Handiness watch case comprising dressing component on which thin layer laminate is accumulated
The portable watch case's thin layer laminate with a phase switching layer achieves a broad color spectrum and residue-free decoration by utilizing crystalline phase changes, addressing limitations in existing technologies.
Patent Information
- Application Number
- JP2024112476
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-23
- Filing Date
- 2024-07-12
- Publication Date
- 2024-10-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing thin layers in portable watch manufacturing are limited in color range, transparency, and angle-dependent aesthetics, requiring laborious and costly structuring steps that generate residues.
A portable watch case with a thin layer laminate comprising a base material layer, a phase switching layer, and a transparent encapsulation layer, which generates interference colors through crystalline phase changes upon exposure to light, allowing for customizable multicolored decoration without residue generation.
The solution provides a wide range of saturated colors and angle-independent aesthetics, eliminating the need for post-deposition cleaning and enabling decoration customization at any stage of the watch's life cycle.
Smart Images

Figure 2024138491000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the field of watch manufacturing (e.g. wristwatches, pocket watches), in particular the stacking of thin layers. It concerns a watch case comprising a dressing component on which a layer is deposited. [Background technology]
[0002] In the field of watch manufacturing, to modify the surface properties of timekeeping components Thin layers are commonly used. They are used especially for decorative purposes. .
[0003] To deposit thin layers, the physical vapor deposition method, known by the acronym "PVD", Chemical Vapor Deposition, known as CVD, and Atomic Layer Deposition, known by the acronym ALD, are Several methods can be used, such as deposition, galvanic growth, etc.
[0004] The thin layer can be made of pure metal, metal alloy, or ceramic material.
[0005] Nevertheless, the range of intrinsic colors that occurs depending on the composition and thickness of such layers Moreover, such thin layers may be more or less dense depending on their composition and thickness. It is very translucent and the color is slightly unsaturated.
[0006] A typically semi-transparent dielectric material that is deposited on a reflective layer formed by a metallic mirror Thanks to the interference colours obtained by stacking different thin layers, A wide range of colors and saturated colors can be achieved.
[0007] Nevertheless, the color of such laminates is typically about one-quarter of the wavelength of visible light. The accuracy of the deposition thickness is closely dependent on the optical thickness of the thin layer, which is the degree of This requires precise control and limits deposition onto substrates that are flat, i.e., have two-dimensional morphology. In addition, the color of such a thin layer as perceived by the user changes with the length of the optical path. This is of great importance in applications where aesthetics are important. This will be a major challenge.
[0008] All the above thin layers are monochrome, for multicolored decoration, the number of deposition steps is as many as the desired colors. After the deposition step, an intermediate structuring step is performed. This is typically In general, photolithography and chemical etching, so-called "lift-off", "shadow This is done using a "laser mask" or laser ablation process.
[0009] Such structuring steps are tedious and expensive in order to comply with tolerance requirements. This is especially true when using chemical baths or when gases, dust, etc. , or other residues. Therefore, before the produced components are assembled into a watch, a cleaning step is performed. Summary of the Invention [Problem to be solved by the invention]
[0010] In this way, the components have bright and saturated colors across a wide range of colors. This ensures that the appearance is little or not affected by the angle from which the component is viewed. The color-producing structure does not produce stains and is prone to emitting gases, dust or other residues. You need to provide something that doesn't exist. [Means for solving the problem]
[0011] The present invention relates to a portable watch case that has a middle section to which a light-transmitting body and a back section are fixed, and that forms an internal space. The watch case has a dressing component in the internal space. The dressing component includes a laminate of layers deposited on the dressing component.
[0012] The laminate of thin layers includes a substrate layer and a solid phase-switching layer, the phase-switching layer comprising: a light-transmitting encapsulation layer and a separation layer separating the phase-switching layer from the substrate layer; do.
[0013] Thanks to the particular configuration of the laminate of these thin layers, the dressing component , has the optical property of producing interference colors.
[0014] Here, the term "interference color" refers to a color that is generated by an optical interference phenomenon.
[0015] The phase-switching layer exhibits thermal effects, particularly when exposed to locally absorbed light. The crystallographic phase change is caused by a change in the refractive index. This involves the formation of a thin film in the stack of layers in areas exposed to the light beam and areas exposed to the light beam. This gives at least two different interference colors between the non-existent regions.
[0016] Therefore, a wide range of saturation temperatures can be achieved by changing the thickness of the phase switching layer and the spacing layer. It is possible to generate Japanese and strong colors, and obtain multicolor decoration of dressing components. It is possible.
[0017] Depending on where the dressing component is placed, a transparent body or a transparent backing may be used. It is noteworthy that the rays pass through the back of the body, if there is one.
[0018] The phase change does not produce any gas, solid or liquid emissions, so that the at least two To generate two interference colors and thus decorate the dressing components does not require a subsequent washing operation.
[0019] Therefore, when the production of portable watch cases is discontinued, when portable watch cases are sold, or after -During the sales period, you can decorate your dressing components. Thanks to this , allowing for any customization of the decoration of the dressing components.
[0020] In a particular embodiment, the present invention further provides and may have one or more of the following features:
[0021] In certain embodiments, the phase-switching layer has two reversibly switchable phases. The phase states are a crystalline phase and an amorphous phase.
[0022] This decoration of the dressing component is therefore reversible.
[0023] In certain embodiments, the encapsulation layer has a refractive index similar to that of the phase-switching layer under the exposure to light. is transparent to wavelengths of light that can vary.
[0024] In a particular embodiment, the substrate layer is formed by a reflective layer.
[0025] In certain embodiments, the laminate comprises all of the dressing components. and the encapsulation layer is deposited on a support formed in whole or in part by the support. It is formed.
[0026] In certain embodiments, the dressing component comprises a dial, a timepiece movement, The components may be the structure of the watch, a transparent body, a needle, decorations, a logo, a disk or a vibration weight.
[0027] Another aspect of the invention is a method for decorating the dressing component of the watch case described above. The method comprises exposing the stack of thin layers to light on a predetermined exposure area. The phase of the phase-switching layer, and therefore its refractive index, is then changed in the exposed areas. The interference color of the laminate is locally changed by applying a tool onto the dressing component. Generates a pattern of tones.
[0028] In this way, when the watch case is assembled, the drawer of the watch case It is therefore possible to create two-tone decorations on the sealing components, Decorate the dressing components at any stage of the life of this portable watch case. Can be customized.
[0029] In implementing the present invention, the control unit controls the local switching of the phase switching layer. The laser beam is then applied to the target to control the temperature rise, exposure time, and shape of the desired exposure area. Causes the following to occur.
[0030] This feature allows the patterns to be created very precisely and allows for a wide variety of decorative ideas. It is possible to determine the size and production quality of such decorations.
[0031] By reading the following detailed description, given by way of example only and with reference to the accompanying drawings, in which: Other features and advantages of the present invention will become apparent. [Brief description of the drawings]
[0032] [Figure 1] 1 shows a schematic cross-sectional view of a watch case according to the invention; [Diagram 2] 2 shows a schematic cross-sectional view of a dressing component in the watch case of FIG. 1; [Diagram 3] 2 shows a schematic cross-sectional view of a dressing component for the watch case of FIG. 1, which dressing component forms a support for forming an encapsulating layer, in another example of an embodiment of the invention; [Figure 4] 2 shows diagrammatically a cross-sectional view of the dressing component for the watch case of FIG. 1, in which the support forms a substrate layer; [Diagram 5] 5 shows a schematic cross-sectional view of the dressing component on the watch case of FIG. 4, in which the substrate layer is light-transmitting. [Figure 6] 4 shows a schematic cross-sectional view of the dressing component on the watch case of FIG. 3, in which the substrate layer is light-transmitting; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0033] FIG. 1 shows a schematic cross-sectional view of a watch case 10 according to the present invention. The case 10 has a middle portion 11 to which a light-transmitting body 12 and a back portion 13 are fixed. These are fixed together to form an internal space.
[0034] The watch case 10 includes a dressing component 14 within the interior space, On this dressing component 14 a stack of thin layers 15 is deposited. The stack of layers 15 forms a coating on the dressing component 14 .
[0035] The laminate 15 is intended to be visible to the user, as will be described in more detail below. On the illustrated surface, several predetermined interference colors are applied to the dressing component 14. It is configured to give
[0036] Preferably, the dial will be fitted with a timepiece such as a rod or plate, as shown in FIG. The structure of the instrument movement 17, the oscillating weight, the flange, and the carrying A back of the watch case 10 is housed in the internal space of the watch case 10 or is on the watch case 10. The dressing part 13, the transparent body 12, and any other components such as a bezel The component 14 can be formed.
[0037] Hereinafter, the term “translucent body” refers to any of the translucent body 12 or the back part 13. Used to describe a transparent body.
[0038] The laminate 15 is interposed between a substrate layer 150, a light-transmitting encapsulation layer 152 and a spacer layer 153. The phase-switching layer 151 is a solid phase-switching layer that is bonded to the substrate 150 and has a spacing layer 153 that is spaced from the phase-switching layer 151. is separated from the substrate layer 150.
[0039] Here, the term "translucency" refers to the ability to transmit all or part of light radiation, especially light visible to the naked eye. It represents the ability of a material to transmit light.
[0040] The interference color may be produced by the encapsulation layer 1 in a reflective or transmissive form according to the relevant embodiment of the present invention. 52, interference caused by the configuration of the phase switching layer 151, the spacer layer 153 and the base layer 150 This occurs due to interference effects.
[0041] In the embodiment of the invention shown in FIG. 2, a support made of any suitable material A stack of thin layers 15 can be deposited on the support, said support being a dressing component. That is, the base layer 150 is formed by all or a part of the support 14. 15, is positioned to separate the spacing layer 153 from the support.
[0042] For example, the support may be a metallic material, silicon including its native oxide, in the form of a film, etc. Can be made of glass, quartz, sapphire, or polyethylene terephthalate do.
[0043] In the embodiment shown in FIG. 2, the substrate layer 150 may be formed by a reflective layer. This can be made, for example, by a metallic mirror, preferably platinum, rhodium, silver, aluminium, etc. The substrate layer is made of a material with high reflectivity, such as aluminum. Here, the thickness, which is defined as the dimension along the direction in which the thin layers overlap each other, is about 100 nm. It can be.
[0044] The spacing layer 153 is made of a light-transmitting dielectric material. The spacing layer 1 can be tin oxide, silicon dioxide, or zinc sulfide. 53 has a thickness in the range of 50 nm to 200 nm.
[0045] The phase switching layer 151, by virtue of its composition, changes color when exposed to suitable light. Thus, the crystalline or amorphous phase changes to the amorphous or crystalline phase, respectively. Has the ability.
[0046] In FIG. 1, such rays are indicated by dashed arrows.
[0047] In particular, the phase-switching layer 151 preferably has two phases that can be switched reversibly. That is, the phase-switching layer 151 is configured to have a phase state when exposed to light. After being heated, the initial crystalline or amorphous phase changes to the final amorphous or crystalline phase. The structure is such that each phase changes and can return to its initial phase.
[0048] In particular, when the thin layer stack 15 is exposed to light, the phase switching layer 151 locally changes temperature. The temperature is raised above the glass transition point for a relatively long time, for example, several seconds or tens of seconds. This causes the phase switching layer 151 to crystallize, i.e., change from the amorphous phase to the crystalline phase. above the melting point for a time short enough to induce the reaction and freeze the amorphous phase without recrystallization. By lowering the temperature, the phase switching layer 151 becomes amorphous, that is, changes from a crystalline phase to an amorphous phase. This induces a change to an amorphous phase.
[0049] In a preferred embodiment, the phase-switching layer 151 is in an amorphous phase such that the initial phase is After being deposited, it contains an amorphous phase.
[0050] The phase switching layer 151 has a refractive index that changes depending on whether it is in a crystalline phase or an amorphous phase. Therefore, when the phase of phase-switching layer 151 changes, the bending of phase-switching layer 151 The refractive index changes and therefore the interference color of the stack depends on the refractive index of the phase-switching layer 151. As long as the text is in the format, the visual appearance as perceived by the user changes.
[0051] That is, the phase-switching layer 151 has a refractive index that changes to one of two values after exposure to light. In addition, the thin-layer laminate 15 is locally formed through the encapsulation layer 152. The outer component has two different interference colors. It becomes possible.
[0052] Preferably, the phase switching layer 151 is made of Ge2Sb2Te5 or AgInSbTe. Preferably, the phase-switching layer 151 is made of a phase-change material having a thickness of 5 nm or more. It has a thickness in the range of 20 nm.
[0053] In the method for decorating a dressing component 14, a light beam is directed to a laminate 15 of thin layers. 1. A predetermined exposure area 16 on the surface is locally applied to the dressing component 14. Such a pattern is therefore It has an interference color different from the rest of the screen and can be used to display logos, text, or any other graphics. It can be a form of expression.
[0054] That is, a portion of the phase-switching layer 151 has an amorphous phase or a crystalline phase, and this phase switching The remainder of the replacement layer 151 has a different phase and therefore a different refractive index. Thus, two different interference colors can be generated.
[0055] The light beam is preferably generated by a laser beam, which is known to those skilled in the art. At least one of the phase switching layers 151 is controlled by a control unit that is naturally aware of the The local temperature increase, the exposure time and the predetermined exposure area 1 on the surface of the stack 15 of thin layers Control the shape of 6.
[0056] Preferably, the laser beam emits light having a wavelength in the infrared range and a wavelength in the visible range. Alternatively, the invention can be implemented using a laser whose beam emits light in the ultraviolet range. The operating power of the laser is relatively low, preferably about 50 mW, with a pulse duration of The time is about 5 ms, that is, the pulse energy is about 250 μJ. Therefore, the phase switching layer 151 may be damaged due to overheating, ablation, etc. 15. The phase-switching layer 151 switches phase without the risk of becoming unstable.
[0057] The encapsulation layer 152 protects the laminate 15, and in particular the phase switching layer 151, from oxygen. Through this encapsulation layer 152, the user can see the phase switching. Layer 151 can be seen.
[0058] Additionally, encapsulation layer 152 is transparent to the wavelength of light to which phase-switching layer 151 is exposed. It is.
[0059] The encapsulation layer 152 is made of indium tin oxide, silicon dioxide, or zinc sulfide, among others. It is possible.
[0060] The thickness and materials of the encapsulation layer 152 and the spacing layer 153 are selected depending on the desired color of the thin layer stack 15. In fact, the thickness and materials of the encapsulation layer 152 and the spacing layer 153 change the corresponding refractive index. , thus changing the interference color.
[0061] Preferably, the encapsulation layer 152 has a thickness of about 10 nm.
[0062] The laminate 15 of thin layers preferably has a very small thickness, so that the watch case can be easily worn. The watch case can be made of a portable watch without changing the design of the case 10 or the dressing component 14. The dressing component 14 of the substrate 10 may be deposited thereon.
[0063] Preferably, in another example embodiment of the invention shown in FIG. 3, the encapsulation layer 152 is It may be formed by a support, which is made of a light-transmitting material.
[0064] The laminate 15 of thin layers is observed by the user through the support.
[0065] In this case, the dressing component 14 is a translucent body made of a translucent material. In this way, the laminate 15 is preferably formed by It is disposed within the internal space of the watch case 10 and does not provide any friction.
[0066] Preferably, in another example embodiment of the present invention shown in FIG. is formed by the support, i.e. the dressing component 14 Here, the dressing component 14 may be made of platinum, rhodium, It is made of a reflective material such as silver or aluminum.
[0067] In the embodiment of the invention shown in FIGS. 2 and 3, the substrate layer 150 is formed by a reflective layer. Therefore, the laminate 15 is likely to reflect the exposed light and is opaque. It produces a beautiful appearance with vivid interference colors.
[0068] In another example embodiment of the invention shown in FIGS. 5 and 6, respectively, the substrate 150 comprises: Unlike the embodiment described above and shown in Figs. 2-4, the reflector is not formed by a reflective layer, but In particular, the base layer 150 is made of polyethylene terephthalate, glass, or the like. The optical fiber is formed from a transparent or semi-transparent material such as glass or sapphire.
[0069] In particular, in the embodiment of the invention shown in FIG. 5, the substrate layer 150 is formed by a support. In the embodiment shown in FIG. 6, the encapsulation layer 152 is formed by a support. .
[0070] In these embodiments of the present invention, the phase-switching layer 151, the spacing layer 153 and the substrate layer 1 The interference effect generated by the arrangement of 50 is of the transmission type.
[0071] In the embodiment shown in Figs. 5 and 6, the decoration produced by the laminate 15 is an encapsulation. Both layer 152 and substrate layer 150 are visible to a user.
[0072] In these embodiments of the invention, the dressing component 14 preferably comprises: It may be constituted by a transparent body or a face plate.
[0073] It should be noted, more generally, that the implementations and embodiments considered above are described by way of example. ,Therefore, other variants can be considered.
[0074] In principle, several different thin layers of the stack of thin layers 15 can be deposited by cathodic sputtering or It may be deposited by another suitable deposition method. [Explanation of symbols]
[0075] 10 Portable watch case 11 Middle Section 12 Translucent body 13 Back 14 Dressing Components 15 Thin layer laminate 16 Exposure Area 17 Timekeeping movements 150 Base material layer 151 Phase switching layer 152 Encapsulation Layer 153 Separation layer
Claims
1. The transparent body (12) and the back part (13) are fixed to the middle part (11) to form an internal space. A portable watch case (10) comprising: The watch case (10) has a dressing component in the internal space. A sensor (14) is provided, A substrate layer (150) and a solid phase-switchable layer (160) are disposed on the dressing component (14). A stack of thin layers (15) including a phase-switching layer (151) is deposited. 1) is a light-transmitting encapsulation layer (152) and a phase-switching layer (151) on the substrate layer (15 0) and a separation layer (153) separating the The phase-switching layer (151) is made of the light-transmitting encapsulation layer (152) and the separation layer (153). ) The separation layer (153) separates the phase-switching layer (151) from the substrate layer (150). Separate, The phase switching layer (151) is provided in the laminate (15) with at least two interference layers. having a refractive index that can be changed by exposure to light to impart color. It is composed of The substrate layer (150) is formed by a reflective layer, The laminate (15) may comprise any of the dressing components (14) or Deposited on a support formed by a part The encapsulation layer (152) is formed by the support. A portable watch case (10) characterized by:
2. The phase-switching layer (151) is configured to have two reversibly switchable phase states. It is composed of The phase states are a crystalline phase and an amorphous phase.
2. A watch case (10) according to claim 1 .
3. The encapsulation layer (152) changes the refractive index of the phase-switching layer (151) under the exposure to light. Translucent to the wavelengths of light that can be detected 2. A watch case (10) according to claim 1 .
4. The dressing component (14) is a dial, a timepiece movement (17) Structure, transparent body, display, needle, decoration, logo, or vibration weight.
2. A watch case (10) according to claim 1 .
5. A dressing component (14) for a watch case (10) according to claim 1 A method of decorating comprising the steps of: The laminate (15) is exposed to light on a predetermined exposure area (16) to form a pre-exposed layer. The phase of the phase-switching layer (151) is locally changed to allow the dressing component ( 14) Form a pattern on top A method comprising:
6. The light beam is generated by a laser beam controlled by a control unit. The local temperature rise of the replacement layer (151), the exposure time, and the predetermined exposed area (16) Controlling the shape of 6. The method of claim 5 .