Polyamic acid, polyamic acid composition, polyimide, polyimide film, and printed circuit board
A polyamic acid-based polyimide with an ester and dimer skeleton, formed via specific reaction conditions, addresses high dielectric and moisture absorption issues, offering low dielectric and moisture absorption for high-frequency applications.
Patent Information
- Application Number
- JP2023050564
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2043-03-27
AI Technical Summary
Existing polyimides exhibit high dielectric properties and moisture absorption, which hinder high-speed signal transmission and reliability in high-frequency applications, and there is a need for materials with low dielectric properties and low moisture absorption.
A polyamic acid is synthesized through a polyaddition reaction using ester-type acid dianhydride and dimer diamine, with a specific molar ratio, to form a polyimide with an ester and dimer skeleton, reducing dielectric constant and moisture absorption.
The resulting polyimide exhibits low dielectric properties, low moisture absorption, and improved heat resistance, suitable for high-frequency applications and flexible printed wiring boards.
Smart Images

Figure 2024139564000001 
Figure 2024139564000002 
Figure 2024139564000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a polyamic acid capable of forming a polyimide exhibiting low dielectric properties and low moisture absorption, and to a polyamic acid composition, a polyimide, a polyimide film and a printed wiring board produced using the same. [Background technology]
[0002] High dielectric strength and heat resistance are required for insulating materials used in mobile communication devices such as smartphones and tablets, and electronic devices such as computers and car navigation systems. Polyimide is a polymer formed by imidizing polyamic acid, which is generally synthesized from acid dianhydride and aromatic diamine compound, and is widely used as such insulating material due to its excellent heat resistance, mechanical properties, and insulating properties.
[0003] In recent years, the development of high-speed, large-capacity printed wiring boards for next-generation high-frequency wireless has been underway, and the adoption of circuit boards with multilayer wiring structures has made high-speed signal transmission possible. Polyimide is used as an interlayer insulating film in multilayer wiring structures, but typical polyimide has high dielectric properties such as dielectric constant, which causes delays in signal transmission and hinders speed increases. Furthermore, a high dielectric constant increases the electrostatic capacitance, so when used for high-speed (high-frequency) communication, the wiring near the insulating film heats up, which can cause failure of the printed wiring board.
[0004] In order to meet such high frequencies, there is an increasing demand for polyimides that exhibit low dielectric properties. For example, Patent Document 1 discloses that a polyimide prepared using an aromatic diamine having a specific structure and a tetracarboxylic dianhydride exhibits a low dielectric constant and is also excellent in heat resistance.
[0005] Also, a method is known in which the imide group concentration is reduced by introducing a fluorene skeleton into a diamine component, the polarity of the entire molecule is reduced, and the dielectric constant of the polyimide is reduced. For example, Patent Document 2 discloses that a polyimide using trimellitic anhydride chloride as the acid anhydride and 9,9-bis(4-aminophenyl)fluorene as the diamine exhibits high heat resistance and low relative dielectric constant.
[0006] On the other hand, since polyimides generally have imide groups that easily absorb water and have significantly different dielectric properties when hydrated and when dry, they are also required to exhibit low dielectric properties even under high humidity conditions. Therefore, it is desirable to form polyamides that exhibit not only low dielectric properties but also low hygroscopicity. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Japanese Patent Application Publication No. 10-152559 [Patent Document 2] JP 2005-298625 A Summary of the Invention [Problem to be solved by the invention]
[0008] In view of the above circumstances, an object of the present invention is to provide a polyamic acid capable of forming a polyimide exhibiting low dielectric properties and low moisture absorption, as well as a polyamic acid composition, a polyimide, a polyimide film, and a printed wiring board produced using the polyamic acid. [Means for solving the problem]
[0009] An embodiment of the present invention is a polyamic acid which is a polyaddition reaction product of (A) an ester-type acid dianhydride and (B) at least two diamines, and which is characterized in that the polyamic acid contains (B1) a dimer diamine in a molar ratio of 0.3 or more relative to the total diamine components.
[0010] In one embodiment of the present invention, the (A) ester-type acid dianhydride has a structure represented by the following formula (1). [ka] (In formula (1), Ar represents a substituted or unsubstituted arylene group.)
[0011] In one embodiment of the present invention, the (B) at least two diamines include (B2) an aromatic diamine.
[0012] Another embodiment of the present invention is a polyamic acid composition containing the above polyamic acid and (C) an organic solvent.
[0013] Another embodiment of the present invention is a polyimide obtained by imidizing the above polyamic acid.
[0014] Another aspect of the present invention is a polyimide film comprising the above polyimide.
[0015] Another aspect of the present invention is a printed wiring board comprising the above-mentioned polyimide film. Effect of the Invention
[0016] According to the present invention, it is possible to provide a polyamic acid capable of forming a polyimide exhibiting low dielectric properties and low moisture absorption, as well as a polyamic acid composition, a polyimide, a polyimide film, and a printed wiring board produced using the polyamic acid. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, an embodiment of the present invention will be described in detail. The polyamic acid of the present invention is a polyaddition reaction product of (A) an ester-type acid dianhydride and (B) at least two diamines, and contains (B1) dimer diamine at a molar ratio of 0.3 or more with respect to the total diamine components. That is, the polyimide formed using the polyamic acid of the present invention has an ester skeleton and a dimer skeleton, and can achieve low water absorption due to the ester skeleton. In addition, low dielectric properties are exhibited due to the dimer skeleton, and by containing a certain amount of dimer diamine as a diamine component, the dielectric constant and dielectric loss tangent can be further reduced, and the desired low dielectric properties can be realized. Furthermore, by the polyamide having a dimer skeleton, heat resistance is improved, and a polyamide with excellent thermal decomposition resistance can be formed.
[0018] (A) Ester-type acid dianhydride The polyamic acid of the present invention has a structural unit derived from an ester-type dianhydride having an ester bond in the molecule as the dianhydride component. The polyamic acid has a structural unit derived from an ester-type dianhydride, so that the polyimide obtained can be given low water absorption. The dianhydride has two acid anhydride groups in one molecule, and is preferably a tetracarboxylic acid dianhydride, and more preferably an aromatic tetracarboxylic acid dianhydride. The number of ester bonds in the molecule may be one or more, preferably one to three, and more preferably one or two. The ester-type dianhydride may be used alone or in combination of two or more kinds.
[0019] Such an ester-type acid dianhydride preferably has a structure represented by the following formula (1). In formula (1), Ar represents a substituted or unsubstituted arylene group, and the substituted arylene group means that a hydrogen atom of an unsubstituted arylene group is substituted with an arbitrary substituent. The number of carbon atoms of the substituted or unsubstituted arylene group (not including the number of carbon atoms of the substituent) is preferably 6 to 20, and more preferably 6 to 12.
[0020] [ka]
[0021] Examples of the unsubstituted arylene group in the group Ar include an o-phenylene group, an m-phenylene group, a p-phenylene group, a 2,6-naphthylene group, a 4,4'-biphenylylene group, etc. Among these, a p-phenylene group, a 2,6-naphthylene group, and a 4,4'-biphenylylene group are preferred.
[0022] The optional substituent in the substituted arylene group includes an alkyl group having 1 to 8 carbon atoms, a halogen atom (fluorine atom, chlorine atom, bromine atom, iodine atom), a halogenated alkyl group in which a hydrogen atom of the alkyl group is substituted with the halogen atom, and the like. Among these substituents, an alkyl group having 1 to 8 carbon atoms is preferred, and a methyl group is more preferred. The number of optional substituents may be one or two or more. When there are two or more substituents, the substituents may be the same or different. Specific examples of the substituted arylene group include a 2,2',3,3',5,5'-hexamethyl-4,4'-biphenylylene group, and the like.
[0023] The group Ar is preferably a p-phenylene group, a 2,6-naphthylene group, a 4,4'-biphenylylene group, a methylphenylene group, or a 2,2',3,3',5,5'-hexamethyl-4,4'-biphenylylene group.
[0024] Preferred examples of the ester-type acid dianhydride represented by formula (1) include a compound represented by the following formula (1-1) and a compound (TAHQ) represented by the following formula (1-2), and a compound (TMPBP-TME) represented by the following formula (1-2) is more preferred.
[0025] [ka]
[0026] (B) Diamine The polyamic acid of the present invention has a structural unit derived from at least two diamines as a diamine component, and one of the diamine components has a structural unit derived from (B1) dimer diamine. Here, dimer diamine means an aliphatic diamine in which two terminal carboxylic acid groups (-COOH) of a cyclic or acyclic dimer acid obtained as a dimer of an unsaturated fatty acid are substituted with a primary aminomethyl group (-CH2-NH2) or an amino group (-NH2). The polyamic acid has a structural unit derived from dimer diamine, so that the obtained polyimide can have low dielectric properties. The dimer diamine may be used alone or in combination of two or more kinds.
[0027] Dimer acid is a dibasic acid obtained by intermolecular polymerization of unsaturated fatty acids. Aliphatic diamines derived from dimer acids can be obtained by polymerizing unsaturated fatty acids such as oleic acid, linoleic acid, and linolenic acid to obtain dimer acids, reducing the dimer acids, and then aminating them. Such dimer diamines are preferably diamine compounds obtained by substituting the terminal carboxylic acid groups of dibasic acid compounds having carbon atoms in the range of 18 to 54, preferably 22 to 44, with primary aminomethyl groups or amino groups.
[0028] Commercially available dimer diamine products include "VERSAMINE (registered trademark) 551" and "VERSAMINE (registered trademark) 552" manufactured by Cognics Japan, and "PRIAMINE (registered trademark) 1073", "PRIAMINE (registered trademark) 1074", and "PRIAMINE (registered trademark) 1075" manufactured by Croda Japan.
[0029] In the polyamic acid of the present invention, the dimer diamine (B1) is contained in a molar ratio of 0.3 or more to the total diamine components. By containing the dimer diamine in a specific molar ratio or more to the total diamines, the resulting polyimide can be given a lower dielectric constant and a lower dielectric loss tangent. The molar ratio of the dimer diamine (B1) to the total diamine components is preferably 0.3 or more, and more preferably 0.4 or more.
[0030] The polyamic acid of the present invention may contain an aromatic diamine (B2) as another diamine component. Examples of the aromatic diamine include p-phenylenediamine (PDA), m-phenylenediamine, 4,4'-oxydianiline (ODA), 3,3'-bistrifluoromethyl-4,4'-diaminobiphenyl (TFMB), 3,4'-diaminodiphenyl ether, 4,4'-diaminodiphenylmethane, 3,3'-dimethyl-4,4'-diaminodiphenylmethane, 2,2-bis[4-(4-aminophenoxy)phenyl]propane, 1,2-bis(anilino)ethane, diaminodiphenylsulfone, Examples of the aromatic diamines include diaminobenzanilide, diaminobenzoate, diaminodiphenyl sulfide, 2,2-bis(p-aminophenyl)propane, 2,2-bis(p-aminophenyl)hexafluoropropane, 1,5-diaminonaphthalene, diaminotoluene, diaminobenzotrifluoride, 1,4-bis(p-aminophenoxy)benzene, 4,4'-bis(p-aminophenoxy)biphenyl, diaminoanthraquinone, and 4,4'-bis(3-aminophenoxyphenyl)diphenylsulfone. Among these aromatic diamines, PDA, ODA, and TFMB are preferred, and ODA is more preferred. The aromatic diamines may be used alone or in combination of two or more.
[0031] The molar ratio of the diamine to the ester-type acid dianhydride [(B) / (A)] is not particularly limited, but is preferably 0.90 to 1.10, more preferably 0.95 to 1.05, even more preferably 0.97 to 1.03, and particularly preferably 0.98 to 1.02.
[0032] <Polyamic Acid and Polyamic Acid Composition> (C) Organic Solvent The polyamic acid of the present invention can be synthesized by a known general method. For example, a polyamic acid composition (polyamic acid solution) can be obtained by reacting an ester-type acid dianhydride with a diamine in an organic solvent (C). The organic solvent used for the polymerization of the polyamic acid is not particularly limited as long as it can dissolve the ester-type acid dianhydride and diamine as monomer components and dissolve the polyamic acid produced by the polyaddition reaction. Examples of such organic solvents include urea-based solvents such as tetramethylurea and N,N-dimethylethylurea; sulfone-based solvents such as dimethylsulfoxide, diphenylsulfone, and tetramethylsulfone; amide-based solvents such as N,N-dimethylacetamide, N,N-dimethylformamide, N,N'-diethylacetamide, N-methyl-2-pyrrolidone, and hexamethylphosphoric acid triamide; ester-based solvents such as γ-butyrolactone; halogenated alkyl solvents such as chloroform and methylene chloride; aromatic hydrocarbon-based solvents such as benzene and toluene; phenol-based solvents such as phenol and cresol; ketone-based solvents such as cyclopentanone; and ether-based solvents such as tetrahydrofuran, 1,3-dioxolane, 1,4-dioxane, dimethyl ether, diethyl ether, and p-cresol methyl ether. These organic solvents may be used alone or in combination of two or more. From the viewpoint of increasing the solubility and reactivity of the polyamic acid, the organic solvent is preferably selected from the group consisting of amide solvents, ketone solvents, ester solvents, and ether solvents, and amide solvents such as N,N-dimethylacetamide, N,N-dimethylformamide, N,N'-diethylacetamide, and N-methyl-2-pyrrolidone are preferred.
[0033] The molecular weight of the polyamic acid can be adjusted by adjusting the molar ratio between the total number of moles of the ester-type acid dianhydride components and the total number of moles of the diamine components. The molecular weight (weight average molecular weight) of the polyamic acid is not particularly limited, but is more preferably 10,000 or more and 100,000 or less from the viewpoint of solubility in organic solvents. The weight average molecular weight of the polyamic acid can be determined, for example, from a standard polystyrene-equivalent value measured by gel permeation chromatography (GPC).
[0034] The synthesis of polyamic acid by the polyaddition reaction of ester-type acid dianhydride and diamine is preferably carried out in an inert atmosphere such as argon or nitrogen. In an inert atmosphere, the ester-type acid dianhydride and diamine are dissolved in an organic solvent and mixed to proceed with the polyaddition reaction. The order of addition of the ester-type acid dianhydride and diamine is not particularly limited. For example, the diamine may be dissolved or dispersed in a slurry in an organic solvent to prepare a diamine solution, and the ester-type acid dianhydride may be added to the diamine solution. The ester-type acid dianhydride and diamine may be added directly to the organic solvent in a solid state, or may be added in a state of being dissolved or dispersed in a slurry in an organic solvent separately.
[0035] The temperature conditions for the polyaddition reaction are not particularly limited, but from the viewpoint of suppressing a decrease in the molecular weight of the polyamic acid due to depolymerization, the reaction temperature is preferably 100° C. or less, and from the viewpoint of allowing the polyaddition reaction to proceed appropriately, the reaction temperature is more preferably 20 to 80° C. The reaction time may be set arbitrarily within the range of 1 to 72 hours, and may be allowed to stand overnight at room temperature as necessary.
[0036] The viscosity of the solution when preparing the polyamic acid composition of the present invention is preferably 500 mPa·s or more from the viewpoint of film-forming properties. The concentration of the polyamic acid in the polyamic acid composition of the present invention is preferably 10% by mass or more, more preferably 15% by mass or more, and even more preferably 25% by mass or more. In particular, if the concentration of the polyamic acid is 15% by mass or more, the productivity when forming a polyimide coating film using the polyamic acid can be increased. The upper limit of the concentration of the polyamic acid is preferably 50% by mass or less, more preferably 30% by mass or less, from the viewpoint of sufficiently dissolving the polyamic acid in an organic solvent.
[0037] In order to impart processing properties and various functionalities to the polyamic acid and the polyimide formed using the polyamic acid, various organic or inorganic low-molecular or high-molecular compounds may be blended into the polyamic acid composition. For example, the polyamic acid composition may contain a dye, a surfactant, a leveling agent, a plasticizer, fine particles, a sensitizer, a silane coupling agent, etc. The fine particles may be either organic fine particles or inorganic fine particles, and may have a porous or hollow structure.
[0038] <Polyimide> The method for converting polyamic acid to polyimide is not particularly limited, but polyimide can be produced by dehydrating and ring-closing (imidizing) the polyamic acid obtained as described above. The dehydrating and ring-closing (imidizing) method can be a known method such as thermal imidization, which involves dehydrating and ring-closing by heating, or chemical imidization, which involves chemical ring-closing using a known dehydrating and ring-closing catalyst.
[0039] In the case of thermal imidization, the heating temperature is preferably 120 to 350°C, more preferably 150 to 250°C. The heating time is preferably 0.5 to 3 hours, more preferably 1 to 2 hours. In the case of chemical imidization, for example, pyridine, triethylamine, acetic anhydride, etc. can be used as the dehydration ring-closing catalyst. In this case, the reaction temperature can be selected from any temperature between 20 and 100°C, and is preferably 50°C or less, and the reaction time is preferably 1 to 3 hours. The imidization may be performed in air, under reduced pressure, or in an inert gas such as nitrogen, but in order to obtain a polyimide film with high transparency, it is preferable to perform the imidization under reduced pressure or in an inert gas such as nitrogen.
[0040] The molecular weight (weight average molecular weight) of the polyimide is not particularly limited, but is preferably from 10,000 to 100,000 in terms of the low dielectric properties, solubility in organic solvents, and film-forming properties of the resulting polyimide. The weight average molecular weight of the polyimide can be determined, for example, from a standard polystyrene-equivalent value measured by gel permeation chromatography (GPC).
[0041] <Polyimide film> The polyimide film of the present invention includes the polyimide obtained as described above. The method for producing such a polyimide film is not particularly limited, and for example, the above-mentioned polyamic acid composition is applied to a film on a substrate (e.g., plastic films such as polyethylene, polypropylene, urethane, polyester, polyethylene terephthalate (PET) or polycarbonate, glass plate, stainless steel plate, copper plate including thin copper foil, aluminum plate, etc.), and then dried and heated to remove the solvent and perform dehydration ring closure (imidization); or the polyimide obtained by converting the polyamic acid into a polyimide is dissolved in an organic solvent, and the polyimide solution is applied to a film on a substrate and the solvent is dried and removed. The method for applying to the substrate is not particularly limited, and a conventionally known application method can be applied.
[0042] The thickness of the polyimide film is not particularly limited and can be appropriately selected depending on the application. The thickness of the polyimide film is preferably 10 to 100 μm, more preferably 20 to 50 μm. The thickness of the polyimide film can be easily controlled by appropriately adjusting the solid concentration, coating thickness, and viscosity of each component in the polyamic acid composition.
[0043] <Printed wiring board> The polyimide film of the present invention is preferably used as a film for various components such as color filters, flexible displays, semiconductor parts, and optical components. Since the polyimide film exhibits insulating properties, it is preferably used as an insulating substrate for printed wiring boards. In addition, since the polyimide film is a thin and flexible film exhibiting insulating properties, it is also effectively used as a base film for flexible circuit boards called flexible printed wiring boards (FPCs). EXAMPLES
[0044] Next, examples of the present invention will be described, but the present invention is not limited to these examples as long as they do not depart from the spirit of the present invention.
[0045] <Examples 1 to 2, Comparative Examples 1 to 3> The organic solvent in which the aromatic diamine shown in Table 1 below was dissolved was added to a separable flask in the blending ratio shown in Table 1 below, and then the dimer diamine and the acid dihydrate shown in Table 1 below were added in this order in the blending ratio shown in Table 1 below. The resulting mixture was stirred at 50 to 80°C for 2 hours, and further stirred at room temperature for 24 hours to prepare polyamic acid compositions used in Examples 1 to 2 and Comparative Examples 1 to 3. The prepared polyamic acid composition was applied to a substrate using a test piece preparation process described below to prepare a test piece. The prepared test pieces were used to evaluate each of the characteristics shown in Table 1 below. The evaluation results are shown in Table 1. The blending amount of each component shown in Table 1 below is in parts by mass unless otherwise specified.
[0046] [Table 1]
[0047] Details of each component in Table 1 are as follows: (A1) Ester-type acid dianhydride TMPBP-TME: Honshu Chemical Co., Ltd., 2,2',3,3',5,5'-hexamethyl[1,1'-biphenyl]-4,4'-diyl bis(1,3-dioxo-1,3-dihydro-2-benzofuran-5-carboxylate) (A2) Tetracarboxylic acid dianhydride PMDA: Pyromellitic dianhydride (B1) Dimer diamine PRIAMINE® 1075: Dimer diamine, manufactured by Croda Japan (B2) Aromatic diamine 4,4-ODA: 4,4-oxydianiline (C) Organic Solvent NMP: N-methyl-2-pyrrolidone
[0048] <Test piece preparation process> A PET film (Nihei Chemical Industries, Ltd., "Micro-adhesive Sheet for Processing PET75": 75 μm thick) used as a substrate was surface-treated (degreased) with isopropyl alcohol, and then the polyamic acid compositions prepared in Examples 1-2 and Comparative Examples 1-3 were applied onto the substrate using a bar coater, followed by pre-drying at 80° C. for 30 minutes. After pre-drying, the substrate was thermally cured by post-curing at 150° C. for 1 hour and then at 180° C. for 30 minutes to form a cured coating film (polyimide film) having a predetermined thickness on the substrate, and a test specimen was prepared.
[0049] <Evaluation> (1) Dielectric constant and dielectric tangent In the test piece preparation process, the test pieces were prepared so that the thickness of the cured coating film was 30 μm ± 10 μm. Next, the obtained test pieces were cut into samples with a length of 50 mm and a width of 2 mm by a cavity resonance method using a network analyzer and a cavity resonator manufactured by Key Sight Technologies, and the dielectric constant and dielectric loss tangent were measured under the conditions of a measurement temperature of 25°C, a measurement humidity of 50 RH%, and a frequency of 10 GHz. In addition, after heating for 200 hours in an atmosphere with a temperature of 85°C and a humidity of 80 RH%, the dielectric constant and dielectric loss tangent at a frequency of 10 GHz were also measured.
[0050] (2) Elastic modulus In the test piece preparation process, test pieces were prepared so that the thickness of the cured coating film was 50 μm ± 10 μm. Next, the formed cured coating film was peeled off from the substrate, and the specimen was cut to a predetermined size. The elastic modulus of the specimen was measured at a pulling speed of 5 mm / min using an autograph manufactured by Shimazu Corporation.
[0051] (3) Elongation and breaking strength The same samples as those prepared for the measurement of elastic modulus were used to measure the elongation and strength at break at a tensile speed of 5 mm / min using an autograph manufactured by Shimazu Corporation.
[0052] (4) Water absorption rate In the test piece preparation step, the test pieces were prepared so that the thickness of the cured coating film was 30 μm±10 μm. The obtained test pieces were cut into 2-3 cm squares, and the samples were immersed in distilled water for 24 hours, then taken out and the moisture on the surface was wiped off with a cloth.Then, using a moisture measuring device manufactured by HIRANUMA, the samples were heated to 150°C by the Karl Fischer method, and the water absorption rate was measured based on the amount of moisture released from the samples.
[0053] (5) Heat decomposition resistance In the test piece preparation process, the test pieces were prepared so that the thickness of the cured coating film was 30 μm ± 10 μm. The obtained test pieces were cut into small pieces, and the temperature at which the weight was reduced by 5% in an air atmosphere at a heating rate of 10°C / min was measured using a thermogravimetric analyzer (Hitachi High-Tech Science Corporation, thermogravimetric analyzer "STA 7200RV"), and evaluated as the thermal decomposition temperature (Td5) [°C].
[0054] (6) Breakdown voltage In the test piece preparation process, the polyamic acid compositions prepared in Examples 1-2 and Comparative Examples 1-3 were uniformly applied to a copper-clad laminate (ESPANEX) using a bar coater so that the thickness of the cured coating film was 30 μm±10 μm, and then the above-mentioned thermal curing process from pre-drying to post-cure was carried out to form a cured coating film. Next, the dielectric breakdown voltage of the formed cured coating film was evaluated using a voltage resistance tester manufactured by Keisoku Gijutsu Kenkyusho Co., Ltd. under the conditions of a set voltage of 12 kv, a set current of 9999 μA, and a voltage rise rate of 500 V / sec.
[0055] As shown in Table 1, in Examples 1 and 2, which used polyamic acids obtained by polyaddition reaction of ester-type acid dianhydride with diamines containing dimer diamine at a molar ratio of 0.3 or more to the total diamine components, polyimides having low dielectric constants, dielectric tangents, and water absorption coefficients and exhibiting low dielectric properties and low moisture absorption were produced.
[0056] On the other hand, in Comparative Example 1, in which tetracarboxylic dianhydride was used as the acid dianhydride instead of the ester type acid dianhydride, the water absorption rate was higher than in Examples 1 and 2, and it was not possible to prepare a polyimide exhibiting the desired low moisture absorption. In Comparative Example 1, since high absorbency was exhibited, the dielectric constant and dielectric loss tangent were not measured after heating for 200 hours in an atmosphere at a temperature of 85°C and a humidity of 80 RH%.
[0057] In addition, in Comparative Examples 2 and 3, in which the molar ratio of dimer diamine to the total diamine components was less than 0.3, the dielectric constant and dielectric loss tangent were high in both cases, and polyimides exhibiting the desired low dielectric properties could not be produced. In particular, in Comparative Example 3, which does not contain dimer diamine as a diamine, the dielectric constant and dielectric loss tangent were higher than those of Examples 1-2 and Comparative Examples 1-2, and further, since thermal imidization was not completed, there was dehydration behavior, the weight loss was rapid, and the thermal decomposition resistance was also poor. In Comparative Examples 2 and 3, since they showed high dielectric constants and dielectric loss tangents, the absorbency was not measured, and in Comparative Example 2, the dielectric constant and dielectric loss tangent after heating for 200 hours in an atmosphere at a temperature of 85°C and a humidity of 80 RH% were not measured. [Industrial Applicability]
[0058] The polyamic acid of the present invention can form a polyimide that exhibits not only good insulating properties and mechanical strength but also low dielectric properties and low moisture absorption. Therefore, a polyimide film prepared using such a polyimide is highly useful, for example, as an insulating substrate for a printed wiring board, in particular as a base film for a flexible printed wiring board.
Claims
1. A polyamic acid which is a polyaddition reaction product of (A) an ester-type dianhydride and (B) at least two diamines, A polyamic acid comprising (B1) a dimer diamine in a molar ratio of 0.3 or more based on the total diamine components.
2. The polyamic acid according to claim 1 , wherein the ester-type acid dianhydride (A) has a structure represented by the following formula (1): 【Chemistry 1】 (In formula (1), Ar represents a substituted or unsubstituted arylene group.)
3. The polyamic acid according to claim 1 or 2, wherein the (B) at least two diamines include (B2) an aromatic diamine.
4. A polyamic acid composition comprising the polyamic acid according to claim 1 or 2 and (C) an organic solvent.
5. A polyimide obtained by imidizing the polyamic acid according to claim 1 or 2.
6. A polyimide film comprising the polyimide according to claim 5 .
7. A printed wiring board comprising the polyimide film according to claim 6.
Citation Information
Patent Citations
Resin composition
JP2012180471A
Thermosetting ink composition and application of the same
JP2013032501A
Solvent-soluble polyimide resin, method for producing the same, polyimide composition containing the polyimide resin, polyimide film and coated article
JP2013155329A
Polyimide composition
JP2015526561A
Low dielectric polyimide composite film for flexible copper clad laminates
KR102473679B1
Cited By
Polyamic acid, polyamic acid compositions, polyimides, polyimide films, resin-coated copper foil, multilayer wiring boards, coil structures, magnetic devices, and insulated wires.
JP2026160629A
Photosensitive polyesterimide resin