Battery electrode manufacturing apparatus and battery electrode manufacturing method

The battery electrode manufacturing apparatus and method enhance dimensional accuracy by using a shaping section to adjust the electrode composition on the base film, addressing supply challenges and ensuring consistent battery quality.

JP2024143729AInactive Publication Date: 2024-10-11APB CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023056544
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods face challenges in supplying electrode composition to a base film during battery electrode manufacturing, leading to difficulties in achieving desired dimensional accuracy.

Method used

A battery electrode manufacturing apparatus and method that includes an electrode composition supply section and a shaping section to accurately shape and supply the electrode composition to a base film, using devices like members or blades to adjust the dimensions of the electrode composition.

Benefits of technology

Improves the dimensional accuracy of the electrode composition supplied to the base film, preventing issues such as gaps or stress concentration that can affect the quality of the manufactured lithium ion batteries.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143729000001_ABST
    Figure 2024143729000001_ABST
Patent Text Reader

Abstract

To improve the dimensional accuracy of an electrode composition applied to a substrate film.SOLUTION: A battery electrode manufacturing apparatus (battery electrode manufacturing apparatus 1000) includes an electrode composition supply portion (electrode composition supply device 300) that supplies an electrode composition including an active material (electrode composition 22C) in a rectangular shape to a transported substrate film (current collector 21B), and a shaping portion (shaping device 500) that shapes at least one side of the electrode composition on the substrate film.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an apparatus and a method for manufacturing a battery electrode. [Background technology]

[0002] Lithium ion batteries are high-capacity secondary batteries that have been used in various applications in recent years. The electrodes of lithium ion batteries are composed of an active material layer, a current collector layer, a separator, and a frame that encapsulates the active material layer (see, for example, Patent Document 1). The active material layer in a lithium ion battery can be formed, for example, as described in Patent Document 2, by intermittently supplying an electrode composition to a strip-shaped substrate film and compressing it. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 6633866 [Patent Document 2] Patent Publication No. 2021-27043 Summary of the Invention [Problem to be solved by the invention]

[0004] From the viewpoint of production efficiency, it is preferable to supply the electrode composition to the transported base film while transporting the strip-shaped base film, as described in Patent Document 2. However, it is not easy to supply the electrode composition to the transported base film and still achieve the desired dimensional accuracy.

[0005] The present invention has been made in consideration of the above circumstances, and aims to provide a battery electrode manufacturing apparatus and a battery electrode manufacturing method that can improve the dimensional accuracy of the electrode composition supplied to the base film. [Means for solving the problem]

[0006] In order to achieve the above-mentioned object, the battery electrode manufacturing apparatus of the present invention includes an electrode composition supply section that supplies an electrode composition containing an active material in a rectangular shape to a transported base film, and a shaping section that shapes at least one side of the electrode composition on the base film. Effect of the Invention

[0007] According to the battery electrode manufacturing apparatus and battery electrode manufacturing method of the present invention, it is possible to improve the dimensional accuracy of the electrode composition supplied to the substrate film. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a schematic cross-sectional view of a single cell of a battery manufactured using the battery electrode manufacturing apparatus of the first embodiment. [Diagram 2] FIG. 2 is a schematic diagram of the battery electrode manufacturing apparatus of the first embodiment. [Diagram 3] FIG. 3 is a diagram showing an electrode composition supplied to the current collector of the first embodiment. [Figure 4A] FIG. 4A is a diagram for explaining the shaping device of the first embodiment. FIG. [Figure 4B] FIG. 4B is a diagram for explaining the shaping device of the first embodiment. [Figure 4C] FIG. 4C is a diagram for explaining the shaping device of the first embodiment. [Figure 5A] FIG. 5A is a diagram for explaining a shaping device according to a second embodiment. [Figure 5B] FIG. 5B is a diagram for explaining the shaping device of the second embodiment. [Figure 5C] FIG. 5C is a diagram for explaining the shaping device of the second embodiment. [Figure 6] FIG. 6 is a schematic diagram of a battery electrode manufacturing apparatus according to the third embodiment. [Figure 7A] FIG. 7A is a diagram for explaining a shaping device according to a third embodiment. [Figure 7B]FIG. 7B is a diagram for explaining the shaping device of the third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] (First embodiment) Hereinafter, the first embodiment will be described with reference to the drawings. Note that the drawings used in the following description may show characteristic parts in an enlarged scale for the purpose of emphasizing the characteristic parts, and the dimensional ratios of each component may not be the same as the actual ones. Also, for the same purpose, some parts may be omitted in the drawings.

[0010] <Battery pack (secondary battery)> The battery electrode manufacturing apparatus and battery electrode manufacturing method of the first embodiment are applied to, for example, the manufacture of lithium ion batteries. Lithium ion batteries are used in the form of a modularized battery assembly formed by combining a plurality of lithium ion single batteries (also referred to as single cells or battery cells), or in the form of a battery pack in which a plurality of such battery assemblies are combined to adjust the voltage and capacity. An example of a lithium ion secondary battery is shown below, but the type of secondary battery according to the present invention is not limited to a lithium ion secondary battery and includes other secondary batteries.

[0011] <Single cell (battery cell)> 1 is a schematic cross-sectional view of a unit cell 10. The above-mentioned battery pack can be produced by combining a plurality of unit cells 10. For example, the unit cell 10 has a positive electrode 20a and a negative electrode 20b as two electrodes 20 (battery electrodes), and a separator 30.

[0012] The separator 30 is disposed between the positive electrode 20a and the negative electrode 20b. In the assembled battery, the multiple single cells 10 are stacked with the positive electrodes 20a and the negative electrodes 20b facing in the same direction.

[0013] The separator 30 holds an electrolyte. Thus, the separator 30 functions as an electrolyte layer. The separator 30 is disposed between the electrode active material layers 22 of the positive electrode 20a and the negative electrode 20b, and prevents them from contacting each other. Thus, the separator 30 functions as a partition wall between the positive electrode 20a and the negative electrode 20b.

[0014] Examples of the electrolyte held in the separator 30 include an electrolytic solution or a gel polymer electrolyte. By using these electrolytes, high lithium ion conductivity is ensured. Examples of the form of the separator include a porous sheet separator made of a polymer or fiber that absorbs and holds the electrolyte, a nonwoven fabric separator, and the like.

[0015] The positive electrode 20a and the negative electrode 20b each have a current collector 21, an electrode active material layer 22, and a frame 35. The electrode active material layer 22 and the current collector 21 are arranged in this order from the separator 30 side. The frame 35 is frame-shaped (annular). The frame 35 surrounds the periphery of the electrode active material layer 22. The frame 35 of the positive electrode 20a and the frame 35 of the negative electrode 20b are welded to each other and integrated. In the following description, when the electrode active material layers 22 of the positive electrode 20a and the negative electrode 20b are to be distinguished from each other, they are called the positive electrode active material layer 22a and the negative electrode active material layer 22b, respectively.

[0016] <Specific examples of positive electrode current collectors> As the positive electrode current collector constituting the positive electrode current collector layer 21a, a current collector used in a known lithium ion cell can be used, for example, a known metal current collector and a resin current collector composed of a conductive material and a resin (such as the resin current collectors described in JP 2012-150905 A and WO 2015 / 005116 A, etc.) can be used. From the viewpoint of battery characteristics, etc., the positive electrode current collector constituting the positive electrode current collector layer 21a is preferably a resin current collector.

[0017] Examples of the metal current collector include one or more metal materials selected from the group consisting of copper, aluminum, titanium, nickel, tantalum, niobium, hafnium, zirconium, zinc, tungsten, bismuth, antimony, alloys containing one or more of these metals, and stainless steel alloys. These metal materials may be used in the form of a thin plate or metal foil. In addition, the above metal materials may be formed on the surface of a substrate made of a material other than the above metal materials by a method such as sputtering, electrodeposition, or coating, and used as the metal current collector.

[0018] The resin collector preferably contains a conductive filler and a matrix resin. Examples of the matrix resin include, but are not limited to, polyethylene (PE), polypropylene (PP), polymethylpentene (PMP), etc. The conductive filler is not particularly limited as long as it is selected from materials having electrical conductivity. The conductive filler may be a conductive fiber having a fibrous shape.

[0019] The resin current collector may contain other components (such as a dispersant, a crosslinking accelerator, a crosslinking agent, a colorant, an ultraviolet absorber, and a plasticizer) in addition to the matrix resin and the conductive filler. A plurality of resin current collectors may be laminated, or a resin current collector and a metal foil may be laminated.

[0020] The thickness of the positive electrode collector layer 21a is not particularly limited, but is preferably 5 to 150 μm. When a plurality of resin collectors are laminated to be used as the positive electrode collector layer 21a, the total thickness after lamination is preferably 5 to 150 μm. The positive electrode collector layer 21a can be obtained, for example, by melt-kneading a matrix resin, a conductive filler, and an optional filler dispersant to obtain a conductive resin composition, and molding the conductive resin composition into a film by a known method.

[0021] <Specific examples of positive electrode active materials> The positive electrode active material layer 22a is preferably a non-binding mixture containing a positive electrode active material. Here, the non-binding means that the position of the positive electrode active material in the positive electrode active material layer is not fixed, and the positive electrode active materials are not irreversibly fixed to each other and to the current collector. When the positive electrode active material layer 22a is a non-binding material, the positive electrode active materials are not irreversibly fixed to each other, so that the interface between the positive electrode active materials can be separated without mechanically destroying it, and even if stress is applied to the positive electrode active material layer 22a, the positive electrode active material moves, so that destruction of the positive electrode active material layer 22a can be prevented, which is preferable. The positive electrode active material layer 22a that is a non-binding material can be obtained by, for example, making the positive electrode active material layer 22a into a positive electrode active material layer 22a that contains a positive electrode active material and an electrolyte but does not contain a binder. In this specification, the binder means a chemical agent that cannot reversibly fix the positive electrode active materials to each other or to the positive electrode active material and the current collector, and examples of such binders include known solvent-dried binders for lithium ion batteries such as starch, polyvinylidene fluoride, polyvinyl alcohol, carboxymethyl cellulose, polyvinylpyrrolidone, tetrafluoroethylene, styrene-butadiene rubber, polyethylene, and polypropylene. These binders are used by dissolving or dispersing them in a solvent, and by volatilizing or distilling off the solvent, the surface becomes solidified without showing any adhesiveness, and therefore cannot reversibly fix the positive electrode active materials to each other or to the positive electrode active material and the current collector.

[0022] Examples of the positive electrode active material include, but are not limited to, composite oxides of lithium and transition metals, composite oxides containing two types of transition metal elements, and composite oxides containing three or more types of metal elements.

[0023] The positive electrode active material may be a coated positive electrode active material having at least a part of its surface coated with a coating material containing a polymer compound. When the positive electrode active material is coated with the coating material, the volume change of the positive electrode is mitigated, and the expansion of the positive electrode can be suppressed.

[0024] As the polymer compound constituting the coating material, those described as active material coating resins in JP 2017-054703 A, WO 2015 / 005117 A, and the like can be suitably used.

[0025] The coating material may contain a conductive agent, which may be the same as the conductive filler contained in the positive electrode current collector layer 21a.

[0026] The positive electrode active material layer 22a may contain an adhesive resin. For example, the adhesive resin may be a resin for coating a non-aqueous secondary battery active material described in JP 2017-054703 A in which a small amount of organic solvent is mixed to adjust the glass transition temperature to room temperature or lower, and a resin described as an adhesive in JP 10-255805 A. The adhesive resin means a resin that does not solidify even when the solvent component is evaporated and dried, and has adhesiveness (the property of adhering by applying a slight pressure without using water, solvent, heat, etc.). On the other hand, the solution-drying type electrode binder used as a binder means a material that dries and solidifies by evaporating the solvent component, thereby firmly adhering and fixing the active materials to each other. Therefore, the above-mentioned binder (solution-drying type electrode binder) and the adhesive resin are different materials.

[0027] The positive electrode active material layer 22a may contain an electrolytic solution containing an electrolyte and a non-aqueous solvent. As the electrolyte, a substance used in a known electrolytic solution can be used. As the non-aqueous solvent, a substance used in a known electrolytic solution (e.g., phosphoric acid ester, nitrile compound, and mixtures thereof) can be used. For example, a mixture of ethylene carbonate (EC) and dimethyl carbonate (DMC), or a mixture of ethylene carbonate (EC) and propylene carbonate (PC) can be used.

[0028] The positive electrode active material layer 22a may contain a conductive assistant, which may be a conductive material similar to the conductive filler contained in the positive electrode current collector layer 21a.

[0029] The thickness of the positive electrode active material layer 22a is not particularly limited, but from the viewpoint of battery performance, it is preferably 300 to 750 μm, and more preferably 350 to 600 μm.

[0030] In the first embodiment, the positive electrode composition supplied to form the positive electrode active material layer 22a may be a wet powder containing a positive electrode active material and a nonaqueous electrolyte solution. The wet powder is more preferably in a pendular or funicular state.

[0031] The proportion of the nonaqueous electrolyte in the wet powder is not particularly limited, but in order to achieve a pendular or funicular state, in the case of a positive electrode, the proportion of the nonaqueous electrolyte is desirably 0.5 to 15% by weight of the entire wet powder.

[0032] <Specific examples of negative electrode current collectors> The negative electrode current collector constituting the negative electrode current collector layer 21b may be appropriately selected from the same configuration as that described for the positive electrode current collector, and may be obtained by the same method. From the viewpoint of battery characteristics, the negative electrode current collector layer 21b is preferably a resin current collector. The thickness of the negative electrode current collector layer 21b is not particularly limited, but is preferably 5 to 150 μm.

[0033] <Specific examples of negative electrode active materials> The negative electrode active material layer 22b is preferably a non-binding material of a mixture containing a negative electrode active material. The reason why the negative electrode active material layer is preferably a non-binding material and the method for obtaining the non-binding negative electrode active material layer 22b are the same as the reason why the positive electrode active material layer 22a is preferably a non-binding material and the method for obtaining the non-binding positive electrode active material layer 22a.

[0034] As the negative electrode active material, for example, a carbon-based material, a silicon-based material, or a mixture thereof can be used, but is not particularly limited.

[0035] The negative electrode active material may be a coated negative electrode active material having at least a part of its surface coated with a coating material containing a polymer compound. When the negative electrode active material is coated with the coating material, the volume change of the negative electrode is mitigated, and the expansion of the negative electrode can be suppressed.

[0036] As the coating material, the same coating material as that constituting the coated positive electrode active material can be suitably used.

[0037] The negative electrode active material layer 22b contains an electrolytic solution containing an electrolyte and a non-aqueous solvent. The composition of the electrolytic solution may be the same as that of the electrolytic solution contained in the positive electrode active material layer 22a.

[0038] The negative electrode active material layer 22b may contain a conductive additive, which may be a conductive material similar to the conductive filler contained in the positive electrode active material layer 22a.

[0039] The negative electrode active material layer 22b may contain an adhesive resin, which may be the same as the adhesive resin that is an optional component of the positive electrode active material layer 22a.

[0040] The thickness of the negative electrode active material layer 22b is not particularly limited, but from the viewpoint of battery performance, it is preferably 450 to 900 μm, and more preferably 500 to 750 μm.

[0041] In the first embodiment, the negative electrode composition supplied to form the negative electrode active material layer 22b may be a wet powder containing a negative electrode active material and a nonaqueous electrolyte solution. The wet powder is more preferably in a pendular or funicular state.

[0042] The proportion of the nonaqueous electrolyte in the wet powder is not particularly limited, but in order to achieve a pendular or funicular state, in the case of a negative electrode, it is desirable that the proportion of the nonaqueous electrolyte be 0.5 to 25% by weight of the entire wet powder.

[0043] <Specific examples of separators> Examples of the electrolyte held in the separator 30 include an electrolytic solution and a gel polymer electrolyte. By using these electrolytes, high lithium ion conductivity is ensured in the separator 30. Examples of the form of the separator 30 include, but are not limited to, a porous film made of polyethylene or polypropylene.

[0044] <Examples of frame bodies> The frame 35 is not particularly limited as long as it is a material that is durable against the electrolyte, but for example, a polymer material is preferable, and a thermosetting polymer material is more preferable. The material constituting the frame 35 may be any material that has insulation properties, sealing properties (liquid-tightness), heat resistance under the battery operating temperature, etc., and a resin material is preferably used. More specifically, the frame 35 may be, for example, an epoxy resin, a polyolefin resin, a polyurethane resin, or a polyvinylidene fluoride resin, and the like, and an epoxy resin is preferable because it is highly durable and easy to handle.

[0045] <Battery electrode manufacturing device and battery electrode manufacturing method> Next, a battery electrode manufacturing apparatus and a battery electrode manufacturing method (hereinafter, abbreviated as manufacturing method) of the first embodiment will be described. For example, in the battery electrode manufacturing apparatus and the battery electrode manufacturing method, the positive electrode 20a and the negative electrode 20b are first manufactured. The manufacturing method of the positive electrode 20a and the manufacturing method of the negative electrode 20b mainly differ in the electrode active material contained in the electrode active material layer 22. Here, as the manufacturing method of the electrode 20, the manufacturing methods of the positive electrode 20a and the negative electrode 20b will be collectively described.

[0046] FIG. 2 is a schematic diagram of a battery electrode manufacturing apparatus 1000. For example, the battery electrode manufacturing apparatus 1000 includes a chamber 100, a conveying device 200, an electrode composition supplying device 300, a pressing device 400, a shaping device 500, and a frame body supplying device 600. The electrode composition supplying device 300 is an example of an electrode composition supplying section, and executes a supplying step. The pressing device 400 is an example of a compression section. The shaping device 500 is an example of a shaping section, and executes a shaping step. The frame body supplying device 600 is an example of a frame body supplying section. In the following, a case where the strip-shaped base film is a strip-shaped current collector 21B will be described as an example.

[0047] The chamber 100 is a room whose interior can be kept at a reduced pressure lower than atmospheric pressure. The interior of the chamber 100 is reduced to a pressure lower than atmospheric pressure by a decompression pump (not shown). The standard atmospheric pressure is about 1013 hPa (about 101 kPa).

[0048] For example, the current collector roll 21R is disposed outside the chamber 100, and the strip-shaped current collector 21B drawn from the current collector roll 21R is transported into the chamber 100 through a slit. Hereinafter, the strip-shaped current collector 21B may be referred to as the current collector 21B. The current collector 21B is the current collector 21 before it is cut into a predetermined shape. The current collector 21B is transported at a predetermined speed along the transport direction Da. In the following description, the direction in which the current collector 21B is transported is referred to as the downstream side Da1, and the opposite direction is referred to as the upstream side Da2. The external space of the chamber 100 in which the current collector roll 21R is disposed may be at normal pressure, or may be reduced in pressure by a chamber different from the chamber 100.

[0049] 2, the upper side in the vertical direction Db is designated as Db1, and the lower side in the vertical direction Db is designated as Db2. The direction perpendicular to the transport direction Da and the vertical direction Db corresponds to the width direction of the current collector 21B and the electrode composition 22C placed on the current collector 21B.

[0050] The conveying device 200 conveys the current collector 21B to the downstream side Da1 in the conveying direction Da. For example, the conveying device 200 is a belt conveyor that supports the current collector 21B from below. After the electrode composition supplying device 300 described below supplies the electrode composition 22C, the conveying device 200 conveys the current collector 21B carrying the electrode composition 22C.

[0051] 2, the electrode composition supplying device 300 supplies the electrode composition 22C to the current collector 21B transported in the chamber 100. The electrode composition 22C is a material containing at least an active material (positive electrode active material or negative electrode active material). The electrode composition 22C is compressed by a pressing device 400 (described later) or the like to form the electrode active material layer 22 (positive electrode active material layer 22a, negative electrode active material layer 22b).

[0052] The electrode composition supplying device 300 of the first embodiment supplies the electrode composition 22C in a rectangular shape to the current collector 21B. Specifically, the electrode composition supplying device 300 supplies the electrode composition 22C so that the electrode composition 22C has a rectangular shape when viewed from the vertical direction Db. The supplied electrode composition 22C has a shape having four sides parallel to the conveyance direction Da or the width direction.

[0053] For example, the electrode composition supplying device 300 includes a hopper that holds the electrode composition 22C therein and a shutter that opens and closes the opening of the hopper. In this case, the electrode composition 22C is supplied while the opening of the hopper is open, and the supply of the electrode composition 22C is stopped while the opening of the hopper is closed. In this way, by opening and closing the opening of the hopper with the shutter, the electrode composition 22C can be supplied in a rectangular shape to the current collector 21B.

[0054] As another example, the electrode composition supplying device 300 includes a hopper that holds the electrode composition 22C therein and has a part or all of an inner wall formed of a moving belt. In this case, by controlling the rotation of the moving belt, the supply and stop of the electrode composition 22C to the current collector 21B can be controlled, and the electrode composition 22C can be supplied in a rectangular shape. A shutter that opens and closes the opening of the hopper may be further provided, and the opening and closing of the opening by the shutter may be linked to the operation of the moving belt, thereby supplying the electrode composition 22C in a rectangular shape.

[0055] The press device 400 compresses the electrode composition 22C supplied to the current collector 21B. For example, the press device 400 has an upper roller 401 and a lower roller 402 as shown in Fig. 2. The press device 400 sandwiches and compresses the electrode composition 22C supplied to the current collector 21B between the upper roller 401 and the lower roller 402. That is, the press device 400 performs roll pressing on the electrode composition 22C.

[0056] Here, in FIG. 2, the cross-sectional shape of the electrode composition 22C supplied onto the current collector 21B parallel to the transport direction Da and the vertical direction Db is shown as a rectangle, but the cross-sectional shape of the powder electrode composition 22C when deposited on the current collector 21B may be a trapezoid, as shown in FIG. 3.

[0057] In addition, the electrode composition supplying device 300 supplies the electrode composition 22C to a rectangular prescribed range having a predetermined dimension, but due to various factors, the actual supply position may deviate from the prescribed range. For example, when the electrode composition 22C is supplied, a part of the electrode composition 22C supplied to the prescribed range may crumble and scatter backward (upstream side Da2 in the conveying direction Da).

[0058] The predetermined dimensions in the above-mentioned specified ranges are set values ​​according to, for example, the dimensions of the electrode active material layer 22 of the unit cell 10 shown in Fig. 1. For example, a lithium ion battery is designed according to the application and required performance, the dimensions of the electrode active material layer 22 of the unit cell 10 are determined, and the predetermined dimensions in the above-mentioned specified ranges are set according to the determined dimensions. The predetermined dimensions in the above-mentioned specified ranges may be the determined dimensions of the electrode active material layer 22 themselves, or may be values ​​calculated in consideration of tolerances and the like.

[0059] It is preferable that the electrode composition 22C is supplied to the current collector 21B accurately according to a predetermined dimension, but as described above, there are cases where the electrode composition 22C scatters outside the specified range, and the tolerance cannot be satisfied. In addition, when compressed by the press device 400, the electrode composition 22C on the current collector 21B may stretch in the conveying direction Da and the width direction, making it impossible to satisfy the tolerance. If the tolerance cannot be satisfied, problems may occur in the subsequent process, which may affect the quality of the manufactured lithium-ion battery. For example, if the dimensions of the electrode composition 22C become larger than the tolerance due to scattering of the electrode composition 22C during supply, when the frame 35 described later is supplied, the electrode composition 22C may be sandwiched between the frame 35 and the current collector 21B, which may cause welding failure. Furthermore, if the dimensions of the electrode composition 22C become smaller than the tolerance, after the frame body 35 described below is supplied, a gap where the electrode composition 22C is not present will be formed in the space surrounded by the frame body 35 and the current collector 21B, which may cause problems such as stress concentration on the current collector 21B and breakage.

[0060] Therefore, the battery electrode manufacturing apparatus 1000 of the first embodiment improves dimensional accuracy by shaping at least one side of the electrode composition 22C supplied in a rectangular shape using a shaping device 500 described below.

[0061] For example, the shaping device 500 includes a member 511 and a member 512 shown in FIG. 4A. The members 511 and 512 are, for example, flat plates parallel to the vertical direction Db and the width direction. The material of the members 511 and 512 is not particularly limited, but as an example, they can be made of resin or metal. A release agent may be applied to the surfaces of the members 511 and 512 that come into contact with the electrode composition 22C.

[0062] As shown in Fig. 4B, the members 511 and 512 slide on the current collector 21B in a direction approaching the rectangularly supplied electrode composition 22C, thereby compressing and shaping the two sides corresponding to the downstream side Da1 and the upstream side Da2 in the conveyance direction Da. In Fig. 4A, the portion P1 of the electrode composition 22C supplied in a rectangular shape to the current collector 21B is described as corresponding to the specified range. That is, the portions P2 and P3 shown in Fig. 4A, the electrode composition 22C scattered during supply, etc. correspond to the difference from the specified dimension.

[0063] Specifically, the member 511 is disposed at a position on the upstream side Da2 from the electrode composition 22C supplied in a rectangular shape, and then slides on the current collector 21B toward the downstream side Da1. At this time, the scattered electrode composition 22C is carried to the downstream side Da1 by the member 511 and compressed to be integrated with the electrode composition 22C in a specified range. Similarly, the member 512 is disposed at a position on the downstream side Da1 from the electrode composition 22C supplied in a rectangular shape, and then slides on the current collector 21B toward the upstream side Da2. At this time, the scattered electrode composition 22C is carried to the upstream side Da2 by the member 512 and compressed to be integrated with the electrode composition 22C in a specified range.

[0064] In addition, in FIG. 4A, the cross-sectional shape of the electrode composition 22C is a trapezoid, and the portion corresponding to the difference between the upper base and the lower base (portion P2 and portion P3 in FIG. 4A) is also compressed by the member 511 and the member 512. The portion P2 and the portion P3 are less likely to be subjected to pressure in the compression process by the press device 400 compared to the portion P1, and are often in a soft state. The member 511 and the member 512 can compress the scattered electrode composition 22C and the portion P2 and portion P3 in a soft state, and can shape two sides of the electrode composition 22C supplied in a rectangular shape corresponding to the downstream side Da1 and the upstream side Da2. For example, the dimensions of the electrode composition 22C after the member 511 and the member 512 are withdrawn are in a state that is approximately equal to the portion P1 corresponding to the specified range, as shown in FIG. 4C. That is, by performing the shaping shown in FIG. 4A to FIG. 4C, the dimensional accuracy can be improved.

[0065] 4A to 4C, there is no particular limitation on the mechanism for operating the members 511 and 512. For example, by holding the member 511 from the upstream side Da2 with a piston, it is possible to realize movement in the conveying direction Da as shown by the arrow in Fig. 4B. Furthermore, by holding the piston with a rail parallel to the vertical direction Db, it is possible to realize movement of the member 511 in the vertical direction Db, and to retract the member 511 from the state shown in Fig. 4B.

[0066] 4B, members 511 and 512 may be reciprocated in the transport direction Da and then retreated. Specifically, it is assumed that when members 511 and 512 are retreated, a part of electrode composition 22C may crumble and scatter. By reciprocating members 511 and 512 in the transport direction Da, the part that has crumbled and scatters can be compressed again, and the dimensional accuracy of electrode composition 22C can be further improved.

[0067] In addition, in Figures 4A to 4C, it has been described that the electrode composition 22C supplied in a rectangular shape has two sides corresponding to the downstream side Da1 and the upstream side Da2 in the conveying direction Da shaped, but the embodiment is not limited to this.

[0068] 4A to 4C, the member 512 may be omitted, and only one side corresponding to the downstream side Da1 may be shaped. It is relatively difficult to control the dimensions of the downstream side Da1, for example, in cases where the electrode composition 22C supplied in a rectangular shape crumbles and scatters backwards, and by configuring so that only one side corresponding to the downstream side Da1 is shaped, it is possible to reduce manufacturing costs while improving dimensional accuracy.

[0069] Moreover, the four sides of the electrode composition 22C supplied in a rectangular shape may be shaped by further providing members similar to the members 511 and 512 on two sides corresponding to the width direction. In addition to the above-mentioned example, any one, two, or three sides of the electrode composition 22C supplied in a rectangular shape may be shaped. That is, the shaping device 500 shapes at least one side of the electrode composition 22C supplied in a rectangular shape.

[0070] The shaping process by the shaping device 500 may be performed consecutively with a compression process by the press device 400 as shown in FIG. 2, or may be performed after the sheet is divided into sheets.

[0071] When the shaping step is performed consecutively with the compression step, the shaping device 500 performs shaping on the electrode composition 22C being transported toward the downstream side Da1. For example, the shaping device 500 performs shaping while moving in synchronization with the transported electrode composition 22C. For example, the shaping device 500 performs the shaping steps of Figs. 4A to 4C while moving toward the downstream side Da1 along a rail parallel to the transport direction Da.

[0072] In the case where the shaping step is performed after the sheets are separated, the battery electrode manufacturing apparatus 1000 includes a cutting device (not shown) that cuts out the strip-shaped current collector 21B at a certain unit. Specifically, the cutting device cuts out the position where the electrode composition 22C is placed and the surrounding area of ​​the strip-shaped current collector 21B. Hereinafter, the current collector cut out from the strip-shaped current collector 21B by the cutting device is also referred to as the current collector 21B'. The shaping device 500 performs the shaping step of FIG. 4A to FIG. 4C on the electrode composition 22C placed on the cut current collector 21B'. The dimensions of the current collector 21B' may be the same as those of the current collector 21 in the single cell 10 shown in FIG. 1, or may be larger than those of the current collector 21. If the dimensions of the current collector 21B' are larger than those of the current collector 21, the dimensions of the current collector 21B' are adjusted at a later stage.

[0073] Returning to FIG. 2, the description will be continued. The frame body supplying device 600 supplies the frame body 35 to the current collector 21B being transported. For example, the frame body supplying device 600 has a robot arm and places the frame body 35, which has been manufactured in advance, at a predetermined position on the current collector 21B. Alternatively, the frame body supplying device 600 may manufacture the frame body 35 on the current collector 21B. As an example, the current collector 21B is used as a base material, and a predetermined material is discharged or applied in a predetermined shape on the current collector 21B by a dispenser, a coater, or the like, to form the frame body 35 on the current collector 21B. Note that, as in the shaping process by the shaping device 500, the supply of the frame body 35 by the frame body supplying device 600 may be performed continuously with the compression process by the press device 400, or may be performed after being divided into sheets.

[0074] 1 is further supplied after the compression process by the press device 400, to produce the unit cell 10. Similarly, the supply of the separator 30 may be performed continuously after the compression process by the press device 400, or may be performed after being separated into sheets.

[0075] Specifically, the positive electrode 20a and the negative electrode 20b are each produced by a battery electrode production apparatus 1000 shown in Fig. 2. Then, a separator 30 is supplied to either the positive electrode 20a or the negative electrode 20b, and then the positive electrode 20a and the negative electrode 20b are bonded together with the separator 30 interposed therebetween to produce a single cell 10. For example, the positive electrode 20a and the negative electrode 20b are bonded together and heat sealed to produce the single cell 10.

[0076] In addition, the specific flow up to the manufacturing of the lithium ion battery can be modified in various ways.

[0077] For example, before bonding the positive electrode 20a and the negative electrode 20b together, an electrolyte solution may be injected into the electrode active material layer 22. Even when the electrode composition 22C supplied by the electrode composition supplying device 300 is a wet powder containing an electrolyte solution and an active material, the electrolyte solution contained in the electrode composition 22C may be a part of the required amount, and a step of injecting the remaining electrolyte solution may be provided later.

[0078] Also, for example, the pressing by the above-described pressing device 400 may be the primary pressing, and a secondary pressing may be further performed later. The secondary pressing may be performed, for example, after the positive electrode 20a and the negative electrode 20b are bonded together.

[0079] When the secondary press is performed, the compression ratio can be set low in the primary press, so that deformation during pressing can be suppressed, improving dimensional accuracy and improving liquid injection. In addition, since the secondary press is performed with the frame 35 provided, deformation during pressing can be suppressed. In order to prevent damage to the separator 30 due to the secondary press, the strength of the separator 30 may be increased or the separator 30 may be doubled.

[0080] As described above, in the first embodiment, each step, such as supplying the electrode composition 22C by the electrode composition supplying device 300 and compressing the electrode composition 22C by the pressing device 400, is performed in the chamber 100, the inside of which is reduced in pressure below atmospheric pressure. This makes it possible to prevent air from remaining inside the electrode composition 22C, and improves the uniformity of the electrode active material layer 22.

[0081] Second embodiment In the above-mentioned first embodiment, an example was described in which at least one side of the electrode composition 22C supplied in a rectangular shape is compressed and shaped by sliding the member 511 or the like on the current collector 21B in a direction approaching the electrode composition 22C supplied in a rectangular shape. In the second embodiment, an example is described in which excess electrode composition is removed from at least one side of the electrode composition 22C supplied in a rectangular shape to shape it. Note that the same reference numerals are used for the points described in the first embodiment, and the description will be omitted. Hereinafter, the second embodiment will be described with reference to FIG. 5A, FIG. 5B, and FIG. 5C.

[0082] For example, the shaping device 500 of the second embodiment includes blade-like members 521 and 522 shown in FIG. 5A. The members 521 and 522 are, for example, flat plates parallel to the vertical direction Db and the width direction. The material of the members 521 and 522 is not particularly limited, but as an example, they can be made of resin or metal. A release agent may be applied to both sides of the members 521 and 522.

[0083] The members 521 and 522 are first placed at a position on the upper side Db1 of the electrode composition 22C supplied in a rectangular shape, as shown in Fig. 5A. Next, the members 521 and 522 move toward the lower side Db2 as shown in Fig. 5B, and are inserted into the electrode composition 22C supplied in a rectangular shape. Specifically, the members 521 and 522 are inserted into the end positions of a specified range of the electrode composition 22C supplied in a rectangular shape.

[0084] Next, as shown in Fig. 5C, the members 521 and 522 slide on the current collector 21B in a direction away from the rectangular electrode composition 22C. This allows the electrode composition 22C supplied in a rectangular shape to be removed from the excess while leaving only the portion included in the specified range, and to shape the two sides corresponding to the downstream side Da1 and the upstream side Da2. Specifically, the members 521 and 522 can remove the portion P2 and the portion P3 shown in Fig. 4A, the scattered electrode composition 22C, and the like as the excess, and can shape the rectangular electrode composition 22C supplied.

[0085] As in the case of the members 511 and 512, the mechanism for operating the members 521 and 522 is not particularly limited. In addition, in Figs. 5A to 5C, the two sides of the electrode composition 22C supplied in a rectangular shape, which correspond to the downstream side Da1 and the upstream side Da2 in the conveying direction Da, are shaped, but the embodiment is not limited thereto. For example, the member 522 may be omitted in Figs. 5A to 5C, and only one side corresponding to the downstream side Da1 may be shaped. In addition, members similar to the members 521 and 522 may be further provided on two sides corresponding to the width direction, so that the four sides of the electrode composition 22C supplied in a rectangular shape may be shaped. In addition to the above-mentioned example, any one, two, or three sides of the electrode composition 22C supplied in a rectangular shape may be shaped. That is, the shaping device 500 of the second embodiment shapes at least one side of the electrode composition 22C supplied in a rectangular shape. The shaping process in FIGS. 5A to 5C may be performed consecutively with a compression process by the press device 400 or may be performed after the sheet is divided into individual sheets.

[0086] Third embodiment In the above-mentioned first and second embodiments, an example has been described in which the shaping device 500 shaping the electrode composition 22C, and then the frame body supplying device 600 supplies the frame body 35. In the third embodiment, as shown in Fig. 6, an example will be described in which the shaping device 500 shaping the electrode composition 22C after the frame body supplying device 600 supplies the frame body 35.

[0087] Fig. 7A shows a state in which electrode composition 22C is supplied by electrode composition supplying device 300, and frame body 35 is supplied by frame body supplying device 600. Fig. 7A also shows a case in which the dimension of electrode composition 22C supplied in a rectangular shape in the conveying direction Da is shorter than a predetermined dimension, and gaps P4 and P5 are generated between electrode composition 22C and frame body 35. In this case, stress that would normally be distributed to electrode composition 22C is concentrated on current collector 21B, which may cause current collector 21B to break.

[0088] Therefore, the shaping device 500 of the third embodiment shapes at least one side of the electrode composition 22C supplied in a rectangular shape by supplying the filler R into the gap between the electrode composition 22C and the frame 35. That is, the shaping device 500 of the third embodiment supplies the filler R to expand the electrode composition 22C so as to make up for the shortage with respect to a predetermined dimension, thereby improving the dimensional accuracy.

[0089] Specifically, the shaping device 500 includes a filler supplying device 531 shown in Fig. 7B. The filler supplying device 531 has, for example, a tubular tip, and can supply the filler R so as to fill the gap between the electrode composition 22C and the frame 35. The type of the filler R is not particularly limited, but as an example, a UV (UltraViolet) curing resin, a two-part mixed resin, or the like can be used.

[0090] For example, the filling material supplying device 531 includes a tubular member through which the filling material R can pass, and a distance sensor. In this case, the filling material supplying device 531 measures the distance to the electrode composition 22C with the distance sensor while moving the position Db1 above the electrode composition 22C in parallel in the conveying direction Da and the width direction. Here, when there is a gap between the electrode composition 22C and the frame 35, the measured distance is longer than when there is no gap, so that the presence of the gap can be detected. Then, when the presence of the gap is detected, the filling material supplying device 531 supplies the filling material R from the tubular member to the detected gap.

[0091] As another example, the filling material supplying device 531 includes a tubular member through which the filling material R can pass, and a camera capable of photographing the electrode composition 22C supplied in a rectangular shape. In this case, the filling material supplying device 531 analyzes the image photographed by the camera to identify the presence and location of a gap. Then, the filling material supplying device 531 supplies the filling material R from the tubular member to the gap whose location has been identified.

[0092] The first to third embodiments described above can be appropriately combined. For example, as shown in Figs. 4A to 4C, the shaping device 500 slides a member 511 or the like in a direction toward the rectangular electrode composition 22C to compact and shape at least one side of the rectangular electrode composition 22C. Alternatively, as shown in Figs. 5A to 5C, the shaping device 500 inserts a blade-shaped member 521 or the like into the rectangular electrode composition 22C and slides it in a direction away from the rectangular electrode composition 22C to remove excess electrode composition 22C from at least one side of the rectangular electrode composition 22C to shape it. Next, the frame supplying device 600 supplies a frame 35 to a position surrounding the rectangular electrode composition 22C. Next, as shown in FIGS. 7A to 7B, the shaping device 500 supplies a filling material R to the gap between the electrode composition 22C and the frame 35, thereby shaping at least one side of the electrode composition 22C supplied in a rectangular shape.

[0093] Shaping device 500 may determine whether to perform the process shown in FIGS. 4A to 4C, the process shown in FIGS. 5A to 5C, or the process shown in FIGS. 7A to 7B.

[0094] For example, the shaping device 500 performs shaping by the process shown in FIG. 7A to FIG. 7B after supplying the frame 35 for the sides of the electrode composition 22C supplied in a rectangular shape that do not reach the predetermined dimension. On the other hand, the shaping device 500 performs shaping by the process shown in FIG. 4A to FIG. 4C or the process shown in FIG. 5A to FIG. 5C before supplying the frame 35 for the sides of the electrode composition 22C supplied in a rectangular shape that exceed the predetermined dimension. For example, the process shown in FIG. 4A to FIG. 4C does not result in waste of the electrode composition 22C, which is preferable from the viewpoint of yield. However, in the case where the predetermined dimension is significantly exceeded, it is more reliable to remove the excess as shown in FIG. 5A to FIG. 5C rather than compressing as shown in FIG. 4A to FIG. 4C. Therefore, the shaping device 500 may set a threshold value and determine whether to perform the process shown in FIG. 4A to FIG. 4C or the process shown in FIG. 5A to FIG. 5C depending on how much the predetermined dimension is exceeded.

[0095] In the above embodiment, the strip-shaped base film to which the electrode composition 22C is supplied is described as the strip-shaped current collector 21B, but the present invention is not limited to this. For example, instead of the strip-shaped current collector 21B shown in FIG. 2, a strip-shaped separator sheet or a strip-shaped release film may be used as the base film. The strip-shaped separator sheet can be trimmed later to form the separator 30 shown in FIG. 1.

[0096] For example, when a separator sheet is used as the base film, electrode composition 22C is supplied onto the separator sheet, current collector 21B is supplied onto the surface of electrode composition 22C opposite the separator sheet, the separator sheet and current collector 21B are trimmed to a predetermined shape, and further, a frame 35 is supplied, thereby making it possible to produce positive electrode 20a or negative electrode 20b.

[0097] When a release film is used as the base film, the electrode composition 22C is supplied onto the release film, the current collector 21B is supplied to the surface of the electrode composition 22C opposite the release film, the release film is collected, and then a separator sheet is supplied to the surface opposite the current collector 21B, the current collector 21B and the separator sheet are trimmed to a predetermined shape, and further a frame 35 is supplied, thereby making it possible to produce the positive electrode 20a or the negative electrode 20b. Note that instead of supplying a separator sheet and then trimming it, a separator 30 may be supplied to the electrode composition 22C.

[0098] Alternatively, the positive electrode 20a or the negative electrode 20b can be produced by supplying the electrode composition 22C onto a release film, supplying a separator sheet onto the surface of the electrode composition 22C opposite the release film, collecting the release film, supplying the current collector 21B onto the surface opposite the separator sheet, trimming the separator sheet and the current collector 21B into a predetermined shape, and further supplying a frame 35. Note that instead of supplying the current collector 21B and then trimming it, the current collector 21 trimmed into a predetermined shape may be supplied to the electrode composition 22C.

[0099] Although the embodiment of the present invention has been described above in detail with reference to the drawings, the specific configuration is not limited to this embodiment, and the changes, combinations, deletions, etc. of the configurations within the scope of the present invention are also included. Furthermore, it goes without saying that the configurations shown in each embodiment can be used in appropriate combination. When the lithium ion secondary battery exemplified in the above description is used among the secondary batteries, it includes a battery using a liquid material for the electrolyte and a battery using a solid material for the electrolyte (so-called all-solid-state battery). Furthermore, the battery in this embodiment includes a battery having a metal foil (metal current collector foil) as a current collector, and includes a battery having a so-called resin current collector made of a resin to which a conductive material has been added instead of the metal foil. When the resin current collector is used as a resin current collector for a bipolar electrode, a positive electrode may be formed on one side of the resin current collector and a negative electrode may be formed on the other side to form a bipolar electrode. The battery in this embodiment includes a battery in which an electrode is formed by applying a positive or negative electrode active material, etc. to a positive or negative electrode current collector, respectively, using a binder, and in the case of a bipolar battery, includes a battery in which a bipolar electrode is formed by applying a positive electrode active material, etc. to one side of a current collector using a binder to form a positive electrode layer, and applying a negative electrode active material, etc. to the opposite side using a binder to form a negative electrode layer. [Explanation of symbols]

[0100] 10: Single cell 20: Electrode 20a: Positive electrode 20b: Negative electrode 21: Current collector 21a: Positive electrode current collector layer 21b: Negative electrode current collector layer 21B: Strip-shaped current collector 21R: Current collector roll 22: Electrode active material layer 22a: Positive electrode active material layer 22b: Negative electrode active material layer 22C: Electrode composition 30: Separator 35:Frame body 100: Chamber 200: Transport device 300: Electrode composition supply device 400: Press equipment 401: Upper roller 402: Lower roller 500: Shaping device 511, 512, 521, 522: Materials 531: Filler supply device 600:Frame supply device 1000:Battery electrode manufacturing equipment P1, P2, P3: Partial P4, P5: Gap R: Filler Da: Transport direction Da1: downstream Da2: Upstream Db: Vertical direction Db1: Upper side Db2: Bottom

Claims

1. an electrode composition supply unit that supplies an electrode composition containing an active material in a rectangular shape to the transported base film; a shaping unit that shapes at least one side of the electrode composition on the substrate film; An apparatus for manufacturing a battery electrode comprising:

2. The battery electrode manufacturing apparatus according to claim 1 , wherein the shaping unit slides over the base film in a direction approaching the electrode composition to compress and shape at least one side of the electrode composition.

3. 2. The battery electrode manufacturing apparatus according to claim 1, wherein the shaping unit removes excess electrode composition from at least one side of the electrode composition by sliding a blade-shaped member over the base film in a direction away from the electrode composition.

4. A frame supply unit supplies a frame to a position surrounding the electrode composition supplied in a rectangular shape, 2. The battery electrode manufacturing apparatus according to claim 1, wherein the shaping unit shapes at least one side of the electrode composition supplied in a rectangular shape by supplying a filler into a gap between the electrode composition and the frame.

5. The battery electrode manufacturing apparatus according to claim 1 , wherein the shaping unit shapes one side of the electrode composition supplied in a rectangular shape, the side corresponding to an upstream side in a conveying direction of the base film by a conveying unit.

6. 2 . The battery electrode manufacturing apparatus according to claim 1 , wherein the shaping section shapes two sides of the electrode composition supplied in a rectangular shape, the sides corresponding to the upstream side and the downstream side in a conveying direction of the base film by the conveying section.

7. The battery electrode manufacturing apparatus according to claim 1 , wherein the shaping unit shapes four sides of the electrode composition supplied in a rectangular shape.

8. A compression unit that compresses the electrode composition supplied in a rectangular shape is further provided, The battery electrode manufacturing apparatus according to claim 1 , wherein the shaping section shapes at least one side of the electrode composition after compression by the compression section.

9. a supplying step of supplying an electrode composition containing an active material in a rectangular shape onto a belt-shaped base film being transported; a shaping step of shaping at least one side of the electrode composition on the substrate film.

Citation Information

Patent Citations

  • Method for manufacturing electrode material for lithium ion battery, and device for manufacturing electrode material for lithium ion battery

    JP2021027043A

  • Battery manufacturing method

    JP6633866B2