimize the propagation of heat and / or sound through the structure.

[0020] The protective material can be divided into multiple protective packaging units. Each protective packaging unit can be provided as a single unit of packing material to provide packing and / or insulation, as described above. For example, in one embodiment, the protective packaging unit is packing that is inserted into a structure and provides structural stability to the structure. In this embodiment, the packing is a packing wall that provides structural stability to the structure. In another embodiment, the protective packaging unit is a packaging container having a protective packaging wall that defines a container cavity provided therein for receiving an object (such as a product for shipment). The packaging container may be a bag, mailer, box, or other packaging container provided for storing an object during transport, etc. In another embodiment, the packaging container is a food container having an insulating wall that defines a food container cavity provided for receiving food, so that hot food or beverages can be placed in the food container cavity without excessively raising the temperature of the outer surface of the food container, thereby minimizing the risk of burns from a hot container.

[0021] The protective material can be supplied as a web. A web is a material with a large surface area and a thin thickness relative to its surface area, and has an overall flat structure.

[0022] For example, the packaging unit 110 shown in the embodiment in Figure 1 is a web of a packaging container. The packaging unit 110 is made of protective packaging walls 118, 120. The walls 118, 120 are two parts of a broad wall of an overlapping web, such that the longitudinal side 124 and transverse side 128 of each wall 118, 120 are sealed together to define a container cavity 198 inside. The side 124, 128 are sealed together with a sealant applied to at least one of the inner surfaces of the walls 118, 120 corresponding to those side 124, 128, as will be further described below. The walls 118, 120, the side 124, 128, the end 126, and the end 130 define a container cavity 198 between them. In particular, walls 118 and 120 define the upper and lower boundaries of the container cavity 198, while sides 124 and 128, end 126, and end 130 define the outer perimeter of the container cavity 198. The container cavity 198 is connected to the opening 197 so that the container cavity 198 can receive objects inserted through the opening 197.

[0023] Wall 118 is cut along its end 130 such that an opening 197 is defined between walls 118, 120, the end 130 of wall 118, and the longitudinal sides 124, 126. The opening 197 is connected to a container cavity 198 and is provided so that an object can be inserted into the packaging unit 110. In this way, the object can be inserted longitudinally into the packaging unit 110 in a top-loading structure. A top-loading structure is a structure in which an object can be inserted into an opening facing an adjacent packaging unit. In another embodiment, the opening is a side-loading structure in which the opening faces away from an adjacent packaging unit and is cut along a portion of the packaging unit adjacent to and parallel to the lateral side so that an object can be inserted laterally into the packaging unit. In yet another embodiment, the opening is cut along a wall at a distance from the end or lateral side of the packaging unit. In this embodiment, another wall extends a distance beyond the opening, allowing the opening to later close over the cut-out wall and function as a flap to accommodate the object (e.g., flap 630 as shown in Figure 13). Furthermore, in other embodiments, the opening is a perforation line, scoring line, or other suitable structure.

[0024] The packaging unit 110 is secured to adjacent packaging units 110 along a weak area 116. The weak area 116 is a perforation or slit line, a scoring line, or another suitable structure that allows each packaging unit 110 to be separated from adjacent packaging units 110 along the web 100.

[0025] The packaging unit 110 is cut along the end 130 from the lateral sides 124, 126, forming lateral slits 122 along each side of the weak region 116. Such lateral slits 122 facilitate the opening of the opening 197 and make it easier to separate the packaging units 110 from each other. In other embodiments, the packaging unit does not have lateral slits, and instead has a weak region along the entire end of the packaging unit.

[0026] The web can be processed to form a supply structure so that the web can be easily pulled out from the supply later. For example, in one embodiment, the supply structure is in the form of a roll configuration, where the web is wound into a roll and can be pulled out from the roll later. In another embodiment, the supply structure is in the form of a fanfold structure, such as the supply structure 150 shown in Figure 1, where the web is folded in an accordion style to form a stack of webs that can be pulled out from the stack later.

[0027] The protective material may include a wall that defines an expansion space for housing an expandable composite. In one embodiment, the expandable composite is provided to be expandable so that it can be activated to expand under specific conditions (e.g., heat or pressure). In this embodiment, the protective material is an expandable protective material having an expandable form that can expand after the expandable composite has been activated. In another embodiment, the expandable composite is expanded so that the expandable composite has already been activated from the expandable composite and expands within the wall. In this embodiment, the protective material is an expanded protective material having an expanded form after the expandable composite has already been activated. In this embodiment, the expanded wall is used as part of a packaging container or as part of a filling wall for a filling. In yet another embodiment, the protective material does not have an expandable composite such that the protective material is not expandable.

[0028] For example, the protective material 10 in the embodiment shown in Figure 1 is an expandable protective material having an expandable composite material that has not yet expanded. In this embodiment, the walls 118, 120 may include expandable composite materials that can be later expanded so that the walls 118, 120 form expanded walls. If the packaging unit 110 is a container, such expanded walls can function as the padded walls of the container and help protect the objects contained within the container from impact. In other embodiments, only one of the walls 118, 120 is expandable, and when the expandable composite is later expanded, only one of the walls 118, 120 may expand. Expandable composites are described in more detail below.

[0029] In one embodiment, the supply structure may be in a high-density configuration, where the expandable composite within the walls of the protective material web is expandable but not provided in an expanded form, thus allowing the web in the supply structure to be in a high-density configuration. In this embodiment, the expandable web of the protective material is a web of expandable, connected, and separable protective material units. In this embodiment, the user can expand the web of the supply structure later if it is received in a high-density configuration. In another embodiment, the supply structure is in a low-density configuration, where the expandable composite within the walls of the protected object web is expanded, resulting in a low-density configuration of the web in the supply structure. In this embodiment, the expanded web of the protective material is a web of expandable, connected, and separable protective material units. In this embodiment, the user can receive the web of the supply structure in a low-density configuration without having to expand it later.

[0030] For example, the supply structure 150 shown in the embodiment of Figure 1 is a high-density fanfold configuration in which the protective material is expandable but has not yet expanded. The packaging units 110 are folded along the weak region 116 so that the packaging units 110 can be stacked on top of each other in the expandable supply structure 150.

[0031] Referring to the embodiments shown in Figures 2 and 3, the system 200 is configured to process stock material into a protective material web, which in this embodiment is provided as a supply structure 150 of a series of interconnected, separable protective material units 110. The system 200 draws material from a material supply section, which in this embodiment is material rolls 102, 104 of each material 106, 108 provided as a web. Each material 106, 108 is drawn from its supply as a web downstream 210. In other embodiments, other supply structures may be used, and separate webs may be combined into fewer webs and folded over to provide the layers described below. In other embodiments, additional webs may be used instead to provide the layers described below.

[0032] In this embodiment, the substrate is made of paper. These paper substrates are permeable to air or water, allowing vapors released from the expandable composite material as the expandable composite material expands to vent through the paper substrate. In other embodiments, the substrate has vents defined along at least one surface of the substrate to allow vapors from the expandable composite material to vent. The paper substrate may be corrugated cardboard, kraft paper, fiberboard, pulp paper, recyclable material (e.g., recyclable paper or plastic), paper, or newspaper. In other embodiments, the paper substrate includes a coating along the substrate so that the paper substrate is impermeable to air or water, but the paper substrate is heat-sealable. For example, the coating may be wax, plastic, water-resistant material, and / or stain-resistant material. In such embodiments, the paper substrate may have a thickness between 20 and 90 microns, preferably between about 30 microns. Furthermore, the paper substrate may be 20 to 90 lbs / ream (or 20 to 90 lbs / 500 substrates). In other embodiments, the substrate can be made of polymers (e.g., polyolefins, polyethylene, polypropylene, polyester, or other suitable polymers), foils, poly or synthetic materials, and / or other suitable materials of appropriate thickness, weight, and dimensions. The substrate can also be made of biodegradable materials (e.g., paper, natural starch, synthetic starch, cellulose, biopolyester, protein, polysaccharide, or other suitable biodegradable materials). As used herein, the term “biodegradable” means that a substance is broken down by exposure to light, air, water, or any combination thereof, or by the action of naturally occurring microorganisms such as bacteria, fungi, and algae. In some embodiments, the paper substrate is made primarily of biodegradable materials. For example, in such embodiments, the paper substrate is made of at least 75% by weight, 85% by weight, or 95% by weight, or substantially entirely of biodegradable materials. In some embodiments, the stock material used to convert the substrate into a packaging unit is made primarily of biodegradable materials. In yet another embodiment, the protective material as a whole is made primarily of biodegradable materials.For example, in such embodiments, the protective material is made of at least 75% by weight, 85% by weight, or 95% by weight, or substantially entirely, biodegradable material. Preferably, the protective material is recyclable. For example, in such embodiments, at least 80% by weight, 85% by weight, 90% by weight, 95% by weight, or substantially entirely, of the protective material is recyclable.

[0033] System 200 processes the webs of substrates 106, 108 to provide the webs of substrates 106, 108 as layer 140. The expandable composite applicator 212 applies the expandable composite 220 to the substrates 140 as the substrates 140 are pulled downstream. The expandable composite 220 may be configured to expand by the application of specific expansion conditions, such as heat, pressure, or chemical reaction, or other suitable means.

[0034] The expandable composite material 220 is generally applied in a pattern that can include regular shapes (e.g., circles, ellipses, squares, rectangles, triangles, polygons, lines, etc.), irregular shapes (e.g., random or probabilistic shapes), or other desired shapes when providing the expandable composite material along a substrate. For example, the expandable composite material 220 can be applied in a pattern that allows the expandable composite material to form a continuous layer when pressure is applied in a later process. In one embodiment, the expandable composite material is applied to cover most or all of the expansion area along the layer, and later to define expansion spaces between substrates (e.g., expansion spaces 117, as shown in Figure 6). For example, the expandable composite material is applied across the entire surface of the layer. In another embodiment, the expandable composite material 220 is applied to the layer as a continuous layer along most or all of the layer. In yet another embodiment, the expandable composite material 220 is applied on part of the layer such that the expandable composite material is applied along the layer at a distance from the edges of the layer. In some preferred embodiments, the expandable composite 220 is applied such that certain areas of the expansion region along the layer contain less of the expandable composite 220, or do not contain any at all, to facilitate easier folding along the natural hinge region in a later step of the process. For example, linear portions of the layer may contain less of the expandable composite 220 than other portions of the layer, or the expandable composite 220 may not be present along that portion, thus forming a natural region (e.g., area 492, as shown in Figure 7) that can be more easily folded in a later step when the expandable composite 220 expands. Alternatively or additionally, after bonding the expandable composite 220, before or after the expansion of the expandable composite 220, pressure is applied along certain linear regions to form hinges along those regions. In yet another option, the expandable composite 220 is applied with a uniform or varying thickness or width.

[0035] The expandable composite material 220 may include a matrix. The matrix may be a fluid matrix such as a gel or liquid and can be applied immediately on the first layer 140. Alternatively or additionally, the matrix may be a solid matrix that can pass through the gel or fluid phase. The matrix may be a mixed matrix containing both a gel or liquid and a solid such that solid particles are incorporated into the gel or fluid.

[0036] The matrix can be made of polymers including emulsion polymers. The polymer can be thermoplastic. The polymer can be at least one of vinyl acetate ethylene, polyvinyl acetate, polyvinyl alcohol, vinyl acetate copolymer, polyvinyl alcohol copolymer, dextrin-stabilized polyvinyl acetate, vinyl acetate copolymer, ethylene copolymer, vinyl acrylic, styrene acrylic, acrylic, styrene butyl rubber, polyurethane, polyolefin, biodegradable materials (e.g., cellulose and starch), and / or other suitable expandable composites.

[0037] In some embodiments, the matrix comprises polyurethane, and the matrix contains 50%, 75%, 90%, or 95% or more polyurethane based on the total weight of the matrix.

[0038] The matrix may or may include a polyolefin dispersion. Preferably, the matrix contains 50%, 75%, 90%, or 95% or more polyolefin based on the total weight of the matrix. The polyolefin dispersion may be polyethylene and / or polypropylene, an ethylene-based thermoplastic polymer, a propylene-based thermoplastic polymer, a polyethylene film or foam, a polymer-based stabilizer containing at least one polar polymer, water, and / or other suitable polyolefin dispersions. The ethylene-based thermoplastic polymer may include high-density polyethylene (HDPE), linear low-density polyethylene (LLDPE), low-density polyethylene (LDPE), or a combination thereof. As used herein, the term "ethylene-based polymer" refers to a polymer consisting mostly of polymerized ethylene monomers (based on the total weight of the polymer) and optionally containing at least one polymerized comonomer. In some embodiments, the ethylene-based polymer contains 50%, 75%, 90%, or 95% or more ethylene portion based on the total weight of the polymer. The propylene-based thermoplastic polymer is optionally oriented polypropylene (OPP). As used herein, the term “propylene-based polymer” refers to a polymer in polymer form that comprises a majority of propylene monomers (based on the total weight of the polymer) and may optionally contain at least one polymeric comonomer. In some embodiments, the propylene-based polymer contains 50%, 75%, 90%, or 95% or more of the propylene portion, based on the total weight of the polymer. Preferred polyolefin dispersions may be, for example, HYPOD™ from Dow Chemical or other suitable polyolefin dispersions.

[0039] The matrix may include a polyolefin-based adhesive. An adhesive is a material that can adhere to opposing surfaces without relying on the opposing surfaces being made of the same or complementary material to form a seal between them. The adhesive may be a liquid adhesive, which typically requires water to form a seal between surfaces. Alternatively, the adhesive may be a dry adhesive, which typically does not require water, solvents, or thermal activation to form a seal between surfaces. Furthermore, the adhesive may be a pressure-sensitive adhesive, which can seal surfaces together after a small, initial external pressure is applied. Examples of such adhesives include water-based, acrylic, pressure-sensitive adhesives, similar to those used in packaging tapes, which often hold two surfaces together through surface contact alone with only a small initial external pressure. For example, dry adhesives that do not require water, solvents, or thermal activation and adhere strongly to many dissimilar surfaces can be cited. Pressure-sensitive adhesives can be selected to be strong and / or semi-permanently tacky at room temperature. The application and use of pressure-sensitive adhesives can be automated. When used in assembly, pressure-sensitive adhesives, which do not require setup or long curing times, can save time compared to using general liquid adhesives. With pressure-sensitive adhesives, bonding is preferably immediate, allowing manufacturing to continue without interruption, resulting in significant time and labor savings. Examples of water-based, acrylic, and pressure-sensitive adhesives include RHOPLEX N-1031 Emulsion, RHOPLEX N-580 Emulsion, RHOPLEX N-619 Emulsion, or other suitable types of pressure-sensitive adhesives. Other emulsion polymer or acrylic polymer blend adhesives are also known, and other suitable types of adhesives and / or contact adhesives can be used.

[0040] Alternatively, the matrix may be an aqueous adhesive. The aqueous adhesive may contain an aqueous polymer. Another option is that the matrix may be based on starch in a natural or synthetic form. The starch may be in the form of ground fine starch powder. The diameter of the ground starch particles may be between about 12 microns and about 20 microns. The starch-based matrix may contain at least one of water or other solvents, surfactants, polar binders, or other fillers. For example, the starch-based matrix may contain up to 50% water. In some embodiments, the matrix contains 25% to 80% or 30% to 40% starch. Such a starch-based matrix may be biodegradable. In other preferred embodiments, the biodegradable matrix contains a starch-based adhesive.

[0041] In yet another embodiment, the expandable composite can be made of multiple materials separated by barriers that, when mixed or in contact with each other, cause the expandable composite to expand into an expanded configuration. For example, the barrier may be a microsphere shell, as disclosed in U.S. Provisional Application No. 62 / 706,110. Such microspheres may be expandable and / or burstable, for example, by applying sufficient heat. Microspheres may have an outer shell and an inner core. A suitable outer shell can be made of, for example, a thermoplastic polymer, not limited to polyacrylonitrile or PVC, as well as glass, rubber, starch, cellulose, ceramic, or other suitable material. In another preferred embodiment, multiple thermally expandable microspheres include a solid, liquid, or gaseous core made from a hydrocarbon, water, or other suitable chemical that can be activated to expand or burst the microsphere shell. In another preferred embodiment, microspheres may be made of a biodegradable material, such as cellulose. Cellulose-based microspheres have a shell that can be made of cellulose. As used herein, the term "cellulose-based microspheres" refers to microspheres containing a majority amount of cellulose based on the total weight of the microspheres. In some embodiments, cellulosic microspheres contain more than 50%, 75%, 90%, or 95% of cellulose based on the total weight of the microspheres. In some embodiments, the expandable composite itself is a cellulosic expandable composite. As used herein, the term "cellulose-based expandable composite" refers to an expandable composite containing a majority amount of cellulose based on the total weight of the expandable composite. Cellulose-based expandable composites preferably contain more than 50%, 75%, 90%, or 95% of cellulose based on the total weight of the expandable composite.

[0042] Microspheres can be mixed with the matrix before being applied to the web, or they can be provided onto the matrix after the matrix has been applied to the web, for example, when the layers are pressed together, by mixing or forcibly supplying the microspheres to the matrix after application to the web.

[0043] Microspheres have an expansion temperature (Texp) at which they begin to expand and a maximum temperature (Tmax) at which they will burst if heated above that temperature. The Texp of a microsphere is not particularly limited, but is generally between about 60°C and about 250°C. The Tmax of a microsphere is generally between about 80°C and about 300°C. In other preferred embodiments, Tmax is higher than 300°C. Microspheres are selected based on their maximum expansion temperature, depending on whether or not it is required that the microspheres burst. Tmax depends on several properties, including the physical properties of the microspheres, the physical properties of the matrix, and the physical properties of the layers on which the matrix and microspheres are deposited. Heat can be generated by appropriate means, such as high-frequency radiation, as will be further discussed with respect to expansion devices. In other preferred embodiments, high-frequency radiation is applied to the expandable composite 220 at a frequency of about 10–45 MHz, or at a frequency suitable for the composition of the microspheres and the material of the matrix. In other embodiments, other frequencies may be used. The selected heating parameters depend on the expandable composite or material 220 used. In such techniques, the expandable composite is dispensed into a container such as a bag, where it is activated and expanded to fill the void in the bag. When a product is present in the container, the expandable composite expands upon activation and forms itself around the product.

[0044] System 200 may include an expansion device for expanding the expandable composite 220. In embodiments where the expandable composite comprises an emulsion polyolefin dispersion, microspheres cause the emulsion polyolefin dispersion to expand upon activation of the expandable microspheres. In some embodiments, the microspheres are encapsulated within the emulsion polyolefin dispersion. The expansion device may include a heating element, a heating coil, a hot air applicator, a high-frequency radiation generator, a ultraviolet applicator, a chemical reaction applicator, a pressure mechanism, or other suitable device for expanding the expandable composite 220. The expandable composite may include a blowing agent. In such embodiments, the expandable microspheres containing the blowing agent, once activated, expand on their own, causing the emulsion polyolefin dispersion to expand. In other embodiments, the expandable composite may include a reactive component, a chemical catalyst, and a heating agent (which can heat the expandable composite and / or cause a temperature rise in the expandable composite) and / or other suitable expansion device. In this embodiment, the expansion device can activate the expandable composite material 220 through at least one of a thermal process, a mechanical process, a chemical process, or other suitable means of activation for expanding the expandable composite material 220. For example, the expansion device can provide at least one of heat, pressure, or a chemical reaction.

[0045] Examples of blowing agents include air, carbon dioxide, nitrogen, argon, helium, methane, ethane, propane, isobutane, n-butane, neopentane, and the like. In some embodiments, the blowing agent may be an inert gas or generally any suitable material. In some embodiments, the gas or mixture of gases is added to the expandable composite by mechanical means. An example of a mechanical means is to whip or foam the expandable composite to impart air or other gases to the expandable composite and increase its volume. In other embodiments, the gas or mixture of gases may also be encapsulated in microspheres. When the microspheres are activated, they expand. The expansion of the microspheres causes the expansion of the expandable composite.

[0046] The chemical reaction can involve mixing two reactive components that react to produce foam. In some embodiments, a catalyst is used to increase the rate of the chemical reaction. In some embodiments, the two reactive components are separated by a barrier before mixing and expansion. The barrier separating the reactive components can be a microsphere shell, where the microsphere core consists of one or more types of reactive components, and the rupture of the microsphere releases its contents into one or more types of other reactive components, triggering the foam-forming reaction. Other barriers, such as walls, capsules, or other barrier-forming containers, can also be used. An example of a reactive component that causes expansion is mixing a liquid isocyanate with a multi-component liquid blend called a polyurethane resin. When these components are combined, carbon dioxide and water vapor are released, producing polyurethane foam. Other reactive components that foam when mixed can also be used.

[0047] The sealant applicator 214 applies the sealant 216 to the exposed surfaces of layer 140 and / or layer 160. The sealant applicator 214 can apply the sealant 216 using tape such as double-sided tape, or other suitable methods for applying the sealant. In some embodiments, the sealant includes polyethylene.

[0048] The sealant 216 is configured to provide a sufficiently strong seal so that when layers 140 and 160 are joined together, the sealed portions of layers 140 and 160 can withstand the expansion of the expandable composite 220 without the expanded material escaping along those sealed portions. The sealant 216 can be configured as a strip seal, coating, or other suitable configuration for sealing layers 140 and 160 together. The sealant 216 can be applied as a continuous layer or as a pattern of discontinuous strip seals.

[0049] The sealant can be selected to be activated under specific conditions to form a seal, such as when heat or pressure is applied. The sealant can be made of cold glue. The sealant can be made of an adhesive element that provides a sealing surface. The adhesive element can be an adhesive as described above that provides an adhesive surface. Alternatively, the adhesive element can be a flocculant that provides an aggregate surface. The flocculant can seal the first surface to the opposing surface by one flocculant on the first surface coming into contact with the same or complementary flocculants along the opposing surface. Generally, flocculants do not adhere well to other materials, or in other appropriate cases, adhere very weakly compared to the bonds that are formed when they adhere to each other, however certain flocculants (e.g., latex flocculants) can be mixed with water to adhere to non-aggregated surfaces, and the flocculant can remain attached to the non-aggregated surface when dry.

[0050] Referring to Figure 4, layer 140 includes a sealant 216 applied along a longitudinal region 144 along a longitudinal end 142, and a transverse region 146. In other embodiments, the sealant 216 can be applied along a longitudinal region 144 adjacent to the longitudinal end 142 but at a distance from the longitudinal end. In the embodiment shown in Figure 4, the sealant 216 is applied between the longitudinal regions 144 along transverse regions 146 that are longitudinally spaced apart from each other. In other embodiments, the sealant 216 is applied along layer 140 parallel to the longitudinal regions 144. In further embodiments, the sealant 216 is applied only along the longitudinal regions 144. In this embodiment, layer 160 does not contain any sealant. Layer 160 defines regions that correspond to portions of layer 140 containing the sealant 216, such that when layers 140 and 160 are later joined together, regions 144 and 146 of layer 140 containing the sealant 216 join with corresponding regions of layer 160 that do not contain the sealant. In particular, layer 160 defines transverse regions 164 and 162 configured to correspond to longitudinal regions 144 and 142, and transverse region 166 configured to correspond to transverse region 146 when layers 140 and 160 are joined together. In a preferred embodiment, layers 140 and 160 are made of biodegradable material, and the protective material as a whole is biodegradable. The biodegradable protective material includes, for example, a biodegradable composite material comprising a biodegradable layer, a biodegradable matrix, and a plurality of cellulose-based expandable microspheres. The biodegradable layer may include a plastic substrate such as a polyolefin, for example, a polyethylene film, or a foam.

[0051] In other embodiments, the second layer 160 also includes a sealant along regions 164, 166 to provide a stronger seal between layers 140, 160. In this embodiment, a longitudinal sealant is applied along the longitudinal region 164, and a transverse sealant is applied along the transverse region 166, so that when layers 140, 160 are joined together, the sealants along regions 164, 166 correspond to the sealants along regions 144, 146. For example, one or more longitudinal seals and one or more transverse seals may include pressure-activated adhesives, low-temperature adhesives (e.g., collagen-based adhesives, polyvinyl acetate-based adhesives, or other suitable adhesives), and / or other suitable sealants.

[0052] The expandable composite material 220 is applied along an expansion region 148 on layer 140. The expansion region 148 is bounded by a longitudinal region 144 and a transverse region 146 to define its periphery. Layer 160 defines an expansion region 168, which is configured to correspond to the expansion region 148 when layers 140 and 160 are joined together. The expansion region 168 is bounded by a longitudinal region 164 and a transverse region 166 to define its periphery. When layers 140 and 160 are later joined together, the expansion regions 148 and 168 can define an expansion space (e.g., an expansion space 117 shown in Figure 6) between them for accommodating the expandable composite material 220.

[0053] In other embodiments, the layer includes a sealant along one side of the region such that the expansion region is constrained only along one of the longitudinal or transverse perimeters for the expansion of the expandable composite 220 within it. In another embodiment, there is no sealant along the layer such that the expandable composite 220 is not constrained by the sealant. In another embodiment, the expandable composite is applied to only a portion of the expansion region.

[0054] In other embodiments, the layers may be configured to join to each other without a sealant, so no sealant applicator is present. For example, in one embodiment, an expandable composite 220 is used as an adhesive that can bond the layers together. In this embodiment, the expandable composite 220 is applied along the layers so that pressure can be applied to the layers to spread the expandable composite 220 evenly between the layers. For example, the expandable composite 220 is pressed between the layers so that it spreads adjacent to the edges of the layers. In another embodiment, the layers include a coating along the layers that can heat-seal the layers together. In yet another embodiment, the roll includes an adhesive that is activated when heated.

[0055] Referring again to Figures 3-4, the system 200 includes a pressure applicator 222, illustrated here as a roller, but other suitable mechanisms can be used. After the expandable composite material 220 and sealant 216 are applied, the pressure applicator 222 applies pressure to the layers 140, 160 in areas of the layers 140, 160 where the sealant 216 is applied between them (e.g., along areas 144, 146, 164, 166), joining the layers 140, 160 together so that the webs of the layers 140, 160 accumulate to form a protective packaging wall 170. The joined layers 140, 160 define an expansion space between them for accommodating the expandable composite material 220 (e.g., expansion space 117, as shown in Figure 6). In some embodiments, the expandable composite material 220 can be expanded to form a continuous layer by pressing the layers together.

[0056] The system 200 includes seal applicators 224, 226, each applying a different sealant. For example, seal applicator 224 can apply sealants 274, 276, and seal applicator 224 can apply a different sealant 278 to the outer surface of wall 170. In other embodiments, seal applicators apply any combination of sealants. In further embodiments, each seal applicator applies the same sealant. In yet another embodiment, there may be only one seal applicator. Seal applicators 224, 226 are similar to seal applicator 214, and sealants 274, 276, 278 may be similar to those described for sealant 216, or other suitable sealants may be used.

[0057] Figure 5 shows an embodiment of the wall 170 after sealant applicators 224, 226 have applied sealant 274, 276, and 278 to the outer surface of the wall 170. Sealant 274 can be applied along a longitudinal region 180. In this embodiment, sealant 274 is applied along a longitudinal region 180 adjacent to a longitudinal end 172, whereas in other embodiments, sealant 274 is applied along a longitudinal region at a distance from the longitudinal end. Sealants 276 and 278 are applied along transverse regions 182 and 184 between the longitudinal regions 180, respectively, with longitudinal spacing between them. However, in other embodiments, either sealant 276 or 278 is applied parallel to the sealant. In further embodiments, sealant is applied only along the longitudinal regions of the wall. Sealants 276 and 278 are separated by a gap 186 having a distance 188. The gap 186 may be configured to provide a space into which an opening or a weak area can be cut.

[0058] If the sealants 274, 276, and 278 are sealants of different conditions (e.g., temperature or pressure), then a particular sealant is selected to be activated under one condition different from the other sealants that are selected to be activated under other conditions. For example, in one embodiment, sealants 274 and 276 may be selected to be activated at a temperature or pressure different from the temperature or pressure required to activate seal 278 to form a seal. In this way, sealants 274 and 276 can form seals along regions 180 and 182 without sealant 278 forming a seal along region 184. However, in other embodiments, the sealants are selected to have similar conditions for creating a seal. In other embodiments, the sealants may be selected to have other combinations of the conditions of each sealant.

[0059] The sealants 274, 276, and 278 can be applied along the folded wall 190 with the same or different widths or lengths to control the size and shape of the container cavity formed from the folded web 170 in a later step. For example, longitudinal sealants may be applied so as to have a thicker width adjacent to transverse sealants, while smoothly transitioning to a thinner width between them. In such a configuration, the expansion space may be defined as having a curved side adjacent to the longitudinal sealant.

[0060] As shown in Figures 2-3, the system 200 includes a folding device 228 for folding the wall 170 over itself after sealing materials 174, 276, and 278 have been applied to the outer surface of the wall 170, thereby forming a folding wall 190 that includes an overlapping protective wall surrounding a container cavity (e.g., a container cavity 398 as shown in Figure 6). In this embodiment, the folding device 228 folds the wall 170 with respect to a folding mechanism 234, and a tension mechanism 230 applies tension to the wall 170 during the folding process. For example, in one embodiment, the folding mechanism 234 is a folding rod and the tension mechanism 230 is a wheel. In this embodiment, the wheel pulls tension on the wall 170 around the folding rod to fold the wall 170 so that the longitudinal regions 174 correspond to each other. The folding mechanism 234 may have a shape suitable for folding the wall 170, such as a V-shape. The folding device 228 further includes a flattening mechanism 190 configured to flatten the folding wall 190. The flattening mechanism 190 may be a flattening rod configured to apply pressure to the folding wall 190 and flatten it. Other suitable folding mechanisms known in the art can be used.

[0061] Next, the sealing device seals the wall 170 so that the sealing materials 174, 276 form a seal along regions 180, 182. The sealing device is configured to apply conditions that activate the sealing materials 174, 276 (e.g., heat, pressure, and / or other suitable means to activate the sealing materials 174, 276). In another preferred embodiment, the planarization mechanism 190 functions as a sealing device. In another embodiment, the system 200 incorporates separate sealing devices along different parts of the process.

[0062] Referring to Figure 5, wall 170 defines a region 192 into which wall 170 is folded by the folding device 228. Wall 170 includes wall portions 118, 120 such that when wall 170 is folded, wall portion 118 aligns with wall portion 120. In particular, the sealing regions 180, 182, 184 of wall portion 118 align with the sealing regions 180, 182, 184 of wall portion 120. Referring to the embodiment shown in Figure 6, the folding wall 190 is typically substantially flat, but for illustrative purposes, the folding wall 190 is shown to have a substantially open container cavity 398. As will be further described below, this joint of sealing regions 180, 182, 184 allows sealing materials 174, 276 to be sealed together in a later stage to form the boundary of the protective packaging unit while the sealing region 184 of wall portions 118, 120 is unsealed at this point in the process. Such unsealed areas can be used later as openings for a packaging unit (e.g., packaging unit 110) to receive objects after the sealant 278 has formed a seal along the seal area 184, but before the seal area 184 by the sealant 278 functions as a closure to close the packaging unit. For example, the seal area 184 may be part of a flap without another layer on top of the sealant 278. In this example, the sealant 278 is a water-activated adhesive so that a user can lick the flap to activate the adhesive. In yet another embodiment, the seal area 184 is left without sealant so that a user can later apply adhesive along the seal area 184. In the embodiment shown in Figure 6, the longitudinal ends 172 of each wall 118, 120 are shown to meet, but in other embodiments, the longitudinal ends of each wall do not meet, and one end of one wall extends over the end of the other wall.

[0063] Referring to Figure 6, the folding wall 190 defines a container cavity 398 between the wall sections 118, 120, which can house one or more objects after the wall 170 is folded along area 192. The container cavity 398 is further enclosed on one side by a seal formed from area 180 of the wall sections 118, 120 and on the other side by a folded layer 160 with respect to area 192. As will be further described below, the container cavity 398 will be further bounded by other sealed areas as the protective packaging unit 110 is defined along the web 100. The expandable composite material 220 can be expanded in a later stage to expand the folded wall 170 (either as individual packaging units 110 or before forming such packaging units 110) so that the wall sections 118, 120 expand to protect the objects housed in the cavity 398 from impact (e.g., during shipment of the objects).

[0064] In other embodiments, the system may not include a folding device, and unfolded walls may be supplied to a later stage of the process without being folded. For example, in such embodiments, another wall is superimposed on the first wall so that the sealing areas of each wall coincide with each other and define a container cavity between them. An example of such a configuration can be seen in Figure 11, in which the web 300 of the protective material 30 consists of two superimposed walls 318, 320 defining a container cavity 398.

[0065] Figure 4 shows a wall 170 having one region 192 into which it can be folded, but other embodiments of the wall may include multiple folding regions. For example, the embodiment in Figure 7 has a wall 470 having linear regions 55 in which the amount of expandable composite 220 is reduced or absent. By reducing or absenting the expandable composite, these regions have a smaller thickness and less internal structure than the filling portions 494, 496, thereby resulting in a natural hinge line 499 that facilitates folding adjacent portions 494, 496 of the wall 470 over each other. Referring in particular to Figures 8-9, the filling portions 494 are folded over the filling portions 496 along line 498 such that the sealing regions 480 of each filling portion 494 (on which sealant 474 is applied) meet over the filling portions 496 to form a folded wall 490. In this embodiment, the sealing regions 480 of each filling portion 494, 496 are joined together and then folded flat on the filling portion 494, so that the sealing regions 480 join to form a folded spine along the length of the web 490 on the central portion of the filling portion 496. However, in other embodiments, the sealing region of one filling portion is on the outer surface of the filling portion (for example, along the edge of that filling portion), and the joining of the sealing region on the inner surface of one filling portion with the outer surface of another filling portion allows the filling portions to be joined together to form a container cavity without forming a central folded spine along the length of the web. The sealant 174 can then form a seal that joins or otherwise fixes the sealing regions 480 so that the filling portions 494, 496 form a container cavity 498 between them. The container cavity 498 is further defined between lines 499 and may be further defined in a later stage by sealing areas 482, 484 being joined to each other or otherwise fixed by sealing materials 276, 278 forming a seal.

[0066] The system 200 is also configured to form a weak region 116 along the folding wall 190 and an opening (such as an opening 117, as shown in Figure 1) for accessing the folding wall 190 of the container cavity 398. In this embodiment, the weak region 116 extends along the folding wall 190 laterally with respect to the direction of the longitudinal end 172, defining the length of individual protective packaging units and facilitating the separation of packaging units 110 from each other, such as by breaking one unit 110 from the next unit.

[0067] The weak areas 116 and openings can be provided as perforation or slit lines, scoring lines, or other suitable structures, and the system 200 may include a cutting device 240 for perforating, scoring, and / or cutting, or other suitable devices for creating the weak areas. The weak areas and openings can be applied before, during, or after other parts of the process described. The cutting device 240 can also be used to remove a longitudinal length of one of the layers to create a flap extending from one wall of the package unit (e.g., a flap 630 as shown in Figure 13).

[0068] Referring to Figures 2, 3, 9, and 10, the cutting device 240 of system 200 includes a blade holder 250 for holding a blade 244 and an anvil, such as a roller 242, which is made of an elastomer or other backing material and can be grooved to receive the blade, or can be penetrated by the blade, or pressed against by the blade to form a desired cut and / or score. Other cutting devices may include a fixed blade or a rotating blade, a heat cutter, and / or known mechanisms for cutting the folding wall 190. In the illustrated embodiment, the blade 244 includes a series of spaced teeth 246 configured to completely penetrate and create holes in all of the wall portions 118, 120 of the folding wall 190. The blade 244 completely cuts through the wall portion 120 to form an opening 197 along the wall portion 118 that crosses the longitudinal end of the folding wall 190. However, because the teeth 246 of the blade 244 include gaps 248 between each tooth, the blade 244 does not completely cut through the wall 120. The teeth 246 and gaps 248 form a perforation line as a weak region 116 along the wall 120 that crosses the longitudinal end of the folded wall 190. In this way, the folded web 190 is cut to form the cut web 100 of the connected, separable packaging unit 110.

[0069] In the embodiment shown in Figure 10, the cutting device 240 is shown cutting the opening 117 and weak area 116 through the gap 186, but in other embodiments, the cutting device cuts the opening and weak area through different parts of the folded web, along a portion of the folded web having the sealant (e.g., along the folded web 190 having the sealant 278), so that the sealant is not yet activated and can form the top surface of the packaging unit. In other embodiments, the blade can cut the entire folded wall, separating the folded wall into the packaging unit. In yet another embodiment, the teeth of the blade can be configured to cut a perforation line through the entire folded wall to form weak areas along both parts of the wall. In yet another embodiment, the cutting device may include one blade for forming the opening along a portion of the folded wall and another blade for forming the weak area along the other part of the folded wall at different times or places in the process.

[0070] The system 200 includes an aggregating device 252 configured to aggregate the cut web 100 into a supply structure 150, such as a fanfold structure in this embodiment (or fanfold structure 150 in Figure 1). In embodiments where the system separates each unit from the next, the aggregating device can organize and stack the separated protective packaging units and optionally place them in a container such as a box or wrapper. In other embodiments, the expandable composite material 220 in the cut web 100 can be expanded before being aggregated into the supply structure so that the supply structure contains the expanded protective packaging units. In other embodiments, the aggregating device 252 includes an expansion device.

[0071] Figure 11 shows an example of a supply structure as a fanfold structure 350. In this example, the fanfold structure 350 includes a web 300 of expandable, connected, separable packaging units 310 in a high-density configuration. The packaging unit 310 consists of protective packaging walls 318, 120 overlapping each other along the longitudinal sides 324, 326 and transverse sides 328 of the packaging unit 310. The sides 324, 326, 328 are parts of the packaging unit 310 that are sealed together by a sealant applied to at least one of the inner surfaces of the walls 318, 320 corresponding to those sides 324, 326, 328, as will be further described below. The wall 318 is cut along the end 330 such that an opening 397 is defined between the walls 318, 320, the end 330 of the wall 318, and the longitudinal sides 324, 326. The opening 397 is provided to allow an object to be inserted into the packaging unit 310 in a top-loading configuration. The packaging unit 310 is fixed to adjacent packaging units 310 along the weak region 316. The packaging unit 310 is cut along the end 330 from the lateral sides 324, 326 to form lateral slits 322 along each side of the weak region 1316. Such lateral slits 322 allow the opening 397 to be easily opened, making it easy to separate the packaging units 310 from each other. In other embodiments, the web does not have lateral slits, and instead has a weak region along the entire end for each packaging unit.

[0072] Figure 12 shows an example of a supply structure as a roll structure 550. In this example, the roll structure 550 constitutes a roll of web 100 in a high-density configuration. The roll structure 550 can be a cored roll structure or a coreless roll structure. However, other embodiments include the web being rolled in an expanded, low-density configuration. The roll structure 550 can be a cored roll structure or a coreless roll structure.

[0073] Figure 13 shows an exemplary protective packaging unit 610 in the form of a mail-like packaging container configured to support an object for shipment. In contrast to packaging unit 110, the walls of packaging unit 610 are not folded over to define a container cavity. Instead, protective packaging unit 610 is formed from walls 618, 620 sealed to each other along the inner surfaces of regions 624, 626, 628 to define a container cavity 698 for storing the object. For example, regions 624, 626, 628 of walls 618, 620 are sealed to each other such that the ends of walls 618, 620 coincide to define the perimeter of packaging unit 610. However, in other embodiments, the edge of one wall may extend over the edge of another wall.

[0074] The end 640 of wall 618, the opposing region 628 along wall 618, and wall 620 define an opening 697 between them so that an object can be top-loaded into the container cavity 698. Wall 620 includes a flap 630 extending beyond the end 640. In this embodiment, the flap 630 includes an adhesive surface 634 and a release layer 632 made of a material that does not strongly adhere to the adhesive surface 634. In other embodiments, the flap has an adhesive surface on the flap and the opposing short wall for closing and sealing the flap, rather than an adhesive surface. When in use, after an object is inserted into the container cavity 698 through the opening 697, the release layer 632 can be peeled off, the flap 630 can be folded over the opening 697, and then the adhesive surface 634 can be sealed to the outside of wall 620. After the flap 630 is sealed to the wall 618, the protective packaging unit 610 closes over the object received in the container cavity 698, thus preventing the object from falling out.

[0075] Referring to Figure 14, the bagging machine 700 is configured to receive webs of a series of connected packaging units, such as the web 300 in Figure 11, while the expandable composite is still in an expandable state. The bagging machine 700 is supplied with the web 300 from the fanfold stack structure 350 of the connected protective packaging unit 310. The bagging machine 700 is configured to receive the web 300, move the web 300 downstream, inflate the web 300 to form an expanded web 380, open each expanded packaging unit 381 along the opening 387 to access the container cavity 388, and insert the object into the container cavity 388.

[0076] The bagging machine 700 includes an inflation device 706 configured to inflate the expandable composite material 220 contained within the walls 318, 320 of the web 300 to form an expanded web 380. Figure 14 shows the inflation device 706 positioned immediately downstream of the fanfold stack configuration 350, but in other embodiments, the inflation device may be positioned at different locations in the process (e.g., after opening the expanded packaging unit, during the insertion of objects into the expanded packaging unit, or following the insertion of objects into the expanded packaging unit). In other embodiments, the bagging machine does not include an inflation device, and the web from the supply structure is already expanded. In yet another embodiment, the bagging machine does not include an inflation device, and the web is supplied through the bagging machine without being expanded.

[0077] To assist in opening the opening 387, the bagging machine 700 may include an opening aid. As shown in Figure 14, the opening aid includes a plurality of fingers 702 for gripping a portion of the inflatable packaging unit 381, a telescopic projection 704 configured to pull a portion of the inflatable packaging unit 381, a suction cup 712 for sucking a portion of the inflatable packaging unit 381, and a blower 714 for applying air pressure to the opening 387. The embodiment shown in Figure 10 shows a bagging machine 700 that includes all of the fingers 702, telescopic projection 704, suction cup 712, and blower 714 as an opening aid, but other embodiments may have any combination of opening aids or only one opening aid.

[0078] When the opening 387 is opened, the object can be top-loaded into the container cavity 398. The filled packaging unit can then be sealed by the sealing device 716 as described above, which operates the sealing materials 274, 276, and 278 to close the filled packaging unit around the object. The sealing device 716 can further separate the filled packaging unit from the adjacent inflated packaging unit 380 by cutting, melting, pulling, breaking, or by other suitable means of separating the packaging unit along the weak region 386.

[0079] Figures 15-16 show a bagging machine 800 of another example in which an expandable wall web 900 is supplied from a supply structure 950. The bagging machine 800 is configured to receive the web 900, move the web 900 downstream, inflate the folded web 900 to form an expandable web 980, fold the expandable web 980 to define an internal container cavity 986, and insert the object into the internal cavity 986.

[0080] The bagging machine 800 includes an inflation device 806 configured to inflate the expandable composite material 220 housed within the walls of the web 900 to form an expanded web 980. Figure 15 shows the inflation device 806 positioned immediately downstream of the supply structure 950, but in other embodiments, the inflation device 06 may be positioned at different points in the process (e.g., after folding, during insertion of the material into the container cavity, or following insertion of the material into the container cavity).

[0081] As illustrated, the inflatable web 980 includes regions 992 configured to facilitate folding of the inflatable web 980 along those portions. Regions 992 may be part of the inflatable web 980, similar to region 492 as shown in Figure 7, where there is less or no inflatable composite material 220, resulting in a natural hinge for facilitating folding of the inflatable web 980. In another embodiment, the bagging machine includes a device that applies pressure to the web during or after the web is inflated, forming regions of the inflatable web having regions of more compressed inflatable material to facilitate folding along the inflated web. In another embodiment, for example, a natural hinge is provided with a uniform amount of inflatable composite material extending laterally across the inflated space, and the device simply folds the wall web toward its center or other desired position to position the wall portions (e.g., filling portions 494, 496 as shown in Figure 7) on top of each other to define the container cavity.

[0082] The bagging machine 800 includes a folding device 806 configured to fold the inflated web 980. The folding device 806 may include bars 808, 810, or other suitable mechanisms to fold the inflated web 980 to define an internal container cavity 986 within the inflated web 980. The folding device 806 C-folds the web 980, but other known types of folding may be used instead. The bagging machine 800 includes a hold-open member, such as a finger 814 or other suitable device, to open and hold the container cavity within the opposing wall of the folded inflated web, providing a laterally facing internal container cavity 312 for side-loading with items.

[0083] The bagging machine 100 includes a sealing device 816 that activates the sealing materials 274, 278 to seal the inflated packaging unit 981. The sealing device 116 is configured to form the finished bag by applying heat, pressure, and / or other suitable means to set the sealing materials 274, 278. For example, if the sealing material is a strip seal, the sealing device applies heat to activate the sealing material.

[0084] The sealing device 816 includes a lateral sealing device 820 and a longitudinal sealing device 818. The lateral sealing device 820 is configured to activate a sealant 278 after the inflatable packaging unit 981 is folded to seal the underside of one inflatable packaging unit 981 and the upper side of an adjacent inflatable packaging unit 981, defining the bottom boundary of the container cavity 986. The longitudinal sealing device 818 is configured to activate a sealant 274 to seal the side boundaries of the inflatable packaging unit 981 and define the side boundaries of the container cavity 986. In this way, the longitudinal sealing device 818 seals and closes the completed bag 999 after the object has been inserted into the container cavity 986.

[0085] In another embodiment, the bagging machine does not include an inflation device in which the web from the supply structure is already inflated. In yet another embodiment, the bagging machine does not include an inflation device, and the web is supplied through the bagging machine without being inflated.

[0086] The bagging machine 800 includes a separation mechanism 818 configured to facilitate the separation of finished bags from the inflatable web 980, similar to the separation means described above for the bagging machine 700. In one embodiment, the sealing device can melt the upper boundary of the finished bag, and the separation mechanism can separate the finished bag from the adjacent packaging unit.

[0087] Although the bagging machines 700, 800 are depicted as being fed from certain non-inflated, high-density configurations (e.g., fanfold stack configuration 150 or roll configuration 550), it is understood that either machine 700, 800 can be fed from either type of aggregated configuration. In other embodiments, the web can be fed entirely through the bagging machines 700, 800 without inflation.

[0088] This disclosure is not limited in terms of the specific embodiments described herein, which are intended to be illustrative of various aspects. As will be apparent to those skilled in the art, many modifications and embodiments can be made without departing from the spirit and scope thereof. In addition to those listed herein, functionally equivalent methods and apparatus within the scope of this disclosure will be apparent to those skilled in the art from the foregoing description. Such modifications and embodiments are intended to be within the scope of the appended claims. This disclosure is limited only by the terms of the appended claims, along with any equivalent scope to which such claims are entitled. Furthermore, it should be understood that the terms used herein are for illustrative purposes only and are not intended to limit to specific embodiments.

[0089] With regard to the use of substantially any plural and / or singular terms herein, those skilled in the art can convert from plural to singular and / or singular to plural as appropriate to the context and / or use. Various singular / plural orderings may be expressly specified herein for clarity.

[0090] While various embodiments and examples have been disclosed herein, other embodiments and examples will be apparent to those skilled in the art. The various embodiments and examples disclosed herein are for illustrative purposes only and are not intended to limit, and the actual scope and spirit are set forth by the following claims.

Claims

1. a first wall and a second wall, each of the first wall and the second wall comprising: overlapping layers enclosing an expansion space therebetween; and an expandable composite material disposed in the expansion space, the expandable composite material comprising: an emulsion polyolefin dispersion comprising one or more polyolefins, a polymeric stabilizer comprising at least one polar polymer, and water; and a plurality of expandable microspheres configured to expand the emulsion polyolefin dispersion upon activation of the expandable microspheres; the first and second walls are nested together to define a container cavity therebetween configured and dimensioned to receive a product to be shipped therein, and expansion spaces of the first and second walls are nested together about the container cavity; The first and second walls are connected to each other on multiple sides of the container cavity.

2. the walls are not sealed to one another at an open side of the container cavity, the open side being dimensioned to permit insertion of a product into the container cavity; and 2. The protective material of claim 1, further comprising a closure on the first wall configured to seal the first wall to the second wall to seal the open side to retain the product within the cavity.

3. the first and second walls further comprising a web defining a plurality of connected protective packaging units configured to be connected to and separated from one another at a series of locations; The protective material of claim 2 , wherein each of the packaging units includes a pair of the expansion spaces overlapping each other for at least one of the protective container cavities.

4. 10. The protective material of claim 1, wherein the one or more polyolefins are thermoplastic.

5. 5. The protective material of claim 4, wherein the one or more polyolefins comprise an ethylene-based thermoplastic polymer, a propylene-based thermoplastic polymer, or a combination thereof.

6. 6. The protective material of claim 5, wherein the ethylene-based thermoplastic polymer comprises high density polyethylene (HDPE), linear low density polyethylene (LLDPE), low density polyethylene (LDPE), or a combination thereof.

7. The protective material according to claim 5 , wherein the propylene-based thermoplastic polymer is oriented polypropylene (OPP).

8. The protective material of claim 1 , wherein the expandable microspheres include a foaming agent.

9. The protective material of claim 1 , wherein the expandable microspheres include a reactive component, a chemical catalyst, or a combination thereof.

10. 9. The protective material of claim 8, wherein the expandable microspheres include a blowing agent including air, carbon dioxide, nitrogen, methane, ethane, propane, isobutane, n-butane, neopentane, an inert gas such as argon or helium, or a combination thereof.

11. The protective material of claim 1 , wherein the plurality of expandable microspheres comprises an outer shell and an inner core.

12. 12. The protective material of claim 11, wherein the shell of the plurality of expandable microspheres comprises a plurality of polyolefins.

13. The protective material of claim 1 , wherein the plurality of expandable microspheres comprises a hydrocarbon, water, or a combination thereof.

14. The protective material of claim 1 , wherein the expandable microspheres are configured to be thermally activated.

15. 10. The protective material of claim 1, wherein the expandable microspheres are configured to expand upon activation, thereby expanding the emulsion polyolefin dispersion.

16. 10. The protective material of claim 1, wherein the emulsion polyolefin dispersion is configured to solidify after expansion.

17. 2. The protective material of claim 1, wherein the expandable composite is provided in the expansion space in an amount sufficient to provide cushioning to a product contained in the container cavity after expansion of the emulsion polyolefin dispersion.

18. The protective material of claim 1 , wherein the microspheres are encapsulated in the emulsion polyolefin dispersion.

19. The inflatable device includes a first wall including a first layer defining an expansion region and an expandable composite of the expansion region, the expandable composite comprising: an emulsion polyolefin dispersion comprising one or more polyolefins, a polymeric stabilizer comprising at least one polar polymer, and water; and A protective material comprising a plurality of expandable microspheres configured to expand the emulsion polyolefin dispersion upon activation of the expandable microspheres.

20. The first wall includes a second layer superimposed and connected to the first layer, the first layer and 20. The protective material of claim 19, wherein the second layer defines a first expansion space therebetween surrounding the expansion region, the expandable composite being contained within the first expansion space.

21. [0023] Further comprising a second wall comprising: opposed substrate layers overlapping and connected to one another to define a second expansion space therebetween; and an additional amount of the expandable composite material contained in the second expansion space; 21. The protective material of claim 20, wherein the first and second walls are nested together to define a container cavity therebetween configured and dimensioned to receive a product to be shipped therein, the expansion spaces of the first and second walls being nested together about the container cavity, and the first and second walls being connected to each other on multiple sides of the container cavity.

22. 1st layer, The second layer, and an expandable composite material disposed between the first layer and the second layer; the expandable composite comprises an emulsion polyolefin dispersion and a plurality of expandable microspheres; and The emulsion polyolefin dispersion comprises one or more polyolefins, a polymeric stabilizer comprising at least one polar polymer, and water.

23. applying an expandable composite material onto a surface of the first layer; applying the second layer over the first layer such that the expandable composite is sandwiched between the first and second layers; The expandable composite material comprises: an emulsion polyolefin dispersion comprising one or more polyolefins, a polymeric stabilizer comprising at least one polar polymer, and water; and A method for making an expandable protective material comprising a plurality of expandable microspheres configured to expand an emulsion polyolefin dispersion upon activation of the expandable microspheres.

24. The protective material described in claim 1, wherein the first and second walls include a paper substrate.

25. The protective material described in claim 21, wherein the first and second walls include a paper substrate.

26. The expandable web of claim 22, wherein the first and second walls are formed from a paper substrate.