Electroluminescent devices with organic transport layers.

JP2023551765A5Active Publication Date: 2024-10-29SHOEI CHEM IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023524117
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2020-10-22
Filing Date
2021-10-21
Publication Date
2024-10-29
Estimated Expiration
2041-10-21

AI Technical Summary

Technical Problem

Existing electroluminescent devices, particularly quantum dot light-emitting diodes (QDLEDs), face challenges in achieving low turn-on voltages and high external quantum efficiencies while maintaining cost-effectiveness for mass production.

Method used

The development of electroluminescent devices with an organic transport layer, specifically an electron transport layer made from an organic material soluble in polar organic solvents, such as (1,3,5-triazine-2,4,6-triyl)tris(benzene-3,1-diyl)tris(diphenylphosphine oxide), which is deposited using a dissolution method to maximize contact area with light-emitting nanostructures, thereby reducing turn-on voltage and enhancing efficiency.

Benefits of technology

The solution results in electroluminescent devices with turn-on voltages below 1 V and external quantum efficiencies greater than 16%, improving device efficiency and cost-effectiveness for mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

An embodiment of an electroluminescent device is described. The electroluminescent device includes a substrate, a first electrode disposed on the substrate, a first transport layer disposed on the first electrode, an emissive layer having luminescent nanostructures disposed on the first transport layer, a second transport layer having an organic layer, and a second electrode disposed on the second transport layer. A first portion of the organic layer is disposed on the emissive layer and a second portion of the organic layer is disposed on the first transport layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an electroluminescent device (e.g., a light-emitting diode (LED)) having a light-emitting layer based on a luminescent nanostructure (NS-based).

Background Art

[0002] Electroluminescent devices are used as light sources in displays (e.g., phones, tablets, monitors, TVs, or digital billboards) and medical applications (e.g., photomedicine). An electroluminescent device can have a pair of transport layers and a light-emitting layer sandwiched between the transport layers. During operation, when a voltage is applied across the stack of the transport layer and the light-emitting layer, light can be emitted through one of the transport layers. Since electrons and holes recombine in the light-emitting layer to emit photons, light can be generated when a voltage is applied. Electrons and holes can be injected from electrodes disposed in the transport layer into the light-emitting layer. The light-emitting layer can include a light-emitting organic film or a luminescent NS (e.g., luminescent quantum dots (QDs)). An electroluminescent device having a light-emitting layer based on a light-emitting organic film is called an OLED, and an electroluminescent device having a light-emitting layer based on a luminescent NS can be called a QDLED.

[0003] One of the challenges of QDLEDs is to fabricate QDLEDs with a low turn-on voltage (e.g., a turn-on voltage less than about 1 V), which can improve, for example, device efficiency. Another challenge is to fabricate QDLEDs with a high external quantum efficiency (e.g., an EQE exceeding about 16%) at low cost using simple processing techniques for ease of mass production.

Summary of the Invention

[0004] The present disclosure provides an exemplary inexpensive QDLED having a low turn-on voltage (e.g., a turn-on voltage less than about 1 V) and a high EQE (e.g., an EQE exceeding about 16%). The present disclosure also provides an exemplary inexpensive method for manufacturing the same.

[0005] According to some embodiments, the electroluminescent device includes an array of pixels, a first transport layer disposed on a first electrode, an emissive layer having emissive nanostructures disposed on the first transport layer, a second transport layer having an organic layer, and a second electrode disposed on the second transport layer. The first portion of the organic layer is disposed on the emissive layer, and the second portion of the organic layer is disposed on the first transport layer.

[0006] According to some embodiments, the second portion of the organic layer is located within the gap between the first transport layer and the light-emitting nanostructure.

[0007] According to some embodiments, the organic material of the organic layer is soluble in polar organic solvents.

[0008] According to some embodiments, the organic material of the organic layer is soluble in alcohol, acetone, or acetonitrile.

[0009] According to some embodiments, the organic layer comprises an organic material having two or more phosphonic acid oxide functional groups (P=O).

[0010] According to some embodiments, the organic layer comprises (1,3,5-triazine-2,4,6-triyl)tris(benzene-3,1-diyl)tris(diphenylphosphine oxide) or 2,4,6-tris[3-(diphenylphosphinyl)phenyl]-1,3,5-triazine.

[0011] According to some embodiments, the turn-on voltage of the electroluminescent device is in the range of approximately 0.7V to approximately 1V.

[0012] According to some embodiments, the luminescent nanostructure comprises indium phosphide (InP).

[0013] According to some embodiments, the luminescent nanostructure includes quantum dots configured to emit light in the visible spectrum.

[0014] According to some embodiments, the light-emitting nanostructure includes a first group of quantum dots configured to emit red light and a second group of quantum dots configured to emit green light.

[0015] According to some embodiments, the first transport layer is a hole transport layer, and the second transport layer is an electron transport layer.

[0016] According to some embodiments, the display device includes an array of pixels and a display screen arranged on the array of pixels. Each pixel in the array of pixels includes a first and a second electroluminescent device. Each of the first and second electroluminescent devices includes a hole transport layer, an emissive layer having an emissive nanostructure arranged on the hole transport layer, and an electron transport layer having an organic layer. The emissive layer of the first electroluminescent device is configured to emit first light having a first peak wavelength. The emissive layer of the second electroluminescent device is configured to emit second light having a second peak wavelength different from the first peak wavelength.

[0017] According to some embodiments, a second portion of the organic layer is positioned within a gap between it and an adjacent luminescent nanostructure.

[0018] According to some embodiments, the organic layer does not contain inorganic material.

[0019] According to some embodiments, the organic layer comprises an organic material having two or more phosphonic acid oxide functional groups (P=O).

[0020] According to some embodiments, the organic layer comprises (1,3,5-triazine-2,4,6-triyl)tris(benzene-3,1-diyl)tris(diphenylphosphine oxide) or 2,4,6-tris[3-(diphenylphosphinyl)phenyl]-1,3,5-triazine.

[0021] According to some embodiments, a method for manufacturing an electroluminescent device includes providing a layer of anode material on a substrate, forming a hole transport layer on the layer of anode material, forming a layer of quantum dots on the hole transport layer, forming an electron transport layer having an organic layer on the layer of quantum dots using a dissolution method, and forming a cathode on the electron transport layer.

[0022] According to some embodiments, forming an electron transport layer involves preparing a solution of the organic material of the organic layer with a polar organic solvent.

[0023] According to some embodiments, forming an electron transport layer involves preparing a solution with an organic material having two or more phosphonic acid oxide functional groups (P=O).

[0024] According to some embodiments, forming a hybrid transport layer involves preparing a solution of (1,3,5-triazine-2,4,6-triyl)tris(benzene-3,1-diyl)tris(diphenylphosphine oxide) having three phosphonic acid oxide functional groups (P=O) with 2,4,6-tris[3-(diphenylphosphinyl)phenyl]-1,3,5-triazine.

[0025] Further features and advantages of the present invention, as well as the structure and operation of various embodiments of the present invention, are described in detail below with reference to the accompanying drawings. It should be noted that the present invention is not limited to the specific embodiments described herein. Such embodiments are presented herein for illustrative purposes only. Additional embodiments will be apparent to those skilled in the art based on the teachings contained herein.

[0026] The accompanying drawings incorporated herein and forming part of this specification, together with the description, illustrate the embodiments disclosed herein, further illustrate the principles of these embodiments, and help enable those skilled in the art to perform and use these embodiments. [Brief explanation of the drawing]

[0027] [Figure 1] A cross-sectional schematic view of an electroluminescent device that emits light from the lower part and has an organic transport layer according to some embodiments is shown. [Figure 2] A cross-sectional schematic view of an electroluminescent device that emits light from the lower part and has an organic transport layer according to some embodiments is shown. [Figure 3] A cross-sectional schematic view of the light-emitting layer and the transport layer of an electroluminescent device according to some embodiments is shown. [Figure 4] A cross-sectional schematic view of the light-emitting layer and the transport layer of an electroluminescent device according to some embodiments is shown. [Figure 5] It is a diagram for explaining the features of an electroluminescent device having an organic transport layer according to some embodiments. [Figure 6] It is a diagram for explaining the features of an electroluminescent device having an organic transport layer according to some embodiments. [Figure 7] It is a diagram for explaining the features of an electroluminescent device having an organic transport layer according to some embodiments. [Figure 8] It is a flowchart of a method for manufacturing an electroluminescent device having an organic transport layer according to some embodiments. [Figure 9] It is an exploded cross-sectional view of a light-emitting diode (LED) display device according to some embodiments. [Figure 10] It is a cross-sectional view of a pixel of an LED display device according to some embodiments. [Figure 11] It is a cross-sectional schematic view of a nanostructure (NS) according to some embodiments.

[0028] The features and advantages of the present invention will become further apparent from the detailed description provided below, in conjunction with the drawings, in which similar reference numerals identify corresponding elements throughout. In the drawings, similar reference numerals indicate identical, functionally similar, and / or structurally similar elements unless otherwise specified. The drawing in which an element first appears is indicated by the leftmost digit(s) in the corresponding reference numeral. Unless otherwise indicated, the drawings provided throughout this disclosure should not be construed as to scale. [Modes for carrying out the invention]

[0029] Specific configurations and arrangements may be discussed, but it should be understood that this is done for illustrative purposes only. Those skilled in the art will understand that other configurations and arrangements may be used without departing from the spirit and scope of the invention. It will be obvious to those skilled in the art that the invention may be employed in a variety of other applications beyond those specifically mentioned herein. It should be understood that the specific implementations shown and described herein are illustrative and are not intended in any way to limit the scope of the application.

[0030] References herein to “one embodiment,” “one example,” “exemplary embodiment,” etc., indicate that the described embodiments may include certain features, structures, or characteristics, but it is known that not all embodiments necessarily include certain features, structures, or characteristics. Furthermore, such expressions do not necessarily refer to the same embodiment. Moreover, if certain features, structures, or characteristics are described in relation to one embodiment, it is expected that achieving such features, structures, or characteristics in relation to other embodiments, whether explicitly stated or not, is within the knowledge of those skilled in the art.

[0031] All numbers in this description indicating the quantity, ratio, physical properties, and / or use of materials should be understood to be modified by the word “approximately,” unless otherwise clearly indicated.

[0032] In embodiments, the term “display device” refers to the arrangement of elements that enable the visible representation of data on a display screen. A suitable display screen may include a flat, curved, or otherwise molded screen, film, sheet, or other structure for visually displaying information to a user. Display devices described herein may include, for example, liquid crystal displays (LCDs), televisions, computers, monitors, mobile phones, smartphones, personal digital assistants (PDAs), game consoles, e-book devices, digital cameras, tablets, wearable devices, car navigation systems, digital billboards, augmented reality, virtual reality, and the like.

[0033] As used herein, the term "approximately" indicates a value of a given quantity changing by ±10% of the value. For example, "approximately 100 nm" encompasses a size range including 90 nm to 110 nm.

[0034] As used herein, the term "substantially" refers to a value of a given quantity change within ±1% to ±5% of the value.

[0035] In the embodiment, the term “optically coupled” means that the components are arranged so that light can pass from one component to another without substantial obstruction.

[0036] As used herein, the term “nanostructure” refers to a structure having at least one region or characteristic dimension having a dimension of less than approximately 500 nm. In some embodiments, the nanostructure has dimensions of less than approximately 200 nm, less than approximately 100 nm, less than approximately 50 nm, less than approximately 20 nm, or less than approximately 10 nm. Typically, the region or characteristic dimension will be along the smallest axis of the structure. Examples of such structures include nanowires, nanorods, nanotubes, branched nanostructures, nanotetrapods, tripods, bipods, nanocrystals, nanodots, QDs, nanoparticles, and the like. The nanostructure can be, for example, substantially crystalline, substantially monocrystalline, polycrystalline, amorphous, or a combination thereof. In some embodiments, each of the three dimensions of the nanostructure has dimensions of less than approximately 500 nm, less than approximately 200 nm, less than approximately 100 nm, less than approximately 50 nm, less than approximately 20 nm, or less than approximately 10 nm.

[0037] As used herein, the terms “QD” or “nanocrystal” refer to nanostructures that are substantially single crystals. Nanocrystals have at least one region or characteristic dimension having dimensions to the order of magnitude less than about 500 nm and less than about 1 nm. It will be readily understood by those skilled in the art that the terms “nanocrystal,” “QD,” “nanodot,” and “dot” represent similar structures and are used interchangeably herein. The present invention also encompasses the use of polycrystalline or amorphous nanocrystals.

[0038] When used in reference to nanostructures, the term “heterostructure” refers to a nanostructure characterized by two different and / or distinct material types. Typically, one region of the nanostructure contains a first material type, while a second region contains a second material type. In some embodiments, the nanostructure comprises a core of a first material and at least one shell of a second (or third, etc.) material, where the different material types are distributed radially, for example, along the long axis of a nanowire, the long axis of an arm of a branched nanowire, or around the center of a nanocrystal. The shell may, but does not need to, cover adjacent materials for a nanostructure that is considered a shell or a heterostructure; for example, a nanocrystal featuring a core of one material covered with small islands of the second material is a heterostructure. In other embodiments, the different material types are distributed at different locations within the nanostructure, for example, along the principal (long) axis of a nanowire or along the long axis of an arm of a branched nanowire. Different regions within a heterostructure may contain completely different materials, or different regions may contain substrates (e.g., silicon) with different dopants or different concentrations of the same dopant.

[0039] As used herein, the term “diameter” of a nanostructure refers to the diameter of a cross-section perpendicular to a first axis of the nanostructure, where the first axis has the greatest difference in length with respect to the second and third axes (the second and third axes being two axes of approximately equal length). The first axis is not necessarily the longest axis of the nanostructure; for example, for a disk-shaped nanostructure, the cross-section is substantially circular and perpendicular to the short longitudinal axis of the disk. If the cross-section is not circular, the diameter is the average of the long and short axes of that cross-section. For elongated or high-aspect-ratio nanostructures such as nanowires, the diameter is measured across a cross-section perpendicular to the longest axis of the nanowire. For spherical nanostructures, the diameter is measured from one face through the center of the sphere to the other.

[0040] When used in reference to nanostructures, the terms “crystalline” or “substantially crystalline” refer to the fact that nanostructures typically exhibit long-term ordering across two or more dimensions of the structure. The term “long-term ordering” will be understood by those skilled in the art to depend on the absolute size of a particular nanostructure, since ordering for a single crystal cannot extend beyond the crystal boundary. In this case, “long-term ordering” would mean substantial ordering across at least the majority of the dimensions of the nanostructure. In some cases, a nanostructure may consist of an oxide or other coating, or a core and at least one shell. In such cases, the oxide, shell(s), or other coating may, but do not need to, exhibit such ordering (e.g., it can be amorphous, polycrystalline, or otherwise). In such cases, the expressions “crystalline,” “substantially crystalline,” “substantially monocrystalline,” or “monocrystalline” refer to the central core of the nanostructure (excluding the coating layer or shell). When the terms “crystalline” or “substantially crystalline” are used herein, they are also intended to encompass structures that include various defects, stacking faults, atomic substitutions, etc., insofar as the structure exhibits substantial long-term ordering (e.g., ordering over at least about 80% of the length of at least one axis of the nanostructure or its core). In addition, it will be understood that interfaces between the core and the outer layer of a nanostructure, or between a core and an adjacent core, or between a shell and a second adjacent shell, may contain amorphous regions, or may even be amorphous. This does not prevent the nanostructure from being crystalline or substantially crystalline as defined herein.

[0041] When used in reference to nanostructures, the term "single-crystalline" indicates that the nanostructure is substantially crystalline and substantially contains a single crystal. When used in reference to heterostructures of nanostructures comprising a core and at least one shell, "single-crystalline" indicates that the core is substantially crystalline and substantially contains a single crystal.

[0042] As used herein, the term “ligand” refers to a molecule that can interact (weakly or strongly) with one or more surfaces of a nanostructure, for example, through covalent bonds, ionic bonds, van der Waals, or other molecular interactions.

[0043] As used herein, the term "quantum yield" (QY) refers to the ratio of emitted photons to photons absorbed by, for example, a nanostructure or a collection of nanostructures. As is known in the art, quantum yield is usually determined by a comparative method using well-characterized standard samples with known quantum yield values.

[0044] As used herein, the term “primary emission peak wavelength” refers to the wavelength at which the emission spectrum exhibits the highest intensity.

[0045] As used herein, the term "full width at half maximum" (FWHM) refers to a measurement of spectral width. In the case of emission spectra, FWHM may refer to the width of the emission spectrum at half the peak intensity value.

[0046] As used herein, the term "Forster radius" is also referred to as "Forster distance" in the art.

[0047] The term "nanostructured (NS) film" is used herein to refer to a film having a light-emitting nanostructure.

[0048] The term “red wavelength region” is used herein to refer to a wavelength region of the visible spectrum that may include wavelengths ranging from approximately 620 nm to approximately 750 nm, according to some embodiments.

[0049] The term “green wavelength region” is used herein to refer to a wavelength region of the visible spectrum that may include wavelengths ranging from approximately 495 nm to approximately 570 nm, according to some embodiments.

[0050] The term “blue wavelength region” is used herein to refer to a wavelength region of the visible spectrum that can include wavelengths ranging from approximately 435 nm to approximately 495 nm, according to some embodiments.

[0051] Published patents, patent applications, websites, company names, and scientific literature referenced herein are incorporated herein by reference in the same manner as if each were specifically and individually directed to be incorporated by reference. Any inconsistencies between the references cited herein and the specific teachings herein should be resolved in favor of the latter. Similarly, any inconsistencies between the definition of a word or phrase as understood in the art and the definition of a word or phrase as specifically taught herein should be resolved in favor of the latter.

[0052] Unless otherwise defined, the technical and scientific terms used herein have meanings that are generally understood by those skilled in the art to which this application relates. Various methodologies and materials known to those skilled in the art are referenced herein.

[0053] Exemplary Embodiments of Electroluminescent Devices with Hybrid Transport Layers Figure 1 illustrates schematic cross-sectional views of a lower-emitting electroluminescent device 100 according to several embodiments. In some embodiments, the electroluminescent device 100 can be used as a light source for a display device to generate an image. In some embodiments, the electroluminescent device 100 can be configured to emit light at a low turn-on voltage (e.g., less than about 1V) and at one or more primary emission peak wavelengths in the visible spectrum (e.g., primary emission peak wavelengths in the range of about 435nm to about 750nm).

[0054] In some embodiments, the electroluminescent device 100 may include a substrate 102 and a device stack 103 disposed on the substrate. The substrate 102 may be configured to support the device stack 103 and optionally to support a control circuit (not shown) for controlling the operation of the device stack 103. In some embodiments, the substrate 102 may be optically transparent so that light 101 generated by the device stack 103 can be emitted through the substrate 102 without substantially absorbing any light 101. The light 101 emitted from the device stack 103 is represented in Figure 1 by a black arrow pointing in the Z direction.

[0055] In some embodiments, the substrate 102 may contain a conductive material and have a vertical dimension (e.g., thickness) along the Z-axis ranging from about 10 μm to about 150 μm (e.g., about 10 μm, about 12 μm, about 25 μm, about 75 μm, about 100 μm, about 125 μm, or about 150 μm). In some embodiments, the surface 102s of the substrate 102 can serve as a screen for displaying an image generated using light 101. In some embodiments, the substrate 102 can serve as a shielding layer to provide environmental protection to the electroluminescent device 100.

[0056] The device stack 103 may, according to several embodiments, include an anode 104 placed on a substrate 102, a hole injection layer (HIL) 108 placed on the anode 104, a hole transport layer (HTL) 110 placed on the HIL 108, an emissive layer (EML) 114 placed on the HTL 110, an organic electron transport layer (OETL) 118 placed on the HTL 110, an electron injection layer (EIL) 120 placed on the OETL 118, and a cathode 122 placed on the EIL 120. In some embodiments, the device stack 103 may include the HTL 110 placed on the anode 104 and the cathode 122 placed on the OETL 118, without including the HIL 108 and EIL 120.

[0057] The electroluminescent device 100 can be configured to emit light 101 in the visible spectrum (e.g., red, green, or blue) based on the composition of the EML 114. The EML 114 may include one or more layers of luminescent NS, one or more luminescent organic layers, or a combination thereof. In some embodiments, the one or more layers of luminescent NS may include one or more layers of luminescent QD 124 placed on the HTL 110 without a matrix material. Each of the luminescent QD 124 may be analogous to the NS 1100 as described below with reference to Figure 11. Although one layer of QD 124 is shown in Figure 1, the EML 114 may have any number of layers of QD 124. Although the QD 124 are shown to have similar dimensions in Figure 1, the QD 124 may have different dimensions from one another. Furthermore, although the QD124 are shown in Figure 1 arranged in a horizontal row and physically touching adjacent QD124s, the EML114 can have QD124s arranged in offset rows, and / or one or more QD124s spaced apart from adjacent QD124s.

[0058] The size and material of the QD124 in the EML114 can be selected based on the desired color (e.g., red, green, or blue) of the light 101 emitted through the substrate 102. In some embodiments, the size and material of the QD124 in the EML114 can be selected to emit light 101 having a primary emission peak wavelength in the red wavelength region (e.g., wavelengths ranging from approximately 620 nm to 750 nm), the green wavelength region (e.g., wavelengths ranging from approximately 495 nm to 570 nm), or the blue wavelength region (e.g., wavelengths ranging from approximately 435 nm to 495 nm) of the visible spectrum. In some embodiments, the EML114 may have a single group of QD124 configured to emit red, green, blue, or any other light in the visible spectrum. In some embodiments, the EML114 may have two or more groups of QD124, each group of QD124 configured to emit light in a different visible spectrum than the other groups of QD124. In some embodiments, EML114 may include QD124 based on indium phosphide (InP) having a diameter ranging from approximately 4 nm to approximately 20 nm.

[0059] Light 101, having a primary emission peak wavelength in the visible spectrum, can be generated from the EML 114 and is emitted from the electroluminescent device 100 when a voltage is applied across the device stack 103 during operation. Since electrons and holes recombine in the EML 114 and emit photons corresponding to the wavelength in the visible wavelength region, light 101 can be generated when a voltage is applied. When a voltage is applied such that the anode 104 is positive with respect to the cathode 122, electrons and holes can be injected from the cathode 122 and the anode 104, respectively.

[0060] OETL118 facilitates electron transport from cathode 122 through EIL120 to EML114 and prevents holes from escaping EML114 during operation. The more electrons injected into EML114, the more photons are emitted from EML114 in the form of light 101, resulting in higher device efficiency, such as higher emission and higher EQE. To maximize electron injection into EML114, the contact area between OETL118 and EML114 is maximized. To maximize the contact area between OETL118 and EML114, OETL118 is formed on EML114 to cover the surface of QD124 that is not covered by adjacent QD124 and HTL110.

[0061] As shown in Figure 1, the OETL 118 can be formed to cover the top surface of the QD 124 and the surface of the QD 124 exposed within the gap of the EML 114. In some embodiments, the OETL 118 may include an organic layer of organic material(s) and may not include any inorganic material(s) and / or structure(s). The organic material of the OETL 118 can be deposited on the EML 114 by a dissolution method, which allows the organic material to be deposited conformally on the QD 124 and to diffuse through one or more layers of the QD 124 to fill the gap 125 and come into contact with the HTL 110. ETLs such as the OETL 118 formed by the dissolution method can provide a larger contact area with the QD 124 than other ETLs such as the ETL 318 containing inorganic nanoparticles as shown in Figure 3 and the ETL 418 containing organic material formed by evaporation under high vacuum as shown in Figure 4. The dissolution method allows for the deposition of OETL118 at a slower rate than the deposition rate used to form ETL418 by the high-vacuum evaporation method. As a result, the dissolution method can be more effective than the high-vacuum evaporation method in filling the gap 125 with organic material in OETL118. In addition, the dissolution method, which can be carried out at atmospheric pressure, may be more cost-effective than the high-vacuum evaporation method for forming OETL418.

[0062] Filling the gap 125 with organic material in OETL118 can also increase the contact area between OETL118 and HTL110. This increased contact between OETL118 and HTL110 can improve device efficiency by lowering the turn-on voltage of the electroluminescent device to less than approximately 1V (e.g., approximately 0.9V, 0.85V, 0.8V, 0.75V, or 0.7V). The lower turn-on voltage is due to the generation of photoluminescent emission by exciplex between the OETL118 and HTL110 materials.

[0063] In some embodiments, OETL118 can have a vertical dimension (e.g., thickness) along the Z-axis ranging from about 20 nm to about 120 nm (e.g., about 20 nm, about 40 nm, about 50 nm, about 60 nm, about 80 nm, about 100 nm, or about 120 nm). The organic material of OETL118 is selected so that the organic material is soluble in polar organic solvents, such as alcohol, acetone, acetonitrile, or a suitable polar organic solvent that does not damage QD124. In some embodiments, the organic material of OETL118 can contain two or more phosphonic acid oxide functional groups (P=O). For example, the organic material may include (1,3,5-triazine-2,4,6-triyl)tris(benzene-3,1-diyl)tris(diphenylphosphine oxide) having three P=O functional groups, 2,4,6-tris[3-(diphenylphosphinnyl)phenyl]-1,3,5-triazine (called POT2T), or bis[2-(diphenylphosphino)phenyl] ether oxide (called DPEPO) having two P=O functional groups. In some embodiments, the presence of P=O functional groups in OETL118 can induce exciplex photoluminescence emission between OETL118 and HTL110.

[0064] The anode 104 can be configured to inject holes into the device stack 103 when it becomes positively biased during operation. The anode 104 can include, according to some embodiments, an electrically conductive and optically transparent material, such as indium tin oxide (ITO). In some embodiments, the anode 104 can have a vertical dimension (e.g., thickness) along the Z axis ranging from about 50 nm to about 150 nm (e.g., about 50 nm, about 80 nm, about 100 nm, about 120 nm, about 125 nm, about 140 nm, or about 150 nm).

[0065] HIL108 can be formed on the anode 104. HIL108 can be configured to facilitate the injection of holes from the anode 104 into HTL110. In some embodiments, HIL108 can have a vertical dimension (e.g., thickness) along the Z axis ranging from about 3 nm to about 70 nm (e.g., about 3 nm, about 10 nm, about 30 nm, about 40 nm, about 50 nm, about 60 nm, or about 70 nm). In some embodiments, HIL108 may include p-type or n-type organic or inorganic semiconductor materials, such as metal oxides (e.g., nickel oxide (NiO), molybdenum oxide (MoO3), vanadium oxide (V2O5), tungsten oxide (WO3)), polyaniline, poly(styrene sulfonate) (PSS)-doped polythiophenes (e.g., poly(3,4-ethylenedioxythiophene) (PEDOT), tris[phenyl(m-tolyl)amino]triphenylamine (mTDATA), or hexaazatriphenylene-hexacarbonitride (HAT-CN)).

[0066] In some embodiments, the HTL110 can be formed on the HIL108 as shown in Figure 1, or on the anode 104 if the HIL108 is optionally not included. The HTL110 can be configured to facilitate the transport of holes from the HIL108 to the EML114. In some embodiments, the HTL110 can have a vertical dimension (e.g., thickness) along the Z axis ranging from about 10 nm to about 30 nm (e.g., about 10 nm, about 20 nm, or about 30 nm). In some embodiments, HTL110 may include p-type organic or inorganic semiconductor materials, such as metal oxides (e.g., nickel oxide (NiO), molybdenum oxide (MoO3), vanadium oxide (V2O5), tungsten oxide (WO3)), polymers (e.g., poly(N-vinylcarbazole), poly(triarylamine), triphenylamine derivatives, or carbazole derivatives), or small organic molecules (e.g., N,N-di(1-naphthyl)-N,N-diphenyl-(1,1-biphenyl)4,4-diamine (NPB)). In some embodiments, HTL110 and HIL108 may include materials similar to or different from each other.

[0067] EIL120 can be formed on OETL118 and configured to facilitate electron injection from cathode 122 to OETL118 by forming contact with the cathode that follows or nearly follows Ohm's law. In some embodiments, EIL120 may include n-type semiconductor materials, alkali metal salts (e.g., lithium fluoride (LiF) or cesium carbonate (Cs2CO3), metals with low work functions (e.g., calcium (Ca), barium (Ba), magnesium (Mg), ytterbium (Yb) or cesium (Cs)), or organic compounds (e.g., polyfluorene, polyethyleneimine ethoxylated (PEIE), or lithium-8-hydroxyquinoline oleate (Liq)). In some embodiments, OETL118 and EIL120 may include materials similar to or different from each other.

[0068] The cathode 122 can be formed on the EIL 120, or directly on the OETL 118 if the EIL 120 is optionally not included. The cathode 122 can be configured to inject electrons into the device stack 103 when negatively biased during operation, as discussed above. In some embodiments, the cathode 122 can have a vertical dimension (e.g., thickness) along the Z axis ranging from about 100 nm to about 5 μm (e.g., about 250 nm, about 280 nm, about 300 nm, about 500 nm, about 1 μm, or about 5 μm). The cathode 122 can include a conductive and optically reflective material, such as aluminum (Al) or silver (Ag), according to some embodiments. The reflective material of the cathode 122 can help reflect light toward the substrate 102 and help prevent light from being emitted through the cathode 122. The light generated by the emission of photons following electron-hole recombination in EML114 (discussed above) can travel toward the cathode 122 and the substrate 102. The reflective material of the cathode 122 helps to redirect these photons toward the substrate 102 for radiation from the electroluminescent device 100.

[0069] In some embodiments, the layer order of device 103 may be reversed, as shown in the electroluminescent device 200 in Figure 2. The discussion of the electroluminescent device 100 applies to the electroluminescent device 200, except that the cathode 122 may contain an optically transparent material and the anode 104 may contain an optically reflective material.

[0070] In some embodiments, the electroluminescent device 100 can be a top-emitting electroluminescent device, where the light 101 may be emitted through the surface 103s of the device 103 instead of the surface 102s of the substrate 102. The discussion of the electroluminescent device 100 applies to a top-emitting electroluminescent device, except that the substrate 102 can be optically reflective and the cathode 122 and anode 104 can be optically transparent.

[0071] Elements described in this disclosure as existing on or over other elements may be directly together with such other elements or have an intervening layer, unless otherwise specified. While some of the elements in Figures 1-2 are shown to have similar dimensions along the X, Y, and / or Z axes with respect to one another, each of these elements may have different dimensions in one or more directions without departing from the scope or spirit of the invention.

[0072] Exemplary features of a field-emitting device with an organic transport layer Figure 5 illustrates (i) PL spectrum 536 of the InP QD layer, (ii) PL spectrum 538 of electroluminescent device A (e.g., electroluminescent device 100) having an EML with InP QDs (e.g., EML114 in Figures 1-2) and an organic ETL with POT2T formed by dissolution (e.g., OETL118), and (iii) PL spectrum 540 of electroluminescent device B having an EML with InP QDs (e.g., EML114 in Figure 3) and an ETL with only a ZnMgO NS layer (e.g., ETL318 in Figure 3). The InP QD can represent QD124 in Figures 1-4. The higher intensity of PL spectrum 538 compared to PL spectrum 540 indicates that a larger contact area between the POT2T layer and the InP QD improves the luminescence characteristics of the electroluminescent device compared to electroluminescent device B. Furthermore, the even higher intensity of PL spectrum 536 compared to PL spectra 538 and 540 indicates that both electroluminescent devices A and B exhibited some degree of PL quenching.

[0073] Figure 6 illustrates (i) plots of current density and drive voltage 642 and luminance and drive voltage 644 for electroluminescent device A, (ii) plots of current density and drive voltage 646 and luminance and drive voltage 648 for electroluminescent device B, and (iii) plots of current density and drive voltage 650 and luminance and drive voltage 652 for electroluminescent device C having an EML with InP QD (e.g., EML114 in Figure 4) and an ETL with a POT2T layer formed by high vacuum evaporation (e.g., ETL418 in Figure 4). Electroluminescent device A, having a dissolved organic ETL, exhibits a lower turn-on voltage than electroluminescent devices B and C.

[0074] Figure 7 illustrates (i) plots of EQE and luminance for electroluminescent device A (754), (ii) plots of EQE and luminance for electroluminescent device B (755), and (iii) plots of EQE and luminance for electroluminescent device C (756). Electroluminescent device A, which has dissolved organic ETL, exhibits a higher EQE than electroluminescent devices B and C. Therefore, the use of dissolved organic ETL improves the device efficiency of electroluminescent device A.

[0075] Exemplary method for manufacturing a field-emitting device with an organic transport layer Figure 8 is a flowchart of an exemplary method 800 for manufacturing an electroluminescent device 100 according to several embodiments. The steps can be carried out in various orders or may not be carried out according to a particular application. It should be noted that method 800 does not have to produce a complete electroluminescent device. Therefore, it is understood that additional processes can be provided before, during, and after method 800, and several other processes may be described herein only briefly.

[0076] In step 805, a substrate with a layer prior to the placement of the anode is provided. For example, as shown in Figure 1, the anode 104 can be placed on the substrate 102. In some embodiments, the substrate 102 can be optically transparent and may contain a conductive material. The anode 104 may, according to some embodiments, contain an electrically conductive and optically transparent material, such as indium tin oxide (ITO). In some embodiments, the anode 104 can be formed on the substrate 102 by depositing and patterning an electrically conductive and optically transparent material onto the substrate 102. Deposition can be carried out, for example, by sputtering, thermal evaporation, or a method suitable for depositing an electrically conductive and optically transparent material. Patterning can be carried out by a lithographic or masking method during deposition.

[0077] In step 810, HIL is formed on the anode and HTL is formed on the HIL. For example, as shown in Figure 1, HIL 108 may be placed on the anode 104 and HTL 110 may be placed on HIL 108. HIL 108 and HTL 110 can each be deposited on their underlying layers by, for example, spin coating, inkjet printing, slot die coating, nozzle printing, contact printing, preferred solution printing techniques, roll-to-roll processing, thermal evaporation, or preferred vapor deposition techniques. In some embodiments, HIL 108 may contain PSS (poly(styrene sulfonate) doped PEDOT (poly(3,4-ethylenedioxythiophene)) and HTL 110 may contain TFB (poly[(9,9-dioctylfluorenyl-2,7-diyl)-co-(4,4'(N-(4-sec-butylphenyl)))diphenylamine)]).

[0078] In step 815, the EML is formed on the HTL. For example, as shown in Figure 1, EML 114 may be placed on the HTL 110. In some embodiments, EML 114 may be formed by preparing a 9 mg / ml solution of QD 124 and depositing the solution on the HTL 110 by, for example, spin coating, inkjet printing, slot die coating, nozzle printing, contact printing, a suitable solution printing technique, thermal evaporation, or a suitable deposition technique. In some embodiments, QD 124 may include indium phosphide (InP) based QDs having a diameter ranging from about 20 nm to about 40 nm and may be configured to emit a primary emission peak wavelength in the red or green wavelength region.

[0079] In some embodiments, step 810 can be any step, and step 805 may be followed by step 815, in which case the EML is formed on the anode.

[0080] In step 820, the OETL is formed on the EML and the EIL is formed on the OETL. For example, as shown in Figure 1, the OETL 118 may be placed on the EML 114 and the EIL 120 may be placed on the OETL 118. In some embodiments, the formation of the OETL 118 may involve preparing a solution of the organic material of the OETL 118 in a polar organic solvent, such as alcohol, acetone, acetonitrile, or a suitable polar organic solvent that does not damage the QD 124, and depositing the solution on the EML 114 by a dissolution method. During the deposition process, the solution diffuses through one or more layers of QD 124, filling the gaps with the organic material and coming into contact with the HTL 110. In some embodiments, the solution may include a 16 mg / ml solution of POT 2T in methanol.

[0081] EIL120 can be deposited on OETL118 by, for example, spin coating, inkjet printing, slot die coating, nozzle printing, contact printing, suitable solution printing techniques, thermal evaporation, or suitable vapor deposition techniques.

[0082] In step 825, the cathode is formed on the EIL. For example, as shown in Figure 1, the cathode 122 may be placed on the EIL 120. According to some embodiments, the cathode 122 may be made of a material that is electrically conductive and optically reflective, such as aluminum (Al) or silver (Ag). In some embodiments, the cathode 122 can be formed by depositing the cathode material on the EIL 120 by, for example, sputtering, thermal evaporation, a suitable solution printing technique, or a method suitable for depositing an electrically conductive and optically reflective material.

[0083] Exemplary Embodiment of an LED Display Device Figure 9 illustrates an exploded cross-sectional schematic view of an LED display device 900 according to several embodiments. According to several embodiments, the LED display device 900 may include a back plate 958, a plurality of pixels 960 arranged in a 2D array on the back plate 958, and a transmissive cover plate 962. The number of pixels shown in Figure 9 is for illustrative purposes only and is not limiting. The device 900 may have any number of pixels without departing from the spirit and scope of this disclosure. The LED display device 900 may be called a QD-LED display device if QD-type electroluminescent devices are used as light sources in the pixels 960.

[0084] The cover plate 962 can serve as a display screen for generating images and / or can be configured to provide environmental sealing for the basic structure of the LED display device. The cover plate 962 can also be configured to be an optically transparent substrate on which other components of the LED display device 900 (e.g., electrodes) can be placed. In some embodiments, the pixels 960 can be trichromatic, having red, green, and blue subpixels. In some embodiments, the pixels 960 can be monochromatic, having red, green, or blue subpixels. In some embodiments, the LED display device 900 can have a combination of both trichromatic and monochromatic pixels 960.

[0085] The LED display device 900 may further include a control circuit (not shown) for the pixels 960. The pixels 960 can be independently controlled by a switching device, such as a thin-film transistor (TFT). Without departing from the spirit and scope of the present invention, the LED display device 900 may have geometric shapes such as, for example, cylindrical, trapezoidal, spherical, or elliptical, but not limited to these, according to various embodiments. Although the back plate 958, the array of pixels 960, and the cover plate 430 are shown in Figure 9 to have similar dimensions along the X-axis, each of these components may have different dimensions in one or more directions according to various embodiments.

[0086] Figure 10 illustrates an exploded cross-section of a trichromatic pixel 960 of an LED display device 900 according to several embodiments. The pixel 960 may include a red subpixel 960R, a green subpixel 960G, and a blue subpixel 960B. The arrangement of the red, green, and blue subpixels 960R, 960G, and 960B is illustrative and not limiting. The red, green, and blue subpixels 960R, 960G, and 960B can be arranged in any order with respect to each other.

[0087] Each of the red, green, and blue subpixels 960R, 960G, and 960B may include electroluminescent devices 1064R, 1064G, and 1064B, respectively, configured to provide primary red, green, and blue light, which may be transmitted to and distributed throughout the display screen (e.g., cover plate 962) of the LED display device 900. Except for the material and size of the QD (e.g., QD124) in the EML (e.g., EML114) of the electroluminescent devices 1064R, 1064G, and 1064B, they may be similar to the electroluminescent devices 100 or 200 described with reference to Figures 1-2. The size and material of the QD in the EML of the electroluminescent devices 1064R, 1064G, and 1064B may be selected to emit light having a primary emission peak wavelength in the red, green, and blue wavelength regions, respectively.

[0088] Exemplary Embodiments of Light-Emitting Nanostructures Coated with a Barrier Layer Figure 11 illustrates the cross-sectional structure of a light-emitting nanostructure (NS) 1100 coated with a barrier layer according to several embodiments. In some embodiments, a group of NS 1100s can represent QD 124 contained in EML 114. A barrier-coated NS 1100 includes NS 1101 and a barrier layer 1106. NS 1101 includes a core 1102 and a shell 1104. The core 1102 contains a light-emitting semiconductor material. Examples of semiconductor materials for the core 1102 include indium phosphide (InP), cadmium selenide (CdSe), zinc sulfide (ZnS), lead sulfide (PbS), indium arsenide (InAs), indium gallium phosphide (InGaP), zinc cadmium selenide (CdZnSe), zinc selenide (ZnSe), and cadmium telluride (CdTe). Any other Group II-VI, Group III-V, tertiary, or quaternary semiconductor structure exhibiting a direct band gap can be successfully used. In one embodiment, core 1102 can also provide several examples including one or more dopants such as metals, halogens, and alloys. Examples of metal dopants include, but are not limited to, zinc (Zn), copper (Cu), aluminum (Al), platinum (Pt), chromium (Cr), tungsten (W), palladium (Pd), or combinations thereof. Examples of halogen dopants include, but are not limited to, fluorine (F), chlorine (Cl), bromine (Br), or iodine (I). The presence of one or more dopants in core 1102 can improve the structural, electrical, and / or optical stability and QY of NS1101 compared to undoped NS.

[0089] The core 1102 can have a size of less than 20 nm in diameter according to several embodiments. In another embodiment, the core 1102 can have a size between approximately 1 nm and approximately 10 nm in diameter. The ability to tailor the size of the core 1102 to the purpose and the resulting size of the NS 1101 in the nanometer range allows for a photon emission range across the entire optical spectrum. Generally, larger NSs emit light toward the red edge of the spectrum, while smaller NSs emit light toward the blue edge of the spectrum. This effect arises because larger NSs have a narrower spacing between energy levels than smaller NSs. This allows the NSs to absorb photons with even lower energy, i.e., closer to the red edge of the spectrum.

[0090] The shell 1104 surrounds the core 1102 and is positioned on the outer surface of the core 1102. The shell 1104 may include, but is not limited to, cadmium sulfide (CdS), zinc cadmium sulfide (ZnCdS), zinc selenide sulfide (ZnSeS), and zinc sulfide (ZnS). In one embodiment, the shell 1104 has a thickness 1104t and can have, for example, one or more single layers. In other embodiments, the shell 1104 may have a thickness 1104t between approximately 1 nm and approximately 10 nm. The shell 1104 can be used to help reduce lattice mismatch with the core 1102 and improve the QY of NS1101. The shell 1104 can help passivate and remove surface trapping conditions such as dangling bonds on the core 1102, thereby increasing the QY of NS1101. The presence of surface trapping conditions provides non-radial recombination centers and can contribute to a decrease in the luminescence efficiency of NS1101.

[0091] In alternative embodiments, NS1101 may include a second shell positioned on the shell 1104, or two or more shells surrounding the core 1102, without departing from the spirit and scope of the invention. In one embodiment, the second shell may be one or more single layers thick and, although not required, is usually a semiconductor material. Other materials may be used without departing from the spirit and scope of the invention, but the material of the second shell may be zinc sulfide (ZnS), and a dopant may also be included.

[0092] The barrier layer 1106 can be configured to form a coating on the NS1101. In one embodiment, the barrier layer is positioned on the outer surface 1104a of the shell 1104 and is in substantial contact with it. In embodiments of the NS1101 having one or more shells, the barrier layer 1106 can be positioned on the outermost shell of the NS1101 and is in substantial contact with it. In exemplary embodiments, the barrier layer 1106 can be configured to act as a spacer between the NS1101 and one or more NS in a solution, composition, and / or film having multiple NSs, where the multiple NSs can be analogous to the NS1101 and / or the NS1101 coated with the barrier layer. In such NS solutions, compositions, and / or NS films, the barrier layer 1106 helps prevent aggregation of the NS1101 with adjacent NSs. Aggregation of the NS1101 with adjacent NSs leads to an increase in the size of the NS1101, which can result in a decrease or quenching of the luminescence properties of the aggregated NS (not shown), including the NS1101. In further embodiments, the barrier layer 1106 provides protection for NS1101 from, for example, moisture, air and / or harsh environments (e.g., high temperatures and chemicals used during lithography of NS and / or during the manufacturing process of NS system equipment) that could adversely affect the structural and optical properties of NS1101.

[0093] The barrier layer 1106 may include one or more materials that are amorphous, optically transparent, and / or electrically inert. Preferred barrier layers include, but are not limited to, inorganic materials such as inorganic oxides, halogen compounds, and nitrides. Examples of materials for the barrier layer 1106 include oxides and / or nitrides of Al, Ba, Ca, Mg, Ni, Si, Ti, or Zr, depending on the various embodiments. The barrier layer 1106 may have a thickness 1106t ranging from about 0.5 nm to about 15 nm in various embodiments.

[0094] The NS1100 coated with the barrier layer further or optionally includes a buffer layer 1107 configured to form a buffered coating on the NS1101. In one embodiment, the buffer layer 1107 is located on the shell 1104 and is in substantial contact with the outer surface 1104a of the shell 1104 and the inner surface 1106a of the barrier layer 1106. The buffer layer 1107 can be configured to act as a buffer between the NS1101 and the chemicals used during subsequent processing on the NS1101, such as the formation of the barrier layer 1106 on the NS1101.

[0095] The buffer layer 1107 can help substantially reduce and / or prevent quenching of the luminescence properties of NS1101 due to reactions with chemicals used during subsequent processing on NS1101. The buffer layer 1107 may include one or more materials that are amorphous, optically transparent, and / or electrically active. The one or more materials of the buffer layer 1107 may include inorganic and organic materials. Examples of inorganic materials for the buffer layer 1107 include metal oxides and / or nitrides, depending on the various embodiments. Examples of metal oxides include ZnO, TiO2, In2O3, Ga2O3, SnO2, Al2O3, or MgO. The buffer layer 1107 may have a thickness 1107t ranging from about 1 nm to about 5 nm in various embodiments.

[0096] As illustrated in Figure 11, the barrier-coated NS1100 further or optionally includes a plurality of ligands or surfactants 1108 according to some embodiments. The ligands or surfactants 1108 may be adsorbed or bound to the outer surface of the barrier-coated NS1100, for example, the outer surface of the barrier layer 1106 or the outer surface of the shell 1104 or a second shell, according to some embodiments. The plurality of ligands or surfactants 1108 may include hydrophilic or polar heads 1108a and hydrophobic or nonpolar tails 1108b. The hydrophilic or polar heads 1108a can bind to the barrier layer 1106. The presence of ligands or surfactants 1108 can help separate NS1100 and / or NS1101 from other NS during their formation, for example, in solutions, compositions and / or films. If NS can aggregate during their formation, the quantum efficiency of NS such as NS1100 and / or NS1101 may decrease. By using a ligand or surfactant 1108, specific properties such as hydrophobicity can be imparted to the barrier-coated NS1100, providing miscibility in nonpolar solvents or a reaction site (e.g., reversed-phase micelle system) to which other compounds can bind.

[0097] A wide variety of ligands exist that can be used as ligand 1108. In some embodiments, the ligand is a fatty acid selected from lauric acid, caproic acid, myristic acid, palmitic acid, stearic acid, and oleic acid. In some embodiments, the ligand is an organic phosphine or organic phosphine oxide selected from trioctylphosphine oxide (TOPO), trioctylphosphine (TOP), diphenylphosphine (DPP), triphenylphosphine oxide, and tributylphosphine oxide. In some embodiments, the ligand is an amine selected from dodecylamine, oleylamine, hexadecylamine, and octadecylamine. In some embodiments, the ligand is trioctylphosphine (TOP). In some embodiments, the ligand is oleylamine. In some embodiments, the ligand is a thiol, for example, octanthiol. In some embodiments, the ligand is diphenylphosphine. In some embodiments, the ligand is a neutral salt of any of these fatty acids, or a chalcogenide of these amines, phosphines, or phosphine oxides, such as zinc oleate, zinc laurate, TOP-selenized, or TOP-sulfurized.

[0098] A wide variety of surfactants exist that can be used as surfactant 1108. Nonionic surfactants can be used as surfactant 1108 in some embodiments. Some examples of nonionic surfactants include polyoxyethylene(5) nonylphenyl ether (trade name IGEPAL CO-520), polyoxyethylene(9) nonylphenyl ether (IGEPAL CO-630), octylphenoxypoly(ethyleneoxy)ethanol (IGEPAL CA-630), polyethylene glycol oleyl ether (Brij 93), polyethylene glycol hexadecyl ether (Brij 52), polyethylene glycol octadecyl ether (Brij S10), polyoxyethylene(10) isooctylcyclohexyl ether (Triton X-100), and polyoxyethylene branched nonylcyclohexyl ether (Triton N-101).

[0099] Anionic surfactants can be used as surfactant 1108 in some embodiments. Some examples of anionic surfactants include sodium dioctyl sulfosuccinate, sodium stearate, sodium lauryl sulfate, sodium monododecyl phosphate, sodium dodecylbenzenesulfonate, and sodium myristyl sulfate.

[0100] In some embodiments, NS1101 and / or NS1100 can be synthesized to emit light in one or more different color ranges, for example, in the range of red, orange, and / or yellow. In some embodiments, NS1101 and / or NS1100 can be synthesized to emit light in the range of green and / or yellow. In some embodiments, NS1101 and / or NS1100 can be synthesized to emit light in the range of blue, indigo, violet, and / or ultraviolet. In some embodiments, NS1101 and / or NS1100 can be synthesized to have primary emission peak wavelengths between 605 nm and 650 nm, between 510 nm and 550 nm, and between 300 nm and 495 nm.

[0101] NS1101 and / or NS1100 can be synthesized to exhibit a high QY. In some embodiments, NS1101 and / or NS1100 can be synthesized to exhibit a QY between 80% and 100%, or between 85% and 90%.

[0102] Therefore, according to various embodiments, NS1100 can be synthesized such that the presence of the barrier layer 1106 on NS1101 does not substantially alter or quench the luminescence properties of NS1101.

[0103] Exemplary Embodiments of Luminescent Nanostructures This specification describes various compositions having luminescent nanostructures (NS) that can represent QD124 of EML114. The various properties of the luminescent nanostructures, including their absorption properties, luminescence properties, and refractive index properties, can be tailored to the purpose and adapted for various applications.

[0104] The material properties of NS can be substantially homogeneous, or in some embodiments, heterogeneous. The optical properties of NS can be determined by its particle size, chemical composition, or surface composition. The ability to tailor the size of emitting NS to a desired range between approximately 1 nm and 20 nm allows for a wide range of photon emission across the entire optical spectrum, providing great versatility in color rendering. Particle encapsulation can provide robustness against chemically and UV-degradable materials.

[0105] The luminescent nanocrystals for use in the embodiments described herein can be manufactured using any method known to those skilled in the art. Preferred methods and exemplary nanocrystals are disclosed in U.S. Patent No. 7,374,807; U.S. Patent Application No. 10 / 796,832 filed March 10, 2004; U.S. Patent No. 6,949,206; and U.S. Provisional Patent Application No. 60 / 578,236 filed June 8, 2004, each of which is incorporated herein by reference as a whole.

[0106] The luminescent NS for use in the embodiments described herein can be manufactured from any suitable material, including inorganic materials, and more preferably inorganic conductive or semiconductor materials. Suitable semiconductor materials include those disclosed in U.S. Patent Application No. 10 / 796,832, and include any type of semiconductor, including Group II-VI, Group IILV, Group IV-VI, Group I-III-VI, and Group IV semiconductors. Suitable semiconductor materials include Si, Ge, Sn, Se, Te, B, C (including diamond), P, BN, BP, BAs, AIN, AlP, AlAs, AlSb, GaN, GaP, GaAs, GaSb, InN, InP, InAs, InSb, AIN, A1P, AlAs, AlSb, GaN, GaP, GaAs, GaSb, ZnO, ZnS, ZnSe, ZnTe, CdS, CdSe, CdTe, HgS, HgSe, HgTe, BeS Examples include, but are not limited to, BeSe, BeTe, MgS, MgSe, GeS, GeSe, GeTe, SuS, SnSe, SnTe, PbO, PbS, PbSe, PbTe, CuF, CuCl, CuBr, Cui, Si3N4, Ge3N4, Al2O3, (Al,Ga,In)2, (S,Se,Te)3, A12CO, CuInGaS, CuInGaSe, and two or more suitable combinations of such semiconductors.

[0107] In some embodiments, the luminescent NS may have a group-derived dopant consisting of a p-type dopant or an n-type dopant. The NS may also be a II-VI or III-V semiconductor. Examples of II-VI or III-V semiconductor NS include any combination of Group II elements from the periodic table, such as Zn, Cd, and Hg, with Group VI elements such as S, Se, Te, and Po; and any combination of Group III elements from the periodic table, such as B, Al, Ga, In, and Tl, with Group V elements such as N, P, As, Sb, and Bi.

[0108] The luminescent NSs described herein may further include ligands bound, linked, associated, or linked to their surface. Suitable ligands include any group known to those skilled in the art, including those disclosed in U.S. Patent Publications 8,283,412; 2008 / 0237540; 2010 / 0110728; 8,563,133; 7,645,397; 7,374,807; 6,949,206; 7,572,393; and 7,267,875, each of which is incorporated herein by reference. The use of such ligands can enhance the ability of luminescent NSs to be incorporated into various solvents and matrices, including polymers. Increased miscibility (i.e., the ability to mix without separation) of luminescent NSs in various solvents and matrices allows them to be dispersed throughout the polymer composition without agglomerating together and thus without scattering light. Such ligands are referred to herein as “miscibility-enhancing” ligands.

[0109] In some embodiments, compositions are provided having luminescent NS distributed or embedded in a matrix material. Suitable matrix materials can be any material known to those skilled in the art, including polymer materials and organic and inorganic oxides. The compositions described herein may be layers, encapsulants, coatings, sheets, or films. In embodiments described herein referring to layers, polymer layers, matrices, sheets, or films, these terms are used interchangeably, and the embodiments described in this manner are not limited to any one type of composition, but should be understood to encompass any matrix material or layer described herein or known in the art.

[0110] Downconverting NS (for example, as disclosed in U.S. Patent No. 7,374,807) utilizes the luminescence properties of luminescent nanostructures that are tuned to absorb light of a specific wavelength and then emit light at a second wavelength, thereby providing improved performance and efficiency of the active source (e.g., LED).

[0111] While luminescent NS can be produced using any method known to those skilled in the art, solution-phase colloid methods can be used for controlling the growth of inorganic nanomaterial phosphorescent bodies. See Alivisatos, AP, "Semiconductor clusters, nanocrystals, and quantum dots," Science, 271:933 (1996); X. Peng, M. Schlamp, A. Kadavanich, A. Alivisatos, "Epitaxial growth of highly luminescent CdSe / CdS Core / Shell nanocrystals with photostability and electronic accessibility," J. Am. Chem. Soc. 30:7019-7029 (1997); and CBMurray, DJ Norris, M. Bawendi, "Synthesis and characterization of nearly monodisperse CdE (E=sulfur,selenium,tellurium) semiconductor nanocrystallites," J. Am. Chem. Soc. 115:8706 (1993), the disclosures of which are incorporated herein by reference in their entirety.

[0112] According to some embodiments, for the relative completion of the synthesis of this material, CdSe can be used as the NS material for visible light downconversion in one example. For general surface chemical use, cadmium-free NS may also be used instead.

[0113] In semiconductor NS, photo-induced emission arises from the band edge states of the NS. Band edge emission originating from the emitting NS competes with radioactive and non-radioactive decay channels originating from the surface electronic states. X. Peng, et al., J. Am. Chem. Soc. 30:7019-7029 (1997). Consequently, the presence of surface defects such as dangling bonds provides non-radioactive recombination centers, contributing to a decrease in emission efficiency. An efficient and permanent method for passivating and removing surface trapped states may be to epitaxially grow an inorganic shell material on the surface of the NS. X. Peng, et al., J. Am. Chem. Soc. 30:701,9-7029 (1997). The shell material can be selected such that its electronic levels are type 1 with respect to the core material (e.g., with a larger band gap that provides a voltage step that localizes electrons and holes in the core). Consequently, the probability of non-radioactive recombination may be reduced.

[0114] The core-shell structure can be obtained by adding an organometallic precursor containing the shell material to a reaction mixture containing the core (NS). In this case, the core acts as a nucleus, allowing the shell to grow from its surface, rather than growth being driven by subsequent nucleation events. The reaction temperature is kept low to favor the addition of the shell material monomer to the core surface, while preventing independent nucleation of nanocrystals of the shell material. A surfactant in the reaction mixture is present to direct the controlled growth of the shell material and ensure solubility. When there is little lattice mismatch between the two materials, a uniform and epitaxially grown shell can be obtained.

[0115] Exemplary materials for preparing core-shell luminescent NS include Si, Ge, Sn, Se, Te, B, C (including diamond), P, Co, Au, BN, BP, BAs, AIN, A1P, AlAs, AlSb, GaN, GaP, GaAs, GaSb, InN, InP, InAs, InSb, AIN, A1P, AlAs, AlSb, GaN, GaP, GaAs, GaSb, ZnO, ZnS, ZnSe, ZnTe, CdS, CdSe, CdTe, HgS, HgSe, HgTc, BeS, BcSe, BcTe, MgS, MgSe, GeS, GeSe, GeT Examples of shell-emitting NS for use in the practice of the present invention include, but are not limited to, e, SnS, SnSe, SnTe, PbO, PbS, PbSe, PbTe, CuP, CuCl, CuBr, Cui, Si3N4, Ge3N4, Al2O3, (Al,Ga,In)2, (S,Se,Te)3, and AlCO. Examples of shell-emitting NS for use in the practice of the present invention include, but are not limited to, CdSe / ZnS, InP / ZnS, InP / ZnSe, PbSe / PbS, CdSe / CdS, CdTe / CdS, CdTe / ZnS, and others (represented as core / shell).

[0116] The emitting NS for use in the embodiments described herein has a size of less than about 100 nm, can be reduced to a size of less than about 1 nm, and can absorb visible light. When used herein, visible light is electromagnetic radiation with wavelengths between about 380 and about 780 nanometers that are visible to the human eye. Visible light can be separated into a spectrum of various colors: red, orange, yellow, green, blue, indigo, and violet. Blue light can include light between about 435 nm and 495 nm, green light can include light between about 495 nm and 570 nm, and red light can include light between about 620 nm and 750 nm.

[0117] According to various embodiments, the light-emitting NSs can have a size and composition such that they absorb photons in the ultraviolet, near-infrared, and / or infrared spectra. The ultraviolet spectrum can include light between wavelengths of about 100 nm and about 400 nm, the near-infrared spectrum can include light between wavelengths of about 750 nm and about 100 μm, and the infrared spectrum can include light between wavelengths of about 750 nm and about 300 μm.

[0118] While other suitable materials can be used as luminescent NS in various embodiments described herein, in some embodiments the NS may be ZnSe, ZnTe, ZnS, InAs, InP, CdSe, or any combination thereof to form a collection of nanocrystals for use in the embodiments described herein. As discussed above, in further embodiments the luminescent NS may be core / shell nanocrystals, e.g., CdSe / ZnS, InP / ZnSe, CdSe / CdS, or InP / ZnS.

[0119] A suitable luminescent nanostructure, and a method for preparing luminescent nanostructures, including the addition of ligands to enhance various solubility, can be found in published U.S. Patent Publication No. 2012 / 0113672, the disclosure of which is incorporated herein by reference in whole.

[0120] While several embodiments are described and presented herein, it should be understood that the claims are not limited to the specific form or arrangement of the described and shown parts. Embodiments are disclosed herein for illustrative purposes, and specific terminology is used, but these are used only in a general and descriptive sense and not for limiting purposes. Modifications and variations of the embodiments are possible in light of the above teachings. Therefore, it should be understood that embodiments may be carried out in ways other than those described.

Claims

1. 1. An electroluminescent device comprising: A substrate; A first electrode; a first transport layer; a light emitting layer comprising light emitting nanostructures disposed directly on the first transport layer; a second transport layer comprising an organic layer; a second electrode; the electroluminescent device, wherein in the region where the first transport layer, the light-emitting layer, and the second transport layer are stacked, a first portion of the organic layer is disposed on the light-emitting layer and a second portion of the organic layer is disposed directly on the first transport layer.

2. 2. The electroluminescent device of claim 1, wherein the second portion of the organic layer is disposed in a gap between the first transport layer and the light-emitting nanostructure, and a surface of the light-emitting nanostructure is covered by the organic layer.

3. An electroluminescent device as described in claim 1 or 2, wherein in the light-emitting layer, the light-emitting nanostructure is in direct contact with the first transport layer.

4. An electroluminescent device as claimed in claim 1, wherein the composition of the first portion of the organic layer is the same as the composition of the second portion of the organic layer.

5. An electroluminescent device as claimed in any one of claims 1 to 4, wherein the first transport layer does not include the light-emitting nanostructure.

6. An electroluminescent device described in any one of claims 1 to 5, wherein in a region where the first transport layer, the light-emitting layer, and the second transport layer are stacked, the area of ​​direct contact between the first transport layer and the second transport layer is larger than the area of ​​direct contact between the first transport layer and the light-emitting layer.

7. The electroluminescent device according to any one of claims 1 to 6, wherein the organic material of the organic layer is soluble in a polar organic solvent.

8. The electroluminescent device according to any one of claims 1 to 7, wherein the organic material of the organic layer is soluble in alcohol, acetone, or acetonitrile.

9. 9. The electroluminescent device of claim 1, wherein the organic layer comprises an organic material having two or more phosphonic acid oxide functional groups (P=O).

10. 10. The electroluminescent device of claim 1, wherein the organic layer comprises (1,3,5-triazine-2,4,6-triyl)tris(benzene-3,1-diyl)tris(diphenylphosphine oxide) or 2,4,6-tris[3-(diphenylphosphinyl)phenyl]-1,3,5-triazine.

11. 11. The electroluminescent device according to any one of claims 1 to 10, wherein a turn-on voltage of said electroluminescent device is in the range between 0.7V and 1V.

12. The electroluminescent device of any one of claims 1 to 11, wherein the light emitting nanostructures comprise indium phosphide (InP).

13. 13. The electroluminescent device of any one of claims 1 to 12, wherein the light emitting nanostructures comprise quantum dots configured to emit light in the visible spectrum.

14. 14. The electroluminescent device of claim 1, wherein the luminescent nanostructure comprises a first population of quantum dots configured to emit red light and a second population of quantum dots configured to emit green light.

15. The electroluminescent device of any one of claims 1 to 14, wherein the first transport layer is a hole transport layer and the second transport layer is an electron transport layer.

16. The electroluminescent device of claim 15, further comprising a hole injection layer between the first electrode and the hole transport layer, and further comprising an electron injection layer between the electron transport layer and the second electrode.

17. The electroluminescent device of any preceding claim, wherein the organic layer is free of inorganic materials.

18. 1. A method of manufacturing an electroluminescent device, the method comprising: providing a layer of an anode material; forming a hole transport layer; forming a layer of quantum dots directly on the hole transport layer; forming an electron transport layer comprising an organic layer using a solution process; forming a cathode; In a region where the hole transport layer, the quantum dot layer, and the electron transport layer are stacked, a first portion of the organic layer is disposed on the quantum dot layer and a second portion of the organic layer is disposed directly on the hole transport layer.

19. 1. A display device, comprising: an array of pixels; a display screen disposed over said array of pixels; each pixel of the array of pixels includes first and second electroluminescent devices; Each of the first and second electroluminescent devices a hole transport layer; a light emitting layer comprising light emitting nanostructures disposed directly on the hole transport layer; an electron transport layer comprising an organic layer; In a region where the hole transport layer, the light emitting layer, and the electron transport layer are stacked, a first portion of the organic layer is disposed on the light emitting layer, and a second portion of the organic layer is disposed directly on the hole transport layer; the light emitting layer of the first electroluminescent device is configured to emit a first light having a first peak wavelength; The display apparatus, wherein the light emitting layer of the second electroluminescent device is configured to emit second light having a second peak wavelength different from the first peak wavelength.