Battery processing method

By submerging electrodes in water and applying electric pulses, the method efficiently separates laminated electrodes in batteries, addressing the inefficiencies of previous techniques and reducing separation time.

JP2024140716APending Publication Date: 2024-10-10HONDA MOTOR CO LTD

Patent Information

Application Number
JP2023052017
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Existing methods for separating laminated electrodes in batteries, such as those in lithium ion and all-solid-state batteries, are time-consuming and may not effectively separate all parts due to orientation variations.

Method used

A method involving submersion in water followed by applying an electric pulse to the laminated electrode to separate the positive and negative electrode plates, using conductive members to facilitate electrical connection and Joule heating for efficient separation.

Benefits of technology

The method allows for easy and rapid separation of laminated electrodes, improving efficiency and reducing the time required compared to conventional methods.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024140716000001_ABST
    Figure 2024140716000001_ABST
Patent Text Reader

Abstract

To separate laminated electrodes easily and in a short time.SOLUTION: In a battery processing method for a lithium ion battery or an all-solid-state battery having a laminated electrode in which positive and negative electrode plates are laminated with a separator interposed therebetween, after deactivating lithium, a submersion process S3 in which the laminated electrode 21 is submerged in water, and a separation process S4 in which an electric pulse is applied to the laminated electrode 21 to separate the laminated electrode 21 are performed.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for treating a battery. [Background technology]

[0002] Some lithium-ion batteries and all-solid-state batteries are equipped with a laminated electrode in which a positive electrode plate and a negative electrode plate are laminated with a separator between them. The positive electrode mixture of this type of battery uses a ternary cathode material (NCM) consisting of nickel, cobalt, and manganese. When disposing of batteries, it is desirable to recover valuable metals such as NCM. The method of crushing batteries to recover valuable metals, etc., is time-consuming and labor-intensive because the disassembled battery material is broken into fine particles. As a method other than crushing, a method has been proposed in which after removing the exterior body made of a laminate film, the laminated electrode is submerged in water and a relative motion is applied between the laminated electrode and the water to separate the positive and negative electrode plates (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 7120158 Publication Summary of the Invention [Problem to be solved by the invention]

[0004] However, the method of separating the workpieces by relative movement takes time, and depending on the orientation of the workpieces in the water, some parts may not be separated. The present invention has been made in consideration of the above-mentioned circumstances, and has an object to separate stacked electrodes easily and in a short time. [Means for solving the problem]

[0005] The present invention provides a method for treating a battery, which is either a lithium ion battery or an all-solid-state battery and has a stacked electrode in which a positive electrode plate and a negative electrode plate are stacked with a separator interposed therebetween, the method comprising: a submersion step of submerging the stacked electrode in water after deactivating lithium; and a separation step of applying an electric pulse to the stacked electrode to separate the stacked electrode. Effect of the Invention

[0006] The laminated electrodes can be separated easily and in a short time. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a diagram illustrating a target battery to which the battery treatment method of the present invention can be applied. [Diagram 2] 1 is a diagram showing each step of a method for treating a target battery. FIG. [Diagram 3] FIG. 1 is a diagram showing a schematic diagram of the state of a target battery before and after a deactivation and submersion process in the case where the target battery is a fully solid state battery. [Figure 4] FIG. 13 is a diagram illustrating a separation process. [Diagram 5] FIG. 13 is a diagram showing a schematic diagram of application of an electric pulse in a separation process. [Figure 6] FIG. 11 is a diagram showing another example of a state in which an electric pulse is applied in the separation process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0009] [Embodiment] FIG. 1 is a diagram illustrating a battery to which the battery treatment method of the present invention can be applied (hereinafter, referred to as a target battery). The subject battery 10 is a secondary battery such as a lithium ion battery or an all-solid-state battery, and is configured as a laminate type. The subject battery 10 has a laminated electrode 21 made of a multi-layer body in which a positive electrode plate 11 and a negative electrode plate 12 are laminated with a separator 13 interposed therebetween. The laminated electrode 21 is covered with a laminate material 22 that constitutes an exterior body, and a pair of current collecting tabs 23A, 23B are exposed to the outside from the laminate material 22.

[0010] The target battery 10 can be a pouch-type battery, a laminate-type battery cell, a pouch-type battery cell, a lithium-ion battery cell, a battery module, or the like. The subject battery 10 is a battery that has attracted attention as an energy storage device with high energy density, and is expected to become even more widespread in the future. In addition, the subject battery 10 contains valuable metals such as nickel-, cobalt-, and manganese-based ternary positive electrode materials (NCMs), and it is therefore desirable to recover the valuable metals when the battery is disposed of.

[0011] The configuration of the subject battery 10 will be further explained. As shown in FIG. 1, the positive electrode plates 11 and the negative electrode plates 12 are arranged alternately, and a plurality of pairs of electrode plate groups each consisting of a positive electrode plate 11 and a negative electrode plate 12 are provided. Each positive electrode plate 11 includes a rectangular positive electrode current collector 31, and a positive electrode composite material 32 containing NCM is provided on both sides of the positive electrode current collector 31. The positive electrode current collector 31 is, for example, an aluminum foil or an aluminum plate. The positive electrode composite material 32 is, for example, a positive electrode active material such as lithium nickel oxide or lithium cobalt oxide, a conductive material, a conductive material agent, a binder, etc. A positive electrode terminal 11A extends from each positive electrode plate 11, and each positive electrode terminal 11A is connected to a positive electrode side current collector tab 23A.

[0012] Each negative electrode plate 12 includes a rectangular negative electrode current collector 41, and has a negative electrode mixture 42 on the surface facing the positive electrode plate 11. A negative electrode terminal 12A extends from each negative electrode plate 12, and each negative electrode terminal 12A is connected to a negative electrode side current collector tab 23B. The pair of current collecting tabs 23A, 23B are formed from a thin metal plate such as copper or aluminum, and are exposed to the outside through between two laminate materials 22 that form the exterior body. The laminate material 22 is, for example, a laminate film whose base material is a metal material such as an aluminum alloy or stainless steel, and functions as an exterior body having a predetermined strength and as a sealant that seals the laminated electrode 21.

[0013] The separator 13 is disposed between the positive electrode plate 11 and the negative electrode plate 12, and prevents a short circuit between the positive electrode plate 11 and the negative electrode plate 12. When the target battery 10 is a lithium ion battery, the inside of the target battery 10, i.e., the inside of the laminate material 22, is filled with an electrolyte. In contrast, when the subject battery 10 is an all-solid-state battery, there is no electrolyte in the laminate material 22, and a solid electrolyte is provided between the positive electrode plate 11 and the negative electrode plate 12. This solid electrolyte also serves as the separator 13.

[0014] As the electrolyte solution and the electrolyte of the solid electrolyte, a lithium salt compound such as lithium hexafluorophosphate (LiPF6) is used. Note that the configurations of the target battery 10 are not limited to the above configurations, and the configurations of conventional laminated batteries can be applied.

[0015] Next, a method for treating the subject battery 10 suitable for extracting valuable metals such as NCM will be described. Fig. 2 is a diagram showing each step of the method for treating the target battery 10. Fig. 3 to Fig. 5 are diagrams showing the state of each step. As shown in FIG. 2, the method for treating the target battery 10 includes a cutting step S1, a deactivation step S2, a submersion step S3, and a separation step S4. In the cutting step S1, a part of the laminate material 22 constituting the exterior body is cut open to make it possible to access the stacked electrode 21 from the outside. If the target battery 10 is a lithium ion battery, the electrolyte is discharged from the cut area.

[0016] In the deactivation step S2, a part of the lithium contained in the laminated electrode 21 is converted to a lithium compound such as lithium hydroxide by using a known method such as submersion or showering, and the lithium is made to dissolve in water. If hydrogen sulfide is generated, it is necessary to perform aeration and neutralization treatment. In the submersion step S3, the laminated electrode 21 is immersed in water to dissolve the water-soluble lithium hydroxide, solid electrolyte, etc. in water.

[0017] Fig. 3 shows a schematic diagram of the state before and after the deactivation and submersion steps S2 and S3 in the case where the target battery 10 is a fully solid battery. As shown in Fig. 3, the deactivation and submersion steps S2 and S3 allow at least a part of the solid electrolyte and elemental lithium to be separated, thereby suppressing the charge and discharge reaction. In the subsequent separation step S4, an electric pulse is applied to the laminated electrode 21 to separate the laminated electrode 21.

[0018] 3, the laminated electrode 21 and its surroundings become sparse, which may cause the laminated electrode 21 to lose continuity and not conduct electricity. Therefore, in the separation step S4, before the application of the electric pulse, a step of electrically connecting the electrode plates 11, 12 of the laminated electrode 21 to each other by passing a predetermined conductive member 51 through the laminated electrode 21, that is, a step of shorting the electrode plates 11, 12 to each other is performed as shown in FIG.

[0019] 4 illustrates an example in which a metal rod with a pointed tip is used as the predetermined conductive member 51, and multiple conductive members 51 are inserted into the laminated electrode 21 from the outside of the laminate material 22 at intervals in the longitudinal direction of the electrode plates 11, 12. This allows the electrode plates 11, 12 to be electrically connected to each other easily and in a short time while the laminated electrode 21 is covered with the laminate material 22. In addition, since the plates 11, 12 are electrically connected to each other at multiple points, a conductive path suitable for short-circuiting the electrode plates 11, 12 can be formed. In order to prevent electrical conduction between the conductive member 51 and the laminate material 22, it is preferable to provide a gap S or the like that physically separates the conductive member 51 and the laminate material 22.

[0020] FIG. 5 shows a schematic diagram of the state in which an electric pulse is applied in the separation step S4. As shown in Fig. 5, an electric pulse application device 55 is connected to a pair of current collecting tabs 23A, 23B of a target battery 10. The electric pulse application device 55 applies an electric pulse to each of the electrode plates 11, 12 of the laminated electrode 21 by applying a high-voltage electric pulse between the pair of current collecting tabs 23A, 23B. The electric pulse generates Joule heat, and the Joule heat melts each part, allowing the electrode plates 11, 12 of the laminated electrode 21 and the residue to be separated. In this case, the part of the positive electrode mixture 32 with high resistance is likely to become hot, making it easier to separate the remaining positive electrode mixture 32. In this manner, by applying an electric pulse using the pair of current collecting tabs 23A, 23B and by utilizing the electric pulse, the stacked electrode 21 can be separated easily and in a short time.

[0021] Incidentally, for example, in the case where an aluminum foil is used for the positive electrode current collector 31 and a copper foil is used for the negative electrode current collector 41, if a plurality of conductive members 51 are inserted through the laminated electrode 21 as shown in Fig. 4, when a current is applied, the current flows more to the copper foil side because copper has a higher electrical conductivity than an aluminum alloy. As a result, the amount of current passing through the aluminum foil decreases, and there is a risk that the separation efficiency of the positive electrode current collector 31, which is the original purpose, may decrease. In this case, as shown in Fig. 6, a single conductive member 51 may be inserted through a region of the stacked electrode 21 near the negative electrode side current collecting tab 23B, and a high voltage electric pulse may be applied between the pair of current collecting tabs 23A, 23B. As a result, the electric pulse flows along the path shown by the dashed line in Fig. 6.

[0022] With regard to the path through which this electric pulse flows, only a portion (corresponding to the path between the negative electrode side current collector tab 23B and the conductive member 51) of the negative electrode current collector 41 serves as the electric current path, while the majority (corresponding to the path between the conductive member 51 and the positive electrode side current collector tab 23A) of the positive electrode current collector 31 serves as the electric current path. This allows more current to be passed through the positive electrode current collector 31 than through the negative electrode current collector 41, and even if the electrical conductivity of the negative electrode current collector 41 is higher than that of the positive electrode current collector 31, it becomes possible to increase the separation efficiency of the positive electrode current collector 31. In other words, in this configuration, the target battery 10 is one in which the negative electrode side current collecting tab 23B is positioned on the opposite side of the positive electrode side current collecting tab 23A across the stacked electrode 21. A conductive member 51 is inserted into the region of the stacked electrode 21 of this target battery 10 closer to the negative electrode side current collecting tab 23B, and an electric pulse is applied to the stacked electrode 21 via the positive and negative electrode side current collecting tabs 23A, 23B. This allows more current to flow to the positive electrode current collector 31 than to the negative electrode current collector 41, and makes it possible to increase the separation efficiency of the positive electrode current collector 31 even when the negative electrode current collector 41 has higher electrical conductivity than the positive electrode current collector 31.

[0023] As described above, in this embodiment, after deactivating lithium, a submersion step S3 is performed in which the laminated electrode 21 is submerged in water, which can suppress the reaction between lithium and water and can dissolve water-soluble lithium hydroxide, solid electrolytes, etc. After the submersion step S3, a separation step S4 is performed in which an electric pulse is applied to the laminated electrode 21 to separate the laminated electrode 21, which can separate the laminated electrode 21 easily and in a short time. This enables the laminated electrode 21 to be separated more easily and in a shorter time than the conventional crushing method or the method of peeling off the electrode plates 11, 12 by relative movement.

[0024] In addition, in the separation step S4, an electric pulse is applied to the laminated electrode 21 after the electrodes 11, 12 of the laminated electrode 21 are brought into electrical conduction with each other. This makes it possible to apply an electric pulse to all of the electrodes 11, 12, making it easier to separate the laminated electrode 21 appropriately.

[0025] In addition, since the electrodes 11, 12 of the laminated electrode 21 are electrically connected to each other by passing a predetermined conductive member 51 through the laminated electrode 21, the electrodes 11, 12 can be easily and quickly connected to each other. Moreover, the electrodes 11, 12 can be electrically connected to each other without removing the laminate material 22 of the laminated electrode 21. The conductive member 51 is not limited to a metal bar having a pointed tip as shown in Fig. 4. For example, a stapler that drives a gate-shaped needle into the stacked electrode 21 may be used to bring the plates 11 and 12 into electrical contact with each other.

[0026] 6, the subject battery 10 is a battery in which the negative electrode side current collector tab 23B is disposed on the opposite side of the positive electrode side current collector tab 23A across the laminated electrode 21, and a conductive member 51 is inserted through a region of the laminated electrode 21 closer to the negative electrode side current collector tab 23B, and an electric pulse is applied to the laminated electrode 21 via the positive and negative electrode side current collector tabs 23A, 23B. This allows more current to be passed through the positive electrode current collector 31 than through the negative electrode current collector 41, and makes it possible to increase the separation efficiency of the positive electrode current collector 31 even when the negative electrode current collector 41 has higher electrical conductivity than the positive electrode current collector 31. The position and number of conductive members 51 may be appropriately changed as long as the separation efficiency of positive electrode current collector 31 can be sufficiently ensured, and the arrangement of conductive members 51 shown in FIG. 3 may be adopted.

[0027] Moreover, the subject battery 10 is a laminate type in which the laminate electrode 21 is covered with a laminate material 22 and a pair of current collecting tabs 23A, 23B are exposed outside the laminate material 22, and an electric pulse is applied to the laminate electrode 21 by using the pair of current collecting tabs 23A, 23B. This allows for easy electrical connection between the electric pulse application device 55 and the laminate electrode 21. Also, it becomes possible to apply an electric pulse to the laminate electrode 21 without removing the laminate material 22.

[0028] Furthermore, if the target battery 10 has an electrolyte, the submersion step S3 is performed after removing the electrolyte, deactivating the lithium, and removing the electrolyte, so that the reaction between lithium and water can be sufficiently suppressed. If the target battery 10 is a laminate type, the electrolyte can be easily removed by cutting open a part of the laminate material 22 and draining the electrolyte. Furthermore, after removing the electrolyte, the laminate type battery can be submerged in a treatment liquid (e.g., salt water) so that the treatment liquid can enter the laminate from the cut part and deactivate the lithium and remove the electrolyte, making the work easy.

[0029] The above embodiment is merely one embodiment of the present invention, and any modifications and applications are possible without departing from the spirit and scope of the present invention. For example, in the above embodiment, the deactivation step S2, the submersion step S3, and the separation step S4 are performed without removing the laminate material 22, but any of the deactivation step S2, the submersion step S3, and the separation step S4 may be performed by removing the laminate material 22.

[0030] In the above embodiment, the electrode plates 11 and 12 are electrically connected to each other by passing the conductive member 51 through the laminated electrode 21, but any method for electrically connecting the electrode plates 11 and 12 to each other may be used. For example, the electrode plates 11 and 12 may be electrically connected to each other by a non-penetrating conductive member.

[0031] In the above embodiment, the battery treatment method of the present invention is applied to a laminated lithium ion battery and a laminated all-solid-state battery, but is not limited thereto. In other words, the battery treatment method of the present invention may be applied to lithium ion batteries and all-solid-state batteries other than the laminated type.

[0032] [Configuration supported by the above embodiment] The above embodiment supports the following configurations.

[0033] (Configuration 1) A method for treating a battery, which is either a lithium ion battery or an all-solid-state battery and has a stacked electrode in which a positive electrode plate and a negative electrode plate are stacked with a separator interposed therebetween, the method comprising: a submersion step of submerging the stacked electrode in water after deactivating lithium; and a separation step of applying an electric pulse to the stacked electrode to separate the stacked electrode. According to this method, the laminated electrodes can be separated easily and in a short time.

[0034] (Configuration 2) The method for treating a battery according to Configuration 1, wherein the separation step comprises applying an electric pulse to the laminated electrode after the plates of the laminated electrode are brought into an electrically conductive state. According to this method, an electric pulse can be applied to all of the electrodes, which facilitates proper separation of the stacked electrodes.

[0035] (Configuration 3) The method for treating a battery according to Configuration 2, further comprising the step of passing a predetermined conductive member through the laminated electrode to bring the plates of the laminated electrode into electrical continuity. According to this method, the electrodes can be easily and quickly brought into electrical contact with each other, and it is also possible to bring the electrodes into electrical contact with each other without removing the outer casing of the laminated electrode.

[0036] (Configuration 4) The battery has a positive electrode side current collecting tab to which the positive electrode plate is connected, and a negative electrode side current collecting tab to which the negative electrode plate is connected, and the negative electrode side current collecting tab is disposed on the opposite side of the stacked electrode to the positive electrode side current collecting tab, and a method for treating a battery according to configuration 3, comprising the steps of: penetrating the conductive member into a region of the stacked electrode closer to the negative electrode side current collecting tab; and applying an electric pulse to the stacked electrode via the positive electrode side and negative electrode side current collecting tabs. According to this method, it is possible to pass more current through the positive electrode current collector than through the negative electrode current collector, and to increase the separation efficiency of the positive electrode current collector even when the negative electrode current collector has higher electrical conductivity than the positive electrode current collector.

[0037] (Configuration 5) A method for treating a battery according to any one of configurations 1 to 4, wherein the battery is a laminate type in which the laminated electrodes are covered with a laminate material and a pair of current collecting tabs are exposed to the outside of the laminate material, and the pair of current collecting tabs are used to apply the electric pulse to the laminated electrodes. According to this method, an electrical connection can be easily made between the device for applying an electric pulse and the laminated electrode, and the electric pulse can be applied to the laminated electrode without removing the laminate material.

[0038] (Configuration 6) The method for treating a battery according to any one of Configurations 1 to 4, wherein, when the battery contains an electrolyte, the electrolyte is removed, and then the submersion step is carried out after deactivating lithium and removing the electrolyte. This method can sufficiently suppress the reaction between lithium and water, and when the target battery is a laminate type, the laminate material is cut open to drain the electrolyte, and then the laminate type battery is submerged in the treatment solution, which allows the treatment solution to penetrate into the laminate through the cut, deactivating the lithium and removing the electrolyte, making the process easy. [Explanation of symbols]

[0039] 10...target battery, 11...positive electrode plate, 12...negative electrode plate, 13...separator, 21...laminated electrode, 22...laminate material, 22A, 22B...current collecting tabs, 31...positive electrode collector, 32...positive electrode composite material, 41...negative electrode collector, 42...negative electrode composite material, 51...conductive member, 55...electric pulse application device

Claims

1. A method for treating a battery, which is either a lithium ion battery or an all-solid-state battery, having a stacked electrode in which a positive electrode plate and a negative electrode plate are stacked with a separator interposed therebetween, comprising: a submersion step of submerging the laminated electrode in water after deactivating lithium; a separation step of applying an electric pulse to the laminated electrodes to separate the laminated electrodes; A method for treating a battery having the above structure.

2. The separation step includes applying an electric pulse to the laminated electrode after the plates of the laminated electrode are electrically connected to each other. A method for treating the battery according to claim 1.

3. The separation step includes passing a predetermined conductive member through the laminated electrode to electrically connect the plates of the laminated electrode to each other. A method for treating a battery according to claim 2.

4. the battery has a positive electrode side current collecting tab to which the positive electrode plate is connected and a negative electrode side current collecting tab to which the negative electrode plate is connected, the negative electrode side current collecting tab being disposed on the opposite side of the positive electrode side current collecting tab across the laminated electrode, the conductive member is inserted through a region of the stacked electrode that is closer to the negative electrode side current collecting tab, and an electric pulse is applied to the stacked electrode via the positive electrode side and negative electrode side current collecting tabs; A method for treating a battery according to claim 3.

5. the battery is a laminate type in which the stacked electrode is covered with a laminate material and a pair of current collecting tabs are exposed to the outside of the laminate material; applying the electric pulse to the stacked electrodes using the pair of current collecting tabs; A method for treating a battery according to any one of claims 1 to 4.

6. When the battery has an electrolyte, After removing the electrolyte, deactivating the lithium, and removing the electrolyte, the water immersion step is performed. A method for treating a battery according to any one of claims 1 to 4.

Citation Information

Patent Citations

  • How to disassemble a lithium-ion battery cell

    JP7120158B2

Cited By

  • Treatment method of waste solid-state battery

    CN122739581A