Operation device, detection system, molding device, operation method, detection method, molding method, operation program, detection program and molding program
Patent Information
- Application Number
- JP2024008901
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-01-24
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2038-06-13
AI Technical Summary
Conventional three-dimensional object manufacturing apparatuses face defects in the manufactured objects due to issues like poor melting, oxidation, and difficulty in repairing defects, especially within the interior of the structure.
A modeling device that includes a detection unit to determine the state of a melted portion of a powder material layer, adjusting modeling conditions based on state information to prevent defects, and a calculation method to change conditions in real-time or for subsequent layers to ensure proper melting and solidification.
The solution effectively prevents defects by maintaining optimal power and energy densities, controlling temperature distribution, and minimizing spatter and fume generation, resulting in high-quality three-dimensional objects with improved structural integrity.
Abstract
Description
[Technical field]
[0001] The present invention relates to a calculation device, a detection system, a modeling device, a calculation method, a detection method, a modeling method, a calculation program, a detection program, and a modeling program. [Background technology]
[0002] Conventionally, there has been known a three-dimensional object manufacturing device that manufactures a three-dimensional object by stacking layers of powdered substances solidified by the action of light or the like (for example, Patent Document 1). However, there is a risk of defects occurring in the manufactured object. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] U.S. Pat. No. 540,758 Summary of the Invention
[0004] According to a first aspect, a calculation device used in a modeling device that creates a three-dimensional object from a solidified layer formed by heating a powder material by irradiating it with energy rays includes a detection unit that determines the state of at least a portion of a specified area including a molten portion in which the powder material is melted by heating by irradiating it with energy rays, and an output unit that outputs state information based on the state determined by the detection unit in order to change the modeling conditions of the modeling device. According to a second aspect, there is provided a calculation method used in a modeling device that forms a three-dimensional object from a solidified layer formed by heating a powder material by irradiating it with energy rays, the method determining the state of at least a portion of a specified area including a molten portion in which the powder material is melted by heating by irradiating it with energy rays, and outputting state information based on the determined state in order to change the modeling conditions of the modeling device. [Brief description of the drawings]
[0005] [Figure 1]FIG. 1 is a block diagram illustrating a schematic configuration of a molding apparatus according to a first embodiment. [Diagram 2] 3A and 3B are diagrams illustrating an example of a specific configuration and arrangement of a modeling optical unit of the modeling apparatus. [Diagram 3] 13A and 13B are diagrams illustrating an example of a specific configuration and arrangement of a shaping optical unit in a modified example. [Figure 4] 1 is a diagram showing a schematic diagram of a molten pool on a material layer and its surroundings caused by irradiation with laser light; FIG. [Diagram 5] 10A and 10B are diagrams illustrating an example of a temperature image corresponding to generated temperature image data. [Figure 6] 11A to 11C are diagrams illustrating a process of determining sputtering from generated temperature image data. [Figure 7] 11A to 11C are diagrams illustrating a process of determining fumes from generated temperature image data. [Figure 8] 13 is a diagram for explaining the relationship between the modeling conditions, the basic conditions of power density, energy density, and temperature distribution, and parameters related to the basic conditions. FIG. [Figure 9] 13 is a diagram for explaining the relationship between the modeling conditions, the basic conditions of power density, energy density, and temperature distribution, and parameters related to the basic conditions. FIG. [Figure 10] 13 is a flowchart illustrating a process when a real-time change is performed. [Figure 11] 13 is a flowchart illustrating a process when a real-time change is performed. [Figure 12] 13 is a flowchart illustrating a process when a real-time change is performed. [Figure 13] 13 is a flowchart illustrating a process in the case where a change is made during formation of the next layer. [Figure 14] 13 is a flowchart illustrating a process in the case where a change is made during formation of the next layer. [Figure 15] 13 is a flowchart illustrating a process in the case where a change is made during formation of the next layer. [Figure 16]13 is a flowchart illustrating a process in the case where a change is made during formation of the next layer. [Figure 17] FIG. 11 is a block diagram illustrating a schematic configuration of a main part of a molding apparatus in a second modification of the first embodiment. [Figure 18] FIG. 13 is a block diagram illustrating a schematic configuration of a main part of a modeling apparatus and a detection system in a third modification of the first embodiment. [Figure 19] FIG. 11 is a block diagram illustrating a schematic configuration of a molding apparatus according to a second embodiment. [Figure 20] 13 is a diagram illustrating an example of a specific configuration and arrangement of a modeling optical unit included in a modeling apparatus according to a second embodiment. FIG. [Figure 21] 13 is a flowchart illustrating a process performed by a molding apparatus according to a second embodiment. [Figure 22] 13 is a flowchart illustrating a process performed by a molding apparatus according to a second embodiment. [Diagram 23] 13 is a flowchart illustrating a process performed by a molding apparatus according to a second embodiment. [Figure 24] 1 is a diagram showing a schematic cross-sectional shape in the ZX plane formed by a predetermined amount of powder material that is the subject of pre-detection. FIG. [Diagram 25] 13 is a flowchart illustrating a process performed by a molding apparatus according to a second embodiment. [Figure 26] FIG. 13 is a block diagram illustrating a schematic configuration of a main part of a molding apparatus according to a modified example of the second embodiment. [Figure 27] FIG. 13 is a block diagram illustrating a schematic configuration of a main part of a modeling apparatus and a detection system in a modified example of the second embodiment. [Figure 28] FIG. 13 is a block diagram illustrating a schematic configuration of a molding apparatus according to a third embodiment. [Figure 29] 13A to 13C are diagrams illustrating an example of a specific configuration and arrangement of a modeling optical unit included in a modeling apparatus according to a third embodiment. [Diagram 30] 13 is a flowchart illustrating a process performed by a molding apparatus according to a third embodiment. [Diagram 31] FIG. 13 is a block diagram illustrating a schematic configuration of a main part of a molding apparatus according to a modified example of the third embodiment. [Diagram 32] FIG. 13 is a block diagram illustrating a schematic configuration of a main part of a modeling apparatus and a detection system in a modified example of the third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0006] -First embodiment- A modeling apparatus according to a first embodiment will be described with reference to the drawings. In the following description, a modeling apparatus that models a three-dimensional object (three-dimensional model) using a known powder bed fusion method (PBF) will be described as an example. Powder bed fusion method (PBF) is also called selective laser sintering (SLS). The modeling apparatus is not limited to powder bed fusion method (PBF), and may be an apparatus that models a three-dimensional object using other methods such as directed energy deposition modeling (DED), material jetting, electron beam melting (EBM), and fused deposition modeling (FDM). First, the configuration of the modeling apparatus 1 will be described with reference to Fig. 1 and Fig. 2. Fig. 1 is a block diagram that shows a schematic structure of the modeling apparatus 1, and Fig. 2 is a diagram that shows a schematic example of a specific configuration and arrangement of a modeling optical unit 35 of the modeling apparatus 1. For the purpose of easy understanding, the following description will be given using an orthogonal coordinate system consisting of an X-axis, a Y-axis, and a Z-axis as shown in Figs. 1 and 2.
[0007] The modeling apparatus 1 includes a housing 10, a material layer forming unit 20, a modeling unit 30, and a computing device 50. The material layer forming unit 20 includes a material supply tank 21 and a recoater 22. The modeling unit 30 includes a modeling tank 31 and a modeling optical unit 35. For ease of explanation, the material layer forming unit 20 and the modeling unit 30 are shown as separate components, but the material layer forming unit 20 and the modeling unit 30 can also be collectively referred to as the modeling unit.
[0008] The material supply tank 21 is a container for containing powder material P, which is a material for forming a three-dimensional object. A bottom surface 211 of the material supply tank 21 moves in the vertical direction (Z direction) by a drive mechanism 212 constituted by, for example, a piston or the like. When the bottom surface 211 of the material supply tank 21 moves toward the + side (upward) in the Z direction, the powder material P inside the material supply tank 21 is pushed out to the outside according to the amount of rise of the bottom surface 211, and this pushed-out powder material P is transferred to a forming tank 31, which will be described later, by a recoater 22, which will be described later.
[0009] The material supply tank 21 is provided with a heater 213 for heating the powder material P contained therein. The heater 213 heats the powder material P to a desired temperature under the control of a calculation device 50 described later. A heater of an existing heating method is used as the heater 213. Note that a temperature control element such as a Peltier element may be used as the heater 213. The heater 213 heats the powder material P in the material supply tank 21, thereby increasing the temperature of the powder material P in advance before the powder material P is transferred to the modeling tank 31 and heated by irradiation with a laser beam described later. This reduces the amount of heat required to raise the temperature of the powder material P heated by irradiation with a laser beam to a desired temperature (for example, a melting point). In addition, the heater 213 heats the powder material P, which has high moisture absorption and low fluidity, thereby reducing the moisture absorption of the powder material P and increasing its fluidity. This makes it easier for the powder material P to be transferred to the modeling tank 31, and the flatness, layer thickness, and density of the material layer formed as described in detail later become uniform. As a result, when the material layer is irradiated with laser light as described in detail below, the temperature rise within the material layer due to the irradiation with the laser light becomes uniform. Note that the material supply tank 21 is not limited to one that pushes the powder material P outward from the lower portion in the Z direction by the drive mechanism 212. The powder material P contained in the material supply tank 21 may be supplied to a dispenser provided below (negative side in the Z direction) the material supply tank 21, the powder material P supplied to the dispenser may fall onto the base plate 311 of the modeling tank 31 from a discharge portion provided below (negative side in the Z direction) the dispenser, and the fallen powder material P may be spread to a uniform thickness by the movement of a blade 221 of a recoater 22 described later.
[0010] As the powder material P, for example, a metal powder, a resin powder, a powder in which metal particles are coated with a resin binder, etc. are used. The metal powder may be a powder mainly composed of an iron-based powder, or a powder containing at least one of nickel powder, nickel-based synthetic powder, copper powder, copper-based alloy powder, and graphite-based powder in addition to the iron-based powder. For example, the powder may be one in which the amount of iron-based powder having an average particle size of about 20 μm is 60 to 90% by weight, the amount of both or either of nickel powder and nickel-based alloy powder is 5 to 35% by weight, the amount of both or either of copper powder and copper-based alloy powder is 5 to 15% by weight, and the amount of graphite powder is 0.2 to 0.8% by weight. As the resin powder, for example, a powder of polyamide, polypropylene, ABS, etc. having an average particle size of about 30 μm to 100 μm can be used. As the powder in which metal particles are coated with a resin binder, for example, a powder in which the surface of metal particles is coated with an additive such as phenol resin or nylon can be used. In addition, a ceramic powder may be used as the powder material P. The ceramic powder may be a powder of an oxide such as alumina or zirconia, or a powder of a nitride such as silicon nitride. The powder material P may be a material other than the above. For example, the powder material P may be an existing metal powder, an existing resin powder, or an existing ceramic powder, or may be a powder material that combines at least two materials, an existing metal, an existing resin, and an existing ceramic. In the following, a case where metal powder is used as the powder material P will be described as an example.
[0011] The recoater 22 has a blade 221 as a material layer forming member, a driving mechanism (not shown), and a blade mounting part (not shown). The blade 221 is, for example, a plate-like member extending along the Y direction. The blade 221 is attached to the blade mounting part so as to be replaceable among a plurality of types having different materials and shapes. The driving mechanism has, for example, a driving mechanism such as a motor or a guide rail extending along the X direction, and moves the blade mounting part along the X direction to move the blade 221 along the X direction between position A (the negative end of the material supply tank 21 in the X direction) and position B (the positive end of the modeling tank 31 in the X direction) in FIG. 1. By moving the blade 221 in this way, the powder material P contained in the material supply tank 21 (more specifically, the powder material P pushed out of the material supply tank 21 according to the amount of rise of the bottom surface 211 of the material supply tank 21 toward the positive side (upward) in the Z direction) is transferred to the modeling tank 31 of the modeling unit 30 described later. At this time, the blade 221 moves while applying pressure to the powder material P so as to press it downward (negative side in the Z direction). This movement of the blade 221 causes the powder material P to be spread in the modeling tank 31 with a constant thickness Δd, forming a layer of powder material (hereinafter referred to as material layer) called a powder bed with a flat surface (surface on the positive side in the Z direction). In other words, the blade 221 functions as a material layer forming member. The blade 221 can apply pressure to the powder material P by a pressing mechanism (not shown) composed of a cylinder or the like.
[0012] When the blade 221 transfers the powder material P to the upper part of the solidified layer formed as described later, after a predetermined time has elapsed since the solidified layer was formed by irradiating the previously formed material layer with a laser beam, the blade 221 again moves from the position A along the X direction to transfer the powder material P to the upper part of the solidified layer. In this specification, this predetermined time is called the waiting time of the blade 221. Note that the above-mentioned certain thickness Δd is the thickness from the surface of the base plate 311 to the surface of the material layer (the surface on the +Z direction side) when the powder material P is transferred onto the base plate 311 described later, and is the thickness from the surface of the upper part of the solidified layer (the surface on the +Z direction side) to the surface of the material layer formed on the upper part of the solidified layer (the surface on the +Z direction side) when the powder material P is transferred to the upper part of the solidified layer (the surface on the +Z direction side) formed as described later. The moving speed of the blade 221, the pressure applied to the powder material by the blade 221, and the waiting time of the blade 221 are variably controlled by the computing device 50. The formation of the material layer will be described in detail later. In this embodiment, the plate-shaped blade 221 is used as an example of the material layer forming member, but the material layer forming member may be a roller or other member that can be used to form a material layer. For example, when a roller is used as the material layer forming member, the roller is attached so that its rotation axis is along the Y-axis direction, and moves while rotating when moved along the X-direction by the driving mechanism. In this way, the roller applies pressure to the powder material P and spreads the powder material P to a certain thickness Δd in the modeling tank 31.
[0013] The modeling tank 31 of the modeling unit 30 is a container for modeling work for forming a three-dimensional object by repeatedly forming a material layer and forming a solidified layer by solidifying the formed material layer, and stacking a plurality of solidified layers along the Z direction. In the present embodiment, the solidified layer is a layer formed by heating the powder material P forming the material layer by irradiation with a laser beam, melting the powder material P by heating, and solidifying the powder material P to form the layer, as described later. The base plate 311, which is the bottom surface of the modeling tank 31, is a support member that supports the formed material layer and the solidified layer from the negative side in the Z direction. The base plate 311 moves in the vertical direction (Z direction) by a drive mechanism 312 such as a motor included in the modeling tank 31. As described later in detail, when the material layer formed by the powder material P supplied on the base plate 311 is heated by irradiation with a laser beam to form the solidified layer, the base plate 311 moves downward (negative side in the Z direction), and then a new material layer is formed on the upper surface (positive side in the Z direction) of the solidified layer. This new material layer is solidified to form a new solidified layer. The base plate 311 is attached to the modeling tank 31 so as to be interchangeable between a plurality of types of plates having different materials and thicknesses in the Z direction. In other words, the base plate 311 is attached to the modeling tank 31 so as to be interchangeable between a plurality of types of plates having different rigidities.
[0014] The base plate 311 is provided with a heater 313 for heating the base plate 311. The heater 313 heats (preheats) the material layer and the solidified layer supported by the base plate 311 to a desired temperature under the control of the calculation device 50 described later. A heater of an existing heating method is used as the heater 313. Note that a temperature control element such as a Peltier element may be used as the heater 313. This heater 313 heats (preheats) the material layer and the solidified layer in the modeling tank 31. The heater 313 preheats the powder material P to increase its temperature before the powder material P constituting the material layer is heated by irradiation with a laser beam. This reduces the amount of heat required for the temperature of the powder material P heated by irradiation with a laser beam to rise to a desired temperature (for example, the melting point). In addition, the heater 313 heats the modeled solidified layer. This suppresses the occurrence of residual stress when the solidified layer is cooled, and relieves residual stress that has occurred in the solidified layer.
[0015] The modeling optical unit 35 of the modeling unit 30 includes an acquisition unit 310, an irradiation unit 32, a scanning unit 33, and a focus lens 323. The acquisition unit 310 includes an imaging device 41, a bifurcated optical system 42, a chromatic aberration correction optical system 43, a half mirror 301, and a field stop 302, which will be described in detail later. The acquisition unit 310 acquires information on at least a part of a predetermined region including a melted portion where the powder material P is melted (a melted portion where the powder material P is melted, an unmelted powder material P (material layer) that has not yet melted, a region that has solidified after melting, etc.) (details will be described later). Note that the half mirror 301 may not be included in the acquisition unit 310 depending on the arrangement of each component of the modeling optical unit 35, which will be described in detail later.
[0016] Here, since the acquisition unit 310 is configured integrally with the irradiation unit 32 and the scanning unit 33, for convenience of explanation, it will be described as a part of the modeling optical unit 35 (i.e., a part of the modeling unit 30). However, since the acquisition unit 310 has a function (a function of acquiring information on at least a part of a predetermined area including a molten part where the powder material P is melted, which will be described later) different from the configuration of the modeling unit 30 other than the acquisition unit 310 (i.e., the modeling tank 31, the irradiation unit 32, the focus lens 323, and the scanning unit 33), it can also be represented as a configuration separate from the modeling unit 30. In this case, the modeling unit 30 has a modeling optical unit 35 having the irradiation unit 32, the scanning unit 33, and the focus lens 323, and the modeling tank 31. In this case, the half mirror 301 is also a part of the modeling optical unit 35, so it can also be represented as a configuration of the modeling optical unit 35 rather than the acquisition unit 310.
[0017] The irradiation unit 32 includes, for example, a laser oscillator 321 that emits laser light as irradiation light for irradiating and heating the material layer, and a collimator lens 322 that collimates the laser light emitted from the laser oscillator 321 into parallel light (see FIG. 2). As the laser oscillator 321, for example, a carbon dioxide laser, a Nd:YAG laser, a fiber laser, or the like can be used. The laser oscillator 321 includes, for example, a resonator mirror and the like, an amplifier filled with a laser medium, and an excitation light source. The light emitted from the laser medium excited by the light from the excitation light source oscillates through repeated reflections in the amplifier and is emitted from the laser oscillator as a laser beam. The laser oscillator 321 has, as an oscillation mode (oscillation form) of the laser beam, a CW (continuous wave) oscillation in which the excitation light source is continuously turned on, a normal pulse oscillation in which the excitation light source is turned on in a pulsed manner and the output waveform of the laser beam is controlled by electrically controlling the excitation light source's on time width and current value, and a Q-switch pulse oscillation in which a laser beam with a narrow pulse width and high peak output is emitted in a short time. The laser oscillator 321 emits, for example, a laser beam with a wavelength of 1070 nm. The laser oscillator 321 may emit light of other wavelengths, for example, infrared light greater than 800 nm, visible light in the range of 400 nm to 800 nm, or ultraviolet light shorter than 400 nm. The specific configuration of the irradiation unit 32 will be described later. The irradiation unit 32, under the control of the computing device 50, switches the intensity distribution of the laser light from the laser oscillator 321 between a Gaussian distribution, a top hat distribution, or the like, by using a known deformable mirror or the like, and emits the laser light. The irradiation unit 32 may irradiate the material layer with an existing light emitting diode (LED) or an existing particle beam such as an electron beam, a proton beam, or a neutron beam instead of a laser beam to heat the powder material P. In this embodiment, the irradiation unit 32 is one capable of emitting energy beams including an existing laser beam, an existing light emitting diode, an existing particle beam, or the like.
[0018] The scanning unit 33 is configured with a galvanometer mirror, and scans the laser light emitted from the irradiation unit 32 on the material layer along at least one of the X direction and the Y direction. The specific configuration of the scanning unit 33 will be described later.
[0019] The imaging device 41 captures an image of the molten portion of the material layer irradiated with the laser light from the irradiation unit 32 and a predetermined area in the vicinity thereof, and generates image data of the image of the predetermined area including the molten portion of the material layer and its vicinity. The generated image data is the signal intensity of each pixel obtained by photoelectrically converting light from the predetermined area including the molten portion of the material layer and its vicinity by an imaging element 411 described later. The generated image data is output to a calculation device 50 described later. The specific configuration of the imaging device 41 will be described later. As described above, the shaping optical unit 35 partially shares the configuration for irradiating the material layer with laser light and the configuration for capturing an image of the material layer, and therefore can also be called an imaging optical system.
[0020] The housing 10 accommodates the material supply tank 21, the recoater 22, and the modeling tank 31 in which the solidified layer is accommodated. Note that a part of the driving mechanism 212 that moves the bottom surface 211 of the material supply tank 21 and a part of the driving mechanism 312 that moves the base plate 311 of the modeling tank 31 may not be accommodated inside the housing 10. The housing 10 is formed with an intake port 11 and an exhaust port 12. A tank 13 filled with an inert gas such as argon or nitrogen is connected to the intake port 11 via an intake device 131 such as a valve. An exhaust device 14 equipped with a vacuum pump or the like is connected to the exhaust port 12. The exhaust device 14 and the intake device 131 controlled by the computing device 50 exhaust the inside of the housing 10 so that a set pressure inside the housing 10 is obtained. The intake device 131 also reduces the oxygen concentration inside the housing 10 by introducing the inert gas filled in the tank 13 into the inside of the housing 10. Since the oxygen concentration in the housing 10 is reduced, oxidation of the powder material P is prevented. The flow rate and flow speed of the inert gas introduced into the housing 10 are controlled by the valve opening of the intake device 131 and the exhaust volume of the exhaust device 14. The housing 10 is provided with a heater 15 for heating the inside, and is controlled by a computing device 50 described later to heat the inside of the housing 10 to a desired temperature. The heater 15 is a heater of an existing heating method. Note that a temperature control element such as a Peltier element may be used as the heater 15. This heater 15 heats the inside of the housing 10, thereby heating the material layer and the solidified layer in the modeling tank 31. The heater 15 increases the temperature of the powder material P before the powder material P constituting the material layer is heated by irradiation with a laser beam. As a result, the temperature of the powder material P irradiated with the laser beam increases to a desired temperature (for example, the melting point), and the required amount of heat is reduced.
[0021] In this manner, the atmosphere inside the housing 10, including the oxygen concentration inside the housing 10, the flow rate and flow speed of the inert gas, the type of inert gas, the pressure inside the housing 10, and the temperature inside the housing 10, is controlled. In addition, at least a portion of the upper surface (Z direction + side) of the housing 10 is made of a light-transmitting material such as glass to transmit the laser light from the irradiation unit 32. This portion of the region is, for example, a region that intersects with the optical path of the laser light directed from the scanning unit 33 toward the material layer.
[0022] Here, an example of a specific configuration and arrangement of the shaping optical unit 35 will be described with reference to FIG. 2, the laser light emitted from the laser oscillator 321 of the irradiation unit 32 toward the negative side in the Z direction is reflected by the half mirror 301 toward the positive side in the X direction, passes through the focus lens 323, and enters the scanning unit 33. The emission direction of the laser light from the irradiation unit 32 is not limited to the negative side in the Z direction, and the direction in which the half mirror 301 reflects the laser light is not limited to the positive side in the X direction. The emission direction of the laser light and the reflection direction of the half mirror 301 are appropriately determined to be preferable directions based on the relationship between the position where the irradiation unit 32 is disposed and the position of the material layer and / or the position where other components of the modeling optical unit 35 are disposed.
[0023] The focus lens 323 has a concave lens 323a and a convex lens 323b. In order to adjust the focal position (focal length) of the laser light reflected by the galvanometer mirrors 331 and 332 described later, the concave lens 323a is configured to be movable along the X direction by a driving mechanism (not shown) under the control of the calculation device 50. Therefore, the beam diameter (spot size) of the laser light on the material layer can be adjusted according to the position of the concave lens 323a in the X direction. In this case, the distance traveled by the laser light to reach the surface of the material layer varies due to the driving of the galvanometer mirrors 331 and 332 described later (i.e., the change in the angle of the galvanometer mirrors 331 and 332). Therefore, the focus lens 323 can adjust the focal position of the laser light according to the driving of the galvanometer mirrors 331 and 332 so that the focal point of the laser light reflected by the galvanometer mirrors 331 and 332 coincides with the surface of the material layer.
[0024] In addition, the focal position of the laser light does not necessarily need to be adjusted so that the focal point of the laser light coincides with the surface of the material layer with the driving of the galvanometer mirrors 331 and 332. For example, the position of the concave lens 323a may be controlled by a driving mechanism (not shown) controlled by the arithmetic device 50 in response to the driving of the galvanometer mirrors 331 and 332 (change in the angle of the galvanometer mirrors 331 and 332) so as to change the beam diameter (spot size) of the laser light for each irradiation position of the laser light on the material layer. Note that the concave lens 323a does not need to be configured to be movable, and the convex lens 323b may be configured to be movable in the X direction by a driving mechanism (not shown), or both the concave lens 323a and the convex lens 323b may be configured to be movable in the X direction by a driving mechanism (not shown). In addition, the focus lens 323 does not need to be a so-called Galilean type including the concave lens 323a and the convex lens 323b, and other existing optical systems may be adopted. Note that the concave lens 323a and the convex lens 323b of the focus lens 323 are not limited to being configured to be movable in the X direction. The movement directions of the concave lens 323a and the convex lens 323b are appropriately determined to be preferable directions based on the relationship between the position where the focus lens 323 is arranged and the positions where other components of the shaping optical unit 35 are arranged.
[0025] The scanning unit 33 has galvanometer mirrors 331 and 332. The galvanometer mirror 331 is disposed at a predetermined angle with respect to the Z axis. The angle of inclination of the galvanometer mirror 331 with respect to the Z axis is changed under the control of the computing device 50. The galvanometer mirror 331 reflects the laser light traveling in the + direction in the X direction from the focus lens 323 toward the galvanometer mirror 332 provided on the + side in the Z direction relative to the galvanometer mirror 331.
[0026] The galvanometer mirror 332 is disposed in a state inclined at a predetermined angle with respect to the XY plane. The inclination angle of the galvanometer mirror 332 with respect to the XY plane is changed under the control of the computing device 50. The laser light reflected by the galvanometer mirror 331 is reflected by the galvanometer mirror 332 and guided to the surface of the material layer. By changing the inclination angle of the galvanometer mirror 331 with respect to the Z axis and the inclination angle of the galvanometer mirror 332 with respect to the XY plane, the position on the material layer irradiated with the laser light moves along at least one of the X axis and the Y axis. This allows the position on the material layer irradiated with the laser light to move, i.e., scan, on the XY plane. The arrangement of the galvanometer mirrors 331 and 332 and the reflection direction of the laser light by the galvanometer mirror 331 are not limited to the above-mentioned arrangement and reflection direction. Based on the relationship between the position where the scanning unit 33 is disposed and the position where other components of the modeling optical unit 35 are disposed, the arrangement of the galvanometer mirrors 331 and 332 and the reflection direction of the laser light by the galvanometer mirror 331 are appropriately determined to be a preferable arrangement and reflection direction.
[0027] When the amount of scanning angle set by the galvanometer mirrors 331 and 332 increases, the scanning distance of the laser light increases. The scanning distance is the distance that the position on the material layer irradiated with the laser light (irradiation position) moves when the position moves on the XY plane. Furthermore, when the speed at which the tilt angle of the galvanometer mirrors 331 and 332 is changed increases, the scanning speed of the laser light increases. The scanning speed is the speed at which the irradiation position on the material layer moves on the XY plane. That is, the calculation device 50 controls the amount of scanning angle and the change speed of the galvanometer mirrors 331 and 332 to control the scanning distance and scanning speed of the laser light. The tilt angle of the galvanometer mirrors 331 and 332 determines the irradiation position of the laser light on the surface of the material layer. When an image is captured by the imaging device 41 described later, the generated image data is stored in the storage unit 58 in association with irradiation position information and time information. The irradiation position information is information indicating the irradiation position of the laser light. As described above, the irradiation position of the laser light moves depending on the tilt angle of the galvanometer mirrors 331 and 332, so the irradiation position of the laser light on the material layer is calculated based on the tilt angle of the galvanometer mirrors 331 and 332 detected by an encoder or the like. The irradiation position information associated with the image data may be the tilt angle of the galvanometer mirrors 331 and 332. The time information is time information indicating the timing at which the image is captured by the imaging device 41 based on the start of the laser light irradiation.
[0028] The scanning unit 33 is not limited to being configured by the galvanometer mirrors 331 and 332 described above. For example, the scanning unit 33 may be configured by a driving mechanism that moves the base plate 311 of the modeling tank 31 along at least one of the X direction and the Y direction. In this case, the driving mechanism is configured by a motor, a guide rail extending in the X direction, a guide rail extending in the Y direction, and the like, and moves the base plate 311 on the XY plane. As a result, the relative positional relationship between the irradiation position of the laser light and the material layer on the XY plane is changed, and the laser light is scanned on the material layer. In this case, the laser light may be scanned by moving the irradiation position of the laser light on the XY plane by the galvanometer mirrors 331 and 332 described above and moving the material layer on the XY plane by moving the base plate 311. Alternatively, the tilt angle of the galvanometer mirrors 331 and 332 described above may be fixed, and the laser light may be scanned by only moving the material layer on the XY plane by moving the base plate 311. The configuration for changing the relative positional relationship between the laser light and the base plate 311 (that is, the material layer) on the XY plane is not limited to the above-mentioned configuration, and other existing configurations may also be applied.
[0029] Light (hereinafter, for convenience of explanation, referred to as thermal radiation light) from at least a part of a predetermined region including a molten part where the powder material P is molten (a molten part where the powder material P is molten, an unmelted powder material P (material layer) that has not yet melted, a region that has solidified after melting, etc.) on the material layer travels in the opposite direction along an optical path coaxial with the laser light. That is, the thermal radiation light travels from the surface of the material layer toward the + side of the Z direction, is reflected by the galvanometer mirror 332 toward the galvanometer mirror 331, and is reflected by the galvanometer mirror 331 toward the - side of the X direction. The light from the predetermined region traveling toward the - side of the X direction enters the focus lens 323, passes through the convex lens 323b and the concave lens 323a, and becomes a parallel light beam. The thermal radiation light that has passed through the focus lens 323 passes through the half mirror 301, travels toward the - side of the X direction, and enters the chromatic aberration correction optical system 43. Note that the optical member that reflects the laser light and transmits the thermal radiation light does not have to be a half mirror. For example, an existing optical member such as a dichroic mirror may be used.
[0030] The chromatic aberration correction optical system 43 corrects axial chromatic aberration, chromatic aberration of magnification, and the like that occurs in the thermal radiation light as a result of passing through the focus lens 323. The chromatic aberration correction optical system 43 includes a first lens 431, a second lens 432, and a third lens 433, which are arranged in this order from the + side in the X direction. The first lens 431 and the second lens 432 are cemented lenses that combine a convex lens and a concave lens. The first lens 431 has a positive refractive index, the second lens 432 has a negative refractive index, and the third lens has a positive refractive index. The first lens 431 and the second lens 432 cause the thermal radiation light that has passed through the half mirror 301 and entered it to enter the third lens 433 on the - side in the X direction in the form of a parallel light beam, and the third lens 433 condenses the parallel light beam to form a primary image surface. The dispersion of the first lens 431, the second lens 432, and the third lens 433 is determined so that no axial chromatic aberration or chromatic aberration of magnification occurs on this primary image surface. In this case, the dispersion of each lens is determined so that the chromatic aberration contained in the thermal radiation light transmitted through the first lens 431 and the second lens 432 is cancelled by the chromatic aberration caused by the focusing of the third lens 433. Note that the first lens 431, the second lens 432, and the third lens 433 of the chromatic aberration correction optical system 43 are not limited to being arranged along the X direction. Based on the relationship between the position where the chromatic aberration correction optical system 43 is arranged and the positions where other components of the molding optical unit 35 are arranged, the directions in which the first lens 431, the second lens 432, and the third lens 433 are arranged are appropriately determined to be preferable directions.
[0031] A field stop 302 is disposed on the primary image plane. The thermal radiation light passes through an opening provided in the field stop 302 toward the negative side in the X direction, thereby restricting the field of view of an image (image data) generated by focusing a light beam incident on an imaging device 41 described later. In this embodiment, the size of the opening of the field stop 302 is determined so that an image (image data) of a predetermined area including the irradiation position of the laser light is generated. This prevents an image outside the predetermined area on the material layer from being included in the image (image data). The thermal radiation light that has passed through the field stop 302 is incident on a bifurcated optical system 42 disposed on the negative side in the X direction of the field stop 302.
[0032] The bifurcating optical system 42 includes an objective lens 421, a beam splitter 422, beam deflectors 423 and 424, a beam combiner 425, an imaging lens 426, a first filter 427, and a second filter 428. The objective lens 421 is a collimator lens, and collimates the thermal radiation light arriving from the field stop 302 into parallel light. The beam splitter 422 is configured, for example, with a dichroic mirror or a beam splitter, and transmits a beam of a specific wavelength of the thermal radiation light and reflects a beam of a wavelength other than the specific wavelength. In this embodiment, the beam splitter 422 transmits light of wavelength λ1 of the incident thermal radiation light and guides it to the first filter 427 provided on the negative side in the X direction, and reflects light of wavelength λ2 and guides it to the beam deflector 423 provided on the positive side in the Z direction. The light beam deflection unit 423 is configured, for example, with a dichroic mirror or the like, and reflects the light with wavelength λ2 and guides it to the second filter 428 provided on the negative side in the X direction. Note that in this embodiment, the wavelength λ1 is described as being, for example, 1250 [nm] and the wavelength λ2 is described as being, for example, 1600 [nm], but the wavelengths λ1 and λ2 are not limited to the above values.
[0033] The first filter 427 is a bandpass filter that transmits light with a wavelength of λ1. The light with a wavelength of λ1 that has been transmitted through the beam splitter 422 is transmitted through the first filter 427 and enters the beam deflector 424 arranged on the negative side in the X direction. The second filter 428 is a bandpass filter that transmits light with a wavelength of λ2. The light with a wavelength of λ2 that has been reflected by the beam deflector 423 is transmitted through the second filter 428 and enters the beam combiner 425. The beam deflector 424 is formed of, for example, a dichroic mirror, and is arranged so that the reflecting surface of the beam is at a predetermined inclination angle with respect to the XY plane.
[0034] The light beam combining unit 425 is configured, for example, by a dichroic mirror or the like, and is arranged so that the reflecting surface of the light beam has a predetermined inclination angle with respect to the XY plane. The light having a wavelength of λ1 reflected by the light beam deflection unit 424 travels toward the + side of the Z direction, passes through the light beam combining unit 425, is collected by the imaging lens 426, and enters the imaging device 41. The light having a wavelength of λ2 that has entered the light beam combining unit 425 travels toward the + side of the Z direction after being reflected by the light beam combining unit 425, is collected by the imaging lens 426, and enters the imaging device 41. Here, the light beam deflection unit 424 and the light beam combining unit 425 are arranged so that the inclination angle of the reflecting surface is different from that of the reflecting surface. As a result, the light with a wavelength of λ1 from the beam deflection unit 424 and the light with a wavelength of λ2 from the beam synthesis unit 425 are incident on the imaging lens 426 at different angles and are focused at different positions on the imaging surface of the imaging element 411 of the imaging device 41 described later.
[0035] In this embodiment, the angles that the reflecting surfaces of the light beam deflector 424 and the light beam combiner 425 make with the XY plane are changeable. That is, a drive mechanism (not shown) for driving the reflecting surfaces of the light beam deflector 424 and the light beam combiner 425 is provided, and the drive mechanism drives the reflecting surfaces of the light beam deflector 424 and the light beam combiner 425 under control of the computing device 50 to change the angles that the reflecting surfaces make with the XY plane. As a result, the incident positions of the light with wavelength λ1 and the light with wavelength λ2 on the image sensor 411 are changed in real time.
[0036] The above-described reflecting surface of the light beam splitter 422 and the reflecting surface of the light beam deflector 423 may be configured to be changeable in angle with the XY plane. That is, a driving mechanism (not shown) for driving the reflecting surface of the light beam splitter 422 and the reflecting surface of the light beam deflector 423 may be provided, and the driving mechanism may drive the reflecting surface of the light beam splitter 422 and the reflecting surface of the light beam deflector 423 under the control of the arithmetic device 50 to change the angle that the reflecting surface forms with the XY plane. In addition, the embodiment is not limited to an example in which the reflecting surface of the light beam splitter 422 and the reflecting surface of the light beam deflector 423 are driven by the driving mechanism, and the reflecting surface of the light beam splitter 422 and the reflecting surface of the light beam deflector 423 may be manually adjusted by a user. This manual adjustment is performed, for example, when starting up the modeling apparatus 1 after delivery or when performing maintenance on the modeling apparatus 1. In addition, the arrangement of each component of the bifurcating optical system 42 and the reflection direction of the thermal radiation light are not limited to the above-mentioned arrangement and reflection direction. Based on the relationship between the position where the bifurcating optical system 42 is arranged and the positions where other components of the shaping optical unit 35 are arranged, the arrangement of each component of the bifurcating optical system 42 and the reflection direction of the thermal radiation light are appropriately determined to be a preferable arrangement and reflection direction.
[0037] The imaging device 41 includes an imaging element 411 configured by, for example, a CMOS, a CCD, or the like, a readout circuit that reads out an image signal photoelectrically converted by the imaging element 411, and a control circuit that controls the driving of the imaging element 411. The thermal radiation light incident on the imaging device 41 is focused on the imaging surface of the imaging element 411 by an imaging lens 426. The imaging device 41 photoelectrically converts the incident light flux, generates image data, and outputs it to the calculation device 50. As described above, the inclination angle of the reflecting surface of the beam deflector 424 and the inclination angle of the reflecting surface of the beam combiner 425 are arranged to be different from each other. Therefore, of the thermal radiation light from the predetermined region of the material layer, the light of wavelength λ1 reflected by the beam deflector 424 and the light of wavelength λ2 reflected by the beam combiner 425 are incident on the imaging lens 426 at different angles and are focused at different positions on the imaging surface of the imaging element 411. In other words, the images of the two lights of different wavelengths of the thermal radiation light from the predetermined region of the material layer appear at different positions on the same image (on the same image data).
[0038] As described above, the angles that the reflecting surfaces of the beam deflection units 422 and 423 make with the XY plane and the angles that the reflecting surfaces of the beam deflection unit 424 and the beam combining unit 425 make with the XY plane can be changed. Therefore, by the calculation device 50 controlling the angles that the reflecting surfaces of the beam deflection unit 424 and the beam combining unit 425 make with the XY plane, it becomes possible to adjust the relative positional relationship between the position where the light of wavelength λ1 of the thermal radiation light is collected on the image sensor 411 and the position where the light of wavelength λ2 is collected on the image sensor 411. As described above, when the angle between the reflecting surface of the beam splitter 422 and the reflecting surface of the beam deflector 423 can be changed, it becomes possible to adjust the positions where the light of wavelength λ1 and the light of wavelength λ2 are collected on the image sensor 411.
[0039] 2, an optical system for irradiating laser light and an optical system for capturing an image by the imaging device 41 are arranged coaxially. This simplifies the configuration of the optical system and prevents the device from becoming large. In addition, the bifurcating optical system 42 is provided, so that light of two different wavelengths λ1 and λ2 is focused at different positions on the image sensor 411. That is, images of two lights of different wavelengths of thermal radiation light from a predetermined region including a melted portion of the powder material P (a melted portion where the powder material P is melted, a powder material P (material layer) that is not yet melted, a region that has solidified after melting, etc.) appear at different positions on the same image (same image data). The detection unit 54 of the calculation device 50 described later converts the ratio of the brightness information of the images at different positions on the same image (same image data) into the temperature of a predetermined region including a melted portion of the powder material P (a melted portion where the powder material P is melted, a powder material P (material layer) that is not yet melted, a region that has solidified after melting, etc.) using a known two-color method described later. Here, the brightness information is a brightness value or a value related to brightness. In the material layer irradiated with the laser light, as described in detail below, there are regions where the powder material P is melted, regions where the powder material P is unmelted, and regions where the powder material P has solidified after melting, and therefore the phase states are different. Therefore, the light emissivity differs for each phase state within a given region of the material layer. The light emissivity also differs depending on the type of powder material P.
[0040] As will be described later in detail, fumes are generated from the area where the powder material P is melted by the irradiation of the laser light. Fumes are numerous fine particles that are generated when the powder material P becomes vapor due to heating by the irradiation of the laser light, and the vapor cools in the air and becomes solid and floats. The thermal radiation light containing two wavelengths is attenuated by scattering by the fumes. However, in the two-color method, the temperature is converted based on the ratio (for example, the ratio of brightness values) between the brightness information of the image data generated based on the light of the wavelength λ1 and the brightness information of the image data generated based on the light of the wavelength λ2, so the emissivity of a predetermined area including the melted part of the powder material P (the melted part where the powder material P is melted, the unmelted powder material P (material layer) that has not yet melted, the area solidified after melting, etc.) and the thermal radiation light containing two wavelengths are not affected by scattering by the fumes. Therefore, based on the image data generated by the imaging device 41, information on the state of the powder material P irradiated with the laser light and the temperature of the material layer are acquired without being affected by fumes, etc.
[0041] The configuration and arrangement of the shaping optical unit 35 are not limited to the example shown in FIG. For example, the acquisition unit 310 may have two imaging devices 41, one of which captures light of wavelength λ1 of the thermal radiation light, and the other of which captures light of wavelength λ2 of the thermal radiation light. The two imaging devices are arranged such that the imaging surface of the imaging element of one imaging device is parallel to the YZ plane, and the imaging surface of the imaging element of the other imaging device is parallel to the XY plane. The bifurcating optical system 42 has a beam splitter 422, a first filter 427, and a second filter 428 shown in FIG. 2. The field stop 302 shown in FIG. 2 is not provided. The third lens 433 of the chromatic aberration correction optical system 43 is arranged in front of each of the two imaging devices 41. That is, the first filter 427, the second filter 428, and the beam splitter 422 of the bifurcating optical system 42 are arranged between the second lens 432 and the third lens 433 of the chromatic aberration correction optical system 43. Of the light beams that have passed through the first lens 431 and the second lens 432 of the chromatic aberration correction optical system 43, the light of wavelength λ1 is transmitted by the light beam splitter 422, passes through the first filter 427, and travels in the negative X direction, and is focused on the imaging element of one of the imaging devices by one of the third lenses 433. The light of wavelength λ2 reflected by the light beam splitter 422 travels in the positive Z direction, passes through the second filter 428, and is focused on the imaging element of the other imaging device by the other third lens 433. This enables the respective imaging devices to generate image data for each wavelength that is different from each other.
[0042] Also, the acquisition unit 310 may use, for example, a filter capable of switching the wavelength of light to be transmitted, instead of the bifurcating optical system 42 shown in FIG. 2. This filter is disposed between the second lens 432 and the third lens 433 of the chromatic aberration correction optical system 43, and has a region (first region) that transmits light of wavelength λ1 and a region (second region) that transmits light of wavelength λ2. The first region and the second region of the filter are alternately inserted into the optical path of the thermal radiation light at a predetermined time interval. For example, a disk-shaped member (turret) is provided with a plurality of filters having different wavelength transmittances, the surface of the turret is disposed parallel to the YZ plane, and the turret is configured to be rotatable around the center of the turret by a driving mechanism (not shown). For example, if a first filter and a second filter are provided on the turret as a plurality of filters having different wavelength transmittances, when the turret is rotated by the driving mechanism, the first filter and the second filter are alternately inserted into the optical path of the thermal radiation light at a time interval according to the rotation speed. Therefore, while the first filter is inserted on the optical path, light of wavelength λ1 of the thermal radiation light is transmitted and collected by the third lens 433 on the imaging element 411 of the imaging device 41, and while the second filter is inserted on the optical path, light of wavelength λ2 is transmitted and collected by the third lens 433 on the imaging element 411. As a result, the imaging device 41 generates image data based on the light of wavelength λ1 and image data based on the light of wavelength λ2 at each time interval according to the rotation speed of the turret. Note that in this case, the field stop 302 shown in FIG. 2 is not provided. As a result, the imaging device 41 can generate image data for each different wavelength at each time interval according to the rotation speed of the turret. Alternatively, a filter for selecting each of the wavelengths λ1 and λ2 may be arranged on the image sensor 411 of the imaging device 41 in accordance with the arrangement of pixels constituting the image sensor 411. In this case, the bifurcating optical system 42 and the field stop 302 shown in Fig. 2 are not provided. This makes it possible to generate image data of the wavelengths λ1 and λ2.
[0043] 3(a), a first focus lens 324 that adjusts the focal position of the laser light on the material layer and a second focus lens 325 that adjusts the focal position of the light emitted from the material layer on the image capture element 411 may be provided. The first focus lens 324 and the second focus lens 325 have concave lenses 324a, 325a and convex lenses 324b, 325b similar to the concave lens 323a and convex lens 323b of the focus lens 323 shown in FIG. In the example shown in FIG. 3(a), the laser light from the laser oscillator 321 travels in the +Z direction, passes through the first focus lens 324, passes through the half mirror 301, and enters the scanning unit 33. The thermal radiation light enters the half mirror 301 via the scanning unit 33, is reflected by the half mirror 301, and travels in the +Z direction. The thermal radiation light passes through the second focus lens 325, passes through the chromatic aberration correction optical system 43 having the same configuration as that shown in FIG. 2, and enters the bifurcating optical system 42. Since the bifurcating optical system 42 also has the same configuration as that shown in FIG. 2, the thermal radiation light is split into two wavelengths, and each of the wavelengths is focused at different positions on the imaging element 411 of the imaging device 41.
[0044] Alternatively, the laser oscillator 321 and the first focus lens 324 may be arranged along the Z direction, and the second focus lens 325, the chromatic aberration correction optical system 43, and the bifurcating optical system 42 may be arranged along the X direction. 3(a), the acquisition unit 310 has an imaging device 41, a bifurcating optical system 42, a chromatic aberration correction optical system 43, a second focus lens 325, and a half mirror 301. With this, the acquisition unit 310 acquires information on a predetermined region including a melted portion of the powder material P (a melted portion of the powder material P, an unmelted powder material P (material layer) that has not yet melted, a region that has solidified after melting, etc.). Note that the acquisition unit 310 has a function (a function of acquiring information on at least a part of a predetermined region including a molten portion where the powder material P is melted) different from the other components of the modeling unit 30 other than the acquisition unit 310, and therefore can be represented as a component separate from the modeling unit 30 (modeling optical unit 35). In this case, the half mirror 301 is also a part of the modeling optical unit 35, and therefore can be represented as a component of the modeling optical unit 35, rather than as the acquisition unit 310.
[0045] 3(b), an fθ lens 326 may be provided between the scanning unit 33 and the material layer instead of the focus lens 323. The fθ lens 326 is a lens that focuses light with an incident angle θ at a position of an image height f×θ, where f is the focal length of the fθ lens 326. Therefore, when the scanning unit 33 scans the laser light, the focal points of the laser light whose incident angle has been changed depending on the tilt angle of the galvanometer mirrors 331 and 332 are set at different positions on the same plane (i.e., on the material layer). In this case, the laser light emitted from the irradiation unit 32 travels in the + direction of the X-axis, passes through the half mirror 301, and is irradiated onto the material layer via the scanning unit 33 and the fθ lens 326. The thermal radiation light reaches the half mirror 301 via the fθ lens 326 and the scanning unit 33, is reflected in the + direction of the Z-axis by the half mirror 301, and enters the imaging device 41 via the first lens 431 and the bifurcating optical system 42. This makes it possible to generate image data for each different wavelength, similar to the case shown in FIG.
[0046] Alternatively, the laser oscillator 321 may be disposed along the Z direction, and the first lens 431 and the bifurcating optical system 42 may be disposed along the X direction. 3(b), the acquisition unit 310 has an imaging device 41, a bifurcating optical system 42, a chromatic aberration correction optical system 43, and a half mirror 301. In this way, the acquisition unit 310 acquires information on a predetermined region including a melted portion of the powder material P (a melted portion of the powder material P, an unmelted powder material P (material layer) that has not yet melted, a region that has solidified after melting, etc.). Note that the acquisition unit 310 has a function (a function of acquiring information on at least a part of a predetermined region including a molten portion where the powder material P is melted) different from the other components of the modeling unit 30 other than the acquisition unit 310, and therefore can be represented as a component separate from the modeling unit 30 (modeling optical unit 35). In this case, the half mirror 301 is also a part of the modeling optical unit 35, and therefore can be represented as a component of the modeling optical unit 35, rather than as the acquisition unit 310.
[0047] The detection unit 54 may not use the two-color method. For example, the temperature image data may be generated based on image data of light of any one wavelength of thermal radiation light from at least a part of a predetermined region including a molten part where the powder material P is melted. In this case, the bifurcating optical system 42 of the acquisition unit 310 may be replaced with a configuration including an objective lens 421, a filter for selecting any one wavelength, and an imaging lens 426. In this case, the chromatic aberration correction optical system 43 of the acquisition unit 310 may not be required. The detection unit 54 may generate temperature image data based on image data of light of any three or more wavelengths, not just light of any one wavelength. Even in this case, it is sufficient to configure the bifurcating optical system 42 of the acquisition unit 310 to increase the number of branches of the optical path.
[0048] 1 is a processor having a microprocessor and its peripheral circuits, and controls each part of the modeling apparatus 1 by reading and executing a control program prestored in a storage unit 58 configured by a non-volatile storage medium (e.g., a flash memory, etc.). The storage unit 50 includes a setting unit 59, a detection unit 54, an output unit 55, a calculation unit 56, and a determination unit 57. The calculation unit 50 may be configured by a CPU, an ASIC, a programmable MPU, etc.
[0049] The setting unit 59 sets various conditions (modeling conditions) for the modeling device 1 to model a three-dimensional object, based on status information output from the output unit 55 (described later). The status information will be described later. The setting unit 59 includes a material control unit 51, a modeling control unit 52, and a housing control unit 53. The material control unit 51 controls the operation of the material layer forming unit 20 according to the material layer forming conditions, which are conditions for forming a material layer. The material layer forming conditions include the moving speed of the blade 221, the pressure that the blade 221 applies to the powder material P, the waiting time of the blade 221, and the material of the blade 211. The material control unit 51 also controls the operation of the material layer forming unit 20 according to the conditions related to the powder material P. The conditions related to the powder material P include the particle size and particle size distribution of the powder material P, the moisture absorption of the powder material P, and the type of the powder material P, which will be described in detail later. In this case, the material control unit 51 controls the operation of the driving mechanism 212 that drives the bottom surface 211 of the material supply tank 21 and the heating temperature by the heater 213 that heats the powder material contained in the material supply tank 21. When the change information is generated by the calculation unit 56, which will be described later, the material control unit 51 changes the operation of the material layer forming unit 20 according to the material layer forming conditions based on the contents of the change information and the conditions related to the powder material P.
[0050] The modeling control unit 52 controls the operation of the modeling unit 30. The modeling control unit 52 controls the irradiation unit 32 based on the conditions of the laser light emitted to the powder material P to heat the powder material P. The conditions of the laser light include the output of the laser light, the wavelength of the laser light, the intensity distribution of the laser light, and the light beam size (spot size) of the laser light, which will be described in detail later. The modeling control unit 52 controls the scanning unit 33 based on the scanning conditions for scanning the laser light to heat the powder material P. The scanning conditions include the scanning speed of the laser light, the interval between the irradiation positions of the laser light, and the scanning path of the laser light, which will be described in detail later. The modeling control unit 52 controls the operation of the base plate 311 based on the support unit conditions related to the base plate 311 that supports the powder material P and the solidified layer. The support unit conditions include the temperature of the base plate 311, which will be described in detail later, and the modeling control unit 52 controls the heating temperature by the heater 313 that heats the base plate 311 based on the support unit conditions. The modeling control unit 52 also controls the operation of the drive mechanism 312 that drives the base plate 311 of the modeling tank 31. The modeling control unit 52 changes the design data of the solidified layer and the three-dimensional object in accordance with the content of the change information. The design data includes slice model data and shape data of the support part, which will be described in detail later. When the change information is generated by the calculation unit 56, which will be described later, the modeling control unit 52 changes the operation of the modeling unit 30 and the design data in accordance with the content of the change information.
[0051] The housing control unit 53 controls the operation of the intake device 131 and the exhaust device 14, and the operation of the heater 15, in accordance with conditions related to the atmosphere inside the housing 10. The conditions related to the atmosphere inside the housing 10 include the flow rate and flow speed of the inert gas introduced into the housing 10, and the temperature inside the housing 10, which will be described in detail later. When change information is generated by the calculation unit 56, which will be described later, the housing control unit 53 changes the operation of the intake device 131, the exhaust device 14, and the heater 15 in accordance with the conditions related to the atmosphere inside the housing 10 based on the contents of the change information. In addition to the control program described above, the memory unit 58 stores various information used in the detection of the state of at least a portion of a specified region including a molten portion by the detection unit 54 described later, the generation of change information by the calculation unit 56, and the judgment processing by the judgment unit 57.
[0052] The detection unit 54 determines the state of at least a part of a predetermined region in the material layer based on the image data generated by the above-mentioned imaging device 41. Here, the predetermined region includes a molten portion where the powder material P is melted by irradiation with laser light, unmelted powder material P (material layer) that has not yet melted, a region that has solidified after melting, a region where sputtering has occurred, and a region where fumes have occurred, as described below. In the following description, this predetermined region will be referred to as a detection target region.
[0053] The output unit 55 outputs status information based on the status of at least a part of the detection target area obtained by the detection unit 54 to the setting unit 59 (i.e., at least one of the material control unit 51, the printing control unit 52, and the housing control unit 53) in order to set the printing conditions of the printing apparatus 1. The status information based on the status of at least a part of the detection target area obtained includes change information for changing the printing conditions for printing a three-dimensional object generated by the calculation unit 56 described later, and information on the status itself of at least a part of the detection target area detected by the detection unit 54. Hereinafter, for convenience of explanation, the expression "at least a part of the detection target area" will be simply referred to as the detection target area.
[0054] The calculation unit 56 generates modification information for modifying the modeling conditions based on the state of the detection target region obtained by the detection unit 54. Furthermore, when the determination unit 57, which will be described later, determines that the modeled solidified layer needs repair, the calculation unit 56 generates repair information for repairing the solidified layer. The determination unit 57 determines whether or not the modeling conditions need to be changed, based on the state of the detection target area obtained by the detection unit 54. In addition, the determination unit 57 determines whether or not the modeled solidified layer needs to be repaired, based on the state of the detection target area obtained by the detection unit 54. The processes performed by the detection unit 54, the calculation unit 56 and the determination unit 57 will be described in detail later.
[0055] Next, the operation of the molding apparatus 1 having the above configuration will be described. First, the housing control unit 53 controls the intake device 131, the exhaust device 14, and the heater 15 so that the interior of the housing 10 is filled with a set atmosphere. The housing control unit 53 controls the valve opening of the intake device 131 and the exhaust amount of the exhaust device 14 so that the set pressure inside the housing 10 is obtained. In addition, the housing control unit 53 controls the valve opening of the intake device 131 to introduce an inert gas into the inside of the housing 10 and reduce the oxygen concentration in the housing 10. By reducing the oxygen concentration, the powder material P is oxidized and an oxide film is suppressed from being formed on the particle surface of the powder material P when the powder material P is irradiated with a laser beam and melted. When an oxide film is formed on the particle surface of the powder material P, the specific heat changes depending on the thickness of the oxide film, so that when the powder material P is irradiated with a laser beam as described later, it may affect the absorption of heat and the conduction of heat by the powder material P due to the irradiation of the laser beam. In this case, the powder material P may not melt, the solidified layer to be formed may have a defective shape or insufficient strength, or a solidified layer having a desired metal structure may not be obtained, which may cause poor melting. By reducing the oxygen concentration in the housing 10, the oxidation of the powder material P, which causes poor melting, as described above, is suppressed. The housing control unit 53 controls the heating output of the heater 15 to heat the inside of the housing 10 to the temperature inside the housing 10 set as the modeling conditions.
[0056] When an inert gas is introduced into the housing 10, the oxygen concentration becomes lower than a predetermined concentration, and the inside of the housing 10 is heated to a set temperature by the heater 15, the material control unit 51 controls the drive mechanism 212 to move (raise) the bottom surface 211 of the material supply tank 21 to the + side in the Z direction. The modeling control unit 52 controls the drive mechanism 312 to move (lower) the base plate 311 of the modeling tank 31 to the - side in the Z direction by the thickness Δd of the material layer to be formed. The material control unit 51 controls the drive mechanism of the recoater 22 to move the blade 221 from position A to position B along the X direction. The blade 221, which starts moving from position A, transfers the powder material P pushed out of the material supply tank 21 by the rise of the bottom surface 211 onto the base plate 311 of the modeling tank 31 on the + side of the X direction. The powder material P transferred onto the base plate 311 is pressed downward (Z direction - side) by the lower end (Z direction - side) of the blade 221 moving in the X direction + side, so that the powder material P is spread out on the base plate 311 with the height (Z direction thickness) from the surface of the base plate 311 being uniform. This forms a material layer with a constant thickness (lamination thickness) from the surface of the base plate 311. At this time, the moving speed of the blade 221 and the pressure applied by the blade 221 to the powder material P are controlled by the material control unit 51, so that the lamination thickness of the material layer, the flatness of the material layer surface, the density, etc., desired by the user can be obtained. Note that density refers to the thickness of the material layer relative to the amount of powder material P in the formed material layer, and the lower the density, the greater the proportion of gaps present in the material layer.
[0057] The irradiation unit 32 irradiates the formed material layer with laser light. The scanning unit 33 scans the surface of the material layer with the laser light from the irradiation unit 32. The path along which the laser light is scanned (scanning path) is set based on slice model data, which is a collection of shape data obtained by slicing design data of a three-dimensional object to be modeled by the modeling apparatus 1, such as CAD data or STL data converted from CAD data, related to the three-dimensional shape of the three-dimensional object, at a predetermined interval (e.g., an interval equal to the stacking thickness of the material layers) along the Z direction. This slice model data is solidified layer shape data that determines the shape of the solidified layer in each layer.
[0058] The modeling control unit 52 of the calculation device 50 determines a scanning path for scanning the laser light by the scanning unit 33 so that the powder material P on the surface of the material layer is irradiated, in accordance with the shape determined by the slice model data of the three-dimensional object corresponding to the Z-direction position of the base plate 311. In order to prevent deformation or damage of the 3D object or the solidified layer during the modeling process, modeling is performed while forming the solidified layer during modeling and a support part that supports the 3D object. Shape data of the support part, which indicates information such as the shape and thickness of the support part, is shape data of the 3D object (i.e., data on the shape of the support part in CAD data or STL data) or slice model data created based on the shape data of the 3D object.
[0059] The printing orientation data of the three-dimensional object is data indicating the printing orientation of the three-dimensional object (shape data of the three-dimensional object) for setting the slice model data. The printing orientation refers to the orientation in which the three-dimensional object is printed, such as when printing a three-dimensional object having a rectangular prism shape, whether solidified layers are stacked along the axial direction of the prism, or whether printing of solidified layers is started from the side of the prism and then stacked along a direction intersecting with the axial direction of the prism. In addition, when generating slice model data, it is preferable to generate slice model data by considering shape changes due to thermal expansion, rather than using design data as is. In particular, when the solidified layer is generated, the solidified layer is heated to a higher temperature by irradiation with laser light compared to room temperature. However, when there is a large difference between the temperature in the environment in which the three-dimensional object is used and the temperature at which the solidified layer is formed, it is preferable to generate slice model data from data (shape data of the three-dimensional object) obtained by modifying the design data as described above, taking into account the linear expansion coefficient due to the temperature difference.
[0060] Furthermore, it is preferable to set allowable tolerance information calculated based on CAD data for each slice model data. For example, the allowable tolerance information can be set for each slice model data in the manner described in Japanese Patent Application Laid-Open No. 2006-59014. The design data relating to the shape of the three-dimensional object includes shape data of the solidified layer, modeling posture data, shape data of a support part supporting the solidified layer or the three-dimensional object, or shape data of the three-dimensional object. The modeling control unit 52 causes the laser light from the irradiation unit 32 to scan the surface of the material layer in accordance with this design data. When the modeling control unit 52 changes the design data of the three-dimensional object and changes the slice model data based on the design data, the modeling control unit 52 causes the laser light from the irradiation unit 32 to scan the surface of the material layer in accordance with the changed slice model data.
[0061] The laser light irradiated to the powder material P is absorbed by the powder material P at an absorption rate determined by the conditions such as the output and wavelength of the emitted laser light, the type of powder material P, the shape of the particles of the powder material P, the surface shape of the material layer, etc. By absorbing the laser light, the powder material P irradiated with the laser light is rapidly heated, the temperature rises, and the heat is conducted to the surrounding powder material P. When the temperature rises due to heating and reaches the melting point of the powder material P, the powder material P on the surface of the material layer melts and vaporizes, and the evaporated material is ejected due to the increase in vapor pressure, forming a molten recess on the surface of the material layer. The laser light irradiated to this recess is further absorbed in the molten part, and melting, vaporization, and ejection of the evaporated material are repeated. As a result, the recess becomes a hole with an increased depth below the material layer (Z direction - side), and the laser light is multiple-reflected on the wall of the hole, which significantly increases the absorption rate of the laser light. As a result, a deep hole (keyhole) with an increased depth below is formed. As described above, the laser light is multiple-reflected on the wall of the hole, and the cross-sectional shape of the keyhole in the XY plane approaches a circle. A keyhole is formed at the position where the laser light is irradiated, and the inside of the material layer is directly heated. It is known that the shape of the keyhole becomes deeper as the energy transmitted to the powder material P by the laser light irradiation increases, and the opening becomes larger as the temperature of the powder material P increases. In the keyhole, the absorption rate of the laser light that is multiple-reflected on the wall surface increases as described above, causing evaporation to occur, which is ejected from the keyhole opening (top opening) as fumes. As the fumes are ejected, part of the molten area around the keyhole (part of the molten powder material P) scatters as particulate spatter.
[0062] When the laser light is scanned by the scanning unit 33 with the keyhole formed, the keyhole is maintained by the balance of forces such as the vapor pressure inside the keyhole, the surface tension of the molten part, and the gravity of the molten part, and the powder material P located in the direction in which the laser light advances by scanning (the +X direction when scanning toward the +X direction) melts. The molten liquid generated by the melting of the powder material P mixes with the molten liquid generated in the powder material P around the keyhole, and forms a molten pool in the liquid phase around the keyhole.
[0063] FIG. 4 is a diagram showing a molten pool and its vicinity caused by irradiating a material layer with a laser beam, in which FIG. 4(a) is a plan view showing a molten pool and its vicinity on the material layer in the XY plane, and FIG. 4(b) is a cross-sectional view in the ZX plane. FIG. 4 shows the keyhole KH formed as described above, the molten pool MP, the powder material P that has not yet started to melt, the fumes FU, the spatters SP, and the solidified region BE formed by the molten pool MP solidifying as described later. FIG. 4 shows the case where the laser beam is scanned from the + side to the - side in the X direction. FIG. 4(a) also shows the isothermal lines in the molten pool MP with broken lines. Inside the molten pool MP, due to the difference in surface tension caused by the temperature difference between the surface and the inside of the molten pool MP, convection occurs as shown by the arrow C in FIG. 4(b), for example. When the convection C becomes larger due to the heat generated by the irradiation of the laser light, the amount of fumes FU generated increases, and part of the molten powder material P around the keyhole KH is blown away from the molten pool MP and scattered around the keyhole KH and the molten pool MP as spatter SP.
[0064] When the heat due to the irradiation of the laser beam becomes excessive, the convection C in the molten pool MP becomes large or becomes turbulent. When the convection C becomes large, the molten pool MP is agitated more, so the amount of spatter SP scattered and the speed at which the spatter SP scattered increase. Furthermore, when the convection C becomes turbulent and irregular in the molten pool MP, the direction in which the spatter SP scattered is not fixed when viewed from the keyhole KH (for example, backward with respect to the scanning direction of the laser beam), and it also scatters forward and to the side of the scanning direction of the laser beam. Furthermore, the more the heat due to the irradiation of the laser beam becomes excessive, the more the amount of fumes FU generated increases, so the concentration of the fumes FU becomes high and the range in which the fumes FU are generated and diffuse from the keyhole KH becomes wide.
[0065] When the keyhole KH moves with the scanning of the laser beam, a new molten pool MP is formed around the keyhole KH on the moving direction side (the negative side of the X direction in FIG. 4), and the already formed (not yet solidified) molten pool MP is relatively located behind the keyhole KH (the positive side of the X direction in FIG. 4), so that the overall shape of the molten pool MP becomes elliptical on the XY plane as shown in FIG. 4(a). As the laser beam is scanned and moves away from the irradiation position, the absorption of the energy of the laser beam weakens, and the area cooled by the influence of the flow rate and flow speed of the inert gas in the housing 10 solidifies to form a solidified region BE. As the keyhole KH continues to move with the scanning of the laser beam, the powder material P solidifies and solidifies in the area of the material layer irradiated with the laser beam, forming a continuous solidified region BE. The laser beam is irradiated so that the gap between the solidified region BE to be formed and the already formed solidified region BE (two solidified regions BE extending in the X direction in FIG. 4(a)) is in contact with each other, and the formed solidified regions BE are welded to each other. The distance between two different solidified regions BE extending in the same direction is determined by the scanning interval (scanning pitch) when scanning the laser light. The scanning interval (scanning pitch) is the distance between two adjacent laser light irradiation positions in a direction (Y direction in FIG. 4(a)) intersecting the scanning direction of the laser light (X direction in FIG. 4(a)). When the formed solidified regions BE are welded together, a layered solidified layer having a predetermined thickness along the Z direction is formed.
[0066] During the formation of the solidified layer, the imaging device 41 captures an image of the surface of the material layer to generate image data. As shown in FIG. 2, the thermal radiation light incident on the imaging device 41 travels in the opposite direction to the laser light emitted from the irradiation unit 32 on the same axis, so that the center of the imaging field of the imaging device 41 (i.e., the center of the image captured by the imaging device 41) is approximately the same as the irradiation position of the laser light on the material layer. When the material layer is irradiated with the laser light from the irradiation unit 32, the imaging device 41 captures an image of a detection target area including the molten pool MP in the XY plane, centered on the irradiation position of the laser light on the surface of the material layer (the position of the keyhole KH if a keyhole KH is generated), to generate image data. That is, the detection target area includes the powder material P (unmelted powder material P) of the material layer just before melting begins, the molten pool MP, and the solidified area BE (in other words, a part of the solidified layer). In addition, when spatter SP or fumes FU are generated from the keyhole KH, the detection target area also includes the spatter SP and fumes FU. As the scanning unit 33 scans with the laser light, the detection target area imaged by the imaging device 41 moves on the surface of the material layer. The imaging device 41 captures images, for example, at predetermined time intervals or each time the scanning unit 33 scans the laser light over a predetermined distance on the XY plane.
[0067] When the solidified layer is formed, the modeling control unit 52 controls the drive mechanism 312 to move (lower) the base plate 311 of the modeling tank 31 to the negative side in the Z direction by the layer thickness Δd of the material layer to be formed. The material control unit 51 controls the drive mechanism 212 to move the bottom surface 211 of the material supply tank 21 to the positive side in the Z direction, and controls the drive mechanism of the recoater 22 to move the blade 221 along the X direction from position A to position B. As a result, the powder material P is spread on the upper part (positive side in the Z direction) of the solidified layer with the height (thickness in the Z direction from the upper part of the solidified layer) being uniform. As a result, a new material layer is formed on the upper part of the solidified layer, the thickness from the upper part of the solidified layer being a constant layer thickness Δd.
[0068] The new material layer is scanned on the XY plane with laser light from the irradiation unit 32 by the scanning unit 33. The powder material P is melted by the irradiation of the laser light to form a molten pool MP, which is welded to the adjacent solidified regions BE in the X and Y directions as described above, and the molten pool MP flows downward (Z direction - side) and is welded to the already formed solidified layer at the bottom (Z direction - side). As a result, a new solidified layer is formed on top of the already formed solidified layer. The modeling apparatus 1 repeats the process of forming a material layer and modeling a solidified layer, and models a three-dimensional object in which a plurality of solidified layers are stacked along the Z direction.
[0069] When a three-dimensional object is being manufactured as described above, if a modeling defect such as a defect, shape abnormality, surface roughness, or abnormality in metal structure occurs in the solidified layer, it is difficult to repair the modeling defect of the three-dimensional object after the three-dimensional object has been manufactured, and it is particularly difficult to repair a modeling defect inside the three-dimensional object. Furthermore, since there are many parameters for setting the conditions for manufacturing the three-dimensional object, it is difficult and time-consuming to set the conditions for manufacturing the three-dimensional object prior to manufacturing so as to prevent the modeling defect from occurring. In the modeling apparatus 1 of this embodiment, the detection unit 54, the calculation unit 56, and the determination unit 57 of the calculation device 50 change various conditions for modeling a three-dimensional object (hereinafter, modeling conditions) or generate information for repairing a solidified layer, based on the state of the detection target area obtained at the start of modeling of the three-dimensional object or during modeling. Based on this information, the material control unit 51, the modeling control unit 52, and the housing control unit 53 control the operation of each component of the modeling apparatus 1 to prevent modeling defects from occurring in the solidified layer during modeling, or to repair the modeling defects when possible, even if they occur.
[0070] The processes performed by the detection unit 54, the calculation unit 56 and the determination unit 57 will be described below. First, the concept behind the detection unit 54, the calculation unit 56 and the determination unit 57 performing the processes described below will be described. In this embodiment, in order to prevent the occurrence of modeling defects in the solidified layer formed by irradiating the powder material P of the material layer with laser light from the irradiation unit 32 and to form a three-dimensional object with reduced modeling defects, the following basic conditions are controlled to be kept within a certain range. The basic conditions are power density PD [J / mm 2 ] and the energy density ED [J / mm 2 [°C] of the powder material P in the molten pool MP melted by the irradiation of the laser beam and in its neighboring area. The power density PD, energy density ED, and temperature distribution T(r) are expressed by the following equations (1) to (3), respectively. PD = {η × (P L +P0)} / (d×v) …(1) ED = ρ × {η × (P L +P0)} / (v×Δy×Δz) …(2) T(r) = {η×P L / (2π×k×r)}×exp{(-v)×(x+r) / 2α}+T0…(3)
[0071] In the formulas (1) to (3), the parameters are as follows: Lis the output of the laser light (hereinafter referred to as the laser output) [W]. P0 represents the energy [W] added to the powder material P by an external heat source, i.e., the base plate 311 or the like, or by a heater or the like outside the modeling apparatus 1. η is the energy absorption rate of the powder material P, and has a different value depending on the type of powder material P, for example. v is the scanning speed of the laser light [mm / s]. d is the beam size (spot size) of the laser light on the surface of the material layer [mm]. Δy is the interval (scanning pitch) [mm] of the scanning path, i.e., the interval between the irradiation positions of the laser light in a direction intersecting with the direction in which the laser light is scanned. Δz is the layer thickness, i.e., the thickness in the Z direction of the material layer to be formed [mm]. ρ is the density of the material layer. k is the thermal conductivity of the powder material P [W / mm / K], r is the distance from the center of the sphere defined around the laser light irradiation position [mm], x is the distance on the XY plane along the scanning direction from the laser light irradiation position [mm], and α is the thermal diffusivity of the powder material P [mm 2 / s], and T0 is the initial temperature of powder material P [℃].
[0072] The larger the value of the power density PD shown in the above formula (1), i.e., the greater the amount of heat flowing into the powder material P, the easier it is for the powder material P to melt. Formula (1) indicates that in order to increase the power density PD and make it easier to melt the powder material P, at least one of the parameters may be controlled based on the following policy. Regarding the parameter η, for example, it is preferable to use a powder material P with a high absorptance of laser light. The parameter P L Regarding parameter ρ and P0, for example, it is preferable to increase the laser output or increase the amount of heat applied to the powder material P from the outside. Regarding parameter d, for example, it is preferable to increase the heat input efficiency of the heat amount flowing into the powder material P by reducing the spot size of the laser light and increasing the amount of heat per unit area on the material layer by irradiation with the laser light. Regarding parameter v, for example, it is preferable to increase the amount of heat flowing into the powder material P by reducing the scanning speed and increasing the time during which the powder material P contained per unit area of the material layer is irradiated with the laser light.
[0073] Moreover, the smaller the value of the power density PD shown in formula (1), the more difficult it is for the powder material P to melt. In cases where the powder material P is over-melted, it is advisable to control at least one of the above-mentioned parameters in a manner opposite to the above-mentioned manner so as to reduce the value of the power density PD in formula (1). The opposite manner means that at least one of the following exemplary manners is carried out. With regard to the parameter η, for example, a powder material P with a low absorption rate is used. The parameter P L For parameter P0, for example, the laser output is reduced or the amount of heat applied from the outside to the powder material P is reduced. For parameter d, for example, the spot size is increased. For parameter v, for example, the scanning speed is increased.
[0074] The larger the value of the energy density ED shown in formula (2), the easier it is for the powder material P to melt. Formula (2) indicates that in order to increase the value of the energy density ED and make the powder material P easier to melt, at least one of the parameters should be controlled based on the following policy. As for the parameter η, as in the case of formula (1) above, for example, a powder material P with a high absorption rate of laser light should be used. Parameter P LRegarding parameter ρ and P0, for example, the laser output is increased, or the amount of heat applied to the powder material P from an external heating device is increased. Regarding parameter ρ, for example, the density of the material layer is increased to reduce the gaps in the material layer. This makes it easier for the heat generated by the irradiation of the laser light to be conducted through the powder material P. Regarding parameter v, for example, the scanning speed is decreased to increase the time during which the laser light is irradiated onto the powder material P contained in each unit area of the material layer. This increases the amount of heat flowing into the powder material P. Regarding parameter Δy, for example, the scanning pitch is narrowed. This increases the influence of heat from the adjacent solidified region BE. Regarding parameter Δz, for example, the layer thickness is reduced. This increases the influence of heat from the solidified layer already formed in the lower layer (Z direction - side), so that the initial temperature of the powder material P becomes higher. As a result, the amount of heat required for the powder material P irradiated with the laser light to rise to the desired temperature (for example, the melting point) is reduced.
[0075] Moreover, the smaller the value of the energy density ED shown in formula (2), the more difficult it is for the powder material P to melt. In cases where the powder material P is over-melted, it is advisable to control at least one of the above parameters in a manner opposite to the above-mentioned manner so as to reduce the value of the energy density ED in formula (2). The opposite manner means that at least one of the following exemplary manners is carried out. With regard to the parameter η, for example, a powder material P with a low absorption rate is used. The parameter P L For parameter ρ and P0, for example, the laser output can be reduced or the amount of heat applied to the powder material P from the outside can be reduced. For parameter ρ, for example, the density can be reduced. For parameter v, for example, the scanning speed can be reduced. For parameter Δy, for example, the scanning pitch can be increased. For parameter Δz, for example, the layer thickness can be increased.
[0076] If the power density PD or the energy density ED is increased, the powder material P becomes easier to melt, but if the power density PD or the energy density ED is increased too much, the convection C in the molten area MP described above is affected, and the generation of spatter SP and fumes FU increases. When the spatter SP scattered from the molten pool MP by the irradiation of the laser light falls onto a material layer that has not yet been irradiated with the laser light or onto an already formed solidified area BE and solidifies, it solidifies and remains as a granular deposit on the surface of the material layer or the upper surface of the solidified layer. Since the spatter SP is spherical, when a new material layer is formed on the solidified layer, it becomes difficult for the powder material P to enter between the bottom of the spatter SP solidified on the solidified area BE and the surface of the solidified layer, and a gap may occur. The gap that is generated when the powder material P does not enter may cause poor melting such as a cavity that occurs inside the solidified layer when the next solidified layer is formed. Furthermore, if the sputter SP is remelted when another solidified region BE is formed, the desired metal structure (crystal structure) may not be obtained at the location where the sputter SP is remelted, which may result in defective molding. In addition, if the fumes FU generated by the irradiation of the laser light remain near the irradiation position of the laser light on the material layer, the energy of the laser light directed toward the material layer is attenuated by the fumes FU, so that the effect of heating the powder material P by the irradiation of the laser light is reduced, and the expected melted state may not be obtained. In this way, poor melting due to the adhesion of spatter SP or the generation of fumes FU may cause defects in the three-dimensional object, poor shape, and poor molding such as insufficient strength due to the failure to obtain the desired metal structure (crystal structure) due to poor melting. Since the spatter SP and fumes FU cause poor molding of the three-dimensional object as described above, it is necessary to control the power density PD and energy density ED so as not to increase too much in order to suppress the generation of spatter SP and fumes FU.
[0077] Furthermore, if the power density PD or the energy density ED is too low, the powder material P will not be able to fully receive the energy of the irradiated laser light, causing the powder material P to not melt (not melted), or causing a molten pool MP of the desired size to not be obtained, resulting in defective molding of the three-dimensional object. For this reason, it is necessary to control the power density PD and the energy density ED so that they do not drop too low. In this way, the power density PD and the energy density ED need to be kept within a certain range without becoming too large or too small. This certain range is calculated from the results of various tests and simulations performed by the user so that the three-dimensional object will be a good product. The certain range of the power density PD and the energy density ED that will result in a good three-dimensional object will be referred to as the desired range.
[0078] The temperature distribution T(r) shown in formula (3) indicates the temperature that is assumed to be obtained at a position (x, y, z) at an arbitrary distance r on or in the material layer from the center, with the laser light irradiation position on the material layer as the center, when the laser light is irradiated on the irradiated material layer under the currently set building conditions. That is, formula (3) is a formula that estimates the state of heat conduction due to the laser light irradiation in the material layer when the laser light is irradiated under the currently set building conditions. Therefore, formula (3) estimates the progress of melting of the powder material P on the surface (X direction and Y direction) and the depth direction (Z direction) of the material layer, or the progress of solidification after melting. Formula (3) can estimate the state in which the temperature of the powder material P changes depending on the distance from the position irradiated with the laser light. Therefore, it is possible to grasp the range (for example, an elliptical range on the XY plane) estimated as the molten pool MP, which is an area with a temperature higher than a predetermined temperature. It is possible to grasp the temperature distribution of the range estimated as the molten pool MP three-dimensionally depending on the distance from the laser light irradiation position. Therefore, by setting the molding conditions so that the temperature distribution T(r) is kept within a certain range, the state in which the temperature changes in the molten pool MP can be controlled, which makes it possible to maintain the desired crystal structure in the solidified layer after solidification and to control the convection C of the molten pool MP.
[0079] In addition, the convection C of the molten pool MP caused by the irradiation of the laser light affects the shape of the molten pool MP (i.e., the shape of the solidified region BE after solidification and the penetration depth when melting in the negative Z direction). Therefore, by keeping the temperature distribution T(r) within a certain range, the state of the convection C of the molten pool MP, which is the behavior of heat caused by the irradiation of the laser light in the molten pool MP, is controlled. This suppresses the occurrence of poor penetration and the occurrence of defective molding such as insufficient strength of the solidified layer and reduced durability. In addition, as described above, since the convection C affects the occurrence of spatters SP and fumes FU, by keeping the temperature distribution T(r) within a certain range, the occurrence of spatters SP and fumes FU is suppressed, and the occurrence of defective molding caused by spatters SP and fumes FU is suppressed. This certain range is calculated from the results of various tests and simulations performed by the user so that the three-dimensional object is a good product. Note that a certain range of the temperature distribution T(r) that makes the three-dimensional object a good product is called a desired range. It is sufficient that at least one of the basic conditions (1) to (3) satisfies a desired range.
[0080] Next, the processes performed by the detection unit 54, the calculation unit 56, and the determination unit 57 to change the modeling conditions based on the above-mentioned formulas (1) to (3) will be described. The detection unit 54 determines the state of the detection target area based on the image data from the imaging device 41. The state of the detection target area includes at least one of the following: the state of the powder material P before being heated by irradiation with the laser light, the melted state in the detection target area, the state of the spatter SP, and the state of the fumes FU generated by being heated by irradiation with the laser light. The detection unit 54 determines, for example, information on the temperature of at least a part of the molten pool MP and its vicinity (a semi-solidified area where the solution is about to become solid after melting and a solidified area BE) as an example of the melted state in the detection target area. The detection unit 54 determines, for example, at least one of the scattering direction, scattering amount, and scattering speed of the spatter SP as the state of the spatter SP. The detection unit 54 determines, for example, at least one of the concentration and range of the fumes FU as the state of the fumes FU. In addition, determining the state of the detection target area can also be rephrased as measuring the state of the detection target area, calculating the state of the detection target area, evaluating the state of the detection target area, or detecting the state of the detection target area, taking into account the state of the detection target area to be determined (specifically, the state of the powder material P mentioned above, the molten state, the state of the sputter SP, the state of the fumes FU, etc.).
[0081] In this embodiment, the change of the modeling conditions based on the state of the detection target area obtained by the detection unit 54 includes a real-time change, a change during the next layer modeling, and a change during the next object modeling. In the real-time change, the modeling conditions are changed for the material layer used to obtain the state of the detection target area when forming a solidified layer by irradiating a laser beam or during the modeling. Therefore, in the real-time change, the modeling conditions are changed for the unmelted powder material P in the material layer during the modeling of the solidified layer. In the change during the next layer modeling, the modeling conditions are changed when the formation of the next material layer or the modeling of the solidified layer is started from the next material layer after the solidified layer is modeled. Therefore, in the change during the next layer modeling, the modeling conditions are changed for the new powder material P supplied on the modeled solidified layer or the new powder material P supplied on the solidified layer. In the change during the next object modeling, the modeling conditions are changed when the modeling of the three-dimensional object is completed by stacking solidified layers and modeling of the next three-dimensional object is started.
[0082] The following will separately describe a process for determining the state of the detection target region by the detection unit 54 and a process for generating change information for changing the modeling conditions by the calculation unit 56.
[0083] (1) Processing to determine the state of the detection target area The detection unit 54 uses the image data generated by the imaging device 41 to determine the state of the detection target area on the material layer. As described above, the image data output from the imaging device 41 includes information on light of different wavelengths λ1 and λ2 among the thermal radiation light from the detection target area. The detection unit 54 determines information on the temperature of at least a part of the molten pool MP and its vicinity based on the ratio between the luminance information of the wavelength λ1 included in the image data obtained by capturing an image of the detection target area and the luminance information of the wavelength λ2 included in the image data. In this case, the detection unit 54 generates image data (hereinafter referred to as temperature image data) in which the luminance information of the wavelengths λ1 and λ2 of the image data is converted to temperature, for example, using a known two-color method. The temperature image data is the signal intensity for each pixel corresponding to the temperature. The detection unit 54 calculates the ratio (for example, the luminance value ratio) between the luminance information of the light of the wavelength λ1 included in the image data and the luminance information of the light of the wavelength λ2 included in the image data, and compares it with the relationship data between the luminance value ratio and temperature that is a reference obtained based on a gray body, a black body, etc., to convert the luminance value ratio of the wavelengths λ1 and λ2 at any position on the image data into temperature. This generates temperature image data that represents the temperature at any position in the detection target area on the image data. The detection unit 54 can obtain the temperature distribution in the detection target area, the maximum temperature, the minimum temperature, the average temperature, and the like from this temperature image data. The detection unit 54 generates temperature image data for each piece of image data generated by the imaging device 41. Every time the detection unit 54 generates temperature image data, it stores and saves it in the storage unit 58.
[0084] Fig. 5 is a diagram showing an example of a temperature image corresponding to the temperature image data generated by the detection unit 54 based on the image data obtained by capturing the detection target area shown in Fig. 4(a), and shows a case where the laser light is scanned on the material layer from the + side to the - side in the X direction. Note that in Fig. 5, for convenience of illustration, the difference in temperature in the molten pool MP in the temperature image is shown by an isothermal line shown by a dashed line, and the range affected by the fumes FU is shown by hatching.
[0085] As described above, when the material layer is irradiated with the laser light, the imaging device 41 captures an image of the detection target region of the material layer including the molten pool MP. Therefore, the generated temperature image data (temperature image) includes the molten pool MP, the solidified region BE where solidification has been completed, and the powder material P, with the keyhole KH as the center of the image. Since the laser light is scanned toward the negative side of the X direction, in the temperature image, the molten pool MP has a larger elliptical region on the positive side of the X direction with respect to the keyhole KH than on the negative side of the X direction. In addition, when granular spatter SP is scattered by the irradiation of the laser light, the spatter SP also has heat and is therefore included in the temperature image data (temperature image). In addition, when fumes FU, which are vaporized materials, are generated by the irradiation of the laser light, the fumes FU also have heat and are therefore included in the temperature image data (temperature image).
[0086] The detection unit 54 obtains, as the state of the detection target area, the state of the powder material P before heating by irradiation with laser light, the melting state in the detection target area, the state of spatter SP, and the state of fumes FU, from a temperature image such as that shown in Fig. 5. Hereinafter, the detection of the state of the detection target area will be described separately for detection of the state of the powder material P before heating by irradiation with laser light, detection of the melting state in the detection target area, detection of the state of spatter SP, and detection of the state of fumes FU.
[0087] <Detection of the state of powder material P before heating by irradiation with laser light> The detection unit 54 obtains, from the temperature image data, information on the temperature of an area other than the molten pool MP and the solidified area BE as the state of the powder material P before heating by irradiation with the laser light. In this case, the detection unit 54 obtains an area that is lower than the first predetermined temperature. The first predetermined temperature is set, for example, based on the melting point of the powder material P. Note that the first predetermined temperature is not limited to the melting point, and may be the solidus temperature or liquidus temperature, or any temperature in the range from the solidus temperature to the liquidus temperature. Here, when the detection unit 54 determines the temperature of the powder material P of the material layer before heating by irradiation with the laser light, it can estimate a region in the scanning direction relative to the irradiation position of the laser light as the region on the material layer where the temperature of the powder material P should be determined. The detection unit 54 determines a region of this estimated region that is lower than the first predetermined temperature as the temperature of the powder material P before heating by irradiation with the laser light.
[0088] The detection unit 54 may obtain the molten pool MP and the solidified region BE from image data of the detection target area captured by an imaging device other than the imaging device 41, and may remove the molten pool MP and the solidified region BE from the temperature image data based on the molten pool MP and the solidified region BE obtained from the image data to obtain the powder material P before heating by irradiation with the laser light on the temperature image data. In this case, the imaging device 41 and the imaging device other than the imaging device 41 need to be controlled so that the timing of capturing the images of the detection target area is synchronized.
[0089] Using the temperature image data, the detection unit 54 determines information regarding the temperature of the powder material P before heating by irradiation with the laser light, such as the temperature distribution, maximum temperature, minimum temperature, average temperature, etc. of the powder material P before heating. This allows the detection unit 54 to determine the initial temperature T0, which is a parameter of the above formula (3). Furthermore, the detection unit 54 may use a known image processing method from the image data captured by the imaging device 41 to determine foreign matter and spatter SP contained in the powder material P as the state of the powder material P before heating.
[0090] The detection unit 54 does not have to determine the state of the powder material P before heating by irradiation with laser light from the temperature image data obtained by the two-color method. For example, the acquisition unit 310 may use an existing radiation thermometer instead of the imaging device 41, the bifurcating optical system 42, the chromatic aberration correction optical system 43, and the field stop 302 to acquire temperature data based on infrared rays from the powder material P before heating by irradiation with laser light. In this case, the detection unit 54 may determine the state of the powder material P before heating by irradiation with laser light based on the temperature data acquired by the acquisition unit 310 (a radiation thermometer not shown).
[0091] The acquisition unit 310 does not have to be a radiation thermometer, and an existing contact thermometer such as a thermocouple may be used. In this case, a plurality of thermocouples are installed at arbitrary positions in the modeling tank 31 of the modeling unit 30 or the material layer forming unit 20 as the acquisition unit 310, and the plurality of thermocouples acquire temperature data at each position. The detection unit 54 may obtain the state of the powder material P before heating by irradiation with the laser light using data on the correlation between the temperature data acquired by the thermocouples and the temperature data of the powder material P before heating by irradiation with the laser light. The data on the correlation between the temperature data acquired by the thermocouples and the temperature data of the powder material P before heating by irradiation with the laser light is stored in advance in the storage unit 58.
[0092] <Detection of melting state> The detection unit 54 obtains information on the temperature of the molten pool MP and its vicinity (the solidified region BE in the detection target region) as the state of melting from the temperature image data. In this case, the detection unit 54 obtains an area of the temperature image data that is higher than a first predetermined temperature as an area including the keyhole KH and the molten pool MP. In addition, when the detection unit 54 obtains the temperature of the solidified region BE after irradiation with laser light, it can estimate an area in the opposite direction to the scanning direction with respect to the irradiation position of the laser light as an area where the temperature of the solidified region BE should be obtained. The detection unit 54 obtains an area of this estimated area that is lower than the first predetermined temperature as the temperature of the solidified region BE after heating by irradiation with laser light. In addition, the detection unit 54 may estimate the area (semi-solidified area) where the liquid phase molten pool MP has started to solidify and become solid, from the keyhole KH and the molten pool MP, within the area of the temperature image data that is equal to or higher than the first predetermined temperature, and determine the temperature of this area.
[0093] The information related to the temperature of at least a part of the molten pool MP and its vicinity obtained by the detection unit 54 includes the temperature distribution of the molten pool MP, the maximum temperature, the minimum temperature, the average temperature, the position of the keyhole KH, the opening diameter (e.g., the length of the minor axis) of the keyhole KH at the top surface (surface of the material layer), the size of the molten pool MP, the thermal conductivity, the temperature gradient on the surface of the molten pool MP, the solidification rate which is the change in temperature at the boundary part of the molten pool MP on the surface, the temperature history, etc. Similarly, the detection unit 54 obtains the temperature distribution, the maximum temperature, the minimum temperature, the average temperature, the size, the thermal conductivity, the temperature gradient, the solidification rate, the temperature history, etc. of the solidified region BE and the semi-solidified region as information related to temperature.
[0094] The detection unit 54, for example, obtains temperatures at a plurality of positions in the region estimated as the molten pool MP in the temperature image data, and obtains the temperature distribution of the molten pool MP by setting isotherms for each predetermined temperature. The detection unit 54 obtains the highest temperature as the maximum temperature and the lowest temperature as the minimum temperature in the region estimated as the molten pool MP in the temperature image data. The detection unit 54 obtains the temperature at each of a plurality of positions in the region estimated as the molten pool MP in the temperature image data, and obtains the average temperature of the molten pool MP by calculating the average of the obtained temperatures. The detection unit 54 obtains the center of the temperature image data as the position of the keyhole KH. The detection unit 54 obtains a range that can be considered to have approximately the same temperature as the temperature at the center of the temperature image data as the opening of the keyhole KH on the top surface, and obtains the length of the minor axis of the obtained opening as the opening diameter.
[0095] The detection unit 54 obtains the size of the molten pool MP from the area of the region on the temperature image that is equal to or higher than the first predetermined temperature. The detection unit 54 obtains the thermal conductivity from the size of the molten pool MP. In this case, the detection unit 54 converts the distance from the keyhole KH to the position of the first predetermined temperature in the temperature image data into the distance r on the material layer, inputs the value of the first predetermined temperature, the distance r, and the values of each parameter determined by the currently set molding conditions into the above-mentioned equation (3), and calculates the thermal conductivity by solving equation (3) for the parameter k. The detection unit 54 determines the temperature gradient on the surface of the molten pool MP and the solidification rate, which is the change in temperature at the boundary of the molten pool MP on the surface, based on the degree of density of the isotherms on the temperature image (temperature image data). Using a plurality of temperature image data generated by capturing images at a predetermined interval, the detector 54 obtains the temperature history of the molten pool MP and its vicinity. The temperature history is data that indicates the temperature change at a certain point in the material layer. An example of the detection of the temperature history is described below.
[0096] As described above, the image data generated by the imaging device 41, the irradiation position information indicating the irradiation position of the laser light (i.e., the position of the keyhole KH), and the time information are stored in association with each other. The detection unit 54 obtains the temperature history based on the irradiation position information associated with the image data. The detection process of the temperature history by the detection unit 54 will be described using an example in which the temperature history is obtained at a position Q1 that is a distance m away from a position Q2 where the keyhole KH (i.e., the center of the image) is located in a certain temperature image (first temperature image). The detection unit 54 obtains the temperature at the position Q1 from the first temperature image data. Then, after a predetermined time (after the irradiation position of the laser light has changed by a predetermined distance), the detection unit 54 obtains the position Q1 on a second temperature image different from the first temperature image.
[0097] Specifically, the detection unit 54 determines the position on the material layer of the keyhole KH1, which is the center of the first temperature image, and the position on the material layer of the keyhole KH2, which is the center of the second temperature image, based on the irradiation position of the laser light when the first image data was generated and the irradiation position of the laser light when the second image data was generated. If the laser light is scanned toward the negative side of the X direction, the position Q2 (the keyhole KH in the first temperature image) on the second temperature image is shifted from the center of the second temperature image toward the positive side of the X direction by a value obtained by converting the difference n between the positions of the keyholes KH1 and KH2 on the material layer into a distance on the temperature image. The detection unit 54 determines the position Q1 as the position that is further away from the position Q2 on the second temperature image toward the positive side of the X direction by a distance m, and determines the temperature at this position from the second temperature image data. The detection unit 54 can subsequently determine the temperature history at the position Q1 by similarly determining the temperature at the position Q1 from a plurality of temperature image data.
[0098] The detection unit 54 obtains information on the temperature of the solidified region BE as the state in the vicinity of the molten pool MP from the temperature image data. In this case, the detection unit 54 obtains the temperature distribution, average temperature, etc. of the solidified region BE. The detection unit 54 may obtain information on the temperature of the powder material P obtained as the state of the powder material P before heating as the state in the vicinity of the molten pool MP.
[0099] The detection unit 54 does not have to obtain information about the temperature of the molten pool MP and its vicinity (solidification region BE in the detection target region) (i.e., the state of melting) from temperature image data obtained by the two-color method. For example, the acquisition unit 310 may use an existing radiation thermometer instead of the imaging device 41, the bifurcating optical system 42, the chromatic aberration correction optical system 43, and the field stop 302 to obtain temperature data based on infrared rays from the molten pool MP and its vicinity. In this case, the detection unit 54 may obtain the state of melting based on the temperature data obtained by the acquisition unit 310 (a radiation thermometer not shown).
[0100] The acquisition unit 310 does not have to be a radiation thermometer, and an existing contact thermometer such as a thermocouple may be used. In this case, a plurality of thermocouples are installed at arbitrary positions in the modeling tank 31 of the modeling unit 30 or the material layer forming unit 20 as the acquisition unit 310, and the plurality of thermocouples acquire temperature data at each position. The detection unit 54 may determine the melting state by using data on the correlation between the temperature data acquired by the thermocouples and the temperature data of the molten pool MP or its vicinity (the solidified region BE in the detection target region). The data on the correlation between the temperature data acquired by the thermocouples and the temperature data of the molten pool MP or its vicinity (the solidified region BE in the detection target region) is stored in advance in the storage unit 58.
[0101] <Detection of sputter SP state> The detection unit 54 determines at least one of the amount, direction, and speed of the spatters SP as the state of the spatters SP. As described above, the state of the spatters SP is related to the convection C in the molten pool MP, so that the detection unit 54 can indirectly determine the state of the convection C in the molten pool MP by determining the state of the spatters SP.
[0102] For convenience of explanation, Fig. 6 shows a temperature image corresponding to the temperature image data used to obtain the state of the sputter SP, in which the fumes FU and the solidification region BE are excluded from Fig. 5. The detection unit 54 sets a region of interest used to obtain the state of the sputter SP within the temperature image data.
[0103] In this case, the detection unit 54 sets, as the region of interest, a region excluding the regions occupied by the keyhole KH and the molten pool MP in the temperature image shown in Fig. 6(a). The detection unit 54 can estimate the region including the keyhole KH and the molten pool MP (region to be excluded) from, for example, the above-mentioned formula (3) representing the temperature distribution T(r). As described above, the formula (3) representing the temperature distribution T(r) represents the temperature of the powder material P at an arbitrary distance r from the irradiation position of the laser light (i.e., the position of the keyhole KH), and uses as parameters the modeling conditions for forming a three-dimensional object, such as the output of the laser light.
[0104] The detection unit 54 determines a high-temperature region having a temperature equal to or higher than a first predetermined temperature including the position of the keyhole KH (i.e., the center of the temperature image) based on the equation (3) expressing this temperature distribution T(r) and the set building conditions, and determines the determined high-temperature region as a region to be excluded. As described above, the molten pool MP has an elliptical shape on the XY plane, so the region consisting of the keyhole KH and the molten pool MP has an elliptical shape. The detection unit 54 inputs the value of the first predetermined temperature and the values of each parameter determined by the currently set building conditions into the temperature distribution T(r) in the equation (3), and calculates the parameter r, thereby calculating the elliptical region having a temperature equal to or higher than the first predetermined temperature. The detection unit 54 detects a region included in the calculated elliptical region on the temperature image data (temperature image) as a high-temperature region, and determines the high-temperature region as a region to be excluded. In addition, the region to be excluded is not limited to an elliptical region including the keyhole KH and the molten pool MP, but an area including the solidification region BE in addition to the above-mentioned elliptical high-temperature region may be detected as the region to be excluded.
[0105] FIG. 6(b) is a diagram showing a schematic diagram of an exclusion target region R1 (shown with diagonal lines in FIG. 6(b)) that the detection unit 54 has determined for the temperature image shown in FIG. 6(a) and a region of interest R2 that has been set based on the determined exclusion target region R1. The region of interest R2 is a region where the powder material P is not melted by the irradiation of the laser light. Therefore, if a high-temperature region exists in the region of interest R2, the detection unit 54 determines the high-temperature region as a spatter SP. The detection unit 54 determines the amount of scattering of the spatter SP by counting the number of high-temperature regions included in the region of interest R2.
[0106] The detector 54 can determine the direction of scattering of the spatters SP on the XY plane by determining the direction from the center of the temperature image, that is, the irradiation position of the laser light, to each high-temperature region included in the region of interest R2. The detection unit 54 uses a plurality of temperature image data to determine the scattering speed of the sputter SP. The detection unit 54 extracts sputter SP that has fallen and adhered to the material layer or solidified region BE, i.e., sputter SP that remains at the same place on the material layer or solidified region BE, from two temperature image data with different time information, in the same manner as in the case of determining the temperature history, and excludes them from the detection target of the scattering speed. The detection unit 54 determines, among the sputter SP remaining as the detection target (i.e., sputter SP displaced with the passage of time), sputter SP whose size and temperature in one temperature image data (temperature image) can be considered to be the same as the size and temperature in the other temperature image data (temperature image), as scattering sputter SP (the same sputter). For the sputter SP determined as the same sputter, the detection unit 54 determines the position (first position) in the space above the material layer from one temperature image data (temperature image), and the position (second position) in the space above the material layer from the other temperature image data (temperature image). The detection unit 54 calculates (detects) the scattering speed of the sputters SP (the same scattered sputters) from the first position, the second position, and the difference in time information of the two temperature image data.
[0107] The detection unit 54 may obtain the state of the sputter SP without setting the region of interest R2 in the temperature image data (temperature image). In this case, the detection unit 54 generates average temperature image data by adding and averaging a plurality of temperature image data generated from the image data output by the imaging device 41. The plurality of temperature image data may be temperature image data generated from image data associated with different time information. The plurality of temperature image data may also be temperature image data at different times or different positions that have been generated in advance and stored in the storage unit 58. The detection unit 54 may generate average temperature image data each time it generates temperature image data, or may generate average temperature image data each time it generates a predetermined number of temperature image data. The occurrence state of the sputter SP (the number, position, size, etc. of the sputter SP on the temperature image data) differs for each temperature image data. Therefore, even if sputter SP is detected in one temperature image at the same position on a plurality of temperature images, sputter SP is not necessarily detected in many other temperature images. In the average temperature image data (average temperature image) generated based on these multiple temperature image data, the positions where spatter SP is detected in one temperature image data (temperature image) are added and averaged with the positions where spatter SP is not detected in the other multiple temperature image data (temperature images), thereby removing the spatter SP. The average temperature image data (average temperature image) from which the spatter SP has been removed includes the keyhole KH and the molten pool MP.
[0108] FIG. 6(c) shows an example of an average temperature image corresponding to the average temperature image data generated by the above process. As shown in FIG. 6(c), the average temperature image does not have any high-temperature areas other than the keyhole KH and the molten pool MP. The detection unit 54 obtains the difference between the temperature image data (detection target image data) corresponding to the temperature image for detecting the spatter SP shown in FIG. 6(a) and the average temperature image data corresponding to the average temperature image shown in FIG. 6(c). As a result, an image in which the keyhole KH and the molten pool MP are removed from the detection target image is generated as shown in FIG. 6(d). Since the high-temperature areas on this image are the spatter SP, the detection unit 54 determines at least one of the scattering amount, scattering direction, and scattering speed of the spatter SP based on the high-temperature areas as described above in the same manner as in the case described using FIG. 6(b). In particular, the detection unit 54 can determine both the scattering direction of the spatter SP scattered toward the X-direction + side (rearward with respect to the scanning direction of the laser light) with respect to the center of the temperature image.
[0109] The detection unit 54 does not need to determine the state of sputters from temperature image data obtained by the two-color method. For example, the acquisition unit 310 may use an imaging device (not shown) instead of the imaging device 41, the bifurcating optical system 42, the chromatic aberration correction optical system 43, and the field stop 302 to acquire image data of the detection target area. The imaging device (not shown) may have the same configuration as the imaging device 41 in FIG. 1, or may have another existing configuration. In this case, the detection unit 54 performs existing image processing using the image data acquired by the acquisition unit 310 (imaging device (not shown)) and detects a circular image of a predetermined size from the image as an image of sputters. The detection unit 54 then determines at least one of the scattering amount, scattering direction, and scattering speed of the sputters SP from the time change in the position of the detected sputter images and the number of sputters.
[0110] The correlation between the state of spatter SP and the melted state of the molten pool MP can be determined from the correlation between the state of spatter SP (amount, direction and speed of scattering of spatter SP) and the convection C of the molten pool MP, and the correlation between the convection C of the molten pool MP and the melted state of the molten pool MP (information relating to temperature). Therefore, the detection unit 54 may (indirectly) determine the melted state of the molten pool MP based on the determined state of spatter SP. In this case, data relating to the correlation between the state of spatter SP and the melted state of the molten pool MP is stored in advance in the memory unit 58.
[0111] <Detecting the state of fume FU> The detection unit 54 determines at least one of the concentration and range of the fumes FU as the state of the fumes FU from the temperature image data. As described above, the state of the fumes FU is related to the convection C in the molten pool MP, so that the detection unit 54 can indirectly determine the state of the convection C inside the molten pool MP by determining the state of the fumes FU.
[0112] Fig. 7 shows an example of a temperature image corresponding to the temperature image data used to obtain the state of the fumes FU. In Fig. 7, for convenience of illustration, the solidified region BE is omitted. As described above, the fumes FU are generated from the molten pool MP generated by irradiating the material with the laser light, so the light from the detection target region of the material layer is affected by the fumes FU and has a reduced brightness. In Fig. 7, the shaded region indicates the region where the brightness value is reduced due to the effect of the fumes FU. Fig. 7(a) is the same temperature image as the temperature image shown in Fig. 5. Fig. 7(b) shows a schematic diagram of the original image data of the temperature image data corresponding to this temperature image, that is, the images corresponding to the respective image data generated by the light of wavelength λ1 and the light of wavelength λ2 being incident on different positions of the imaging element 411. In the original image of Fig. 7(b), an image D1 due to the light of wavelength λ1 is shown on the left side of the page, and an image D2 due to the light of wavelength λ2 is shown on the right side of the page.
[0113] As described above, the luminance value of the light emitted from the detection target region of the material layer is reduced due to the influence of the fumes FU, so that both the images D1 and D2 have reduced luminance values. Assume that the image D1 is brighter (higher luminance) than the image D2. However, because light is scattered due to the influence of the fumes FU, the luminance of both the bright image D1 and the dark image D2 is reduced in the regions R3 and R4 affected by the fumes FU. In this case, the rate of reduction in luminance of the bright image D1 and the dark image D2 is substantially equal. The detection unit 54 distinguishes between the molten pool MP, the keyhole KH, the spatter SP, and the fumes FU based on whether or not the ratio of luminance values changes between the images D1 and D2. The fumes FU block the light from the molten pool MP, so the luminance values of both the light of wavelength λ1 and the light of wavelength λ2 are reduced, but the ratio of luminance values does not change between the images D1 and D2. In contrast, the ratio of luminance values changes between the molten pool MP, the keyhole KH, and the spatter SP. Since the brightness information of each pixel in the images D1 and D2 is known, the detection unit 54 can distinguish between the molten pool MP, the keyhole KH, the spatters SP, and the fumes FU based on the presence or absence of a change in the ratio of brightness values. The detection unit 54 determines the fumes FU thus separated (region R3 in the image D1 and region R4 in the image D2) as the range of the fumes FU.
[0114] The detection unit 54 obtains the concentration of the fume FU by obtaining the degree of the decrease in the luminance value using either the image D1 or the image D2. The detection unit 54 calculates the difference between the luminance value of the range of the fume FU obtained as described above (the region R3 of the image D1 or the region R4 of the image D2) and the luminance value of the other region, i.e., the region that is not affected by the fume FU and therefore has not decreased in luminance value, and calculates the concentration of the fume FU based on this difference. Note that data in which the difference in luminance value and the concentration of the fume are associated with each other is stored in advance in the storage unit 58, and the detection unit 54 refers to this data and calculates the concentration of the fume FU from the calculated difference. Note that the detection unit 54 may calculate the difference by comparing the luminance value of the image D1 or the image D2 in the image data obtained at a time different from when the image data corresponding to the original image shown in FIG. 7(b) was obtained with the luminance value of the image D1 or the image D2 in the image data of the original image in FIG. 7(b). In addition, since the brightness values of both images D1 and D2 are reduced due to the influence of the fumes FU, the temperature image generated based on the ratio of the brightness information of the light with wavelength λ1 to the brightness information of the light with wavelength λ2 is not affected by the thermal radiation light being obstructed by the fumes FU.
[0115] The detection unit 54 may obtain the state of the fumes FU by using the average temperature image data. The average temperature image data is generated in the same manner as described in the process of obtaining the state of the sputter SP. The generation state of the fumes FU (concentration and range on the temperature image data of the fumes FU) differs for each temperature image data. Therefore, even if a fume FU is detected in a temperature image at the same position on a plurality of temperature images, the fume FU is not necessarily detected in a large number of other temperature images. In the average temperature image data generated by averaging these multiple temperature image data, the position affected by the fume FU in the certain temperature image data is added and averaged with the position not affected by the fume FU in the other large number of temperature image data, thereby removing the influence of the fume FU. The average temperature image data from which the fume FU has been removed includes the keyhole KH and the molten pool MP. In this case, the detection unit 54 generates average temperature image data corresponding to the average temperature image similar to that shown in FIG. 6(c).
[0116] The detection unit 54 obtains the difference between the temperature image data (detection target image data) corresponding to the temperature image for detecting the fumes FU shown in FIG. 7(a) and the average temperature image data. As a result, an image in which the keyhole KH and the molten pool MP are removed from the detection target image is generated as shown in FIG. 7(c). The high-temperature areas on this image (image data) are the fumes FU and the spatters SP. Since the spatters SP appear as small grains on the image (image data), the detection unit 54 obtains the range of the fumes FU by excluding these grain-like high-temperature areas on the image data. As a result, the detection unit 54 obtains the diffusion state of the fumes FU, that is, the range of the fumes FU. Since the fumes FU also have heat, the detection unit 54 obtains the temperature of the range of the detected fumes FU from the image data corresponding to the image shown in FIG. 7(c). It is considered that the higher the temperature, the more fumes FU are generated, that is, the higher the concentration of the fumes FU. Therefore, the detection unit 54 obtains the concentration of the fumes FU based on the temperature within the obtained range of the fumes FU. In this case, data relating the temperature and concentration of the fume FU is stored in advance in the memory unit 58, and the detection unit 54 can refer to this data to determine the concentration of the fume FU from the temperature obtained from the image shown in Figure 7(c).
[0117] In the above-mentioned process for determining the state of the spatters SP, the description has been given using FIG. 6 in which the fumes FU are omitted. However, in reality, the fumes FU may be generated, and the image of the fumes FU may be included in the temperature image data. Therefore, the detection unit 54 uses the method described in the process for determining the state of the fumes FU to separate the molten pool MP, the keyhole KH, and the spatters SP from the fumes FU, and removes the fumes FU from the temperature image data (temperature image). The detection unit 54 may determine the state of the spatters SP from the temperature image data (temperature image) from which the fumes FU have been removed, using the method described using FIG. 6. The detection unit 54 may also determine the state of the spatters SP by separating the fumes FU from the spatters SP based on the difference in area from the image data corresponding to the image shown in FIG. 7(c) generated based on the average temperature image data. In this case, an area that can be assumed as the size of the spatters SP is set in advance as a threshold, and the detection unit 54 determines the area larger than this threshold as the fumes FU, and the area smaller than the threshold as the spatters SP.
[0118] The detection unit 54 does not need to obtain the state of the fume FU from the temperature image data obtained by the two-color method. For example, the acquisition unit 310 may use an illumination device and an imaging device (not shown) instead of the imaging device 41, the bifurcating optical system 42, the chromatic aberration correction optical system 43, and the field stop 302. In this case, as an example, in the space between the base plate 311 and the modeling optical system 35, an illumination device is disposed on the +X-direction side and an imaging device is disposed on the -X-direction side with respect to the center of the base plate 311 in FIG. 1. The illumination device and the imaging device are disposed opposite to each other so that the illumination light from the illumination device is received by the imaging device. As an example, the illumination device (not shown) is an existing surface-emitting type LED, and the imaging device (not shown) has the same configuration as the imaging device 41 in FIG. 1.
[0119] Here, when fumes FU are generated in the space between the base plate 311 and the modeling optical system 35 by irradiation with the laser light, the illumination light from the illumination device is scattered by the fumes FU and received by the imaging device. That is, the intensity of the light received through the area where the fumes FU are generated is lower than the intensity of the light received through the area where the fumes FU are not generated. Therefore, the detection unit 54 can find the range where the fumes are generated by comparing the signal intensity of each pixel in the image data generated by the imaging device with a predetermined threshold value. Moreover, the higher the concentration of the fumes FU, the greater the effect of scattering caused by the fumes FU, and the greater the attenuation of the intensity of the illumination light from the illumination device. Therefore, the detection unit 54 can obtain the concentration (concentration distribution) of the fumes FU based on the signal intensity of each pixel in the image data generated by the imaging device.
[0120] The acquisition unit 310 may be configured by arranging pairs of lighting devices and imaging devices (not shown) in different orientations (as an example, lighting devices are arranged on the positive X-direction side and the positive Y-direction side, and imaging devices are arranged on the negative X-direction side and the negative Y-direction side, respectively, with respect to the center of the base plate 311), and the detection unit 54 may determine the spatial range in which fumes FU are generated and the spatial concentration (concentration distribution) based on the signal intensity of each pixel in the image data generated by each imaging device.
[0121] The lighting device (not shown) does not have to be a surface-emitting LED, and any other existing configuration may be used as long as it is capable of emitting surface light in the space where fumes FU may be generated. Also, it is not necessary to emit light from a surface, and an existing point-emitting lighting device may be used. The correlation between the state of the fumes FU and the melting state of the molten pool MP can be found from the correlation between the state of the fumes FU (range and concentration of spatters SP) and the convection C of the molten pool MP, and the correlation between the convection C of the molten pool MP and the melting state of the molten pool MP (information related to temperature). Therefore, the detection unit 54 may (indirectly) determine the melting state of the molten pool MP based on the determined state of the fumes FU. In this case, data related to the correlation between the state of the fumes FU and the melting state of the molten pool MP is stored in advance in the memory unit 58.
[0122] (2) Processing to change modeling conditions When it is necessary to change the modeling conditions based on the state of the detection target area obtained by the detection unit 54 as described above, the calculation unit 56 sets the values of the above-mentioned parameters included in each formula so that at least one of the values of the power density PD, the energy density ED, and the temperature distribution T(r) expressed by the above formulas (1) to (3) is kept within a desired range. A case where it is necessary to change the modeling conditions is a case where there is a possibility that a modeling defect such as insufficient melting, shape abnormality, or failure to obtain desired metal crystals may occur in a three-dimensional modeled object when modeling is performed under the currently set modeling conditions. The determination unit 57 determines whether or not the modeling conditions need to be changed. When the state of the detection target area obtained by the detection unit 54 satisfies a reference range described later, the determination unit 57 determines that the modeling conditions need to be changed.
[0123] The calculation unit 56 generates change information, which is information for changing the modeling conditions so as to achieve the set parameter values. In this embodiment, the following (2-1) to (2-7) are given as examples of the modeling conditions to be changed. (2-1) Conditions of the laser light emitted toward the powder material P of the material layer, i.e., conditions related to the irradiation unit 32 (2-2) Scanning conditions for scanning the material layer with the laser light, i.e., conditions related to the scanning unit 33 (2-3) Conditions related to the atmosphere inside the housing 10 (2-4) Material layer formation conditions for forming a material layer (2-5) Support Conditions Related to the Base Plate 311 of the Modeling Tank 31 (2-6) Design information (design data) regarding the shape of the solidified layer or the three-dimensional object (2-7) Conditions related to powder material P
[0124] Specific examples of the above molding conditions (2-1) to (2-7) are shown below. As an example, Fig. 8 and Fig. 9 show the relationship between the main printing conditions, the basic conditions of power density PD, energy density ED, and temperature distribution T(r), and the parameters shown in Equations (1) to (3). In Fig. 8 and Fig. 9, the basic conditions that can be controlled by each printing condition are indicated by a circle, and the basic conditions that cannot be controlled or have little effect even if controlled are indicated by a blank. Fig. 8 and Fig. 9 also show the parameters of Equations (1) to (3) that are related to each printing condition. As a note, Fig. 8 and Fig. 9 show at what timing each printing condition can be changed: the above-mentioned real-time change, the change during the printing of the next layer, and the change during the printing of the next object.
[0125] (2-1) Conditions related to the irradiation unit 32 Specific examples of modeling conditions related to the conditions of the laser light emitted from the irradiation unit 32 include at least one of the following conditions: the output power [W] of the laser light (laser output), the wavelength [nm] of the laser light, the intensity distribution (profile) of the laser light, and the size [mm] of the light beam of the laser light (spot size), as shown in Figure 8.
[0126] The laser output affects the amount of heat given to the powder material P irradiated with the laser light emitted from the laser oscillator 321, and the higher the laser output, the greater the amount of heat absorbed by the powder material P. The laser output is determined by the above-mentioned parameter P L The modification information is generated in relation to the above-mentioned modeling conditions. As described above, when the laser output is increased, the values of the power density PD, the energy density ED, and the temperature distribution T(r) increase. The modification information for changing the laser output is a new output value of the laser light emitted from the irradiation unit 32, or a correction value for the currently set output value of the laser light.
[0127] The wavelength of the laser light is related to the absorptance of the powder material P to absorb the laser light. It is generally known that the shorter the wavelength of the laser light, the higher the absorptance of the powder material P. That is, the wavelength of the laser light is a molding condition for which change information is generated in relation to the parameter η, and the value of the parameter η decreases as the wavelength of the laser light increases. For this reason, the wavelength of the laser light affects the values of the power density PD and the energy density ED. The change information for changing the wavelength of the laser light is, for example, information indicating which wavelength of the laser light is to be emitted from among the wavelengths that can be emitted as the laser light.
[0128] In the present embodiment, as the intensity distribution (profile) of the laser light, as described above, the laser light having a Gaussian distribution and the laser light having a top hat distribution can be switched. The intensity distribution of the laser light having a Gaussian distribution is strongest near the central axis of the laser light beam and gradually weakens toward the periphery. Compared with the laser light having a Gaussian distribution, the intensity distribution of the laser light having a top hat distribution is uniform even in the peripheral portion away from the central axis of the laser light beam. As a result, in the case of the laser light having a top hat distribution, the laser light having the intensity required to melt the powder material P is irradiated over a wide area on the material layer compared with the laser light having a Gaussian distribution. For this reason, the intensity distribution of the laser light affects the spot size of the laser light on the upper surface of the material layer. That is, the intensity distribution of the laser light is a modeling condition for which change information is generated in relation to the parameter d. When the intensity distribution of the laser light is switched to a top hat distribution, the spot size becomes larger, and the amount of heat flowing into the powder material P per unit area on the material layer due to the irradiation of the laser light decreases. For this reason, when the intensity distribution of the laser light has a top hat distribution, the value of the parameter d increases, and the values of the power density PD and the energy density ED decrease.
[0129] With laser light having a Gaussian distribution, the intensity distribution is strongest near the central axis of the laser light beam, so compared to laser light having a top-hat distribution, the laser light having the intensity required to melt the powder material P is irradiated over a narrower range on the material layer. This reduces the spot size, and increases the amount of heat that flows into the powder material P per unit area on the material layer due to the irradiation of the laser light. For this reason, when the intensity distribution has a Gaussian distribution, the value of the parameter d decreases, and the values of the power density PD and energy density ED increase. The modification information for modifying the intensity distribution of the laser beam is, for example, information indicating whether the laser beam is to be emitted with a Gaussian distribution or a top hat distribution. The intensity distribution of the laser light is determined by the laser quality [M 2 ] is affected. 2 When is 1, the intensity distribution of the laser light is a single-mode Gaussian distribution, and M 2 The more it changes from 1 (M 2 is a value equal to or greater than 1), the intensity distribution of the laser light changes from a single-mode Gaussian distribution. Therefore, the value of the parameter d changes depending on the laser quality.
[0130] The spot size of the laser light affects the range on the XY plane of the material layer irradiated by the laser light. The smaller the spot size of the laser light irradiating the upper surface of the material layer, the more the amount of heat per unit area on the material layer increases, and the more the amount of heat flowing into the powder material P per unit area on the material layer due to the irradiation of the laser light increases. As a result, the melting of the powder material P irradiated by the laser light is promoted, affecting the convection C in the molten pool MP. For this reason, the spot size of the laser light is a molding condition for which change information is generated in relation to the parameter d. When the spot size increases, the parameter d increases, and the amount of heat flowing into the powder material P per unit area on the material layer due to the irradiation of the laser light decreases, so the values of the power density PD and the energy density ED decrease. The spot size affects the value of the temperature distribution T(r). The change information for changing the spot size of the laser light is, for example, the position in the X direction of the concave lens 323a of the focus lens 323, or the amount of movement from the current position of the concave lens 323a. The wavelength of the laser light can be changed when the next object is formed. The other modeling conditions can be changed in real time, when the next layer is formed, or when the next object is formed.
[0131] (2-2) Conditions related to the scanning unit 33 Specific examples of modeling conditions for scanning conditions for scanning a material layer with laser light include at least one of the following: the scanning speed of the laser light [mm / s], the distance (scanning pitch) [mm] between two adjacent irradiation positions of the laser light in a direction intersecting the scanning direction of the laser light, and the scanning path of the laser light. The scanning speed of the laser light is related to the time that the laser light is irradiated per unit area of the surface of the material layer, and affects the amount of heat that flows into the powder material P per unit area of the material layer due to the irradiation of the laser light and the temperature change (temperature gradient) in the molten pool MP due to the movement of the position where the laser light is irradiated. When the scanning speed of the laser light is high, the amount of heat that flows into the powder material P contained in the surface of the material layer per unit area due to the irradiation of the laser light is small. When the scanning speed of the laser light is low, the amount of heat that flows into the powder material P contained in the surface of the material layer per unit area due to the irradiation of the laser light is large. The scanning speed of the laser light is a modeling condition for which change information is generated in relation to the above parameter v. When the scanning speed increases, the parameter v also increases, and the values of the power density PD, the energy density ED, and the temperature distribution T(r) decrease. The change information for changing the scanning speed is, for example, a new change speed of the tilt angle of the galvanometer mirrors 331 and 332, or a correction value of the change speed of the currently set tilt angle.
[0132] When the scanning pitch is small, the influence of heat from the adjacent solidified region BE already formed by the irradiation of the laser light is large. Therefore, the initial temperature of the powder material P not irradiated with the laser light rises, and the amount of heat required to raise the temperature to a desired temperature (e.g., melting point) decreases. In other words, the smaller the scanning pitch, the greater the heat absorption rate of the powder material P, and the greater the scanning pitch, the smaller the heat absorption rate of the powder material P. Also, when the scanning pitch is small, heat from a direction different from the scanning direction of the laser light affects the convection C in the molten pool MP.
[0133] When the scanning pitch is large, the thermal influence from the adjacent solidified region BE already formed by irradiation with the laser light is small, so a larger amount of heat is required to raise the initial temperature of the powder material P that is not irradiated with the laser light to the desired temperature (e.g., the melting point). The scanning pitch is a modeling condition for which modification information is generated in relation to the parameters η and Δy. When the scanning pitch is large, the value of the parameter η is small, the value of the parameter Δy is large, and the value of the energy density ED is small. The scanning pitch affects the values of the power density PD and the temperature distribution T(r). The modification information for changing the scanning pitch is, for example, a new setting angle to be changed from the current setting angle of the galvanometer mirrors 331 and 332, or a correction value for changing from the current setting angle to the new setting angle.
[0134] The scanning path of the laser light is a modeling condition related to a method of setting a path for irradiating the surface of the material layer with the laser light. For example, the scanning path may be irradiated with the laser light along the contour of the shape (modeling model) based on the slice model data, and then irradiated with the laser light inside the contour, or irradiated with the laser light inside the contour of the shape (modeling model) based on the slice model data, and then irradiated with the laser light along the contour of the shape (modeling model) based on the slice model data. The scanning path of the laser light is determined based on the initial temperature T0 of the material layer before the laser light is irradiated, for example, so as to be a path that makes it difficult for residual stress to occur in the solidified layer modeled by the laser light.
[0135] As an example of the scanning path of the laser light, when the laser light is irradiated along the contour of the shape (modeling model) based on the slice model data and then the inside of the contour is irradiated with the laser light as exemplified above, the initial temperature of the powder material P inside the contour rises due to the diffusion of heat from the laser light already irradiated to the contour of the shape (modeling model) based on the slice model data. Therefore, the scanning path of the laser light is a modeling condition for which change information is generated in relation to the parameter P0 depending on the scanning path to be changed, and affects the values of the power density PD, the energy density ED, and the temperature distribution T(r). The change information for changing the scanning path is, for example, information on the new tilt angle value of the galvanometer mirrors 331 and 332 and the timing for setting the tilt angle value. Each of the above-mentioned modeling conditions can be changed in real time, when the next layer is modeled, or when the next object is modeled.
[0136] (2-3) Conditions related to the atmosphere inside the housing 10 As a specific example of the atmosphere inside the housing 10 as the modeling condition, the flow rate [mm 3 / s], the flow rate [mm / s] of the inert gas introduced into the housing 10, and the temperature [° C.] inside the housing 10. In this embodiment, the flow rate and flow velocity of the inert gas affect the initial temperature of the material layer before the laser beam is irradiated and the fumes FU generated from the powder material P due to the laser beam irradiation. For example, when the flow rate and flow velocity of the inert gas are high, the surface of the material layer is cooled by the inert gas, and the amount of heat required to raise the temperature of the powder material P irradiated with the laser beam to a desired temperature (e.g., melting point) increases. Therefore, the flow rate and flow velocity of the inert gas affect the initial temperature of the powder material P before it is irradiated with the laser beam, and are therefore shaping conditions related to the parameter P0.
[0137] Also, for example, when the flow rate or flow speed of the inert gas is low, the fumes FU generated by the irradiation of the laser light remain near the irradiation position of the laser light and block the optical path of the laser light toward the material layer. As a result, the amount of heat flowing into the powder material P due to the irradiation of the laser light may decrease, resulting in a melting state different from the expected melting state. Therefore, the flow rate and flow speed of the inert gas affect the absorption rate when the powder material P absorbs the heat caused by the irradiation of the laser light, and are therefore modeling conditions related to the parameter η. The flow rate and flow speed of the inert gas are modeling conditions for which change information is generated in relation to the parameters P0 and η. For example, when the flow rate of the inert gas increases and the flow speed increases, the value of the parameter P0 decreases, the value of the parameter η increases, and the value of the temperature distribution T(r) decreases. The flow rate and flow speed of the inert gas affect the values of the power density PD and the energy density ED. The change information for changing the flow rate and flow speed of the inert gas is, for example, a new valve opening of the valve that is the intake device 131, a new exhaust volume of the exhaust device 14, or a correction value of the currently set valve opening and exhaust volume.
[0138] The temperature inside the housing 10 affects the initial temperature of the material layer before the laser beam is irradiated, and is a modeling condition for which change information is generated in relation to the parameter P0. The higher the temperature inside the housing 10, the more the powder material P is heated and the higher the initial temperature becomes, so that the amount of heat required for the temperature of the powder material P to rise to a desired temperature (e.g., melting point) by the irradiation of the laser beam becomes smaller. Therefore, the temperature inside the housing 10 affects the initial temperature before the powder material P is irradiated with the laser beam, and is therefore a modeling condition related to the parameter P0. For example, when the temperature inside the housing 10 rises, the value of the parameter P0 increases, and the values of the power density PD, the energy density ED, and the temperature distribution T(r) increase. The change information for changing the temperature inside the housing 10 is, for example, a new heating output value of the heater 15 or a correction value of the currently set heating output of the heater 15.
[0139] The temperature inside the housing 10 can be changed when the temperature is changed during the formation of the next layer or the formation of the next object. The flow rate and flow speed of the inert gas introduced into the housing 10 can be changed in real time, when the temperature is changed during the formation of the next layer, or when the temperature is changed during the formation of the next object.
[0140] (2-4) Material layer formation conditions for forming a material layer Specific examples of molding conditions for forming a material layer include at least one of the following: the moving speed [mm / s] of the blade 221, the pressure [Pa] that the blade 221 applies to the powder material P, the time [s] that the blade 221 waits after molding the solidified layer before starting to form a new material layer on top of the solidified layer, the shape of the blade 221, the material of the blade 221, and the layer thickness [mm] of the material layer on the base plate 311.
[0141] The moving speed of the blade 221 and the pressure applied by the blade 221 to the powder material P affect the flatness of the surface of the material layer to be formed, the lamination thickness, and the density of the material layer. For example, when the moving speed of the blade 221 is fast, the flatness of the surface of the material layer decreases, the lamination thickness increases, and the density decreases compared to when the moving speed of the blade 221 is slow. Also, when the pressure applied by the blade 221 to the powder material P is high, the flatness of the surface of the material layer increases, the lamination thickness decreases, and the density increases compared to when the pressure is low. Therefore, the moving speed of the blade 221 is a modeling condition that affects the parameters Δz, ρ, k, and α, and for example, when the moving speed of the blade 221 is changed, the values of the energy density ED and the temperature distribution T(r) are affected. The pressure applied by the blade 221 to the powder material P is a modeling condition for which change information is generated in relation to the parameters Δz, ρ, k, and α. For example, when the pressure increases, the values of the parameters ρ, k, and α increase, the value of the parameter Δz decreases, and the values of the energy density ED and the temperature distribution T(r) increase. The change information for changing the moving speed of the blade 221 is a new value of the motor output of a driving mechanism for moving the blade 221 or a currently set correction value of the motor output. The change information for changing the pressure applied to the powder material P by the blade 221 may be, for example, a new value of the driving amount of the pressing mechanism or a currently set correction value of the driving amount of the pressing mechanism.
[0142] As described above, the waiting time of the blade 221 is the time from when the irradiation of the laser light on the material layer for forming the solidified layer is completed until the blade 221 starts transferring the powder material P from the material supply tank 21 to the modeling tank 31. The waiting time of the blade 221 affects the initial temperature of the material layer newly formed on the solidified layer. That is, the longer the waiting time, the lower the temperature of the solidified layer raised by the irradiation of the laser light, so that the initial temperature of the material layer newly formed on the upper part of the solidified layer becomes difficult to rise. In this case, the amount of heat required to raise the temperature of the powder material P irradiated with the laser light to a desired temperature (for example, the melting point) becomes large. Therefore, the waiting time of the blade 221 is a modeling condition for which change information is generated in relation to the parameter P0. For example, when the waiting time becomes long, the value of the parameter P0 becomes small, and the values of the power density PD, the energy density ED, and the temperature distribution T(r) decrease. The change information for changing the waiting time of the blade 221 is, for example, a value indicating the timing at which the motor constituting the drive mechanism for moving the blade 221 starts to drive, or a correction value for the currently set timing at which the motor starts to drive.
[0143] For example, if the blade 221 has a defect, the thickness of the material layer will not be constant depending on the shape of the defect, and the flatness will decrease, the lamination thickness will differ from the desired thickness, the density in the material layer will not be uniform, or the planar roughness will increase. Even if the blade 221 has no defect, if the shape of the blade 221 changes, the contact area of the blade 221 with the powder material P will change, and the density, flatness, and lamination thickness of the material layer will change depending on the shape. Depending on the characteristics of the material of the blade 221 and the material (type) of the powder material P, friction and other factors may cause the movement of the blade 221 to be hindered, and the powder material P may not be transferred uniformly onto the base plate 311 or the solidified layer, resulting in a decrease in the flatness of the material layer that is formed, a difference in the lamination thickness from the desired thickness, a decrease in uniformity of the density in the material layer, or an increase in planar roughness. Therefore, the shape and material of the blade 221 are shaping conditions that affect the parameters Δz, ρ, k, and α, and when the shape and material of the blade 221 are changed, the values of the energy density ED and the temperature distribution T(r) are affected.
[0144] The shape and material of the blade 221 can be changed by changing the type of the blade 221. In this case, the change information for changing the shape and material of the blade 221 is, for example, information indicating replacement of the blade 221. In this case, the modeling apparatus 1 issues a notification to encourage replacement of the blade 221, for example. As a method of notification, the modeling apparatus 1 may display a message on a monitor (not shown) informing that the type of inert gas needs to be changed, or may emit a sound from a speaker (not shown). In addition, when the blade 211 has a configuration that allows automatic replacement between a plurality of types, the type of the blade 211 is automatically replaced according to control from the material control unit 51. In addition, when the above-mentioned blade 221 has a variable shape, the shape of the blade 221 can be changed according to control from the material control unit 51. The change information generated in this case is, for example, information instructing a change in the shape of the blade 221.
[0145] When the lamination thickness of the material layer is large, the amount of heat generated by the irradiation of the laser light does not sufficiently reach the surface (lower surface) of the material layer in the negative Z direction, which may cause defective molding such as insufficient melting. The lamination thickness is a molding condition for which change information is generated in relation to the parameter Δz. For example, as the lamination thickness increases, the value of the parameter Δz increases and the value of the energy density ED decreases. The change information for changing the lamination thickness may be, for example, the above-mentioned new pressure value that the blade 221 of the recoater 22 applies to the powder material P or a correction value for the current pressure, or may be a new value of the drive amount of the pressing mechanism of the blade 221 or a correction value for the currently set drive amount of the pressing mechanism. The shape and material of the blade 221 can be changed when forming the next object. The moving speed of the blade 221, the pressure applied to the powder material P, the waiting time, and the layer thickness of the material layer can be changed when forming the next layer or the next object.
[0146] (2-5) Support Conditions Related to the Base Plate 311 of the Modeling Tank 31 The modeling conditions related to the base plate 311 of the modeling tank 31 include the temperature [° C.] of the base plate 311 . The temperature of the base plate 311 affects the initial temperature of the material layer formed on the upper part, and the higher the temperature of the base plate 311, the warmer the powder material P is. Therefore, the higher the temperature of the base plate 311, the higher the initial temperature of the powder material P. In this case, the amount of heat required to raise the temperature of the powder material P irradiated with the laser light to a desired temperature (for example, the melting point) is reduced. Therefore, the temperature of the base plate 311 is a modeling condition for which change information is generated in relation to the parameter P0. When the temperature of the base plate 311 is high, the value of the parameter P0 increases, and the values of the power density PD, the energy density ED, and the temperature distribution T(r) increase. The change information for changing the temperature of the base plate 311 is, for example, a new heating output value of the heater 313 or a correction value of the currently set heating output of the heater 313.
[0147] In addition, when the temperature of the base plate 311 is high, the amount of temperature drop when the temperature of the solidified layer increased by the irradiation of the laser light decreases is small, so the effect of the residual stress generated when the molten pool MP solidifies is reduced. Also, as described above, when the temperature of the base plate 311 is high, the amount of heat required to raise the temperature of the powder material P irradiated with the laser light to a desired temperature is small, so that the scanning speed can be increased without changing the output of the laser light. The temperature of the base plate 311 can be changed when the next layer is formed or when the next object is formed.
[0148] (2-6) Design data related to the shape of the solidified layer or the three-dimensional object A specific example of a case where design data related to the shape of the solidified layer or the three-dimensional object is used as a modeling condition is at least one of slice model data, which is shape data of the solidified layer to be modeled, and shape data of a support part that supports the solidified layer or the three-dimensional object.
[0149] The slice model data is shape data for determining the shape of the solidified layer on the XY plane to be formed, the thickness of the solidified layer (slice pitch), etc. The slice model data is a forming condition for which change information is generated in relation to the parameter Δz. That is, as the thickness of the solidified layer increases, the value of the parameter Δz increases. When the slice model data, which is shape data, is changed, various forming conditions of the laser light from the irradiation unit 32 and various forming conditions for scanning by the scanning unit 33 may be changed, so the slice model data affects the values of the power density PD, the energy density ED, and the temperature distribution T(r). The change information for changing the slice model data is, for example, a new shape or a new thickness of the solidified layer on the XY plane, or a correction value of the shape or the thickness of the solidified layer on the XY plane.
[0150] As described above, the shape data of the support part indicates the shape of the thickness, length, etc. of the support part that supports the three-dimensional object to prevent deformation or damage between solidified layers or the three-dimensional object. The shape of the support part is determined by the shape, size, etc. of the solidified layer and the three-dimensional object that it supports. The larger the volume of the support part, the greater the effect that the heat of the part of the solidified layer that is shaped as the support part by irradiation with the laser light has on the material layer (powder material P) formed on the solidified layer. In addition, the higher the initial temperature of the powder material P heated by the base plate 311, the greater the amount of heat transferred from the base plate 311 to the material layer (powder material P) through the part of the solidified layer that is shaped as the support part. For this reason, the shape data of the support part is a shaping condition that affects the parameter P0 depending on the volume of the support part and the temperature of the base plate 311, and affects the values of the energy density ED and the temperature distribution T(r). The change information for changing the shape data of the support part is, for example, a value of the new shape (length, thickness, etc.) of the support part, or a correction value of the current shape (length, thickness, etc.) of the support part. The slice model data and the shape data of the supporting members can be corrected when they are changed during the formation of the next object.
[0151] (2-7) Conditions related to powder material P Specific examples of the molding conditions related to the powder material P include at least one of the particle size and particle size distribution of the powder material P, the moisture absorption of the powder material P, and the type of the powder material P. The variation in the particle size and particle size distribution of the powder material P in the material layer may affect the thermal diffusivity and thermal conductivity of the material layer irradiated with the laser light, which may cause poor melting. In addition, when the powder material P with a variation in the particle size and particle size distribution is transferred to the modeling tank 31 by the blade 221, the thickness and density may vary in the material layer, which may result in defects such as voids in the solidified layer to be modeled. The particle size and particle size distribution are modeling conditions for which change information is generated in relation to the parameters Δz, ρ, k, and α. For example, when the particle size and particle size distribution become larger (the variation becomes larger), the value of the parameter Δz becomes larger, the values of the parameters ρ, k, and α become smaller, and the values of the energy density ED and the temperature distribution T(r) increase. The change information for changing the particle size and particle size distribution of the powder material P is, for example, information instructing the removal of the formed material layer and the formation of a new material layer.
[0152] A powder material P with high moisture absorption has low fluidity and is difficult to be smoothly transferred to the modeling tank 31 by the blade 221. For this reason, the flatness and lamination thickness of the formed material layer are difficult to be uniform, and the surface roughness is likely to be large. That is, the moisture absorption of the powder material P is a modeling condition that affects the parameter Δz. In addition, if the moisture absorption of the powder material P is high, the flatness, lamination thickness, and density of the material layer are difficult to be uniform, so the temperature rise due to the irradiation of the laser light is not uniform, and defects such as voids in the solidified layer formed due to poor melting may occur. Furthermore, since the powder material P with high moisture absorption has low thermal conductivity and thermal diffusivity, defects such as voids in the solidified layer formed due to poor melting may occur. Therefore, the moisture absorption of the powder material P is a modeling condition for which change information is generated in relation to the parameters k and α. For example, if the moisture absorption of the powder material P is high, the values of the parameters k and α decrease, and the value of the temperature distribution T(r) decreases. In addition, the moisture absorption of the powder material P affects the values of the power density PD and the energy density ED. The change information for changing the moisture absorption includes, for example, information indicating that the powder material P needs to be heated by the heater 213 and the value of the heating output of the heater 213.
[0153] There are different types of powder materials P, each having different powder materials and additives. Different types of powder materials P have different powder particle sizes, thermal conductivity, thermal diffusivity, and the like. In addition, even if the same pressure is applied to powder materials P of different particle sizes by the blade 221 when forming a material layer, when a powder material P with a large particle size is used, the gap between the particles in the material layer is larger than when a powder material P with a small particle size is used, so that the layer thickness of the material layer increases and the density decreases. For this reason, the type of powder material P is a modeling condition that affects the parameters Δz, ρ, k, and α, and affects the energy density ED and the temperature distribution T(r). The change information for changing the type of powder material P is, for example, information indicating that a different type of powder material P is used. In this case, the modeling apparatus 1 notifies the user to, for example, replace the powder material P. As a method of notifying, the modeling apparatus 1 may display a message on a monitor (not shown) informing that the type of powder material P needs to be changed, or may emit a sound from a speaker (not shown). In addition, when a different type of powder material P is stored in each of the multiple material supply tanks 21 and the multiple material supply tanks 21 are configured to be automatically replaceable, the type of powder material P is automatically replaced by replacing the material supply tank 21 in accordance with the control of the material control unit 51.
[0154] The particle size, particle size distribution, and type of the powder material P can be changed when the powder material P is changed during the formation of the next object. The moisture absorption of the powder material P can be corrected when the powder material P is changed during the formation of the next layer or the next object. In the description using the above-mentioned Figures 8 and 9, the parameters that are particularly related to each of the printing conditions included in the above (2-1) to (2-7) and change significantly when the printing conditions are changed are exemplified as related parameters. However, when each printing condition is changed, parameters other than the above-exemplified parameters among the parameters included in the above formulas (1) to (3) are also affected. Therefore, taking into account the change of parameters other than the above-exemplified parameters, change information for changing the printing conditions so that at least one of the power density PD, the energy density ED, and the temperature distribution T(r) is within a desired range may be generated.
[0155] In this embodiment, in addition to the above-described modeling conditions (2-1) to (2-8), the modeling conditions may include other existing modeling conditions in the modeling apparatus 1. The other modeling conditions include the oscillation mode of the laser light from the irradiation unit 32, the polarization state of the laser light, the type of inert gas, the oxygen concentration in the casing 10, the pressure [Pa] in the casing 10, the type of base plate 311, modeling posture data, shape data of the three-dimensional object, and the oxygen concentration of the powder material P.
[0156] As described above, in this embodiment, the oscillation mode of the laser light can be switched between CW (continuous wave) oscillation and pulse oscillation. In the case of pulse oscillation, the on time is shorter than that of CW oscillation, so the amount of heat absorbed by the powder material P at the position irradiated with the laser light is smaller than that of CW oscillation. For this reason, the amount of heat flowing into the powder material P varies depending on the oscillation mode, which affects the melting of the powder material P, and is known to affect in particular the depth of the keyhole KH and the width of the solidified region BH. That is, the oscillation mode affects the values of the power density PD, the energy density ED, and the temperature distribution T(r). The change information for changing the oscillation mode of the laser light is, for example, information indicating in which mode, CW (continuous wave) oscillation or pulse oscillation, the laser light is emitted. The oscillation mode of the laser light can be changed in any of the following cases: real-time change, change during the formation of the next layer, and change during the formation of the next object.
[0157] The polarization state of the laser light includes, for example, circular polarization and linear polarization. When the powder material P is a metal material, the absorption of the laser light is affected by the polarization state of the laser light. That is, the polarization state of the laser light affects the amount of heat flowing into the powder material P irradiated with the laser light. For this reason, the polarization state of the laser light is a modeling condition that affects at least one of the values of the power density PD, the energy density ED, and the temperature distribution T(r). The change information for changing the polarization state of the laser light is, for example, information indicating which polarization state is to be set among the polarization states (for example, circular polarization, linear polarization, etc.) that can be set for the laser light emitted from the irradiation unit 32. The polarization state of the laser light can be changed when changing the polarization state during modeling of the next object.
[0158] The type of inert gas can be selected from, for example, nitrogen, argon, and the like. The type of inert gas is a modeling condition selected according to the type of powder material P. For example, when the powder material P is titanium, if nitrogen is used as the inert gas, the powder material P will react with the nitrogen, so argon is preferably used as the inert gas. In this way, if an appropriate inert gas is not selected for the type of powder material P, the powder material P will react with the inert gas, which will affect the values of the power density PD, the energy density ED, and the temperature distribution T(r). The change information for changing the type of inert gas is information indicating that a different type of inert gas is to be used. In this case, the modeling apparatus 1 issues a notice to the user to encourage the user to change the inert gas, for example. As a method of notice, the modeling apparatus 1 may display a message on a monitor (not shown) informing the user that the type of inert gas needs to be changed, or may emit a sound from a speaker (not shown). The type of inert gas can be changed by changing the tank 13. Furthermore, in the case where the multiple tanks 13 each contain a different type of inert gas and the multiple tanks 13 are configured to be automatically replaceable, the type of inert gas is automatically replaced by replacing the tank 13 under the control of the housing control unit 53. The type of inert gas can be changed when the next object is formed.
[0159] The oxygen concentration in the housing 10 is a modeling condition for setting the concentration so as not to oxidize the material layer during melting and solidification. As described above, an oxide film is formed on the surface of the oxidized powder material P, and the specific heat changes depending on the thickness of the oxide film, which affects the heat absorption and heat conduction of the powder material P. For this reason, the oxygen concentration in the housing 10 is a modeling condition that affects the values of the energy density ED and the temperature distribution T(r). The change information for changing the oxygen concentration in the housing 10 is, for example, a new valve opening of the valve that is the intake device 131, a new exhaust volume of the exhaust device 14, or a correction value of the currently set valve opening and exhaust volume. The oxygen concentration in the housing 10 can be changed when changing the next layer modeling or when changing the next object modeling.
[0160] Since the formation of a three-dimensional object is performed with the inside of the housing 10 kept at a predetermined pressure, the pressure inside the housing 10 is controlled as a forming condition. The pressure inside the housing 10 affects the surface tension of the molten pool MP. As described above, the convection C in the molten pool MP occurs due to the difference in surface tension between the surface and the inside of the molten pool MP, so the pressure inside the housing 10 is a forming condition that affects the convection C of the molten pool MP. Since the convection C affects the temperature distribution in the molten pool MP, the pressure inside the housing 10 is a forming condition that affects the temperature distribution T(r). The change information for changing the pressure inside the housing 10 is, for example, a new exhaust volume of the exhaust device 14, or a correction value of the currently set exhaust volume. The pressure inside the housing 10 can be changed when changing the pressure when forming the next layer or the next object.
[0161] The modeling posture data is data indicating the modeling posture of the solidified layer or the three-dimensional object as described above, and is used when setting slice model data. When the modeling posture is changed, various modeling conditions of the laser light from the irradiation unit 32 and various modeling conditions for scanning by the scanning unit 33 may be changed. For this reason, the modeling posture data affects the values of the power density PD, the energy density ED, and the temperature distribution T(r). The change information generated for the modeling posture data is, for example, information indicating the slice direction when a new modeling posture is set. The modeling posture data can be changed when changing the modeling of the next object.
[0162] The shape data of the three-dimensional object is design data (i.e., CAD data or STL data). Therefore, the shape data of the three-dimensional object is a modeling condition that, when changed, may change various modeling conditions of the laser light from the irradiation unit 32 and various modeling conditions for scanning by the scanning unit 33. Therefore, the shape data of the three-dimensional object affects the values of the power density PD, the energy density ED, and the temperature distribution T(r). Change information for changing the shape data of the three-dimensional object is, for example, a value indicating a new shape of the three-dimensional object, or a correction value for the current shape of the three-dimensional object. The shape data of the three-dimensional object can be corrected when changing during modeling of the next object.
[0163] As described above, in this embodiment, the base plate 311 is configured to be able to be attached by selecting from a plurality of types having different thicknesses and materials. The type of base plate 311 is a modeling condition for selecting a base plate 311 having the rigidity (thickness and material) required to prevent the solidified layer from being deformed due to the residual stress generated when the molten pool MP solidifies and to maintain the shape of the solidified layer. Since the residual stress occurs according to the temperature change until the molten powder material P solidifies, the type of base plate 311 for suppressing the occurrence of the residual stress is a modeling condition related to the temperature distribution T(r). The base plate 311 can be changed when forming the next object. The change information for changing the type of the base plate 311 is, for example, information indicating that a different type of base plate 311 is used. In this case, the modeling apparatus 1 notifies the user to, for example, replace the base plate 311. As a method of notifying, the modeling apparatus 1 may display a message on a monitor (not shown) informing that the type of the base plate 311 needs to be changed, or may emit a sound from a speaker (not shown). In addition, in the case where the base plate 311 has a configuration that allows automatic exchange between a plurality of types, the type of the base plate 311 is automatically exchanged according to the control from the formation control unit 52.
[0164] When the powder material P oxidizes, an oxide film is formed on the surface of the powder material P as described above, and the specific heat changes depending on the thickness of the oxide film. The oxide film of the powder material P affects the thermal conduction of the powder material P and may cause poor melting, etc. For this reason, the oxygen concentration of the powder material P becomes a molding condition and affects the value of the energy density ED. The change information generated for the oxygen concentration of the powder material P includes, for example, information indicating that the powder material P needs to be heated by the heater 213 and the heating output value of the heater 213. The oxygen concentration of the powder material P can be changed when changing the molding time of the next object.
[0165] Next, a description will be given of a specific example of the change information generated by the calculation unit 56. In the following description, a case will be taken as an example in which the calculation unit 56 generates the change information in order to keep at least one of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range.
[0166] Based on the state of the detection target area obtained by the detection unit 54, a parameter P L The case where the parameter P is changed is explained below. L In order to increase the parameter P, that is, to increase the value of the power density PD, the energy density ED, or the temperature distribution T(r), the calculation unit 56 generates modification information to increase the laser output of the laser light from the irradiation unit 32, for example. L In order to reduce the power density PD, the energy density ED, or the temperature distribution T(r), the calculation unit 56 generates change information to reduce the laser output of the laser light from the irradiation unit 32. The change information generated in this case is the output value of the laser light emitted from the irradiation unit 32. The output unit 55 outputs the generated change information to the modeling control unit 52 of the setting unit 59 as state information. The modeling control unit 52, for example, changes the set output value of the laser light to the output value indicated by the change information, and causes the irradiation unit 32 to emit the laser light at the changed output value. Parameter P L The data correlating the value of and the laser output is stored in advance in the storage unit 58. The calculation unit 56 calculates the parameter P LThe value of the laser output corresponding to the desired value is read out as the new laser output value, and the read out new laser output value is generated as the change information.
[0167] A case where the parameter P0 is changed based on the state of the detection target area obtained by the detection unit 54 will be described. When the parameter P0 is increased, that is, when the value of the power density PD, the energy density ED, or the temperature distribution T(r) is increased, the calculation unit 56 generates change information so that at least one of the following changes in the printing conditions is performed. In this case, the changes in the printing conditions include, for example, a decrease in the flow rate and a decrease in the flow speed of the inert gas, an increase in the temperature inside the housing 10, a shortening of the standby time of the blade 221, and an increase in the temperature of the base plate 311. When the parameter P0 is decreased, that is, when the value of the power density PD, the energy density ED, or the temperature distribution T(r) is decreased, the calculation unit 56 generates change information so that at least one of the following changes in the printing conditions is performed. In this case, the changes in the printing conditions include, for example, an increase in the flow rate and an increase in the flow speed of the inert gas, a decrease in the temperature inside the housing 10, an extension of the standby time of the blade 221, and a decrease in the temperature of the base plate 311.
[0168] When change information for changing the flow rate and flow speed of the inert gas is generated, the output unit 55 outputs the generated change information as state information to the housing control unit 53 of the setting unit 59. The housing control unit 53 changes, for example, the set valve opening of the intake device 131 and the exhaust volume of the exhaust device 14 to the valve opening and exhaust volume indicated in the change information, and operates the intake device 131 and the exhaust device 14 with the changed valve opening and exhaust volume. When change information for changing the temperature inside the housing 10 is generated, the output unit 55 outputs the generated change information as status information to the housing control unit 53. The housing control unit 53, for example, changes the set heating output of the heater 15 to the heating output indicated by the change information, and operates the heater 15 at the changed heating output.
[0169] When change information for changing the waiting time of the blade 221 is generated, the output unit 55 outputs the generated change information as status information to the material control unit 51 of the setting unit 59. The material control unit 51 changes the set waiting time to the waiting time indicated by the change information, for example, and moves the blade 221 at the changed waiting time. When change information for changing the temperature of the base plate 311 is generated, the output unit 55 outputs the generated change information as state information to the modeling control unit 52 of the setting unit 59. The modeling control unit 52 changes the set heating output of the heater 313 to the heating output indicated by the change information, and operates the heater 313 with the changed heating output.
[0170] Data in which the value of the parameter P0, the flow rate and flow speed of the inert gas, the temperature inside the housing 10, the waiting time of the blade 221, and the temperature of the base plate 311 are associated with each other is stored in advance in the storage unit 58. The calculation unit 56 reads out the values of each modeling condition corresponding to desired values as the parameter values from this data, and generates the read new values as change information. In addition, since parameter P0 is also affected by the scanning path of the laser light, the volume of the support part, and the shape of the support part (thickness, length, etc.) depending on the temperature of the base plate 311, the calculation unit 56 may generate change information for the scanning path of the laser light and the shape data of the support part.
[0171] A case will be described where the parameter η is changed based on the state of the detection target area obtained by the detection unit 54. When the parameter η is increased, that is, when the value of the temperature distribution T(r) is decreased or the value of the energy density ED is increased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include changing the wavelength of the laser light to a shorter wavelength, decreasing the scanning pitch, increasing the flow rate of the inert gas, and increasing the flow velocity of the inert gas. On the other hand, when the parameter η is decreased, that is, when the value of the temperature distribution T(r) is increased or the value of the energy density ED is decreased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include changing the wavelength of the laser light to a longer wavelength, increasing the scanning pitch, and decreasing the flow rate and flow speed of the inert gas.
[0172] The change information of the wavelength of the laser light is output to the modeling control unit 52 by the output unit 55. The modeling control unit 52 changes, for example, the set wavelength of the laser light to the wavelength indicated by the change information, and causes the irradiation unit 32 to emit the laser light at the changed wavelength. When change information for changing the wavelength of the laser light is generated, the output unit 55 outputs the generated change information as state information to the modeling control unit 52 of the setting unit 59. The modeling control unit 52 changes the set wavelength of the laser light to the wavelength indicated by the change information, and causes the irradiation unit 32 to emit the laser light at the changed wavelength. When modification information for changing the scanning pitch is generated, the output unit 55 outputs the generated modification information as state information to the modeling control unit 52 of the setting unit 59. The modeling control unit 52 changes, for example, the current setting angles of the galvano mirrors 331 and 332 to new setting angles indicated by the modification information, and operates the scanning unit 33 at the changed setting angle. When change information for changing the flow rate and flow speed of the inert gas is generated, similarly to the above-mentioned case, the output unit 55 outputs the state information to the housing control unit 53 of the setting unit 59. The housing control unit 53 operates the intake device 131 and the exhaust device 14, for example, with the valve opening degree and exhaust amount changed based on the change information. Data in which the value of the parameter η, the scanning pitch, and the flow rate and flow speed of the inert gas are associated with each other is stored in advance in the storage unit 58. The calculation unit 56 reads out the values of each modeling condition corresponding to the desired values as the parameters from this data, and generates the read new values as change information.
[0173] A case where the parameter d is changed based on the state of the detection target area obtained by the detection unit 54 will be described. When the parameter d is increased, that is, when the values of the power density PD and the energy density ED are decreased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include changing the intensity distribution of the laser light to a top hat distribution and increasing the spot size of the laser light. When the parameter d is decreased, that is, when the values of the power density PD and the energy density ED are increased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include changing the intensity distribution of the laser light to a Gaussian distribution and reducing the spot size of the laser light.
[0174] When the modification information for changing the intensity distribution of the laser light is generated, the output unit 55 outputs the generated modification information as state information to the modeling control unit 52 of the setting unit 59. The modeling control unit 52, for example, changes the set intensity distribution of the laser light to the intensity distribution indicated by the modification information, and causes the irradiation unit 32 to emit the laser light with the changed intensity distribution. When modification information for changing the spot size is generated, the output unit 55 outputs the generated modification information as state information to the forming control unit 52 of the setting unit 59. The forming control unit 52 controls, for example, a driving mechanism (not shown) to move the concave lens 323a to the position in the X direction indicated by the modification information. Data in which the parameter d is associated with the intensity distribution and spot size of the laser light is pre-stored in the storage unit 58. The calculation unit 56 reads out values of each modeling condition corresponding to a desired value as a parameter from this data, and generates the read new value as change information. When changing the parameter d, the calculation unit 56 may generate change information regarding the divergence angle of the laser light, which affects the intensity distribution of the laser light.
[0175] A case will be described where the parameter v is changed based on the state of the detection target region obtained by the detection unit 54. When the parameter v is increased, i.e., when the values of the power density PD, the energy density ED, and the temperature distribution T(r) are decreased, the calculation unit 56 generates modification information to, for example, increase the scanning speed of the laser light. When the parameter v is decreased, i.e., when the values of the power density PD, the energy density ED, and the temperature distribution T(r) are increased, the calculation unit 56 generates modification information to, for example, decrease the scanning speed of the laser light.
[0176] When modification information for changing the scanning speed of the laser light is generated, the output unit 55 outputs the generated modification information as state information to the modeling control unit 52 of the setting unit 59. The modeling control unit 52 changes, for example, the value of the set value of the change speed of the tilt angle of the galvanometer mirrors 331 and 332 to the change speed of the tilt angle indicated by the modification information, and operates the scanning unit 33 at the change speed of the changed tilt angle. Data in which the parameter v is associated with the scanning speed of the laser beam is stored in advance in the storage unit 58. The calculation unit 56 reads out the value of the scanning speed corresponding to a desired value of the parameter v from this data, and generates a new scanning speed of the laser beam as change information.
[0177] A case where the parameter Δy is changed based on the state of the detection target area obtained by the detection unit 54 will be described. When the parameter Δy is increased, that is, when the value of the energy density ED is decreased, the calculation unit 56 generates modification information so that the scanning pitch is increased. When the parameter Δy is decreased, that is, when the value of the energy density ED is increased, the calculation unit 56 generates modification information so that the scanning pitch is decreased. As described above, the generated modification information is output by the output unit 55 to the modeling control unit 52 of the setting unit 59 as state information. The modeling control unit 52 changes the setting angle to a new setting angle indicated by the modification information, for example, and operates the scanning unit 33 at the changed setting angle. Data associating the parameter Δy with the scanning pitch is pre-stored in the storage unit 58. The calculation unit 56 reads out the value of the scanning pitch corresponding to the desired value of the parameter Δy from this data, and generates a new scanning pitch as change information.
[0178] A case where the parameter Δz is changed based on the state of the detection target region obtained by the detection unit 54 will be described. When the parameter Δz is increased, that is, when the value of the energy density ED or the temperature distribution T(r) is decreased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include decreasing the pressure applied by the blade 221 to the powder material P to increase the layer thickness, increasing the particle size and particle size distribution to increase the variation in particle size, and increasing the thickness of the slice model data, which is the shape data of the solidified layer. This makes it difficult for the heat caused by the irradiation of the laser light to be transmitted to the powder material P. When the parameter Δz is decreased, that is, when the value of the energy density ED or the temperature distribution T(r) is increased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include increasing the pressure applied by the blade 221 to the powder material P to decrease the layer thickness, decreasing the particle size and particle size distribution to decrease the variation in particle size, and decreasing the thickness of the slice model data. This allows the heat generated by the irradiation of the laser light to be easily transferred to the powder material P.
[0179] When change information for changing the pressure that the blade 221 applies to the powder material P is generated, the output unit 55 outputs the generated change information as state information to the material control unit 51 of the setting unit 59. The material control unit 51 controls, for example, the pressing mechanism of the blade 221 to cause the blade 221 to apply a pressure based on the change information to the powder material P. When change information for changing the particle size and particle size distribution is generated, the output unit 55 outputs the generated change information as state information to the material control unit 51 and the modeling control unit 52 of the setting unit 59. The material control unit 51 and the modeling control unit 52 control, for example, the recoater 22, the driving mechanism 212, and the driving mechanism 312 to perform operations for removing the formed material layer and forming a new material layer.
[0180] When modification information for modifying the slice model data, which is the shape data of the solidified layer, is generated, the output unit 55 outputs the generated modification information as state information to the modeling control unit 52 of the setting unit 59. The modeling control unit 52 changes the values of the modeling conditions for the irradiation unit 32 to emit the laser light, the values of the modeling conditions for the scanning unit 33 to scan the laser light, and the movement amount of the drive mechanism 312 so that a solidified layer having a new thickness based on the modification information can be modeled. In this case, data in which the thickness of the solidified layer to be modeled is associated with the values of the modeling conditions for the irradiation unit 32 to emit the laser light and the modeling conditions for the scanning unit 33 to scan the laser light is stored in the storage unit 58. The modeling control unit 52 operates the irradiation unit 32 and the scanning unit 33 under modeling conditions suitable for the thickness of the new solidified layer by referring to this data.
[0181] Data in which the parameter Δz, the pressure applied to the powder material P, the particle size, particle size distribution, and the thickness of the slice model data are associated with each other is pre-stored in the storage unit 58. The calculation unit 56 reads out the values of each modeling condition corresponding to a desired value as the parameter Δz from this data, and generates the read-out new values as change information. In addition, since the parameter Δz is also affected by the moving speed of the blade 221, the type (shape and material) of the blade 221, the moisture absorption of the powder material P, and the type of powder material P, the calculation unit 56 may generate change information for each of the above. In addition, since Δz can also be changed by changing the amount of movement of the base plate 311 in the Z direction, the calculation unit 56 may generate change information based on the drive amount of the drive mechanism 312 for moving the base plate 311.
[0182] A case where the parameters ρ, k, and α are changed based on the state of the detection target region obtained by the detection unit 54 will be described. When the parameters ρ, k, and α are increased, that is, when the values of the energy density ED and the temperature distribution T(r) are increased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include increasing the pressure applied by the blade 221 to the powder material P and decreasing the particle size and particle size distribution to reduce the particle size variation. This increases the density of the powder material P, and increases the thermal conductivity and thermal diffusivity of the powder material P. As a result, the heat generated by the irradiation of the laser light is easily conducted through the material layer. When the parameters ρ, k, and α are decreased, that is, when the values of the energy density ED and the temperature distribution T(r) are decreased, the calculation unit 56 generates change information so that, for example, at least one of the following changes in the modeling conditions is performed. In this case, the changes in the modeling conditions include decreasing the pressure applied by the blade 221 to the powder material P and increasing the particle size and particle size distribution to increase the particle size variation. This reduces the density of the powder material P, and reduces the thermal conductivity and thermal diffusivity of the powder material P. As a result, the heat generated by the irradiation of the laser light is less likely to be conducted through the material layer.
[0183] Data in which the parameters ρ, k, and α are associated with the pressure applied to the powder material P and the particle size and particle size distribution is pre-stored in the storage unit 58. The calculation unit 56 reads out the values of each modeling condition corresponding to the desired values as the values of each parameter from this data, and generates the read new values as change information. In addition, since the parameters ρ, k, and α are also affected by the moving speed of the blade 221, the type (shape and material) of the blade 221, and the type of powder material P, the calculation unit 56 may generate change information for each of the above. The parameters k and α are also affected by the moisture absorption of the powder material P. When the parameters k and α are increased, that is, when the value of the temperature distribution T(r) is increased, the calculation unit 56 reduces the moisture absorption.
[0184] When the calculation unit 56 generates the change information as described above, the output unit 55 outputs the generated change information as state information to the material control unit 51, the modeling control unit 52, and the housing control unit 53 of the setting unit 59 according to the content of the modeling conditions to be changed. The material control unit 51 controls, for example, the operation of the material layer forming unit 20, that is, the operation of the driving mechanism 212 that drives the bottom surface 211 of the material supply tank 21, the operation of the blade 221 (the moving speed of the blade 221, the pressure that the blade 221 applies to the powder material P, and the standby time of the blade 221), and the heating temperature by the heater 213 that heats the powder material contained in the material supply tank 21. In addition, for example, the modeling control unit 52 controls the operations of the irradiation unit 32, the scanning unit 33, and the base plate 311, and the operation of the driving mechanism 312 that drives the heater 313 according to the content of the change information, thereby changing the design data. Furthermore, for example, the housing control unit 53 controls the operation of the heater 15, the intake device 131, and the exhaust device 14 in accordance with the change information, thereby controlling the atmosphere inside the housing 10. The calculation unit 56 may set a correction value, which is a difference between the new value of each generated modeling condition and the current value of the modeling condition, as the change information. In this case, the output unit 55 outputs the change information generated by the calculation unit 56 to the setting unit 59 as state information. The material control unit 51, the modeling control unit 52, and the housing control unit 53 use the input state information as a correction value for correcting the modeling conditions to control the operation of each unit.
[0185] Next, a description will be given of an example of a specific example of the processing performed by the detection unit 54 and the calculation unit 56 in the case of real-time change and the case of change during formation of the next layer. First, a specific example of the process when real-time change is performed will be described. In the following description, a case where the detection unit 54 determines the state of the powder material P before heating as the state of the detection target area and a case where the detection unit 54 determines the molten state will be described as examples. First, as an example of processing during real-time change, the detection unit 54 obtains information on the temperature of the powder material P (i.e., the vicinity of the molten pool MP) that has not yet started to melt before being heated by the irradiation of the laser light as the state of the detection target area, and the calculation unit 56 generates change information so as to keep the value of the energy density ED within a desired range. Note that the calculation unit 56 is not limited to generating change information so as to keep the value of the energy density ED within a desired range, and may generate change information so as to keep at least one of the values of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range.
[0186] Each process of the flowchart shown in FIG. 10 is stored in the storage unit 58 of the arithmetic device 50, and is read and executed by the arithmetic device 50. In step S31, the material control unit 51 causes the material layer forming unit 20 to form a material layer under the set modeling conditions, and the process proceeds to step S32. In step S32, the modeling control unit 52 causes the modeling unit 30 to model a solidified layer under the set modeling conditions. When the irradiation unit 32 starts irradiating the laser light, the calculation unit 50 causes the imaging device 41 to image the detection target area on the surface of the material layer. The detection unit 54 generates temperature image data based on the image data generated by the imaging device 41, and determines the temperature of the powder material P in the material layer before melting from the temperature image data. The detection unit 54 may also determine the temperature of a solidified region BE adjacent to the path along which the laser light is scanned.
[0187] In step S33, the determination unit 57 determines whether or not the temperature of the powder material P of the material layer obtained by the detection unit 54 satisfies a first predetermined reference range. The first reference range is a temperature range of the material layer (powder material P) for maintaining the energy density ED within the desired range described above. This first reference range (temperature range of the powder material P) is set based on the correlation between the temperature of the powder material P and the energy density ED obtained, for example, by various tests or simulations by the user. This first reference range is stored in advance in the storage unit 58, and the determination unit 57 reads out this first reference range and uses it in the determination process of step S33 and step S34 described later.
[0188] The temperature range of the first reference range may be, for example, 20°C±5°C at room temperature and 200°C±10°C when preheating when the powder material P is aluminum. If the determination unit 57 determines that the temperature of the material layer does not satisfy the first reference range, the process proceeds to step S34, and if the determination unit 57 determines that the temperature of the material layer satisfies the first reference range, the process proceeds to step S37 described later. In other words, in step S33, the determination unit 57 determines whether or not it is necessary to generate change information. The above-mentioned first reference range is not limited to the energy density ED, and may be set so that the power density PD or the temperature distribution T(r) is kept within a desired range.
[0189] In step S34, the determination unit 57 determines whether the temperature of the material layer is higher or lower than the first reference range. If the determination unit 57 determines that the temperature of the material layer is higher than the first reference range, the process proceeds to step S35, and if the determination unit 57 determines that the temperature of the material layer is lower than the first reference range, the process proceeds to step S36. In addition, when the detection unit 54 determines the temperature of the adjacent solidification region BE, the judgment unit 57 compares it with a first reference range set as a range of the temperature of the material layer in which at least one of the energy density ED, the power density PD, and the temperature distribution T(r) is maintained within a desired range when affected by the heat of the adjacent solidification region BE.
[0190] In step S35, the calculation unit 56 generates modification information for modifying the modeling conditions so as to lower the value of the energy density ED in order to include the energy density ED within the desired range. The reason for lowering the energy density ED is as follows. Since the temperature of the material layer is higher than the first reference range, when the powder material P is irradiated with the laser light, the temperature of the powder material P rises to a desired temperature (e.g., the melting point) even with a small amount of heat. For this reason, it is predicted that the energy density ED of the energy absorbed by the powder material P will be excessive. In order to lower the value of the energy density ED and reduce the energy absorbed by the powder material P, it is possible to reduce the output of the laser light from the irradiation unit 32 to reduce the energy absorbed by the powder material P. It is also possible to reduce the effect of heating the powder material P due to the irradiation of the laser light by increasing the flow rate of the inert gas and increasing the flow speed of the inert gas to cool the surface of the material layer and reduce the temperature of the powder material P. It is also possible to reduce the energy absorbed by the powder material P by increasing the scanning speed of the laser light by the scanning unit 33 to shorten the time during which the laser light irradiates the same position on the material layer.
[0191] Based on the above concept, the calculation unit 56 reduces the value of the energy density ED by, for example, adjusting the parameter P L , P0, and increasing the parameter v. In this case, the calculation unit 56 generates the modification information so that at least one of the following changes to the modeling conditions is performed: LThe change in the modeling condition related to parameter P1 is to decrease the laser power. The change in the modeling condition related to parameter P0 is to increase the flow rate and flow speed of the inert gas. The change in the modeling condition related to parameter v is to increase the scanning speed.
[0192] In this case, the calculation unit 56 calculates the amount by which the value of the energy density ED is to be reduced (amount of reduction) based on the difference between the temperature of the material layer obtained by the detection unit 54 and an arbitrary value (for example, the maximum value or the median value) within the first reference range. In this case, data correlating the amount of reduction in the energy density ED with the difference between the temperature of the material layer and an arbitrary value (for example, the maximum value or the median value) within the first reference range is stored in advance in the storage unit 58, and the calculation unit 56 calculates the amount of reduction in the value of the energy density ED by referring to this data. The calculation unit 56 calculates the amount of reduction in the value of each parameter P L , P0, and v. The calculation unit 56 refers to data in which the value of each parameter is associated with the value of each modeling condition, which is stored in advance in the storage unit 58, to calculate the value of each modeling condition corresponding to the calculated new parameter value, and generates the value of the modeling condition as change information. As described above, the calculation unit 56 may generate a correction value, which is a difference between the value of the new modeling condition and the value of the current modeling condition, as change information, and the output unit 55 may output this correction value to the setting unit 59 as state information.
[0193] The output unit 55 outputs the change information generated by the calculation unit 56 to the setting unit 59 (at least one of the modeling control unit 52 and the housing control unit 53) as state information. When the modeling control unit 52 inputs the change information, the modeling control unit 52 causes at least one of the irradiation unit 32 and the scanning unit 33 to perform at least one of the following operations. In this case, the operation of the irradiation unit 32 is to emit laser light with a new laser output based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a new change speed of the tilt angle based on the change information. When the housing control unit 53 inputs the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with a new valve opening degree and exhaust amount based on the change information. After that, the process returns to step S32.
[0194] In step S36, the calculation unit 56 generates change information for changing the modeling conditions so as to increase the value of the energy density ED. The reason for increasing the value of the energy density ED is as follows. Since the temperature of the material layer is lower than the first reference range, when the powder material P is irradiated with laser light, a large amount of heat is required to raise the temperature of the powder material P to a desired temperature (for example, the melting point). For this reason, it is predicted that the energy density ED of the energy absorbed by the powder material P will be insufficient.
[0195] In this case, the calculation unit 56 changes the modeling conditions so as to increase the value of the energy density ED, based on the opposite idea to that in step S35 described above. In this case, the calculation unit 56 changes the modeling conditions so as to increase the value of the energy density ED. L In this case, the calculation unit 56 generates modification information so that at least one of the following changes to the modeling conditions is performed: increasing the parameter P LThe change in the modeling condition related to parameter P0 is to increase the laser output. The change in the modeling condition related to parameter v is to decrease the flow rate and the flow speed of the inert gas. The change in the modeling condition related to parameter v is to decrease the scanning speed. The calculation unit 56 calculates the amount by which the value of the energy density ED is increased (increase) based on the difference between the temperature of the material layer obtained by the detection unit 54 and an arbitrary value in the first reference range (e.g., the minimum value or the median). In this case, too, data in which the increase amount and the difference between the temperature of the material layer and an arbitrary value in the first reference range (e.g., the minimum value or the median) are associated with each other is stored in the memory unit 58 in advance, and the calculation unit 56 calculates the increase amount of the value of the energy density ED by referring to this data. The calculation unit 56 calculates the increase amount of each parameter P based on the increase amount of the energy density ED. L , P0, and v. The calculation unit 56 refers to data in which the values of each parameter and the values of each modeling condition are associated with each other, which is stored in advance in the storage unit 58, to calculate the values of each modeling condition that correspond to the calculated new parameter values, and generates the values of the modeling conditions as change information.
[0196] The output unit 55 outputs the change information as state information to the setting unit 59 (at least one of the modeling control unit 52 and the housing control unit 53). When the modeling control unit 52 inputs the change information, the modeling control unit 52 causes at least one of the irradiation unit 32 and the scanning unit 33 to perform at least one of the following operations. In this case, the operation of the irradiation unit 32 is to emit laser light with a new laser output based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a new change speed of the tilt angle based on the change information. When the housing control unit 53 inputs the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with a new valve opening degree and exhaust amount based on the change information. After that, the process returns to step S32. In this case, too, the calculation unit 56 may generate a correction value, which is the difference between the value of the new modeling condition and the value of the current modeling condition, as change information, and the output unit 55 may output this correction value to the setting unit 59 as status information.
[0197] In step S37, which is reached when the temperature of the material layer satisfies the first reference range, the arithmetic device 50 judges whether or not the modeling of one solidified layer has been completed. If the modeling of one solidified layer has not been completed, the arithmetic device 50 makes a negative judgment in step S37, and the process returns to step S32. If the modeling of one solidified layer has been completed, the arithmetic device 50 makes a positive judgment in step S37, and the process proceeds to step S38. In step S38, the arithmetic device 50 judges whether or not the modeling of all solidified layers has been completed. If the processing of all solidified layers has not been completed, the arithmetic device 50 makes a negative judgment in step S38, and the process proceeds to step S31. If the processing of all solidified layers has been completed, the arithmetic device 50 makes a positive judgment in step S38, and all processes are terminated.
[0198] In the above description, the detection unit 54 determines the temperature of the powder material P before it is heated by irradiation with the laser light, but the present invention is not limited to this example. For example, the detection unit 54 may determine foreign matter and spatter SP mixed in the powder material P of the material layer. In this case, the detection unit 54 may determine the foreign matter and spatter SP from the image data captured by the imaging device 41 using a known image processing method without obtaining information on the temperature using the two-color method. In this case, the detection unit 54 may, for example, use a teacher image obtained in advance to separate the powder material P, foreign matter, and spatter SP from the image data captured by the imaging device 41 based on the differences in the size and shape of the particles, foreign matter, and spatter SP of the powder material P. In addition, the detection unit 54 may determine the foreign matter and spatter SP on a color image captured and generated by an imaging device different from the imaging device 41. By performing the above processing, the energy density ED, which is one of the basic conditions for the powder material P to melt and solidify, can be kept within the desired range, and poor molding of the solidified layer due to insufficient or excessive energy for the powder material P can be suppressed.
[0199] Next, as one example of a specific example of processing when making real-time changes, a case will be taken as an example in which the detection unit 54 obtains information on the temperature of the molten pool MP and its vicinity as the melting state, and the calculation unit 56 generates change information so as to keep the value of the energy density ED within a desired range. Note that the calculation unit 56 is not limited to generating change information so as to keep the value of the energy density ED within a desired range, and may generate change information so as to keep at least one of the values of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range.
[0200] Each process of the flowchart shown in FIG. 11 is stored in the storage unit 58 of the arithmetic device 50, and is read and executed by the arithmetic device 50. The processes of steps S41 and S42 are similar to the processes of steps S31 and S32 shown in the flowchart of Fig. 10. However, in step S42, the detection unit 54 obtains the temperature distribution of the molten pool MP as information on the temperature of the molten pool MP and its vicinity, using temperature image data generated from image data captured by the imaging device 41. In the specific example shown in Fig. 11, the detection unit 54 obtains the diameter of an isotherm of an arbitrary temperature in the molten pool MP from the temperature image data.
[0201] In step S43, the judgment unit 57 judges whether or not the temperature distribution of the molten pool MP obtained by the detection unit 54, i.e., the diameter of the isotherm of an arbitrary temperature of the molten pool MP, satisfies a first predetermined reference range. The first reference range is a range of the diameter of the isotherm for maintaining the temperature distribution T(r) within a desired range. This first reference range is set based on the correlation between the temperature distribution of the molten pool MP (diameter of the isotherm of an arbitrary temperature) obtained by various tests or simulations by the user and the temperature distribution T(r). This first reference range is stored in advance in the storage unit 58, and the judgment unit 57 reads out this first reference range and uses it for the judgment process of step S43 and step S44 described later. If the judgment unit 57 judges that the diameter of the isotherm of the molten pool MP does not satisfy the first reference range, the process proceeds to step S44, and if the judgment unit 57 judges that the diameter of the isotherm satisfies the first reference range, the process proceeds to step S47, described later. In other words, in step S43, the determination unit 57 determines whether or not it is necessary to generate change information. The first reference range is not limited to the temperature distribution T(r), and may be set so that the power density PD or the energy density ED is kept within a desired range. The range of isotherm diameters that is the first reference range may be the range of isotherm diameters that corresponds to the temperature range between the melting point and liquidus temperature of the powder material P used and the temperature range between the melting point and solidus temperature.
[0202] In step S44, the determination unit 57 determines whether the diameter of the isotherm is higher than the first reference range or lower than the first reference range. If the determination unit 57 determines that the diameter of the isotherm is higher than the first reference range, the process proceeds to step S45, and if the determination unit 57 determines that the diameter of the isotherm is lower than the first reference range, the process proceeds to step S46.
[0203] In step S45, the calculation unit 56 generates modification information for modifying the building conditions to lower the value of the energy density ED so that the value of the energy density ED falls within a desired range. The reason for lowering the value of the energy density ED is as follows. The fact that the diameter of the isotherm of the molten pool MP is larger than the first reference range means that the molten pool MP is larger than the molten pool MP expected to be obtained under the currently set building conditions. This makes it possible to estimate that the energy density ED of the energy absorbed by the powder material P inside the material layer is excessive.
[0204] In this case, the calculation unit 56 reduces the value of the energy density ED in the same manner as in step S35 of FIG. 10 by adjusting the parameter P L , P0 and increasing the parameter v. That is, the calculation unit 56 generates the change information so that at least one of the following is performed: lowering the laser output, increasing the flow rate and flow speed of the inert gas, and lowering the scanning speed. The specific process performed by the calculation unit 56 to generate the change information is performed while referring to the data stored in the storage unit 58, similar to the case of step S35 described in FIG. 10. The output unit 55 outputs the change information generated by the calculation unit 56 as state information to the setting unit 59 (at least one of the formation control unit 52 and the housing control unit 53). When the formation control unit 52 inputs the change information, the formation control unit 52 causes at least one of the irradiation unit 32 and the scanning unit 33 to perform at least one of the following operations. The operation of the irradiation unit 32 in this case is to emit laser light with a new laser output based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a new change speed of the tilt angle based on the change information. When the housing control unit 53 inputs the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with the new valve opening degree and exhaust amount based on the change information. After that, the process returns to step S42.
[0205] In step S46, the calculation unit 56 generates modification information for modifying the building conditions to increase the value of the energy density ED so that the value of the energy density ED falls within the desired range. The reason for increasing the energy density ED is as follows. If the diameter of the isotherm in the molten pool MP is smaller than the first reference range, it means that the molten pool MP is smaller than the molten pool MP expected to be obtained under the currently set building conditions. This makes it possible to estimate that the energy density ED of the energy absorbed by the powder material P inside the material layer is insufficient.
[0206] In this case, the calculation unit 56 calculates the parameter P L , P0 and the parameter v are increased. That is, the calculation unit 56 generates the change information so that at least one of increasing the laser output, decreasing the flow rate and the flow speed of the inert gas, and decreasing the scanning speed is performed. The specific process performed by the calculation unit 56 to generate the change information is performed while referring to the data stored in the storage unit 58, similar to the case of step S36 described in FIG. 10. The output unit 55 outputs the change information generated by the calculation unit 56 as state information to the setting unit 59 (at least one of the modeling control unit 52 and the housing control unit 53). When the modeling control unit 52 inputs the change information, the modeling control unit 52 causes at least one of the irradiation unit 32 and the scanning unit 33 to perform at least one of the following operations. The operation of the irradiation unit 32 in this case is to emit laser light with a new laser output based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a change speed of the new tilt angle based on the change information. When the housing control unit 53 receives the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with new valve openings and exhaust volumes based on the change information. After that, the process returns to step S42. In addition, in steps S45 and S46, the calculation unit 56 may generate a correction value, which is the difference between the value of the new modeling condition and the value of the current modeling condition, as change information, and the output unit 55 may output this correction value to the setting unit 59 as status information.
[0207] The processes of steps S47 and S48 to which the process proceeds when the diameter of the isotherm satisfies the first reference range are similar to the processes of steps S37 and S38 in FIG. By carrying out the above-mentioned processing, the basic conditions for the powder material P to melt and solidify can be maintained within a desired range, and the occurrence of defective molding of the solidified layer due to insufficient or excessive melting can be suppressed. In step S42, the detection unit 54 may obtain the ratio of the major axis to the minor axis of the molten pool MP on the XY plane and the temperature gradient of the molten pool MP on the XY plane as information on the temperature of the molten pool MP and its vicinity. In this case, the ratio of the major axis to the minor axis of the molten pool MP on the XY plane and the temperature gradient of the molten pool MP on the XY plane that keeps at least one of the energy density ED, power density PD, and temperature distribution T(r) within a desired range may be used as the first reference range. In this case, the first reference range is set based on the results of various tests and simulations by the user, as described above.
[0208] If the ratio of the major axis to the minor axis of the molten pool MP is greater than the first reference range, it can be estimated that the energy density ED of the energy absorbed by the powder material P is excessive, and the molten pool MP is larger than the molten pool MP expected from the currently set molding conditions. Therefore, the calculation unit 56 may generate change information in the same manner as in step S45 so as to reduce the value of the energy density ED. If the ratio of the major axis to the minor axis of the molten pool MP is smaller than the first reference range, the calculation unit 56 may generate change information in the same manner as in step S46, based on the opposite idea. Furthermore, if the temperature gradient of the molten pool MP is larger than the first reference range, it can be estimated that the energy density ED of the energy absorbed by the powder material P is excessive, causing drastic temperature changes in the molten pool MP. Therefore, the calculation unit 56 generates change information in the same manner as in step S45 so as to reduce the value of the energy density ED. If the temperature gradient of the molten pool MP is smaller than the first reference range, the calculation unit 56 generates change information in the same manner as in step S46, based on the opposite idea.
[0209] Next, as an example of a specific example of processing when real-time change is performed, a case will be taken as an example where the detection unit 54 determines the state of the sputter SP, and the calculation unit 56 generates change information so as to keep the value of the energy density ED within a desired range. Note that the calculation unit 56 is not limited to generating change information so as to keep the value of the energy density ED within a desired range, and may generate change information so as to keep at least one of the value of the power density PD, the value of the energy density ED, and the value of the temperature distribution T(r) within a desired range.
[0210] Each process of the flowchart shown in FIG. 12 is stored in the storage unit 58 of the arithmetic device 50, and is read and executed by the arithmetic device 50. The processes of steps S51 and S52 are similar to the processes of steps S31 and S32 shown in the flowchart of Fig. 10. However, in step S52, the detection unit 54 uses temperature image data generated from image data generated by imaging by the imaging device 41 to determine the state of the spatters SP from the temperature image data by the method described using Fig. 6. In the specific example shown in the flowchart of Fig. 12, a case will be taken as an example in which the detection unit 54 determines the amount of scattering of the spatters SP as the state of the spatters SP.
[0211] In step S53, the determination unit 57 determines whether the state of the sputter SP obtained by the detection unit 54, that is, the amount of scattering of the sputter SP, satisfies a first reference range. The first reference range is a range of the amount of scattering of the sputter SP for maintaining the energy density ED in a desired range. This range of the amount of scattering of the sputter SP is set based on the correlation between the amount of scattering of the sputter SP and the energy density ED obtained, for example, by various tests or simulations by the user. This range of the amount of scattering of the sputter SP (first reference range) is stored in advance in the storage unit 58, and the determination unit 57 reads out this first reference range and uses it for the determination process of step S53 and step S54 described later. If the determination unit 57 determines that the amount of scattering of the sputter SP does not satisfy the first reference range, the process proceeds to step S54, and if the determination unit 57 determines that the amount of scattering of the sputter SP satisfies the first reference range, the process proceeds to step S57 described later. In other words, in step S53, the determination unit 57 determines whether or not it is necessary to generate change information. The above-mentioned first reference range is not limited to the energy density ED, and may be set so that the power density PD or the temperature distribution T(r) is kept within a desired range.
[0212] In step S54, the determination unit 57 determines whether the amount of scattering sputters SP is greater than or less than the first reference range. If the determination unit 57 determines that the amount of scattering sputters SP is greater than the first reference range, the process proceeds to step S55, and if the determination unit 57 determines that the amount of scattering sputters SP is less than the first reference range, the process proceeds to step S56.
[0213] In step S55, the calculation unit 56 generates modification information for modifying the molding conditions so as to lower the value of the energy density ED so that the value of the energy density ED falls within a desired range. The reason for lowering the value of the energy density ED is as follows. That is, the fact that the amount of scattering of the sputter SP is greater than the first reference range means that the amount of heat applied to the powder material P is excessive and the convection C of the molten pool MP is large. In other words, it can be estimated that the energy density ED of the energy absorbed by the powder material P is excessive.
[0214] In this case, the calculation unit 56 reduces the value of the energy density ED by adjusting the parameter P L , P0 and increasing the parameter v. That is, the calculation unit 56 generates the change information so that at least one of the following is performed: lowering the laser output, increasing the flow rate and speed of the inert gas, and increasing the scanning speed. The specific process performed by the calculation unit 56 to generate the change information is performed while referring to the data stored in the storage unit 58, in the same manner as described in FIG. 10. The output unit 55 outputs the change information generated by the calculation unit 56 as state information to the setting unit 59 (at least one of the modeling control unit 52 and the housing control unit 53). When the modeling control unit 52 inputs the change information, the modeling control unit 52 performs at least one of the following: making the irradiation unit 32 emit the laser light with a new laser output based on the change information; and making the scanning unit 33 drive the galvanometer mirrors 331 and 332 at a change speed of the new tilt angle based on the change information. When the housing control unit 53 receives the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with the new valve opening and exhaust amount based on the change information. After that, the process returns to step S52.
[0215] In step S56, the calculation unit generates modification information for modifying the molding conditions so as to increase the value of the energy density ED so that the value of the energy density ED falls within a desired range. The reason for increasing the value of the energy density ED is as follows. That is, the amount of scattering of the sputter SP being less than the first reference range means that the amount of heat applied to the powder material P is insufficient and the convection C of the molten pool MP is small. In other words, it is possible to estimate that the energy density ED of the energy absorbed by the powder material P is insufficient.
[0216] In this case, the calculation unit 56 increases the value of the energy density ED by adjusting the parameter P L , P0 and decreasing the parameter v. That is, the calculation unit 56 generates the modification information so that at least one of increasing the laser output, decreasing the flow rate and speed of the inert gas, and decreasing the scanning speed is performed. The specific process performed by the calculation unit 56 to generate the modification information is performed while referring to the data stored in the storage unit 58, similar to the case described with reference to FIG.
[0217] The output unit 55 outputs the change information generated by the calculation unit 56 as state information to at least one of the formation control unit 52 and the housing control unit 53. When the formation control unit 52 inputs the change information, the formation control unit 52 causes at least one of the irradiation unit 32 and the scanning unit 33 to perform at least one of the following operations. In this case, the operation of the irradiation unit 32 is to emit laser light with a new laser output based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a new change speed of the tilt angle based on the change information. When the housing control unit 53 inputs the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with a new valve opening degree and exhaust amount based on the change information. After that, the process returns to step S52. In addition, in steps S55 and S56, the calculation unit 56 may generate a correction value, which is the difference between the value of the new modeling condition and the value of the current modeling condition, as change information, and the output unit 55 may output this correction value to the setting unit 59 as status information.
[0218] The processes in steps S57 and S58, which are carried out when the amount of scattered sputters satisfies the first reference range, are similar to the processes in steps S37 and S38 in FIG. By carrying out the above-mentioned processing, the state inside the molten pool MP during melting is controlled, thereby reducing the occurrence of internal defects in the solidified layer formed by solidifying the molten pool MP.
[0219] In step S52, the detection unit 54 may determine the scattering direction and scattering speed of the sputters SP as the state of the sputters SP by the method described with reference to FIG. When the detection unit 54 determines the scattering direction of the spatter SP, the first reference range is the range of the scattering direction of the spatter SP for keeping at least one of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range. This range of the scattering direction of the spatter SP (first reference range) is set, for example, based on the results of various tests and simulations by the user, as in the above-mentioned step S53. The judgment unit 57 judges that the first reference range is not satisfied when the scattering direction of the spatter SP centered on the keyhole KH is not fixed in a certain direction (for example, backward with respect to the scanning direction of the laser light) and varies irregularly. As described above, the scattering direction of the spatter SP is not fixed in a certain direction, which means that the powder material P receives excessive energy. This state means that the keyhole KH is deep and the convection C of the molten pool MP is intense, so the calculation unit 56 generates change information to reduce the value of the energy density ED.
[0220] When the detection unit 54 determines the scattering speed of the spatter SP, the first reference range is the range of the scattering speed of the spatter SP for maintaining at least one of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range. This range of the scattering speed of the spatter SP (first reference range) is set based on the results of various tests and simulations by the user, for example, as in step S53 described above. The determination unit 57 determines that the first reference range is not satisfied when the scattering speed is high. As described above, a high scattering speed of the spatter SP means that the convection C of the molten pool MP is intense, so the calculation unit 56 generates change information to reduce the value of the energy density ED.
[0221] Furthermore, the detection unit 54 may obtain the state of the fumes FU as the state of the detection target area. A case will be described in which the detection unit 54 obtains the concentration of the fume FU as the state of the fume FU by the method described with reference to FIG. 7. In this case, the first reference range is the range of the concentration of the fume FU for keeping at least one of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range. This range of the concentration of the fume FU (first reference range) is set based on the results of various tests and simulations by the user, for example, as in the above-mentioned steps S33, S43, and S53. The determination unit 57 determines that the higher the concentration, the less the first reference range is satisfied. As described above, the higher the concentration of the fume FU, the more excessive the fume FU is generated, which means that the temperature in the molten pool MP is too high due to the excessive energy absorbed by the powder material P. Therefore, the calculation unit 56 generates change information to reduce the value of the energy density ED.
[0222] A case will be described in which the detection unit 54 determines the range of the fume FU as the state of the fume FU by the method described with reference to FIG. 7. In this case, the first reference range is the range of the fume FU for which at least one of the power density PD, the energy density ED, and the temperature distribution T(r) is kept within a desired range. This range of the fume FU (first reference range) is set based on the results of various tests and simulations performed by the user, for example, as in step S53 described above. The determination unit 57 determines that the first reference range is not satisfied when the range of the fume FU, that is, the area on the temperature image, is large. As described above, a wide range of the fume FU means that the amount of fume FU generated is large, the energy absorbed by the powder material P is excessive, and the temperature in the molten pool MP is too high. For this reason, the calculation unit 56 generates change information to reduce the value of the energy density ED.
[0223] In steps S35, S36, S45, S46, S55 and S56 in the flowcharts shown in FIGS. 10, 11 and 12, the calculation unit 56 calculates the parameter P L Which of the parameters P, P0, and v should be changed or not changed depends on the user's request for the modeling of the three-dimensional object. For example, if the user wishes to avoid an increase in the modeling time, the calculation unit 56 changes the parameters P in steps S36, S46, and S56 so as not to reduce the scanning speed of the laser light. L In one embodiment, when the energy density ED is lower than the desired range, the calculation unit 56 does not change the value of the parameter v, and the calculation unit 56 changes the value of the parameter P L In this case, the modeling time is maintained, but the temperature change during the solidification process of the powder material P melted by the irradiation of the laser light increases, so the residual stress in the solidified layer increases, and the quality of the three-dimensional model to be formed may decrease.
[0224] On the other hand, if the user wishes to avoid a decrease in the quality of the three-dimensional object to be formed, in the above steps S36, S46, and S56, the calculation unit 56 changes the value of the parameter v to reduce the parameter P L As an example, when the energy density ED is lower than the desired range, the calculation unit 56 may not change the value of the parameter P L Modification information is generated so as to decrease the value of parameter v without increasing the value of v. In this case, the residual stress in the solidified layer due to temperature change does not increase, and the quality of the printed 3D object is maintained, but the printing time may increase.
[0225] As described above, since there are multiple types of parameters that can be changed in order to maintain the energy density ED within a desired range, the parameters to be changed by the calculation unit 56 may be determined based on an instruction from the user. In this case, the calculation unit 56 notifies the user of information for accepting a predetermined designation by the user (hereinafter referred to as designation target information) in order to determine the parameters to be changed. For example, the calculation unit 56 may notify the user of information for accepting a predetermined designation by the user in order to maintain the energy density ED within a desired range (for example, the parameter v and the parameter P L ) may be displayed as designation target information on a display device (not shown), such as a liquid crystal display configured to be able to communicate with the calculation unit 56. Then, the user uses a designation device (not shown), such as a mouse, to designate a parameter displayed on the display device (designate parameter v, as an example). The calculation unit 56 generates modification information for modifying the value of the parameter (parameter v, as an example) designated by the user so as to maintain the energy density ED within a desired range.
[0226] For convenience of explanation, the parameters v and P are L In the above example, two types of parameters are displayed on a display device (not shown) as the specified target information. However, the parameters to be displayed on the display device as the specified target information are the parameter v and the parameter P LFor example, the calculation unit 56 may calculate the parameter v and the parameter P L Among the above-mentioned parameters P0, η, d, Δy, Δz, ρ, k, r, x, α, and T0, which are different from the above, a plurality of parameters that can be changed in order to maintain the basic conditions and detailed conditions (described later) within a desired range may be displayed on the display device as the designation target information. When at least one of the displayed plurality of parameters is designated by the user, the calculation unit 56 generates modification information for modifying the value of the parameter designated by the user so that the basic conditions and detailed conditions (described later) are maintained within a desired range.
[0227] In addition, the designation target information that the calculation unit 56 displays on a display device (not shown) is not limited to parameters. For example, the calculation unit 56 may display, on a display device as designation target information, a plurality of modeling conditions that can be changed in order to maintain basic conditions and detailed conditions (described later) within a desired range among the above-mentioned modeling conditions. In addition, since the modeling time and quality of a three-dimensional object are affected by the parameters and modeling conditions to be changed, the user is not limited to designating the parameters and modeling conditions to be changed as described above. The user may select whether to prioritize (maintain) the modeling time of the three-dimensional object or to prioritize (maintain) the quality of the three-dimensional object. In this case, as an example, the calculation unit 56 displays items related to the time priority and the quality priority on a display device (not shown) as designation target information. The user designates one of the items related to the time priority and the quality priority displayed on the display device using a designation device (not shown) such as a mouse. The calculation unit 56 generates change information for changing the values of the parameters and modeling conditions according to the items designated by the user so that the basic conditions and detailed conditions (described later) are maintained within a desired range. For example, when the energy density ED is lower than the desired range, if the item related to the time priority is designated by the user, the calculation unit 56 does not change the value of the parameter v, and changes the parameter P L On the other hand, if the user specifies an item related to the emphasis on quality, the calculation unit 56 generates modification information to change the value of the parameter P L The value of is not changed, but change information is generated to change the value of parameter v.
[0228] In addition to the time emphasis and the quality emphasis, an item related to the emphasis on balance, which emphasizes the balance between the modeling time and the quality, may be displayed on a display device (not shown) as the designated target information together with at least one of the items related to the time emphasis and the quality emphasis. For example, when the energy density ED is lower than the desired range, if the item related to the emphasis on balance is designated by the user, the calculation unit 56 calculates the parameter v and the parameter P L Then, change information is generated to change both values. The display format of each of the items relating to time-oriented, quality-oriented, and balance-oriented on the display device may be any existing format such as text or icons as long as the user can identify it. The display device (not shown) does not have to be a liquid crystal display, but may be an existing display device such as an organic electroluminescence display or a head-mounted display. The designation device (not shown) does not have to be a mouse, but may be an existing device such as a touch panel. The method of notifying the user of the designated information is not limited to displaying it on the display device. For example, using a speaker and a microphone (not shown), the calculation unit 56 may notify the user of the designated information by the speaker (audio) and receive the designation from the user by the microphone (audio), or may use another existing method. In steps S35, S36, S45, S46, S55 and S56, the calculation unit 56 calculates the above-mentioned parameter P L In addition to P0, v, the energy density ED is also affected, and change information of the modeling conditions that can be changed in real time may be generated. For example, the calculation unit 56 may generate change information for the oscillation mode of the laser light of the irradiation unit 32, the intensity distribution of the laser light, the spot size of the laser light, and the scanning path and scanning pitch of the laser light by the scanning unit 33.
[0229] Next, an example of a specific example of a process when a change is made during formation of the next layer will be described. In the following description, the case where the detection unit 54 detects a molten state as the state of the detection target region and the case where the detection unit 54 detects a sputter SP state will be described separately. First, the following case will be taken as an example of processing when making changes during the formation of the next layer. The detection unit 54 obtains information on the temperature of the molten pool MP and its vicinity as a molten state during the formation of the solidified layer. The calculation unit 56 generates change information so as to keep the value of the energy density ED when a new solidified layer is formed on top of the solidified layer, based on the information on the temperature obtained by the detection unit 54 during the formation of the solidified layer, within a desired range. Note that the calculation unit 56 is not limited to generating change information so as to keep the value of the energy density ED within a desired range, and may generate change information so as to keep at least one of the values of the power density PD, the energy density ED, and the temperature distribution T(r) within a desired range.
[0230] Each process of the flowcharts shown in FIGS. 13 and 14 is stored in the storage unit 58 of the arithmetic device 50, and is read and executed by the arithmetic device 50. In step S61, the modeling control unit 52 causes the modeling unit 30 to model the solidified layer under the set modeling conditions. During the modeling of the solidified layer, the calculation unit 50 causes the imaging device 41 to capture an image of the detection target area on the surface of the material layer, for example, at a predetermined time interval or every time the laser light is scanned by the scanning unit 33 for a predetermined distance on the XY plane. The detection unit 54 generates temperature image data every time image data is output from the imaging device 41, obtains information on the temperature of the molten pool MP and its vicinity for each generated temperature image data, and stores the information in the storage unit 58. In the specific example shown in the flowcharts of Figures 13 and 14, the detection unit 54 obtains the average temperature of the molten pool MP as information on the temperature of the molten pool MP and its vicinity. The detection unit 54 obtains a high-temperature area of the temperature image data that is equal to or higher than a first predetermined temperature as an area on the image corresponding to the molten pool MP, obtains the temperature of any point in the high-temperature area on the image, and calculates the average of the obtained temperatures to obtain the average temperature of the molten pool MP. In addition, the detection unit 54 generates temperature image data and stores it in the memory unit 58 when forming the solidified layer, and after the formation of one solidified layer is completed, the average temperature of the molten pool MP can be calculated from each of the multiple temperature image data stored in the memory unit 58.
[0231] In step S62, the calculation device 50 judges whether or not the modeling of one solidified layer has been completed. If the modeling of one solidified layer has been completed, the calculation device 50 judges in step S62 as positive, and the process proceeds to step S63. If the modeling of one solidified layer has not been completed, the calculation device 50 judges in step S62 as negative, and the process returns to step S61.
[0232] In step S63, the judgment unit 57 judges whether the temperature distribution of the molten pool MP obtained by the detection unit 54, i.e., the average temperature of the molten pool MP, satisfies a second predetermined reference range. The second reference range is a range of the average temperature of the molten pool MP for maintaining the energy density ED within a desired range. This second reference range (range of the average temperature of the molten pool MP) is set based on the correlation between the average temperature of the molten pool MP and the energy density ED obtained, for example, from the results of various tests and simulations performed by a user. The second reference range is stored in advance in the storage unit 58, and the judgment unit 57 reads out this second reference range and uses it for the judgment process of step S63 and step S65 described later. If the judgment unit 57 judges that the average temperature of the molten pool MP does not satisfy the second reference range, the process proceeds to step S64, and if the judgment unit 57 judges that the average temperature of the molten pool MP satisfies the second reference range, the process proceeds to step S71 described later. In other words, in step S63, the determination unit 57 determines whether or not it is necessary to generate change information. The second reference range is not limited to the energy density ED, and may be set so that the power density PD or the temperature distribution T(r) is kept within a desired range. The average temperature range, which is the second reference range, may be a temperature range between the melting point and liquidus temperature of the powder material P used and between the melting point and solidus temperature.
[0233] In step S64, the determination unit 57 determines whether the average temperature of the molten pool MP obtained by the detection unit 54 satisfies the third reference range. The third reference range is a range of the average temperature of the molten pool MP for maintaining the energy density ED in a desired range when the molding conditions are changed. The maximum value of the third reference range is greater than the maximum value of the second reference range, and the minimum value of the third reference range is smaller than the minimum value of the second reference range. The third reference range may be a range between a value near the maximum value and a value near the minimum value. If the average temperature of the molten pool MP satisfies the third reference range, that is, if the determination unit 57 determines that the energy density ED is maintained in a desired range by changing the molding conditions (that is, the occurrence of molding defects can be suppressed), the process proceeds to step S65. If the average temperature of the molten pool MP does not satisfy the third reference range, that is, if the determination unit 57 determines that the energy density ED is not maintained in a desired range by changing the molding conditions (that is, the occurrence of molding defects cannot be suppressed), the process proceeds to step S68, which will be described later. In addition, the above-mentioned third reference range is not limited to the energy density ED, and may be set so that the power density PD and the temperature distribution T(r) are kept within a desired range when the modeling conditions are changed. In addition, the range of the average temperature, which is the third reference range, may be a temperature range between the melting point and liquidus temperature of the powder material P used and between the melting point and solidus temperature. In addition, the third reference range is stored in advance in the storage unit 58.
[0234] In step S65, the judgment unit 57 judges whether the average temperature of the molten pool MP is higher than the second reference range or lower than the second reference range. If the average temperature of the molten pool MP is higher than the second reference range, that is, if the judgment unit 57 judges that the energy density ED of the energy absorbed by the powder material P is excessive but the value of the energy density ED can be set to the desired range by changing the building conditions, the process proceeds to step S66. If the average temperature of the molten pool MP is lower than the second reference range, that is, if the judgment unit 57 judges that the energy density ED of the energy absorbed by the powder material P is insufficient but the value of the energy density ED can be set to the desired range by changing the building conditions, the process proceeds to step S67.
[0235] In step S66, the calculation unit 56 generates modification information for modifying the building conditions to lower the value of the energy density ED so that the value of the energy density ED falls within the desired range. The reason for lowering the value of the energy density ED is as follows. The average temperature of the molten pool MP being greater than the second reference range means that the amount of heat to the molten pool MP is greater than the amount of heat expected to be obtained under the currently set building conditions, and the temperature of the molten pool MP is too high. For this reason, it is estimated that the energy density ED of the energy absorbed by the powder material P is excessive.
[0236] In order to lower the value of the energy density ED and reduce the amount of heat applied to the powder material P, it is possible to reduce the output of the laser light from the irradiation unit 32 to reduce the energy received by the powder material P. It is also possible to increase the amount of heat required to raise the temperature of the powder material P to a desired temperature (e.g., melting point) by irradiation with the laser light, by increasing the flow rate and flow speed of the inert gas and cooling the surface of the material layer to lower the temperature of the powder material P.
[0237] In addition, since the temperature of the powder material P before the laser beam is irradiated is higher than the expected temperature, the amount of heat required for the temperature of the powder material P to rise to the desired temperature may be less. In this case, it is possible to reduce the effect of heat from the molded solidified layer on the powder material P by at least one of lowering the temperature of the base plate 311 to lower the temperature of the powder material P before the laser beam is irradiated, or by lengthening the time until the material layer is formed on the solidified layer and cooling the solidified layer with an inert gas. Furthermore, it is also possible that the thickness of the material layer formed on the solidified layer in the Z direction is thin, so that the heat of the solidified layer is easily conducted to the upper part (Z direction + side) of the material layer. In such a case, it is also possible to increase the heat capacity by increasing the thickness of the material layer (i.e., increasing the layer thickness) to make it difficult for the heat of the already molded solidified layer to be conducted to the upper part of the material layer.
[0238] In addition, since the scanning distance when the laser light is scanned is long, the time during which the material layer is heated by the irradiation of the laser light is long, and the temperature may increase. For this reason, it is possible to set the scanning path so that the scanning distance when the laser light is scanned is shortened, thereby shortening the time during which the material layer is exposed to the irradiation of the laser light and is affected by the heat. It is also possible to shorten the time during which the laser light irradiates the same position on the material layer by increasing the scanning speed of the laser light by the scanning unit 33, thereby reducing the amount of energy absorbed by the powder material P per unit time. In addition, since the spot size of the laser light is small, the amount of heat is concentrated in a narrow range of the material layer, and the amount of energy of the material layer per unit area may be large, it is also possible to increase the spot size and suppress the concentration of heat generated by the laser light in a narrow range of the material layer.
[0239] In addition, since the scanning pitch is small, the influence of heat conducted from the already solidified solidification region BE to the molten pool MP may be large, so it is possible to widen the scanning pitch to suppress the influence of heat conducted from the already solidified solidification region BE. In addition, if the density of the material layer is high, the heat generated by the irradiation of the laser light may be easily conducted within the material layer, so it is possible to make it difficult for heat to be conducted through the material layer by reducing the pressure applied to the powder material P by the blade 221 to reduce the density.
[0240] Based on the above concept, in order to reduce the energy density ED during the formation of the next solidified layer from the current level, the calculation unit 56 calculates the parameter P L In this case, the calculation unit 56 generates modification information so that at least one of the following changes in the modeling conditions is performed: decreasing the parameters P, P0, and ρ, and increasing the parameters v, Δy, and Δz. L The change in the building conditions associated with parameter P0 is at least one of increasing the flow rate and increasing the flow speed of the inert gas, decreasing the output of the heater 313 to decrease the temperature of the base plate 311, extending the waiting time of the blade 221, and changing the scanning path. The change in the building conditions associated with parameter ρ is at least one of decreasing the pressure applied by the blade 221 to the material layer. The change in the building conditions associated with parameter v is at least one of increasing the scanning speed. The change in the building conditions associated with parameter Δy is at least one of increasing the spot size of the laser light and increasing the scanning pitch. The change in the building conditions associated with parameter Δz is at least one of increasing the layer thickness.
[0241] The calculation unit 56 generates change information by referring to data in which parameter values and modeling condition values are associated with each other, which is stored in advance in the storage unit 58, in the same manner as in the case described above with reference to FIGS. 10, 11, and 12. The output unit 55 outputs the change information generated by the calculation unit 56 as state information to the setting unit 59 (at least one of the material control unit 51, the modeling control unit 52, and the housing control unit 53). When the material control unit 51 inputs the change information, the material control unit 51 causes the recoater 22 to perform at least one of the following operations. The operation of the recoater 22 in this case includes moving the blade 221 after a new waiting time based on the change information has elapsed, and moving the blade 221 with a new pressure based on the change information. When the modeling control unit 52 inputs the change information, the modeling control unit 52 causes at least one of the irradiation unit 32, the scanning unit 33, and the heater 313 to perform at least one of the following operations. In this case, the operation of the irradiation unit 32 includes emitting laser light with a new laser output based on the change information and moving the focus lens 323 to a new position in the X direction based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a new tilt angle or a change speed of the tilt angle based on the change information. The operation of the heater 313 is to operate with a new heating output based on the change information. When the housing control unit 53 inputs the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with a new valve opening degree and exhaust amount based on the change information. After that, the process returns to step S61.
[0242] In step S67, the calculation unit 56 generates modification information for modifying the building conditions to increase the value of the energy density ED so that the value of the energy density ED falls within the desired range. The reason for increasing the energy density ED is as follows. The average temperature of the molten pool MP being smaller than the second reference range means that the amount of heat to the molten pool MP is less than the amount of heat expected to be obtained under the currently set building conditions, and the temperature of the molten pool MP is too low. For this reason, it is estimated that the energy density ED of the energy absorbed by the powder material P is insufficient.
[0243] In this case, the calculation unit 56 generates change information so as to increase the value of the energy density ED by using the opposite idea to that of step S66 described above. L In this case, the calculation unit 56 generates modification information so that at least one of the following changes in the modeling conditions is performed: increasing the parameters P, P0, and ρ, and decreasing the parameters v, Δy, and Δz. L The change in the modeling condition associated with parameter P is to increase the laser output. The change in the modeling condition associated with parameter P0 is at least one of decreasing the flow rate and the flow speed of the inert gas, increasing the output of the heater 313 to increase the temperature of the base plate 311, shortening the waiting time of the blade 221, and changing the scanning path. The change in the modeling condition associated with parameter ρ is to increase the pressure applied by the blade 221 to the material layer. The change in the modeling condition associated with parameter v is to decrease the scanning speed. The change in the modeling condition associated with parameter Δy is at least one of decreasing the spot size of the laser light and decreasing the scanning pitch. The change in the modeling condition associated with parameter Δz is to decrease the layer thickness.
[0244] The calculation unit 56 generates change information by referring to data in which the parameter values and the modeling condition values are associated with each other, which is stored in advance in the storage unit 58, in the same manner as in the case described above with reference to FIGS. 10, 11, and 12. The output unit 55 outputs the change information generated by the calculation unit 56 as state information to the setting unit 59 (at least one of the material control unit 51, the modeling control unit 52, and the housing control unit 53). When the material control unit 51 inputs the change information, the material control unit 51 causes the recoater 22 to perform at least one of the following operations. The operation of the recoater 22 in this case includes moving the blade 221 after a new waiting time based on the change information has elapsed, and moving the blade 221 with a new pressure based on the change information. When the modeling control unit 52 inputs the change information, the modeling control unit 52 causes at least one of the irradiation unit 32, the scanning unit 33, and the heater 313 to perform at least one of the following operations. In this case, the operation of the irradiation unit 32 includes emitting laser light with a new laser output based on the change information and moving the focus lens 323 to a new position in the X direction based on the change information. The operation of the scanning unit 33 is to drive the galvanometer mirrors 331 and 332 at a new tilt angle or a change speed of the tilt angle based on the change information. The operation of the heater 313 is to operate with a new heating output based on the change information. When the housing control unit 53 inputs the change information, the housing control unit 53 operates the intake device 131 and the exhaust device 14 with a new valve opening degree and exhaust amount based on the change information. After that, the process returns to step S61. Note that in steps S66 and S67, the calculation unit 56 may generate, as change information, a difference value between the value of the new modeling condition and the value of the current modeling condition.
[0245] In step S68 shown in FIG. 14, the judgment unit 57 judges whether the average temperature of the molten pool MP satisfies the fourth reference range. The fourth reference range is a range of the average temperature of the molten pool MP that allows the energy density ED to be kept within a desired range by performing a predetermined repair on the formed solidified layer. In other words, the judgment unit 57 judges whether the solidified layer needs to be repaired in step S68. The maximum value of the fourth reference range is a value that is a predetermined percentage larger than the maximum value of the third reference range. The minimum value of the fourth reference range is a value that is a predetermined percentage smaller than the minimum value of the third reference range. The fourth reference range may be a range between a value near the maximum value and a value near the minimum value. If the average temperature of the molten pool MP satisfies the fourth reference range, that is, if the judgment unit 57 judges that the value of the energy density ED can be set within the desired range by repairing the formed solidified layer, the process proceeds to step S69. In this case, if the average temperature of the molten pool MP satisfies the third standard range, the judgment unit 57 judges that generation of change information is necessary, and if the third standard range is not satisfied, the judgment unit 57 judges that repair of the solidified layer is necessary.
[0246] If the average temperature of the molten pool MP does not satisfy the fourth standard range, i.e., if the judgment unit 57 judges that the energy density ED cannot be brought into the desired range even if the formed solidified layer is repaired, the processing proceeds to step S70. The fourth reference range may be set so that the power density PD and the temperature distribution T(r) are kept within a desired range, not limited to the energy density ED, when the molded solidified layer is repaired. The average temperature range, which is the fourth reference range, may be a temperature range between the melting point and liquidus temperature of the powder material P used and between the melting point and solidus temperature. The fourth reference range is stored in advance in the storage unit 58.
[0247] In step S69, the calculation unit 56 generates repair information for performing the repair process. As the repair process, the modeling apparatus 1 performs, for example, a remelt process in which the modeled solidified layer is melted and solidified by irradiating the solidified layer with a laser beam again. In this case, the calculation unit 56 generates, as repair information, values of modeling conditions for the irradiation unit 32 to irradiate the laser beam, that is, values of the laser output, ...
Claims
1. A modeling system for forming a three-dimensional object by solidifying a powder material melted by irradiation with an energy beam, comprising: an acquisition unit that acquires information on at least a part of a molten portion when the molten portion is formed by irradiating the powder material with an energy beam; a modeling unit that models the three-dimensional object under modeling conditions that are set based on a melted state of at least a part of the melt portion that is determined based on the acquired information, A modeling system in which the modeling conditions include a scanning pitch of the energy beam.
2. In the molding system according to claim 1, the modeling conditions include support part conditions related to a support part that supports at least a part of the three-dimensional object, A molding system in which the support conditions include a temperature of the support.
3. In the molding system according to claim 1, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object from a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; the modeling conditions include material layer formation conditions for forming the material layer, The material layer forming conditions are The material layer forming conditions include a moving speed of a material layer forming member that forms the material layer, and and a wait time before starting to form the material layer on top of the solidified layer.
4. In the molding system according to claim 1, the modeling conditions include design data related to a shape of the three-dimensional object, A modeling system in which the design data regarding the shape includes shape data of a support part that supports at least a portion of the three-dimensional object.
5. In the molding system according to claim 1, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, A modeling system in which the conditions of the energy beam include an oscillation mode of the energy beam.
6. In the molding system according to claim 5, An embodied modeling system, wherein the energy beam oscillation mode includes at least one of continuous oscillation and pulse oscillation.
7. In the molding system according to claim 1, the molding conditions include conditions related to an atmosphere inside a housing in which the powder material is melted by irradiation with the energy beam, A molding system, wherein the conditions related to the atmosphere inside the enclosure include pressure inside the enclosure.
8. In the molding system according to claim 1, the molding conditions include conditions of the energy rays irradiated to the powder material in order to melt the powder material, A modeling system in which the energy beam conditions include an intensity distribution of the energy beam.
9. In the molding system according to claim 8, A modeling system in which the intensity distribution of the energy beam includes at least one of a Gaussian distribution and a top hat distribution.
10. In the molding system according to any one of claims 1 to 9, A molding system in which the molten state of at least a portion of the molten portion, determined based on the acquired information, includes information regarding the temperature of at least a portion of the molten portion.
11. In the molding system according to any one of claims 1 to 9, The acquisition unit is a molding system that acquires the information based on thermal radiation light from at least a portion of the molten portion.
12. In the molding system according to any one of claims 1 to 9, The acquisition unit is configured to acquire information of at least a portion of a predetermined region including the molten portion, the modeling unit is configured to model the three-dimensional object under modeling conditions that are set based on a state of at least a part of the specified area and that are determined based on the acquired information of at least a part of the specified area, A modeling system in which the state of at least a portion of the specified region determined based on the acquired information of at least a portion of the specified region includes the state of the powder material before it is melted by irradiation with the energy beam.
13. In the molding system according to any one of claims 1 to 9, The acquisition unit is configured to acquire information of at least a portion of a predetermined region including the molten portion, the modeling unit is configured to model the three-dimensional object under modeling conditions that are set based on a state of at least a part of the specified area and that are determined based on the acquired information of at least a part of the specified area, A molding system in which the state of at least a portion of the specified area determined based on the acquired information of at least a portion of the specified area includes at least one of the state of spatter generated by the melting and the state of fumes generated by the melting.
14. In the molding system according to claim 13, A molding system in which the state of the sputtering includes information on at least one of the direction, amount, and speed of the sputtering, and the state of the fumes includes information on at least one of the concentration and range of the fumes.
15. The molding system according to any one of claims 1 to 9, The acquisition unit is configured to acquire information of at least a portion of a predetermined region including the molten portion, the modeling unit is configured to model the three-dimensional object under modeling conditions that are set based on a state of at least a part of the specified area and that are determined based on the acquired information of at least a part of the specified area, The acquired information on at least a portion of the predetermined region includes luminance information for each different wavelength included in image data obtained by capturing an image of at least a portion of the predetermined region, A molding system in which the state of at least a portion of the specified region is determined based on the acquired information of at least a portion of the specified region, and the state includes at least one of the following information: information regarding the temperature of at least a portion of the molten portion, at least one of information regarding the direction, amount, and speed of sputtering, and at least one of information regarding the concentration and range of fumes.
16. In the molding system according to any one of claims 1 to 9, The modeling unit is a modeling system that performs modeling on the unmelted powder material under the modeling conditions that were set when the powder material was melted to form the three-dimensional object.
17. In the molding system according to any one of claims 1 to 9, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object using a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; The modeling unit is a modeling system that performs modeling on the powder material supplied to the top of the solidified layer or the powder material supplied to the top of the solidified layer under the set modeling conditions.
18. In the molding system according to any one of claims 1 to 9, The modeling unit is a modeling system that, after modeling of the three-dimensional object is completed, performs modeling of a new three-dimensional object to be modeled under the set modeling conditions.
19. In the molding system according to claim 5 or 8, The conditions of the energy beam further include at least one of the output of the energy beam, the wavelength of the energy beam, the polarization state of the energy beam, and the spot size of the energy beam irradiating the powder material.
20. In the molding system according to any one of claims 1 to 9, A molding system in which the molding conditions further include a scanning speed of the energy beam.
21. In the molding system according to claim 7, A molding system in which conditions related to the atmosphere inside the housing include, in addition to the pressure inside the housing, at least one of the following conditions: the type of inert gas introduced into the housing, the flow rate of the inert gas introduced into the housing, the flow velocity of the inert gas introduced into the housing, the oxygen concentration inside the housing, and the temperature inside the housing.
22. In the molding system according to claim 3, The material layer forming conditions further include at least one of the following conditions: the pressure applied to the powder material by the material layer forming member, the shape of the material layer forming member, the material of the material layer forming member, and the lamination thickness of the material layer.
23. In the molding system according to claim 2, A modeling system in which the support conditions further include a type of the support.
24. In the molding system according to claim 4, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object using a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; the design data relating to the shape further includes at least one of shape data of the solidified layer to be modeled, modeling attitude data, and shape data of the three-dimensional object; A modeling system, wherein the shape data of the support part that supports at least a portion of the three-dimensional object is shape data of the support part that supports at least a portion of the solidified layer.
25. The molding system according to any one of claims 1 to 9, The modeling unit is a modeling system that models the three-dimensional object using conditions related to the powder material as the modeling conditions.
26. In the molding system according to claim 25, A molding system in which the conditions related to the powder material include at least one of the following conditions: particle size distribution of the powder material, moisture absorption of the powder material, oxygen concentration of the powder material, and type of the powder material.
27. In the molding system according to any one of claims 1 to 9, The acquisition unit is configured to acquire information of at least a portion of a predetermined region including the molten portion, the modeling unit is configured to model the three-dimensional object under modeling conditions that are set based on a state of at least a part of the specified area and that are determined based on the acquired information of at least a part of the specified area, The modeling system further includes a judgment unit that judges whether or not repair is necessary for the portion where the powder material melted by irradiation with the energy beam has solidified, based on the condition of at least a portion of the specified area, which is obtained based on the information of at least a portion of the specified area acquired.
28. In the molding system according to any one of claims 1 to 9, The acquisition unit is configured to acquire information of at least a portion of a predetermined region including the molten portion, the modeling unit is configured to model the three-dimensional object under modeling conditions that are set based on a state of at least a part of the specified area and that are determined based on the acquired information of at least a part of the specified area, The modeling system further includes a determination unit that determines whether or not it is necessary to generate change information for changing the modeling conditions that are set based on the state of at least a portion of the specified area, the change information being obtained based on information of at least a portion of the specified area.
29. In the molding system according to claim 27, The determination unit determines that it is necessary to generate change information for changing the modeling conditions when the state of at least a portion of the specified area determined based on the information of at least a portion of the specified area acquired by the acquisition unit satisfies a first reference value, and determines that it is necessary to repair the portion where the powder material melted by irradiation with the energy beam has solidified when the state of at least a portion of the specified area determined based on the information of at least a portion of the specified area acquired by the acquisition unit does not satisfy the first reference value.
30. In the molding system according to claim 27, The determination unit determines that repair is necessary for a portion of the powder material melted by the irradiation of the energy beam and solidified, when the state of at least a portion of the specified region determined based on the information of at least a portion of the specified region acquired by the acquisition unit satisfies a second reference value, and determines that it is necessary to stop modeling of the three-dimensional object, when the state of at least a portion of the specified region determined based on the information of at least a portion of the specified region acquired by the acquisition unit does not satisfy the second reference value.
31. In the molding system according to claim 27, When the judgment unit determines that repair is necessary for the portion of the powder material that was melted by the irradiation of the energy beam and has now solidified, the modeling unit repairs the three-dimensional object based on repair information for re-melting at least a portion of the portion of the powder material that was melted by the irradiation of the energy beam and has now solidified, in a modeling system.
32. The molding system according to claim 27, When the judgment unit determines that repair is necessary for the portion where the powder material melted by the irradiation of the energy beam has solidified, the modeling unit repairs the three-dimensional object based on repair information for repairing the portion by applying heat treatment to at least a portion of the portion where the powder material melted by the irradiation of the energy beam has solidified.
33. In the molding system according to any one of claims 1 to 9, A detection unit for determining the melted state based on the information acquired by the acquisition unit is further provided. The modeling unit is a modeling system that models the three-dimensional object under the modeling conditions that are set based on the melting state determined by the detection unit.
34. In the molding system according to any one of claims 1 to 9, a calculation unit that generates the modeling conditions based on the melted state obtained based on the information acquired by the acquisition unit, The modeling unit is a modeling system that models the three-dimensional object under the modeling conditions generated by the calculation unit.
35. In the molding system according to any one of claims 1 to 9, the acquisition unit acquires information on at least a portion of a predetermined region including a molten portion in which the powder material is melted by the irradiation of the energy beam; The modeling system further includes a detection unit that determines a state of at least a portion of the specified area based on acquired information of at least a portion of the specified area.
36. In the molding system according to claim 35, A modeling system in which the information acquired by the acquisition unit includes image data of light having a first wavelength from at least a portion of the specified area and light having a second wavelength different from the first wavelength from at least a portion of the specified area.
37. A method for forming a three-dimensional object by solidifying a powder material melted by irradiation with an energy beam, comprising the steps of: When a molten portion in which the powder material is melted by irradiation with an energy beam is formed, information on at least a part of the molten portion is acquired; forming the three-dimensional object under modeling conditions that are set based on a melted state of at least a part of the melt portion that is determined based on the acquired information, A modeling method in which the modeling conditions include a scanning pitch of the energy beam.
38. In the molding method according to claim 37, the modeling conditions include support part conditions related to a support part that supports at least a part of the three-dimensional object, A molding method, wherein the support part condition includes a temperature of the support part.
39. In the molding method according to claim 37, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object from a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; the modeling conditions include material layer formation conditions for forming the material layer, The material layer forming conditions are The material layer forming conditions include a moving speed of a material layer forming member that forms the material layer, and and a waiting period before starting to form the material layer on top of the solidified layer.
40. The molding method according to claim 37, the modeling conditions include design data related to a shape of the three-dimensional object, A modeling method, wherein the design data relating to the shape includes shape data of a support part that supports at least a part of the three-dimensional object.
41. The molding method according to claim 37, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, A modeling method in which the conditions of the energy beam include an oscillation mode of the energy beam.
42. In the molding method according to claim 41, A modeling method in which the oscillation mode of the energy beam includes at least one of continuous oscillation and pulse oscillation.
43. The molding method according to claim 37, the molding conditions include conditions related to an atmosphere inside a housing in which the powder material is melted by irradiation with the energy beam, A molding method, wherein the conditions related to the atmosphere inside the housing include the pressure inside the housing.
44. The molding method according to claim 37, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, A modeling method in which the conditions of the energy beam include an intensity distribution of the energy beam.
45. In the molding method according to claim 44, A modeling method in which the intensity distribution of the energy beam includes at least one of a Gaussian distribution and a top hat distribution.
46. A computer-readable medium having recorded thereon a modeling program that causes a computer to execute processing in the modeling method described in any one of claims 37 to 45.
47. An information acquisition device used to set modeling conditions for a three-dimensional object formed by solidifying a powder material melted by irradiation with an energy beam, comprising: an acquisition unit that acquires information on at least a part of a molten portion when the molten portion is formed by irradiating the powder material with the energy beam; an output unit that outputs the acquired information, the three-dimensional object is modeled under modeling conditions that are set based on a melted state of at least a part of the melt portion that is determined based on the information output from the output unit, An information acquisition device in which the modeling conditions include a scanning pitch of the energy beam.
48. In the information acquisition device according to claim 47, the modeling conditions include support part conditions related to a support part that supports at least a part of the three-dimensional object, The information acquisition device, wherein the support part condition includes a temperature of the support part.
49. In the information acquisition device according to claim 47, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object from a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; the modeling conditions include material layer formation conditions for forming the material layer, The material layer forming conditions are The material layer forming conditions include a moving speed of a material layer forming member that forms the material layer, and and a waiting time before starting to form the material layer on top of the solidified layer.
50. In the information acquisition device according to claim 47, the modeling conditions include design data related to a shape of the three-dimensional object, The information acquisition device, wherein the design data relating to the shape includes shape data of a support portion that supports at least a portion of the three-dimensional object.
51. In the information acquisition device according to claim 47, the molding conditions include conditions of the energy rays irradiated to the powder material in order to melt the powder material, An information acquisition device, wherein the conditions of the energy beam include an oscillation mode of the energy beam.
52. In the information acquisition device according to claim 51, An information acquisition device, wherein the oscillation mode of the energy beam includes at least one of continuous oscillation and pulse oscillation.
53. In the information acquisition device according to claim 47, the molding conditions include conditions related to an atmosphere inside a housing in which the powder material is melted by irradiation with the energy beam, An information acquisition device, wherein the conditions related to the atmosphere inside the housing include pressure inside the housing.
54. In the information acquisition device according to claim 47, the molding conditions include conditions of the energy rays irradiated to the powder material in order to melt the powder material, An information acquisition device in which the conditions of the energy beam include an intensity distribution of the energy beam.
55. In the information acquisition device according to claim 54, An information acquisition device, wherein the intensity distribution of the energy beam includes at least one of a Gaussian distribution and a top hat distribution.
56. An information processing method for use in an information acquisition device used to set modeling conditions for a three-dimensional object formed by solidifying a powder material melted by irradiation with an energy beam, comprising: acquiring information on at least a part of the molten portion when the molten portion is formed by irradiating the energy beam with the powder material; and outputting the acquired information. The three-dimensional object is formed under modeling conditions that are set based on a melted state of at least a part of the melt portion that is determined based on the output information, An information processing method, wherein the modeling conditions include a scanning pitch of the energy beam.
57. The information processing method according to claim 56, the modeling conditions include support part conditions related to a support part that supports at least a part of the three-dimensional object, An information processing method, wherein the support part condition includes a temperature of the support part.
58. The information processing method according to claim 56, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object from a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; the modeling conditions include material layer formation conditions for forming the material layer, The material layer forming conditions are The material layer forming conditions include a moving speed of a material layer forming member that forms the material layer, and and a waiting time until starting to form the material layer on top of the solidified layer.
59. The information processing method according to claim 56, the modeling conditions include design data related to a shape of the three-dimensional object, An information processing method, wherein the design data relating to the shape includes shape data of a support portion that supports at least a portion of the three-dimensional object.
60. The information processing method according to claim 56, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, An information processing method, wherein the condition of the energy beam includes an oscillation mode of the energy beam.
61. The information processing method according to claim 60, The information processing method, wherein the oscillation mode of the energy beam includes at least one of continuous oscillation and pulse oscillation.
62. The information processing method according to claim 56, the molding conditions include conditions related to an atmosphere inside a housing in which the powder material is melted by irradiation with the energy beam, An information processing method, wherein the condition related to the atmosphere inside the housing includes pressure inside the housing.
63. The information processing method according to claim 56, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, An information processing method, wherein the condition of the energy beam includes an intensity distribution of the energy beam.
64. The information processing method according to claim 63, An information processing method, wherein the intensity distribution of the energy beam includes at least one of a Gaussian distribution and a top-hat distribution.
65. A computer-readable medium having recorded thereon an information processing program that causes a computer to execute the processing in the information processing method described in any one of claims 56 to 64.
66. A computing device used in a modeling device that forms a three-dimensional object by solidifying a powder material melted by irradiation with energy rays, comprising: a detection unit for detecting a melting state of at least a part of a melting portion in which the powder material is melted by irradiation with an energy beam; a molding condition of the molding apparatus is set based on a melted state of at least a part of the melted portion acquired by the detection unit, An arithmetic device in which the modeling conditions include a scanning pitch of the energy beam.
67. The computing device of claim 66, the modeling conditions include support part conditions related to a support part that supports at least a part of the three-dimensional object, A computing device in which the support part condition includes a temperature of the support part.
68. The computing device of claim 66, the modeling unit forms a layer of material using the powder material, and models the three-dimensional object from a solidified layer formed by solidifying at least a portion of the material layer that has been melted by the irradiation of the energy beam; the modeling conditions include material layer formation conditions for forming the material layer, The material layer forming conditions are The material layer forming conditions include a moving speed of a material layer forming member that forms the material layer, and and a wait time before starting to form the material layer on top of the solidified layer.
69. The computing device of claim 66, the modeling conditions include design data related to a shape of the three-dimensional object, A computing device, wherein the design data relating to the shape includes shape data of a support portion that supports at least a portion of the three-dimensional object.
70. The computing device of claim 66, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, A computing device in which the conditions of the energy beam include an oscillation mode of the energy beam.
71. The computing device of claim 70, An arithmetic device, wherein the oscillation mode of the energy beam includes at least one of continuous oscillation and pulse oscillation.
72. The computing device of claim 66, the molding conditions include conditions related to an atmosphere inside a housing in which the powder material is melted by irradiation with the energy beam, A computing device, wherein the conditions related to the atmosphere inside the housing include a pressure inside the housing.
73. The computing device of claim 66, the molding conditions include conditions of the energy beam irradiated to the powder material in order to melt the powder material, A computing device in which the conditions of the energy beam include an intensity distribution of the energy beam.
74. The computing device of claim 73, A computing device in which the intensity distribution of the energy beam includes at least one of a Gaussian distribution and a top-hat distribution.
75. The computing device according to any one of claims 66 to 74, The computing device further includes an output device configured to output the melted state of at least a portion of the melted portion acquired by the detection unit.
76. The arithmetic device according to any one of claims 66 to 74, a calculation unit configured to generate change information for changing modeling conditions used for modeling the three-dimensional object, based on the melted state of at least a part of the melted portion acquired by the detection unit, The modeling condition of the modeling apparatus is changed based on the change information generated by the calculation unit.
77. The arithmetic device according to any one of claims 66 to 74, The detection unit is further configured to acquire a state of at least a part of a predetermined region including the molten portion, A computing device in which the state of at least a portion of the specified region includes the state of the powder material before it is melted by irradiation with the energy beam.
78. The arithmetic device according to any one of claims 66 to 74, The detection unit is further configured to acquire information of at least a portion of a predetermined region including the molten portion, A computing device, wherein the state of at least a portion of the specified region includes at least one of a state of spatter generated by the melting and a state of fumes generated by the melting.
79. The computing device of claim 78, A computing device in which the molten state of at least a portion of the molten portion includes information regarding the temperature of at least a portion of the molten portion, the state of the sputtering includes at least one piece of information regarding the scattering direction, scattering amount, and scattering speed of the sputtering, and the state of the fumes includes at least one piece of information regarding the concentration and range of the fumes.
80. The arithmetic device according to any one of claims 66 to 74, The detection unit is configured to acquire a state of at least a part of a predetermined region including the molten portion, A computing device configured such that, based on brightness information for different wavelengths contained in image data capturing at least a portion of the specified region, the detection unit acquires at least one of the following information: information regarding the temperature of at least a portion of the molten portion; at least one of information regarding the direction, amount, and speed of sputtering; and at least one of information regarding the concentration and range of fumes.
81. The computing device of claim 76, The detection unit is configured to acquire a state of at least a part of a predetermined region including the molten portion, The calculation unit is configured to generate the change information based on a state of at least a portion of the predetermined area acquired by the detection unit.
82. The computing device of claim 76, The calculation unit is a calculation device configured to generate change information for changing modeling conditions related to unmelted powder material when the three-dimensional object is formed by melting the powder material.
83. The computing device of claim 76, the modeling apparatus forms a layer of material using the powder material, and models the three-dimensional object using a solidified layer formed by solidifying at least a portion of the material layer that has been melted by irradiation with the energy beam; The calculation unit is a calculation device configured to generate the change information for changing the powder material supplied to the top of the solidified layer or the molding conditions for the powder material supplied to the top of the solidified layer.
84. The computing device of claim 76, The calculation unit is a calculation device configured to generate, after completion of modeling of the three-dimensional object, the change information for changing the modeling conditions for a new three-dimensional object to be modeled.
85. The computing device of claim 70 or 73, The conditions of the energy beam further include at least one condition of the output of the energy beam, the oscillation mode of the energy beam, the wavelength of the energy beam, the polarization state of the energy beam, and the spot size of the energy beam irradiating the powder material.
86. The arithmetic device according to any one of claims 66 to 74, A calculation device in which the modeling conditions further include a scanning speed of the energy beam.
87. The computing device of claim 72, A computing device in which the conditions related to the atmosphere inside the housing include, in addition to the pressure inside the housing, at least one condition of the type of inert gas introduced into the housing, the flow rate of the inert gas introduced into the housing, the flow velocity of the inert gas introduced into the housing, the oxygen concentration inside the housing, and the temperature inside the housing.
88. The computing device of claim 68, The material layer forming conditions further include at least one condition of the pressure applied to the powder material by the material layer forming member, the shape of the material layer forming member, the material of the material layer forming member, and the lamination thickness of the material layer.
89. The computing device of claim 67, A computing device in which the support part condition further includes a type of the support part.
90. The computing device of claim 69, the modeling apparatus forms a layer of material using the powder material, and models the three-dimensional object using a solidified layer formed by solidifying at least a portion of the material layer that has been melted by irradiation with the energy beam; the design data relating to the shape further includes at least one of shape data of the solidified layer to be modeled, modeling attitude data, and shape data of the three-dimensional object; A computing device, wherein the shape data of the support portion is shape data of the support portion that supports at least a portion of the solidified layer.
91. The arithmetic device according to any one of claims 66 to 74, A calculation device in which the molding conditions include conditions related to the powder material as the molding conditions.
92. The computing device of claim 91, A calculation device in which the conditions related to the powder material include at least one condition of a particle size distribution of the powder material, a moisture absorption of the powder material, an oxygen concentration of the powder material, and a type of the powder material.
93. The computing device of claim 76, The detection unit is configured to acquire a state of at least a part of a predetermined region including the molten portion, The computing device further includes a judgment unit that judges whether or not repair is required for the portion where the powder material melted by irradiation with the energy beam and solidified is solidified, and / or whether or not the change information is required to be generated, based on the state of at least a portion of the specified area acquired by the detection unit.
94. The computing device of claim 93, The determination unit is determining that it is necessary to generate change information for changing the modeling conditions when the state of at least a portion of the specified region acquired by the detection unit satisfies a first reference value, and determining that it is necessary to repair a portion where the powder material melted by the irradiation of the energy beam has solidified when the state of at least a portion of the specified region acquired by the detection unit does not satisfy the first reference value; and / or determining that repair is required for a portion where the powder material melted by the irradiation of the energy beam and solidified is required, when the state of at least a part of the specified region acquired by the detection unit satisfies a second reference value, and determining that modeling of the three-dimensional object needs to be stopped, when the state of at least a part of the specified region acquired by the detection unit does not satisfy the second reference value.
95. The computing device of claim 93, When the judgment unit determines that repair is necessary for the portion of the powder material that was melted by the irradiation of the energy beam and has now solidified, the calculation unit is a calculation device that generates repair information for re-melting at least a portion of the portion of the powder material that was melted by the irradiation of the energy beam and has now solidified, thereby repairing the portion.
96. An acquisition unit that acquires information about at least a portion of a molten portion in which a powder material is melted by irradiation with an energy beam; and a computing device according to any one of claims 66 to 95, The calculation unit of the calculation device is configured to acquire a melted state of at least a portion of the melt portion based on information acquired by the acquisition unit.
97. The detection system of claim 96, A detection system, wherein the information acquired by the acquisition unit includes image data of light of a first wavelength from at least a portion of the specified area, and light of a second wavelength different from the first wavelength from at least a portion of the specified area.
98. A molding apparatus comprising: A computing device according to any one of claims 66 to 95, a setting device that sets a modeling condition of the modeling apparatus based on the melted state output from the arithmetic device; and and a modeling unit that forms a three-dimensional object by solidifying the powder material melted by irradiating it with energy rays based on the modeling conditions set by the setting device.
99. A molding apparatus comprising: A detection system according to claim 96 or 97; a setting device that sets a modeling condition of the modeling apparatus based on the melted state output from the arithmetic device of the detection system; and and a modeling unit that forms a three-dimensional object by solidifying the powder material melted by irradiating it with energy rays based on the modeling conditions set by the setting device.
100. A molding apparatus comprising: A setting device that sets a modeling condition of the modeling device based on the melted state output from the arithmetic device according to any one of claims 66 to 95; and a modeling unit that forms a three-dimensional object by solidifying the powder material melted by irradiating it with energy rays based on the modeling conditions set by the setting device.
101. A calculation method used in a modeling apparatus for a three-dimensional object formed by solidifying a powder material melted by irradiation with an energy beam, comprising: acquiring a molten state of at least a part of a molten portion in which the powder material is melted by the irradiation of the energy beam, a molding condition of the molding apparatus is set based on the acquired melted state of at least a part of the melted portion, The modeling conditions include a scanning pitch of the energy beam.
102. The method of claim 101, the modeling conditions include support part conditions related to a support part that supports at least a part of the three-dimensional object, The support part condition includes a temperature of the support part.
103. The method of claim 101, the modeling apparatus forms a layer of material using the powder material, and models the three-dimensional object from a solidified layer in which at least a portion of the material layer melted by irradiation with the energy beam is solidified; the modeling conditions include material layer formation conditions for forming the material layer, The material layer forming conditions are The material layer forming conditions include a moving speed of a material layer forming member that forms the material layer, and and a waiting time before starting to form the material layer on top of the solidified layer.
104. The method of claim 101, the modeling conditions include design data related to a shape of the three-dimensional object, The design data relating to the shape includes shape data of a support portion that supports at least a portion of the three-dimensional object.
105. The method of claim 101, the molding conditions include conditions of the energy rays irradiated to the powder material in order to melt the powder material, A calculation method in which the conditions of the energy beam include an oscillation mode of the energy beam.
106. The method of claim 105, The oscillation mode of the energy beam includes at least one of continuous oscillation and pulse oscillation.
107. The method of claim 101, the molding conditions include conditions related to an atmosphere inside a housing in which the powder material is melted by irradiation with the energy beam, A calculation method, wherein the condition related to the atmosphere inside the housing includes a pressure inside the housing.
108. The method of claim 101, the molding conditions include conditions of the energy rays irradiated to the powder material in order to melt the powder material, A calculation method in which the condition of the energy beam includes an intensity distribution of the energy beam.
109. The method of claim 108, A calculation method in which the intensity distribution of the energy beam includes at least one of a Gaussian distribution and a top-hat distribution.
110. Obtaining information on at least a portion of a molten portion in which a powder material is melted by irradiation with an energy beam; A detection method comprising: acquiring a molten state of at least a portion of the molten portion by the calculation method according to any one of claims 66 to 95.
111. The detection method according to claim 110, A detection method in which the acquired information includes image data of light of a first wavelength from at least a portion of the specified area, and light of a second wavelength different from the first wavelength from at least a portion of the specified area.
112. Setting a molding condition of the molding apparatus based on the melted state obtained by the calculation method according to any one of claims 101 to 109; and forming a three-dimensional object by solidifying the powder material melted by irradiating it with energy rays based on the set forming conditions.
113. Setting a molding condition of a molding apparatus based on the melting state obtained by the detection method according to claim 110 or 111; and forming a three-dimensional object by solidifying the powder material melted by irradiating it with energy rays based on the set forming conditions.
114. A computer-readable medium having recorded thereon an arithmetic program for causing a computer to execute the processing in the arithmetic method described in any one of claims 101 to 109.
115. A computer-readable medium having recorded thereon a detection program that causes a computer to execute the processing in the detection method described in claim 110 or 111.
116. A computer-readable medium having recorded thereon a modeling program that causes a computer to execute the processing in the modeling method described in claim 112 or 113.