Lithium ion secondary battery and charging method thereof
A lithium ion secondary battery with a non-aqueous electrolyte and LiNiMnO4 positive electrode ensures thermal stability and high voltage operation, addressing the limitations of existing batteries by preventing corrosion and maintaining performance at 4.6V and above.
Patent Information
- Application Number
- JP2023045601
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
Existing lithium ion secondary batteries lack thermal stability and cannot be driven at high voltages above 4.6V, necessitating improvements in electrolyte additives and electrode materials.
A lithium ion secondary battery comprising a non-aqueous electrolyte with a higher molar concentration of cyclic anion-containing lithium salts, a positive electrode with LiNiMnO4, and a current collector foil of aluminum, ensuring thermal stability and enabling operation at high voltages up to 4.8V.
The battery achieves thermal stability and can be charged to high voltages of 4.6V or higher, maintaining performance and preventing corrosion of the aluminum current collector foil.
Smart Images

Figure 2024135086000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a lithium ion secondary battery and a charging method thereof. [Background technology]
[0002] The uses of lithium-ion batteries are changing with the global trend of electrifying automobiles. In order to achieve higher energy density, development of batteries that can be driven at high voltages (hereinafter sometimes abbreviated as "high-voltage batteries") is progressing. Against this background, not only are electrode materials being improved, but additives to electrolytes and lithium salts are also being developed.
[0003] For example, Patent Document 1 reports that by using an electrolyte solution that combines an imide-based alkali metal salt represented by a specific general formula with a specific amount of a fluorine-containing carbonate, corrosion of the aluminum current collector foil can be prevented, thereby realizing a high-voltage battery of 4.2 V or more. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2014-203748 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, Patent Document 1 does not disclose anything about providing a battery that can ensure the thermal stability of the electrolyte and can be driven at a high voltage of 4.6 V or more.
[0006] The problem to be solved by the present invention is to provide a lithium ion secondary battery capable of ensuring the thermal stability of the electrolyte and being driven at a high voltage of 4.6 V or more. Another problem to be solved by the present invention is to provide a method for charging such a lithium ion secondary battery. [Means for solving the problem]
[0007] One aspect of the present invention is as follows. [1] A lithium ion secondary battery comprising: a positive electrode containing a lithium compound containing Li, Ni, Mn, and O as a positive electrode active material, and aluminum as a current collecting foil; a negative electrode containing graphite as a negative electrode active material; and a non-aqueous electrolyte solution, The non-aqueous electrolyte solution is The lithium salt includes a non-aqueous solvent and a cyclic anion-containing lithium salt, and may include a non-cyclic anion-containing lithium salt; The lithium ion secondary battery has a higher molar concentration of the cyclic anion-containing lithium salt in an electrolyte solvent than that of the non-cyclic anion-containing lithium salt. [2] The positive electrode active material is represented by the following formula (A): Li x Ni y Mn z O4... (A) {where, 0.9≦x≦1.1, 0 <y<1、1<z<2である。} 2. The lithium ion secondary battery according to item 1, comprising lithium nickel manganese oxide represented by the formula: [3] The cyclic anion-containing lithium salt is represented by the following formula (1): [ka] {where, R f each independently represents a fluorine atom or a perfluoro group having 4 or less carbon atoms, and n is an integer of 1 to 5.} 3. The lithium ion secondary battery according to item 1 or 2, comprising a compound represented by the formula: [4] The cyclic anion-containing lithium salt is represented by the following formula (1-2): [ka] 4. The lithium ion secondary battery according to any one of items 1 to 3, having a compound structure represented by the following formula: [5] 5. The lithium ion secondary battery according to any one of items 1 to 4, wherein the non-cyclic anion-containing lithium salt contains LiPF6. [6] 6. A method for charging a lithium ion secondary battery, comprising the step of charging the lithium ion secondary battery according to any one of items 1 to 5 at a voltage of 4.6 V or higher. [7] 7. A method for charging a lithium ion secondary battery according to claim 6, comprising the step of charging at a voltage of 4.7 V or higher. [8] 8. A method for charging a lithium ion secondary battery according to claim 6, comprising the step of charging at a voltage of 4.8 V or higher. Effect of the Invention
[0008] According to the present invention, it is possible to provide a lithium ion secondary battery which can ensure the thermal stability of the electrolyte and can be driven at a high voltage of 4.6 V or more. Furthermore, according to the present invention, it is possible to provide a charging method for charging such a lithium ion secondary battery at a high voltage. [Brief description of the drawings]
[0009] [Figure 1] 1 is a plan view illustrating a schematic example of a nonaqueous secondary battery according to an embodiment of the present invention. [Diagram 2] 2 is a cross-sectional view taken along line AA in FIG. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention (hereinafter, simply referred to as "the present embodiment") will be described. In this specification, a numerical range described using "to" includes the numerical values described before and after it. In this specification, an upper limit or lower limit value in a numerical range described in stages may be replaced with a corresponding upper limit or lower limit value in another numerical range described in stages, or may be replaced with a corresponding value in an example.
[0011] <Non-aqueous secondary battery> The nonaqueous secondary battery of this embodiment is a secondary battery comprising the above-mentioned nonaqueous electrolyte together with a positive electrode and a negative electrode, and may be, for example, a lithium ion battery, more specifically, a lithium ion battery as shown in a schematic plan view in FIG. 1 and a schematic cross-sectional view in FIG. 2. The lithium ion battery 100 shown in FIGS. 1 and 2 comprises a separator 170, a positive electrode 150 and a negative electrode 160 sandwiching the separator 170 from both sides, a positive electrode lead body 130 (connected to the positive electrode 150) and a negative electrode lead body 140 (connected to the negative electrode 160) sandwiching a laminate of these (the separator 170, the positive electrode 150, and the negative electrode 160), and a battery exterior 110 that houses them. The laminate of the positive electrode 150, the separator 170, and the negative electrode 160 is impregnated with the nonaqueous electrolyte according to this embodiment.
[0012] <1.Non-aqueous electrolyte> The "non-aqueous electrolyte" in this embodiment refers to a non-aqueous electrolyte containing 1% by mass or less of water relative to the total amount of the non-aqueous electrolyte and containing a non-aqueous solvent and a lithium salt (particularly, a cyclic anion-containing lithium salt). The non-aqueous electrolyte according to this embodiment is preferably free of water as much as possible, but may contain a very small amount of water as long as it does not impede the solution of the problem of the present invention. The content of such water is 300 ppm by mass or less, preferably 200 ppm by mass or less, based on the total amount of the non-aqueous electrolyte. As long as the non-aqueous electrolyte has a configuration for achieving the solution of the problem of the present invention, the other components can be appropriately selected and applied from the constituent materials in the known non-aqueous electrolyte used in lithium ion batteries.
[0013] In particular, the nonaqueous electrolyte of this embodiment is The lithium salt includes a non-aqueous solvent and a cyclic anion-containing lithium salt, and may include a non-cyclic anion-containing lithium salt; The cyclic anion-containing lithium salt has a higher molar concentration in the non-aqueous electrolyte than the non-cyclic anion-containing lithium salt.
[0014] <1-1.Non-aqueous solvents> In the present embodiment, the term "non-aqueous solvent" refers to elements in the non-aqueous electrolyte excluding lithium salt and various additives. When the non-aqueous electrolyte contains an additive for protecting electrodes, the term "non-aqueous solvent" refers to elements in the non-aqueous electrolyte excluding lithium salt and additives other than the additive for protecting electrodes. Examples of non-aqueous solvents include alcohols such as methanol and ethanol; aprotic solvents, etc. Among them, aprotic solvents are preferred as non-aqueous solvents. The non-aqueous solvent may contain a solvent other than the aprotic solvent as long as it does not hinder the problem solving of the present invention. The non-aqueous solvent for the non-aqueous electrolyte includes a chain carbonate and a cyclic carbonate.
[0015] By using a fluorinated solvent, it is possible to suppress the oxidation-reduction reaction of the electrolyte itself, and a fluorinated chain carbonate or a fluorinated cyclic carbonate such as fluoroethylene carbonate may be added.
[0016] Examples of other aprotic solvents include lactones, organic compounds having sulfur atoms, cyclic ethers, acetonitrile, mononitriles other than acetonitrile, alkoxy group-substituted nitriles, dinitriles, cyclic nitriles, short-chain fatty acid esters, linear ethers, fluorinated ethers, ketones, and compounds in which some or all of the H atoms of the aprotic solvents have been substituted with halogen atoms.
[0017] Examples of fluorine-free cyclic carbonates include ethylene carbonate, propylene carbonate, 1,2-butylene carbonate, trans-2,3-butylene carbonate, cis-2,3-butylene carbonate, 1,2-pentylene carbonate, trans-2,3-pentylene carbonate, cis-2,3-pentylene carbonate, vinylene carbonate (VC), 4,5-dimethylvinylene carbonate, and vinylethylene carbonate;
[0018] Fluoroethylene carbonates include, for example, 4-fluoro-1,3-dioxolane-2-one, 4,4-difluoro-1,3-dioxolane-2-one, cis-4,5-difluoro-1,3-dioxolane-2-one, trans-4,5-difluoro-1,3-dioxolane-2-one, 4,4,5-trifluoro-1,3-dioxolane-2-one, 4,4,5,5-tetrafluoro-1,3-dioxolane-2-one, and 4,4,5-trifluoro-5-methyl-1,3-dioxolane-2-one;
[0019] Lactones include γ-butyrolactone, α-methyl-γ-butyrolactone, γ-valerolactone, γ-caprolactone, δ-valerolactone, δ-caprolactone, and ε-caprolactone;
[0020] Examples of organic compounds having sulfur atoms include ethylene sulfite, propylene sulfite, butylene sulfite, pentene sulfite, sulfolane, 3-sulfolene, 3-methyl sulfolane, 1,3-propane sultone, 1,4-butane sultone, 1-propene 1,3-sultone, dimethyl sulfoxide, tetramethylene sulfoxide, and ethylene glycol sulfite;
[0021] Examples of chain carbonates include ethyl methyl carbonate, dimethyl carbonate, diethyl carbonate, methyl propyl carbonate, methyl isopropyl carbonate, dipropyl carbonate, methyl butyl carbonate, dibutyl carbonate, ethyl propyl carbonate, and diisobutyl carbonate;
[0022] Cyclic ethers include, for example, tetrahydrofuran, 2-methyltetrahydrofuran, 1,4-dioxane, and 1,3-dioxane;
[0023] Examples of mononitriles other than acetonitrile include propionitrile, butyronitrile, valeronitrile, benzonitrile, and acrylonitrile;
[0024] Alkoxy group-substituted nitriles include, for example, methoxyacetonitrile and 3-methoxypropionitrile;
[0025] Dinitriles include, for example, malononitrile, succinonitrile, glutaronitrile, adiponitrile, 1,4-dicyanoheptane, 1,5-dicyanopentane, 1,6-dicyanohexane, 1,7-dicyanoheptane, 2,6-dicyanoheptane, 1,8-dicyanooctane, 2,7-dicyanooctane, 1,9-dicyanononane, 2,8-dicyanononane, 1,10-dicyanodecane, 1,6-dicyanodecane, and 2,4-dimethylglutaronitrile;
[0026] Cyclic nitriles include, for example, benzonitrile;
[0027] Examples of short-chain fatty acid esters include methyl acetate, methyl propionate, methyl isobutyrate, methyl butyrate, methyl isovalerate, methyl valerate, methyl pivalate, methyl hydroangelate, methyl caproate, ethyl acetate, ethyl propionate, ethyl isobutyrate, ethyl butyrate, ethyl isovalerate, ethyl valerate, ethyl pivalate, ethyl hydroangelate, ethyl caproate, propyl acetate, propyl propionate, propyl isobutyrate, propyl butyrate, propyl isovalerate, propyl valerate, propyl pivalate, propyl hydroangelate, propyl caproate, isopropyl acetate, isopropyl propionate, isopropyl isobutyrate, isopropyl butyrate, isopropyl isovalerate, isopropyl valerate, and isopropyl pivalate. propyl, isopropyl hydroangelate, isopropyl caproate, butyl acetate, butyl propionate, butyl isobutyrate, butyl butyrate, butyl isovalerate, butyl valerate, butyl pivalate, butyl hydroangelate, butyl caproate, isobutyl acetate, isobutyl propionate, isobutyl isobutyrate, isobutyl butyrate, isobutyl isovalerate, isobutyl valerate, isobutyl pivalate, isobutyl hydroangelate, isobutyl caproate, tert-butyl acetate, tert-butyl propionate, tert-butyl isobutyrate, tert-butyl butyrate, tert-butyl isovalerate, tert-butyl valerate, tert-butyl pivalate, tert-butyl hydroangelate, and tert-butyl caproate;
[0028] Chain ethers include, for example, dimethoxyethane, diethyl ether, 1,3-dioxolane, diglyme, triglyme, and tetraglyme;
[0029] Examples of fluorinated ethers include Rf 20 -OR 21 (In the formula, Rf 20 represents an alkyl group containing a fluorine atom, and R 7 represents a monovalent organic group which may contain a fluorine atom;
[0030] Ketones, for example, acetone, methyl ethyl ketone, and methyl isobutyl ketone;
[0031] Examples of the aprotic solvent compound in which some or all of the H atoms have been replaced with halogen atoms include compounds in which the halogen atoms are fluorine; Examples include:
[0032] Here, examples of fluorinated chain carbonates include methyl trifluoroethyl carbonate, trifluorodimethyl carbonate, trifluorodiethyl carbonate, trifluoroethylmethyl carbonate, methyl 2,2-difluoroethyl carbonate, methyl 2,2,2-trifluoroethyl carbonate, and methyl 2,2,3,3-tetrafluoropropyl carbonate. The above-mentioned fluorinated chain carbonates are represented by the following general formula: R 1 -OC(O)OR 2 {where, R 1 and R 2 is CH3, CH2CH3, CH2CH2CH3, CH(CH3)2, and CH2Rf 3 Rf is at least one selected from the group consisting of 3 is an alkyl group having 1 to 3 carbon atoms in which a hydrogen atom is substituted with at least one fluorine atom, and R 1 and / or R 2 contains at least one fluorine atom. It can be expressed as:
[0033] Examples of fluorinated short-chain fatty acid esters include fluorinated short-chain fatty acid esters such as 2,2-difluoroethyl acetate, 2,2,2-trifluoroethyl acetate, and 2,2,3,3-tetrafluoropropyl acetate. Fluorinated short-chain fatty acid esters are represented by the following general formula: R 10 -C(O)OR 11 {where, R 10is CH3, CH2CH3, CH2CH2CH3, CH(CH3)2, CF3CF2H, CFH2, CF2Rf 12 , CFHRf 12 , and CH2Rf 13 and R is at least one selected from the group consisting of 11 is CH3, CH2CH3, CH2CH2CH3, CH(CH3)2, and CH2Rf 13 Rf is at least one selected from the group consisting of 12 is an alkyl group having 1 to 3 carbon atoms in which a hydrogen atom may be substituted with at least one fluorine atom, and Rf 13 is an alkyl group having 1 to 3 carbon atoms in which a hydrogen atom is substituted with at least one fluorine atom, and R 10 and / or R 11 contains at least one fluorine atom, and R 10 If is CF2H, R 11 is not CH3. It can be expressed as:
[0034] In the present embodiment, the aprotic solvent may be used alone or in combination of two or more kinds.
[0035] The presence of fluorine atoms in the solvent tends to improve oxidation resistance, but the high polarity of the solvent also tends to reduce impregnation into the separator, etc. In this embodiment, high voltage charging is possible without using a solvent having fluorine atoms, and the solvent contained in the non-aqueous solvent does not need to have fluorine atoms.
[0036] In the present embodiment, the non-aqueous solvent preferably contains at least one cyclic carbonate and at least one chain carbonate in combination, from the viewpoint of improving the stability of the non-aqueous electrolyte solution.
[0037] <1-2. Electrolyte salt> The nonaqueous electrolyte solution of the present embodiment is for use in lithium ion secondary batteries, and contains a cyclic anion-containing lithium salt as a main salt component (a component contained in a larger amount than other lithium salts) as an electrolyte salt.
[0038] Here, in this embodiment, the molar concentration of the cyclic anion-containing lithium salt in the non-aqueous electrolyte is higher than that of the non-cyclic anion-containing lithium salt. Although the mechanism of action is not necessarily clear, this requirement allows the function of the cyclic anion-containing lithium salt to be exerted effectively, ensures the thermal stability of the electrolyte, and provides a battery that can be driven at a high voltage of 4.6V or more.
[0039] In the nonaqueous electrolyte solution of the present embodiment, (Total molar concentration of cyclic anion-containing lithium salt and non-cyclic anion-containing lithium salt) / (Molar concentration of cyclic anion-containing lithium salt) The value calculated by this formula is equal to or greater than 1.0 and less than 2.0, and preferably equal to or greater than 1.0 and less than 1.5.
[0040] The molar concentrations of the cyclic anion-containing lithium salt and the non-cyclic anion-containing lithium salt in the non-aqueous electrolyte solution are derived from the number of moles of each type of lithium salt dissolved relative to the volume of the non-aqueous electrolyte solution during preparation. The molar concentrations of the cyclic anion-containing lithium salt and the non-cyclic anion-containing lithium salt can be analyzed by tracing back from the non-aqueous electrolyte solution based on known analytical methods (e.g., NMR, etc.), and the analytical values (molar concentrations) obtained in this manner can be regarded as the number of moles of each type of lithium salt relative to the volume of the non-aqueous electrolyte solution at the time of preparation.
[0041] The cyclic anion-containing lithium salt preferably includes a lithium salt containing an imide anion having a cyclic structure, and is, for example, a lithium salt represented by the following formula (1): [ka] {where, R f each independently represents a fluorine atom or a perfluoro group having 4 or less carbon atoms, and n is an integer of 1 to 5.} According to this, the effect of the present embodiment can be easily achieved.
[0042] The cyclic anion-containing lithium salt preferably contains a five-membered ring cyclic anion-containing lithium salt, for example, a lithium salt represented by the following formula (1-2): [ka] According to this, the effect of the present embodiment can be more easily achieved. However, the cyclic anion-containing lithium salt is not limited to the structure of the above formula.
[0043] The content of the cyclic anion-containing lithium salt is preferably 0.6 mol or more per 1 L of the non-aqueous solvent, more preferably 0.8 mol or more, and even more preferably 1 mol or more, so that the lithium salt is present in the electrolyte as the main lithium ion component and thus exhibits sufficiently high ionic conductivity.
[0044] By including a cyclic anion-containing lithium salt in the non-aqueous electrolyte, aluminum corrosion may be suppressed even at high voltages, and therefore the non-cyclic anion-containing lithium salt (e.g., LiPF6) for forming an aluminum passivation film may not be included. However, by mixing a small amount of a non-cyclic anion-containing lithium salt, such as LiPF6, the corrosion resistance tends to be improved even at higher voltages, and the amount added is preferably 0.01 mol to 0.5 mol per 1 L of the non-aqueous solvent.
[0045] The lithium salt may include a non-cyclic anion-containing lithium salt. The non-cyclic anion-containing lithium salt may further include a fluorine-containing inorganic lithium salt other than LiPF6, for example, LiBF4, LiAsF6, Li2SiF6, LiSbF6, Li2B 12 F b H 12-b(wherein b is an integer of 0 to 3) and the like may be included. "Inorganic lithium salt" refers to a lithium salt that does not contain a carbon atom in the anion and is soluble in acetonitrile. "Fluorine-containing inorganic lithium salt" refers to a lithium salt that does not contain a carbon atom in the anion, contains a fluorine atom in the anion, and is soluble in acetonitrile. Fluorine-containing inorganic lithium salts are excellent in that they form a passive film on the surface of the metal foil that is the positive electrode current collector, and inhibit the corrosion of the positive electrode current collector. These fluorine-containing inorganic lithium salts are used alone or in combination of two or more. As the fluorine-containing inorganic lithium salt, a compound that is a double salt of LiF and a Lewis acid is desirable, and among them, it is more preferable to use a fluorine-containing inorganic lithium salt having a phosphorus atom, since it is easy to release free fluorine atoms. A typical fluorine-containing inorganic lithium salt is LiPF6, which dissolves and releases PF6 anions. When a fluorine-containing inorganic lithium salt having a boron atom is used as the fluorine-containing inorganic lithium salt, it is preferable because it is easy to capture excess free acid components that may cause battery deterioration, and from this viewpoint, LiBF4 is particularly preferable.
[0046] The content of the fluorine-containing inorganic lithium salt other than LiPF6 in the non-aqueous electrolyte of this embodiment is not particularly limited, but is preferably 0.01 mol or more, more preferably 0.02 mol or more, and even more preferably 0.03 mol or more per 1 L of the non-aqueous solvent. When the content of the fluorine-containing inorganic lithium salt is within the above-mentioned range of 0.01 mol or more, the ion conductivity increases and high output characteristics tend to be exhibited. In addition, the content of the fluorine-containing inorganic lithium salt is preferably 0.5 mol or less, more preferably 0.4 mol or less, and even more preferably 0.3 mol or less per 1 L of the non-aqueous solvent. When the content of the fluorine-containing inorganic lithium salt is within the above-mentioned range of 0.5 mol or less, the ion conductivity increases and high output characteristics can be exhibited, and the decrease in ion conductivity associated with the increase in viscosity at low temperatures tends to be suppressed, and the high temperature cycle characteristics and other battery characteristics of the non-aqueous secondary battery tend to be further improved while maintaining the excellent performance of the non-aqueous electrolyte.
[0047] The nonaqueous electrolyte solution of the present embodiment may contain an organic lithium salt as the cyclic anion-containing lithium salt and / or the noncyclic anion-containing lithium salt. The "organic lithium salt" refers to a lithium salt that contains a carbon atom in the anion and is soluble in acetonitrile.
[0048] The organic lithium salt may be an organic lithium salt having an oxalic acid group. Specific examples of the organic lithium salt having an oxalic acid group include organic lithium salts represented by LiB(C2O4)2, LiBF2(C2O4), LiPF4(C2O4), and LiPF2(C2O4)2, and among them, at least one lithium salt selected from the lithium salts represented by LiB(C2O4)2 and LiBF2(C2O4) is preferred. It is more preferred to use one or more of these together with a fluorine-containing inorganic lithium salt. The organic lithium salt having an oxalic acid group may be added to a non-aqueous electrolyte solution or may be contained in the negative electrode (negative electrode active material layer).
[0049] The amount of the organic lithium salt having an oxalic acid group added to the non-aqueous electrolyte is preferably 0.005 mol or more, more preferably 0.02 mol or more, and even more preferably 0.05 mol or more, per 1 L of the non-aqueous solvent of the non-aqueous electrolyte, in order to better ensure the effect of its use. However, if the amount of the organic lithium salt having an oxalic acid group in the non-aqueous electrolyte is too large, there is a risk of precipitation. Therefore, the amount of the organic lithium salt having an oxalic acid group added to the non-aqueous electrolyte is preferably less than 1.0 mol, more preferably less than 0.5 mol, and even more preferably less than 0.2 mol, per 1 L of the non-aqueous solvent of the non-aqueous electrolyte.
[0050] It is known that organic lithium salts having oxalic acid groups are poorly soluble in organic solvents with low polarity, particularly in chain carbonates. Organic lithium salts having oxalic acid groups may contain a small amount of lithium oxalate, and may react with a small amount of water contained in other raw materials when mixed to form a non-aqueous electrolyte solution, resulting in the generation of new white precipitation of lithium oxalate. Therefore, the content of lithium oxalate in the non-aqueous electrolyte solution of this embodiment is not particularly limited, but is preferably 0 to 500 ppm.
[0051] In addition to the lithium salts listed above, lithium salts generally used for non-aqueous secondary batteries may be added supplementarily as the lithium salt in this embodiment. Specific examples of other lithium salts include LiClO4, LiAlO4, LiAlCl4, LiB 10 Cl 10 Inorganic lithium salts that do not contain fluorine atoms in the anion, such as chloroborane Li; LiCF3SO3, LiCF3CO2, Li2C2F4(SO3)2, LiC(CF3SO2)3, LiC n F (2n+1) SO3 {wherein n ≧ 2}, organic lithium salts such as lower aliphatic carboxylic acids, Li tetraphenylborate, and LiB(C3O4H2)2; LiPF such as LiPF5(CF3) n (C p F 2p+1 ) 6-n [wherein n is an integer of 1 to 5, and p is an integer of 1 to 8]; LiBF such as LiBF3(CF3) q (C s F 2s+1 ) 4-q an organic lithium salt represented by the formula (wherein q is an integer of 1 to 3, and s is an integer of 1 to 8); a lithium salt combined with a polyvalent anion; The following formula (a): LiC(SO2R A )(SO2R B )(SO2R C ) (a) {where, R A , R B , and R Cmay be the same or different and represent a perfluoroalkyl group having 1 to 8 carbon atoms. The following formula (b): LiN(SO2OR D )(SO2OR E ) (b) {where, R D , and R E may be the same or different and represent a perfluoroalkyl group having 1 to 8 carbon atoms.}, and The following formula (c) LiN(SO2R F )(SO2OR G ) (c) {where, R F , and R G may be the same or different and represent a perfluoroalkyl group having 1 to 8 carbon atoms.} One or more of these can be used together with the fluorine-containing inorganic lithium salt.
[0052] <1-3. Additives> The nonaqueous electrolyte according to the present embodiment may contain additives in addition to the nonaqueous solvent and electrolyte salt described above.
[0053] <Other electrode protection additives> Other electrode protection additives are not particularly limited as long as they do not impede the solution of the problems by the present invention, and may substantially overlap with the substance that plays the role of a solvent for dissolving lithium salts (i.e., the above-mentioned non-aqueous solvent), and examples thereof include vinylene carbonate and fluoroethylene carbonate. The electrode protection additive is preferably a substance that contributes to improving the performance of the non-aqueous electrolyte and non-aqueous secondary battery in this embodiment, but also includes substances that are not directly involved in electrochemical reactions.
[0054] Specific examples of other electrode protection additives include, for example, 4-fluoro-1,3-dioxolane-2-one, 4,4-difluoro-1,3-dioxolane-2-one, cis-4,5-difluoro-1,3-dioxolane-2-one, trans-4,5-difluoro-1,3-dioxolane-2-one, 4,4,5-trifluoro-1,3-dioxolane-2-one, 4,4,5,5-tetrafluoro-1,3-dioxolane-2-one, Fluoroethylene carbonates such as 4,4,5-trifluoro-5-methyl-1,3-dioxolan-2-one; unsaturated bond-containing cyclic carbonates such as 4,5-dimethylvinylene carbonate and vinylethylene carbonate; γ-butyrolactone, γ-valerolactone, γ-caprolactone, δ-valerolactone, δ-caprolactone, and ε-caprolactone. lactones, cyclic ethers, cyclic ethers, cyclic sulfur compounds, cyclic sulfur compounds, cyclic sulfur compounds, cyclic anhydrides ...
[0055] The content of the electrode protection additive in the nonaqueous electrolyte solution in this embodiment is not particularly limited, but the content of the electrode protection additive relative to the total amount of the nonaqueous solvent is preferably 0.1 to 30 volume %, more preferably 0.3 to 15 volume %, and even more preferably 0.5 to 4 volume %.
[0056] In this embodiment, the greater the content of the electrode protection additive, the more the deterioration of the non-aqueous electrolyte solution is suppressed. However, the smaller the content of the electrode protection additive, the more the high-output characteristics of the non-aqueous secondary battery in a low-temperature environment are improved. Therefore, by adjusting the content of the electrode protection additive within the above-mentioned range, it is possible to maximize the excellent performance based on the high ionic conductivity of the non-aqueous electrolyte solution without impairing the basic function of the non-aqueous secondary battery. By preparing the non-aqueous electrolyte solution with such a composition, it is possible to further improve all of the cycle performance of the non-aqueous secondary battery, the high-output performance in a low-temperature environment, and other battery characteristics.
[0057] <Other optional additives> In this embodiment, for the purpose of improving the charge / discharge cycle characteristics, high-temperature storage properties, and safety (e.g., prevention of overcharging) of the nonaqueous secondary battery, an optional additive selected from sulfonic acid esters, diphenyl disulfide, cyclohexylbenzene, biphenyl, fluorobenzene, tert-butylbenzene, phosphate esters [ethyl diethyl phosphonoacetate (EDPA): (C2H5O)2(P=O)-CH2(C=O)OC2H5, tris(trifluoroethyl) phosphate (TFEP): (CF3CHO)3P=O, triphenyl phosphate (TPP): (C6H5O)3P=O: (CH2=CHCHO)3P=O, triallyl phosphate, etc.], nitrogen-containing cyclic compounds with no steric hindrance around the unshared electron pair [pyridine, 1-methyl-1H-benzotriazole, 1-methylpyrazole, etc.], and derivatives of these compounds can also be appropriately added to the nonaqueous electrolyte. In particular, phosphoric acid esters are effective in suppressing side reactions during storage.
[0058] The content of other optional additives in this embodiment is calculated as a mass percentage relative to the total mass of all components constituting the non-aqueous electrolyte. There is no particular limitation on the content of other optional additives, but it is preferably in the range of 0.01 mass% to 10 mass%, more preferably 0.02 mass% to 5 mass%, and even more preferably 0.05 mass% to 3 mass% relative to the total amount of the non-aqueous electrolyte. By adjusting the content of other optional additives within the above range, there is a tendency that even better battery characteristics can be added without impairing the basic function as a non-aqueous secondary battery.
[0059] <2. Positive electrode and positive electrode current collector> The positive electrode 150 shown in Fig. 1 and Fig. 2 is composed of a positive electrode active material layer made of a positive electrode mixture and a positive electrode current collector. The positive electrode 150 is not particularly limited as long as it acts as a positive electrode of a non-aqueous secondary battery, and may be a known one. The positive electrode in this embodiment preferably contains a lithium-containing compound containing Fe, and more preferably contains nickel (Ni) at a relatively high ratio.
[0060] The positive electrode active material layer is disposed on one or both sides of the positive electrode current collector, and contains a positive electrode active material, and preferably further contains a conductive assistant and a binder as necessary.
[0061] The positive electrode active material layer preferably contains a material capable of absorbing and releasing lithium ions as the positive electrode active material. When such a material is used, it is preferable because it tends to be possible to obtain a high voltage and a high energy density. In this embodiment, a lithium compound containing Li, Ni, Mn, and O is used as the positive electrode active material.
[0062] The positive electrode active material capable of obtaining high voltage and high energy is represented by the following formula (A): Li x Ni y Mn z O4... (A) {where 0.9 ≦ x ≦ 1.1, 0 < y < 1, and 1 < z < 2.} Examples include lithium nickel manganate represented by .
[0063] Specific examples of the cathode active material other than that represented by formula (A) include, for example, Li compounds such as LiFePO4, or lithium cobalt oxides typified by LiCoO2; lithium manganese oxides typified by LiMnO2, LiMn2O4, and Li2Mn2O4; lithium nickel oxides typified by LiNiO2; LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2, LiNi 0.5 Co 0.2 Mn 0.3 O2, LiNi 0.8 Co 0.2 O2, and lithium-containing composite metal oxides represented by Li z MO2 (where M contains at least one transition metal element selected from the group consisting of Ni, Mn, and Co, and represents two or more metal elements selected from the group consisting of Ni, Mn, Co, Al, and Mg, and z represents a number greater than 0.9 and less than 1.2). The cathode of the present embodiment may contain these active materials in addition to the lithium compound containing Li, Ni, Mn, and O.
[0064] In addition, as a cathode active material that can particularly obtain a high voltage, the general formula (B): Li p Ni q Co r Mn s M t O u ··· (B) {where M is at least one metal selected from the group consisting of Al, Sn, In, Fe, V, Cu, Mg, Ti, Zn, Mo, Zr, Sr, and Ba, and 0 < p < 1.3, 0 < q < 1.2, 0 < r < 1.2, 0 ≦ s < 0.5, 0 ≦ t < 0.3, 0.7 ≦ q + r + s + t ≦ 1.2, and 1.8 < u < 2.2, and p is a value determined by the charge and discharge state of the battery.} Examples include Li-containing metal oxides represented by this formula. When the Ni content ratio q is 0.5 < q < 1.2, it is preferable because both reduction of the amount of rare metal Co used and increase in energy density can be achieved. Such a positive electrode active material includes, for example, LiNi 0.6 Co 0.2 Mn 0.2 O2, LiNi 0.75 Co 0.15 Mn 0.15 O2, LiNi 0.8 Co 0.1 Mn 0.1 O2, LiNi 0.85 Co 0.075 Mn 0.075 O2, LiNi 0.8 Co 0.15 Al 0.05 O2, LiNi 0.81 Co 0.1 Al 0.09 O2, LiNi 0.85 Co 0.1 Al 0.05 O2, etc., and lithium-containing composite metal oxides typified thereby.
[0065] On the other hand, the higher the Ni content ratio in the positive electrode active material layer, the more likely it is to deteriorate at a low voltage. The positive electrode active material of the Li-containing metal oxide represented by the general formulas (A) and (B) essentially has active points that oxidatively deteriorate the non-aqueous electrolyte, and these active points may inadvertently consume the compound added to protect the negative electrode on the positive electrode side. Among them, acid anhydrides tend to be particularly affected. In particular, when acetonitrile is contained as the non-aqueous solvent, the addition effect of the acid anhydride is extremely large, so the consumption of the acid anhydride on the positive electrode side is a fatal problem.
[0066] In addition, the decomposition products of these additives that are taken in and deposited on the positive electrode side not only increase the internal resistance of the non-aqueous secondary battery, but also accelerate the deterioration of the lithium salt. Furthermore, the protection of the negative electrode surface, which was the original purpose, becomes insufficient. In order to deactivate the active sites that essentially cause the oxidative deterioration of the non-aqueous electrolyte, it is important to control the Jahn-Teller distortion or to coexist with a component that plays a role as a neutralizer. Therefore, it is preferable that the positive electrode active material contains at least one metal selected from the group consisting of Al, Sn, In, Fe, V, Cu, Mg, Ti, Zn, Mo, Zr, Sr, and Ba.
[0067] For the same reason, it is preferable that the surface of the positive electrode active material is coated with a compound containing at least one metal element selected from the group consisting of Zr, Ti, Al, and Nb. It is more preferable that the surface of the positive electrode active material is coated with an oxide containing at least one metal element selected from the group consisting of Zr, Ti, Al, and Nb. Furthermore, it is particularly preferable that the surface of the positive electrode active material is coated with at least one oxide selected from the group consisting of ZrO2, TiO2, Al2O3, NbO3, and LiNbO2, since this does not inhibit the permeation of lithium ions.
[0068] The positive electrode may contain a lithium-containing compound other than the Li-containing metal oxide represented by formula (A) or (B) as a positive electrode active material. Examples of such lithium-containing compounds include composite oxides containing lithium and a transition metal element, metal chalcogenides containing lithium, and metal silicate compounds containing lithium and a transition metal element. From the viewpoint of obtaining a higher voltage, the lithium-containing compound is preferably a metal phosphate compound containing lithium and at least one transition metal element selected from the group consisting of Co, Ni, Mn, Fe, Cu, Zn, Cr, V, and Ti. More specifically, the lithium-containing compound is represented by the following formula (Xa): Li v M I D2 (Xa) In the formula, D represents a chalcogen element, and M Irepresents one or more transition metal elements, and the value of v is determined depending on the charge / discharge state of the battery and represents a number from 0.05 to 1.10.}, and The following formula (Xb): Li t M II u SiO4 (Xb) {In formula, M II represents one or more transition metal elements, the value of t is determined depending on the charge / discharge state of the battery and represents a number from 0.05 to 1.10, and u represents a number from 0 to 2.} Examples of the compounds include those represented by the following formula:
[0069] The lithium-containing compound represented by the above formula (Xa) has a layered structure, and the compounds represented by the above formula (1) and the above formula (Xb) have an olivine structure. These lithium-containing compounds may be those in which a part of the transition metal element is replaced by Al, Mg, or other transition metal element, those in which these metal elements are included in the crystal grain boundaries, those in which a part of the oxygen atoms is replaced by fluorine atoms, etc., and those in which at least a part of the surface of the positive electrode active material is coated with another positive electrode active material, etc., for the purpose of stabilizing the structure.
[0070] As the positive electrode active material in this embodiment, the lithium-containing compound as described above may be used alone, or the lithium-containing compound may be used in combination with other positive electrode active materials.
[0071] Examples of such other positive electrode active materials include metal oxides or metal chalcogenides having a tunnel structure and a layer structure, sulfur, conductive polymers, etc. Examples of metal oxides or metal chalcogenides having a tunnel structure and a layer structure include MnO2, FeO2, FeS2, V2O5, and V6O 13 Examples of the conductive polymer include oxides, sulfides, and selenides of metals other than lithium, such as TiO2, TiS2, MoS2, and NbSe2. Examples of the conductive polymer include conductive polymers such as polyaniline, polythiophene, polyacetylene, and polypyrrole.
[0072] The above-mentioned other positive electrode active materials can be used alone or in combination of two or more, and are not particularly limited. However, it is preferable that the positive electrode active material layer contains at least one transition metal element selected from Ni, Mn, and Co, because it can reversibly and stably absorb and release lithium ions and achieve high energy density.
[0073] When a lithium-containing compound and another positive electrode active material are used in combination as the positive electrode active material, the ratio of the two is preferably 80 mass % or more, and more preferably 85 mass % or more, of the lithium-containing compound relative to the total positive electrode active material.
[0074] Examples of the conductive additive include carbon black, such as graphite, acetylene black, and ketjen black, and carbon fiber. The content of the conductive additive is preferably 10 parts by mass or less, and more preferably 1 to 5 parts by mass, relative to 100 parts by mass of the positive electrode active material.
[0075] Examples of the binder include polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), polyacrylic acid, styrene butadiene rubber, and fluororubber. The content of the binder is preferably 10 parts by mass or less, more preferably 0.5 to 8 parts by mass, relative to 100 parts by mass of the positive electrode active material.
[0076] The positive electrode active material layer is formed by dispersing a positive electrode mixture, which is a mixture of a positive electrode active material and, if necessary, a conductive assistant and a binder, in a solvent to form a positive electrode mixture-containing slurry, applying the slurry to a positive electrode current collector, drying (solvent removal), and pressing as necessary. There is no particular restriction on such a solvent, and a conventionally known solvent can be used. Examples of the solvent include N-methyl-2-pyrrolidone, dimethylformamide, dimethylacetamide, and water.
[0077] The positive electrode current collector is made of a metal foil such as aluminum foil, nickel foil, stainless steel foil, etc. The positive electrode current collector may have a carbon coating on the surface, or may be processed into a mesh shape. The thickness of the positive electrode current collector is preferably 5 to 40 μm, more preferably 7 to 35 μm, and further preferably 9 to 30 μm.
[0078] <3. Negative electrode and negative electrode current collector> 1 and 2 is composed of a negative electrode active material layer made of a negative electrode mixture and a negative electrode current collector. The negative electrode 160 can function as the negative electrode of a non-aqueous secondary battery.
[0079] The negative electrode active material layer is disposed on one or both sides of the negative electrode current collector, and preferably contains a negative electrode active material and, if necessary, a conductive assistant and a binder. As described above, the non-aqueous lithium ion secondary battery according to this embodiment preferably has a structure that allows injection of X% by mass of a non-aqueous electrolyte solution relative to the mass of the negative electrode active material.
[0080] Examples of the negative electrode active material include amorphous carbon (hard carbon), graphite (e.g., artificial graphite, natural graphite, etc.), pyrolytic carbon, coke, glassy carbon, baked bodies of organic polymer compounds, mesocarbon microbeads, carbon fibers, activated carbon, carbon colloids, and carbon black, as well as metal lithium, metal oxides, metal nitrides, lithium alloys, tin alloys, silicon alloys, intermetallic compounds, organic compounds, inorganic compounds, metal complexes, and organic polymer compounds. The negative electrode active material is used alone or in combination of two or more. As the negative electrode active material, graphite is preferable from the viewpoint of the use of the nonaqueous electrolyte according to this embodiment.
[0081] The negative electrode active material layer uses lithium ions as the negative electrode active material at 0.4V vs. Li / Li in order to increase the battery voltage. + It is preferable that the hydrogen-containing gas contains a material capable of absorbing at a potential lower than the hydrogen potential.
[0082] Examples of the conductive assistant include carbon black, such as graphite, acetylene black, and ketjen black, and carbon fiber. The content of the conductive assistant is preferably 20 parts by mass or less, and more preferably 0.1 to 10 parts by mass, relative to 100 parts by mass of the negative electrode active material.
[0083] Examples of the binder include carboxymethyl cellulose, PVDF, PTFE, polyacrylic acid, and fluororubber. Also included are diene rubbers such as styrene-butadiene rubber. The content of the binder is preferably 10 parts by mass or less, more preferably 0.5 to 8 parts by mass, based on 100 parts by mass of the negative electrode active material.
[0084] The negative electrode active material layer is formed by dispersing a negative electrode mixture, which is a mixture of a negative electrode active material and, if necessary, a conductive assistant and a binder, in a solvent to form a negative electrode mixture-containing slurry, applying the slurry to a negative electrode current collector, drying (solvent removal), and pressing if necessary. There is no particular restriction on such a solvent, and a conventionally known solvent may be used. Examples of the solvent include N-methyl-2-pyrrolidone, dimethylformamide, dimethylacetamide, and water.
[0085] The negative electrode current collector is made of a metal foil such as copper foil, nickel foil, stainless steel foil, etc. The surface of the negative electrode current collector may be carbon-coated or processed into a mesh shape. The thickness of the negative electrode current collector is preferably 5 to 40 μm, more preferably 6 to 35 μm, and further preferably 7 to 30 μm.
[0086] <4. Separator> 2, the nonaqueous secondary battery 100 in this embodiment is preferably provided with a separator 170 between the positive electrode 150 and the negative electrode 160 from the viewpoint of preventing short circuits between the positive electrode 150 and the negative electrode 160 and providing safety such as shutdown. The separator 170 is not limited, but may be the same as that provided in known nonaqueous secondary batteries, and is preferably an insulating thin film having high ion permeability and excellent mechanical strength. Examples of the separator 170 include woven fabric, nonwoven fabric, and synthetic resin microporous membrane, and among these, synthetic resin microporous membrane is preferable.
[0087] As the synthetic resin microporous film, for example, a microporous film containing polyethylene or polypropylene as a main component, or a polyolefin-based microporous film such as a microporous film containing both of these polyolefins is preferably used. As the nonwoven fabric, for example, a porous film made of a heat-resistant resin such as glass, ceramic, polyolefin, polyester, polyamide, liquid crystal polyester, or aramid can be used.
[0088] Separator 170 may be a single layer or multiple layers of one type of microporous film, or a laminate of two or more types of microporous films. Separator 170 may be a single layer or multiple layers of a mixed resin material obtained by melting and kneading two or more types of resin materials.
[0089] For the purpose of providing functions, inorganic particles may be present on the surface or inside of the separator, or other organic layers may be further coated or laminated. Also, a crosslinked structure may be included. In order to improve the safety performance of the non-aqueous secondary battery, these methods may be combined as necessary.
[0090] By using such a separator 170, it is possible to realize the good input / output characteristics and low self-discharge characteristics required for the lithium ion battery for the above-mentioned high-power applications.
[0091] The thickness of the microporous membrane usable as a separator is not particularly limited, but is preferably 1 μm or more from the viewpoint of membrane strength, and is preferably 500 μm or less from the viewpoint of permeability. The thickness of the microporous membrane is preferably 5 μm or more and 30 μm or less, and more preferably 10 μm or more and 25 μm or less, from the viewpoint of use in high-output applications such as safety tests that have a relatively high heat generation amount and require self-discharge characteristics higher than conventional ones, and from the viewpoint of winding properties in a large battery winding machine. In addition, the thickness of the microporous membrane is more preferably 15 μm or more and 25 μm or less when emphasis is placed on both short circuit resistance and output performance, but is more preferably 10 μm or more and less than 15 μm when emphasis is placed on both high energy density and output performance.
[0092] The porosity of the microporous membrane usable as a separator is preferably 30% to 90%, more preferably 35% to 80%, and even more preferably 40% to 70%, from the viewpoint of following the rapid movement of lithium ions during high output. When priority is given to improving output performance while ensuring safety, the porosity of the microporous membrane is particularly preferably 50% to 70%, and when emphasis is placed on achieving both short circuit resistance and output performance, the porosity is particularly preferably 40% to less than 50%.
[0093] The air permeability of a microporous membrane that can be used as a separator is set to 1 second / 100 cm from the viewpoint of the balance between the membrane thickness and the porosity. 3 More than 400 seconds / 100cm 3 Less than 100 seconds / 100 cm is preferable. 3 More than 350 / 100cm 3 When it is important to achieve both short circuit resistance and output performance, the air permeability of the microporous membrane is preferably 150 sec / 100 cm. 3 More than 350 seconds / 100cm 3 The following is particularly preferable. If you prioritize improving output performance while ensuring safety, 100 / 100cm 3 150 seconds / 100cm 3is particularly preferably less than 10 mS / cm. On the other hand, when a non-aqueous electrolyte with low ionic conductivity is combined with a separator within the above range, the lithium ion migration rate is determined not by the structure of the separator but by the high ionic conductivity of the non-aqueous electrolyte, and the expected input / output characteristics tend not to be obtained. Therefore, the ionic conductivity of the non-aqueous electrolyte is preferably 10 mS / cm or more, more preferably 15 mS / cm, and even more preferably 20 mS / cm. However, the membrane thickness, air permeability and porosity of the separator, and the ionic conductivity of the non-aqueous electrolyte are not limited to the above examples.
[0094] <5. Battery exterior> The configuration of the battery exterior 110 of the nonaqueous secondary battery 100 shown in Figures 1 and 2 is not particularly limited, and for example, either a battery can or a laminate film exterior can be used. As the battery can, for example, a metal can made of steel, stainless steel, aluminum, clad material, or the like, which may be rectangular, rectangular tube, cylindrical, elliptical, flat, coin, or button-shaped, etc., can be used. As the laminate film exterior, for example, a laminate film made of a three-layer structure of heat-melting resin / metal film / resin can be used.
[0095] The laminate film exterior body can be used as an exterior body by stacking two sheets with the heat-melting resin side facing inward, or by folding the laminate film exterior body so that the heat-melting resin side faces inward, and sealing the ends by heat sealing. When using a laminate film exterior body, the positive electrode lead body 130 (or a lead tab connected to the positive electrode terminal and the positive electrode terminal) may be connected to the positive electrode current collector, and the negative electrode lead body 140 (or a lead tab connected to the negative electrode terminal and the negative electrode terminal) may be connected to the negative electrode current collector. In this case, the laminate film exterior body may be sealed with the ends of the positive electrode lead body 130 and the negative electrode lead body 140 (or the lead tabs connected to the positive electrode terminal and the negative electrode terminal, respectively) pulled out to the outside of the exterior body.
[0096] <6. How to make a battery> The nonaqueous secondary battery 100 in this embodiment is produced by a known method using the above-mentioned nonaqueous electrolyte, a positive electrode 150 having a positive electrode active material layer on one or both sides of a current collector, a negative electrode 160 having a negative electrode active material layer on one or both sides of a current collector, a battery exterior 110, and, if necessary, a separator 170.
[0097] First, a laminate consisting of a positive electrode 150, a negative electrode 160, and optionally a separator 170 is formed. For example: A mode in which a long positive electrode 150 and a long negative electrode 160 are wound in a stacked state with the long separator interposed between the positive electrode 150 and the negative electrode 160 to form a laminate having a wound structure; A mode in which the positive electrode 150 and the negative electrode 160 are cut into a plurality of sheets having a certain area and shape, and the positive electrode sheets and the negative electrode sheets are alternately stacked with a separator sheet interposed therebetween to form a laminate having a laminated structure; A mode in which a long separator is zigzag-folded and positive electrode sheets and negative electrode sheets are alternately inserted between the zigzag-folded separators to form a laminate having a laminate structure; etc. are possible.
[0098] Next, the above-mentioned laminate is housed in a battery exterior 110 (battery case), the nonaqueous electrolyte solution according to this embodiment is poured into the battery case, and the laminate is immersed in the nonaqueous electrolyte solution and sealed, thereby producing the nonaqueous secondary battery according to this embodiment.
[0099] Alternatively, a gel-state electrolyte membrane may be prepared in advance by impregnating a substrate made of a polymer material with a nonaqueous electrolyte solution, and a laminated structure may be formed using sheet-like positive electrode 150, negative electrode 160, and electrolyte membrane, as well as separator 170 as necessary, and then the laminated structure may be housed in battery exterior 110 to prepare nonaqueous secondary battery 100.
[0100] In addition, if the arrangement of the electrodes is designed so that there is a portion where the outer peripheral edge of the negative electrode active material layer overlaps with the outer peripheral edge of the positive electrode active material layer, or there is a portion where the width is too small in the non-facing portion of the negative electrode active material layer, the position of the electrodes may be shifted during battery assembly, which may deteriorate the charge-discharge cycle characteristics of the non-aqueous secondary battery. Therefore, it is preferable that the electrode positions of the electrode body used in the non-aqueous secondary battery are fixed in advance by tapes such as polyimide tape, polyphenylene sulfide tape, and polypropylene (PP) tape, adhesives, etc.
[0101] In this embodiment, when a non-aqueous electrolyte using acetonitrile is used, the lithium ions released from the positive electrode during the initial charge of the non-aqueous secondary battery may diffuse throughout the negative electrode due to its high ionic conductivity. In non-aqueous secondary batteries, the area of the negative electrode active material layer is generally made larger than that of the positive electrode active material layer. However, if lithium ions diffuse and are absorbed to a portion of the negative electrode active material layer that does not face the positive electrode active material layer, the lithium ions will not be released during the initial discharge and will remain in the negative electrode. Therefore, the contribution of the lithium ions that are not released becomes irreversible capacity. For these reasons, the initial charge / discharge efficiency may be low in non-aqueous secondary batteries using a non-aqueous electrolyte containing acetonitrile.
[0102] On the other hand, if the area of the positive electrode active material layer is larger than that of the negative electrode active material layer or they are the same, current concentration is likely to occur at the edge portions of the negative electrode active material layer during charging, making lithium dendrites more likely to form.
[0103] For the above reasons, the ratio of the area of the entire negative electrode active material layer to the area of the portion where the positive electrode active material layer and the negative electrode active material layer face each other is not particularly limited, but is preferably greater than 1.0 and less than 1.1, more preferably greater than 1.002 and less than 1.09, even more preferably greater than 1.005 and less than 1.08, and particularly preferably greater than 1.01 and less than 1.08. In a nonaqueous secondary battery using a nonaqueous electrolyte solution containing acetonitrile, the initial charge / discharge efficiency can be improved by reducing the ratio of the area of the entire negative electrode active material layer to the area of the portion where the positive electrode active material layer and the negative electrode active material layer face each other.
[0104] Reducing the ratio of the area of the entire negative electrode active material layer to the area of the portion where the positive electrode active material layer and the negative electrode active material layer face each other means limiting the ratio of the area of the portion of the negative electrode active material layer that does not face the positive electrode active material layer. This makes it possible to reduce as much as possible the amount of lithium ions absorbed in the portion of the negative electrode active material layer that does not face the positive electrode active material layer among the lithium ions released from the positive electrode during the initial charge (i.e., the amount of lithium ions that are not released from the negative electrode during the initial discharge and become irreversible capacity). Therefore, by designing the ratio of the area of the entire negative electrode active material layer to the area of the portion where the positive electrode active material layer and the negative electrode active material layer face each other within the above range, it is possible to improve the load characteristics of the battery by using acetonitrile, increase the initial charge / discharge efficiency of the battery, and further suppress the generation of lithium dendrites.
[0105] The nonaqueous secondary battery 100 in this embodiment can function as a battery by initial charging, but is stabilized by decomposing a part of the nonaqueous electrolyte during the initial charging. There is no particular limitation on the method of initial charging, but the initial charging is preferably performed at 0.001 to 0.3 C, more preferably at 0.002 to 0.25 C, and even more preferably at 0.003 to 0.2 C. It is also preferable that the initial charging is performed via a constant voltage charge in the middle. By setting the voltage range in which the lithium salt participates in the electrochemical reaction to be long, a stable and strong SEI is formed on the surface of the electrode (negative electrode 160), and there is an effect of suppressing an increase in internal resistance. In addition, the reaction product is not firmly fixed only to the negative electrode 160, but in some way has a good effect on members other than the negative electrode 160, such as the positive electrode 150 and the separator 170. For this reason, it is very effective to perform the initial charging in consideration of the electrochemical reaction of the lithium salt dissolved in the nonaqueous electrolyte.
[0106] The nonaqueous secondary battery 100 in this embodiment can also be used as a battery pack in which a plurality of nonaqueous secondary batteries 100 are connected in series or in parallel. From the viewpoint of managing the charge / discharge state of the battery pack, the operating voltage range per battery is preferably 2 to 5 V.
[0107] <7. How to charge a lithium-ion secondary battery> In this embodiment, the method for charging a lithium ion secondary battery includes a step of charging the lithium ion secondary battery at a voltage of 4.6 V (for example, 4.60 V) or higher. In the conventional example using an electrolyte containing a chain-like imide salt, it was necessary to combine an equal amount of LiPF6 with the imide salt and to use a fluorinated solvent in order to achieve high-voltage operation of 4.6 V or more. This is thought to be because lithium salts often have poor ability to form an aluminum passivation film, and it was preferable to use LiPF6 in combination, which is advantageous for forming a passivation film. On the other hand, even if an electrolyte containing LiPF6 as its main component can prevent aluminum corrosion, there are concerns about its low thermal stability. In this regard, as described above, by using the lithium ion secondary battery of this embodiment, the thermal stability of the electrolyte can be ensured, and further, it is possible to operate the battery at a high voltage of 4.6 V or more.
[0108] The charging method of the present embodiment may include a step of charging at a voltage of 4.7 V or more, or may include a step of charging at a voltage of 4.8 V or more. The lithium ion secondary battery of the present embodiment can be driven even at such a high voltage.
[0109] Although the embodiment of the present invention has been described above, the present invention is not limited to the above embodiment. The present invention can be modified in various ways without departing from the gist of the present invention. EXAMPLES
[0110] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0111] [Example 1] (1) Preparation of non-aqueous electrolyte In an inert atmosphere, various non-aqueous solvents and various additives were mixed to a predetermined concentration, and further various lithium salts were mixed to a predetermined concentration to prepare a non-aqueous electrolyte solution. (Lithium salts) LiCTFSI: a compound represented by formula (1-2) LiFSI: Lithium bis(fluorosulfonyl)imide LiPF6: Lithium hexafluorophosphate (Non-aqueous solvent) EMC: Ethyl methyl carbonate EC: Ethylene carbonate VC: Vinylene carbonate AcN: Acetonitrile ES: Ethylene sulfite
[0112] (2) Preparation of non-aqueous secondary battery (2-1) Preparation of positive electrode LiNi as the positive electrode active material 0.5 Mn 1.5 The positive electrode mixture slurry containing the compound represented by O4 was applied to an aluminum current collector foil having a thickness of 16 μm while adjusting the basis weight of the slurry, and the solvent was dried and removed in a hot air drying oven. After that, the density of the positive electrode active material layer was 2.3 g / cm 3 The positive electrode was obtained by rolling the positive electrode active material layer and the positive electrode current collector so that the weight of the positive electrode was 13.52 mg / cm. 2 It was.
[0113] (2-2) Preparation of negative electrode The negative electrode mixture slurry containing graphite as the negative electrode active material was applied to one side of a 10 μm thick copper foil as a negative electrode current collector, and the solvent was dried and removed in a hot air drying oven. After that, the density of the negative electrode active material layer was 1.4 g / cm 3 The negative electrode was obtained by rolling the negative electrode active material layer and the negative electrode current collector so that the coating weight of the negative electrode was 11.4 mg / cm. 2 It was.
[0114] (2-3) Assembly of non-aqueous secondary battery (coin type) In a nitrogen glove box with a dew point temperature of -60 to -20 ° C, a polypropylene gasket was set in a CR2032 type battery case (SUS304 / Al clad). Then, in the center, the positive electrode obtained as described above was punched into a disk shape with a diameter of 15.958 mm, and the positive electrode active material layer was set facing up. On top of that, a glass fiber filter paper (Advantec, GA-100) was punched into a disk shape with a diameter of 16.156 mm, and 150 μL of non-aqueous electrolyte was injected. Then, the negative electrode (A1, A2) obtained as described above was punched into a disk shape with a diameter of 16.156 mm, and the negative electrode active material layer was set facing down. Furthermore, after setting the spacer and spring, the battery cap was fitted and crimped with a crimping machine. The laminate was kept at 25° C. for 12 hours to allow the nonaqueous electrolyte to fully penetrate the laminate, thereby obtaining a coin-type nonaqueous secondary battery (Example 1).
[0115] [Examples 2 to 4] and [Comparative Examples 1 to 4] Coin-type nonaqueous secondary batteries (Examples 2 to 4 and Comparative Examples 1 to 4) were obtained in the same manner as in Example 1, except that the type of lithium salt and the composition of the nonaqueous solvent were changed as shown in the table.
[0116] (3) Evaluation of non-aqueous secondary batteries The battery obtained as described above was first charged according to the procedure in (3-1) below. Next, a high-voltage charge-discharge cycle test was performed on the battery according to the procedure in (3-2). The charge-discharge was performed using a charge-discharge device ACD-M01A (product name) manufactured by Asuka Electronics Co., Ltd. and a programmable thermostatic chamber IN804 (product name) manufactured by Yamato Scientific Co., Ltd.
[0117] Here, 1C means the current value at which a fully charged battery is expected to be discharged completely in one hour when discharged at a constant current.
[0118] (3-1) Initial charge / discharge treatment of non-aqueous secondary batteries The ambient temperature of the fabricated non-aqueous secondary battery was set to 25°C, and constant current charging of 0.1 C was performed, followed by CCCV charging until the battery voltage reached 4.8 V or the charge capacity reached 8 mAh. After that, the battery was paused for 10 minutes, and then CC discharged to 3.3 V at 0.1 C.
[0119] The maximum voltage reached during the initial charging process is summarized for each battery shown in Table 1. However, 4.8V was set as the upper limit voltage.
[0120] [Table 1]
[0121] In the initial charging of the battery by the method described in (3-1), it is desirable that the battery voltage rise to 4.6V or more. In Examples 1 to 3, charging to a high voltage was possible. On the other hand, in Comparative Examples 1 and 2, the charging voltage remained below 4.6V. This is considered to be because the rise in the positive electrode potential stopped due to corrosion of the aluminum current collector foil. From this, it was confirmed that charging to a high voltage of 4.6V or more is possible in this embodiment.
[0122] (3-2) Cycle test of non-aqueous secondary batteries After the initial charge and discharge was performed in the same manner as in (3-1), the battery was charged to 4.8 V at 0.1 C. After a 10-minute break, the battery was discharged to 3.3 V at 0.1 C. This constitutes one cycle. Table 2 shows the capacity retention rate for each battery when the battery was charged to 4.8 V and discharged for 10 cycles.
[0123] (3-3) Presence or absence of black spots on aluminum after cycle testing After the cycle test in (3-2) above, the coin-type nonaqueous secondary battery was disassembled in a glove box under an Ar atmosphere, and then the positive electrode was taken out and the surface of the aluminum current collector foil was visually observed. If black spots were observed, it was evaluated as having black spots, and if no black spots were observed visually, it was evaluated as not having black spots.
[0124] [Table 2]
[0125] In Example 4, a sufficient capacity retention rate (%) was ensured even after 10 cycles, i.e., charging and discharging were possible even after 10 cycles. On the other hand, in Comparative Examples 3 and 4, a sufficient capacity retention rate (%) was not ensured after 10 cycles, i.e., in these Comparative Examples, corrosion occurred, and therefore charging and discharging were impossible. Therefore, it was confirmed that this embodiment is capable of charging and discharging cycles at a high charging voltage.
[0126] Furthermore, in Example 4, the result of "no" Al black spots was obtained. On the other hand, in Comparative Examples 3 and 4, the result of "present" Al black spots was obtained. Therefore, it was confirmed that this embodiment can suitably prevent aluminum corrosion even after 10 cycles. [Industrial Applicability]
[0127] The lithium ion secondary battery of the present invention (i.e., nonaqueous secondary battery) is expected to be used, for example, as an automotive storage battery for hybrid automobiles, plug-in hybrid automobiles, electric automobiles, and the like, as well as an industrial storage battery for power tools, drones, electric motorcycles, and the like, and further as a residential power storage system. [Explanation of symbols]
[0128] 100 Nonaqueous secondary battery 110 Battery housing 120 Space in battery housing 130 Positive electrode lead body 140 Negative electrode lead body 150 positive electrode 160 negative electrode 170 Separator
Claims
1. A lithium ion secondary battery comprising: a positive electrode including a lithium compound including Li, Ni, Mn, and O as a positive electrode active material, and aluminum as a current collecting foil; a negative electrode including graphite as a negative electrode active material; and a non-aqueous electrolyte solution, The non-aqueous electrolyte solution is The lithium salt includes a non-aqueous solvent and a cyclic anion-containing lithium salt, and may include a non-cyclic anion-containing lithium salt; The lithium ion secondary battery has a higher molar concentration of the cyclic anion-containing lithium salt in an electrolyte solvent than that of the non-cyclic anion-containing lithium salt.
2. The positive electrode active material is represented by the following formula (A): Li x Ni y Mn z O 4 ・・・ (A) {wherein 0.9≦x≦1.1, 0<y<1, and 1<z<2.} The lithium ion secondary battery according to claim 1 , comprising a lithium nickel manganese oxide represented by the formula:
3. The cyclic anion-containing lithium salt is represented by the following formula (1): 【Chemistry 1】 {In the formula, R f each independently represents a fluorine atom or a perfluoro group having 4 or less carbon atoms, and n is an integer from 1 to 5. The lithium ion secondary battery according to claim 1 or 2, comprising a compound represented by the formula:
4. The cyclic anion-containing lithium salt is represented by the following formula (1-2): 【Chemistry 2】 The lithium ion secondary battery according to claim 1 or 2, having a compound structure represented by:
5. The non-cyclic anion-containing lithium salt is LiPF 6 The lithium ion secondary battery according to claim 1 or 2, comprising:
6. A method for charging a lithium ion secondary battery, comprising the step of charging the lithium ion secondary battery according to claim 1 or 2 at a voltage of 4.6 V or more.
7. The method for charging a lithium ion secondary battery according to claim 6, further comprising the step of charging at a voltage of 4.7 V or higher.
8. The method for charging a lithium ion secondary battery according to claim 6, further comprising the step of charging at a voltage of 4.8 V or higher.
Citation Information
Patent Citations
Nonaqueous secondary battery
JP2008021517A
Fluorine-containing cyclic sulfonylimide salt, and method for producing same, non-aqueous electrolyte, non-aqueous secondary battery
WO2022203074A1
Nonaqueous electrolytic solution for lithium ion secondary batteries, and lithium ion secondary battery having the same
JP2014203748A